Tea polyphenol antibacterial nanofiber membrane and spinning solution and preparation method thereof, cotton sliver and preparation method thereof, and yarn

The tea polyphenols/β-cyclodextrin inclusion complex nanofiber membrane is prepared through electrospinning technology, which solves the problem of easy solubility and high temperature decomposition of tea polyphenols, achieves efficient antibacterial and antioxidant effects, and reduces production costs.

CN118773758APending Publication Date: 2024-10-15BINZHOU WEIQIAO NATIONAL SCIENCE & TECHNOLOGY ADVANCED TECHNOLOGY RESEARCH INSTITUTE
View PDF 0 Cites 4 Cited by

Patent Information

Application Number
CN202410983538.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

The application of tea polyphenols in the antibacterial field is limited by its characteristics of being easily soluble in water, easily oxidized and photodegradable, and the existing melt spinning and wet spinning processes have problems with high temperature decomposition and high production costs.

Method used

Using a combined spinning solution of tea polyphenols/β-cyclodextrin inclusion complex, high molecular polymer and solvent, nanofiber membranes were prepared through electrospinning technology to reduce the water solubility of tea polyphenols and improve their stability and biological properties. Utilization.

Benefits of technology

The antibacterial effect and production efficiency of the nanofiber membrane are improved, the process flow is simplified, the production cost is reduced, and the long-term bactericidal and antioxidant properties of tea polyphenols are achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118773758A_ABST
    Figure CN118773758A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of antibacterial material manufacturing, and discloses a tea polyphenol antibacterial nanofiber membrane, a spinning solution and a preparation method of the tea polyphenol antibacterial nanofiber membrane, a cotton sliver, a preparation method of the cotton sliver and yarn. The spinning solution for the tea polyphenol antibacterial nanofiber membrane comprises a high-molecular polymer, a tea polyphenol / beta-cyclodextrin inclusion compound and a solvent, wherein in the spinning solution, the proportion of the high-molecular polymer is 8wt%-15wt%, the proportion of the tea polyphenol / beta-cyclodextrin inclusion compound is 0.5 wt%-8wt%, and the balance is the solvent in percentage by mass. According to the spinning solution provided by the invention, by adding the tea polyphenol / beta-cyclodextrin inclusion compound, on one hand, the biological activity of tea polyphenol is utilized, so that the prepared nanofiber membrane has antibacterial activity and oxidation resistance; on one hand, by adopting the tea polyphenol / beta-cyclodextrin inclusion compound, beta-cyclodextrin is used as a subject, tea polyphenol is used as an object, and tea polyphenol is included, so that the water solubility of tea polyphenol can be effectively reduced, and the solubility and dispersity of tea polyphenol in a spinning solution are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of antibacterial material production, for example, to a tea polyphenol antibacterial nanofiber membrane and its spinning solution, preparation method, cotton strip and its preparation method, and yarn. Background Art

[0002] Tea polyphenols are a natural complex of polyphenolic substances and their derivatives extracted from tea leaves, referred to as TP. It is a natural antioxidant with a broad application prospect and has a variety of biological activities, including antioxidant and antiviral. However, tea polyphenols are easily soluble in water, easily oxidized in the air, and easily deteriorated by light, which restricts their long-term effect and greatly limits the application of tea polyphenols in the antibacterial field. β-cyclodextrin has a unique hydrophobic cavity structure and can selectively include foreign guest molecules to form a stable supramolecular compound, referred to as β-CD. Taking β-cyclodextrin with low water solubility as the main body and tea polyphenols as the guest, the inclusion of tea polyphenols can effectively reduce the water solubility of tea polyphenols, improve stability and bioavailability, and achieve a long-term bactericidal effect due to its sustained-release characteristics.

[0003] In the related art, the application of tea polyphenol / β-cyclodextrin inclusion complex adopts melt spinning or wet spinning to prepare film. Among them, melt spinning is a chemical fiber spinning method in which the polymer is heated and melted, extruded through a spinneret hole, and cooled and solidified in the air to form fibers. The process is short and the production efficiency is high, but the heating temperature is generally 220-300°C. Too high a temperature can easily cause the inclusion complex to decompose. Wet spinning is a chemical fiber spinning method in which the polymer is dissolved in a solvent, a thin stream is ejected through a spinneret hole, and a coagulation bath is entered to form fibers. The wet spinning speed is low, the process is complex, and the production cost is high. Summary of the invention

[0004] In order to provide a basic understanding of some aspects of the disclosed embodiments, a brief summary is given below. The summary is not an extensive review, nor is it intended to identify key / critical elements or delineate the scope of protection of these embodiments, but rather serves as a prelude to the detailed description that follows.

[0005] The embodiments of the present disclosure provide a tea polyphenol antibacterial nanofiber membrane and its spinning solution, preparation method, cotton strip and its preparation method, and yarn, which improve the antibacterial effect of the prepared nanofiber membrane, cotton strip and yarn, and simplify the production process and reduce production costs.

[0006] In some embodiments, a spinning solution for tea polyphenol antibacterial nanofiber membrane is provided, comprising: a high molecular polymer, a tea polyphenol / β-cyclodextrin inclusion complex and a solvent; wherein, in terms of mass percentage, in the spinning solution, the high molecular polymer accounts for 8wt% to 15wt%, the tea polyphenol / β-cyclodextrin inclusion complex accounts for 0.5wt% to 8wt%, and the balance is the solvent.

[0007] Optionally, the high molecular polymer includes one or more of polyacrylonitrile, polylactic acid, polyvinylidene fluoride, polyether sulfone, polyurethane and polyvinylidene fluoride.

[0008] Optionally, when the high molecular polymer includes one or more of polyacrylonitrile, polyethersulfone, polyurethane, and polyvinylidene fluoride, the solvent is N,N-dimethylformamide or N,N-dimethylacetamide; or when the high molecular polymer includes polylactic acid (PLA) and / or polyvinyl lactone, the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide.

[0009] Optionally, when the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide, the mixing ratio of dichloromethane to N,N-dimethylformamide is in a range of 6:4 to 8:2.

[0010] In some embodiments, a method for preparing a spinning solution for a nanofiber membrane is provided, comprising: preparing a tea polyphenol / β-cyclodextrin inclusion complex; dissolving a high molecular weight polymer and the tea polyphenol / β-cyclodextrin inclusion complex in a solvent, and stirring at a preset temperature until completely dissolved to obtain a spinning solution.

[0011] Optionally, when N,N-dimethylformamide is used alone as the solvent, the preset temperature ranges from 25°C to 70°C; or, when N,N-dimethylacetamide is used alone as the solvent, the preset temperature ranges from 25°C to 75°C; or, when a mixed solvent of dichloromethane and N,N-dimethylformamide is used as the solvent, the preset temperature ranges from 25°C to 30°C.

[0012] Optionally, the steps of preparing the tea polyphenol / β-cyclodextrin inclusion complex include: dissolving β-cyclodextrin in a mixed solution of ultrapure water and anhydrous ethanol at 40°C to 80°C, and stirring until the β-cyclodextrin is completely dissolved to obtain a β-cyclodextrin mother liquor; dissolving tea polyphenol in anhydrous ethanol at room temperature, and stirring until the tea polyphenol is completely dissolved to obtain a tea polyphenol solution; wherein the ratio of β-cyclodextrin to tea polyphenol is 1:0.5 to 1:6; cooling the β-cyclodextrin mother liquor to a first set temperature, and maintaining a constant temperature, and dripping the tea polyphenol solution into the β-cyclodextrin mother liquor under continuous stirring to obtain a mixed solution; placing the mixed solution in the dark, and continuously stirring at a second set temperature at 200r / min to 600r / min for a first preset time; placing the mixed solution at a third set temperature and standing for a second preset time; after standing, filtering, washing and drying to obtain a tea polyphenol / β-cyclodextrin inclusion complex.

[0013] In some embodiments, a method for preparing a tea polyphenol antibacterial nanofiber membrane is provided, which is applied to an electrospinning device. The electrospinning device includes a liquid supply component and a receiving roller. The liquid supply component is used to store the spinning liquid as described in any of the above embodiments, and the receiving roller is used to set a receiving substrate. The preparation method includes: determining the receiving distance, spinning voltage and liquid supply speed according to the spinning liquid; controlling the distance between the liquid outlet end of the liquid supply component and the receiving substrate to the receiving distance; controlling the operation of the receiving roller according to a preset rotation speed; and controlling the operation of the electrospinning device according to the spinning voltage and liquid supply speed.

[0014] Optionally, the preset distance ranges from 10 cm to 20 cm; and / or the spinning voltage ranges from 10 kV to 25 kV; and / or the liquid supply rate ranges from 0.5 ml / h to 2 ml / h; and / or the preset rotation speed ranges from 200 rpm to 400 rpm.

[0015] Optionally, according to the spinning solution, determining the receiving distance, the spinning voltage and the liquid supply speed includes: when the spinning solution includes polyacrylonitrile in the component, the preset distance is in the range of 10 cm to 20 cm; and / or, the spinning voltage is in the range of 15 kV to 25 kV; and / or, the liquid supply speed is in the range of 0.8 ml / h to 1.5 ml / h; When the spinning solution includes polylactic acid, the preset distance ranges from 13 cm to 17 cm; and / or the spinning voltage ranges from 12 kV to 18 kV; and / or the liquid supply rate ranges from 0.6 ml / h to 0.8 ml / h.

[0016] Optionally, the electrostatic spinning device is controlled to operate, and after the spinning is completed, the process further includes: placing the spun nanofiber membrane into an oven at 60° C. to 120° C. for 10 to 15 hours.

[0017] In some embodiments, a method for preparing cotton slivers is provided, which is applied to a cotton carding machine. The cotton carding machine is provided with an electrospinning device, and the electrospinning device includes a liquid supply part, which is used to store the spinning liquid as described in any of the above embodiments. The preparation method includes: adjusting the distance between the liquid outlet end of the liquid supply part and the receiving cotton web to 15 cm to 35 cm; according to the propulsion speed of the spinning liquid of 30 mL / h to 60 mL / h and the applied voltage of 30 kV to 65 kV, controlling the electrospinning device to spin.

[0018] In some embodiments, a tea polyphenol antibacterial nanofiber membrane is provided, comprising: a tea polyphenol antibacterial nanofiber membrane prepared by the preparation method of the tea polyphenol antibacterial nanofiber membrane as described in any of the above embodiments.

[0019] In some embodiments, a tampon is provided, comprising: a tampon prepared by the tampon preparation method as described in any of the above embodiments.

[0020] In some embodiments, a yarn is provided, comprising: a cotton strip as described in any of the above embodiments, spun by a spinning machine.

[0021] The tea polyphenol antibacterial nanofiber membrane and its spinning solution, preparation method, cotton strip and its preparation method, and yarn provided in the embodiments of the present disclosure can achieve the following technical effects: The spinning solution provided by the present invention includes: a high molecular polymer, a tea polyphenol / β-cyclodextrin inclusion complex and a solvent; wherein, in terms of mass percentage, in the spinning solution, the high molecular polymer accounts for 8wt% to 15wt%, the tea polyphenol / β-cyclodextrin inclusion complex accounts for 0.5wt% to 8wt%, and the balance is the solvent.

[0022] In the spinning solution provided by the present disclosure, a high molecular weight polymer is added, and the polymer is reasonably set to account for 8wt% to 15wt% in the spinning solution to increase the viscosity of the spinning solution, thereby improving the continuity and stability of the filaments produced during the electrostatic spinning process. By adding 0.5wt% to 8wt% of tea polyphenols / β-cyclodextrin inclusion complex, on the one hand, the biological activity of tea polyphenols is utilized to make the prepared nanofiber membrane have antibacterial and antioxidant properties. On the one hand, by using tea polyphenols / β-cyclodextrin inclusion complex, with β-cyclodextrin as the main body and tea polyphenols as the object, tea polyphenols are enclosed, which can effectively reduce the water solubility of tea polyphenols and improve the solubility and dispersibility of tea polyphenols in the spinning solution.

[0023] The spinning solution provided by the present disclosure adopts a high molecular polymer, a tea polyphenol / β-cyclodextrin inclusion compound and a solvent, and reasonably sets the ratio to improve the continuity and stability of electrospinning.

[0024] The above general description and the following description are exemplary and explanatory only and are not intended to limit the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] One or more embodiments are exemplarily described by corresponding drawings, which do not limit the embodiments. Elements with the same reference numerals in the drawings are shown as similar elements, and the drawings do not constitute a scale limitation, and wherein: Figure 1 It is a schematic diagram of a method for preparing a spinning solution for tea polyphenol antibacterial nanofiber membrane provided by an embodiment of the present disclosure; Figure 2 is a schematic diagram of a method for preparing a tea polyphenol / β-cyclodextrin inclusion compound provided by an embodiment of the present disclosure; Figure 3 is a schematic diagram of a method for preparing a tea polyphenol antibacterial nanofiber membrane provided by an embodiment of the present disclosure; Figure 4 is a SEM image of a PAN / (tea polyphenols / β-cyclodextrin inclusion complex) nanofiber membrane before washing provided by an embodiment of the present disclosure; Figure 5 is a SEM image of a PAN / (tea polyphenols / β-cyclodextrin inclusion complex) nanofiber membrane after washing provided by an embodiment of the present disclosure; Figure 6 is a SEM image of a PAN / tea polyphenol nanofiber membrane before washing provided by an embodiment of the present disclosure; Figure 7 is a SEM image of a PAN / tea polyphenol nanofiber membrane after washing provided by an embodiment of the present disclosure; Figure 8 is a SEM image of a PLA / (tea polyphenols / β-cyclodextrin inclusion complex) nanofiber membrane before washing provided by an embodiment of the present disclosure; Fig. 9 is a SEM image of a PLA / (tea polyphenols / β-cyclodextrin inclusion complex) nanofiber membrane after washing provided by an embodiment of the present disclosure; Fig.10 is a SEM image of a PLA / tea polyphenol nanofiber membrane before washing provided by an embodiment of the present disclosure; Fig.11 is a SEM image of a PLA / tea polyphenol nanofiber membrane after washing provided by an embodiment of the present disclosure; Fig.12 It is a schematic diagram of a method for preparing a tampon provided in one embodiment of the present disclosure. DETAILED DESCRIPTION

[0026] In order to be able to understand the features and technical contents of the embodiments of the present disclosure in more detail, the implementation of the embodiments of the present disclosure is described in detail below in conjunction with the accompanying drawings. The attached drawings are for reference only and are not used to limit the embodiments of the present disclosure. In the following technical description, for the convenience of explanation, a full understanding of the disclosed embodiments is provided through multiple details. However, one or more embodiments can still be implemented without these details. In other cases, to simplify the drawings, well-known structures and devices can be simplified for display.

[0027] The terms "first", "second", etc. in the specification and claims of the embodiments of the present disclosure and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the terms used in this way can be interchanged where appropriate, so that the embodiments of the embodiments of the present disclosure described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions.

[0028] Unless otherwise stated, the term "plurality" means two or more.

[0029] In the embodiment of the present disclosure, the character " / " indicates that the preceding and following objects are in an "or" relationship. For example, A / B indicates: A or B.

[0030] The term "and / or" is a description of the association relationship between objects, indicating that three relationships can exist. For example, A and / or B means: A or B, or, A and B.

[0031] The term "correspondence" may refer to an association relationship or a binding relationship. The correspondence between A and B means that there is an association relationship or a binding relationship between A and B.

[0032] In some embodiments, a spinning solution for tea polyphenol antibacterial nanofiber membrane is provided, comprising: a polymer, a tea polyphenol / β-cyclodextrin inclusion compound, and a solvent. In particular, in the spinning solution, the polymer accounts for 8wt% to 15wt%, the tea polyphenol / β-cyclodextrin inclusion compound accounts for 0.5wt% to 8wt%, and the balance is the solvent.

[0033] In the spinning solution provided by the present disclosure, a high molecular weight polymer is added, and the polymer is reasonably set to account for 8wt% to 15wt% in the spinning solution to increase the viscosity of the spinning solution, thereby improving the continuity and stability of the filaments produced during the electrostatic spinning process. By adding 0.5wt% to 8wt% of tea polyphenols / β-cyclodextrin inclusion complex, on the one hand, the biological activity of tea polyphenols is utilized to make the prepared nanofiber membrane have antibacterial and antioxidant properties. On the one hand, by using tea polyphenols / β-cyclodextrin inclusion complex, with β-cyclodextrin as the main body and tea polyphenols as the object, tea polyphenols are enclosed, which can effectively reduce the water solubility of tea polyphenols and improve the solubility and dispersibility of tea polyphenols in the spinning solution.

[0034] The spinning solution provided by the present disclosure adopts a high molecular polymer, a tea polyphenol / β-cyclodextrin inclusion compound and a solvent, and reasonably sets the ratio to improve the continuity and stability of electrospinning.

[0035] Optionally, the high molecular polymer includes one or more of polyacrylonitrile, polylactic acid, polyvinylidene fluoride, polyether sulfone, polyurethane and polyvinylidene fluoride.

[0036] In this embodiment, polyacrylonitrile (PAN) is added to the spinning solution to improve the uniformity and continuity of the fibers formed during the electrospinning process, thereby improving the production efficiency of electrospinning. Polylactic acid (PLA) is added to the electrospinning solution to improve the biodegradability and biocompatibility of the nanofibers obtained by spinning. Polycaprolactin (PCL) is added to the electrospinning solution to improve the flexibility, biodegradability and biocompatibility of the nanofibers obtained by spinning. Polyethersulfone (PES) is added to the electrospinning solution to improve the thermal stability of the nanofibers obtained by spinning, improve the production efficiency of electrospinning, and improve the continuity and stability of the filaments. Polyurethane (PU) is added to the electrospinning solution to improve the elasticity, flexibility and biocompatibility of the nanofibers obtained by spinning. Polyvinylidene fluoride (PVDF) is added to the electrospinning solution to improve the chemical corrosion resistance, heat resistance and electrical insulation of the nanofibers obtained by spinning. In the process of preparing the electrospinning solution, one or more of polyacrylonitrile, polylactic acid, polygalactone, polyethersulfone, polyurethane and polyvinylidene fluoride may be selected and added to obtain the spinning solution.

[0037] Optionally, when the high molecular polymer includes one or more of polyacrylonitrile, polyethersulfone, polyurethane, and polyvinylidene fluoride, the solvent is N,N-dimethylformamide or N,N-dimethylacetamide.

[0038] Optionally, when the high molecular polymer includes polylactic acid (PLA) and / or polygalactone, the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide.

[0039] In this embodiment, according to the characteristics of the type of the added polymer, a solvent matching the characteristics of the added polymer is selected to achieve the ability to dissolve the polymer without affecting the characteristics of the polymer. Specifically, when the polymer includes one or more of polyacrylonitrile, polyethersulfone, polyurethane, and polyvinylidene fluoride, the solvent is N,N-dimethylformamide or N,N-dimethylacetamide. The boiling points of N,N-dimethylformamide and N,N-dimethylacetamide are relatively high, while polyacrylonitrile, polyethersulfone, polyurethane, and polyvinylidene fluoride can also withstand the temperature corresponding to the solvent. In this way, these polymers can be efficiently dissolved, the dissolution efficiency can be improved, and the characteristics of the polymer can be not affected. When the polymer includes polylactic acid (PLA) and / or polyvinylidene fluoride, the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide. The boiling point of the mixed solvent of dichloromethane and N,N-dimethylformamide is relatively low, and the corresponding polylactic acid (PLA) and polylactide can be easily dissolved at the corresponding temperature. In this way, the two polymers can be dissolved and the volatilization of the solvent during the dissolution process can be avoided.

[0040] Optionally, when the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide, the mixing ratio of dichloromethane to N,N-dimethylformamide is in the range of 6:4 to 8:2.

[0041] In this embodiment, by setting the mixing ratio of dichloromethane and N,N-dimethylformamide in the range of 6:4 to 8:2, the high molecular polymer and tea polyphenols / β-cyclodextrin inclusion complex are dissolved, and the spinning solution obtained by electrospinning has a better morphology of the nanofiber membrane.

[0042] Optionally, when the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide, the mixing ratio of dichloromethane to N,N-dimethylformamide is specifically 6:4, 7:3 or 8:2.

[0043] In some embodiments, in combination Figure 1 As shown, a method for preparing a spinning solution for tea polyphenol antibacterial nanofiber membrane is provided, comprising: S101, preparing tea polyphenols / β-cyclodextrin inclusion complex.

[0044] S102, dissolving the high molecular polymer and the tea polyphenol / β-cyclodextrin inclusion compound in a solvent, and stirring at a preset temperature until they are completely dissolved to obtain a spinning solution.

[0045] The preparation method of the spinning solution provided by the present disclosure includes: first, preparing a tea polyphenol / β-cyclodextrin inclusion complex. By using the tea polyphenol / β-cyclodextrin inclusion complex, taking β-cyclodextrin with low water solubility as the main body and tea polyphenol as the object, the tea polyphenol is enclosed, which can effectively reduce the water solubility and stability of the tea polyphenol, and at the same time achieve a long-lasting bactericidal effect due to the sustained release characteristics. Secondly, the polymer and the tea polyphenol / β-cyclodextrin inclusion complex are dissolved in a solvent, and stirred at a preset temperature until completely dissolved to obtain a spinning solution that can be used for electrostatic spinning. By using the spinning solution prepared by the present disclosure, it can be used for electrostatic spinning, and then a nanofiber membrane including the tea polyphenol / β-cyclodextrin inclusion complex can be prepared by the electrostatic spinning method. Compared with the process methods of melt spinning and wet spinning used in the related art, the electrostatic spinning method is simple in process, and the prepared nanofiber membrane has better water solubility resistance and a more lasting antibacterial effect.

[0046] Optionally, when N,N-dimethylformamide is used alone as the solvent, the preset temperature ranges from 25°C to 70°C.

[0047] In this embodiment, when the preset temperature is higher than 70°C, N,N-dimethylformamide is volatile. When the preset temperature is lower than 25°C, it will affect the dissolution state of the polymer. Therefore, when N,N-dimethylformamide is used alone as the solvent, the preset temperature range is set to 25°C to 70°C to reduce the volatilization of N,N-dimethylformamide and the impact on the concentration of the spinning solution, and the appropriate temperature can be selected according to the dissolution efficiency requirements to achieve the dissolution of the polymer and the tea polyphenol / β-cyclodextrin inclusion complex.

[0048] Optionally, when N,N-dimethylformamide is used alone as the solvent, the preset temperature includes but is not limited to: 25°C, 30°C, 35°C, 40°C, 45°C, 50°C, 55°C, 60°C, 65°C or 70°C.

[0049] Optionally, when N,N-dimethylacetamide is used alone as the solvent, the preset temperature ranges from 25°C to 75°C.

[0050] In this embodiment, when the preset temperature is higher than 75°C, N,N-dimethylacetamide is volatile. When the preset temperature is lower than 25°C, it will affect the dissolution state of the polymer. Therefore, when N,N-dimethylacetamide is used alone as the solvent, the preset temperature range is set to 25°C to 75°C to reduce the volatilization of N,N-dimethylacetamide and the impact on the concentration of the spinning solution, and the appropriate temperature can be selected according to the dissolution efficiency requirements to achieve the dissolution of the polymer and the tea polyphenol / β-cyclodextrin inclusion complex.

[0051] Optionally, when N,N-dimethylacetamide is used alone as the solvent, the preset temperature includes but is not limited to: 25°C, 30°C, 35°C, 40°C, 45°C, 50°C, 55°C, 60°C, 65°C, 70°C or 75°C.

[0052] Optionally, when the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide, the preset temperature ranges from 25°C to 30°C.

[0053] In this embodiment, when the preset temperature is higher than 30°C, dichloromethane is volatile. When the preset temperature is lower than 25°C, it will affect the dissolution state of the polymer. Therefore, when the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide, the preset temperature is set to a value range of 25°C to 30°C to reduce the volatilization of dichloromethane and the influence on the concentration of the spinning solution, and the appropriate temperature can be selected according to the dissolution efficiency requirements to achieve the dissolution of the polymer and the tea polyphenol / β-cyclodextrin inclusion complex.

[0054] Optionally, when the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide, the preset temperature includes but is not limited to: 25°C, 26°C, 27°C, 28°C, 29°C or 30°C.

[0055] In some embodiments, in combination Figure 2 As shown, a method for preparing a tea polyphenol / β-cyclodextrin inclusion compound is provided, comprising: S201, dissolving β-cyclodextrin in a mixed solution of ultrapure water and anhydrous ethanol at 40° C. to 80° C., and stirring until the β-cyclodextrin is completely dissolved to obtain a β-cyclodextrin mother solution.

[0056] In this embodiment, a β-cyclodextrin mother solution is prepared. Specifically, the dissolution is carried out at 40°C to 80°C to improve the solubility and uniformity of the β-cyclodextrin. Using a mixed solution of ultrapure water and anhydrous ethanol as a solvent helps to improve the dissolution rate and solubility of the β-cyclodextrin. The dissolution rate and uniformity of the dissolution are improved by continuous stirring.

[0057] The volume ratio of ultrapure water to anhydrous ethanol is 2:1 to optimize the dissolution rate and solubility of β-cyclodextrin. The stirring time lasts for 14 to 16 minutes, and the specific stirring time can be adjusted and set as needed.

[0058] S202, dissolving tea polyphenols in anhydrous ethanol at room temperature, stirring until the tea polyphenols are completely dissolved, to obtain a tea polyphenol solution.

[0059] Among them, the ratio of β-cyclodextrin to tea polyphenols is 1:0.5 to 1:6.

[0060] In this embodiment, a tea polyphenol solution is prepared. Specifically, tea polyphenol is dissolved in anhydrous ethanol at room temperature, and stirred continuously until the tea polyphenol is completely dissolved. Anhydrous ethanol is selected as the solvent to enhance the dissolution effect of tea polyphenol.

[0061] The stirring time is greater than 1 hour, and the specific time can be set according to the dissolution of tea polyphenols.

[0062] Furthermore, the addition ratio of the mass of β-cyclodextrin to the mass of tea polyphenols is 1:0.5 to 1:6, so as to optimize the inclusion effect of the obtained tea polyphenols / β-cyclodextrin inclusion complex.

[0063] Optionally, the mass ratio of tea polyphenols to anhydrous ethanol is 1:10 to 1:70. The solubility of tea polyphenols in anhydrous ethanol decreases with increasing concentration. By adjusting the mass ratio of tea polyphenols to anhydrous ethanol, tea polyphenol solutions of different concentrations can be prepared to meet different application requirements.

[0064] S203, cooling the β-cyclodextrin mother solution to a first set temperature and maintaining a constant temperature, and dripping the tea polyphenol solution into the β-cyclodextrin mother solution under continuous stirring to obtain a mixed solution.

[0065] Optionally, the value range of the first set temperature is 45° C. to 55° C. The specific value of the first set temperature includes but is not limited to: 45° C., 47° C., 49° C., 50° C., 53° C. or 55° C.

[0066] S204, placing the mixed solution in a dark condition, and continuously stirring at a second set temperature at 200 r / min to 600 r / min for a first preset time.

[0067] Optionally, the second set temperature ranges from 45° C. to 55° C. Specific values ​​of the second set temperature include but are not limited to: 45° C., 47° C., 49° C., 50° C., 53° C. or 55° C.

[0068] Optionally, the first preset duration ranges from 12 hours to 24 hours. Specific values ​​of the first preset duration include but are not limited to: 12 hours, 14 hours, 16 hours, 18 hours, 20 hours, 22 hours or 24 hours.

[0069] S205, placing the mixed solution at a third set temperature and leaving it to stand for a second preset time.

[0070] Optionally, the third set temperature has a value range of -5°C to -3.5°C. The specific value of the third set temperature includes but is not limited to: -5°C, -4°C, or -3.5°C.

[0071] Optionally, the second preset time length has a value range of 20 hours to 25 hours. Specific values ​​of the second preset time length include but are not limited to: 20 hours, 22 hours, 23 hours, 24 hours or 25 hours.

[0072] In this embodiment, the prepared β-cyclodextrin mother liquor is mixed with the tea polyphenol solution. Specifically, the temperature of the β-cyclodextrin mother liquor is reduced to 45°C to 55°C, which helps to maintain the stability of β-cyclodextrin and tea polyphenols and avoid degradation caused by high temperature. Then, the constant temperature is maintained by heating in a water bath so that the temperature remains unchanged during the mixing process, which helps to form a uniform inclusion complex. During continuous stirring, the tea polyphenol solution is slowly dripped into the β-cyclodextrin mother liquor using a constant pressure funnel to obtain a mixed solution. By controlling the mixing speed, local overconcentration or unevenness is avoided and the uniformity of the mixed solution is improved. The mixed solution is placed in a dark environment to reduce the effect of light on tea polyphenols and β-cyclodextrin. The temperature is maintained at 45°C to 55°C, and continuous stirring is continued at 200r / min to 600r / min for 12h to 24h to allow tea polyphenols to fully contact β-cyclodextrin and form a stable inclusion complex. Then, the mixed solution is placed in an environment of -5°C to -3.5°C and allowed to stand for 20h to 25h, which is conducive to the crystallization and precipitation of the inclusion complex and facilitates subsequent separation and purification.

[0073] S206, after standing, filtering is performed.

[0074] Optionally, a circulating vacuum pump may be used for filtration.

[0075] S207, after filtering, washing is performed.

[0076] Optionally, wash once with water and once with absolute ethanol.

[0077] S208, washing and drying to obtain a tea polyphenol / β-cyclodextrin inclusion complex.

[0078] Optionally, drying is performed under vacuum.

[0079] In this embodiment, the mixed solution after standing is filtered by a circulating vacuum pump to improve the filtering efficiency and quickly separate the solid inclusion compound and the liquid. After filtering, it is washed once with water and once with anhydrous ethanol to remove impurities and unreacted tea polyphenols attached to the surface of the inclusion compound. Then vacuum drying is performed, and the structural integrity of the tea polyphenol / β-cyclodextrin inclusion compound is improved by controlling the drying speed and temperature.

[0080] In some embodiments, in combination Figure 3As shown, a method for preparing a tea polyphenol antibacterial nanofiber membrane is provided, which is applied to an electrospinning device. The electrospinning device includes a liquid supply part and a receiving roller. The liquid supply part is used to store the spinning solution as described in any of the above embodiments, and the receiving roller is used to set a receiving substrate. The preparation method includes: S301, determining a receiving distance, a spinning voltage and a liquid supply speed according to the spinning solution.

[0081] S302, controlling the distance between the liquid outlet of the liquid supply component and the receiving substrate to a receiving distance.

[0082] S303, controlling the receiving roller to run at a preset speed. S304, controlling the operation of the electrospinning device according to the spinning voltage and the liquid supply speed.

[0083] The method for preparing tea polyphenol antibacterial nanofiber membrane provided by the embodiments of the present disclosure is applied to an electrostatic spinning device. The electrostatic spinning device includes a liquid supply part and a receiving roller. The liquid outlet end of the liquid supply part is connected to the positive electrode of a high-voltage power supply. The receiving roller is connected to the negative electrode of the high-voltage power supply. A receiving substrate is arranged on the receiving roller. The spinning solution prepared in any of the above embodiments is loaded into the liquid supply part. The distance from the liquid outlet end of the liquid supply part to the receiving substrate is adjusted to the receiving distance. And the receiving roller is controlled to rotate at a preset speed. According to the spinning voltage and the liquid supply speed, the operation of the electrostatic spinning device is controlled to perform spinning to form a nanofiber membrane on the surface of the receiving substrate.

[0084] The disclosed embodiment adopts electrostatic spinning equipment to spin a spinning solution containing tea polyphenols / β-cyclodextrin inclusion complex to obtain a nanofiber membrane. Electrostatic spinning technology is a method for preparing nanofibers, which is a process of forming slender fibers by applying high voltage to a polymer solution. Different from melt spinning and wet spinning, electrostatic spinning has low manufacturing cost and simple process, and can quickly obtain ultrafine fibers with fiber diameter distribution ranging from a few nanometers to a few microns and a wide variety. The three-dimensional nanofiber membrane not only has the characteristics of small nanoparticle size and large specific surface area, but also has the advantages of good mechanical stability, small fiber membrane pore size, high porosity, and good fiber continuity. The disclosed embodiment adopts electrostatic spinning technology to electrostatically spin a spinning solution containing tea polyphenols / β-cyclodextrin inclusion complex to prepare a nanofiber membrane, which has good water solubility resistance and long-term antibacterial effect.

[0085] Optionally, the preset distance has a value range of 10 cm to 20 cm. Specific values ​​of the preset distance include but are not limited to 10 cm, 12 cm, 14 cm, 16 cm, 18 cm or 20 cm.

[0086] Optionally, the spinning voltage ranges from 10 kV to 25 kV. According to the thickness requirements of the nanofibers, the spinning voltage is reasonably set to improve the stability of the spinning and have better uniformity. The specific values ​​of the spinning voltage include but are not limited to: 10 kV, 12 kV, 14 kV, 16 kV, 18 kV, 20 kV, 22 kV, 23 kV or 25 kV.

[0087] Optionally, the liquid supply speed ranges from 0.5 ml / h to 2 ml / h. The liquid supply speed is reasonably set to improve the stability and continuity of the wire production. The specific values ​​of the liquid supply speed include but are not limited to: 0.5 ml / h, 0.7 ml / h, 0.9 ml / h, 1.1 ml / h, 1.3 ml / h, 1.5 ml / h, 1.8 ml / h or 2 ml / h.

[0088] Optionally, the preset speed ranges from 200 rpm to 400 rpm. The specific value of the preset speed includes but is not limited to: 200 rpm, 250 rpm, 350 rpm or 400 rpm. By matching the preset speed and receiving distance with the liquid supply speed, the uniformity of the nanofiber membrane formation and the spinning efficiency are improved.

[0089] Optionally, the receiving substrate comprises tin foil.

[0090] In some embodiments, according to the spinning solution, determining the receiving distance, the spinning voltage and the liquid supply speed includes: when the spinning solution includes polyacrylonitrile, the preset distance is in the range of 10 cm to 20 cm. And / or, the spinning voltage is in the range of 15 kV to 25 kV. And / or, the liquid supply speed is in the range of 0.8 ml / h to 1.5 ml / h.

[0091] In this embodiment, when the spinning solution includes polyacrylonitrile, considering that polyacrylonitrile has good mechanical stability, the preset distance, spinning voltage and liquid supply speed are set accordingly to improve the stability and continuity of the spinning, so as to improve the integrity of the prepared nanofiber membrane.

[0092] In some embodiments, according to the spinning solution, determining the receiving distance, the spinning voltage and the liquid supply speed includes: when the spinning solution includes polylactic acid, the preset distance is in the range of 13 cm to 17 cm. And / or, the spinning voltage is in the range of 12 kV to 18 kV. And / or, the liquid supply speed is in the range of 0.6 ml / h to 0.8 ml / h.

[0093] In this embodiment, when the spinning solution includes polylactic acid, considering that the solvent used for polylactic acid is volatile, the preset distance, spinning voltage and liquid supply speed are adjusted to improve the spinning effect and reduce the occurrence of blockage at the liquid outlet due to solvent volatilization.

[0094] Optionally, the electrostatic spinning device is controlled to operate, and after the spinning is completed, the process further includes: placing the spun nanofiber membrane into an oven at 60° C. to 120° C. for 10 to 15 hours.

[0095] In this embodiment, after the spinning of the nanofiber membrane is completed, the spun nanofiber membrane is placed in an oven at 60° C. to 120° C. for 10 to 15 hours. In this way, the solvent in the spun nanofiber membrane is evaporated to reduce the residual solvent rate, thereby obtaining a dried nanofiber membrane.

[0096] Optionally, the electrospinning device includes: a single-needle electrospinning machine, a multi-needle electrospinning machine or a needleless electrospinning machine.

[0097] In some embodiments, a tea polyphenol antibacterial nanofiber membrane is provided, comprising: a tea polyphenol antibacterial nanofiber membrane prepared by the preparation method of the tea polyphenol antibacterial nanofiber membrane as described in any of the above embodiments.

[0098] The nanofiber membrane provided in the embodiment of the present disclosure is prepared by spinning with an electrostatic spinning device using the spinning solution provided in any of the above embodiments and the preparation method of the nanofiber membrane provided in any of the above embodiments. In this way, the tea polyphenol / β-cyclodextrin inclusion complex is prepared by electrostatic spinning to obtain a natural and environmentally friendly antibacterial film with a nanofiber structure and a large specific surface area, thereby providing excellent antibacterial biological activity. Moreover, compared with melt spinning and wet spinning in the related art, the antibacterial film prepared by electrostatic spinning has high production efficiency, simple process and low cost. The prepared nanofiber membrane reduces the water solubility of tea polyphenols and improves the stability and antibacterial long-term effect of tea polyphenols. Moreover, compared with the antibacterial fabrics prepared by melt spinning and wet spinning, the product quality problems caused by the conventional antibacterial function finishing method are avoided, such as: stiff hand feel, non-persistent functionality, and non-water washability. The nanofiber membrane prepared by the present disclosure is more fitted and soft.

[0099] Exemplarily, the preparation case of tea polyphenol antibacterial nanofiber membrane is prepared by using the spinning solution provided in any of the above embodiments and the preparation method of tea polyphenol antibacterial nanofiber membrane provided in any of the above embodiments as follows: Example 1 First, prepare the spinning solution, weigh 80g polyacrylonitrile (PAN) and 20g tea polyphenol / β-cyclodextrin inclusion complex with an electronic balance, dissolve in 400ml N,N-dimethylformamide (DMF), stir the spinning solution magnetically at room temperature for 5h until the solute is completely dissolved, and let it stand for use. Draw the spinning solution into the syringe of the single-needle electrospinning machine, set the receiving distance to 15cm, the liquid supply speed to 0.8ml / h, the spinning voltage to 18kV, and use tin foil to receive the ejected micro-nano fibers.

[0100] Comparative Example 1 First, prepare the spinning solution, weigh 80g polyacrylonitrile (PAN) and 20g tea polyphenols with an electronic balance, dissolve them in 400ml N,N-dimethylformamide (DMF), stir the spinning solution with magnetic force at room temperature for 5h until the solute is completely dissolved, and let it stand for use. Draw the spinning solution into the syringe of the single-needle electrospinning machine, set the receiving distance to 15cm, the liquid supply speed to 0.8ml / h, the spinning voltage to 18kV, and use tin foil to receive the ejected micro-nano fibers.

[0101] Example 2 First, prepare the spinning solution, weigh 60g of polylactic acid (PLA) and 40g of tea polyphenol / β-cyclodextrin inclusion complex using an electronic balance, dissolve in 250ml of dichloromethane (DCM) and 100ml of N,N-dimethylformamide (DMF), stir the spinning solution magnetically at room temperature for 5h until the solute is completely dissolved, and let it stand for use. Draw the spinning solution into the syringe of the single-needle electrospinning machine, set the receiving distance to 15cm, the liquid supply speed to 0.6ml / h, the spinning voltage to 15kV, and use tin foil to receive the ejected micro-nano fibers.

[0102] Comparative Example 2 First, prepare the spinning solution. Use an electronic balance to weigh 60g of polylactic acid (PLA) and 40g of tea polyphenols, dissolve them in 250ml of dichloromethane (DCM) and 100ml of N,N-dimethylformamide (DMF). Stir the spinning solution magnetically at room temperature for 5h until the solute is completely dissolved, and then let it stand for use. Draw the spinning solution into the syringe of the single-needle electrospinning machine, set the receiving distance to 15cm, the liquid supply speed to 0.5ml / h, the spinning voltage to 15kV, and use tin foil to receive the ejected micro-nano fibers.

[0103] The performance tests of the nanofiber membranes obtained in Example 1, Example 2, Comparative Example 1, and Comparative Example 2 were performed as follows: The nanofiber membrane was immersed in water and stirred for 20 minutes, then taken out and dried to obtain the washed nanofiber membrane. The surface morphology of the nanofiber membrane was characterized by SEM, and the loading of TP on the fiber before and after washing was observed.

[0104] in, Figure 4 and Figure 5 The SEM images of PAN / (tea polyphenols / β-cyclodextrin inclusion complex) nanofiber membrane before and after washing. Figure 6 and Figure 7 The SEM images of PAN / tea polyphenols nanofiber membrane before and after washing. Figure 8 and Fig. 9 The SEM images of PLA / (tea polyphenols / β-cyclodextrin inclusion complex) nanofiber membranes before and after washing. Fig.10 and Fig.11 The SEM images of PLA / tea polyphenols nanofiber membranes before and after washing.

[0105] Combination Figure 6 and Figure 7 , Fig.10 and Fig.11 As shown in the figure, after washing the PAN / tea polyphenols or PLA / tea polyphenols composite nanofiber membrane, the tea polyphenols particles on the fiber surface fell off or precipitated. Figure 4 and Figure 5 , Figure 8 and Fig. 9 As shown in the figure, after tea polyphenols are encapsulated in β-CD, the tea polyphenol / β-cyclodextrin inclusion complex is electrospun again. After washing, the tea polyphenol particles do not fall off, and the fiber thickness is uniform and the morphology is good. That is, the nanofiber membrane obtained by electrospinning the tea polyphenol / β-cyclodextrin inclusion complex carries more tea polyphenols, and thus has a better antibacterial effect.

[0106] In some embodiments, in combination Fig.12 As shown, a method for preparing cotton sliver is provided, which is applied to a carding machine. The carding machine is provided with an electrostatic spinning device, and the electrostatic spinning device includes a liquid supply part, which is used to store the spinning solution as described in any of the above embodiments. The preparation method includes: S1201, adjust the distance between the liquid outlet end of the liquid supply part and the receiving cotton mesh to 15 cm to 35 cm.

[0107] S1202, controlling the electrospinning device to perform spinning according to a propulsion speed of the spinning solution of 30 mL / h to 60 mL / h and an applied voltage of 30 kV to 65 kV.

[0108] The method for preparing cotton strips provided in the embodiments of the present disclosure is applied to a carding machine, and the carding machine is provided with an electrostatic spinning device, and the electrostatic spinning device includes a liquid supply part, and the liquid supply part is used to store the spinning solution as described in any of the above embodiments. The preparation method includes: adjusting the distance between the liquid outlet end of the liquid supply part and the receiving cotton net to 15cm to 35cm to improve the deposition effect of the fiber. According to the propulsion speed of the spinning solution of 30mL / h to 60mL / h and the applied voltage of 30kV to 65kV, the electrostatic spinning device is controlled to spin to improve the spinning efficiency, and improve the stability and continuity of the silk output.

[0109] In the embodiment of the present disclosure, the spinning solution is prepared and injected into the liquid supply part. The distance between the liquid outlet end of the liquid supply part and the receiving cotton web is adjusted to 15 cm to 35 cm. After the preliminary preparations are completed, the cotton carding machine is started, and the cotton carding machine drives the cotton web forward. During the forward movement, the spinning solution is sprayed onto the cotton web through the electrostatic spinning device, and the cotton web is then passed through the drawing device of the cotton carding machine to form cotton strips. The method for preparing cotton strips provided by the embodiment of the present disclosure has a larger spinning solution propulsion speed and applied voltage, thereby improving the preparation efficiency of cotton strips, and making it easier to achieve mass production of cotton strips with antibacterial properties.

[0110] Optionally, the specific value of the distance between the liquid outlet end of the liquid supply component and the receiving cotton web includes but is not limited to: 15 cm, 20 cm, 25 cm, 30 cm or 35 cm.

[0111] Optionally, specific values ​​of the applied voltage include but are not limited to: 30 kV, 35 kV, 40 kV, 45 kV, 50 kV, 55 kV, 60 kV or 65 kV.

[0112] Optionally, specific values ​​of the propulsion speed of the spinning solution include but are not limited to: 30 mL / h, 40 mL / h, 50 mL / h or 60 mL / h.

[0113] In some embodiments, a tampon is provided, comprising: a tampon prepared by the tampon preparation method as described in any of the above embodiments.

[0114] The tampons provided in the present disclosure are prepared using the spinning solution provided in any of the above embodiments and the tampons preparation method provided in any of the above embodiments. In this way, the tea polyphenols / β-cyclodextrin inclusion complex is sprayed onto a cotton net through an electrostatic spinning device to prepare a natural and environmentally friendly antibacterial tampons. The fibers formed on the cotton net by electrostatic spinning have a nanofiber structure and a large specific surface area, thereby providing excellent antibacterial biological activity. Moreover, compared with melt spinning and wet spinning in the related art, electrostatic spinning for preparing tampons has high production efficiency, simple process and low cost. The prepared tampons reduce the water solubility of tea polyphenols and improve the stability and antibacterial long-term effect of tea polyphenols.

[0115] In some embodiments, a yarn is provided, comprising: a cotton strip as described in any of the above embodiments, spun by a spinning machine.

[0116] The yarn provided by the embodiment of the present disclosure is a yarn produced by a spinning mechanism using the cotton strip described in any of the above embodiments. The yarn has all the beneficial effects of the cotton strip described in any of the above embodiments, which will not be described in detail here.

[0117] Exemplarily, a preparation case of tea polyphenol antibacterial yarn prepared by a spinning machine using the spinning solution provided in any of the above embodiments and the cotton sliver preparation method provided in any of the above embodiments is as follows: Example 3 First, prepare the spinning solution, weigh 240g polyacrylonitrile (PAN) and 60g tea polyphenol / β-cyclodextrin inclusion complex with an electronic balance, dissolve in 1200ml N,N-dimethylformamide (DMF), and stir the spinning solution magnetically at room temperature until the solute is completely dissolved. Place the dissolved spinning solution in the extractor of the electrospinning device, set the vertical height of the spinning nozzle to 25cm from the cotton net, the propulsion speed of the spinning solution to 50ml / h, the spinning voltage to 55kV, spray the spinning solution onto the cotton net in the process of advancing, and then pass through the drawing device to form strips, and prepare cotton yarn through the spinning machine.

[0118] Comparative Example 3 First, prepare the spinning solution, weigh 240g polyacrylonitrile (PAN) and 60g tea polyphenols with an electronic balance, dissolve them in 1200ml N,N-dimethylformamide (DMF), and stir the spinning solution with magnetic force at room temperature until the solute is completely dissolved. Place the dissolved spinning solution in the extractor of the electrospinning device, set the vertical height of the spinning nozzle to 25cm from the cotton net, the propulsion speed of the spinning solution to 50ml / h, the spinning voltage to 55kV, spray the spinning solution onto the cotton net in the process of advancing, and then pass through the drawing device to form strips, and then prepare cotton yarn through the spinning machine.

[0119] Example 4 First, prepare the spinning solution. Use an electronic balance to weigh 240g of polylactic acid (PLA) and 60g of tea polyphenol / β-cyclodextrin inclusion complex, dissolve them in 840ml of dichloromethane (DCM) and 360ml of N,N-dimethylformamide (DMF). The spinning solution is magnetically stirred at room temperature until the solute is completely dissolved. Place the dissolved spinning solution in the extractor of the electrospinning device, set the vertical height of the spinning nozzle to 25cm from the cotton net, set the propulsion speed of the spinning solution to 45ml / h, and the spinning voltage to 60kV. Spray the spinning solution onto the cotton net in the process of moving forward, and then pass through the drawing device to form strips, and then prepare cotton yarn through a spinning machine.

[0120] Comparative Example 4 First, prepare the spinning solution, weigh 240g of polylactic acid (PLA) and 60g of tea polyphenols with an electronic balance, dissolve them in 840ml of dichloromethane (DCM) and 360ml of N,N-dimethylformamide (DMF), and stir the spinning solution magnetically at room temperature until the solute is completely dissolved. Place the dissolved spinning solution in the extractor of the electrospinning device, set the vertical height of the spinning nozzle to 25cm from the cotton net, the propulsion speed of the spinning solution to 45ml / h, the spinning voltage to 60kV, spray the spinning solution onto the cotton net in the process of moving forward, and then form it into strips through the drawing device, and prepare it into cotton yarn through the spinning machine.

[0121] The yarn was washed 50 times in accordance with GB / T 12490-2014 “Textiles - Tests for Colour Fastness - Colour Fastness to Domestic and Commercial Washing”, and the antibacterial properties of the yarns prepared in Example 3, Example 4, Comparative Example 3 and Comparative Example 4 were tested in accordance with GB / T 20944.3-2008 “Evaluation of Antibacterial Properties of Textiles - Part 3: Oscillation Method”, and the antibacterial properties of the yarns were tested as shown in Table 1.

[0122] As shown in Table 1, the cotton yarn prepared in Comparative Example 3 and the cotton yarn prepared in Comparative Example 4 have no antibacterial effect, indicating that after 50 times of washing, the tea polyphenols loaded on the fibers in the yarn are dissolved by water. However, according to the evaluation standard of GB / T 20944.3-2008, after 50 times of washing, the cotton yarn prepared in Example 3 and the cotton yarn prepared in Example 4 are loaded with tea polyphenols / β-cyclodextrin inclusion complex, have antibacterial effect, and reach the AAA grade standard (Escherichia coli antibacterial rate>80%, Staphylococcus aureus antibacterial rate>70%, Staphylococcus aureus antibacterial rate>60%), and have good antibacterial effect.

[0123] Table 1 Test results of yarn antibacterial properties

[0124] The above description and the accompanying drawings sufficiently illustrate the embodiments of the present disclosure to enable those skilled in the art to practice them.

[0125] The flowcharts and block diagrams in the accompanying drawings show the architecture, functions and operations that may be implemented according to the systems and methods of the embodiments of the present disclosure. In some alternative implementations, the functions marked in the boxes may also occur in an order different from that marked in the accompanying drawings. For example, two consecutive boxes can actually be executed substantially in parallel, and they may sometimes be executed in the opposite order, which may depend on the functions involved. In the descriptions corresponding to the flowcharts and block diagrams in the accompanying drawings, the operations or steps corresponding to different boxes may also occur in an order different from that disclosed in the description, and sometimes there is no specific order between different operations or steps. For example, two consecutive operations or steps may actually be executed substantially in parallel, and they may sometimes be executed in the opposite order, which may depend on the functions involved.

Claims

1. A spinning solution for tea polyphenol antibacterial nanofiber membrane, characterized in that: include: High molecular weight polymer, tea polyphenol / β-cyclodextrin inclusion compound and solvent; Among them, according to the mass percentage, in the spinning solution, the high molecular polymer accounts for 8wt% to 15wt%, the tea polyphenol / β-cyclodextrin inclusion complex accounts for 0.5wt% to 8wt%, and the balance is the solvent.

2. The spinning solution according to claim 1, characterized in that The high molecular polymer includes one or more of polyacrylonitrile, polylactic acid, polyvinylidene fluoride, polyether sulfone, polyurethane and polyvinylidene fluoride.

3. The spinning solution according to claim 2, characterized in that When the high molecular polymer includes one or more of polyacrylonitrile, polyethersulfone, polyurethane, and polyvinylidene fluoride, the solvent is N,N-dimethylformamide or N,N-dimethylacetamide; or When the high molecular polymer includes polylactic acid (PLA) and / or polygalactone, the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide.

4. The spinning solution according to claim 3, characterized in that When the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide, the mixing ratio of dichloromethane to N,N-dimethylformamide is in the range of 6:4 to 8:

2.

5. A method for preparing a spinning solution for tea polyphenol antibacterial nanofiber membrane, characterized in that: include: preparing tea polyphenols / β-cyclodextrin inclusion complex; The high molecular polymer and tea polyphenol / β-cyclodextrin inclusion compound are dissolved in a solvent and stirred at a preset temperature until they are completely dissolved to obtain a spinning solution.

6. The preparation method according to claim 5, characterized in that: When N,N-dimethylformamide is used as the solvent alone, the preset temperature ranges from 25°C to 70°C; or, When N,N-dimethylacetamide is used as the solvent alone, the preset temperature ranges from 25°C to 75°C; or, When the solvent is a mixed solvent of dichloromethane and N,N-dimethylformamide, the preset temperature ranges from 25°C to 30°C.

7. The preparation method according to claim 5 or 6, characterized in that: The steps of preparing the tea polyphenol / β-cyclodextrin inclusion compound include: Dissolving β-cyclodextrin in a mixed solution of ultrapure water and anhydrous ethanol at 40° C. to 80° C., and stirring until the β-cyclodextrin is completely dissolved to obtain a β-cyclodextrin mother solution; Dissolve tea polyphenols in anhydrous ethanol at room temperature, and stir until the tea polyphenols are completely dissolved to obtain a tea polyphenol solution; Among them, the ratio of β-cyclodextrin to tea polyphenols is 1:0.5 to 1:6; The β-cyclodextrin mother solution is cooled to a first set temperature and kept at a constant temperature, and under continuous stirring, the tea polyphenol solution is dropped into the β-cyclodextrin mother solution to obtain a mixed solution; The mixed solution is placed in darkness and continuously stirred at a second set temperature at 200 r / min to 600 r / min for a first preset time; placing the mixed solution at a third set temperature and leaving it to stand for a second preset time; After standing, the mixture was filtered, washed and dried to obtain a tea polyphenol / β-cyclodextrin inclusion complex.

8. A method for preparing tea polyphenols antibacterial nanofiber membrane, characterized in that: Applied to an electrospinning device, the electrospinning device comprises a liquid supply part and a receiving roller, the liquid supply part is used to store the spinning solution as claimed in any one of claims 1 to 4, and the receiving roller is used to set a receiving substrate, and the preparation method comprises: According to the spinning solution, the receiving distance, spinning voltage and liquid supply speed are determined; Controlling the distance between the liquid outlet of the liquid supply component and the receiving substrate to the receiving distance; Control the receiving roller to run at a preset speed; and The operation of the electrospinning device is controlled according to the spinning voltage and the liquid supply speed.

9. The preparation method according to claim 8, characterized in that: The preset distance ranges from 10 cm to 20 cm; and / or, The spinning voltage ranges from 10 kV to 25 kV; and / or, The liquid supply rate ranges from 0.5 ml / h to 2 ml / h; and / or, The preset speed ranges from 200 rpm to 400 rpm.

10. The preparation method according to claim 9, characterized in that: According to the spinning solution, the receiving distance, spinning voltage and liquid supply speed are determined including: When the spinning solution includes polyacrylonitrile, the preset distance is in the range of 10 cm to 20 cm; and / or the spinning voltage is in the range of 15 kV to 25 kV; and / or the liquid supply rate is in the range of 0.8 ml / h to 1.5 ml / h; When the spinning solution includes polylactic acid, the preset distance ranges from 13 cm to 17 cm; and / or the spinning voltage ranges from 12 kV to 18 kV; and / or the liquid supply rate ranges from 0.6 ml / h to 0.8 ml / h.

11. The preparation method according to any one of claims 8 to 10, characterized in that: Control the operation of the electrospinning device, and after spinning is completed, it also includes: The spun nanofiber membrane is placed in an oven at 60°C to 120°C for 10 to 15 hours.

12. A method for preparing a tampon, characterized in that: Applied to a carding machine, the carding machine is provided with an electrostatic spinning device, the electrostatic spinning device comprises a liquid supply part, the liquid supply part is used to store the spinning solution as described in any one of claims 1 to 4, and the preparation method comprises: Adjust the distance between the liquid outlet of the liquid supply part and the receiving cotton mesh to 15 cm to 35 cm; The electrospinning device is controlled to perform spinning according to a propulsion speed of the spinning solution of 30 mL / h to 60 mL / h and an applied voltage of 30 kV to 65 kV.

13. A tea polyphenol antibacterial nanofiber membrane, characterized in that: include: The antibacterial nanofiber membrane of tea polyphenols is prepared by the preparation method of any one of claims 8 to 11.

14. A tampon, characterized in that: include: The sliver is prepared by the method for preparing the sliver as claimed in claim 12.

15. A yarn, characterized in that: include: The sliver as claimed in claim 14 is obtained by spinning through a spinning machine.

Citation Information

Cited By

  • Composite nano-filtration material and preparation method thereof

    CN119455523A

  • Natural antibacterial regenerated fiber medical textile fabric and preparation method thereof

    CN120158873A

  • Preparation process of deodorization electrostatic spinning solution and method for producing deodorization yarn

    CN120330898A

  • Zedoary turmeric oil nanofiber membrane, preparation method and application thereof, and cotton sliver containing zedoary turmeric oil

    CN121588071A