Forging process for light and thin forgings

By combining the cold trimming process and magnetic equipment in the production of light and thin forgings, the operational difficulties and safety hazards in the hot trimming process are solved, a more uniform and safer trimming process is achieved, and product quality and safety are improved. Production safety.

CN118720640APending Publication Date: 2024-10-01CHANGZHOU LEAP FORGING CO LTD

Patent Information

Application Number
CN202410672243.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-28
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the production process of light and thin forgings, the hot-cut edge process leads to operational difficulties, safety hazards and uneven trimming problems. In particular, due to the high temperature of the forgings, it is difficult to clamp and the positioning space is limited, which can easily cause safety accidents and product appearance problems.

Method used

The cold trimming process is used to grab and trim the forgings through the cold trimming die and magnetic equipment to ensure the uniformity and safety of the trimming. The positioning cavity and return spring of the cold trimming die are used to correct and trim the forgings. Trimming, combined with magnetic equipment to assist the operation.

Benefits of technology

It achieves a faster and safer trimming process, avoids forgings being skewed and trimming residues, improves product appearance quality and production safety, reduces operational risks, and is suitable for a wide range of light and thin forgings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118720640A_ABST
    Figure CN118720640A_ABST
Patent Text Reader

Abstract

The invention discloses a forging process of a light and thin forge piece, which specifically comprises the following steps: blanking, heating, upsetting, finish forging, trimming, heat treatment, shot blasting, inspection and warehousing, and is characterized in that a cold trimming process is adopted in the trimming process, a cold trimming die is adopted to correct the forge piece when cold trimming is carried out, and a cold trimming die is adopted to correct the forge piece when cold trimming is carried out; a positioning cavity is formed in the center of the cold trimming die, a die core is arranged in the middle of the positioning cavity, a reset spring is arranged at the bottom of the die core, a forge piece is grabbed through magnetic attraction equipment in the transferring process, the cold trimming process is adopted, the trimming residue problem of a product is thoroughly solved, and residues are completely cut off. Hot trimming is changed into cold trimming, so that the risk of being scalded can be effectively avoided; and meanwhile, magnetic attraction equipment is used for assisting in production to grab and place the forgings, the problem of difficult operation of staff is solved, the accident risk caused by misoperation is reduced, the production efficiency is improved, and meanwhile the production safety is further enhanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of precision forging, and in particular relates to a forging process for light and thin forgings. Background Art

[0002] At present, such thin and light forgings are used in many industries. Similar products are used in automobile manufacturing, machinery manufacturing and other industries, and have broad prospects.

[0003] For this type of light and thin forgings, the current process route is: cutting - heating - upsetting - final forging - trimming - heat treatment - shot peening - inspection - storage, among which the trimming process basically adopts the hot trimming process; the hot trimming process can be completed at the production site without going to other places, saving time and cost; at the same time, due to the hot trimming, the trimming resistance is small, which can effectively extend the service life of the trimming die; so in most cases, the hot trimming process is the first choice for the trimming process, such as the high-precision steel forging production and processing process provided by the publication number CN115401142A, but for Figure 1 , Figure 2 When the product shown in the figure is used, there is a big problem in choosing the hot trimming process, that is, it is not easy for operators to operate; during forging itself, the temperature of the forging is extremely high, reaching about 1150℃, and when it flows to the trimming process, it is also at least 850℃ high. The forging can only be clamped and placed by pliers, which is very inconvenient; when faced with such thin forgings, clamping becomes more difficult, and there are safety hazards while being difficult to operate. It is easy to cause safety accidents if you are careless, which is very dangerous; and because the forging is too thin, the positioning space is limited when placed on the trimming die, and it is very easy to put it crooked, resulting in uneven trimming and residue, which seriously affects the appearance of the product.

[0004] Therefore, the above problems are issues that should be considered and solved in the production process of the above-mentioned thin and light forgings. Summary of the invention

[0005] In view of the above problems, the purpose of the present invention is to provide a new trimming process, so that when facing such thin and light forgings, the trimming process can be completed faster, better and safer; and the problems of difficult operation for employees and substandard product appearance can be solved.

[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is a forging process for light and thin forgings, which specifically includes the following steps: blanking → heating → upsetting → final forging → trimming → heat treatment → shot peening → inspection → storage. The trimming process adopts a cold trimming process. When performing cold trimming, a cold trimming die is used to calibrate the forging. A positioning cavity is provided in the center of the cold trimming die, a die core is provided in the middle of the positioning cavity, and a reset spring is provided at the bottom of the die core. The forging is grabbed by a magnetic suction device during the transfer process. .

[0007] A further improvement of the present invention is that the trimming process is carried out by placing the final forging into a cold trimming die, the cold trimming die comprises an upper die plate and a lower die plate, a guide column is provided above the lower die plate, and a guide sleeve corresponding to the guide column is provided below the upper die plate.

[0008] A further improvement of the present invention is that the positioning cavity is fixed to the lower mold plate by bolts, and a trimming punch corresponding to the mold core is provided below the upper mold plate.

[0009] A further improvement of the present invention is that the gap between the guide sleeve and the guide post is no greater than 0.1 mm.

[0010] A further improvement of the present invention is that in the trimming process, the trimming gap is 0.1 mm.

[0011] A further improvement of the present invention is that in the heating process, the heating temperature is 1100-1200°C.

[0012] A further improvement of the present invention is that in the shot peening process, the trimmed forging is sequentially ground and shot peened, wherein the grinding includes circular grinding and chamfer grinding, and the surface is treated by shot peening to obtain a finished workpiece before entering the next process.

[0013] A further improvement of the present invention is that in the final forging process, the oxide scale on the surface of the pre-forged blank is removed, and the pre-forged blank is placed in a final forging die cavity and hammered to obtain a final forging.

[0014] A further improvement of the present invention is that the forging is subjected to a sulfurizing treatment after the heat treatment process.

[0015] Compared with the prior art, the beneficial effects of the present invention are as follows: the present invention changes the traditional trimming process, adopts a cold trimming process, and sets a positioning cavity, so that when facing thin and light forgings, the trimming process can be completed faster, better and safer to prevent them from being skewed, so that the problem of trimming residue of the product is completely solved, the trimming is more uniform, the residue is completely removed, and the incision is smooth and burr-free, and the appearance quality is very good; and the hot cutting is changed to cold cutting, and the risk of burns can also be effectively avoided; at the same time, magnetic suction equipment is used to assist production in grabbing and placing forgings, which solves the problem of employees' difficult operation, reduces the risk of accidents caused by improper operation, improves production efficiency, and further enhances production safety. This process is suitable for light and thin forgings and is suitable for wide promotion and use. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 , Figure 2 It is a schematic diagram of forging; Figure 3 It is a schematic diagram of the cold trimming die in the present invention. DETAILED DESCRIPTION

[0017] The present invention is further illustrated by the following examples: The present invention can be better understood according to the following examples. However, it is easy for those skilled in the art to understand that the specific process conditions and results described in the examples are only used to illustrate the present invention, and should not and will not limit the present invention described in detail in the claims.

[0018] This embodiment provides a forging process for a thin and light forging, which mainly solves the problem of trimming residue and operation difficulty of the thin and light forging, improves product quality and production efficiency, and specifically includes the following steps: S1: Cutting materials. The forging materials are accurately calculated by using the material calculation disk, and then the required blanks are cut by using the fully automatic high-speed cutting machine. The material calculation and cutting steps can improve the material utilization rate, realize the refinement of forging materials, avoid the phenomenon of material waste, and achieve the purpose of saving resources. S2: Heating, placing the blank into a heating furnace, setting the heating temperature to 1100-1200°C, and using continuous feeding; S3: upsetting, placing the blank on an upsetting die and upsetting it through a punch press to obtain a pre-forged part; S4: Final forging, removing the oxide scale on the surface of the pre-forged part, placing it into the final forging die cavity, and hammering it to obtain the final forging part; S5: trimming, using cold trimming process, during which a cold trimming die is used to trim the forgings, the trimming gap is 0.1mm, and the forgings are grabbed by a magnetic device during the transfer process; S6: Heat treatment, the trimmed forgings are placed in a resistance furnace for heating, so that the forging temperature reaches 850℃±50℃, the resistance furnace is set to a speed of 200r / min, the speed is uniform, the holding time is 3h, and then air-cooled at room temperature, the hardness is tested to reach HB130-180, and the microstructure is tested by metallographic microscope to reach level 1-4; S7: Sulfurizing: Place the forgings in a salt bath for electrolytic sulfurizing treatment to improve the wear resistance of the forging surface; S8: Shot peening, grinding and shot peening the forging in sequence, wherein the grinding includes circular grinding and chamfer grinding, and the surface is treated by shot peening to remove oxide scale and burrs; S9: Inspection, storage, check the magnetic detection results with a flaw detector, and require that there are no cracks on all sides of the forgings. If there are cracks, mark them with chalk and place them in the waiting area. After polishing, inspect them again. The qualified workpieces will be inspected for the corresponding specifications and parameters, and those that meet the standards will be sent to storage.

[0019] In this embodiment, a cold trimming process is used, in which the final forging is placed in a cold trimming die, wherein Figure 3 As shown, the cold trimming mold includes an upper template 1 and a lower template 2. A guide column 3 is provided above the lower template 2, and a guide sleeve 4 corresponding to the guide column 3 is provided below the upper template 1. The gap between the guide sleeve and the guide column is 0.1mm to ensure the guiding accuracy. The guide column 3 is set at the rear to avoid interference operation.

[0020] A positioning cavity 5 is provided at the center of the lower template 2, and the positioning cavity 5 is fixed to the lower template 2 by bolts. A core 6 is provided in the middle of the positioning cavity 5, and a return spring 7 is provided at the bottom of the core 6. A trimming punch 8 corresponding to the core 6 is provided below the upper template 1.

[0021] In this embodiment, the process steps of cold trimming are: placing the forging with flash on the positioning cavity 5, and controlling the equipment to push the trimming punch 8 to force the forging into the groove to complete the trimming (when the trimming punch 8 is pressed down, the trimming punch 8 and the mold core 6 completely wrap the forging to prevent the forging from being deformed by force). After the trimming punch 8 is released, the bottom reset spring 7 pushes the mold core to reset, completing a trimming process.

[0022] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of ordinary technicians in the relevant technical field without departing from the purpose of the present invention.

Claims

1. A forging process for thin and light forgings, specifically comprising the following steps: blanking → heating → upsetting → final forging → trimming → heat treatment → shot peening → inspection → storage, Features: The trimming process adopts a cold trimming process. When cold trimming is performed, a cold trimming mold is used to calibrate the forging. A positioning cavity is provided at the center of the cold trimming mold, a mold core is provided in the middle of the positioning cavity, and a return spring is provided at the bottom of the mold core. The forging is grabbed by a magnetic suction device during the transfer process.

2. The forging process of the thin and light forging according to claim 1, Features: The trimming process is performed by placing the final forging into a cold trimming die. The cold trimming die comprises an upper die plate and a lower die plate. A guide column is disposed above the lower die plate, and a guide sleeve corresponding to the guide column is disposed below the upper die plate.

3. The forging process of the thin and light forging according to claim 2, Features: The positioning cavity is fixed to the lower mold plate by bolts, and a trimming punch corresponding to the mold core is provided below the upper mold plate.

4. The forging process of the thin and light forging according to claim 1, Features: The gap between the guide sleeve and the guide post is no greater than 0.1 mm.

5. The forging process of the thin and light forging according to claim 1, Features: In the trimming process, the trimming gap is 0.1 mm.

6. The forging process of the thin and light forging according to claim 1, Features: In the heating process, the heating temperature is 1100-1200°C.

7. The forging process of the thin and light forging according to claim 1, Features: In the shot peening process, the trimmed forging is sequentially ground and shot peened, wherein the grinding includes circular grinding and chamfer grinding, and the surface is treated by shot peening to obtain a finished workpiece, which then enters the next process.

8. The forging process of the thin and light forging according to claim 1, Features: In the final forging process, the oxide scale on the surface of the pre-forged blank is removed, and it is placed in the final forging die cavity and hammered to obtain the final forging.

9. The forging process of the thin and light forging according to claim 1, Features: After the heat treatment process, the forgings are sulfurized.

Citation Information

Patent Citations

  • Finishing die mold structure for stainless steel die forging

    CN102463316A

  • Retaining ring of automobile damper and forging method of retaining ring

    CN106427549A

  • Efficient forging method for agricultural machinery forgings

    CN113118350A

  • Automatic transfer device for forged and pressed workpieces

    CN115446238A

  • Elastic pressing type forging, trimming and character pressing composite die

    CN210188362U

Cited By

  • Machining method of flow guide window blade

    CN119188181A

  • A processing method for guide window blades

    CN119188181B