A piezoelectric energy collector with a hollow portion and a preparation method thereof

By designing hollow parts and combined mass on the MEMS linear cantilever beam structure, the problems of stress concentration and high natural frequency are solved, the efficiency and stability of the piezoelectric energy harvester are improved, and a wider application is achieved.

CN112564546BActive Publication Date: 2024-11-22SHANGHAI INST OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011530916.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-22
Publication Date
2024-11-22
Estimated Expiration
2040-12-22

AI Technical Summary

Technical Problem

The existing MEMS linear cantilever beam structure is concentrated during external excitation, resulting in a narrow effective area of ​​the piezoelectric material, affecting the energy collection efficiency, and high natural frequency, making it difficult to match the resonant frequency in the natural environment, limiting its application.

Method used

Design a piezoelectric energy harvester with hollowed-out part. By forming grooves on the silicon substrate and hollowing out using a KrF excimer laser, a trapezoidal hollow part is formed, combining the upper and lower mass blocks to reduce the natural frequency and uniformize the stress. distributed.

Benefits of technology

It effectively improves the output efficiency of the piezoelectric energy harvester, reduces the natural frequency, increases the stability and application value of the device, and achieves high-precision and large-scale production through micro-processing processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112564546B_ABST
    Figure CN112564546B_ABST
Patent Text Reader

Abstract

The present invention relates to a piezoelectric energy harvester with a hollowed-out portion and a preparation method thereof, the method comprising: S1: obtaining a silicon substrate, cleaning and drying the silicon substrate; S2: obtaining a PZT piezoelectric layer, and respectively plating a metal layer on the upper side of the silicon substrate obtained in step S1 and the lower side of the PZT piezoelectric layer; S3: eutectic bonding the metal layers of the silicon substrate and the PZT piezoelectric layer; S4: grinding and thinning the upper side of the PZT piezoelectric layer to a preset thickness range; S5: etching the lower surface of the silicon substrate to obtain a groove; S6: using a KrF excimer laser to perform a hollowing process in the groove area to form a hollowed-out portion to obtain the final piezoelectric energy harvester. Compared with the prior art, the present invention has the advantages of fewer process steps, simple processing, low natural frequency, and high power output.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of piezoelectric energy harvesters, and in particular to a piezoelectric energy harvester with a hollow portion and a preparation method thereof. Background Art

[0002] Among the many MEMS structures in the field of piezoelectric energy harvesting, the linear cantilever beam structure has become the preferred structural type for piezoelectric energy harvesters because of its advantages such as low structural stiffness, high sensitivity and easy realization through micro-machining.

[0003] However, when MEMS linear cantilever beams are stimulated by external forces, their stress is mostly concentrated at the fixed end, resulting in a very narrow effective area of ​​the piezoelectric material, which seriously affects the energy production efficiency of energy harvesting devices. In addition, due to the limited size of traditional linear cantilever beams, their natural frequency is very high and it is difficult to match the resonant frequency existing in the natural environment, which greatly restricts their application. Summary of the invention

[0004] The purpose of the present invention is to overcome the defects of the above-mentioned prior art and to provide a piezoelectric energy harvester with a hollow portion and a preparation method thereof to improve the output efficiency of the piezoelectric energy harvester.

[0005] The purpose of the present invention can be achieved by the following technical solutions:

[0006] A piezoelectric energy harvester with a hollow portion comprises a silicon substrate, a metal layer and a PZT piezoelectric layer which are arranged in sequence from bottom to top, wherein the silicon substrate and the PZT piezoelectric layer are connected by eutectic bonding through the metal layer, a groove is provided on the lower side of the middle portion of the silicon substrate, and the hollow portion penetrating the silicon substrate, the metal layer and the PZT piezoelectric layer is provided in the groove region.

[0007] Furthermore, the silicon substrate is formed with a fixed end and a free end on both sides of the groove, respectively; the upper side of the free end is connected to an upper mass block, and the lower side is connected to a lower mass block.

[0008] Furthermore, the upper mass block and the lower mass block are respectively bonded to free ends of the silicon substrate.

[0009] Furthermore, the shape of the hollow portion is trapezoidal.

[0010] Furthermore, the hollow portion is provided with rounded corners.

[0011] Furthermore, the material of the metal layer is Cr or Au.

[0012] The present invention also provides a method for preparing a piezoelectric energy harvester provided with a hollow portion, comprising the following steps:

[0013] S1: obtaining a silicon substrate, and performing cleaning and drying treatment on the silicon substrate;

[0014] S2: Obtain a PZT piezoelectric layer, and respectively plate a metal layer on the upper side of the silicon substrate and the lower side of the PZT piezoelectric layer obtained in step S1;

[0015] S3: eutectic bonding the silicon substrate and the metal layer of the PZT piezoelectric layer;

[0016] S4: grinding and thinning the upper side of the PZT piezoelectric layer to a preset thickness range;

[0017] S5: etching the lower surface of the silicon substrate to obtain a groove;

[0018] S6: A KrF excimer laser is used to perform a hollowing process in the groove area to form a hollow portion, thereby obtaining a final piezoelectric energy harvester.

[0019] Furthermore, the step S4 further includes: using the silicon substrate as a fixed end and a free end on both sides of the groove, and connecting an upper mass block and a lower mass block on the upper side and the lower side of the free end, respectively.

[0020] Furthermore, the step S4 specifically includes firstly using a grinding device equipped with a diamond abrasive suspension to mechanically grind the PZT piezoelectric layer, and then using a grinding paste to finely grind the PZT piezoelectric layer.

[0021] Furthermore, the grinding device uses a metal grinding disc with a rotation speed of 100 to 140 r / min and a grinding head with a rotation speed set to 60 to 100 r / min. After the mechanical grinding, the PZT piezoelectric layer is thinned to within the range of 50 to 200 um. After the fine grinding, the PZT piezoelectric layer is thinned to within the range of 20 to 45 um.

[0022] Furthermore, in step S6, during the hollowing process, the KrF excimer laser is set to a scanning speed within the range of 80 to 150 m / s, a scanning frequency within the range of 120 to 200 Hz, and a laser pulse energy within the range of 9 to 15 mJ / pulse.

[0023] Furthermore, in step S6, during the hollowing process, the materials of the upper mass block and the lower mass block are both nickel or tungsten.

[0024] Furthermore, in step S1, the thickness of the silicon substrate is within the range of 400 to 1000 um, and the cleaning and drying treatments are specifically performed by first performing ultrasonic cleaning for 1 to 2 minutes and then performing drying treatment for 1 to 2 minutes.

[0025] Furthermore, in step S2, the thickness of the metal layer is within the range of 10 to 80 um, and the metal layer is evaporated using a vacuum evaporation device. The current of the evaporation process is 50 to 80 A, and the time is 40 to 60 s.

[0026] Furthermore, in step S3, the temperature is maintained at 500-600° C. and the pressure is set at 660-800 mbar during the eutectic bonding process, and the bonding is cooled to room temperature after the bonding is completed.

[0027] Compared with the prior art, the present invention has the following advantages:

[0028] (1) Compared with the prior art, the present invention overcomes the problem of excessive stress concentration in traditional piezoelectric linear cantilever beams, and can produce a relatively uniform stress range on both sides of the hollow shape, thereby improving the output efficiency of the energy harvester; at the same time, compared with the defect of high natural frequency of traditional cantilever beams, the device can effectively reduce the natural frequency and has a wider application value in natural environments and daily life.

[0029] (2) By setting the bottom corner of the trapezoid to a rounded corner, the stress at the sharp corner is dispersed, which effectively reduces the possibility of the device being broken during the excitation process and increases the stability of the device.

[0030] (3) The preparation method provided by the present invention combines KrF excimer laser processing and micro-machining (MEMS process), and the prepared trapezoidal hollow piezoelectric energy harvester has high precision, good repeatability, can be mass-produced and has high flexibility. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 It is a schematic structural diagram of a piezoelectric energy harvester with a hollow portion in an embodiment of the present invention;

[0032] Figure 2 A schematic diagram of the dimensions of a piezoelectric energy harvester with a hollow portion in an embodiment of the present invention;

[0033] Figure 3 It is a flow chart of a method for preparing a piezoelectric energy harvester with a hollow portion according to an embodiment of the present invention;

[0034] Figure 4 The voltage output of the piezoelectric energy harvester with a hollow portion in the embodiment of the present invention;

[0035] In the figure, 1, elastic layer, 2, fixed end, 3, hollow part, 4, rounded corner, 5, upper mass block, 6, lower mass block, 7, silicon substrate, 8, metal layer, 9, PZT piezoelectric layer. DETAILED DESCRIPTION

[0036] The present invention is described in detail below in conjunction with the accompanying drawings and specific embodiments. This embodiment is implemented based on the technical solution of the present invention, and provides a detailed implementation method and specific operation process, but the protection scope of the present invention is not limited to the following embodiments.

[0037] Example 1

[0038] The present embodiment provides a piezoelectric energy harvester with a hollow portion, comprising a silicon substrate 7, a metal layer 8 and a PZT piezoelectric layer 9 arranged in sequence from bottom to top, the silicon substrate 7 and the PZT piezoelectric layer 9 are eutectic bonded through the metal layer 8, a groove is provided on the lower middle side of the silicon substrate 7, the groove area is provided with a hollow portion 3 that penetrates the silicon substrate 7, the metal layer 8 and the PZT piezoelectric layer 9, and the material of the metal layer 8 is Cr or Au.

[0039] As a preferred embodiment, the silicon substrate 7 is formed with a fixed end 2 and a free end on both sides of the groove, the upper side of the free end is connected to an upper mass block 5, and the lower side is connected to a lower mass block 6, and the upper mass block 5 and the lower mass block 6 can be connected to the free end of the silicon substrate 7 by bonding. In the embodiment, the model of the PZT piezoelectric layer 9 is PZT-5H, and the elastic modulus C of PZT-5H is 11 and C 12 are 120.3 GPa and 80.2 GPa respectively, and the piezoelectric constant is e 31 -5.4C / m 2 , dielectric constant ε 33 is 1433.6, the vacuum dielectric constant ε 0 It is 8.85×10-12F / m.

[0040] As a preferred embodiment, the shape of the hollow portion 3 is rectangular or trapezoidal, preferably trapezoidal.

[0041] As a preferred embodiment, the hollow portion 3 is provided with rounded corners 4. When the shape of the hollow portion 3 is a trapezoid, the two lower bottom corners of the trapezoid are rounded corners with a radius between 0.1 and 2 mm.

[0042] An optimal implementation can be obtained by combining the preferred implementations of the piezoelectric energy harvester. The working principle of the piezoelectric energy harvester obtained by the optimal implementation is described below.

[0043] The device is connected to a vibration source through a fixed end, and the vibration source drives the device to vibrate, so that the elastic layer of the cantilever beam, i.e., the piezoelectric layer 1 and the Si layer 2, generates a large stress, so that the positive and negative charges inside the piezoelectric material are separated, thereby generating energy, and the device is designed to match the frequency of the vibration source, causing the resonance of the device to achieve maximum output energy efficiency. The trapezoidal hollowing 3 operation performed by laser makes the stress concentrated at the fixed end uniform, which can greatly improve the utilization efficiency of the piezoelectric layer material. The natural frequency of the device is reduced by bonding the upper mass block 5 and the lower mass block 6.

[0044] This embodiment also provides a method for preparing a piezoelectric energy harvester having a hollow portion, comprising the following steps:

[0045] S1: Obtain a silicon substrate 7, and perform cleaning and drying treatment on the silicon substrate 7;

[0046] S2: Obtain a PZT piezoelectric layer 9, and respectively plate a metal layer 8 on the upper side of the silicon substrate 7 obtained in step S1 and on the lower side of the PZT piezoelectric layer 9;

[0047] S3: eutectic bonding the silicon substrate 7 and the metal layer 8 of the PZT piezoelectric layer 9;

[0048] S4: grinding and thinning the upper side of the PZT piezoelectric layer 9 to a preset thickness range;

[0049] S5: etching the lower surface of the silicon substrate 7 to obtain a groove;

[0050] S6: Use a KrF excimer laser to perform hollowing processing in the groove area to form a hollow portion 3 to obtain a final piezoelectric energy harvester.

[0051] In the preparation method, the most critical step is KrF excimer laser processing, which has the characteristics of high power peak and large pulse energy, and can be flexibly applied to the processing of PZT materials. The number of scans, the energy of the laser beam and the movement parameters are set according to the thickness of the elastic layer to be hollowed out to achieve the processing purpose. Traditional PZT processing often uses slicing and etching methods. However, the traditional cutting method has too much concentrated stress, which can easily cause cracks in the PZT material, and the mechanical slicing method is difficult to achieve complex shape processing. The etching method has a long product cycle and high cost, which is not suitable for large-scale PZT hollowing process processing.

[0052] The piezoelectric energy harvester with a hollow portion obtained by the above preparation method comprises a silicon substrate obtained by a micromachining process, a PZT piezoelectric layer and the mass block; the mass block is bonded to the tail end of the free end of the device.

[0053] As a preferred implementation, step S4 further includes: using the silicon substrate 7 as a fixed end 2 and a free end on both sides of the groove, and connecting an upper mass block 5 and a lower mass block 6 on the upper side and the lower side of the free end, respectively.

[0054] As a preferred implementation, step S4 specifically includes firstly mechanically grinding the PZT piezoelectric layer 9 with a grinding device equipped with a diamond abrasive suspension, and then finely grinding the PZT piezoelectric layer 9 with a grinding paste.

[0055] Furthermore, as a preferred embodiment, the grinding device uses a metal grinding disc with a rotation speed of 100 to 140 r / min and a grinding head with a rotation speed set to 60 to 100 r / min. After mechanical grinding, the PZT piezoelectric layer 9 is thinned to within the range of 50 to 200 um. After fine grinding, the PZT piezoelectric layer 9 is thinned to within the range of 20 to 45 um.

[0056] As a preferred embodiment, in step S6, during the hollowing process, the KrF excimer laser is set to a scanning speed within the range of 80 to 150 m / s, a scanning frequency within the range of 120 to 200 Hz, and a laser pulse energy within the range of 9 to 15 mJ / pulse.

[0057] As a preferred implementation, in step S6, during the hollowing process, the materials of the upper mass block 5 and the lower mass block 6 are both nickel or tungsten.

[0058] As a preferred implementation, in step S1, the thickness of the silicon substrate 7 is within the range of 400 to 1000 um, and the cleaning and drying treatments are specifically performed by first performing ultrasonic cleaning for 1 to 2 minutes and then performing drying treatment for 1 to 2 minutes.

[0059] As a preferred embodiment, in step S2, the thickness of the metal layer 8 is within the range of 10 to 80 um, and the metal layer 8 is evaporated using a vacuum evaporation device. The current of the evaporation process is 50 to 80 A and the time is 40 to 60 s.

[0060] As a preferred embodiment, in step S3, the temperature is maintained at 500-600° C. and the pressure is set at 660-800 mbar during the eutectic bonding process, and the bonding is cooled to room temperature after the bonding is completed.

[0061] An optimal implementation can be obtained by combining the preferred implementations in the preparation method, and the optimal implementation is described in detail below.

[0062] A method for preparing a piezoelectric energy harvester with a hollow portion comprises the following steps:

[0063] 1) Select a silicon substrate of 400-1000um, perform ultrasonic cleaning for 1-2 minutes, and then dry it for 1-2 minutes;

[0064] 2) Using a vacuum evaporation device, a 10-80 μm metal layer 8 is evaporated on the upper side of the silicon substrate 7 and the lower side of the PZT piezoelectric layer 9, the current is 50-80 A, the time is 40-60 seconds, and the material of the metal layer 8 is Cr or Au;

[0065] 3) Bond the evaporated PZT-Au and Au-Si eutectic, keep the temperature at 500-600°C and the pressure at 660-800mbar, and cool to room temperature after bonding;

[0066] 4) Prepare a diamond abrasive suspension, use a metal grinding disc at a speed of 100 to 140 r / min and a grinding head at a speed of 60 to 100 r / min, control the thinning thickness by a thickness measuring instrument, use a mechanical grinding method to thin the PZT piezoelectric layer 9 to 50 to 200 um, and then use a grinding paste to finely thin the PZT to 20 to 45 um;

[0067] 5) performing deep reactive ion etching on the lower surface of the silicon substrate 7 to form an elastic layer 1 structure, wherein the elastic layer 1 corresponds to the integral structure of the metal layer and the PZT piezoelectric layer 9 in the groove region formed by etching the silicon substrate 7;

[0068] 6) bonding the upper mass block 5 and the lower mass block 6 to the tail of the cantilever beam to obtain the linear cantilever beam piezoelectric energy harvesting device;

[0069] 7) A KrF excimer laser is used to perform trapezoidal hollowing at the elastic layer 1 with the bottom corners all being rounded 4. The operating conditions are set to a scanning speed of 80 to 150 m / s, a scanning frequency of 120 to 200 Hz, and a laser pulse energy of 9 to 15 mJ / pulse. The scanning is repeated until penetration occurs to form the trapezoidal hollow piezoelectric energy harvester.

[0070] A best example of this optimal implementation is provided below.

[0071] like Figure 3 As shown, a method for preparing a piezoelectric energy harvester with a hollow portion comprises the following steps:

[0072] A1: Select a 400um silicon substrate 7 and perform ultrasonic cleaning for 2 minutes, followed by drying for 2 minutes;

[0073] A2: Use a vacuum evaporation device to evaporate a 20 μm Cr / Au metal layer 8 on the upper part of the silicon substrate 7 and the upper and lower parts of the PZT piezoelectric layer 9, with a current of 65 A for 50 seconds;

[0074] A3: Bond the evaporated bulk PZT-Au to the Au-Si eutectic. The temperature is kept at 550°C and the pressure is set at 760mbar. After bonding, it is cooled to room temperature.

[0075] A4: Prepare diamond abrasive suspension, use a metal grinding disc at a speed of 120r / min and a grinding head at a speed of 80r / min, control the thinning thickness through a thickness measuring instrument, use mechanical grinding to thin the block PZT piezoelectric layer 9 to 50um, and then use grinding paste to finely thin the PZT piezoelectric layer 9 to 40um;

[0076] A5: performing deep reactive ion etching on the lower surface of the silicon substrate 7 to form an elastic layer 1 structure;

[0077] A6: bonding the upper mass block 5 and the lower mass block 6 to the tail of the cantilever beam to obtain the linear cantilever beam piezoelectric energy harvesting device;

[0078] A7: A KrF excimer laser is used to perform a trapezoidal hollowing 3 operation with the bottom corners all being rounded 4 at the elastic layer 1. The conditions are set to a scanning speed of 100 m / s, a scanning frequency of 200 Hz and a laser pulse energy of 11 mJ / pulse. The scanning is repeated until penetration occurs, thereby forming the trapezoidal hollow piezoelectric energy harvesting device.

[0079] In the embodiment, the model of the PZT piezoelectric layer 9 is PZT-5H, and the elastic modulus C of PZT-5H is 11 and C 12 are 120.3 GPa and 80.2 GPa respectively, and the piezoelectric constant is e 31 -5.4C / m 2 , dielectric constant ε 33 is 1433.6, the vacuum dielectric constant ε 0 It is 8.85×10-12F / m.

[0080] according to Figure 4 As shown, the voltage output of the piezoelectric energy harvester with a hollowed-out portion in the embodiment of the present invention shows that, compared with the non-hollowed-out device, the natural frequency of the hollowed-out device is reduced by 30% and the peak voltage output is increased by 89%.

[0081] like Figure 1 and 2 As shown, the dimensions of the piezoelectric energy harvester obtained by this preparation method are shown in Table 1.

[0082] Table 1

[0083]

[0084] Compared with the prior art, this embodiment breaks through the problem of excessive stress concentration in traditional piezoelectric linear cantilever beams, and can produce a relatively uniform stress range on both sides of the hollow shape, thereby improving the output efficiency of the energy harvester. By setting the bottom corner of the trapezoid as a rounded corner, the stress at the sharp corner is dispersed, effectively reducing the possibility of the device being broken during the excitation process, and increasing the stability of the device. At the same time, compared with the defect of the high natural frequency of the traditional cantilever beam, the device can effectively reduce the natural frequency and has a wider application value in the natural environment and daily life. And through the combination with the micro-machining process, the device has the advantages of simple preparation and operation and mass production.

[0085] Compared with the currently manufactured linear cantilever piezoelectric energy harvesters, the method of using a trapezoidal hollow elastic layer can improve the energy harvesting efficiency and reduce its natural frequency. The operation of converting the lower bottom angle of the trapezoid into a rounded corner can improve the stability and service life of the device. The method of hollowing out PZT using a KrF excimer laser has high efficiency, high yield rate, and strong operability. It has the advantage of mass production when combined with micro-machining technology, and a large number of hollow cantilever piezoelectric energy harvesting devices can be obtained at one time.

[0086] The preferred specific embodiments of the present invention are described in detail above. It should be understood that a person skilled in the art can make many modifications and changes based on the concept of the present invention without creative work. Therefore, any technical solution that can be obtained by a person skilled in the art through logical analysis, reasoning or limited experiments based on the concept of the present invention on the basis of the prior art should be within the scope of protection determined by the claims.

Claims

1. A piezoelectric energy harvester with a hollow portion, characterized in that: The invention comprises a silicon substrate (7), a metal layer (8) and a PZT piezoelectric layer (9) which are arranged in sequence from bottom to top, wherein the silicon substrate (7) and the PZT piezoelectric layer (9) are eutectic bonded via the metal layer (8), a groove is provided at the lower middle side of the silicon substrate (7), and a hollow portion (3) is provided in the groove region which penetrates the silicon substrate (7), the metal layer (8) and the PZT piezoelectric layer (9); The silicon substrate (7) is formed with a fixed end (2) and a free end on both sides of the groove, respectively; the upper side of the free end is connected to an upper mass block (5), and the lower side is connected to a lower mass block (6); The shape of the hollow portion (3) is a closed trapezoidal structure.

2. A piezoelectric energy harvester with a hollow portion according to claim 1, characterized in that: The hollow portion (3) is provided with rounded corners (4).

3. The piezoelectric energy harvester with a hollow portion according to claim 1, characterized in that: The material of the metal layer (8) is Cr or Au.

4. A method for preparing a piezoelectric energy harvester with a hollow portion as claimed in any one of claims 1 to 3, characterized in that: The following steps are involved: S1: obtaining a silicon substrate (7), and performing cleaning and drying treatment on the silicon substrate (7); S2: obtaining a PZT piezoelectric layer (9), and respectively plating a metal layer (8) on the upper side of the silicon substrate (7) and the lower side of the PZT piezoelectric layer (9) obtained in step S1; S3: eutectic bonding the silicon substrate (7) and the metal layer (8) of the PZT piezoelectric layer (9); S4: grinding and thinning the upper side of the PZT piezoelectric layer (9) to a preset thickness range; S5: etching the lower surface of the silicon substrate (7) to obtain a groove; S6: using a KrF excimer laser to perform a hollowing process in the groove area to form a hollowing portion (3), thereby obtaining a final piezoelectric energy harvester.

5. The method according to claim 4, characterized in that The step S4 further comprises: using the silicon substrate (7) as a fixed end (2) and a free end on both sides of the groove, and connecting an upper mass block (5) and a lower mass block (6) on the upper side and the lower side of the free end, respectively.

6. The method according to claim 5, characterized in that In step S6, during the hollowing process, the materials of the upper mass block (5) and the lower mass block (6) are both nickel or tungsten.

7. The method according to claim 4, characterized in that Specifically, the step S4 comprises firstly using a grinding device equipped with a diamond abrasive suspension to mechanically grind the PZT piezoelectric layer (9), and then using a grinding paste to finely grind the PZT piezoelectric layer (9).

8. The method according to claim 4, characterized in that In step S6, during the hollowing process, the KrF excimer laser is set to a scanning speed within the range of 80 to 150 m / s, a scanning frequency within the range of 120 to 200 Hz, and a laser pulse energy within the range of 9 to 15 mJ / pulse.