M-Z light wave heat conduction optical switch of polymer silicon dioxide heterogeneous modulation arm

By adopting laterally coupled polymer and high-refractive index silicon dioxide waveguide structure on the silicon dioxide photonic chip and combining electrode design, the problems of high power consumption and heterogeneous integrated coupling loss of thermal tuning devices of silicon dioxide chips are solved. It realizes low power consumption and low loss optical waveguide thermal optical switch, suitable for high-speed optical communication.

CN118963006APending Publication Date: 2024-11-15SHENZHEN TECH UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411228192.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing silicon dioxide photonic chips have high driving power consumption in thermally tuning devices, and the difference in refractive index results in high coupling loss when heterogeneously integrated with polymer materials, limiting the performance and miniaturization of the device.

Method used

The substrate chip adopts a three-layer film structure, combining polymer and high-refractive index silica waveguides through lateral coupling, reduce switching time and power consumption, and spin-coated the electrode layer on the polymer cladding to optimize modulation efficiency.

Benefits of technology

It realizes low-power and low-loss optical waveguide thermal optical switches, which are suitable for large-scale production, meet the needs of high-speed optical communications, and improves the reliability and stability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118963006A_ABST
    Figure CN118963006A_ABST
Patent Text Reader

Abstract

The invention provides an M-Z optical wave heat conduction optical switch of a polymer silicon dioxide heterogeneous modulation arm, the system comprises a substrate chip, an M-Z optical waveguide structure layer is formed on the substrate chip, the M-Z optical waveguide structure layer comprises a polymer waveguide and a high refractive index silicon dioxide waveguide, and the polymer waveguide and the high refractive index silicon dioxide waveguide are located on the same plane; a lateral coupling mode is adopted between the polymer waveguide and the high-refractive-index silicon dioxide waveguide; the height of the polymer waveguide is lower than that of the high-refractive-index silicon dioxide waveguide; a polymer cladding is spin-coated on the M-Z optical waveguide structure layer, an electrode layer is arranged on the polymer cladding, and the electrode layer is located right above the polymer waveguide in the M-Z optical waveguide structure. Loss is reduced through a lateral coupling mode, switching power consumption is reduced through a polymer material with a high thermo-optical coefficient, and switching time and power consumption are reduced through a mode of reducing the thickness of a polymer layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of polymer optical waveguide and silicon dioxide waveguide hybrid integrated photonic chip manufacturing, and in particular to a Mach-Zenhder (MZ) hybrid integrated optical waveguide thermo-optic switch of polymer silicon dioxide coplanar heterogeneous waveguide modulation arms. Background Art

[0002] Silica photonic chips are core devices for optical communications and optical networks. They have the characteristics of high stability, low transmission loss, and low fiber coupling loss, and are widely used in beam splitters, AWGs, and other fields. Due to the stability of silica materials, thermal tuning is the only way to achieve adjustability. However, the thermal-optical coefficient of silica is about 10 -5 K -1 The driving power consumption of silicon dioxide thermal tuning devices, such as thermo-optic switches and variable optical attenuators, is tens to hundreds of milliwatts.

[0003] Hybrid integration of multiple materials is an important solution to the above problems, that is, combining different materials through end-face connection or multi-layer heterogeneity to improve the function and performance of the chip. However, the refractive index difference between silicon dioxide and functional materials such as silicon, silicon nitride, and lithium niobate is relatively large. The huge difference in waveguide size using end-face coupling leads to high coupling loss, while the use of regional integration and other methods is not conducive to the miniaturization of existing chips and increases chip costs.

[0004] Polymers have become an important solution for hybrid integration with silica. The refractive index range of polymer materials and silica materials is close, and thus they have closer waveguide sizes, reducing coupling losses and mode mismatch problems. Polymer materials have good compatibility and can be coated on the surface of silica chips in the form of cladding or core layers. However, with the cladding covering solution, the efficiency of light and polymer interaction is low, which is not conducive to reducing the power consumption of the switch. However, in the existing structure, fewer devices have realized heterogeneous integrated switch structures with polymer and silica as core layers. In the coupling process, the waveguide and optical fiber need to have better matching, so the refractive index of the silica core layer cannot be too high, and the size is close to that of the optical fiber; but in the heating area of ​​the thermo-optical switch, the smaller the waveguide size, the less heat is required, and the switching time and power consumption are lower. Therefore, the polymer waveguide size needs to be small and can confine the light field, so the refractive index of the heterogeneous integrated polymer should be improved. Therefore, there is a certain difference in the refractive index between silica and polymer materials. In the heterogeneous integration process, the direct coupling method with a high refractive index difference has a certain mode mismatch loss, and the greater the refractive index difference, the higher the mode mismatch loss. Therefore, in the polymer and silica heterogeneous integrated switch, the coupling loss of waveguides of materials with different refractive indices becomes a bottleneck that needs to be solved for high-performance devices. Summary of the invention

[0005] In order to solve the above problems existing in the prior art, the purpose of the present invention is to provide an MZ optical waveguide thermo-optical switch with a polymer-silicon dioxide heterogeneous modulation arm, which reduces losses by lateral coupling and reduces switching time and power consumption by reducing the thickness of the polymer layer.

[0006] The present invention achieves the above-mentioned purpose through the following technical solutions:

[0007] A polymer silicon dioxide heterogeneous modulation arm MZ optical waveguide thermo-optic switch, comprising:

[0008] A substrate chip with a three-layer film structure (the three-layer film structure is, from bottom to top, a silicon substrate (for the convenience of cutting and dissociation), a low-refractive-index silicon dioxide layer (for the lower cladding of the waveguide), and a high-refractive-index silicon dioxide layer (for preparing the silicon dioxide part of the MZ structure);

[0009] An MZ optical waveguide structure layer is formed on the substrate chip, wherein the MZ optical waveguide structure layer includes a polymer waveguide and a high-refractive-index silica waveguide, and the lower edges of the two waveguides are located on the same plane; wherein the high-refractive-index silica waveguide is obtained by etching the high-refractive-index silica layer in the substrate chip, and the polymer waveguide is obtained by photolithography development;

[0010] The polymer waveguide and the high refractive index silica waveguide are coupled sideways;

[0011] The height of the polymer waveguide is lower than that of the silica waveguide;

[0012] A polymer cladding layer is spin-coated on the MZ optical waveguide structure layer, an electrode layer is disposed on the polymer cladding layer, and the electrode layer is located directly above the polymer waveguide in the MZ optical waveguide structure.

[0013] According to a polymer-silicon dioxide heterogeneous modulation arm MZ optical waveguide thermo-optic switch provided by the present invention, the substrate chip comprises, from top to bottom:

[0014] A high refractive index doped silicon dioxide layer, the refractive index of which is 1.455 to 1.48 and the thickness of which is 2 to 10 μm;

[0015] A low-refractive-index silicon dioxide layer, whose refractive index is 1.44 to 1.45 and whose thickness is 3 to 15 μm;

[0016] The bottom layer is a silicon-based silicon dioxide layer, the silicon dioxide layer is larger than 3 μm, the refractive index is 1.44-1.45, and the thickness of the two layers is 100-1000 μm.

[0017] According to a polymer-silicon dioxide heterogeneous modulation arm MZ optical waveguide thermo-optic switch provided by the present invention, the steps of preparing the MZ optical waveguide structure layer include:

[0018] Providing a high refractive index doped silicon dioxide layer as the silicon dioxide waveguide part of the MZ optical waveguide structure layer, wherein the refractive index thereof is 1.455 to 1.48 and the thickness thereof is 2 to 10 μm;

[0019] Select a substrate chip that is projected as a rectangle in the vertical direction;

[0020] Evaporating a mask layer on a substrate chip to form a mask layer for a silicon dioxide waveguide;

[0021] Spin-coating photoresist to form a photoresist film layer with a thickness of 0.1 to 5 μm;

[0022] A photoresist mask layer is obtained by introducing a pattern on the photoresist film layer using a photolithography plate or a maskless photolithography machine, performing photolithography and then developing the pattern.

[0023] According to the MZ optical waveguide thermo-optical switch of a polymer silicon dioxide heterogeneous modulation arm provided by the present invention, the two MZ structures of the MZ pattern reticle include: the length L of the input and output regions (a) a A straight waveguide of 0.02 to 5 mm; the length L of the input and output Y branch region (b) b , which is the length of the Y branch region along the waveguide propagation direction; when a photolithography plate is used for photolithography, the photolithography plate is a straight waveguide pattern, the waveguide length L2 is a rectangle with a length of 10100 to 50100 μm, the waveguide structure width x2 is 3 to 10 μm, the long side of the waveguide is parallel to the long side of the substrate chip, the distance between the long side of the waveguide and the long side of the substrate chip in the x direction is 2 to 50 μm, and it intersects the two short sides perpendicularly in the z direction, that is, the length in the z direction is greater than the length of the long side of the substrate chip.

[0024] According to the MZ optical waveguide thermo-optic switch of a polymer-silicon dioxide heterogeneous modulation arm provided by the present invention, when manufacturing the silicon dioxide waveguide, a mask etching agent is used to etch the mask layer to obtain a waveguide mask pattern;

[0025] The waveguide core layer is obtained by plasma etching or ICP etching, and the etching depth is d3;

[0026] The photoresist mask layer is removed with a corresponding photoresist developer, and the waveguide mask pattern is removed with a corresponding solution to obtain a silicon dioxide waveguide chip.

[0027] According to the MZ optical waveguide thermo-optic switch of the polymer-silicon dioxide heterogeneous modulation arm provided by the present invention, a waveguide core material is spin-coated on a silicon dioxide waveguide chip to obtain a polymer waveguide core material film, wherein the film thickness d6 is 1 to 10 μm, which is approximately half of the waveguide layer thickness d3;

[0028] An MZ pattern photolithography plate is used for photolithography or a maskless photolithography machine is used to import a graphic file consistent with the MZ pattern photolithography plate, and a polymer waveguide is obtained after development, thereby forming an MZ optical waveguide structure layer.

[0029] According to the MZ optical waveguide thermo-optic switch of a polymer silica heterogeneous modulation arm provided by the present invention, when the waveguide core layer material is spin-coated on the silica waveguide chip, the spin-coating speed is 2500-10000 rpm, the spin-coating time is 30-300 s, and after curing, a polymer waveguide core layer material film is obtained, and the film thickness d6 is 1-10 μm, which is about half of the waveguide layer thickness d3.

[0030] According to the MZ optical waveguide thermo-optic switch of a polymer-silicon dioxide heterogeneous modulation arm provided by the present invention, the thickness d7 of the polymer cladding is 1.5-5 μm thicker than d6, and the thickness d8 of the electrode layer is 20-500 nm.

[0031] Before forming the electrode pattern layer, a photoresist layer is spin-coated on the electrode layer to obtain an electrode material mask layer with a thickness of 0.2-2 μm, and then a mask plate with an electrode pattern is covered on the photoresist layer.

[0032] According to the MZ optical waveguide thermo-optic switch of the polymer silicon dioxide heterogeneous modulation arm provided by the present invention, the middle strip structure of the mask plate with the electrode pattern has a width x7 of 3 to 15 μm and a length L6 of 0.1 to 1 mm, and ensures that the straight electrode part is completely parallel and covers one arm of the MZ optical waveguide structure;

[0033] The electrode pin adopts a same-side structure, and two identical pins extend outward from the two ends of the straight electrode structure to the outside of the MZ optical waveguide structure. The difference x8 between the pin structure and the strip structure in the x direction is 1 to 2 μm. The electrode pin is a rectangle with a length L7 of 5 to 15 μm and a width x9 of 5 to 15 μm in the z direction.

[0034] After photolithography, the mask is removed, and the photoresist layer and the electrode material layer are etched with an aqueous sodium hydroxide solution (mass ratio 4-6‰), and the photoresist layer on the electrode is removed with acetone or a corresponding photoresist stripper (note that it cannot react with the upper cladding material) to obtain an electrode pattern layer.

[0035] According to the MZ optical waveguide thermo-optic switch of the polymer silicon dioxide heterogeneous modulation arm provided by the present invention, the MZ optical waveguide structure after obtaining the electrode pattern layer is directly cut, and the input and output straight waveguides are perpendicular to the projection direction and connected to the L a The input waveguide segments intersect vertically, thus obtaining a double-arm heterogeneous optical waveguide thermo-optic switch, which is finally connected to an optical fiber, a photodetector, a signal generator and an oscilloscope for testing.

[0036] It can be seen that compared with the prior art, the present invention has the following beneficial effects:

[0037] The lateral hybrid integration scheme has low process tolerance and loss: In the scheme of lateral coupling hybrid integrated optical waveguide thermo-optical switch of polymer waveguide and silica waveguide, the lateral coupling mode between polymer waveguide and silica waveguide is conducive to realizing efficient optical signal transmission and modulation. Compared with the direct docking coupling mode, the present invention has wider refractive index adaptability and lower light field leakage loss.

[0038] Cost-effectiveness: Polymer materials and silica materials have their own advantages in terms of cost and manufacturing process. Polymer materials are usually low-cost, simple to manufacture, and suitable for large-scale production. Silica materials have the characteristics of low transmission loss and low coupling loss. The combination of the two can realize low-cost and high-performance devices.

[0039] Performance optimization: By combining the high thermo-optic coefficient of polymers and the low transmission loss of silicon dioxide, devices with low power loss and small size can be designed.

[0040] The two arms are made of different materials and at different heights, resulting in lower switching time, power consumption and loss: The design of the polymer waveguide being lower in height than the silica waveguide helps reduce the scattering and loss of light between waveguides and improves the overall performance of the device. Compared with the traditional asymmetric MZ with two arms of the same material, the two arms of the present invention are made of different materials, and a heating electrode is placed on the polymer arm. The high thermo-optical coefficient of the polymer is used to reduce the switching power consumption. The two arms are of different heights. The large size of the silica waveguide reduces the coupling loss with the optical fiber, and the polymer waveguide reduces the height, which reduces the time required for the thermo-optical switch to dissipate heat and the total amount of heat, thereby further reducing the switching time and power consumption.

[0041] Electrode design: Evaporating the electrode material layer on the polymer cladding and setting the electrode pattern layer can achieve precise modulation and control. This design helps optimize the modulation efficiency and response speed while reducing the interference of the electrode on the optical signal.

[0042] Polymer cladding: The polymer cladding not only protects the waveguide structure, but also further improves the performance of the device through its material properties. For example, some polymer materials may have a low refractive index or good thermal conductivity, which helps to reduce the insertion loss of the device and improve thermal stability.

[0043] Low power consumption: By optimizing the waveguide size and electrode design, the power consumption of the device can be reduced compared to silicon dioxide switching devices. This is of great significance for large-scale integration and practical applications.

[0044] Fast response: Combining the high thermo-optical coefficient of polymers and optimized electrode design, a faster response speed can be achieved compared to all-polymer switching devices, meeting the needs of high-speed optical communication systems.

[0045] High reliability: Made of mature materials and processes, it helps to improve the reliability and stability of the device and reduce maintenance costs.

[0046] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0047] Figure 1 It is a first structural schematic diagram of a substrate chip in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0048] Figure 2 It is a second structural schematic diagram of a substrate chip in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0049] Figure 3 It is a structural schematic diagram of a mask layer and a photoresist film layer in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0050] Figure 4 It is a structural schematic diagram of a mask layer and a photolithography plate in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0051] Figure 5 It is a structural schematic diagram of a waveguide mask plate in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0052] Figure 6 It is a structural schematic diagram of a photoresist mask layer in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0053] Figure 7 It is a structural schematic diagram of a mask layer in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0054] Figure 8 It is a structural schematic diagram of the core layer in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0055] Fig. 9 It is a schematic structural diagram of a silicon dioxide chip in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0056] Fig.10 It is a first structural schematic diagram of a waveguide core material in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silica heterogeneous modulation arm of the present invention.

[0057] Fig.11 It is a second structural schematic diagram of the waveguide core material in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silica heterogeneous modulation arm of the present invention.

[0058] Fig.12 It is a structural schematic diagram of an MZ pattern photolithography plate in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0059] Fig.13 It is a schematic diagram of the principle of an MZ pattern photolithography plate in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0060] Fig.14 It is a structural schematic diagram of an MZ optical waveguide structure in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0061] Fig.15 It is a schematic structural diagram of the cladding in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silica heterogeneous modulation arm of the present invention.

[0062] Fig.16 It is a structural schematic diagram of the evaporated electrode material in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0063] Fig.17 It is a planar schematic diagram of the evaporated electrode material in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0064] Fig.18 It is a structural schematic diagram of spin coating photoresist on an electrode material layer in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0065] Fig.19 It is a structural schematic diagram of a mask with an electrode pattern in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0066] Fig. 20 It is a plan view schematic diagram of a mask with an electrode pattern in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0067] Fig.21 It is a structural schematic diagram of an electrode pattern layer in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silicon dioxide heterogeneous modulation arm of the present invention.

[0068] Fig. 22 It is a structural schematic diagram of access optical fiber detection in an embodiment of an MZ optical waveguide thermo-optic switch of a polymer silica heterogeneous modulation arm of the present invention. DETAILED DESCRIPTION

[0069] In order to make the purpose, technical solution and advantages of the embodiment of the present invention clearer, the technical solution of the embodiment of the present invention will be clearly and completely described below in conjunction with the drawings of the embodiment of the present invention. Obviously, the described embodiment is a part of the embodiment of the present invention, not all of the embodiments. Based on the described embodiment of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0070] The present embodiment provides a polymer-silicon dioxide heterogeneous modulation arm MZ optical waveguide thermo-optical switch 100, comprising:

[0071] Substrate chip;

[0072] An MZ optical waveguide structure layer is formed on the substrate chip, wherein the MZ optical waveguide structure layer includes a polymer waveguide and a high-refractive-index silica waveguide, and both are located on the same plane; wherein the high-refractive-index silica waveguide is obtained by etching the high-refractive-index silica layer in the substrate chip;

[0073] The polymer waveguide and the high refractive index silica waveguide are coupled sideways;

[0074] The height of the polymer waveguide is lower than that of the silica waveguide;

[0075] A polymer cladding layer 16 is spin-coated on the MZ optical waveguide structure layer, and an electrode layer 17 is evaporated on the polymer cladding layer 16 . The electrode layer 17 is located directly above the polymer waveguide in the MZ optical waveguide structure.

[0076] In this embodiment, the substrate chip includes, from top to bottom:

[0077] The bottom layer 1 is a silicon-based silicon dioxide layer, the silicon dioxide layer is larger than 3 μm, the refractive index thereof is 1.44-1.45, and the thickness d1 of the two layers thereof is 100-1000 μm.

[0078] A low-refractive-index silicon dioxide layer 2, whose refractive index is 1.44 to 1.45 and whose thickness d2 is 3 to 15 μm;

[0079] A high refractive index doped (Ge) silicon dioxide layer 3, whose refractive index is 1.455-1.48 and whose thickness d3 is 2-10 μm;

[0080] In this embodiment, the steps of preparing the MZ optical waveguide structure layer include:

[0081] Providing a high refractive index doped silicon dioxide layer as the silicon dioxide waveguide part of the MZ optical waveguide structure layer, wherein the refractive index thereof is 1.455 to 1.48 and the thickness thereof is 2 to 10 μm;

[0082] Select a substrate chip that is projected as a rectangle in the vertical direction;

[0083] Evaporating a mask layer 4 (the mask layer material here can be Al, Cr or silicon nitride material, with a thickness of d410-200nm) on the substrate chip to make a mask layer for the silicon dioxide waveguide;

[0084] Spin-coat the photoresist to form a photoresist film layer 5 (such as BP212, AZ photoresist, etc., with a thickness of d50.1-5 μm), with a thickness of 0.1-5 μm, a spin-coating speed of 1000-10000 rpm, and a time of 30-300 s. Figure 3 , 4 shown.

[0085] A photoresist mask layer 10 is obtained by introducing a pattern on the photoresist film layer 5 using a photolithography plate or a maskless photolithography machine, performing photolithography and then developing.

[0086] In this embodiment, when a photolithography plate is used for photolithography, the photolithography plate is a straight waveguide pattern, such as Figure 5 As shown, the waveguide length L2 is a rectangle with a length of 10100 to 50100 μm, the waveguide structure width x2 is 3 to 10 μm (the straight waveguide is the opaque part, or the two sides are exposure areas during maskless lithography), the long side of the waveguide is parallel to the long side of the substrate chip, the spacing between the long side of the waveguide and the long side of the substrate chip in the x direction is 2 to 50 μm, and it intersects the two short sides perpendicularly in the z direction, that is, the length in the z direction is greater than the length of the long side of the substrate chip.

[0087] The photoresist mask layer 10 is obtained by photolithography (photolithography exposure intensity 15-50 mW / cm2, time 2-100 s) and development (development in a developer corresponding to the photoresist, time: 30-300 s), and its structure is as follows: Figure 6 shown.

[0088] In this embodiment, when manufacturing the silicon dioxide waveguide chip, a mask etching agent (sodium hydroxide, etc.) is used to etch the mask layer 4 to obtain a waveguide mask pattern 11, the structure of which is as follows: Figure 7 shown.

[0089] The waveguide core layer 12 is obtained by plasma etching or ICP etching, and the etching depth is the depth of d1, such as Figure 8 shown.

[0090] The photoresist mask layer 10 is removed with a corresponding photoresist developer, and the waveguide mask pattern 11 is removed with a corresponding solution to obtain a silicon dioxide waveguide chip. Fig. 9 shown.

[0091] In this embodiment, the waveguide core material is spin-coated on the silicon dioxide waveguide chip, such as Fig.10 As shown, the spin coating speed is 2500-10000 rpm, the spin coating time is 30-300 s, and after curing (curing can be performed in an oven or a hot plate, the curing temperature is 50-70° C., 5-15 min, 85-95° C., 5-30 min), a polymer waveguide core layer material film 13 is obtained, as shown Fig.11 As shown, the film thickness d6 is 1 to 10 μm, which is approximately half of the waveguide layer thickness d3.

[0092] The MZ pattern photomask is used for photolithography or a maskless photolithography machine is used to import a graphic file consistent with the MZ pattern photomask (in gds format), and then the polymer waveguide 15 is obtained after development, thereby forming an MZ optical waveguide structure layer.

[0093] In this embodiment, when the waveguide core material is spin-coated on the silicon dioxide waveguide chip, the spin-coating speed is 2500-10000 rpm, the spin-coating time is 30-300 s, and after curing, a polymer waveguide core material film 13 is obtained, and the film thickness d6 is 1-10 μm, which is about half of the waveguide layer thickness d3.

[0094] MZ pattern lithography board Fig.13 As shown, both MZ structures are divided into: Input and output area (a) length L a The straight waveguide is 0.02 to 5 mm; the length of the input and output Y branch region (b) is L b Among them, the branch graph is a cosine structure, because the transmission loss and bending loss of the cosine-shaped function curve waveguide are low, and the curve equation is: The a and b parameters are defined by the branch angle θ and the branch distance d (d = 2 × x5). The branch angle θ is less than 1 degree, and θ is affected by the offset x6 in the x direction and the offset L in the z direction. b Determine, the formula is:

[0095] The distance x6 between the two branch arms is 10 to 60 μm. The curvature radius R is guaranteed to be 3500 to 7000 μm: To reduce the bending loss of the device. Section (c) is the other arm of the waveguide, and its length is L c The length of the two sections (d) is 1000 to 30000 μm, and the two sections (d) are parallel regions, where one side of the photoresist is parallel to the waveguide and fits in place, with a length of L d (e) is a coupling section, the starting section of which starts from one end of (d) and the extension in the z direction is L e The distance between the end point and the straight waveguide is 50 to 1000 μm, and the offset in the x direction is x2, so that the end point is completely aligned with the straight waveguide. The constraint formula is L e ≥2(L d +L e ) and (L a +L b +L c )≤L1. The last one is the output waveguide (a).

[0096] The polymer waveguide 15 is obtained by photolithography and development. Fig.14 As shown, the polymer upper cladding layer 16 is spin-coated (spinning speed 2500-10000 rpm, spin coating time 30-300 s, and cured by the desired curing method), and the cladding layer 16 material is as follows Fig.15 As shown, the electrode material is evaporated (electron beam evaporation, thermal evaporation or sputtering) on ​​the cladding material 16 to obtain an electrode material layer 17, as shown in FIG. Fig.16 The front view after spin coating the cladding material 16 and evaporating the electrode material is shown in FIG. Fig.17 shown.

[0097] In this embodiment, the thickness d7 of the polymer coating 16 is 1.5-5 μm thicker than d6 , and the thickness d8 of the electrode material layer 17 is 20-500 nm.

[0098] Before forming the electrode pattern layer 20, a photoresist layer 18 is spin-coated on the electrode material layer 17 (spin coating speed 1000-10000 rpm, time 30-300 s) to obtain an electrode material mask layer with a thickness of 0.2-2 μm. Subsequently, a mask plate with an electrode pattern is covered on the photoresist layer or the electrode pattern is introduced using a maskless photolithography machine, and the plate is aligned on the maskless photolithography machine.

[0099] like Fig.19 , 20 As shown, the middle strip structure of the mask plate with the electrode pattern has a width x7 of 3 to 15 μm and a length L6 of 0.1 to 1 mm, and ensures that the straight electrode part is completely parallel and covers one arm of the polymer waveguide 15 .

[0100] The electrode pins adopt a same-side structure, and two identical pins extend outward from the two ends of the straight electrode structure to the outside of the polymer waveguide 15. The difference x8 between the pin structure and the strip structure in the x direction is 1 to 2 μm. The electrode pins are rectangular with a length L7 of 5 to 15 μm and a width x9 of 5 to 15 μm in the z direction. The three-dimensional schematic diagram after covering is as shown in FIG. Fig.19 shown.

[0101] After photolithography (photolithography exposure intensity 15-50 mW / cm2, time 2-100 s), the mask is removed, and the photoresist layer and the electrode material layer 17 are etched with a 5‰ sodium hydroxide aqueous solution, and the photoresist layer on the electrode is removed with acetone to obtain an electrode pattern layer 20, such as Fig.21 shown.

[0102] The MZ optical waveguide structure layer after obtaining the electrode pattern layer 20 is directly cut, and the projection direction is perpendicular to the input and output straight waveguide (a) and connected to L a The input waveguides of the two segments intersect vertically, and the double-arm heterogeneous optical waveguide thermo-optic switch is obtained. Finally, the optical fiber, photodetector, signal generator and oscilloscope are connected for testing. Fig. 22 As shown, the feasibility of the results is verified.

[0103] In practical applications, a commercial (Rockchip) three-layer film structure substrate sheet with a rectangular projection in the vertical direction is first selected (the substrate sheet thickness is 693 μm, its length L1 is 3 cm, and its width x1 is 2 cm), such as Figure 1 , 2 As shown. Among them, the three-layer film structure from top to bottom, the top layer is high refractive index doped (Ge) silicon dioxide, its refractive index is 1.48, thickness is d1 (2 ~ 10μm), the second layer is low refractive index silicon dioxide, its refractive index is 1.445, thickness is d2 (3 ~ 15μm), the third layer is silicon-based silicon dioxide layer thickness 675μm.

[0104] Evaporate the mask layer 4 (the mask layer material can be Al, Cr or silicon nitride material, the thickness d4 is 2nm) on the wafer, spin-coat the photoresist (positive photoresist) to form a photoresist film layer, use SU-8 series 2002 model photoresist, the thickness is 1.5μm, spin-coating speed is 3000rpm, time is 30S, as shown in FIG. Figure 3 , 4 A photomask and a photolithography machine, or a maskless photolithography machine is used to import a pattern for photolithography. The photomask is a straight waveguide pattern, and its planar schematic diagram is shown in FIG. Figure 5As shown, the waveguide length L2 is a rectangle of 30100μm, and the waveguide structure width x2 is 3μm (the straight waveguide is the opaque part, or the two sides are the exposure area in maskless lithography). The long side of the waveguide is parallel to the long side of the wafer structure, and the distance between the long side of the waveguide and the long side of the wafer in the x direction is 50μm. In the z direction, it intersects perpendicularly with the two short sides, that is, the length in the z direction is greater than the length of the long side of the wafer.

[0105] After photolithography (photolithography exposure intensity 20mW / cm2, time 8s), development (development in a developer corresponding to the photoresist, time: 30s) is performed to obtain a photoresist mask layer 10, the structure of which is as follows: Figure 6 Then, the photoresist mask layer 10 is obtained by washing with isopropyl alcohol and deionized water, and a waveguide mask pattern 11 is obtained, and its structure is as shown in FIG. Figure 7 The waveguide core layer 12 is obtained by ICP etching, and the etching depth is d1, as shown in FIG. Figure 8 The photoresist mask layer 10 is removed with a corresponding photoresist developer, and the waveguide mask pattern 11 is removed with a corresponding solution (development time 5s), to obtain a silicon dioxide waveguide chip, as shown. Fig. 9 shown.

[0106] The waveguide core material is spin-coated on a silicon dioxide chip, such as Fig.10 The spin coating speed is 50000 rpm, the spin coating time is 60 s, and after curing (curing can be performed in an oven or a hot plate, the curing temperature is 60° C., 5 min, 90° C., 10 min), a polymer waveguide core layer material film 13 is obtained, as shown. Fig.11 As shown, the film thickness d6 is 1.5 μm. (Here, it can be SU-8 material) Using MZ pattern photolithography plate 14, such as Fig.12 Perform photolithography or use a maskless photolithography machine to import the above-mentioned photolithography consistent (GDS format) graphic file.

[0107] MZ pattern lithography board Fig.13 As shown. Both MZ structures are divided into: Input and output area (a) length L a The straight waveguide is 4 mm long; the length of the input and output Y branch region (b) is L b Among them, the branch graph is a cosine structure, because the transmission loss and bending loss of the cosine-shaped function curve waveguide are low, and the curve equation is: The a and b parameters are defined by the branch angle θ and the branch distance d (d = 2 × x5). The branch angle θ is less than 1 degree, and θ is affected by the offset x6 in the x direction and the offset L in the z direction. b Determine, the formula is:

[0108] The distance x6 between the two branch arms is 10-60 μm, the angle between the two branches is less than 1 degree, the branch is a straight waveguide, an inverse sine or inverse cosine function, and when it is an inverse sine and cosine, its curvature radius is greater than 3000 μm. (c) Segment is the other arm of the waveguide, and its length L c The length of the two sections (d) is 1000 to 30000 μm, and the two sections (d) are parallel regions, where one side of the photoresist is parallel to the waveguide and fits in place, with a length of L d (e) is a coupling section, the starting section of which starts from one end of (d) and the extension in the z direction is L e The length of the waveguide is 50 to 1000 μm, and the offset in the x direction is x2, so that the end point is completely aligned with the straight waveguide. The constraint formula is L e ≥2(L d +L e ) and (L a +L b +L c )≤L1, and finally the output waveguide (a).

[0109] After photolithography and development, a polymer waveguide 15 is obtained. Fig.14 As shown, the polymer upper cladding layer 16 is spin-coated (spinning speed 5000 rpm, spin coating time 60 s, and cured by the desired curing method), and the cladding layer 16 material is as follows Fig.15 As shown, the thickness d7 of the cladding 16 is 1.5 μm thicker than d6. Electrode material is evaporated (electron beam evaporation, thermal evaporation or sputtering) on ​​the cladding 16 material to obtain an electrode material layer 17, as shown in FIG. Fig.16 As shown, its thickness d8 is 500nm. The front view after spin coating the cladding material 16 and evaporating the electrode material is as follows Fig.17 shown.

[0110] A photoresist layer 18 is spin-coated on the electrode material layer 17 (spin-coating speed 5000 rpm, time 60 s) to obtain an electrode material mask layer with a thickness of 2 μm. Fig.18 Then, a mask plate with an electrode pattern is covered on the photoresist (or the electrode pattern is introduced using a maskless photolithography machine and the plate is aligned on the maskless photolithography machine).

[0111] In this embodiment, the middle strip structure of the mask with the electrode pattern has a width of x7 of 3μm and a length of L6 of 1mm, and ensures that the straight electrode part is completely parallel and covers one arm of MZ. The electrode pin adopts a same-side structure, and two identical pins extend outward from the two end points of the straight electrode structure. The difference x8 between its pin structure and the strip structure in the x direction is 2μm, and the electrode pin is a rectangle with a length L7 of 5μm and a width x9 of 15μm in the z direction. The schematic diagram after covering is as follows Fig.19Then, photolithography (photolithography exposure intensity 25mW / cm2, time 8s), after photolithography, the mask is removed, the photoresist material layer and the electrode layer are etched with a 5‰ sodium hydroxide aqueous solution, and acetone is used to remove the photoresist layer on the electrode to obtain an electrode pattern layer 20, as shown in the schematic diagram. Fig.21 shown.

[0112] In this embodiment, a dicing machine or a blade is used to directly cut the input and output straight waveguides (a) along the projection direction perpendicular to the input and output straight waveguides (a) and L a The input waveguides of the two segments intersect vertically, and the optical waveguide thermo-optic switch with heterogeneous arms and input and output interfaces 21 is obtained. Finally, the optical fiber, photodetector, signal generator and oscilloscope are connected for testing. Fig. 22 As shown, the feasibility of the results is verified.

[0113] In summary, in the scheme of the hybrid integrated optical waveguide thermo-optical switch of the lateral coupling of the polymer waveguide and the silica waveguide of the present invention, the lateral coupling mode between the polymer waveguide and the silica waveguide is conducive to realizing efficient optical signal transmission and modulation. Compared with the direct docking coupling mode, the refractive index adaptability of the present invention is wider and the light field leakage loss is lower.

[0114] Since polymer materials and silica materials each have advantages in cost and manufacturing process, polymer materials are usually low in cost, simple to manufacture, and suitable for large-scale production; while silica materials have the characteristics of low transmission loss and low coupling loss. The combination of the two can achieve low-cost and high-performance devices.

[0115] The present invention can design a device with low power loss and small size by combining the high thermo-optic coefficient of polymer and the low transmission loss of silicon dioxide.

[0116] The design of polymer waveguide height lower than silica waveguide helps to reduce light scattering and loss between waveguides and improve the overall performance of the device. Compared with the traditional asymmetric MZ with two arms of the same material, the two arms of the present invention are made of different materials, and heating electrodes are placed on the polymer arms. The high thermo-optical coefficient of the polymer is used to reduce the power consumption of the switch. The two arms are of different heights. The large size of the silica waveguide reduces the coupling loss with the optical fiber, and the polymer waveguide reduces the height, which reduces the time required for the heat dissipation of the thermo-optical switch and the total amount of heat, thereby further reducing the switching time and power consumption.

[0117] The present invention deposits an electrode material layer on the polymer cladding and arranges an electrode pattern layer, which can achieve precise modulation and control. This design helps to optimize the modulation efficiency and response speed, while reducing the interference of the electrode to the optical signal. In addition, the polymer cladding not only protects the waveguide structure, but also further improves the performance of the device through its material properties. For example, some polymer materials may have a low refractive index or good thermal conductivity, which helps to reduce the insertion loss of the device and improve thermal stability.

[0118] The present invention can reduce the power consumption of the device by optimizing the waveguide size and electrode design. This is of great significance for large-scale integration and practical applications. The present invention combines the high thermo-optical coefficient of the polymer and the optimization of the electrode design to achieve a faster response speed and meet the requirements of high-speed optical communication systems. The present invention is made of mature materials and processes, which helps to improve the reliability and stability of the device and reduce maintenance costs.

[0119] The above-mentioned embodiments are only preferred embodiments of the present invention and cannot be used to limit the scope of protection of the present invention. Any non-substantial changes and substitutions made by technicians in this field on the basis of the present invention shall fall within the scope of protection required by the present invention.

Claims

1. A MZ optical waveguide thermo-optical switch with a polymer-silicon dioxide heterogeneous modulation arm, characterized in that: include: Substrate chip; An MZ optical waveguide structure layer is formed on the substrate chip, wherein the MZ optical waveguide structure layer includes a polymer waveguide and a high-refractive-index silica waveguide, and both are located on the same plane; wherein the high-refractive-index silica waveguide is obtained by etching the high-refractive-index silica layer in the substrate chip; The polymer waveguide and the high refractive index silica waveguide are coupled sideways; The height of the polymer waveguide is lower than that of the high refractive index silica waveguide; A polymer cladding layer is spin-coated on the MZ optical waveguide structure layer, an electrode layer is disposed on the polymer cladding layer, and the electrode layer is located directly above the polymer waveguide in the MZ optical waveguide structure.

2. The MZ optical waveguide thermo-optic switch according to claim 1, characterized in that: The substrate chip includes, from top to bottom: A high refractive index doped silicon dioxide layer, the refractive index of which is 1.455 to 1.48 and the thickness of which is 2 to 10 μm; A low-refractive-index silicon dioxide layer, whose refractive index is 1.44 to 1.45 and whose thickness is 3 to 15 μm; The bottom layer is a silicon-based silicon dioxide layer with a thickness of 100 to 1000 μm.

3. The MZ optical waveguide thermo-optic switch according to claim 1, characterized in that: The steps of preparing the MZ optical waveguide structure layer include: Providing a high refractive index doped silicon dioxide layer as the silicon dioxide waveguide part of the MZ optical waveguide structure layer, wherein the refractive index thereof is 1.455 to 1.48 and the thickness thereof is 2 to 10 μm; Select a substrate chip that is projected as a rectangle in the vertical direction; Evaporating a mask layer on a substrate chip to form a mask layer for a silicon dioxide waveguide; Spin-coating photoresist to form a photoresist film layer with a thickness of 0.1 to 5 μm; A photoresist mask layer is obtained by introducing a pattern on the photoresist film layer using a photolithography plate or a maskless photolithography machine, performing photolithography and then developing the pattern.

4. The MZ optical waveguide thermo-optic switch according to claim 1, characterized in that: The two MZ structures of the MZ pattern reticle include: The length L of the input and output area (a) a A straight waveguide of 0.02 to 5 mm; The length L of the input and output Y branch region (b) b , which is the length of the Y branch region along the waveguide propagation direction; When a photolithography plate is used for photolithography, the photolithography plate is a straight waveguide pattern, the waveguide length L2 is a rectangle of 10100 to 50100 μm, the waveguide structure width x2 is 3 to 10 μm, the long side of the waveguide is parallel to the long side of the substrate chip, the spacing between the long side of the waveguide and the long side of the substrate chip in the x direction is 2 to 50 μm, and it intersects the two short sides perpendicularly in the z direction, that is, the length in the z direction is greater than the length of the long side of the substrate chip.

5. The MZ optical waveguide thermo-optic switch according to claim 3, characterized in that: When manufacturing a silicon dioxide waveguide, a mask etching agent is used to etch the mask layer to obtain a waveguide mask pattern; The waveguide core layer is obtained by plasma etching or ICP etching, and the etching depth is the depth of d1; The photoresist mask layer is removed with a corresponding photoresist developer, and the waveguide mask pattern is removed with a corresponding solution to obtain a silicon dioxide waveguide chip.

6. The MZ optical waveguide thermo-optic switch according to claim 5, characterized in that: Spin coating the waveguide core material on the silicon dioxide waveguide chip to obtain a polymer waveguide core material film, wherein the film thickness d6 is 1 to 10 μm, which is about half of the waveguide layer thickness d3; An MZ pattern photolithography plate is used for photolithography or a maskless photolithography machine is used to import a graphic file consistent with the MZ pattern photolithography plate, and a polymer waveguide is obtained after development, thereby forming an MZ optical waveguide structure layer.

7. The MZ optical waveguide thermo-optic switch according to claim 6, characterized in that: When the waveguide core material is spin-coated on the silicon dioxide waveguide chip, the spin-coating speed is 2500-10000 rpm, the spin-coating time is 30-300 s, and after curing, a polymer waveguide core material film is obtained, and the film thickness d6 is 1-10 μm, which is about half of the waveguide layer thickness d3.

8. The MZ optical waveguide thermo-optic switch according to claim 7, characterized in that: The thickness d7 of the polymer cladding is 1.5-5 μm thicker than d6, and the thickness d8 of the electrode layer is 20-500 nm; Before forming the electrode pattern layer, a photoresist layer is spin-coated on the electrode layer to obtain an electrode material mask layer with a thickness of 0.2-2 μm, and then a mask plate with an electrode pattern is covered on the photoresist layer.

9. The MZ optical waveguide thermo-optic switch according to claim 8, characterized in that: The middle strip structure of the mask with the electrode pattern has a width x7 of 3 to 15 μm and a length L6 of 0.1 to 1 mm, and ensures that the straight electrode part is completely parallel and covers one arm of the MZ optical waveguide structure; The electrode pin adopts a same-side structure, and two identical pins extend outward from the two ends of the straight electrode structure to the outside of the MZ optical waveguide structure. The difference x8 between the pin structure and the strip structure in the x direction is 1 to 2 μm. The electrode pin is a rectangle with a length L7 of 5 to 15 μm and a width x9 of 5 to 15 μm in the z direction. After photolithography, the mask is removed, and the photoresist layer and the electrode material layer are etched with an aqueous sodium hydroxide solution (mass ratio 4-6‰), and the photoresist layer on the electrode is removed with acetone or a corresponding photoresist stripper to obtain an electrode pattern layer.

10. The MZ optical waveguide thermo-optic switch according to claim 9, characterized in that: The MZ optical waveguide structure after obtaining the electrode pattern layer is directly cut along the projection direction perpendicular to the input and output straight waveguides and connected to L a The input waveguide segments intersect vertically, thus obtaining a double-arm heterogeneous optical waveguide thermo-optic switch, which is finally connected to an optical fiber, a photodetector, a signal generator and an oscilloscope for testing.