A polymer micelle freeze-dried preparation of taxane anti-tumor drug for injection

By adding povidone to the polymer micelle solution of taxane antitumor drugs, and using film hydration method and freeze-drying technology, the problem of poor stability of micellar preparations at room temperature was solved and drug micelles were realized. Improved long-term stability, suitable for a variety of poorly soluble drugs.

CN114246831BActive Publication Date: 2024-10-15LUNAN PHARMA GROUP CORPORATION
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010999347.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-09-22
Publication Date
2024-10-15
Estimated Expiration
2040-09-22

AI Technical Summary

Technical Problem

The existing polymer micellar preparations of taxane antitumor drugs have poor stability at room temperature and are difficult to maintain clear and transparent for a long time, affecting the safety and efficacy of the drugs.

Method used

By adding povidone to the micellar solution to improve its stability, the polymer micelle freeze-dried formulation of taxane antitumor drugs is prepared using thin film hydration method and freeze-drying technology to ensure long-term stability at room temperature. sex.

Benefits of technology

The stability of taxane drug micelles is significantly improved. The prepared preparation can maintain stability for more than 8 days at room temperature, which is better than the existing technology and is suitable for a variety of poorly soluble drugs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0002693722050000091
    Figure BDA0002693722050000091
Patent Text Reader

Abstract

The present invention provides a taxane polymer micelle lyophilized preparation, comprising a taxane drug, polyvidone, and a polyether / polyester block copolymer; and provides a related preparation method. The taxane polymer micelle lyophilized preparation of the present invention improves the safety of medication and greatly improves the stability of the drug solution.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of pharmaceutical preparations, and in particular relates to a taxane polymer micelle freeze-dried preparation for injection. Background Art

[0002] In clinical oncology, chemotherapy is the main treatment approach. However, traditional chemotherapy agents, such as small molecule anti-tumor drugs, have not achieved good therapeutic effects due to their low solubility, poor stability, rapid degradation rate and non-targeted tissue distribution, and also have serious adverse reactions. At present, most anti-tumor drugs used in clinical practice are hydrophobic drugs, such as paclitaxel and docetaxel of the taxane class, and hydroxycamptothecin; although the above drugs have been widely used in clinical practice, the commercial preparations still have many problems as follows, such as the commercial preparation Taxol, which is a colorless viscous solution made of polyoxyethylene castor oil / anhydrous ethanol (50 / 50). However, the polyoxyethylene castor oil in the preparation causes serious side effects in patients, such as allergic reactions, neurotoxicity and nephrotoxicity. The commercially available preparation of docetaxel also contains a high concentration of Tween-80 as a solubilizer. A large amount of Tween can easily cause adverse reactions such as hemolysis and allergies. In order to prevent the occurrence of the above-mentioned allergic reactions, patients need to be pretreated with antiallergic drugs such as dexamethasone before taking the medicine. These problems bring many inconveniences to clinical medication and also seriously affect the efficacy and safety of the drugs.

[0003] In order to reduce the toxicity of paclitaxel preparations and improve their efficacy, new dosage forms of paclitaxel have been developed clinically in recent years. The polymer micelle drug delivery system can effectively improve the solubility of poorly soluble drugs, has good biocompatibility and strong solubilization ability, and has the advantages of protecting the encapsulated drugs, while improving the water solubility of poorly soluble drugs and effectively reducing the toxic side effects of drugs on the human body. In recent years, the research on paclitaxel polymer micelles has received widespread attention. Genexol-PM, a paclitaxel polymer micelle dosage form launched in South Korea, has shown good prospects in preclinical and clinical phase I-III studies in the United States.

[0004] However, after the polymer micelles are prepared into micelle solutions, there is a problem of poor drug solution stability. After being placed at room temperature for a period of time, the drug precipitates, causing the drug solution to become turbid. In order to improve the technical problems of low drug loading and stability of drug-loaded polymer micelles, the prior art attempts to improve the stability of carrier polymers by selecting different polymers, and to add different additives to improve the stability of micelles.

[0005] Chinese patent CN201110105540.2 discloses a polymer micelle freeze-dried preparation of taxane anti-tumor drugs, its preparation method and application, and selects polyether / polyester block copolymer as the micelle carrier material. Chinese patent CN201610802372.5 further optimizes CN201110105540.2, using polyether / polyester block copolymers after ultrafiltration and freeze drying to prepare taxane anti-tumor drug polymer micelles, aiming to reduce the incidence of allergic reactions and improve the safety of taxane anti-tumor drug polymer micelles. Both patents use polyether / polyester block copolymers to form micelles through molecular self-assembly, in which poorly soluble tumor drugs are encapsulated in the hydrophobic core formed by polyester. Patent CN200610145383.7 discloses a paclitaxel mixed polymer micelle with amphiphilic pro-segment copolymer mPEG-PDLLA and phospholipid as carriers; the stability of the mixed polymer micelle is improved compared with the polymer micelle; but when the taxane docetaxel micelle preparation prepared by the same technical scheme, its stability is not improved. Patent CN201010001047.1 discloses a paclitaxel polymer micelle and docetaxel polymer micelle prepared by adding an amino acid preferably arginine with an amphiphilic pro-segment copolymer mPEG-PDLLA as a carrier, and the micelle solution is kept at 25°C for 24 hours, and is visually clear and transparent without precipitation. Patent CN201410196183.9 discloses a paclitaxel micelle using mPEG-PLA-glutamic acid triblock copolymer as a micelle carrier, and its in vitro stability test shows that the maximum stable time at room temperature (25°C) is only 24 hours. Patent CN201510250848.4 discloses a paclitaxel and docetaxel micelle freeze-dried preparation with a polyvidone-polylactic acid block copolymer as a carrier, and its drug loading capacity is improved, but the micelle stability is poor. Therefore, the existing technology attempts to change the stability of taxane micelles, but on the one hand, the stability time is still not ideal; on the other hand, the universality of application is not ideal, especially for taxane drugs, the technical solution of increasing its micelle stability can improve the stability of paclitaxel micelles, but the improvement of the micelle stability of other taxane drugs is not obvious.

[0006] In summary, the stability of the taxane micelles currently prepared still cannot meet the requirements. It is still an urgent problem to study and provide a technical solution for a polymer micelle composition to further improve the stability and be applicable to similar poorly soluble drugs. Summary of the invention

[0007] The purpose of the present invention is to overcome the above-mentioned deficiencies of the prior art and provide a polymer micelle freeze-dried preparation encapsulating taxane anti-tumor drugs. The taxane micelle freeze-dried preparation prepared by the present invention further improves the stability and safety of the drug-loaded micelles.

[0008] The inventor first prepared a micellar solution and then tried to improve the stability of the solution. It was unexpectedly found that after adding povidone, the stability of the solution was greatly improved. Even at room temperature, it still maintained good stability after standing for 180 hours. Based on this experiment, the inventor creatively prepared a stable micellar preparation.

[0009] Specifically, the present invention is achieved through the following technologies:

[0010] The polymer micelle freeze-dried preparation of a taxane anti-tumor drug of the present invention contains a taxane drug, povidone and a polyether / polyester block copolymer.

[0011] Preferably, the povidone is one of povidone K-12, K-17, K-25, K-30, K-90 or a combination thereof; more preferably povidone K-12, K-17, K-25.

[0012] Preferably, the polyether block is polyethylene glycol (PEG), one of polyethylene glycol monomethyl ether, polypropylene glycol or polybutylene glycol, with a number average molecular weight of 1000-5000, preferably polyethylene glycol monomethyl ether with a molecular weight of 2000.

[0013] Preferably, the polyester block is one of polylactide (PDLLA), polyglycolide lactide (PLGA), polycaprolactone (PCL), and polyorthoester (POE), and has a number average molecular weight of 1000-5000, preferably polylactide with a molecular weight of 2000.

[0014] In the polyether / polyester block copolymer of the present invention, the polyether / polyester block copolymer is preferably polyethylene glycol monomethyl ether 2000-polylactide.

[0015] Preferably, the total weight of the polyether blocks accounts for 30% to 70% of the amphiphilic polymer, and more preferably 50%.

[0016] Preferably, the taxane drug is paclitaxel, docetaxel, cabazitaxel or a mixture thereof.

[0017] Preferably, the weight ratio of the taxane drug to the polyether / polyester block copolymer is 1:1-99; further, the weight ratio of the taxane drug to the polyether / polyester block copolymer is preferably 1:4-50.

[0018] Preferably, the weight ratio of the taxane drug to povidone is 1:1-3.

[0019] A further object of the present invention is to provide a method for preparing a polymer micelle freeze-dried preparation of a taxane anti-tumor drug.

[0020] The method for preparing the polymer micelle freeze-dried preparation of the taxane anti-tumor drug of the present invention is a thin film hydration method, which specifically comprises the following steps:

[0021] a) weighing the prescribed amount of taxanes and polyether / polyester block copolymer, adding an organic solvent and ultrasonically heating to dissolve;

[0022] b) concentrating the organic solvent to dryness at room temperature to the boiling point of the organic solvent under normal pressure or reduced pressure to obtain a mixed film;

[0023] c) adding an aqueous solution containing povidone to fully hydrate the film to obtain a transparent drug-loaded micelle solution.

[0024] d) The drug-loaded micelle solution is sterilized, filtered, and freeze-dried to obtain a polymer micelle freeze-dried powder injection loaded with taxane drugs.

[0025] Preferably, the organic solvent is selected from one or two of ethanol, methanol, acetonitrile, acetone, chloroform, and ethyl acetate, and more preferably one or two of ethanol, methanol, and acetonitrile; the amount of the organic solvent is 2 to 10 times the total weight of the taxane and the polyether / polyester block copolymer.

[0026] In the present invention, the micellar solution can be directly freeze-dried or freeze-dried after adding a freeze-dried protective agent. The freeze-dried protective agent used can be selected from any one or a mixture of mannitol, glucose, anhydrous lactose, lactose, trehalose, dextran, glycine, and polyethylene glycol; preferably, the amount of the freeze-dried protective agent is 0.5%-15% of the total amount of the prescription.

[0027] In a preferred embodiment, the above polyether / polyester block copolymer can be prepared by the following method:

[0028] Under nitrogen protection, add polyether to a glass polymerization bottle, keep warm at 125-130℃, stir, and vacuum to remove water. Add metal catalyst / toluene solution, stir and disperse, keep warm at 125-130℃, stir, and vacuum to remove toluene. Add polyester, keep warm at 125-130℃, stir and react. After the reaction is completed, cool down, add dichloromethane, stir and dissolve, and add metal scavenger for treatment. Filter to remove the metal scavenger, add the filtrate to anhydrous ether, dissolve and crystallize. After the filter cake is dissolved in dichloromethane, filter through a PTFE membrane, add the filtrate to anhydrous ether for crystallization, filter, and dry the filter cake to obtain a polyether-polyester diblock copolymer.

[0029] Preferably, the catalyst is selected from one or two of stannous octoate, stannous chloride, diethyltin, zinc chloride or triethylaluminum; preferably, the amount of the catalyst is 0.05%-0.5% of the total weight of the reactants.

[0030] In one embodiment, the drying method of the filter cake obtained above is vacuum drying, and the detailed drying process can be: the filter cake is first vacuum dried at below 20°C and -0.08 to -0.1 MPa for 6 to 10 hours, turned over, and then vacuum dried at 20 to 30°C and -0.08 to -0.1 MPa for 10 to 24 hours to obtain a polyether-polyester diblock copolymer.

[0031] Beneficial effects of the present invention:

[0032] The technical solution of adding povidone to micelle preparations of the present invention is generally applicable to taxane drugs and improves the stability of taxane drug micelles. After the prepared paclitaxel micelle preparation is reconstituted, it can remain stable for up to 8 days at room temperature; the stability of micelle preparations of other poorly soluble taxane drugs has been greatly improved compared with the prior art. DETAILED DESCRIPTION

[0033] The present invention is further illustrated by examples. It should be correctly understood that the examples of the present invention are only provided for illustrating the present invention, rather than limiting the present invention, so simple improvements to the present invention under the premise of the method of the present invention are within the scope of protection claimed in the present invention. All products and reagents in the examples of the present invention can be prepared with reference to the prior art, or can be purchased.

[0034] Example 1 Preparation of polyethylene glycol-polyorthoester block copolymer

[0035] Under nitrogen protection, add polyethylene glycol to the glass polymerization bottle. 2000 70g, 125-130℃, keep warm, stir, vacuum and remove water for 4h; add stannous isooctanoate (0.5g) / toluene solution, stir and disperse for 30min, keep warm, stir, vacuum and remove toluene for 1.5h at 125-130℃; add 30g polyorthoester, keep warm, stir and react for 3-4h at 125-130℃; cool down after the reaction, add dichloromethane, stir and dissolve, add metal scavenger for treatment three times. Filter and remove the metal scavenger, add the filtrate to anhydrous ether, dissolve and crystallize twice; after dissolving with dichloromethane, filter through a PTFE membrane (3μm), add the filtrate to anhydrous ether for crystallization; the obtained product is first dried at below 20℃, -0.08~-0.1MPa in vacuum for 6h, turn over, and then control the temperature at 20~30℃, -0.08~-0.1MPa in vacuum and dry for 24h to obtain polyethylene glycol. 2000 - Polyorthoester diblock copolymers.

[0036] Example 2 Preparation of polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer

[0037] Under nitrogen protection, add polyethylene glycol monomethyl ether into the glass polymerization bottle 200050g, 125-130℃, keep warm, stir, vacuum and remove water for 4h; add stannous isooctanoate (0.128g) / toluene solution, stir and disperse for 30min, keep warm, stir, vacuum and remove toluene for 1.5h at 125-130℃; add 50g DL-lactide, keep warm, stir and react for 3-4h at 125-130℃; cool down after the reaction, add dichloromethane, stir and dissolve, add metal scavenger for treatment three times. Filter and remove the metal scavenger, add the filtrate to anhydrous ether, dissolve and crystallize twice; after dissolving with dichloromethane, filter through PTFE membrane (3μm), add the filtrate to anhydrous ether for crystallization; the obtained product is first dried at below 20℃, -0.08--0.1MPa in vacuum for 6h, turn over, and then control the temperature at 20-30℃, -0.08--0.1MPa in vacuum for 24h to obtain methoxy polyethylene glycol. 2000 - Polylactide diblock copolymer.

[0038] Example 3 Preparation of polypropylene glycol-polyglycolide-lactide block copolymer

[0039] Under nitrogen protection, add polypropylene glycol to the glass polymerization bottle. 1000 30g, keep warm at 125-130℃, stir and vacuum to remove water for 4h; add stannous isooctanoate (0.05g) / toluene solution, stir and disperse for 30min, keep warm at 125-130℃, stir and vacuum to remove toluene for 1.5h; add 70g of poly(glycolide)-lactide, keep warm at 125-130℃, stir and react for 3-4h; after the reaction, cool down, add dichloromethane, stir and dissolve, and add metal scavenger for treatment three times. Filter by suction to remove the metal scavenger, add the filtrate into anhydrous ether, dissolve and crystallize twice; dissolve with dichloromethane, filter through a PTFE membrane (3μm), add the filtrate into anhydrous ether for crystallization; the obtained product is first dried under vacuum at below 20°C and -0.08 to -0.1MPa for 6h, turned over, and then dried under vacuum at 20 to 30°C and -0.08 to -0.1MPa for 24h to obtain a polypropylene glycol-polyglycolide lactide diblock copolymer.

[0040] Example 4 Preparation of Paclitaxel Polyethylene Glycol-Polyorthoester Block Copolymer Micelles

[0041] Weigh 0.6 g of paclitaxel and 2.4 g of polyethylene glycol-polyorthoester block copolymer (prepared in Example 1), add organic solvent acetonitrile (about 15 g), heat at 50° C. and ultrasonically dissolve; evaporate the organic solvent at 50° C. to dryness under reduced pressure to obtain a mixed film; add 6 mg / ml polyvidone K-25 aqueous solution (100 ml) to fully hydrate the film to obtain a transparent drug-loaded micelle solution; sterilize and filter the polymer micelle solution loaded with paclitaxel, and freeze-dry to obtain a paclitaxel polymer micelle freeze-dried preparation.

[0042] Example 5 Preparation of Paclitaxel Polyethylene Glycol Monomethyl Ether-Poly (D, L) Lactide Block Copolymer Micelle

[0043] Weigh 0.6 g of paclitaxel and 6 g of polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer (prepared in Example 2), add organic solvent ethanol (about 30 g), heat at 50° C. and ultrasonically dissolve; evaporate the above organic solvent to dryness under reduced pressure at 45° C. to obtain a mixed film; add 12 mg / ml polyvidone K-12 aqueous solution (100 ml) to fully hydrate the film to obtain a transparent drug-loaded micelle solution; add lyophilization protective agent lactose (1.5 g) to the above polymer micelle solution containing paclitaxel, sterilize and filter, and freeze-dry to obtain a paclitaxel polymer micelle freeze-dried preparation.

[0044] Example 6 Preparation of Paclitaxel Polypropylene Glycol-Poly(Lactide-Glycol) Block Copolymer Micelle

[0045] Weigh 0.6 g of paclitaxel and 3 g of polypropylene glycol-poly(glycolide-lactide) block copolymer (prepared in Example 3), add organic solvent methanol (about 35 ml), and dissolve them by ultrasonic heating at 50°C; evaporate the above organic solvent to dryness under reduced pressure at 40°C to obtain a mixed film; add 18 mg / ml polyvidone K-17 aqueous solution (100 ml) to fully hydrate the film to obtain a transparent drug-loaded micelle solution; add lyophilization protective agent mannitol (2 g) to the above polymer micelle solution containing paclitaxel drug, sterilize and filter, and freeze-dry to obtain a paclitaxel polymer micelle freeze-dried preparation.

[0046] Example 7 Preparation of docetaxel polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer micelles

[0047] Weigh 0.6 g of docetaxel and 12 g of polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer (prepared in Example 2), add an organic solvent acetonitrile (about 60 g), heat at 50° C. and ultrasonically dissolve; evaporate the above organic solvent at 50° C. under reduced pressure to dryness to obtain a mixed film; add 12 mg / ml polyvidone K-12 aqueous solution (100 ml) to fully hydrate the film to obtain a transparent drug-loaded micelle solution; add a lyophilization protective agent lactose (1.5 g) to the above polymer micelle solution loaded with docetaxel, sterilize and filter, and freeze-dry to obtain a docetaxel polymer micelle lyophilized preparation.

[0048] Example 8 Preparation of Cabazitaxel Polyethylene Glycol Monomethyl Ether-Poly (D, L) Lactide Block Copolymer Micelle

[0049] Weigh 0.6 g of cabazitaxel and 24 g of polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer (prepared in Example 2), add organic solvent ethanol (about 70 g), heat at 50° C. and ultrasonically dissolve; evaporate the above organic solvent to dryness under reduced pressure at 45° C. to obtain a mixed film; add 12 mg / ml povidone K-12 aqueous solution (100 ml) to fully hydrate the film to obtain a transparent drug-loaded micelle solution; add lyophilization protective agent lactose (1.5 g) to the above polymer micelle solution containing cabazitaxel, sterilize, filter, and freeze-dry to obtain a cabazitaxel polymer micelle lyophilized preparation.

[0050] Comparative Example 1

[0051] Weigh 0.6 g of paclitaxel and 6 g of polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer (prepared in Example 2), add organic solvent ethanol (about 30 g), heat at 50°C and ultrasonically dissolve; evaporate the above organic solvent to dryness under reduced pressure at 45°C to obtain a mixed film; add about 100 ml of water for injection to fully hydrate the film to obtain a transparent drug-loaded micelle solution; add lyophilization protective agent lactose (1.5 g) to the above polymer micelle solution containing paclitaxel, sterilize and filter, and freeze-dry to obtain a paclitaxel polymer micelle freeze-dried preparation.

[0052] Comparative Example 2

[0053] Take about 26.5g of polyethylene glycol monomethyl ether (molecular weight 2000) and 25.8g of D, L-lactide and add them to a fully dried polymerization bottle, add 1ml of stannous octoate / dichloromethane solution with a concentration of 0.1g / ml; heat to 80°C to dissolve the polyethylene glycol monomethyl ether, start stirring and vacuum to remove residual water and dichloromethane in the system; after vacuuming for 6 hours, seal the polymerization bottle under vacuum, and heat the polymerization reaction at 180°C for 1 hour; take the product and dissolve it in deionized water, stir at room temperature for 24 hours, then heat to 70°C to precipitate the polymer, vacuum dry the precipitate and dissolve it in dichloromethane, centrifuge at 10000 rpm for 10 minutes, precipitate the supernatant with a large amount of anhydrous ether, and vacuum dry to obtain the copolymer mPEG2000-PLA;

[0054] About 0.3 g of paclitaxel and 2.5 g of mPEG2000-PLA were placed in a 500 ml round-bottom flask, 100 ml of acetonitrile was added, and the mixture was stirred until dissolved. The mixture was heated to 50°C and the acetonitrile was removed by rotary evaporation to obtain a transparent gel-like drug film. The mixture was placed in a vacuum drying oven at room temperature and dried overnight. A 50°C phosphate buffer solution (20 mM, 50 ml) with a pH of 7.0 was added to dissolve and disperse the drug film to obtain a polymer micelle solution with a light blue opalescence. The mixture was sterilized by filtering with a 0.22 um sterile filter membrane, and then the mixture was packaged and freeze-dried to obtain a paclitaxel polymer freeze-dried micelle preparation.

[0055] Comparative Example 3

[0056] Weigh 16g of methyl polyethylene glycol and 24g of lactide, add them into a sealed reactor, add 50mg of stannous octoate, heat to 130°C under nitrogen flow to melt the solid, and then continue to raise the temperature to 160°C for 6 hours. Cool to obtain a white solid crude product. Dissolve the crude product in 1ml of dichloromethane, add 100ml of ether under stirring, filter, wash with ether three times, and vacuum dry the product for 24 hours to obtain a polymer;

[0057] Take 6 ml of 50 mg / ml polymer acetonitrile solution and 6 ml of 10 mg / ml paclitaxel acetonitrile solution, add into an eggplant-shaped bottle, place on a rotary evaporator, water bath temperature 50°C, reduced pressure (-0.1 MPa), rotary evaporation at 20 rpm for 30 minutes, add 25 ml of 0.2 mg / ml aspartic acid aqueous solution, rotate and hydrate for 1 minute, remove the eggplant-shaped bottle, vortex on a vortexer for 1 minute, filter the resulting solution through a 0.22 μm filter membrane, and lyophilize to obtain a white solid.

[0058] Comparative Example 4

[0059] Weigh 16g of methyl polyethylene glycol and 24g of lactide, add them into a sealed reactor, add 50mg of stannous octoate, heat to 130°C under nitrogen flow to melt the solid, and then continue to raise the temperature to 160°C for 6 hours. Cool to obtain a white solid crude product. Dissolve the crude product in 1ml of dichloromethane, add 100ml of ether under stirring, filter, wash with ether three times, and vacuum dry the product for 24 hours to obtain a polymer;

[0060] Take 10 ml of 50 mg / ml polymer acetonitrile solution and 10 ml of 5 mg / ml docetaxel acetonitrile solution, add into an eggplant-shaped bottle, place on a rotary evaporator, water bath temperature 50°C, reduced pressure (-0.1 MPa), rotary evaporate at 20 rpm for 30 minutes, add 50 ml of 0.2 mg / ml arginine aqueous solution, rotate and hydrate for 1 minute, remove the eggplant-shaped bottle, vortex on a vortexer for 1 minute, filter the resulting solution through a 0.22 μm filter membrane, and lyophilize to obtain a white solid.

[0061] Comparative Example 5

[0062] Weigh 16g of methyl polyethylene glycol and 24g of lactide, add them into a sealed reactor, add 50mg of stannous octoate, and 2ml of toluene solution, heat to 130°C under nitrogen flow to melt the solid and evaporate the toluene; continue to raise the temperature to 160°C to react for 6 hours. Cool to obtain a white solid crude product. After the crude product is dissolved in 1ml of dichloromethane, add 100ml of ether under stirring, filter, wash with ether three times, and vacuum dry the product for 24 hours to obtain PEG-PDLLA polymer;

[0063] Take 300 mg of paclitaxel, 1 mg of PEG-PDLLA polymer, and 100 mg of lecithin and put them in a flask, add 150 ml of acetonitrile, and stir to dissolve; heat to 60°C and evaporate the acetonitrile under reduced pressure; add 150 ml of 60°C water for injection, hydrate to obtain a light blue opalescent mixture, homogenize with a high-speed homogenizer for 30 seconds, filter through a 0.22 μm filter membrane for sterilization, and then freeze-dry to obtain paclitaxel polymer micelles.

[0064] Comparative Example 6

[0065] 0.6 g of docetaxel, 12 g of polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer (prepared in Example 2), and 0.2 g of lecithin were weighed, added into an organic solvent acetonitrile (about 60 g), and heated at 50° C. for ultrasonic dissolution; the organic solvent was evaporated at 50° C. under reduced pressure to dryness to obtain a mixed film; about 100 ml of water for injection was added to fully hydrate the film to obtain a transparent drug-loaded micelle solution; a freeze-drying protective agent lactose (1.5 g) was added into the above polymer micelle solution loaded with docetaxel, sterilized and filtered, and freeze-dried to obtain a docetaxel polymer micelle freeze-dried preparation.

[0066] Comparative Example 7

[0067] Weigh 0.6 g of cabazitaxel, 24 g of polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer (prepared in Example 2), and 0.2 g of lecithin, add an organic solvent acetonitrile (about 70 g), and heat at 50° C. and ultrasonically dissolve; evaporate the above organic solvent to dryness under reduced pressure at 50° C. to obtain a mixed film; add about 100 ml of water for injection to fully hydrate the film to obtain a transparent drug-loaded micelle solution; add a freeze-drying protective agent lactose (1.5 g) to the above polymer micelle solution containing cabazitaxel, sterilize and filter, and freeze-dry to obtain a cabazitaxel polymer micelle freeze-dried preparation.

[0068] Comparative Example 8

[0069] Weigh 0.6 g of cabazitaxel and 24 g of polyethylene glycol monomethyl ether-poly (D, L) lactide block copolymer (prepared in Example 2), add organic solvent ethanol (about 70 g), heat at 50° C. and ultrasonically dissolve; evaporate the above organic solvent to dryness under reduced pressure at 45° C. to obtain a mixed film; add 6 mg / ml arginine aqueous solution (100 ml) to fully hydrate the film to obtain a transparent drug-loaded micelle solution; add lyophilization protective agent lactose (1.5 g) to the above polymer micelle solution loaded with cabazitaxel, sterilize and filter, and freeze-dry to obtain a cabazitaxel polymer micelle freeze-dried preparation.

[0070] Comparative Example 9

[0071] Under the protection of dry high-purity nitrogen, 20 g of povidone and 20 g of polylactic acid were weighed into a fully dried polymerization reactor, 0.08 g of stannous octoate was added, the povidone was heated to dissolve, and the polymerization reaction was carried out in a 150°C oil bath under vacuum conditions for about 10 hours; after the polymerization reaction, 18 g of dichloromethane was added to the solid obtained in the reactor to dissolve it; the above solution was added into a container containing 180 g of isopropyl ether (pre-cooled at -20°C) to precipitate the target product, and the precipitate was collected by filtration; the above operation was repeated once for the collected precipitate to obtain a white solid, which was vacuum dried at room temperature for 48 hours to obtain a povidone-polylactic acid block copolymer.

[0072] Weigh 0.3 g of paclitaxel and 1.5 g of polyvidone-polylactic acid block copolymer and add them to a liquid preparation tank, add 15 g of ethanol, control the temperature at 70°C and stir to dissolve, obtain a clear liquid, heat and evaporate the ethanol to obtain a mixed drug film; add 30 L of 5 mM phosphate buffer prepared with water for injection to the liquid preparation tank, fully dissolve the gel-like drug film, and obtain a paclitaxel micelle solution; adsorb on activated carbon, filter out the activated carbon with a carbon rod filter, sterilize by filtration at 0.22 μm, and freeze-dry to obtain a paclitaxel micelle freeze-dried preparation.

[0073] Stability test

[0074] The freeze-dried powders prepared in Examples 4 to 8 and Comparative Examples 1 to 9 were respectively reconstituted with 0.9% sodium chloride injection, and the solutions were observed with naked eyes under a clarity detector at 4°C and 25°C under normal indoor lighting conditions every 2 hours to see if precipitation or turbidity was produced. If precipitation or turbidity was produced, it means that the micelle solution has ended the stable state. The test results are shown in Table 1.

[0075] Table 1 Comparison of stability of drug-loaded micelles in different embodiments

[0076]

Claims

1. A polymer micelle freeze-dried preparation of a taxane anti-tumor drug, It is characterized in that The preparation contains taxane drugs, polyvidone, and polyether / polyester block copolymer; the weight ratio of the taxane drugs to the polyvidone is 1:1-3; the weight ratio of the taxane drugs to the polyether / polyester block copolymer is 1:4-50; wherein the taxane drugs are paclitaxel.

2. The polymer micelle freeze-dried preparation according to claim 1, It is characterized in that The povidone is one of povidone K-12, K-17, K-25, K-30, K-90 or a combination thereof.

3. The polymer micelle freeze-dried preparation according to claim 1, It is characterized in that The povidone is one of povidone K-12, K-17, K-25 or a combination thereof.

4. The polymer micelle freeze-dried preparation according to claim 1, It is characterized in that The polyether block is one of polyethylene glycol, polyethylene glycol monomethyl ether, polypropylene glycol or polybutylene glycol, or a combination thereof.

5. The polymer micelle freeze-dried preparation according to claim 1, It is characterized in that The polyester block is one of polylactide, polyglycolide lactide, polycaprolactone, polyorthoester or a combination thereof.

6. The polymer micelle freeze-dried preparation according to claim 1, It is characterized in that The polyether / polyester block copolymer is polyethylene glycol monomethyl ether 2000-polylactide.

7. A method for preparing the polymer micelle freeze-dried preparation according to any one of claims 1 to 6, It is characterized in that The preparation method comprises the following steps: a) weighing the prescribed amount of taxanes and polyether / polyester block copolymer, adding an organic solvent and ultrasonically heating to dissolve them; b) concentrating the organic solvent to dryness at room temperature to the boiling point of the organic solvent under normal pressure or reduced pressure to obtain a mixed film; c) adding an aqueous solution containing povidone to fully hydrate the film to obtain a transparent drug-loaded micelle solution; d) The drug-loaded micelle solution is sterilized, filtered, and freeze-dried to obtain a polymer micelle freeze-dried powder injection loaded with taxane drugs.

8. The preparation method according to claim 7, It is characterized in that The organic solvent is selected from one or two of ethanol, methanol, acetonitrile, acetone, chloroform and ethyl acetate.

9. The preparation method according to claim 7, It is characterized in that The organic solvent is selected from one or two of ethanol, methanol and acetonitrile.