Stamping die for alloy sleeve of aircraft landing gear
Through the assembled mold structure and auxiliary maintenance mechanism, the problem of traditional mold wear due to cold mold forming is solved, efficient processing and low-cost maintenance of the aircraft landing gear alloy sleeve, and stamping and punching operations are completed simultaneously.
Patent Information
- Application Number
- CN202411401121.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-09
- Publication Date
- 2024-11-05
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The stamping mold of the landing gear alloy sleeve of the traditional aircraft is formed by continuous temperature loss and hardening, resulting in extrusion and wear of the inner wall of the mold, and frequent stamping leads to changes in the inner dimensions of the mold, which increases processing time and maintenance costs.
A assembly mold structure is designed, using an upper die stamping head to stamp and shape and punch the blank, and the auxiliary maintenance mechanism and the auxiliary stamping mechanism can be used to achieve rapid material withdrawal and maintenance of the mold, and the inner sleeve structure can be replaced and reduced. Maintenance cost.
It improves the processing efficiency of the alloy sleeve, reduces mold loss, reduces maintenance costs, and realizes the synchronous progress of stamping and punching.
Smart Images

Figure CN118893134A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of stamping dies, in particular to an alloy sleeve stamping die for an aircraft landing gear. Background Art
[0002] As an important safety functional component of the aircraft, the aircraft landing gear is an important support system for the aircraft takeoff, landing, ground taxiing and parking. It is the main load-bearing component of the aircraft. It absorbs and dissipates the impact energy generated by the aircraft and the ground during landing and taxiing, ensuring the safety of the aircraft during ground movement. The alloy sleeve in the landing gear, which serves as a shock-absorbing and pressure-bearing component, is made of titanium alloy or high-strength steel. Due to the high strength of the casting material, it requires a specific mold for processing.
[0003] After heat treatment, the alloy sleeve in the landing gear of traditional aircraft needs to be quickly transferred to the cold mold for stamping. Traditional stamping requires multiple preheating and stamping of the blank until it is formed. The workpiece must be stamped in the cold mold and the cold mold must cooperate to maintain the pressure of the stamped blank until the workpiece cools naturally. However, as the workpiece cools together with the mold, the continuous temperature loss and hardening process will cause extrusion wear on the inner wall of the traditional mold. Frequent stamping will cause a certain change in the size of the inner mold.
[0004] In view of this, a stamping die for an alloy sleeve of an aircraft landing gear is designed to solve the above problems. Summary of the invention
[0005] The present invention aims to solve one of the technical problems existing in the prior art or related technology.
[0006] To this end, the technical solution adopted in the present invention is: A stamping die for an alloy sleeve of an aircraft landing gear, comprising a carrier mechanism and an upper die punch head arranged in the carrier mechanism, an auxiliary maintenance mechanism installed in the carrier mechanism and an auxiliary stamping mechanism arranged on the auxiliary maintenance mechanism; the carrier mechanism is used to provide a stable support platform for the assembled die; the upper die punch head is used to provide stamping and shaping force for the alloy sleeve blank, and to perform punching operations on the workpiece after cold die forming; the auxiliary maintenance mechanism comprises a horizontally placed load-bearing outer frame, a slide fixedly mounted on the load-bearing outer frame, and a material stripping assembly arranged in the middle of the top surface of the slide; the auxiliary stamping mechanism comprises two protective traction members arranged in the load-bearing outer frame and symmetrically distributed, a main die assembly and a secondary die assembly arranged in the two protective traction members and bearing pressure on the top of the slide.
[0007] In a preferred example, the present invention can be further configured as follows: two symmetrically distributed slide grooves are provided inside the slide, four limit transverse grooves are provided inside the slide, and a hollow concave hole is provided in the middle of the slide; The material stripping assembly comprises a mother tube fixedly mounted on the top of the slide, a sub-rod movably mounted inside the mother tube, an auxiliary pressure ring mounted on the top of the sub-rod, and a return spring arranged outside the mother tube and the sub-rod after assembly; The bottom end of the return spring is pressed on the slide table, and the top end of the return spring is pressed on the bottom of the auxiliary pressure ring.
[0008] In a preferred example, the present invention can be further configured as follows: the main mold assembly includes a first mold, a main pre-installation hole is opened on the inner side of the first mold, and a first inner sleeve is arranged in the main pre-installation hole, and two first studs are installed at the bottom of the first inner sleeve; The secondary mold assembly includes a second mold, a secondary pre-installation hole is opened on the inner side of the second mold, and a second inner sleeve is arranged in the secondary pre-installation hole, and two second studs are installed at the bottom of the second inner sleeve; The first stud and the second stud are both provided with locking nuts.
[0009] In a preferred example, the present invention can be further configured as follows: the carrier mechanism includes four feet placed on the ground, a suspension mounted on the four feet, and two beams mounted in two adjacent feet; A discharge hole for withdrawing materials is provided in the middle of the suspension; A supporting frame plate is arranged outside two adjacent groups of beams, and the upper die punching head is movably installed in a notch on the top of the supporting frame plate.
[0010] In a preferred example, the present invention can be further configured as follows: the auxiliary maintenance mechanism also includes a hydraulic component installed in the load-bearing external frame, a chuck is installed at the top of the hydraulic sub-rod in the hydraulic component, and two force arms are movably installed in the grooves at both ends of the chuck.
[0011] In a preferred example, the present invention can be further configured as follows: the load-bearing outer frame is composed of a U-shaped support plate and two end plates installed on the inner wall of the U-shaped support plate, and limiting slots are provided at both ends of the U-shaped support plate; The protective traction member is composed of an L-shaped pull rod and a U-shaped clamp frame, and a circular gasket is installed on the outer end of the L-shaped pull rod, and the circular gasket is pressed on the top of the limiting groove.
[0012] In a preferred example, the present invention can be further configured as follows: the auxiliary punching mechanism further includes two sliders and four partitions; One of the sliders is fixedly mounted on the bottom of the first mold, and the other slider is fixedly mounted on the bottom of the second mold; Two of the baffles are mounted on the first mold, and the other two baffles are mounted on the second mold; An inclined groove is provided inside the partition.
[0013] In a preferred example, the present invention can be further configured as follows: the punch assist mechanism further includes two position control baffles, the circular ends of the position control baffles are clamped on the L-shaped pull rod, and the circular ends are fixed to the L-shaped pull rod by bolts; The inclined surface of the position control baffle is adapted to fit in the inclined groove.
[0014] In a preferred example, the present invention can be further configured as follows: the punching assistance mechanism further includes two limit rods and two tension springs; The inner end of the limiting rod is provided with a screw hole; The slider is provided with an insert hole, and the inner end of the limit rod is adapted to penetrate into the insert hole; One end of the tension spring is connected to the slider, and the other end of the tension spring is connected to a cushion block.
[0015] In a preferred example, the present invention can be further configured as follows: the bottoms of the inner cavities of the first inner sleeve and the second inner sleeve are both provided with semicircular annular grooves, and the auxiliary pressure ring is adapted to fit in the two semicircular annular grooves.
[0016] By adopting the above technical solution, the beneficial effects achieved by the present invention are: 1. The present invention arranges the lower die of the traditional integral structure into a multi-die structure of an assembled structure. After the upper die punch extrude the blank, the blank is stamped and shaped in the cold die state. At the same time, the punching end at the bottom of the upper die punch can punch the bottom of the blank, so that the blank can be stamped and punched simultaneously in the cold die, thereby improving the processing efficiency.
[0017] 2. The present invention movably assembles two assembled molds on a slide, and sets two symmetrically distributed protective traction parts on the outside of the two molds. The two control baffles set on the two protective traction parts can control the opening and closing distance of the two molds. At this time, the device can quickly return the material after the alloy sleeve is cold molded, and the mold cavity in the exposed state can also facilitate the workers' quick maintenance.
[0018] 3. The present invention arranges two inner sleeves of the same structure in the inner cavities of the two molds. When the two inner sleeves are closed, the blank can be stamped and formed in the inner cavities of the two inner sleeves after closing under the auxiliary pressure-bearing action of the auxiliary pressure ring (393). The two inner sleeves are replaceable structures, thereby reducing the above-mentioned maintenance cost without directly damaging the two molds. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a schematic diagram of the present invention when used; Figure 2 It is a bottom view schematic diagram of the present invention; Figure 3 is a schematic diagram of the carrier mechanism of the present invention; Figure 4 is a schematic diagram of the auxiliary maintenance mechanism of the present invention; Figure 5 It is a schematic diagram of the material stripping assembly of the present invention; Figure 6 It is a schematic diagram of the punching auxiliary mechanism of the present invention; Figure 7 For the present invention Figure 6 Explosion diagram of Figure 8 It is a schematic diagram of the main mold assembly and the auxiliary mold assembly of the present invention.
[0020] Reference numerals: 100, carrier mechanism; 110, footrest; 120, suspension; 130, beam; 140, support frame; 150, discharge hole; 200, upper die punch head; 300, auxiliary maintenance mechanism; 310, load-bearing outer frame; 320, hydraulic parts; 330, chuck; 340, lever arm; 350, slide; 360, cushion block; 370, slide groove; 380, limit horizontal groove; 390, material withdrawal assembly; 391, mother tube; 392, sub-rod; 393, auxiliary pressure ring; 394, reset spring; 400, auxiliary stamping mechanism; 410, protective traction member; 420, control baffle; 430, main mold assembly; 431, first mold; 432, first inner sleeve; 433, first stud; 440, sub-mold assembly; 441, second mold; 442, second inner sleeve; 443, second stud; 450, slider; 460, partition; 470, limit rod; 480, tension spring. DETAILED DESCRIPTION
[0021] To make the purpose, technical solution and advantages of the present invention more clear, the present invention is further described in detail below in combination with specific implementations and with reference to the accompanying drawings. It should be noted that the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict.
[0022] It is to be understood that these descriptions are exemplary only and are not intended to limit the scope of the invention.
[0023] An alloy sleeve stamping die for an aircraft landing gear provided by some embodiments of the present invention will be described below in conjunction with the accompanying drawings. Embodiment 1:
[0024] Combination Figure 1-Figure 8As shown, the present invention provides an alloy sleeve stamping die for an aircraft landing gear, comprising a carrier mechanism 100 and an upper die punch head 200 arranged in the carrier mechanism 100, an auxiliary maintenance mechanism 300 installed in the carrier mechanism 100, and an auxiliary stamping mechanism 400 arranged on the auxiliary maintenance mechanism 300, the carrier mechanism 100 is used to provide a stable support platform for the assembled die, the upper die punch head 200 is used to provide stamping shaping force for the alloy sleeve blank, and to perform punching operations on the workpiece after cold die forming.
[0025] The carrier mechanism 100 includes four feet 110 placed on the ground, a suspension 120 installed on the four feet 110, and two beams 130 installed in two adjacent feet 110; A discharge hole 150 for withdrawing materials is provided in the middle of the suspension 120; A support frame plate 140 is disposed outside two adjacent groups of beams 130, and an upper die punch 200 is movably installed in a notch on the top of the support frame plate 140; The auxiliary maintenance mechanism 300 includes a horizontal load-bearing outer frame 310, a slide 350 fixedly mounted on the load-bearing outer frame 310, a material stripping assembly 390 arranged in the middle of the top surface of the slide 350, and a hydraulic component 320 installed in the load-bearing outer frame 310. A chuck 330 is installed at the top of the hydraulic sub-rod in the hydraulic component 320, and two force arms 340 are movably installed in the grooves at both ends of the chuck 330. The load-bearing outer frame 310 is composed of a U-shaped support plate and two end plates installed on the inner wall of the U-shaped support plate, and limiting grooves are provided at both ends of the U-shaped support plate; The protective traction member 410 is composed of an L-shaped pull rod and a U-shaped clamp frame, and a circular gasket is installed at the outer end of the L-shaped pull rod, and the circular gasket is pressed on the top of the limiting groove; The auxiliary stamping mechanism 400 includes two limit rods 470 and two tension springs 480, two protective traction members 410 arranged in the load-bearing outer frame 310 and symmetrically distributed, and a main mold assembly 430 and a secondary mold assembly 440 arranged in the two protective traction members 410 and bearing pressure on the top of the slide 350; A screw hole is provided at the inner end of the limiting rod 470; The main mold assembly 430 includes a first mold 431 , a main pre-installation hole is formed on the inner side of the first mold 431 , and a first inner sleeve 432 is disposed in the main pre-installation hole. Two first studs 433 are installed at the bottom of the first inner sleeve 432 ; The secondary mold assembly 440 includes a second mold 441, a secondary pre-installation hole is opened on the inner side of the second mold 441, and a second inner sleeve 442 is arranged in the secondary pre-installation hole, and two second studs 443 are installed at the bottom of the second inner sleeve 442; Locking nuts are disposed on the first stud 433 and the second stud 443 .
[0026] Since the aircraft landing gear is to improve the pavement floatation of large transport aircraft, and the landing gear structure mostly adopts a multi-wheel and multi-pillar structure layout, in order to improve the compressive strength and improve the stability of the aircraft after landing, the various components of the landing gear are mainly stamped with titanium alloy and high-strength steel to form a seamless structure. Among them, the alloy sleeve is an important component of the straight tube in the landing gear assembly. After calcination in a heat treatment furnace, it needs to be quickly transferred to a cold mold for frequent processing. However, the traditional cold mold is an integral structure. When the heat-treated blank is placed inside the cold mold for penguin cup stamping, the alloy sleeve after stamping to pressure-holding forming will cause certain wear on the traditional mold inner mold. In severe cases, it will cause the subsequent specifications of the alloy sleeve to change after stamping. The stamped alloy sleeve needs to be transferred to the next link for punching, which not only increases the time consumption of the alloy sleeve processing, but also increases the maintenance cost after the mold is damaged.
[0027] The device is configured by setting the traditional lower mold as an assembled structure, and symmetrically disposing the first inner sleeve 432 and the second inner sleeve 442 on the inner side of the assembled first mold 431 and the second mold 441. When the first inner sleeve 432 and the second inner sleeve 442 are closed, the blank is placed in the first inner sleeve 432 and the second inner sleeve 442 and can be stamped and punched by the upper mold punch head 200. At this time, after the first inner sleeve 432 and the second inner sleeve 442 in the assembled structure are opened and closed, the stamped alloy sleeve can be quickly exposed. Once the inner walls of the first inner sleeve 432 and the second inner sleeve 442 are worn due to cold pressing of the workpiece, the worker can take out the first inner sleeve 432 and the second inner sleeve 442 and perform maintenance. At this time, the device can reduce mold damage and increase maintenance costs while performing stamping and punching simultaneously, thereby improving the efficiency of alloy sleeve stamping. Embodiment 2:
[0028] Combination Figure 4-Figure 8 As shown, on the basis of Example 1, two symmetrically distributed slide grooves 370 are opened inside the slide 350, four limiting transverse grooves 380 are opened inside the slide 350, and a hollow concave hole is opened in the middle of the slide 350; The material stripping assembly 390 includes a mother tube 391 fixedly mounted on the top of the slide 350, a sub-rod 392 movably mounted inside the mother tube 391, an auxiliary pressure ring 393 mounted on the top of the sub-rod 392, and a return spring 394 arranged outside the mother tube 391 and the sub-rod 392 after the combination; The bottom end of the return spring 394 is pressed on the slide 350, and the top end of the return spring 394 is pressed on the bottom of the auxiliary pressure ring 393; The bottoms of the inner cavities of the first inner sleeve 432 and the second inner sleeve 442 are both provided with semicircular annular grooves, and the auxiliary pressure ring 393 is adapted to fit in the two semicircular annular grooves.
[0029] By using symmetrically distributed vertical grooves opened on the inner walls of the first mold 431 and the second mold 441, and at this time, the combined sub-rod 392 and the mother tube 391 can provide a stable supporting force for the auxiliary pressure ring 393 at the top of the slide 350. When the first inner sleeve 432 and the second inner sleeve 442 are closed, the auxiliary pressure ring 393 elastically supported by two return springs 394 can slowly deliver the blank carried on its top downward until the blank is placed at the bottom of the inner cavity of the first inner sleeve 432 and the second inner sleeve 442. As the auxiliary pressure ring 393 docks with the semicircular annular grooves at the bottom of the inner cavity of the first inner sleeve 432 and the second inner sleeve 442, the pressurized blank can be accurately and stably stamped and punched by the upper die punch 200. After the above-mentioned blank is made, the cold-pressed alloy sleeve can be quickly removed from the gap exposed by the expanded first inner sleeve 432 and the second inner sleeve 442. At the same time, the complete exposure of the inner mold can also facilitate workers to quickly clean the mold cavity to increase the service life of the mold. Embodiment three:
[0030] Combination Figure 3-Figure 8 As shown, based on the embodiment 1, the punching auxiliary mechanism 400 further includes two position control baffles 420, two sliders 450 and four partitions 460; The circular end of the position control baffle 420 is clamped on the L-shaped pull rod, and the circular end is fixed on the L-shaped pull rod by bolts; The inclined surface of the position control baffle 420 is adapted to fit in the inclined groove; One of the sliders 450 is fixedly mounted on the bottom of the first mold 431 , and the other slider 450 is fixedly mounted on the bottom of the second mold 441 ; Two of the partitions 460 are mounted on the first mold 431, and the other two partitions 460 are mounted on the second mold 441; The partition 460 has an inclined groove formed inside; The slider 450 has an insert hole formed inside, and the inner end of the limit rod 470 is adapted to penetrate into the insert hole; One end of the tension spring 480 is connected to the slider 450 , and the other end of the tension spring 480 is connected to the cushion block 360 .
[0031] When the hydraulic sub-rod in the hydraulic part 320 is lifted upward, the pushed clamp 330 can push the two force arms 340 to extend outward, and the two protective traction parts 410 can move outward along the two end plates in the load-bearing outer frame 310. At the same time, the control baffle 420 moving outward along the protective traction part 410 can release the pressure on the partition 460. At this time, the tension spring 480 in the stretched state will pull the relaxed slider 450 to move outward. At this time, the main mold assembly 430 and the auxiliary mold assembly 440 can expand at equal intervals along the top of the slide 350. At this time, the waste material punched out of the blank can fall from the concave hole in the middle of the slide 350, and the alloy sleeve after pressure-holding molding can be quickly withdrawn; After the above-mentioned forming alloy sleeve is withdrawn, the wear degree of the inner walls of the first inner sleeve 432 and the second inner sleeve 442 is regularly checked. When the inner walls of the first inner sleeve 432 and the second inner sleeve 442 are excessively worn, they can be directly replaced, thereby reducing the pressure of the forming workpiece on the mold body and reducing the maintenance cost of the mold body.
[0032] The working principle and use process of the present invention are as follows: Since the main components of the aircraft landing gear are made of titanium alloy or high-strength steel, and since the melting points of the above two materials are relatively high, the titanium alloy and the high-strength steel are heated in a heating furnace to exceed the austenitizing temperature for a period of time until the internal structures of the titanium alloy and the high-strength steel are uniformly austenitized, and then the heat-treated titanium alloy and high-strength steel are taken out and placed in a cold pressing mold for thermoplastic forming.
[0033] In the above steps, after the blank is placed in the inner cavities of the first inner sleeve 432 and the second inner sleeve 442 after the closure is formed, the blank will be pressurized by the auxiliary pressure ring 393. At this time, the blank will press the auxiliary pressure ring 393 down to the bottom of the inner cavities of the first inner sleeve 432 and the second inner sleeve 442 under the action of gravity. After the external kinetic energy gives the upper die punch 200 a downward punching force, it will fall down along the vertical hole at the top of the support frame plate 140. The punching end at the bottom of the upper die punch 200 can punch a hole in the center of the heat-treated alloy sleeve blank in the inner cavities of the first inner sleeve 432 and the second inner sleeve 442. 00 is continuously pressed downward, and the blank with a central punch hole is squeezed and shaped in the inner cavities of the first inner sleeve 432 and the second inner sleeve 442. At this time, along the outer wall of the punching end at the bottom of the upper die punch head 200, the blank is effectively shaped in the cold die. After the alloy sleeve has undergone the above-mentioned initial tension and has been formed in the cold die, the punching end at the bottom of the upper die punch head 200 needs to be continuously stored in the first inner sleeve 432 and the second inner sleeve 442 until the alloy sleeve is pressurized after forming. During the pressure-holding process, the alloy sleeve is cooled down, and finally the upper die punch head 200 can be taken out.
[0034] When the alloy sleeve is cold formed and the upper die punch 200 is withdrawn, the hydraulic component 320 is then operated. At this time, the hydraulic sub-rod in the hydraulic component 320 will cooperate with the chuck 330 to simultaneously push the two force arms 340 to lift upward at the same speed. At this time, the two force arms 340 will push the two protective traction members 410 to expand outward. When the two protective traction members 410 are completely withdrawn from the outside of the first mold 431 and the second mold 441, under the traction of the two tension springs 480, the first mold 431 and the second mold 441 will extend outward along the top of the slide 350. At this time, the cold-formed alloy sleeve workpiece can be exposed from the inner cavity of the first inner sleeve 432 and the second inner sleeve 442. At this time, the mold can reduce the damage of its main workpiece due to cold forming and extrusion, and can also improve the workers' maintenance efficiency. At the same time, the device can combine punching and extrusion shaping to reduce the steps of drilling required for subsequent forming of the alloy sleeve.
[0035] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. An alloy sleeve stamping die for an aircraft landing gear, comprising a carrier mechanism (100) and an upper die stamping head (200) arranged in the carrier mechanism (100), characterized in that: Also included is an auxiliary inspection mechanism (300) installed in the carrier mechanism (100) and an auxiliary stamping mechanism (400) arranged on the auxiliary inspection mechanism (300); The carrier mechanism (100) is used to provide a stable supporting platform for the assembled mould; The upper die punch head (200) is used to provide a punching and shaping force for the alloy sleeve blank and to perform a punching operation on the workpiece after cold die forming; The auxiliary maintenance mechanism (300) comprises a horizontally placed load-bearing outer frame (310), a slide table (350) fixedly mounted on the load-bearing outer frame (310), and a material stripping assembly (390) disposed in the middle of the top surface of the slide table (350); The auxiliary punching mechanism (400) comprises two protective traction members (410) arranged in a load-bearing outer frame (310) and symmetrically distributed, and a main mold assembly (430) and a secondary mold assembly (440) arranged in the two protective traction members (410) and bearing pressure on the top of the slide table (350).
2. The alloy sleeve stamping die for aircraft landing gear according to claim 1, characterized in that: Two symmetrically distributed slide grooves (370) are provided inside the slide table (350), four limit transverse grooves (380) are provided inside the slide table (350), and a hollow concave hole is provided in the middle of the slide table (350); The material-removing assembly (390) comprises a mother tube (391) fixedly mounted on the top of the slide (350), a sub-rod (392) movably mounted inside the mother tube (391), an auxiliary pressure ring (393) mounted on the top of the sub-rod (392), and a return spring (394) arranged outside the mother tube (391) and the sub-rod (392) after assembly; The bottom end of the return spring (394) is pressed on the slide table (350), and the top end of the return spring (394) is pressed on the bottom of the auxiliary pressure ring (393).
3. The alloy sleeve stamping die for aircraft landing gear according to claim 1, characterized in that: The main mold assembly (430) comprises a first mold (431), a main pre-installation hole is formed on the inner side of the first mold (431), a first inner sleeve (432) is arranged in the main pre-installation hole, and two first studs (433) are installed at the bottom of the first inner sleeve (432); The secondary mold assembly (440) comprises a second mold (441), a secondary pre-installation hole is formed on the inner side of the second mold (441), a second inner sleeve (442) is arranged in the secondary pre-installation hole, and two second studs (443) are installed at the bottom of the second inner sleeve (442); The first stud (433) and the second stud (443) are both provided with locking nuts.
4. The alloy sleeve stamping die for aircraft landing gear according to claim 1, characterized in that: The carrier mechanism (100) comprises four pads (110) placed on the ground, a suspension (120) installed on the four pads (110), and two beams (130) installed in two adjacent pads (110); A material discharge hole (150) for discharging materials is provided in the middle of the suspension (120); A support frame plate (140) is arranged outside two adjacent groups of beams (130), and the upper die punch head (200) is movably mounted in a notch on the top of the support frame plate (140).
5. The alloy sleeve stamping die for aircraft landing gear according to claim 1, characterized in that: The auxiliary maintenance mechanism (300) further comprises a hydraulic component (320) installed in the load-bearing outer frame (310), a chuck (330) being installed at the top end of the hydraulic sub-rod in the hydraulic component (320), and two force arms (340) being movably installed in grooves at both ends of the chuck (330).
6. The alloy sleeve stamping die for aircraft landing gear according to claim 1, characterized in that: The load-bearing outer frame (310) is composed of a U-shaped support plate and two end plates installed on the inner wall of the U-shaped support plate, and limiting grooves are provided at both ends of the U-shaped support plate; The protective traction member (410) is composed of an L-shaped pull rod and a U-shaped clamp frame, and a circular gasket is installed on the outer end of the L-shaped pull rod, and the circular gasket is pressed on the top of the limiting groove.
7. The alloy sleeve stamping die for aircraft landing gear according to claim 1, characterized in that: The punch assisting mechanism (400) further comprises two sliders (450) and four partitions (460); One of the sliders (450) is fixedly mounted on the bottom of the first mold (431), and the other slider (450) is fixedly mounted on the bottom of the second mold (441); Two of the partitions (460) are mounted on the first mold (431), and the other two partitions (460) are mounted on the second mold (441); An inclined groove is provided inside the partition (460).
8. The alloy sleeve stamping die for aircraft landing gear according to claim 1, characterized in that: The punch assist mechanism (400) further comprises two position control baffles (420), wherein the circular ends of the position control baffles (420) are clamped on the L-shaped pull rod, and the circular ends are fixed on the L-shaped pull rod by bolts; The inclined surface of the position control baffle (420) is adapted to fit in the inclined groove.
9. The alloy sleeve stamping die for aircraft landing gear according to claim 7, characterized in that: The punch assisting mechanism (400) further comprises two limit rods (470) and two tension springs (480); A screw hole is formed at the inner end of the limiting rod (470); The sliding block (450) is provided with an insertion hole inside, and the inner end of the limiting rod (470) is adapted to penetrate into the insertion hole; One end of the tension spring (480) is connected to the slider (450), and the other end of the tension spring (480) is connected to the cushion block (360).
10. The alloy sleeve stamping die for aircraft landing gear according to claim 3, characterized in that: The bottoms of the inner cavities of the first inner sleeve (432) and the second inner sleeve (442) are both provided with semicircular annular grooves, and the auxiliary pressure ring (393) is adapted to fit in the two semicircular annular grooves.
Citation Information
Patent Citations
SVertical stamping rounding mould with four sleeve petals and availability for automatic demoulding
CN102974700A
Split type sheet metal part stamping die
CN210098635U
Sheet metal stamping die with replaceable punch
CN214556680U
Split type composite material forming mold structure
CN218256998U
Punching and punching double-station composite die
CN221312137U
Cited By
High-efficiency stretching die for lithium battery shell
CN119216482A