Concrete column circumferential reinforcing structure and reinforcing method
By using shape memory alloy plates on the outside of concrete columns for pre-stretching and thermal excitation to generate prestress, the problems of complex construction and damage to the original structure in the repair of cracks in concrete columns are solved, and an effective reinforcement effect is achieved.
Patent Information
- Application Number
- CN202410880041.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-02
- Publication Date
- 2024-11-05
AI Technical Summary
Existing methods for repairing cracks in concrete columns have problems such as complex construction, high cost, and easy damage to the original structure. In addition, traditional reinforcement methods affect the usable area of the building.
Shape memory alloy plates are used to reinforce concrete columns in the circumferential direction. Prestress is generated through pre-stretching and thermal excitation. The shape memory alloy plates are used to wrap and reinforce areas that have cracked or are at risk of cracking, and are fixed by anchors and pads.
It effectively inhibits the initiation and propagation of cracks, improves the load-bearing capacity and ductility of concrete columns, adapts to concrete columns of different shapes, requires no complex construction equipment, and does not damage the original structure.
Smart Images

Figure CN118895879A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of civil engineering reinforcement, and in particular to a concrete column annular reinforcement structure and a reinforcement method. Background Art
[0002] Concrete columns are widely used vertical load-bearing components that play a supporting role. With the increase of service life, a large number of buildings have gradually developed cracks due to various factors such as structural aging, natural disasters, and human damage, which seriously affects their safety. In order to avoid the extremely high cost of demolition, reinforcing the existing cracked structures has become the current mainstream method.
[0003] Traditional repair methods for concrete column cracks include increasing the cross-section, external reinforcement, and replacement concrete reinforcement. However, these technologies often bring new problems. For example, increasing the cross-section will reduce the usable area of the building and require a large amount of construction. The external reinforcement method does not require wet work and is easy to operate, but it has problems with durability and high maintenance costs. The replacement concrete method is prone to damage the original structure during operation and creates a new source of damage.
[0004] Shape memory alloy refers to an alloy that deforms under external force within a certain temperature range and can restore its original shape under heating conditions. This shape-recoverable property is called the shape memory effect. If the deformation of the shape memory alloy is restricted during the heating process, a very considerable recovery stress can be generated. Introducing this recovery stress into the concrete structure can serve as prestress for structural reinforcement.
[0005] It is now necessary to design a concrete column circumferential reinforcement structure and reinforcement method so as to apply shape memory alloys to the repair work of concrete columns. Summary of the invention
[0006] In view of the above problems existing in the prior art, the present invention is proposed.
[0007] Therefore, an object of the present invention is to provide a concrete column annular reinforcement structure.
[0008] In order to solve the above technical problems, the present invention provides the following technical solutions: a concrete column annular reinforcement structure, comprising:
[0009] A main body structure, comprising a concrete column and a surrounding component adapted to be installed on the outside of the concrete column;
[0010] The surrounding component includes a shape memory alloy plate arranged outside the concrete column, a pad arranged outside the shape memory alloy plate, and an anchor adapted to be installed inside the shape memory alloy plate and the pad.
[0011] As a preferred solution of the circumferential reinforcement structure of the concrete column of the present invention, the shape memory alloy plate is made of iron-based shape memory alloy plate, and the cushion block is made of glass fiber reinforced material.
[0012] As a preferred solution of the circumferential reinforcement structure of concrete columns of the present invention, the shape memory alloy plate generates prestrain by pre-stretching, and the shape memory alloy plate generates prestress by thermal excitation.
[0013] In order to solve the above technical problems, the present invention also provides the following technical solutions: a reinforcement method, comprising the above concrete column annular reinforcement structure, and:
[0014] The area on the surface of the concrete column that has cracked or is at risk of cracking is named the area to be reinforced. The area to be reinforced and the shape memory metal are pretreated, and the shape of the area to be reinforced is determined. The area to be reinforced is wrapped with the pretreated shape memory metal and thermally excited so that the shape memory metal wraps the concrete column, and the anchoring is completed after cooling.
[0015] As a preferred embodiment of the reinforcement method of the present invention, the surface of the area to be reinforced is decontaminated, polished, and cleaned before reinforcement, and structural adhesive is evenly applied on the surface of the area to be reinforced;
[0016] The shape memory metal is cut out to completely wrap the surface of the area to be reinforced, and the shape memory metal is pre-stretched to make the shape memory metal produce pre-strain.
[0017] As a preferred solution of the reinforcement method of the present invention, the shape of the area to be reinforced is determined as follows:
[0018] If it is cylindrical, the pre-stretched shape memory metal is wrapped around the outside of the area to be reinforced, and the shape memory metal is completely attached to the structural adhesive. Under the adhesion of the structural adhesive, the shape memory metal is initially fixed to the area to be reinforced;
[0019] If it is other shapes, the pre-stretched shape memory metal is wrapped around the outside of the area to be reinforced, and the shape memory metal is made to fit the structural adhesive as much as possible until the shape memory metal is initially fixed in the area to be reinforced.
[0020] As a preferred solution of the reinforcement method of the present invention, different thermal excitation methods are adopted according to the shape of the area to be reinforced, specifically:
[0021] If the area to be reinforced is cylindrical, the shape memory metal is thermally stimulated by a single heating method;
[0022] If the area to be reinforced is in other shapes, the shape memory metal is thermally stimulated by gradually increasing the temperature.
[0023] As a preferred embodiment of the reinforcement method of the present invention, for a cylindrical concrete column in the area to be reinforced, a single heating thermal excitation method is used to make the shape memory metal produce prestress, and under the action of the prestress, the shape memory metal is tightly attached to the concrete column, and after being heated to above 100°C, the structural adhesive softens, thereby losing the fixing effect. After cooling, holes are opened at both ends of the shape memory metal, and the two ends of the shape memory metal are anchored using anchors and pads.
[0024] As a preferred embodiment of the reinforcement method of the present invention, for concrete columns with other shapes of areas to be reinforced, a progressive heating thermal excitation method is adopted. During multiple progressive thermal excitations, the shape memory metal generates prestress, and under the action of the prestress, the shape memory metal will cling to the concrete column, and the temperature of multiple thermal excitations is not lower than 100°C.
[0025] As a preferred embodiment of the reinforcement method of the present invention, for concrete columns with other shapes of areas to be reinforced, after cooling, the excess shape memory metal due to shrinkage and close contact with the concrete column is cut, and a final thermal excitation is performed. After cooling, holes are opened at both ends of the shape memory metal, and the two ends of the shape memory metal are anchored using anchors and pads.
[0026] The beneficial effects of the present invention are as follows: by using shape memory alloy plates to wrap and reinforce areas of concrete columns that have cracked or are at risk of cracking, the stress amplitude at the cracked parts of the structure can be reduced, thereby inhibiting the initiation and expansion of cracks. No complicated construction equipment is required, and the present invention has strong adaptability to conditions where construction space is limited, and has good adaptability to concrete columns of various shapes. In addition, the present invention will not damage the original structure while reinforcing the structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. Among them:
[0028] Figure 1 It is a schematic diagram of the overall structure of the present invention.
[0029] Figure 2 It is a schematic diagram of the gradient heating recovery stress-temperature curve of the present invention.
[0030] Figure 3 It is a schematic diagram of the single temperature rise recovery stress-temperature curve of the present invention. DETAILED DESCRIPTION
[0031] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are described in detail below in conjunction with the accompanying drawings.
[0032] In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.
[0033] Secondly, the term "one embodiment" or "embodiment" as used herein refers to a specific feature, structure, or characteristic that may be included in at least one implementation of the present invention. The term "in one embodiment" that appears in different places in this specification does not necessarily refer to the same embodiment, nor does it refer to a separate or selective embodiment that is mutually exclusive with other embodiments.
[0034] Secondly, the present invention is described in detail with reference to the schematic diagram. When describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional diagrams showing the device structure will not be partially enlarged according to the general scale, and the schematic diagrams are only examples, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.
[0035] Example 1
[0036] Reference Figure 1 , which is the first embodiment of the present invention, provides a concrete column annular reinforcement structure,
[0037] include,
[0038] The main body 100 includes a concrete column 101 and a surrounding component 102 adapted to be installed outside the concrete column 101;
[0039] The surrounding component 102 includes a shape memory alloy plate 102a disposed outside the concrete column 101, a spacer 102b disposed outside the shape memory alloy plate 102a, and an anchor 102c adapted to be installed inside the shape memory alloy plate 102a and the spacer 102b.
[0040] Specifically, the shape memory alloy plate 102a is made of an iron-based shape memory alloy plate, and the pad 102b is made of glass fiber reinforced plastic (GFRP).
[0041] Furthermore, the shape memory alloy plate 102a generates pre-strain through pre-stretching, and the shape memory alloy plate 102a generates pre-stress through thermal excitation.
[0042] Iron-based shape memory alloy has the advantages of low cost, high strength, good plasticity, high elastic modulus, good hot and cold processing performance, etc. It is a new type of structural reinforcement material with great application potential and good development prospects. Therefore, the shape memory alloy plate 102a uses an iron-based shape memory alloy plate.
[0043] By arranging a pre-stretched shape memory alloy plate 102a on the outside of the concrete column 101 and thermally exciting the shape memory alloy plate 102a, the shape memory alloy plate 102a can be contracted inwardly, thereby tightly wrapping the concrete column 101, and the thermally excited shape memory alloy plate 102a is anchored by the pad 102b and the anchor 102c to prevent it from loosening and falling off.
[0044] Active reinforcement of cracked or cracking-risked areas of the concrete column 101 using shape memory alloy plates 102a, pads 102b and anchors 102c can effectively inhibit crack initiation and expansion, reduce stress concentration at the crack tip, improve its uniaxial compressive strength, and thereby improve the bearing capacity and ductility of the component.
[0045] Example 2
[0046] Reference Figure 1 , which is the second embodiment of the present invention, and which is different from the first embodiment in that: a reinforcement method is provided, including a concrete column annular reinforcement structure, and,
[0047] The area on the surface of the concrete column that has cracked or is at risk of cracking is named the area to be reinforced. The area to be reinforced and the shape memory metal are pretreated, and the shape of the area to be reinforced is determined. The area to be reinforced is wrapped with the pretreated shape memory metal and thermally excited so that the shape memory metal wraps the concrete column, and the anchoring is completed after cooling.
[0048] Furthermore, the surface of the area to be reinforced is decontaminated, polished, and cleaned before reinforcement, and structural adhesive is evenly applied on the surface of the area to be reinforced;
[0049] The shape memory metal is cut out to completely wrap the surface of the area to be reinforced, and the shape memory metal is pre-stretched to make the shape memory metal produce pre-strain.
[0050] Furthermore, the shape of the area to be reinforced is determined as follows:
[0051] If it is cylindrical, the pre-stretched shape memory metal is wrapped around the outside of the area to be reinforced, and the shape memory metal is completely attached to the structural adhesive. Under the adhesion of the structural adhesive, the shape memory metal is initially fixed to the area to be reinforced;
[0052] If it is other shapes, the pre-stretched shape memory metal is wrapped around the outside of the area to be reinforced, and the shape memory metal is made to fit the structural adhesive as much as possible until the shape memory metal is initially fixed in the area to be reinforced.
[0053] Specifically, different thermal excitation methods are adopted according to the shape of the area to be reinforced, specifically:
[0054] If the area to be reinforced is cylindrical, the shape memory metal is thermally stimulated by a single heating method;
[0055] If the area to be reinforced is in other shapes, the shape memory metal is thermally stimulated by gradually increasing the temperature.
[0056] More specifically, for concrete columns with cylindrical areas to be reinforced, a single heating-up thermal excitation method is used to generate prestress in the shape memory metal. Under the action of the prestress, the shape memory metal clings to the concrete column, and after being heated to above 100°C, the structural adhesive softens and loses its fixing effect. After cooling, holes are opened at both ends of the shape memory metal, and anchors and pads are used to anchor the two ends of the shape memory metal.
[0057] In addition, for concrete columns with other shapes in the area to be reinforced, a progressive heating thermal excitation method is adopted. During the multiple progressive thermal excitation processes, the shape memory metal generates prestress, and under the action of the prestress, the shape memory metal will cling to the concrete column, and the temperature of multiple thermal excitations is not lower than 100°C.
[0058] Among them, for concrete columns with other shapes in the area to be reinforced, after cooling, the excess shape memory metal due to shrinkage and close to the concrete column is cut, and the last thermal excitation is carried out. After cooling, holes are opened at both ends of the shape memory metal, and the two ends of the shape memory metal are anchored using anchors and pads.
[0059] The prestress generated by the shape memory alloy plate 102a through thermal excitation is related to the heating temperature, heating method, and the pre-stretching degree of the shape memory alloy plate 102a. The present invention selects the activation temperature of the shape memory alloy plate 102a according to its "recovery stress-temperature curve".
[0060] Six temperature gradients are set for the heating activation of the shape memory alloy plate 102a, which are 150℃, 200℃, 250℃, 300℃, 350℃ and 400℃ respectively. This paper adopts two heating activation modes: "pre-stretching unloading-gradient heating-restoring stress" and "pre-stretching unloading-single heating-restoring stress". The gradient heating is to carry out the gradient heating process of 25℃ (room temperature) → 150℃ → 25℃ → 200℃ → 25℃ → 250℃ → 25℃ → 300℃ → 25℃ → 350℃ → 25℃ → 400℃ → 25℃ while keeping the strain constant. The single heating is to carry out single heating activation at 150℃, 200℃, 250℃, 300℃, 350℃ and 400℃ while keeping the strain constant.
[0061] The pre-stretching of the shape memory alloy plate 102a is set to five gradients, namely 2%, 3%, 4%, 6%, and 8%.
[0062] The shape memory alloy plate 102a generates pre-strain through tensioning. The magnitude of the pre-stress is related to the pre-strain level. If the pre-strain is too small, the performance of the shape memory alloy plate 102a cannot be fully exerted; if the pre-strain is too large, α-martensite without shape memory effect will be produced in the shape memory alloy plate 102a.
[0063] The thermal actuation of the shape memory alloy plate 102a is performed by covering the shape memory alloy plate 102a with a ceramic heating sheet and energizing the ceramic heating sheet to a specified temperature.
[0064] The glass transition temperature of commonly used structural adhesives is generally below 100° C. Therefore, when the shape memory alloy plate 102 a is thermally actuated, if the thermal actuation temperature is greater than 100° C., the structural adhesive will soften and lose its fixing effect.
[0065] Therefore, in the above-mentioned gradient heating and single heating, the minimum heating temperature is 150°C, so that when the non-cylindrical area to be reinforced is subjected to gradient heating, it can be ensured that the structural adhesive softens and loses its fixing effect, so as to prevent the adhesion of the structural adhesive from hindering the deformation of the shape memory alloy plate 102a, thereby causing the shape memory alloy plate 102a to be unable to fully fit the non-cylindrical concrete column 101. In addition, through the gradient heating method, the shape memory alloy plate 102a undergoes multiple internal shrinkages with different prestresses at different temperatures, so that it can better fit the surface of the non-cylindrical concrete column 101 during the multiple shrinkage processes.
[0066] In summary, using shape memory alloy plates 102a to wrap and reinforce areas of concrete columns 101 that have cracked or are at risk of cracking can reduce the stress amplitude at the cracked parts of the structure, thereby inhibiting the initiation and expansion of cracks. It does not require complex construction equipment, has strong adaptability to conditions with limited construction space, and has good adaptability to concrete columns 101 of various shapes. In addition, the present invention will not damage the original structure while reinforcing the structure.
[0067] Example 3
[0068] Reference Figure 2 and Figure 3 , which is the third embodiment of the present invention. This embodiment is different from the second embodiment in that it includes a detailed method for selecting the activation temperature of the shape memory alloy plate 102a by using the "recovery stress-temperature curve".
[0069] As attached Figure 2 As shown, it is the "recovery stress-temperature curve" in the gradient heating thermal excitation mode, where the activation temperature is the last heating temperature in the gradient heating.
[0070] As attached Figure 3 As shown, it is the "recovery stress-temperature curve" in the single heating thermal excitation mode, wherein the activation temperature is the direct heating temperature in the single heating.
[0071] Attached Figure 2 and attached Figure 3 The specific parameters are as follows:
[0072] Table 1 Activation recovery stress of iron-based shape memory alloy (Fe-SMA)
[0073]
[0074]
[0075] As shown in the accompanying drawings and tables, in single heating and gradient heating, the recovery stress of the shape memory alloy plate 102a at each pre-stretching degree gradually increases with the increase of activation temperature. When the activation temperature is 400°C and the pre-stretching degree is 8%, the recovery stress of the shape memory alloy plate 102a is the largest.
[0076] However, considering that the concrete column 101 in conventional use can withstand a temperature of 300°C, 400°C cannot be selected, but 300°C should be selected. Figure 2 , Attachment Figure 3 It can be seen from the table that at 300° C., the recovery stress of the shape memory alloy plate 102 a is the largest, and the pre-stretching is 4%.
[0077] In addition, if a heat-insulating layer is provided or a heat-insulating material is coated on the outside of the concrete column 101, the temperature resistance of the concrete column 101 can reach 400°C. At this time, according to the accompanying drawings and tables, an 8% pre-stretched shape memory alloy plate 102a can be preferably used, and an activation temperature of 400°C can be used. If the temperature exceeds 400°C, the concrete column 101 will be damaged, so a higher temperature is no longer used.
[0078] In summary, taking into account the recovery stress of the shape memory alloy plate 102a and the tolerable temperature of the concrete column 101, when no heat insulation treatment is taken for the concrete column 101, a 4% pre-stretched shape memory alloy plate 102a should be preferred, and an activation temperature of 300°C should be adopted; when heat insulation treatment is taken, an 8% pre-stretched shape memory alloy plate 102a can be preferred, and an activation temperature of 400°C can be adopted.
[0079] Importantly, it should be noted that the construction and arrangement of the present application shown in a plurality of different exemplary embodiments are only exemplary. Although only a few embodiments are described in detail in this disclosure, it should be readily understood by those who refer to this disclosure that many modifications are possible (e.g., the size, scale, structure, shape and proportion of various elements, and parameter values (e.g., temperature, pressure, etc.), installation arrangement, use of materials, color, directional changes, etc.) without substantially departing from the novel teachings and advantages of the subject matter described in the application. For example, the element shown as integrally formed can be composed of multiple parts or elements, the position of the element can be inverted or otherwise changed, and the nature or number or position of the discrete element can be changed or changed. Therefore, all such modifications are intended to be included in the scope of the present invention. The order or sequence of any process or method steps can be changed or reordered according to alternative embodiments. In the claims, any "device plus function" clause is intended to cover the structure of performing the function described herein, and is not only structurally equivalent but also equivalent structure. Without departing from the scope of the present invention, other replacements, modifications, changes and omissions can be made in the design, operating conditions and arrangement of the exemplary embodiments. Therefore, the invention is not limited to a specific embodiment, but extends to numerous modifications still falling within the scope of the appended claims.
[0080] Additionally, in order to provide a concise description of exemplary embodiments, all features of an actual embodiment (ie, those features that are not relevant to the best mode presently contemplated for carrying out the invention or those that are not relevant to implementing the invention) may not be described.
[0081] It should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solutions of the present invention may be modified or replaced by equivalents without departing from the spirit and scope of the technical solutions of the present invention, which should all be included in the scope of the claims of the present invention.
Claims
1. A concrete column circumferential reinforcement structure, Features: include, A main body structure (100) comprises a concrete column (101) and a surrounding component (102) adapted to be installed outside the concrete column (101); The surrounding component (102) comprises a shape memory alloy plate (102a) arranged outside the concrete column (101), a pad (102b) arranged outside the shape memory alloy plate (102a), and an anchor (102c) adapted to be installed inside the shape memory alloy plate (102a) and the pad (102b).
2. The concrete column annular reinforcement structure according to claim 1, Features: The shape memory alloy plate (102a) is made of an iron-based shape memory alloy plate, and the cushion block (102b) is made of a glass fiber reinforced material.
3. The concrete column annular reinforcement structure according to claim 2, Features: The shape memory alloy plate (102a) generates pre-strain by pre-stretching, and the shape memory alloy plate (102a) generates pre-stress by thermal excitation.
4. A reinforcement method, Features: The invention comprises the concrete column annular reinforcement structure according to any one of claims 1 to 3, and The area on the surface of the concrete column that has cracked or is at risk of cracking is named the area to be reinforced. The area to be reinforced and the shape memory metal are pretreated, and the shape of the area to be reinforced is determined. The area to be reinforced is wrapped with the pretreated shape memory metal and thermally excited so that the shape memory metal wraps the concrete column, and the anchoring is completed after cooling.
5. The reinforcement method according to claim 4, Features: Decontaminate, polish and clean the surface of the area to be reinforced before reinforcement, and evenly apply structural adhesive on the surface of the area to be reinforced; The shape memory metal is cut out to completely wrap the surface of the area to be reinforced, and the shape memory metal is pre-stretched to make the shape memory metal produce pre-strain.
6. The reinforcement method according to claim 5, Features: The determination of the shape of the area to be reinforced is specifically as follows: If it is cylindrical, the pre-stretched shape memory metal is wrapped around the outside of the area to be reinforced, and the shape memory metal is completely attached to the structural adhesive. Under the adhesion of the structural adhesive, the shape memory metal is initially fixed to the area to be reinforced; If it is other shapes, the pre-stretched shape memory metal is wrapped around the outside of the area to be reinforced, and the shape memory metal is made to fit the structural adhesive as much as possible until the shape memory metal is initially fixed in the area to be reinforced.
7. The reinforcement method according to claim 6, Features: Different thermal excitation methods are adopted according to the shape of the area to be reinforced, specifically: If the area to be reinforced is cylindrical, the shape memory metal is thermally stimulated by a single heating method; If the area to be reinforced is in other shapes, the shape memory metal is thermally stimulated by gradually increasing the temperature.
8. The reinforcement method according to claim 7, Features: For cylindrical concrete columns in the area to be reinforced, a single heating-up thermal excitation method is used to make the shape memory metal produce prestress. Under the action of prestress, the shape memory metal clings to the concrete column. After heating to above 100°C, the structural adhesive softens and loses its fixing effect. After cooling, holes are opened at both ends of the shape memory metal, and anchors and pads are used to anchor the two ends of the shape memory metal.
9. The reinforcement method according to claim 8, Features: For concrete columns with other shapes in the area to be reinforced, a progressive heating thermal excitation method is adopted. During the multiple progressive thermal excitation processes, the shape memory metal generates prestress, and under the action of the prestress, the shape memory metal will cling to the concrete column, and the temperature of the multiple thermal excitations is not lower than 100°C.
10. The reinforcement method according to claim 9, Features: For concrete columns with other shapes in the area to be reinforced, after cooling, the excess shape memory metal due to shrinkage and close to the concrete column is cut, and the last thermal excitation is carried out. After cooling, holes are opened at both ends of the shape memory metal, and the two ends of the shape memory metal are anchored using anchors and pads.
Citation Information
Patent Citations
Reinforcing method for winding thermal excitation embedded shape memory alloy wires on concrete column
CN106639351A
Shape memory alloy prestressed U-stirrup-FRP reinforced concrete beam and construction technology thereof
CN110984620A
Round concrete column transverse prestress reinforcing structure and reinforcing method
CN114908991A
CFRP chilled casting group anchor inhaul cable with Fe-SMA casing pipe and anchoring method of CFRP chilled casting group anchor inhaul cable
CN115094754A
Method to strengthen or repair concrete and other structures
US20210115684A1