Preparation method of steel ladle paste
By using the ratio of electric calcined coal, metal silicon powder, graphite crushing and modified asphalt, ladle paste is prepared, which solves the problems of low usage times, high cost and insufficient performance of existing ladle materials, and achieves higher oxidation resistance and resistance Impact performance extends service life.
Patent Information
- Application Number
- CN202411189235.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-11-12
AI Technical Summary
The existing ladle materials have low usage times, high cost, complex construction, and lack excellent anti-slag, desulfurizer erosion, thermal shock, and mechanical erosion properties, and have high porosity and poor thermal expansion properties.
The ratio of electrocalcined coal, metal silicon powder, 0-2 particle size graphite crushed, graphite powder and modified asphalt is used to prepare ladle paste through stirring and heating treatment to improve its adhesion and oxidation resistance.
It reduces manufacturing costs, extends the number of uses, improves the resistance to slag, desulfurizer erosion, thermal shock, and mechanical erosion, and reduces porosity and thermal expansion performance. The number of uses can reach 250 times.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of carbon refractory materials, and in particular to a method for preparing ladle paste. Background Art
[0002] Refractoriness refers to the Celsius temperature at which a cone-shaped sample of a refractory material can resist high temperature without softening and melting under no load. Refractory materials are widely used, and the refractory materials used in different fields are also different. For ladle paste, based on the analysis of damage mechanism, it can be considered that ladle paste should have the following characteristics: first, excellent slag resistance; second, low reactivity with desulfurizer and resistance to the erosion of desulfurizer; third, excellent thermal shock resistance, no cracking and peeling; fourth, high strength and excellent resistance to mechanical erosion or impact; fifth, low thermal expansion performance; sixth, low porosity.
[0003] As a common refractory material, in the existing configuration of ladle materials, the ladle wall working layer adopts aluminum silicon carbide bricks with vertical width bricks and the ladle bottom working layer adopts bottom layer of vertical width carbon bricks.
[0004] However, there are many types of existing ladle materials, the materials used are expensive and the construction is relatively complicated. In terms of the number of times the ladle materials are used, the number of times the ladle materials are used is relatively low. Usually, a number of measures are taken, such as brick shape design and masonry optimization, working lining material and configuration optimization, and ladle operation management optimization, to gradually extend the number of times the ladle is used. The current average number of times is 80 times. Summary of the invention
[0005] In view of the deficiencies in the prior art, the present invention provides a method for preparing ladle paste, which solves the problems raised in the above background technology.
[0006] To achieve the above object, the present invention is implemented by the following technical scheme: A method for preparing ladle paste, comprising the following preparation steps: Step 1: Add the raw materials into a kneading pot according to the proportion and stir; Step 2: After stirring in the kneading pot in step 1, dry mixing is completed, and then 20% to 25% of the modified asphalt is added to the kneading pot.
[0007] Preferably, the raw materials added in step 1 are electric calcined coal, metallic silicon powder, 0-2 particle size graphite fragments, and graphite powder.
[0008] Preferably, in the step 1, the time for uniformly stirring the raw materials in the kneading pot is 20 to 30 minutes, and the stirring temperature of the kneading pot is 130 to 150°C.
[0009] Preferably, the temperature for adding the reformed asphalt in step 2 is controlled to be 170-190° C., and the reformed asphalt is stirred for 25-35 minutes after adding.
[0010] A ladle paste comprises the following raw materials in percentage by weight: Electric calcined coal 50-60%; Metal silicon powder 5-10%; 0-2 particle size graphite 5-10%; Graphite powder 5-10%; Reformed asphalt 20-25%; And the total mass ratio of each raw material is 100%.
[0011] Preferably, the electrically calcined coal comprises the following raw materials in mass percentage according to particle size: Electric calcined coal with particle size above 10: 20-25%: 6-10 particle size electric calcined coal 10-15%; 0-6 particle size electric calcined coal 15-20%.
[0012] Preferably, the electrically calcined coal is produced at high temperature in an electric furnace.
[0013] Preferably, the content of elemental silicon in the metallic silicon powder is not less than 97%, and the rest is silicon dioxide and inevitable impurities.
[0014] Preferably, the carbon content in the graphite fragments is greater than 95%, and the rest is inevitable impurities.
[0015] Preferably, the content of carbon in the graphite powder is 96%, and the rest is inevitable impurities, and the particle size of the graphite powder is smaller than the particle size of the graphite fragments.
[0016] The present invention provides a method for preparing ladle paste, which has the following beneficial effects: The present invention does not require the addition of new equipment and has a simple process. Compared with the current use of carbon bricks in the industry, the manufacturing cost is reduced and the product is resistant to erosion, the oxidation resistance of the product is improved, the number of uses is extended, the slag resistance is improved, the corrosion resistance of the desulfurizer and the thermal shock resistance are enhanced, and the product has excellent resistance to mechanical erosion or impact, low thermal expansion performance and low porosity. After many experiments, the maximum number of uses of the ladle using this product can reach 250. DETAILED DESCRIPTION
[0017] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0018] Embodiment 1 This embodiment provides a ladle paste, comprising the following raw materials in percentage by weight: Electric calcined coal 54%, and the electric calcined coal is made by high temperature in electric furnace, including: Electric calcined coal with a particle size of 10 or above accounts for 23%, electric calcined coal with a particle size of 6-10 accounts for 13%, and electric calcined coal with a particle size of 0-6 accounts for 18%; 8% metallic silicon powder, of which the content of elemental silicon in the metallic silicon powder is not less than 97%, and the rest is silicon dioxide and unavoidable impurities; 0-2 particle size graphite crumbs 8%, of which the carbon content in the graphite crumbs is greater than 95%, and the rest are unavoidable impurities; 8% graphite powder, wherein the content of carbon in the graphite powder is 96%, and the rest is inevitable impurities, and the particle size of the graphite powder is smaller than the particle size of the graphite powder; reformed asphalt 22%; The total mass ratio of the above raw materials is 100%. The electric calcined coal has good thermal stability and thermal conductivity, as well as high mechanical strength. The electric calcined powder is used to fill the gaps between the above materials to increase the packing density. Graphite has good thermal stability and a low thermal expansion coefficient. Metal silicon powder can increase the strength of the product at high temperatures. The modified asphalt plays a better bonding role and cokes after reaching a certain temperature. The main component of metallic silicon powder is crystalline silicon. At first, it is in block form and its color is relatively stable. After a series of crushing or grinding, it becomes powder. Graphite powder is a mineral powder, the main component of which is carbon. It is soft and black-gray in color. Graphite powder is a substance with very sensitive chemical reactions. Its resistivity will change in different environments, that is, its resistance value will change. But one thing will not change. Graphite powder is one of the best non-metallic conductive materials. As long as the graphite powder is uninterrupted in an insulating object, it will be electrified like a thin wire. However, there is no accurate number for the resistance value, because the thickness of graphite powder is different, and the resistance value of graphite powder will be different when used in different materials and environments.
[0019] Embodiment 2: Based on the above-mentioned provision of a ladle paste raw material, this embodiment proposes a method for preparing a ladle paste, comprising the following preparation steps: Step 1: Add electric calcined coal, metallic silicon powder, 0-2 particle size graphite powder and graphite powder into a kneading pot according to the proportion and stir, wherein the stirring time of the kneading pot is 25 minutes and the stirring temperature of the kneading pot is 140°C; Step 2: After stirring in the kneading pot in step 1, complete dry mixing, and then add 22% of modified asphalt into the kneading pot, wherein the temperature of adding the modified asphalt is controlled to be 180° C., and stir for 30 minutes after adding the modified asphalt.
[0020] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for preparing ladle paste, characterized in that: The method comprises the following preparation steps: Step 1: Add the raw materials into a kneading pot according to the proportion and stir; Step 2: After stirring in the kneading pot in step 1, dry mixing is completed, and then 20% to 25% of the modified asphalt is added to the kneading pot.
2. The method for preparing ladle paste according to claim 1, characterized in that: The raw materials added in step 1 are electric calcined coal, metallic silicon powder, 0-2 particle size graphite pieces, and graphite powder.
3. The method for preparing ladle paste according to claim 1, characterized in that: In the step 1, the raw materials are uniformly stirred in the kneading pot for 20 to 30 minutes, and the stirring temperature of the kneading pot is 160-180°C.
4. The method for preparing ladle paste according to claim 1, characterized in that: The temperature of adding the reformed asphalt in step 2 is controlled to be 170-190° C., and the reformed asphalt is stirred for 25-35 minutes after adding.
5. A ladle paste, using the method for preparing a ladle paste according to any one of claims 1 to 4, characterized in that: Including the following raw materials in mass percentage: Electric calcined coal 50-60%; Metal silicon powder 5-10%; 0-2 particle size graphite 5-10%; Graphite powder 5-10%; Reformed asphalt 20-25%; And the total mass ratio of each raw material is 100%.
6. The ladle paste according to claim 5, characterized in that: The electric calcined coal includes the following raw materials in terms of mass percentage according to particle size: Electric calcined coal with particle size above 10: 20-25%: 6-10 particle size electric calcined coal 10-15%; 0-6 particle size electric calcined coal 15-20%.
7. The ladle paste according to claim 5, characterized in that: The electric calcined coal is produced by using an electric furnace at high temperature.
8. The ladle paste according to claim 5, characterized in that: The content of elemental silicon in the metallic silicon powder is not less than 97%, and the rest is silicon dioxide and inevitable impurities.
9. The ladle paste according to claim 5, characterized in that: The content of carbon in the graphite fragments is greater than 95%, and the rest is inevitable impurities.
10. The method for preparing ladle paste according to claim 5, characterized in that: The content of carbon in the graphite powder is 96%, and the rest is inevitable impurities. The particle size of the graphite powder is smaller than that of the graphite fragments.