A method and device for controlling verticality between micro-spring plates
By using a fixture composed of a support plate, a positioning plate and a guide column to slightly compress and position the micro spring, the problem of micro spring offset and deformation in CCGA packaged devices is solved, and the feasibility and reliability of micro spring welding are improved. Efficient welding of vertical interconnections between boards is ensured.
Patent Information
- Application Number
- CN202210319645.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-29
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2042-03-29
AI Technical Summary
When CCGA packaged devices use micro spring pins, there are problems with micro spring deflection, deformation and poor temperature uniformity, resulting in poor controllability of the welding process and low reliability of solder joints, affecting the achievability and reliability of vertical interconnections between boards. .
By designing a method and device to control the verticality between micro-spring plates, a clamp composed of a support plate, a positioning plate and a guide column is used to slightly compress and position the micro-spring to avoid deviation, and the support plate and the support plate are fixed through positioning pins. Positioning plate ensures the verticality and flatness of the micro spring, thereby achieving precise positioning and reliable welding.
It improves the feasibility and reliability of micro spring welding, solves the problems of micro spring offset and deformation, improves welding quality and efficiency, and ensures the accurate alignment and welding quality of micro spring and PCB board.
Smart Images

Figure CN114698265B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of electronic packaging, and in particular relates to a method and a device for controlling the verticality between micro-spring plates. Background Art
[0002] Usually CCGA (ceramic column grid array) packaged devices have three forms of interconnect pins, namely cast solder columns, copper tape wrapped solder columns and micro spring solder columns. CCGA packaged devices with cast solder columns or copper tape wrapped solder columns as interconnect pins have good vibration and impact resistance in the horizontal direction, but poor mechanical vibration resistance in the Z direction and low mechanical strength. The spring contacts of micro spring solder columns have better impact resistance, vibration resistance, flexibility and other characteristics, especially the ability to resist large deformation in the Z direction. While ensuring the electrical performance of the contact interconnection, it provides better flexibility for the interconnection of interlayer spring contact arrays in high temperature and harsh environments.
[0003] However, the micro-spring itself has a small mass and poor stability. It is easily offset by external forces, and vertical interconnection of micro-springs is more difficult to achieve than solder columns. When CCGA uses micro-spring pins for interconnection, the number of micro-spring arrays is large, and the micro-spring pin material has strong heat transfer capacity, and the thermal matching with substrates, pads and other materials is not high. In particular, the clamping of the micro-spring conversion tooling will lead to poor temperature uniformity, large temperature gradients, and prominent thermal stress problems at the micro-spring solder joints during the welding process. The controllability of the welding process is poor, and problems such as coplanarity and inclination caused by micro-spring offset will occur. In addition, during the micro-spring pin implantation process of the CCGA device, whether the micro-spring pin is coaxial with the device substrate pad will directly affect the alignment and matching of the pin and PCB pad during the CCGA device assembly process, thereby affecting the device pin welding quality and reliability. The micro-spring pin conversion assembly process is prone to defects such as pin misalignment, pin deformation and non-coplanarity, which in turn causes the micro-spring pins of the CCGA device to deviate from the pads when assembled with the PCB board, incomplete solder wrapping of the micro-spring pins, or some micro-spring pins being desoldered or partially soldered from the solder paste, resulting in poor solder joint reliability. Therefore, micro-spring assembly precision control technology is extremely important. Summary of the invention
[0004] Based on the above problems, the present invention proposes a method and device for controlling the verticality between micro-spring plates, which positions and clamps the welding by a fixed fixture, controls the deviation of the micro-spring during the welding process, realizes precise positioning and reliable welding of the micro-spring based on vertical interconnection between plates, and solves the problems of micro-spring deviation, deformation, low flatness, etc. in CCGA welding, thereby improving the feasibility and reliability of vertical interconnection between plates.
[0005] The technical solution adopted by the present invention is a method for controlling the verticality between micro-spring plates, comprising the following steps:
[0006] Step 1: Place the PCB with solder applied and micro springs placed facing up;
[0007] Step 2: compress all micro springs to a predetermined length at the same time, keep all micro springs in the same horizontal plane and keep them stable;
[0008] Step 3: Re-solder the bottom end of the micro spring and the PCB, and check whether the welding result meets the standard;
[0009] Step 4. Place another PCB coated with solder with its front side facing up. Flip the PCB with the micro spring soldered on it and align the micro spring with the soldering point of the other PCB and move it downward so that the micro spring is compressed to a predetermined length and remains stable. Re-solder the bottom end of the micro spring to the PCB and check whether the welding result is up to standard.
[0010] A device for controlling the verticality between micro-spring plates, the device for controlling the verticality between micro-spring plates is used in the method for controlling the verticality between micro-spring plates, the device for controlling the verticality between micro-spring plates comprises: a first support plate, a second support plate and a positioning plate;
[0011] A PCB slot is provided in the center of the support plate 1 and the support plate 2, positioning slots are symmetrically provided on the opposite sides of the support plate 1, and positioning blocks 1 are provided on both sides of the support plate 2 to match the positioning slots; a plurality of guide columns are vertically provided at a predetermined distance in the center of the bottom surface of the positioning plate, and the plurality of guide columns correspond to the micro springs one by one, and positioning blocks 2 are provided on both sides of the positioning plate corresponding to the positioning slots; the support plate 2 and the positioning plate are connected to the support plate 1 by respectively embedding the positioning slots at the bottom of the positioning block 1 and the positioning block 2.
[0012] Preferably, when the positioning plate and the support plate 1 or the support plate 1 and the support plate 2 are connected and fixed, the micro spring is compressed by 0.1-0.2 mm.
[0013] Preferably, the guide column is cylindrical, the outer diameter of which matches the inner diameter of the micro-spring, and the length of the guide column is 0.4-0.6 mm.
[0014] Preferably, the PCB slot is in a rectangular shape matching the PCB, and positioning columns are vertically provided near the four corners of the PCB slot.
[0015] Preferably, through holes are respectively formed on the outer side of the positioning groove and through the support plate 1, and a connecting hole 1 is formed at a lower end of the positioning block corresponding to the through hole, and a positioning pin is used to pass through the through hole and the connecting hole 1 to fix the positioning block 1 and the support plate 1.
[0016] Preferably, a second connecting hole is formed at the lower end of the second positioning block corresponding to the through hole, and a positioning pin is used to pass through the through hole and the second connecting hole to fix the second positioning block and the first supporting plate.
[0017] The guide column is prepared by the following process:
[0018] S1 pretreatment: the substrate is cleaned with acetone, alcohol and deionized water respectively, and then dried with a spin dryer; finally, the surface is activated by ion beam bombardment;
[0019] S2 coating: drop AZ5214 photoresist onto the substrate surface, then vacuum absorb the substrate and rotate at high speed to make the photoresist thin and evenly cover the substrate surface;
[0020] S3 pre-baking: pre-baking the substrate at a predetermined temperature;
[0021] S4 exposure and development: Expose the pre-baked substrate, develop it with AZ300MIF developer, and blow dry it with nitrogen;
[0022] S5 cleaning: using AZ5214 developer to clean and remove the unexposed part of AZ5214 positive photoresist to obtain a hole groove;
[0023] S6 casting: SU-8 and pyrolytic graphite are mixed in a mass ratio of 2:8 and then cast into the empty slot to obtain a guide column;
[0024] S7 cleaning: Use acetone solution to remove the AZ5214 positive photoresist.
[0025] Preferably, the pre-baking temperature of the substrate is 100° C. and the time is 1 minute.
[0026] Preferably, the exposure dose is 40 mJ / cm2, the exposure time is 40S, and the development time is 60S.
[0027] Compared with the prior art, the present invention has the following beneficial effects:
[0028] 1) The present invention uses a plane to slightly compress the micro-spring to position and clamp the micro-spring, avoid the micro-spring offset during welding, achieve precise positioning and reliable welding of the micro-spring based on vertical interconnection between boards, solve the problems of micro-spring offset and deformation in CCGA welding, and at the same time, maintain the flatness of the micro-spring, thereby improving the feasibility and reliability of vertical interconnection between boards; the operation method is simple, and the welding quality and efficiency are improved;
[0029] 2) The present invention uses a support plate 1, a support plate 2 and a positioning plate to form a fixture for welding micro springs, wherein a guide column is arranged on the positioning plate to insert the micro springs for guiding and positioning, thereby avoiding the micro springs from deflecting during compression and maintaining the verticality of the micro springs, and the connection between the positioning plate and the support plate 1 can effectively stabilize the compression state of the micro springs, thereby achieving a balanced clamping and positioning effect on the micro springs;
[0030] 3) The outer diameter of the guide column of the present invention is adapted to the inner diameter of the micro spring, ensuring that the guide column is smoothly inserted into the micro spring and has a limiting effect on the micro spring, ensuring that the micro spring is vertically compressed to avoid deformation. In normal conditions, the length of the micro spring is 1 mm, and the length of the guide column is 0.4-0.6 mm, which effectively guides and positions the micro spring;
[0031] 4) The PCB slot and positioning column make the PCB more stable and facilitate the alignment of the micro spring and the solder joint to avoid deviation during the welding process;
[0032] 5) This design uses the method of inserting the locating pin to fix the locating block one or the locating block two and the support plate one, which effectively fixes the support plate one and the support plate two to avoid the deformation of the micro spring caused by the offset during welding. In addition, during the micro spring pin conversion assembly process, the problems of pin misalignment, pin deformation and non-coplanarity are solved. The connection is quick and reliable, the device structure is simple and compact, and it is practical. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 Assembling the present invention Figure 1 ;
[0034] Figure 2 Assembling the present invention Figure 2 ;
[0035] Figure 3 This is a schematic diagram of the assembly of the present invention;
[0036] Figure 4 This is a structural schematic diagram of a support plate of the present invention;
[0037] Figure 5 This is a structural schematic diagram of the second support plate of the present invention;
[0038] Figure 6 This is a schematic diagram of the positioning plate structure of the present invention;
[0039] Markings in the figure: 1. Support plate 1, 2. Support plate 2, 3. Positioning plate, 4. PCB slot, 5. Positioning slot, 6. Positioning block 1, 7. Guide column, 8. Positioning block 2, 9. PCB, 10. Positioning column, 11. Through hole, 12. Connecting hole 1, 13. Positioning pin, 14. Connecting hole 2. DETAILED DESCRIPTION
[0040] The present invention will be further explained below in conjunction with the accompanying drawings to facilitate better understanding by professionals skilled in the art.
[0041] Example 1
[0042] When CCGA uses micro-spring pins for interconnection, the number of micro-spring arrays is large, the micro-spring itself has a small mass, poor stability, and is easily offset by external forces. The controllability is poor during the welding process, and defects such as pin misalignment and pin deformation and non-coplanarity are prone to occur, which in turn causes the micro-spring pins of the CCGA device to deviate from the pads when assembled with the PCB board, the solder does not completely wrap the micro-spring pins, or some micro-spring pins are desoldered or partially welded from the solder paste, resulting in poor solder joint reliability and other problems. The present invention provides a method for controlling the verticality between micro-spring plates, comprising the following steps:
[0043] Step 1: Place the PCB with solder applied and micro springs placed facing up;
[0044] Step 2: compress all micro springs to a predetermined length at the same time, keep all micro springs in the same horizontal plane and keep them stable;
[0045] Step 3: Re-solder the bottom end of the micro spring and the PCB, and check whether the welding result meets the standard;
[0046] Step 4. Place another PCB coated with solder with its front side facing up. Flip the PCB with the micro spring soldered on it and align the micro spring with the soldering point of the other PCB and move it downward so that the micro spring is compressed to a predetermined length and remains stable. Re-solder the bottom end of the micro spring to the PCB and check whether the welding result is up to standard.
[0047] The method for controlling the verticality between micro-spring plates provided by the present invention utilizes a plane to slightly compress the micro-spring to position and clamp the micro-spring, thereby avoiding the micro-spring offset during welding, achieving precise positioning and reliable welding of the micro-spring based on vertical interconnection between plates, and solving the problems of micro-spring offset and deformation in CCGA welding. At the same time, the flatness of the micro-spring is maintained, thereby improving the feasibility and reliability of vertical interconnection between plates; the operation method is simple, and the welding quality and efficiency are improved.
[0048] Example 2
[0049] A device for controlling the verticality between micro-spring plates, such as Figure 1-6 As shown, the device for controlling the verticality between micro-spring plates is used in the method for controlling the verticality between micro-spring plates, and the device for controlling the verticality between micro-spring plates includes: a support plate 1, a support plate 2 and a positioning plate 3.
[0050] The support plate 1 and the support plate 2 are rectangular plates with a predetermined thickness. A PCB groove 4 is provided in the center of the support plate 1 and the support plate 2 for placing the PCB 9 to prevent the PCB 9 from shifting. Positioning grooves 5 are symmetrically provided on the opposite sides of the support plate 1, and positioning blocks 6 are provided on both sides of the support plate 2 to match the positioning grooves 5. A plurality of guide columns 7 are vertically provided at a predetermined distance in the center of the bottom surface of the positioning plate 3, and the plurality of guide columns 7 correspond to the micro springs one by one. Positioning blocks 2 8 are provided on both sides of the positioning plate 3 corresponding to the positioning grooves 5. The support plate 2 2 and the positioning plate 3 are connected to the support plate 1 by respectively embedding the positioning grooves 5 at the lower parts of the positioning blocks 1 6 and the positioning blocks 2 8.
[0051] The present invention uses support plate 1, support plate 2 and positioning plate 3 to form a fixture for welding micro springs. When in use, the guide pillars 7 are inserted into the micro springs one by one to guide and position them, and the positioning block 2 8 is inserted into the positioning groove 5. At this time, the micro springs are slightly compressed. The guide pillars 7 can prevent the micro springs from deviating during the compression process and maintain the verticality of the micro springs; and the connection between the positioning plate 3 and the support plate 1 can effectively stabilize the compression state of the micro springs, thereby playing a balanced clamping and positioning role for the micro springs.
[0052] When the positioning plate 3 and the support plate 1 or the support plate 1 and the support plate 2 2 are connected and fixed, the micro spring is compressed by 0.1-0.2 mm, which will not over-compress the micro spring to make it invalid, while ensuring the clamping effect of the device on the micro spring.
[0053] The guide column 7 is cylindrical, and its outer diameter is adapted to the inner diameter of the micro-spring, ensuring that the guide column 7 is smoothly inserted into the micro-spring and has a limiting effect on the micro-spring, ensuring vertical compression of the micro-spring to avoid deformation; and the length of the guide column 7 is 0.4-0.6mm. Since the length of the micro-spring is 1mm under normal conditions, the length of the guide column 7 is 0.4-0.6mm, which effectively guides and positions the micro-spring.
[0054] The PCB slot 4 is a rectangle that matches the PCB9. Positioning columns 10 are vertically upwardly arranged near the four corners of the PCB slot 4. Corresponding positioning columns are punched on the PCB9. The positioning columns 10 can temporarily fix the PCB9 in the PCB slot 4 of the support plate 1 and the support plate 2, which is beneficial to the precise positioning of the support plate 1 and the support plate 2, and convenient for the conversion and assembly of the micro-spring pins.
[0055] The outer side of the positioning groove 5 penetrates the support plate 1 to respectively form a through hole 11, and the lower end of the positioning block 6 forms a connecting hole 12 corresponding to the through hole 11, and a positioning pin 13 is used to pass through the through hole 11 and the connecting hole 12 to fix the positioning block 6 and the support plate 1; the structure is simple, the installation and disassembly operations are convenient, and the connection stability between the support plate 1 and the support plate 2 is enhanced.
[0056] A second connecting hole 14 is formed at the lower end of the positioning block 8 corresponding to the through hole 11, and a positioning pin 13 is used to pass through the through hole 11 and the second connecting hole 14 to fix the positioning block 8 and the support plate 1; the positioning plate 3 and the support plate 1 are effectively fixed to avoid deformation of the micro spring caused by offset during welding. In addition, during the micro spring pin conversion and assembly process, the problems of pin non-coaxiality and pin deformation and non-coplanarity are solved, and the practicability is strong.
[0057] In this embodiment, the method for preparing the guide column 7 comprises the following steps:
[0058] S1 pretreatment: the substrate is cleaned with acetone, alcohol and deionized water respectively, and then dried with a spin dryer; finally, the surface is activated by ion beam bombardment;
[0059] S2 coating: drop AZ5214 photoresist onto the substrate surface, then vacuum absorb the substrate and rotate at high speed to make the photoresist thin and evenly cover the substrate surface;
[0060] S3 pre-baking: pre-baking the substrate at a predetermined temperature; specifically, the temperature is 100° C. and the time is 1 minute;
[0061] S4 exposure and development: Expose the substrate with an exposure dose of 40mJ / cm 2 , exposure time 40S, developed with AZ300MIF developer for 60S, and dried with nitrogen;
[0062] S5 cleaning: using AZ5214 developer to clean and remove the unexposed part of AZ5214 positive photoresist to obtain a hole groove;
[0063] S6 casting: SU-8 and pyrolytic graphite are mixed in a mass ratio of 2:8 and then cast into the empty slot to obtain a guide column;
[0064] S7 cleaning: Use acetone solution to remove the AZ5214 positive photoresist.
[0065] Specific usage:
[0066] Place the PCB9 coated with solder and with the micro spring in the PCB slot 4 of the support plate 1, insert the guide column 7 one by one into the micro spring downward, insert the positioning block 28 into the positioning slot 5, and use the positioning pin 13 to insert the through hole 11 from the outside of the support plate 1 to fix the positioning block 28 and the support plate 1. At this time, the micro spring is slightly compressed, and the support plate 1, the positioning plate 3 and the guide column 7 have the function of clamping and positioning the micro spring, and the first part of the welding is completed by reflow soldering. Remove the positioning plate 3 and check whether the welding result is up to standard. Place another PCB9 in the PCB slot 4 of the support plate 2, flip the support plate 1 and slowly move downward corresponding to the support plate 2, so that the positioning block 28 is inserted into the positioning slot 5, and fixed with the positioning pin 13. At this time, the unwelded end of the micro spring is accurately connected with the PCB4 solder joint on the support plate 2, and the second part of the welding is completed by reflow soldering. Separate the support plate 1, the support plate 2 and the PCB9.
[0067] The above description is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed by the present invention, which should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. A method for controlling the verticality between micro-spring plates, characterized in that: The following steps are involved: Step 1: Place the PCB with solder applied and micro springs placed facing up; Step 2: compress all micro springs to a predetermined length at the same time, keep all micro springs in the same horizontal plane and keep them stable; Step 3: Re-solder the bottom end of the micro spring and the PCB, and check whether the welding result meets the standard; Step 4: Place another PCB coated with solder with its front side facing up, flip the PCB with the micro spring soldered on it, align the micro spring with the soldering point of the other PCB and move it downward, so that the micro spring is compressed to a predetermined length and remains stable, re-solder the bottom end of the micro spring to the PCB, and check whether the welding result is up to standard; The device for controlling the verticality between micro-spring plates comprises: a support plate 1 (1), a support plate 2 (2) and a positioning plate (3); a PCB slot (4) is provided in the center of the support plate 1 (1) and the support plate 2 (2); positioning slots (5) are symmetrically provided on opposite sides of the support plate 1 (1); positioning blocks 1 (6) are provided on both sides of the support plate 2 (2) to match the positioning slots (5); a plurality of guide posts (7) are vertically provided at a predetermined interval in the center of the bottom surface of the positioning plate (3); the plurality of guide posts (7) correspond to the micro-springs one by one; positioning blocks 2 (8) are provided on both sides of the positioning plate (3) to correspond to the positioning slots (5); the support plate 2 (2) and the positioning plate (3) are connected to the support plate 1 (1) by respectively embedding the lower parts of the positioning blocks 1 (6) and the positioning blocks 2 (8) into the positioning slots (5); The PCB coated with solder and with the micro springs placed thereon is placed in the PCB slot (4) of the first support plate (1), the guide posts (7) are inserted downwardly corresponding to the micro springs one by one, the second positioning block (8) is inserted into the positioning slot (5) correspondingly, and the positioning pin (13) is inserted into the through hole (11) from the outside of the first support plate (1) to fix the second positioning block (8) and the first support plate (1). At this time, the micro springs are slightly compressed, and the first support plate (1), the positioning plate (3) and the guide posts (7) have a clamping and positioning effect on the micro springs, and the welding of the first part is completed by reflow soldering.
2. A method for controlling the verticality between micro-spring plates according to claim 1, characterized in that: When the positioning plate (3) and the first support plate (1) or the first support plate (1) and the second support plate (2) are connected and fixed, the micro spring is compressed by 0.1-0.2 mm.
3. A method for controlling the verticality between micro-spring plates according to claim 1, characterized in that: The guide column (7) is cylindrical, with an outer diameter matching the inner diameter of the micro spring, and a length of the guide column (7) of 0.4-0.6 mm.
4. A method for controlling the verticality between micro-spring plates according to claim 1, characterized in that: The PCB slot (4) is in a rectangular shape matching the PCB (9), and positioning posts (10) are respectively provided vertically upward near the four corners of the PCB slot (4).
5. The method for controlling the verticality between micro-spring plates according to claim 1, characterized in that: The outer side of the positioning groove (5) penetrates through the support plate (1) to respectively form a through hole (11), and the lower end of the positioning block (6) is provided with a connecting hole (12) corresponding to the through hole (11), and a positioning pin (13) is used to pass through the through hole (11) and the connecting hole (12) to fix the positioning block (6) and the support plate (1).
6. A method for controlling the verticality between micro-spring plates according to claim 1, characterized in that: A second connecting hole (14) is formed at the lower end of the second positioning block (8) corresponding to the through hole (11), and a positioning pin (13) is passed through the through hole (11) and the second connecting hole (14) to fix the second positioning block (8) and the first supporting plate (1).
7. A method for controlling the verticality between micro-spring plates according to claim 1, characterized in that: The guide column is prepared by the following process: S1 pretreatment: the substrate is cleaned with acetone, alcohol and deionized water respectively, and then dried with a spin dryer; finally, the surface is activated by ion beam bombardment; S2 coating: drop AZ5214 photoresist onto the substrate surface, then vacuum absorb the substrate and rotate at high speed to make the photoresist thin and evenly cover the substrate surface; S3 pre-baking: pre-baking the substrate at a predetermined temperature; S4 exposure and development: Expose the pre-baked substrate, develop it with AZ300MIF developer, and blow dry it with nitrogen; S5 cleaning: using AZ5214 developer to clean and remove the unexposed part of AZ5214 positive photoresist to obtain a hole groove; S6 casting: SU-8 and pyrolytic graphite are mixed in a mass ratio of 2:8 and then cast into the empty slot to obtain a guide column; S7 cleaning: Use acetone solution to remove the AZ5214 positive photoresist.
8. A method for controlling the verticality between micro-spring plates according to claim 7, characterized in that: The pre-baking temperature of the substrate is 100° C. and the time is 1 minute.
9. A method for controlling the verticality between micro-spring plates according to claim 7, characterized in that: The exposure dose is 40 mJ / cm 2 , exposure time 40S, development time 60S.
Citation Information
Cited By
High-frequency integrated device board-level elastic interconnection structure and processing method
CN119943795A
A high-frequency integrated device board-level flexible interconnection structure and a processing method thereof