Safety and durability evaluation method for I-shaped steel-concrete combined continuous beam bridge
By calculating the failure probability and reliability degradation rate of the bridge system under the ultimate bearing capacity state, the problem of inaccurate assessment of safety and durability of I-steel-concrete composite continuous beam bridge in the prior art is solved, and the bridge quality is achieved Accurate screening and follow-up construction guidance.
Patent Information
- Application Number
- CN202411145177.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-08-20
AI Technical Summary
The prior art is difficult to accurately and objectively evaluate the safety and durability of I-concrete composite continuous beam bridges, resulting in insufficient construction quality assessment, affecting project quality and subsequent maintenance.
By calculating the failure probability and reliability degradation rate of the bridge system under the load capacity limit state, functional functions such as bending load capacity formula, shear load capacity formula and mid-carrying position bending load capacity formula, combined with the Monte Carlo method and qualitative parameters to evaluate the safety and durability of the bridge.
It realizes accurate and intuitive characterization of the safety and durability of I-concrete composite continuous beam bridges, and can screen out bridges with good construction quality, providing effective guidance for subsequent construction.
Smart Images

Figure QLYQS_9 
Figure QLYQS_16 
Figure QLYQS_19
Abstract
Description
Technical Field
[0001] The present invention relates to the field of bridge system reliability evaluation, and more specifically, to a safety durability evaluation method for an I-beam-concrete composite continuous beam bridge. Background Art
[0002] Reliability refers to the ability of a product to complete its intended function within a specified time and under specified conditions. It includes the safety and durability of the structure. When measured by probability, it is called reliability. System safety can be reflected by the probability of failure. At present, for I-beam-concrete composite continuous beam bridges, a target reliability value (the target reliability is converted from the failure probability) is pre-designed before the construction plan is designed. According to the target reliability value, some parameter values required in the construction, such as the cross-sectional size of the steel beam, are calculated. After the construction is completed, it is necessary to evaluate the safety and durability of these bridges to judge the quality of the project and provide guidance for subsequent construction and maintenance. However, in actual construction, sometimes hundreds of bridges are constructed on the route of the same highway project. In order to determine which I-beam-concrete composite continuous beam bridge has better safety and durability, it is usually necessary to conduct a safety evaluation on each constructed bridge. At present, there are several methods for evaluating the safety of bridges, such as experimental testing and manual inspection and scoring. The experimental testing method usually involves arranging vehicles with a certain load to travel on the bridge before the bridge is opened to traffic, and detecting the stress and deformation of the bridge to comprehensively judge the safety of the bridge; the manual inspection and scoring method usually involves manually inspecting and scoring the constructed bridge, and finally conducting a comprehensive analysis of the scores obtained to judge the safety and durability of the bridge. However, both the experimental testing method and the manual inspection and scoring method have the problems of being not objective, not accurate, time-consuming, labor-intensive, and material-intensive, and are greatly affected by the subjective experience of the scorers. Therefore, there is an urgent need for an evaluation method that is more objective, can accurately and intuitively characterize the safety and durability of I-beam-concrete composite continuous beam bridges, and achieve a comprehensive measurement of bridge safety and durability. For multiple bridges of the same type, bridges with better construction quality can be screened out, providing effective guidance for the subsequent construction and maintenance of this type of bridge. Summary of the invention
[0003] An object of the present invention is to solve at least the above-mentioned problems and provide a safety and durability evaluation method for an I-beam-concrete composite continuous beam bridge, which can more accurately and intuitively characterize the safety and durability of the I-beam-concrete composite continuous beam bridge, and realize a comprehensive measurement of the safety and durability of the bridge. For multiple bridges of the same type, bridges with better construction quality can be screened out. The construction plans of the screened bridges with better quality are helpful for the learning of subsequent construction personnel, and also provide effective guidance for the subsequent construction of bridges of the same type.
[0004] In order to achieve these purposes and other advantages according to the present invention, a safety durability evaluation method for an I-beam-concrete composite continuous beam bridge is provided, which evaluates the safety of the bridge under the ultimate bearing capacity state by the failure probability of the bridge system under the ultimate bearing capacity state, and evaluates the durability of the bridge under the ultimate bearing capacity state by the reliability degradation rate of the bridge system under the ultimate bearing capacity state.
[0005] Preferably, the safety evaluation of the bridge under the ultimate bearing capacity state specifically includes the following steps: S1. Determine the function: The functional functions used to calculate the failure probability of the bridge system under the ultimate bearing capacity state include the bending bearing capacity formula Z1, the shear bearing capacity formula Z2, and the bending bearing capacity formula Z3 at the middle support position; The specific formula Z1 is: Z1=M R -M S ; Among them, M R The calculation formula is: When the plastic neutral axis is within the concrete panel section, , when the plastic neutral axis is within the steel beam section, ;M S The calculation formula is: ; The specific formula Z2 is: Z2=V R -V S ; Among them, V R The calculation formula is: , V S The calculation formula is: ; Formula Z3 is specifically: ; Among them, M R,0 The calculation formula is: , The calculation formula is: ; In the formulas Z1 to Z3, the parameters involved are divided into nominal value parameters, design value parameters, random variable parameters, and qualitative parameters η c , the qualitative parameter η c Characterizes the closeness between the appearance quality of the bridge structure concrete and the acceptance standard. The closer to the acceptance standard, the better the η c The closer the value of is to 1; The nominal value parameters are characterized as follows: f cd is the compressive strength of concrete material, f d is the tensile strength of steel, f s is the tensile strength of the longitudinal reinforcement in the concrete panel, f vdis the shear strength of steel; The design value parameters are specifically characterized as follows: k is the fitting coefficient considering the slip effect; A c is the cross-sectional area of the concrete bridge deck; y1 is the distance from the centroid of the concrete bridge deck section in the compression zone to the centroid of the steel beam section in the tension zone; A sc is the cross-sectional area of the steel beam in compression; y2 is the distance from the centroid of the steel beam in compression to the centroid of the steel beam in tension; A r is the cross-sectional area of the longitudinal reinforcement in the concrete bridge deck on the upper side of the plastic neutral axis; y4 is the distance from the centroid of the cross section of the longitudinal reinforcement in the concrete bridge deck to the centroid of the cross section of the tensile zone of the steel beam; A cc is the area of the concrete bridge deck on the upper side of the plastic neutral axis; g is the constant load; L is the length of a single span of the bridge; 1+μ is the impact coefficient; h w is the web height of the steel beam; t w A is the thickness of the steel beam web; st h is the tensile area of the I-beam; s A is the height of the tension zone; r h is the cross-sectional area of the longitudinal reinforcement in the concrete bridge deck above the plastic neutral axis; c is the height of the compression zone; x is the distance between the neutral axis of the cross section and the top surface of the I-beam; The random variable parameters include structural uncertainty parameters and load parameters. The structural uncertainty parameters are characterized as follows: γ cf Characterizes the degree of deviation between the compressive strength value of concrete material and the nominal value of the compressive strength of concrete material, γ cf = compressive strength of concrete material / f cd ; γ s Characterizes the deviation between the tensile strength of steel and the nominal value of the tensile strength of steel, γ s = steel tensile strength value / f d ; γ ds Characterizes the degree of deviation between the cross-sectional dimension of the steel beam and the nominal value of the cross-sectional dimension of the steel beam, γ ds = Steel beam cross-section size value / design value of steel beam cross-section size; γ dc Characterizes the degree of deviation between the cross-sectional size of the bridge concrete panel and the design value of the cross-sectional size of the bridge concrete panel, γ dc = Bridge concrete panel cross-sectional dimension value / bridge concrete panel cross-sectional dimension design value; γ r Characterizes the deviation between the tensile strength of steel bars and the nominal value of the tensile strength of steel bars, γ r = tensile strength of steel bar / f s ; The load parameters are characterized as follows: q is the uniform lane load; P k For concentrated lane loads; S2. Calculation of failure probability of bridge system under ultimate bearing capacity state: The above random variable parameters are used as sampling objects, and formulas Z1, Z2, and Z3 are used as function functions to calculate the values of each function. When any function value is less than or equal to 0, it indicates that the bridge system has failed, otherwise the bridge system is valid. Repeat the sampling N times, and count the number of failures n, then the failure probability is n / N. S3. Safety evaluation of bridge system under the ultimate bearing capacity state: Comparing the failure probabilities of any two I-beam-concrete composite continuous beam bridges under the ultimate bearing capacity state, the lower the failure probability, the higher the safety of the bridge under the ultimate bearing capacity state.
[0006] Preferably, the implementation of step S2 is specifically as follows: obtaining the statistical characteristics of the uncertainty parameters at the structural level, sampling using the Monte Carlo method based on MATLAB, and calculating the system failure probability under the ultimate state of the bridge bearing capacity; wherein: γ cf The statistical characteristics of γ are obtained as follows: taking multiple concrete material compressive strength values measured on site as statistical objects, the mean μ1 and standard deviation σ1 of the concrete material compressive strength are calculated, and then γ is obtained. cf The normal distribution statistical characteristics of N (μ1 / f cd ,σ1 / f cd ); γ ds The specific acquisition of the statistical characteristics of is as follows: taking multiple steel beam cross-sectional dimensions measured on site as statistical objects, calculating μ2 and standard deviation σ2 of the steel beam cross-sectional dimensions, and then obtaining γ ds The normal distribution statistical characteristics of N (μ2 / design value of steel beam cross-section size, σ2 / design value of steel beam cross-section size); γ dc The specific acquisition of the statistical characteristics of is as follows: taking the cross-sectional dimensions of multiple bridge concrete panels measured on site as statistical objects, the cross-sectional dimensions of the bridge concrete panels μ3 and the standard deviation σ3 are calculated, and then γ is obtained. dc The normal distribution statistical characteristics of N (μ3 / design value of the cross-sectional size of the bridge concrete panel, σ3 / design value of the cross-sectional size of the bridge concrete panel); γ s The statistical characteristics of are obtained as follows: the tensile strength values of multiple steels measured on site are used as statistical objects, the mean μ4 and standard deviation σ4 of the tensile strength of the steels are calculated, and then γ s The normal distribution statistical characteristics of N (μ4 / fd ,σ4 / f d ); γ r The statistical characteristics of γ are obtained as follows: the tensile strength values of multiple steel bars measured on site are used as statistical objects, the mean μ5 and standard deviation σ5 of the tensile strength of the steel bars are calculated, and then γ is obtained. r The normal distribution statistical characteristics of N (μ5 / f s ,σ5 / f s ).
[0007] Preferably, the qualitative parameter η c The specific value of is as follows: According to the qualitative description of the appearance of the bridge concrete structure in the design specification, the quantitative description of the bridge assessment standard is determined. The quantitative description includes five scales, as follows: Scale 1: intact; under this scale, η c The value range is 0.95~1.0; Scale 2: The cumulative area of network cracks is ≤ 20% of the component area, and the area of a single crack is ≤ 1.0m 2 , or the length of the main beam crack is ≤ 1 / 3 of the cross-sectional size; under this scale, η c The value range is 0.9~0.95; Scale 3: The cumulative area of network cracks is ≤ 20% of the component area, and the area of a single crack is > 1.0m 2 , or the length of the main beam crack is > 1 / 3 of the cross-sectional size and ≤ 2 / 3 of the cross-sectional size; under this scale, η c The value range is 0.85~0.90; Scale 4: The length of the main beam crack is greater than 2 / 3 of the cross-sectional size, and the spacing is less than 20 cm. c The value range is 0.80~0.850; Scale 5: The width of the cracks in the main beam is >1.0mm, and the spacing is ≤10cm; under this scale, η c The value range is below 0.80.
[0008] Preferably, the safety of the bridge under the serviceability limit state is evaluated by the failure probability of the bridge system under the serviceability limit state, which specifically includes the following steps: A1. Determine the function: The functional functions used to calculate the failure probability of the bridge system under the normal serviceability limit state include the maximum crack width formula Z4 and the mid-span deflection formula Z5; Formula Z4 is specifically: , ; Formula Z5 is specifically: ; Among them, f1 is the short-term deflection, f2 is the long-term deflection; the calculation formula of f1 is: , , , ;in, , , , , , , ; The calculation formula of f2 is as follows: ,in, , ; In formula Z4 and formula Z5, the parameters are represented as follows: γ is the uncertainty coefficient of the calculation model; α cr is the stress characteristic coefficient of the component; f t is the tensile strength of steel fiber concrete; ρ te is the effective reinforcement ratio of the longitudinal tensile reinforcement; rs is the stress of the longitudinal tensile reinforcement at the crack section of the reinforced concrete member; l a is the average spacing of transverse reinforcement; f ry is the yield strength of non-prestressed steel bars in the composite beam; f py A is the yield strength of the prestressed steel bars in the composite beam; s is the cross-sectional area of the steel beam; f y is the yield strength of the steel beam; A P is the cross-sectional area of the external prestressed tendons; f allow is the allowable deflection; B is the converted section stiffness of the composite beam; z1 is the distance from the centroid of the end prestressed tendon to the centroid of the converted section of the composite beam; l 1 is the projection length of the first section of prestressed tendons in the local coordinate system; θ1 is the angle between the first section of prestressed tendons and the horizontal line; θ2 is the angle between the second section of prestressed tendons and the horizontal line; B s is the converted section stiffness of the composite beam considering slip; m is the ratio of the distance from the beam end to the single point concentrated load loading point to the calculated span of the composite beam; r is the shear connection degree; K L h is the shear stiffness of the shear connector per unit length; sc E is the distance from the centroid of the steel beam section to the centroid of the concrete section; c is the elastic modulus of concrete; E s is the elastic modulus of steel; I c is the moment of inertia of the concrete section; I s is the moment of inertia of the steel beam section; A cis the cross-sectional area of the concrete bridge deck; A s is the cross-sectional area of the steel beam; n s is the number of rows of studs or perforated plate connectors; k is the shear stiffness of a single shear connector; p is the spacing between connectors; σ e is the effective tension prestress of the prestressed tendons; λ(t) is a coefficient related to time; k1 is a coefficient related to the average stress of the concrete bridge deck; is the average stress of the concrete bridge deck; T p is the effective pretension of the prestressed tendons; A0 is the cross-sectional area of the composite beam after the cross-sectional conversion; I0 is the moment of inertia of the composite beam after the cross-sectional conversion; e is the eccentricity of the prestressing force; A2. Calculation of failure probability of bridge system under serviceability limit state: With ρ te 、f t , A r 、f ry , A P 、f py , A s 、f y 、E s 、E c , A c , A s , A0, q, P k The sampling object is the formula Z4 and Z5 as the function function, and the value of each function function is calculated. When any function function value is less than or equal to 0, it indicates that the bridge system is invalid, otherwise the bridge system is valid; repeat the sampling M times, count the number of failures m, and the failure probability is m / M; A3. Safety evaluation of bridge system under normal use limit state: Comparing the failure probabilities of any two I-beam-concrete composite continuous beam bridges under the serviceability limit state, the lower the failure probability, the higher the safety of the bridge under the serviceability limit state.
[0009] Preferably, the specific steps for evaluating the durability of the bridge system under the ultimate bearing capacity state are as follows: B1. Determine the calculation formula: The calculation formula for the reliability degradation rate of the bridge under the ultimate bearing capacity state is: ; The bearing capacity limit state is one of the bending bearing capacity limit state, the shear bearing capacity limit state, and the bending bearing capacity limit state at the middle support position; α1 represents the reliability degradation rate of the bridge under the bearing capacity limit state, μ R01 Characterizes the mean resistance of the bridge structure at the initial moment under the ultimate bearing capacity state; σ R01 Characterizes the standard deviation of the resistance of the bridge structure at the initial moment under the ultimate bearing capacity state; σS1 represents the standard deviation of the load effect of the bridge structure under the ultimate bearing capacity state; λ´ represents the corrosion rate of the steel web; γ0 represents the design thickness of the steel web; B2. Calculation of reliability degradation rate of bridge under ultimate bearing capacity state: Take λ´ and γ0 as sampling objects, calculate the α1 value, repeat the sampling P times, calculate the mean of the α1 values of P samplings, and obtain the reliability degradation rate under the corresponding bearing capacity limit state; B3. Evaluation of bridge durability under the ultimate bearing capacity state: Compare the reliability degradation rates of any two I-beam-concrete composite continuous beam bridges under the corresponding ultimate bearing capacity state. The lower the reliability degradation rate, the higher the durability of the bridge under the ultimate bearing capacity state.
[0010] Preferably, it also includes the evaluation of the durability of the bridge system under the normal service limit state, which specifically includes the following steps: C1. Determine the calculation formula: The calculation formula for the reliability degradation rate of the bridge under the normal service limit state is: ; Wherein, the normal service limit state is one of the concrete cracking limit state in the negative bending moment zone and the mid-span deflection limit state; α2 represents the reliability degradation rate of the bridge under the normal service limit state; When the serviceability limit state is the concrete cracking limit state in the negative moment zone, μ R02 Characterizes the maximum crack width limit, σ R02 is 0, σ S2 Characterizes the standard deviation of the maximum crack width; When the serviceability limit state is the mid-span deflection limit state, μ R02 Characterizes the deflection limit of the bridge mid-span, σ R02 is 0, σ S2 Characterizes the standard deviation of the actual deflection of the bridge at mid-span; C2. Calculation of reliability degradation rate of bridges under serviceability limit state: Take λ´ and γ0 as sampling objects, calculate the α2 value, repeat the sampling Q times, calculate the mean of the α2 values of Q samplings, and obtain the required reliability degradation rate; C3. Evaluation of bridge durability under normal use limit state: Compare the reliability degradation rates of any two I-beam-concrete composite continuous beam bridges under the corresponding normal service limit state. The lower the reliability degradation rate, the higher the durability of the bridge under the normal service limit state.
[0011] Preferably, the cross-sectional dimensions in the steel beam cross-sectional dimension values are derived from any one of the thickness of the upper flange plate, the thickness of the lower flange plate, the web thickness, the web width, and the width of the steel beam; and the cross-sectional dimensions in the bridge concrete panel cross-sectional dimension values are derived from any one of the length, width, and height of the concrete panel.
[0012] The present invention has at least the following beneficial effects: For the safety evaluation of I-beam-concrete composite continuous beam bridges, uncertainty parameters and qualitative parameters reflecting construction influencing factors are introduced on the basis of the original formula of the functional function of each limit state, and the functional function of each limit state is sampled and calculated using a series model to obtain the failure probability. The lower the failure probability, the higher the safety of the bridge system. Among them, the functional function under the bearing capacity limit state includes the bending bearing capacity formula, the shear bearing capacity formula and the bending bearing capacity formula at the middle support position, and the functional function under the normal use limit state includes the maximum crack width calculation formula and the mid-span underwinding formula. For the durability evaluation of I-beam-concrete composite continuous beam bridges, the reliability degradation rate of the bridge is calculated based on the calculation formula after introducing uncertainty parameters and qualitative parameters. The lower the reliability degradation rate, the higher the durability of the bridge. Overall, a safety and durability evaluation method for I-beam-concrete composite continuous beam bridges is provided, which can characterize the safety and durability of I-beam-concrete composite continuous beam bridges more accurately and intuitively, and realize the comprehensive measurement of bridge safety and durability. For multiple bridges of the same type, bridges with better construction quality can be screened out. The construction plans of the screened bridges with better quality are helpful for the learning of subsequent construction personnel, and also provide effective guidance for the subsequent construction of bridges of the same type.
[0013] Other advantages, objectives and features of the present invention will be embodied in part through the following description, and in part will be understood by those skilled in the art through study and practice of the present invention. DETAILED DESCRIPTION
[0014] The present invention is further described in detail below in conjunction with embodiments so that those skilled in the art can implement the invention with reference to the description.
[0015] The present invention provides a safety durability evaluation method for an I-beam-concrete composite continuous beam bridge, which is designed by the inventor based on the following design principles: The inventors have integrated a large amount of research data and construction experience, considered the impact of various factors in the construction process on the safety and durability of bridges, and based on the five principles of "leadership, representativeness, comparability, accessibility, and timeliness", considered the two dimensions of safety and durability of I-beam-concrete composite continuous beam bridges, and preliminarily formulated a set of reliability evaluation indicators for the safety and durability of highway concrete beam bridges from multiple levels of bridge structure-related data-structural materials-component performance-structural system. Through expert survey method and hierarchical analysis method, some factors with relatively small influence were eliminated, and the final reliability evaluation indicator set was screened out. According to the final reliability evaluation indicator set, a series of uncertainty factors (i.e., the structural level uncertainty parameters mentioned below) and qualitative parameters (concrete appearance quality) that characterize various influencing factors in the construction process are formed. Combined with the inventors' theoretical research and work practice, the above uncertainty factors and qualitative parameters are introduced into GB 50917-2013. The calculation formulas for bearing capacity and normal service limit state in the steel-concrete composite bridge design specification are intended to characterize the impact of various factors on the bridge construction quality during the construction process, and ultimately characterize the safety and durability of the bridge based on the calculated failure probability and reliability degradation rate. Among them, the failure probability is converted to obtain the reliability value, and the reliability value is compared with the target reliability value set in the construction design plan, which can also characterize the gap between the construction quality and the target construction quality. See below for more details.
[0016] The present invention provides a safety durability evaluation method for an I-beam-concrete composite continuous beam bridge, which evaluates the safety of the bridge under the ultimate bearing capacity state by the failure probability of the bridge system under the ultimate bearing capacity state, and evaluates the durability of the bridge under the ultimate bearing capacity state by the reliability degradation rate of the bridge system under the ultimate bearing capacity state, wherein the safety evaluation of the bridge under the ultimate bearing capacity state specifically includes the following steps: S1. Determine the function: The functional functions used to calculate the failure probability of the bridge system under the ultimate bearing capacity state include the bending bearing capacity formula Z1, the shear bearing capacity formula Z2, and the bending bearing capacity formula Z3 at the middle support position; The specific formula Z1 is: Z1=M R -M S ; Among them, M R The calculation formula is: When the plastic neutral axis is within the concrete panel section, , when the plastic neutral axis is within the steel beam section, ;M S The calculation formula is: ; The specific formula Z2 is: Z2=V R -V S ; Among them, VR The calculation formula is: , V S The calculation formula is: ; Formula Z3 is specifically: ; Among them, M R,0 The calculation formula is: , The calculation formula is: ; In the formulas Z1 to Z3, the parameters involved are divided into nominal value parameters, design value parameters, random variable parameters, and qualitative parameters η c , the qualitative parameter η c Characterizes the closeness between the appearance quality of the bridge structure concrete and the acceptance standard. The closer to the acceptance standard, the better the η c The closer the value of is to 1, the c It is a constant obtained after scoring and has no unit. The nominal value parameters are characterized as follows: f cd is the compressive strength of concrete material, unit: MPa; f d is the tensile strength of steel, unit: MPa; f s is the tensile strength of the longitudinal reinforcement in the concrete panel, in MPa; f vd is the shear strength of steel, in MPa; The design value parameters are specifically characterized as follows: k is the fitting coefficient considering the slip effect, without unit; A c is the cross-sectional area of the concrete bridge deck, in mm; y1 is the distance from the centroid of the concrete bridge deck section in compression to the centroid of the steel beam section in tension, in mm; A sc is the cross-sectional area of the steel beam in compression zone, in mm; y2 is the distance from the centroid of the steel beam in compression zone to the centroid of the steel beam in tension zone, in mm; A r is the cross-sectional area of the longitudinal reinforcement in the concrete bridge deck above the plastic neutral axis, in mm 2 ; y4 is the distance from the centroid of the cross section of the longitudinal reinforcement in the concrete bridge deck to the centroid of the cross section of the steel beam in the tension zone, unit: mm; A cc is the area of the concrete bridge deck on the upper side of the plastic neutral axis, in mm 2 ; g is the constant load, unit is kN / m; L is the length of a single span of the bridge, unit is m; 1+μ is the impact coefficient, unitless; h w is the web height of the steel beam, in mm; t w A is the thickness of the web of the steel beam, in mm; st is the tensile area of the I-beam, in mm 2 ;hs A is the height of the tension zone, in mm; r is the cross-sectional area of the longitudinal reinforcement in the concrete bridge deck above the plastic neutral axis, in mm 2 ;h c is the height of the compression zone, in mm; x is the distance between the neutral axis of the cross section and the top surface of the I-beam, in mm; The random variable parameters include structural uncertainty parameters and load parameters. The structural uncertainty parameters are characterized as follows: γ cf Characterizes the degree of deviation between the compressive strength value of concrete material and the nominal value of the compressive strength of concrete material, γ cf = compressive strength of concrete material / f cd ; γ s Characterizes the deviation between the tensile strength of steel and the nominal value of the tensile strength of steel, γ s = steel tensile strength value / f d ; γ ds Characterizes the degree of deviation between the cross-sectional dimension of the steel beam and the nominal value of the cross-sectional dimension of the steel beam, γ ds = Steel beam cross-section size value / design value of steel beam cross-section size; γ dc Characterizes the degree of deviation between the cross-sectional size of the bridge concrete panel and the design value of the cross-sectional size of the bridge concrete panel, γ dc = Bridge concrete panel cross-sectional dimension value / bridge concrete panel cross-sectional dimension design value; γ r Characterizes the deviation between the tensile strength of steel bars and the nominal value of the tensile strength of steel bars, γ r = tensile strength of steel bar / f s ; The load parameters are characterized as follows: q is the uniform lane load, unit kN / m; P k is the concentrated lane load, in kN / m; S2. Calculation of failure probability of bridge system under ultimate bearing capacity state: The above random variable parameters are used as sampling objects, and formulas Z1, Z2, and Z3 are used as function functions to calculate the values of each function. When any function value is less than or equal to 0, it indicates that the bridge system has failed, otherwise the bridge system is valid. Repeat the sampling N times, and count the number of failures n, then the failure probability is n / N. S3. Safety evaluation of bridge system under the ultimate bearing capacity state: Compare the failure probabilities of any two I-beam-concrete composite continuous beam bridges under the ultimate bearing capacity state. The lower the failure probability, the higher the safety of the bridge under the ultimate bearing capacity state. In the above technical solution, the ultimate bearing capacity state includes the ultimate bending bearing capacity state, the ultimate shear bearing capacity state, and the ultimate bending bearing capacity state at the middle support position. Among them, the function function under the ultimate bending bearing capacity state is Z1. In formula Z1, M R is the bending moment that the bridge can bear, M S is the mid-span bending moment. When the plastic neutral axis is within the concrete panel section and when the plastic neutral axis is within the steel beam section, these two states are the boundary positions of the tension zone and the compression zone in the composite beam under the load. The calculation formula is different according to the different positions. In actual use, after the load is determined, it can be determined which of the above two states the bridge is in. These are all existing technologies well known to those skilled in the art and will not be elaborated here. The functional function of the ultimate limit state of shear bearing capacity is Z2. In the formula Z2, V R is the shear bearing capacity of the bridge, V S is the maximum shear force; the function function of the ultimate state of bending bearing capacity at the middle support position is Z3. In formula Z3, is the bending moment that the bridge support can bear, is the bending moment at the bridge support under load; In the above formulas Z1~Z3, the parameters involved are divided into nominal value parameters, design value parameters, random variable parameters and qualitative parameters. The nominal value parameters and design value parameters are various parameters inherent in the original formula in the steel-concrete composite continuous beam bridge design specification. The nominal value parameters are usually various mechanical performance parameters, such as the compressive strength of concrete materials, the compressive strength of steel materials, etc. The design value parameters are usually other parameters such as section size, coefficient, etc. The representation and units of the design value parameters and nominal value parameters are all recorded in the existing GB 50917-2013 Steel-Concrete Composite Bridge Design Specification. For more details, please refer to the design specification and other existing materials; The random variable parameters are divided into structural uncertainty parameters and load parameters. Among them, the structural uncertainty parameters and qualitative parameters η c are parameters screened by the inventor through expert investigation, hierarchical analysis, theoretical research and practical experience. They characterize the influence of various factors such as construction materials, construction templates, labor and other factors on the construction quality during the construction process. They can be regarded as influence coefficients, which comprehensively consider the degree of deviation between the overall quality of the bridge and the expected quality caused by various factors during the construction process. Among them, the qualitative parameter η c Characterizes the closeness between the appearance quality of the bridge structure concrete and the acceptance standard. The closer to the acceptance standard, the better the η c The closer the value is to 1, that is, the value of 1 is taken as the standard. The closer it is to the standard, the better the appearance of the concrete of the bridge structure is. The acceptance standard can be set according to the relevant design specifications. The structural uncertainty parameters include: γ, which represents the degree of deviation between the concrete material compressive strength value and the nominal value of the concrete material compressive strength; cf , γ, which characterizes the deviation between the tensile strength of steel and the nominal value of the tensile strength of steel s , γ, which represents the degree of deviation between the cross-sectional dimension of the steel beam and the nominal value of the cross-sectional dimension of the steel beam ds , γ, which represents the degree of deviation between the cross-sectional dimension of the bridge concrete panel and the design value of the cross-sectional dimension of the bridge concrete panel dc , γ, which characterizes the deviation between the tensile strength of the steel bar and the nominal value of the tensile strength of the steel bar r , where γ ds Characterizes the degree of deviation between the cross-sectional dimension of the steel beam and the nominal value of the cross-sectional dimension of the steel beam. Here, the cross-sectional dimension of the steel beam refers to any dimension of the cross-sectional dimension of the steel beam in the bridge, such as the thickness of the upper flange plate, the thickness of the lower flange plate, the thickness of the web plate, the width of the web plate, and the width of the steel beam. Similarly, γ dc Characterizes the degree of deviation between the cross-sectional dimension value of the bridge concrete panel and the design value of the cross-sectional dimension of the bridge concrete panel. Here, the cross-sectional dimension of the concrete panel refers to any dimension of the cross-sectional dimension of the bridge concrete panel, such as the length, width, and height of the concrete panel. They reflect to a certain extent the construction factors that affect the most important types of structural intrinsic safety levels during the construction process. The load parameters are the randomly changing loads known in the art, including the uniformly distributed lane load q and the concentrated lane load P. k ; In this technical solution, when it is used specifically, the values of the random variable parameters are first determined. The values of the structural uncertainty parameters in the random variables can come from on-site measurements (such as the test results of different batches of raw materials of the construction unit or the test results of the compressive strength of concrete of the cast structure) or data records (such as those recorded in the design specifications, which can reduce the workload and greatly increase the value range of the parameter). The values of the load random variables can be obtained through data records or actual traffic tests. Multiple values are taken for the above-mentioned random variable parameters to form a sampling sample, and then the above-mentioned function function is used as the sampling function function for sampling calculation. In the actual sampling process, sampling calculation is performed in accordance with the series mode (that is, under the three limit states, the calculated value of the function function of any limit state is less than or equal to 0, which indicates that the bridge system has failed. The series mode is a method well known in the art). The failure probability of the bridge system in the overall sampling is statistically analyzed. The lower the failure probability, the higher the safety of the bridge under the limit state of bearing capacity. The technical solution has the beneficial effect of providing a safety and durability evaluation method for an I-beam-concrete composite continuous beam bridge, which can more accurately and intuitively characterize the safety and durability of the I-beam-concrete composite continuous beam bridge, and realize the comprehensive measurement of the safety and durability of the bridge. The failure probability of the bridge is calculated, and the failure probability is converted to obtain a reliability value (the conversion method of the failure probability and the reliability value is shown in GB / T 50283 1999 Unified Standard for Reliability Design of Highway Engineering Structures). By comparing the reliability value with the target reliability value designed during the bridge construction, the degree of deviation between the bridge and the design standard can be known, and then the construction quality can be evaluated. At the same time, for multiple bridges of the same type, by comparing the size of the failure probability values, a bridge with a smaller failure probability value can be screened out, indicating that the construction quality of the bridge is better. The construction plan or construction process of the screened bridge with better quality is helpful for the learning of subsequent construction personnel, and also provides effective guidance for the subsequent construction of the same type of bridges.
[0017] In another technical solution, the implementation of step S2 is as follows: obtaining the statistical characteristics of the uncertainty parameters at the structural level, sampling using the Monte Carlo method based on MATLAB, and calculating the system failure probability under the ultimate state of the bridge bearing capacity; wherein: γ cf The statistical characteristics of γ are obtained as follows: taking multiple concrete material compressive strength values measured on site as statistical objects, the mean μ1 and standard deviation σ1 of the concrete material compressive strength are calculated, and then γ is obtained. cf The normal distribution statistical characteristics of N (μ1 / f cd ,σ1 / f cd ); γ ds The specific acquisition of the statistical characteristics of is as follows: taking multiple steel beam cross-sectional dimensions measured on site as statistical objects, calculating μ2 and standard deviation σ2 of the steel beam cross-sectional dimensions, and then obtaining γ ds The normal distribution statistical characteristics of N (μ2 / design value of steel beam cross-section size, σ2 / design value of steel beam cross-section size); γ dc The specific acquisition of the statistical characteristics of is as follows: taking the cross-sectional dimensions of multiple bridge concrete panels measured on site as statistical objects, the cross-sectional dimensions of the bridge concrete panels μ3 and the standard deviation σ3 are calculated, and then γ is obtained. dc The normal distribution statistical characteristics of N (μ3 / design value of the cross-sectional size of the bridge concrete panel, σ3 / design value of the cross-sectional size of the bridge concrete panel); γ s The statistical characteristics of are obtained as follows: the tensile strength values of multiple steels measured on site are used as statistical objects, the mean μ4 and standard deviation σ4 of the tensile strength of the steels are calculated, and then γ sThe normal distribution statistical characteristics of N (μ4 / f d ,σ4 / f d ); γ r The statistical characteristics of γ are obtained as follows: the tensile strength values of multiple steel bars measured on site are used as statistical objects, the mean μ5 and standard deviation σ5 of the tensile strength of the steel bars are calculated, and then γ is obtained. r The normal distribution statistical characteristics of N (μ5 / f s ,σ5 / f s ); In the above technical solution, the on-site measurement can be the test results of different batches of raw materials of the construction unit or the test results of relevant components on the constructed bridge (cast concrete / constructed steel beam components). The Monte Carlo method based on MATLAB is a very existing sampling calculation method, which will not be elaborated here. The beneficial effect of adopting this technical solution is that by obtaining the statistical characteristics of uncertainty parameters at the structural level and combining the Monte Carlo method based on MATLAB for sampling calculation, the failure probability can be quickly obtained, which greatly improves the calculation efficiency.
[0018] In another technical solution, the qualitative parameter η c The specific value of is as follows: According to the qualitative description of the appearance of the bridge concrete structure in the design specification, the quantitative description of the bridge assessment standard is determined. The quantitative description includes five scales, as follows: Scale 1: intact; under this scale, η c The value range is 0.95~1.0; Scale 2: The cumulative area of network cracks is ≤ 20% of the component area, and the area of a single crack is ≤ 1.0m 2 , or the length of the main beam crack is ≤ 1 / 3 of the cross-sectional size; under this scale, η c The value range is 0.9~0.95; Scale 3: The cumulative area of network cracks is ≤ 20% of the component area, and the area of a single crack is > 1.0m 2 , or the length of the main beam crack is > 1 / 3 of the cross-sectional size and ≤ 2 / 3 of the cross-sectional size; under this scale, η c The value range is 0.85~0.90; Scale 4: The length of the main beam crack is greater than 2 / 3 of the cross-sectional size, and the spacing is less than 20 cm. c The value range is 0.80~0.850; Scale 5: The width of the cracks in the main beam is >1.0mm, and the spacing is ≤10cm; under this scale, η c The value range is below 0.80.
[0019] In the above technical solution, scales 1 to 5 are used to score and evaluate the appearance quality of the constructed bridge concrete panels. The design contents of scales 1 to 5 are designed with reference to existing standards. The "intact" in scale 1 indicates that the concrete panel is intact and has no defects such as cracks. The components in scales 2 to 3 refer to the bridge concrete panels. The spacing in scales 4 to 5 refers to the width of the cracks in the main beam. When in use, the construction personnel score the appearance quality of the bridge concrete panel structure according to these five scales. After the scores of multiple construction personnel are averaged, the final qualitative parameter η can be obtained. c The value of represents objectivity and accuracy.
[0020] In another technical solution, the safety of the bridge under the serviceability limit state is evaluated by the failure probability of the bridge system under the serviceability limit state, which specifically includes the following steps: A1. Determine the function: The functional functions used to calculate the failure probability of the bridge system under the normal serviceability limit state include the maximum crack width formula Z4 and the mid-span deflection formula Z5; Formula Z4 is specifically: , ; Formula Z5 is specifically: ; Among them, f1 is the short-term deflection, which is positive when it is downward, and f2 is the long-term deflection. The formula of f1 is as follows: , , , ;in, , , , , , , ; The calculation formula of f2 is as follows: ,in, , ; In formula Z4 and formula Z5, the parameters involved are characterized as follows: γ is the uncertainty coefficient of the calculation model, which has no unit and can be taken as 1.0 in actual calculation; α cr is the stress characteristic coefficient of the component, unitless; f t is the tensile strength of steel fiber concrete, unit: MPa; ρ te is the effective reinforcement ratio of the longitudinal tensile reinforcement, unitless; σ rs is the stress of the longitudinal tensile reinforcement at the crack section of the reinforced concrete member, in MPa; l ais the average spacing of transverse reinforcement, in mm; f ry A is the yield strength of non-prestressed steel bars in the composite beam, in MPa; r The representation of is as mentioned above, that is, the cross-sectional area of the longitudinal reinforcement in the concrete bridge deck on the upper side of the plastic neutral axis, in mm 2 ;f py A is the yield strength of the prestressed steel bars in the composite beam, in MPa; s is the cross-sectional area of the steel beam, in mm; f y A is the yield strength of the steel beam, in MPa; P is the cross-sectional area of the external prestressed tendons, in mm 2 ;f allow is the allowable deflection, in mm; B is the converted section stiffness of the composite beam, in N·mm 2 ; z1 is the distance from the centroid of the end prestressed tendon to the centroid of the converted section of the composite beam, in mm. The centroid of the prestressed tendon is positive when it is above the converted centroid; l 1 is the projection length of the first section of prestressed tendons in the local coordinate system, in mm; θ1 is the angle between the first section of prestressed tendons and the horizontal line, in ° (degrees); θ2 is the angle between the second section of prestressed tendons and the horizontal line, in ° (degrees); B s Converted section stiffness of composite beam considering slip, unit N·mm 2 ; m is the ratio of the distance from the beam end to the single point concentrated load loading point to the calculated span of the composite beam, unitless; r is the shear connection degree, unitless; K L h is the shear stiffness of the shear connector per unit length, in MPa; sc E is the distance from the centroid of the steel beam section to the centroid of the concrete section, in mm; c is the elastic modulus of concrete, unit: MPa; E s is the elastic modulus of steel, unit: MPa; I c is the moment of inertia of the concrete section, in mm 4 ;I s is the moment of inertia of the steel beam section, in mm 4 ; A c is the cross-sectional area of the concrete bridge deck, in mm 2 ; A s is the cross-sectional area of the steel beam, in mm 2 ;n s is the number of rows of studs or perforated plate connectors, unitless; k is the shear stiffness of a single shear connector, unit N / mm, using stud connectors; p is the spacing between connectors, unit mm; σ eis the effective tension prestress of the prestressed tendons, unit MPa; λ(t) is a coefficient related to time, unitless, t is the calculation time, unit d; k1 is a coefficient related to the average stress of the concrete bridge deck, unitless; is the average stress of the concrete bridge deck, in MPa, with a negative value for compression and 0 for tension; T p is the effective prestressing force of the prestressed tendons, in N; A0 is the cross-sectional area of the composite beam after the cross-sectional conversion, in mm 2 ; I0 is the moment of inertia of the composite beam after the cross section is converted, unit: mm 4 ; e is the prestressing eccentricity, unit: mm; A2. Calculation of failure probability of bridge system under serviceability limit state: With ρ te 、f t , A r 、f ry , A P 、f py , A s 、f y 、E s 、E c , A c , A s , A0, q, P k The sampling object is the formula Z4 and Z5 as the function function, and the value of each function function is calculated. When any function function value is less than or equal to 0, it indicates that the bridge system is invalid, otherwise the bridge system is valid; repeat the sampling M times, count the number of failures m, and the failure probability is m / M; A3. Safety evaluation of bridge system under normal use limit state: Comparing the failure probabilities of any two I-beam-concrete composite continuous beam bridges under the serviceability limit state, the lower the failure probability, the higher the safety of the bridge under the serviceability limit state.
[0021] In the above technical solution, the representations of the above parameters are existing, and specific reference may be made to GB 50917-2013 Specification for Design of Steel-Concrete Composite Bridges (hereinafter referred to as the design specification), wherein the random variable parameters in the parameters include: ρ te 、f t 、f ry 、 f py 、 A s 、f y , A P 、E c 、E s , A c , A s , A0, q, P k, the rest are fixed value parameters. Among the fixed value parameters, those involving mechanical properties are nominal value parameters, and the others are design value parameters. Both nominal value parameters and design value parameters are common knowledge in this field and will not be elaborated here. The value of random variables can be obtained by field measurement or from existing data, preferably from field measurement; the normal service limit state mainly tests whether the maximum crack width and mid-span deflection generated during the use of the bridge are within the normal range. If they are beyond the range, the system fails. The normal service limit state specifically includes the mid-span deflection limit state (the corresponding function function is formula Z5) and the negative moment zone concrete cracking limit state (the corresponding function function is formula Z4). In the actual sampling calculation process, these two limit states are sampled and calculated in series mode to obtain the failure probability. The lower the failure probability, the higher the safety of the bridge under the normal service limit state; The beneficial effect of adopting this technical solution is that it provides a method for evaluating the safety of a bridge under the limit state of normal use. It can simultaneously evaluate the safety of an I-beam-concrete composite continuous beam bridge under the ultimate state of bearing capacity and the limit state of normal use. The evaluation is comprehensive and has a wider applicability.
[0022] In another technical solution, the specific steps for evaluating the durability of the bridge system under the ultimate bearing capacity state are as follows: B1. Determine the calculation formula: The calculation formula for the reliability degradation rate of the bridge under the ultimate bearing capacity state is: ; The bearing capacity limit state is one of the bending bearing capacity limit state, the shear bearing capacity limit state, and the bending bearing capacity limit state at the middle support position; α1 represents the reliability degradation rate of the bridge under the bearing capacity limit state, μ R01 Characterizes the mean resistance of the bridge structure at the initial moment under the ultimate bearing capacity state; σ R01 Characterizes the standard deviation of the resistance of the bridge structure at the initial moment under the ultimate bearing capacity state; σ S1 represents the standard deviation of the load effect of the bridge structure under the ultimate bearing capacity state; λ´ represents the corrosion rate of the steel web; γ0 represents the design thickness of the steel web; B2. Calculation of reliability degradation rate of bridge under ultimate bearing capacity state: Take λ´ and γ0 as sampling objects, calculate the α1 value, repeat the sampling P times, calculate the mean of the α1 values of P samplings, and obtain the reliability degradation rate under the corresponding bearing capacity limit state; B3. Evaluation of bridge durability under the ultimate bearing capacity state: Compare the reliability degradation rates of any two I-beam-concrete composite continuous beam bridges under the corresponding ultimate bearing capacity state. The lower the reliability degradation rate, the higher the durability of the bridge under the ultimate bearing capacity state.
[0023] In the above technical solution, the calculation formula of the reliability degradation rate specifically refers to GB 50917-2013 Code for Design of Steel-Concrete Composite Bridges, wherein the ultimate bearing capacity state is one of the ultimate bearing capacity state of bending, the ultimate bearing capacity state of shear, and the ultimate bearing capacity state of bending at the middle support. In actual calculation, the reliability degradation rate values under the ultimate bearing capacity state of bending, the ultimate bearing capacity state of shear, and the ultimate bearing capacity state of bending at the middle support are calculated respectively, and the reliability degradation rate values of the two bridges under the corresponding ultimate states are compared respectively, so as to obtain the durability evaluation of the bridge under the corresponding ultimate state; μ R01 , σ R01 , σ S1 The specific value method is as follows: Under the ultimate bending bearing capacity state: μ R01 is M in the above formula Z1 R The mean of M in Z1 R Formula, perform multiple sampling calculations, and take the mean value as μ R01 The standard deviation is σ R01 Value; σ S1 Characterizes the standard deviation of the load effect of the bridge structure under the ultimate bearing capacity state, which is obtained by M in Z1 above. S Formula, multiple sampling calculations are performed, and the standard deviation is taken as σ S1 value; Under the ultimate shear bearing capacity state: μ R01 V in the above formula Z2 R The mean value of V in Z2 R Formula, perform multiple sampling calculations, and take the mean value as μ R01 The standard deviation is σ R01 Value; σ S1 Characterizes the standard deviation of the load effect of the bridge structure under the ultimate bearing capacity state, which is expressed by V in the above Z2 formula S The calculation formula is to perform multiple sampling calculations and take the standard deviation as σ S1 value; Under the ultimate state of bending bearing capacity at the middle support position: μ R01 is M in the above formula Z3 R,0 The mean of M in Z3 R,0 Formula, perform multiple sampling calculations, and take the mean value as μ R01 The standard deviation is σR01 Value; σ S1 Characterizes the standard deviation of the load effect of the bridge structure under the ultimate bearing capacity state, which is expressed by M in the above Z3 formula S,0 Formula, multiple sampling calculations are performed, and the standard deviation is taken as σ S1 value; It should be noted that the above-mentioned multiple sampling calculations can be directly carried out by taking the sampling samples for calculating the failure probability under the ultimate state of bearing capacity as the sampling samples; The values of λ´ and γ0 may be information from existing research literature; In this technical solution, when used, first determine the ultimate bearing capacity state to be evaluated, then calculate the mean resistance of the bridge structure at the initial moment under the ultimate bearing capacity state, the standard deviation of the resistance of the bridge structure at the initial moment, and the standard deviation of the load effect of the bridge structure, and obtain the calculation formula of the reliability degradation rate, then design the value of the random variable (λ´, γ0) and form a sampling sample, use the sampling sample as the sample library, sample multiple times and calculate the reliability degradation rate value, and take the average value as the reliability degradation rate under the corresponding ultimate bearing capacity state. The lower the reliability degradation rate, the higher the durability of the bridge. The beneficial effect of adopting this technical solution is that it provides a method for evaluating the durability of the bridge system under the ultimate bearing capacity state. It can intuitively, accurately and quickly judge the durability of the bridge, and then screen out bridges with better durability, providing meaningful guidance for the subsequent construction of similar bridges.
[0024] Another technical solution also includes the evaluation of the durability of the bridge system under the normal service limit state, which specifically includes the following steps: C1. Determine the calculation formula: The calculation formula for the reliability degradation rate of the bridge under the normal service limit state is: ; Wherein, the normal service limit state is one of the concrete cracking limit state in the negative bending moment zone and the mid-span deflection limit state; α2 represents the reliability degradation rate of the bridge under the normal service limit state; When the serviceability limit state is the concrete cracking limit state in the negative moment zone, μ R02 Characterizes the maximum crack width limit, σ R02 is 0, σ S2 Characterizes the standard deviation of the maximum crack width; When the serviceability limit state is the mid-span deflection limit state, μ R02 Characterizes the deflection limit of the bridge mid-span, σ R02 is 0, σ S2 Characterizes the standard deviation of the actual deflection of the bridge at mid-span; C2. Calculation of reliability degradation rate of bridges under serviceability limit state: Take λ´ and γ0 as sampling objects, calculate the α2 value, repeat the sampling Q times, calculate the mean of the α2 values of Q samplings, and obtain the required reliability degradation rate; C3. Evaluation of bridge durability under normal use limit state: Compare the reliability degradation rates of any two I-beam-concrete composite continuous beam bridges under the corresponding serviceability limit state. The lower the reliability degradation rate, the higher the durability of the bridge under the serviceability limit state. In the above technical solution, the calculation formula of the reliability degradation rate specifically refers to GB 50917-2013 Code for Design of Steel-Concrete Composite Bridges, where the normal service limit state includes the mid-span deflection limit state (corresponding to the functional function of the mid-span deflection) and the maximum crack width limit state (i.e. the concrete cracking limit state in the negative moment zone, corresponding to the functional function of the maximum crack width); μ R02 , σ R02 , σ S2 The specific value method is as follows: Under the ultimate limit state of concrete cracking in the negative moment zone: μ R02 Characterizes the maximum crack width limit, which is a default value in this field and is taken as 0.2 in the above formula Z4, that is, μ R02 =0.2;σ R02 Characterizes the standard deviation of the maximum crack width limit. Since the maximum crack width limit is a default value in this field, σ R02 The value is 0; S2 Characterizes the standard deviation of the maximum crack width, where the calculation formula for the maximum crack width is the part after "0.2-" in the above formula Z4, that is, the maximum crack width = , calculated according to this formula, σ S2 The value of is: the random variable involved in the formula (ρ te 、f t , A r 、f ry , A P 、f py , A s 、f y 、E s ) is a sampling sample, and the maximum crack width is calculated according to the maximum crack width formula to obtain multiple maximum crack width calculation values. The multiple maximum crack width calculation values are used as statistical objects, and the standard deviation of the maximum crack width is calculated, which is σ S2 The value of Under the mid-span deflection limit state: μ R02The deflection limit that represents the mid-span deflection of the bridge is also known as the allowable deflection (f allow ), σ R02 Characterizes the standard deviation of the deflection limit of the bridge mid-span deflection, where the deflection limit is an exact fixed value. The deflection limit is calculated by multiplying the deflection-to-span ratio limit by the bridge span. The deflection-to-span ratio limit is determined by consulting the design specifications. In actual application, due to μ R02 is an exact constant, so σ R02 =0; S2 The standard deviation of the actual deflection that characterizes the mid-span deflection of the bridge is obtained by performing multiple sampling calculations on the deflection calculation formula and obtaining the value statistically. Specifically, the calculation formulas for short-term deflection (f1) and long-term deflection (f2) in formula Z5 are used as the calculation formulas, and the random variables involved in these two formulas are used to construct sampling samples. The actual deflection of each sampling is calculated (in each sampling, the short-term deflection and the long-term deflection are calculated at the same time, and the largest calculation result is selected as the calculation result of this sampling). After multiple samplings, multiple actual deflection values are obtained, and the mean and standard deviation of the actual deflection of the multiple samplings are calculated, where the standard deviation is σ S2 The above formulas and parameter representations are inherent in the design specifications, and more specific reference may be made to the design specifications; The beneficial effect of adopting this technical solution is that it provides a method for judging the durability of bridge systems under normal use limit states, which can comprehensively evaluate the durability of bridge systems under major limit states, facilitate the screening of bridges with better durability, and provide guiding opinions for the subsequent construction of similar bridges.
[0025] Although the embodiments of the present invention have been disclosed as above, they are not limited to the applications listed in the specification and the implementation modes. They can be fully applied to various fields suitable for the present invention. For those familiar with the art, additional modifications can be easily implemented. Therefore, without departing from the general concept defined by the claims and the scope of equivalents, the present invention is not limited to the specific details and the embodiments shown and described herein.
Claims
1. A safety and durability evaluation method for an I-beam-concrete composite continuous beam bridge, characterized in that: The safety of bridges under the ultimate bearing capacity state is evaluated by the failure probability of the bridge system under the ultimate bearing capacity state; The durability of the bridge under the ultimate bearing capacity state is evaluated by the reliability degradation rate of the bridge system under the ultimate bearing capacity state.
2. The safety and durability evaluation method of an I-beam-concrete composite continuous beam bridge according to claim 1, characterized in that: The safety evaluation of bridge under the ultimate bearing capacity state specifically includes the following steps: S1. Determine the function: The functional functions used to calculate the failure probability of the bridge system under the ultimate bearing capacity state include the bending bearing capacity formula Z1, the shear bearing capacity formula Z2, and the bending bearing capacity formula Z3 at the middle support position; The specific formula Z1 is: Z1=M R -M S ; Among them, M R The calculation formula is: When the plastic neutral axis is within the concrete panel section, , when the plastic neutral axis is within the steel beam section, ;M S The calculation formula is: ; The specific formula Z2 is: Z2=V R -V S ; Among them, V R The calculation formula is: , V S The calculation formula is: ; Formula Z3 is specifically: ;in, The calculation formula is: , The calculation formula is: ; In the formulas Z1 to Z3, the parameters involved are divided into nominal value parameters, design value parameters, random variable parameters, and qualitative parameters η c , the qualitative parameter η c Characterizes the closeness between the appearance quality of the bridge structure concrete and the acceptance standard. The closer to the acceptance standard, the better the η c The closer the value of is to 1; The nominal value parameters are characterized as follows: f cd is the compressive strength of concrete material, f d is the tensile strength of steel, f s is the tensile strength of the longitudinal reinforcement in the concrete panel, f vd is the shear strength of steel; The design value parameters are specifically characterized as follows: k is the fitting coefficient considering the slip effect; A c is the cross-sectional area of the concrete bridge deck; y1 is the distance from the centroid of the concrete bridge deck section in the compression zone to the centroid of the steel beam section in the tension zone; A sc is the cross-sectional area of the steel beam in compression; y2 is the distance from the centroid of the steel beam in compression to the centroid of the steel beam in tension; A r is the cross-sectional area of the longitudinal reinforcement in the concrete bridge deck on the upper side of the plastic neutral axis; y4 is the distance from the centroid of the cross section of the longitudinal reinforcement in the concrete bridge deck to the centroid of the cross section of the tensile zone of the steel beam; A cc is the area of the concrete bridge deck on the upper side of the plastic neutral axis; g is the constant load; L is the length of a single span of the bridge; 1+μ is the impact coefficient; h w is the web height of the steel beam; t w A is the thickness of the steel beam web; st h is the tensile area of the I-beam; s A is the height of the tension zone; r h is the cross-sectional area of the longitudinal reinforcement in the concrete bridge deck above the plastic neutral axis; c is the height of the compression zone; x is the distance between the neutral axis of the cross section and the top surface of the I-beam; The random variable parameters include structural uncertainty parameters and load parameters. The structural uncertainty parameters are characterized as follows: γ cf Characterizes the degree of deviation between the compressive strength of concrete materials and the nominal value of the compressive strength of concrete materials, γ cf = compressive strength of concrete material / f cd ; γ s Characterizes the deviation between the tensile strength of steel and the nominal value of the tensile strength of steel, γ s = steel tensile strength value / f d ; γ ds Characterizes the degree of deviation between the cross-sectional dimension of the steel beam and the nominal value of the cross-sectional dimension of the steel beam, γ ds = Steel beam cross-section size value / design value of steel beam cross-section size; γ dc Characterizes the degree of deviation between the cross-sectional size of the bridge concrete panel and the design value of the cross-sectional size of the bridge concrete panel, γ dc = Bridge concrete panel cross-sectional dimension value / bridge concrete panel cross-sectional dimension design value; γ r Characterizes the deviation between the tensile strength of steel bars and the nominal value of the tensile strength of steel bars, γ r = tensile strength of steel bar / f s ; The load parameters are characterized as follows: q is the uniform lane load; P k For concentrated lane loads; S2. Calculation of failure probability of bridge system under ultimate bearing capacity state: The above random variable parameters are used as sampling objects, and formulas Z1, Z2, and Z3 are used as function functions to calculate the values of each function. When any function value is less than or equal to 0, it indicates that the bridge system has failed, otherwise the bridge system is valid. Repeat the sampling N times, and count the number of failures n, then the failure probability is n / N. S3. Safety evaluation of bridge system under the ultimate bearing capacity state: Comparing the failure probabilities of any two I-beam-concrete composite continuous beam bridges under the ultimate bearing capacity state, the lower the failure probability, the higher the safety of the bridge under the ultimate bearing capacity state.
3. The safety and durability evaluation method of an I-beam-concrete composite continuous beam bridge according to claim 2, characterized in that: The implementation of step S2 is as follows: obtain the statistical characteristics of the uncertainty parameters at the structural level, use the Monte Carlo method based on MATLAB for sampling, and calculate the system failure probability under the ultimate state of the bridge bearing capacity; where: γ cf The statistical characteristics of γ are obtained as follows: taking multiple concrete material compressive strength values measured on site as statistical objects, the mean μ1 and standard deviation σ1 of the concrete material compressive strength are calculated, and then γ is obtained. cf The normal distribution statistical characteristics of N (μ1 / f cd ,σ1 / f cd ); γ ds The specific acquisition of the statistical characteristics of is as follows: taking multiple steel beam cross-sectional dimensions measured on site as statistical objects, calculating μ2 and standard deviation σ2 of the steel beam cross-sectional dimensions, and then obtaining γ ds The normal distribution statistical characteristics of N (μ2 / design value of steel beam cross-section size, σ2 / design value of steel beam cross-section size); γ dc The specific acquisition of the statistical characteristics of is as follows: taking the cross-sectional dimensions of multiple bridge concrete panels measured on site as statistical objects, the cross-sectional dimensions of the bridge concrete panels μ3 and the standard deviation σ3 are calculated, and then γ is obtained. dc The normal distribution statistical characteristics of N (μ3 / design value of the cross-sectional size of the bridge concrete panel, σ3 / design value of the cross-sectional size of the bridge concrete panel); γ s The statistical characteristics of are obtained as follows: the tensile strength values of multiple steels measured on site are used as statistical objects, the mean μ4 and standard deviation σ4 of the tensile strength of the steels are calculated, and then γ s The normal distribution statistical characteristics of N (μ4 / f d ,σ4 / f d ); γ r The statistical characteristics of γ are obtained as follows: the tensile strength values of multiple steel bars measured on site are used as statistical objects, the mean μ5 and standard deviation σ5 of the tensile strength of the steel bars are calculated, and then γ is obtained. r The normal distribution statistical characteristics of N (μ5 / f s ,σ5 / f s ).
4. The safety and durability evaluation method of an I-beam-concrete composite continuous beam bridge according to claim 2, characterized in that: Qualitative parameter η c The specific value of is as follows: According to the qualitative description of the appearance of the bridge concrete structure in the design specification, the quantitative description of the bridge assessment standard is determined. The quantitative description includes five scales, as follows: Scale 1: intact; under this scale, η c The value range is 0.95~1.0; Scale 2: The cumulative area of network cracks is ≤ 20% of the component area, and the area of a single crack is ≤ 1.0m 2 , or the length of the main beam crack is ≤ 1 / 3 of the cross-sectional size; under this scale, η c The value range is 0.9~0.95; Scale 3: The cumulative area of network cracks is ≤ 20% of the component area, and the area of a single crack is > 1.0m 2 , or the length of the main beam crack is > 1 / 3 of the cross-sectional size and ≤ 2 / 3 of the cross-sectional size; under this scale, η c The value range is 0.85~0.90; Scale 4: The length of the main beam crack is greater than 2 / 3 of the cross-sectional size, and the spacing is less than 20 cm. c The value range is 0.80~0.850; Scale 5: The width of the cracks in the main beam is >1.0mm, and the spacing is ≤10cm; under this scale, η c The value range is below 0.
80.
5. The safety and durability evaluation method of an I-beam-concrete composite continuous beam bridge according to claim 2, characterized in that: It also includes evaluating the safety of the bridge under the serviceability limit state by the failure probability of the bridge system under the serviceability limit state, which specifically includes the following steps: A1. Determine the function: The functional functions used to calculate the failure probability of the bridge system under the normal serviceability limit state include the maximum crack width formula Z4 and the mid-span deflection formula Z5; Formula Z4 is specifically: , ; Formula Z5 is specifically: ; Among them, f1 is the short-term deflection, f2 is the long-term deflection; the calculation formula of f1 is: , , , ;in, , , , , , , ; The calculation formula of f2 is as follows: ,in, , ; In formula Z4 and formula Z5, the parameters are represented as follows: γ is the uncertainty coefficient of the calculation model; α cr is the stress characteristic coefficient of the component; f t is the tensile strength of steel fiber concrete; ρ te is the effective reinforcement ratio of the longitudinal tensile reinforcement; rs is the stress of the longitudinal tensile reinforcement at the crack section of the reinforced concrete member; l a is the average spacing of transverse reinforcement; f ry is the yield strength of the non-prestressed steel bars in the composite beam; f py A is the yield strength of the prestressed steel bars in the composite beam; s is the cross-sectional area of the steel beam; f y is the yield strength of the steel beam; A P is the cross-sectional area of the external prestressed tendons; f allow is the allowable deflection; B is the converted section stiffness of the composite beam; z1 is the distance from the centroid of the end prestressed tendon to the centroid of the converted section of the composite beam; l 1 is the projection length of the first section of prestressed tendons in the local coordinate system; θ1 is the angle between the first section of prestressed tendons and the horizontal line; θ2 is the angle between the second section of prestressed tendons and the horizontal line; B s is the converted section stiffness of the composite beam considering slip; m is the ratio of the distance from the beam end to the single point concentrated load loading point to the calculated span of the composite beam; r is the shear connection degree; K L h is the shear stiffness of the shear connector per unit length; sc E is the distance from the centroid of the steel beam section to the centroid of the concrete section; c is the elastic modulus of concrete; E s is the elastic modulus of steel; I c is the moment of inertia of the concrete section; I s is the moment of inertia of the steel beam section; A c is the cross-sectional area of the concrete bridge deck; A s is the cross-sectional area of the steel beam; n s is the number of rows of studs or perforated plate connectors; k is the shear stiffness of a single shear connector; p is the spacing between connectors; σ e is the effective tension prestress of the prestressed tendons; λ(t) is a coefficient related to time; k1 is a coefficient related to the average stress of the concrete bridge deck; is the average stress of the concrete bridge deck; T p is the effective pretension of the prestressed tendons; A0 is the cross-sectional area of the composite beam after the cross-sectional conversion; I0 is the moment of inertia of the composite beam after the cross-sectional conversion; e is the eccentricity of the prestressing force; A2. Calculation of failure probability of bridge system under serviceability limit state: With ρ te 、f t , A r 、f ry , A P 、f py , A s 、f y 、E s 、E c , A c , A s , A0, q, P k The sampling object is the formula Z4 and Z5 as the function function, and the value of each function function is calculated. When any function function value is less than or equal to 0, it indicates that the bridge system is invalid, otherwise the bridge system is valid; repeat the sampling M times, count the number of failures m, and the failure probability is m / M; A3. Safety evaluation of bridge system under normal use limit state: Comparing the failure probabilities of any two I-beam-concrete composite continuous beam bridges under the serviceability limit state, the lower the failure probability, the higher the safety of the bridge under the serviceability limit state.
6. The safety and durability evaluation method of an I-beam-concrete composite continuous beam bridge according to claim 2, characterized in that: The specific steps for evaluating the durability of a bridge system under the ultimate bearing capacity state are as follows: B1. Determine the calculation formula: The calculation formula for the reliability degradation rate of the bridge under the ultimate bearing capacity state is: ; The bearing capacity limit state is one of the bending bearing capacity limit state, the shear bearing capacity limit state, and the bending bearing capacity limit state at the middle support position; α1 represents the reliability degradation rate of the bridge under the bearing capacity limit state, μ R01 Characterizes the mean resistance of the bridge structure at the initial moment under the ultimate bearing capacity state; σ R01 Characterizes the standard deviation of the resistance of the bridge structure at the initial moment under the ultimate bearing capacity state; σ S1 represents the standard deviation of the load effect of the bridge structure under the ultimate bearing capacity state; λ´ represents the corrosion rate of the steel web; γ0 represents the design thickness of the steel web; B2. Calculation of reliability degradation rate of bridge under ultimate bearing capacity state: Take λ´ and γ0 as sampling objects, calculate the α1 value, repeat the sampling P times, calculate the mean of the α1 values of P samplings, and obtain the reliability degradation rate under the corresponding bearing capacity limit state; B3. Evaluation of bridge durability under the ultimate bearing capacity state: Compare the reliability degradation rates of any two I-beam-concrete composite continuous beam bridges under the corresponding ultimate bearing capacity state. The lower the reliability degradation rate, the higher the durability of the bridge under the ultimate bearing capacity state.
7. The safety and durability evaluation method of an I-beam-concrete composite continuous beam bridge according to claim 6, characterized in that: It also includes the evaluation of the durability of the bridge system under the normal service limit state, which specifically includes the following steps: C1. Determine the calculation formula: The calculation formula for the reliability degradation rate of the bridge under the normal service limit state is: ; Wherein, the normal service limit state is one of the concrete cracking limit state in the negative bending moment zone and the mid-span deflection limit state; α2 represents the reliability degradation rate of the bridge under the normal service limit state; When the serviceability limit state is the concrete cracking limit state in the negative moment zone, μ R02 Characterizes the maximum crack width limit, σ R02 is 0, σ S2 Characterizes the standard deviation of the maximum crack width; When the serviceability limit state is the mid-span deflection limit state, μ R02 Characterizes the deflection limit of the bridge mid-span, σ R02 is 0, σ S2 Characterizes the standard deviation of the actual deflection of the bridge at mid-span; C2. Calculation of reliability degradation rate of bridges under serviceability limit state: Take λ´ and γ0 as sampling objects, calculate the α2 value, repeat the sampling Q times, calculate the mean of the α2 values of Q samplings, and obtain the required reliability degradation rate; C3. Evaluation of bridge durability under normal use limit state: Compare the reliability degradation rates of any two I-beam-concrete composite continuous beam bridges under the corresponding normal service limit state. The lower the reliability degradation rate, the higher the durability of the bridge under the normal service limit state.
8. The safety and durability evaluation method of an I-beam-concrete composite continuous beam bridge according to claim 2, characterized in that: The cross-sectional dimensions in the steel beam cross-sectional dimension value are derived from any one of the thickness of the upper flange plate, the thickness of the lower flange plate, the web thickness, the web width, and the width of the steel beam; the cross-sectional dimensions in the bridge concrete panel cross-sectional dimension value are derived from any one of the length, width, and height of the concrete panel.
Citation Information
Patent Citations
Bridge reliability predicting method and maintenance method of bridge
CN105893689A
Prestress concrete bridge corrosion fatigue life prediction method
CN109030333A
Reliability analysis method for reinforced concrete column
CN115408759A
Concrete beam reliability calculation method considering stress corrosion
CN117540562A
Method and system for predicting corrosion fatigue life of prestressed concrete bridges
US20210199560A1
Cited By
Aircraft wing beam section multi-objective optimization design method based on reinforcement learning
CN119180097A
A multi-objective optimization design method for aircraft wing beam cross section based on reinforcement learning
CN119180097B
Design method of assembly type combined cover beam and assembly type combined cover beam
CN120449287A
Composite beam bridge technical condition evaluation component weight calculation method based on stress state
CN121167861A