Semiconductor process method and semiconductor structure
By using atomic layer deposition to fill hard mask layer gaps and negative photoresist exposure development in semiconductor processes, the problems of low process efficiency and high cost in self-aligned dual imaging technology are solved, and the doubling of high-density patterns is achieved and Efficient graphics density filling.
Patent Information
- Application Number
- CN202411090721.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
AI Technical Summary
The existing self-aligned dual imaging technology has low process efficiency and high process cost. The closed pattern of the spacer layer leads to an increase in additional steps and material requirements, which affects the density multiplication effect of the circuit pattern.
By stacking the hard mask layer and the photoresist in sequence on the structure to be etched, the third hard mask layer gap is filled with atomic layer deposition, instead of the sidewall deposition step, combined with negative photoresist exposure development , reduce additional masking and etching steps to improve graphics density.
It avoids the formation of closed patterns, improves process efficiency and reduces costs, realizes filling and pattern density multiplication of high-density graphics, and is suitable for high-density lines.
Smart Images

Figure CN119008390A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of semiconductor integrated circuit manufacturing, and in particular relates to a semiconductor process method and a semiconductor structure. Background Art
[0002] In the manufacturing process of semiconductor integrated circuits, with the continuous advancement of semiconductor manufacturing technology, the critical dimensions have been continuously reduced, which has exceeded the physical limits of the current mainstream lithography technology. Therefore, self-aligned double patterning technology (SADP) came into being and has been widely used.
[0003] The existing self-aligned double imaging technology generally obtains a patterned photoresist through one lithography, and then etches the underlying hard mask using the patterned photoresist as a mask; after obtaining the patterned hard mask, a spacer layer is deposited on the patterned sidewalls of the hard mask, and then the patterned hard mask is removed to obtain a patterned spacer layer; then the underlying hard mask is etched using the patterned spacer layer as a mask, and after repeating the steps of etching the hard mask and depositing the spacer layer on the sidewalls, the pattern density of the hard mask obtained finally is doubled, and the structural layer etched downward using the finally obtained hard mask as a mask can also obtain a doubled pattern density, so that the pattern density is not limited by the pattern density that can be achieved by the photoresist.
[0004] However, during the implementation of this method, due to the method of depositing the spacer layer on the sidewall of the hard mask pattern, a closed pattern will appear at the edge of the spacer pattern of the obtained spacer layer, so that the spacer pattern actually obtained is still connected at the edge. In order to avoid the adverse effects of such closed patterns on the circuit pattern, it is usually necessary to use an additional mask to etch the spacer layer after forming the spacer layer to remove the closed pattern and completely separate the spacer pattern. This process not only increases the process steps, but also requires additional masks and etching materials, which greatly reduces the process efficiency and increases the process cost.
[0005] Therefore, a method for improving the process efficiency and reducing the process cost of the self-aligned dual imaging technology is urgently needed.
[0006] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of the present application and for the convenience of understanding by those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because these solutions are described in the background technology part of the present application. Summary of the invention
[0007] In view of the above shortcomings of the prior art, an object of the present invention is to provide a semiconductor process method and a semiconductor structure, which are used to solve the problems of low process efficiency and high process cost of the self-aligned dual imaging technology in the prior art.
[0008] To achieve the above object, the present invention provides a semiconductor process method, the semiconductor process method comprising:
[0009] Providing a structure to be etched, on which a first hard mask layer, a second hard mask layer, a third hard mask layer and a patterned photoresist are sequentially stacked from bottom to top;
[0010] Etching the third hard mask layer through the patterned photoresist to obtain the patterned third hard mask layer;
[0011] Filling the first hard mask material in the gap of the patterned third hard mask layer by atomic layer deposition, wherein the first hard mask material completely fills the gap of the third hard mask layer, and the filled first hard mask material constitutes a first spacer layer;
[0012] removing the third hard mask layer to obtain the patterned first spacer layer;
[0013] The first spacer layer is used as a mask to continuously perform a self-aligned double imaging process on the second hard mask layer, the first hard mask layer and the structure to be etched, so as to obtain a patterned structure to be etched.
[0014] Optionally, the photoresist is a negative photoresist.
[0015] Optionally, a stop layer is arranged between the structure to be etched and the first hard mask layer, a stop layer is arranged between the first hard mask layer and the second hard mask layer, a stop layer is arranged between the second hard mask layer and the third hard mask layer, and a stop layer is arranged between the photoresist and the third hard mask layer; the stop layer includes a nitrogen-free dielectric anti-reflective coating.
[0016] Optionally, the material of the first hard mask layer, the second hard mask layer and / or the third hard mask layer is amorphous carbon.
[0017] Optionally, the first hard mask material is oxide.
[0018] Optionally, the method of performing a self-aligned double imaging process on the second hard mask layer, the first hard mask layer and the structure to be etched includes:
[0019] Using the first spacer layer as a mask, etching the second hard mask layer to obtain a patterned second hard mask layer;
[0020] Depositing a second hard mask material on the sidewalls of the patterned second hard mask layer, wherein the second hard mask material on the sidewalls constitutes a second spacer layer;
[0021] removing the second hard mask layer to obtain the patterned second spacer layer;
[0022] Using the second spacer layer as a mask, etching the first hard mask layer to obtain a patterned first hard mask layer;
[0023] The structure to be etched is etched using the patterned first hard mask layer as a mask to obtain the patterned structure to be etched.
[0024] Optionally, the second hard mask material is oxide.
[0025] Optionally, after the patterned second spacer layer is obtained, the edges of the spacer patterns included in the formed second spacer layer have closed patterns, and the closed patterns of the second spacer layer are removed by a mask to obtain the second spacer layer without connection between adjacent spacer patterns.
[0026] Optionally, when the first hard mask material is filled in the gap of the patterned third hard mask layer using atomic layer deposition, the first hard mask material also covers the upper surface of the third hard mask layer. The first hard mask material on the upper surface of the third hard mask layer is removed to make the first spacer layer flush with the upper surface of the third hard mask layer.
[0027] The present invention further provides a semiconductor structure, which is the structure to be etched in any one of the semiconductor process methods described above, and the semiconductor structure is patterned using any one of the semiconductor process methods described above.
[0028] As described above, the semiconductor process method and semiconductor structure of the present invention have the following beneficial effects:
[0029] The present invention uses atomic layer deposition to fill the gap of the patterned third hard mask layer to replace the first step of sidewall deposition in the self-aligned double imaging technology, thereby avoiding the formation of closed patterns and eliminating the step of using a mask to remove the closed patterns obtained at the edge after sidewall deposition, thereby improving preparation efficiency and saving process costs.
[0030] The invention can obtain a higher density pattern by exposing and developing with a negative photoresist, eliminating the need to correct the optical proximity effect of the photoresist mask when using a positive photoresist, thereby improving process efficiency.
[0031] The present invention forms a first spacer layer by filling with atomic layer deposition, realizes high-density pattern gap filling, and is beneficial to the application in high-density circuits. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a schematic structural diagram of the structure to be etched in step 1 of the semiconductor process method according to the first embodiment of the present invention.
[0033] Figure 2 It is a schematic structural diagram of the patterned third hard mask layer obtained in step 2 in the semiconductor process method according to the first embodiment of the present invention.
[0034] Figure 3 It is a schematic structural diagram of forming a first spacer layer in step 3 of the semiconductor process method according to the first embodiment of the present invention.
[0035] Figure 4 The diagram shows a schematic diagram of a structure presented by a closed pattern of a spacer layer in a self-aligned double imaging process in the prior art.
[0036] Figure 5 The diagram shows a schematic diagram of the structure presented by an additional mask in a self-aligned double imaging process in the prior art.
[0037] Figure 6 The diagram shows a structure diagram of separated spacer patterns in a self-aligned double imaging process in the prior art.
[0038] Figure 7 It is a schematic structural diagram showing the first hard mask material covering the third hard mask layer in an optional example of step 3 in the semiconductor process method of the first embodiment of the present invention.
[0039] Figure 8 It is a schematic structural diagram showing the removal of the third hard mask layer in step 4 of the semiconductor process method according to the first embodiment of the present invention.
[0040] Fig. 9 It is a schematic diagram of the structure presented by etching the second hard mask layer in an optional example of step 5 in the semiconductor process method of embodiment 1 of the present invention.
[0041] Fig.10 It is a schematic diagram of the structure of forming a second spacer layer in an optional example of step 5 in the semiconductor process method of embodiment 1 of the present invention.
[0042] Fig.11 It is a schematic structural diagram of removing the second hard mask layer in an optional example of step 5 in the semiconductor process method of embodiment 1 of the present invention.
[0043] Fig.12 It is a schematic diagram of the structure presented by etching the first hard mask layer in an optional example of step 5 in the semiconductor process method of embodiment 1 of the present invention.
[0044] Component number description
[0045] 1. Structure to be etched; 2. First hard mask layer; 3. Second hard mask layer; 4. Third hard mask layer; 5. Photoresist; 51. Negative photoresist; 6. Stop layer; 7. First spacer layer; 8. Second spacer layer; 91. Additional mask; 92. Closed pattern; 93. Spacer pattern. DETAILED DESCRIPTION
[0046] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0047] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the schematic diagrams showing the device structure will not be partially enlarged according to the general scale, and the schematic diagrams are only examples, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.
[0048] For convenience of description, spatially relative terms such as "under", "below", "below", "below", "above", "on", etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatially relative terms are intended to encompass other orientations of the device in use or operation in addition to the orientation depicted in the drawings.
[0049] In the context of the present application, a structure in which a first feature is described as being "above" a second feature may include embodiments in which the first and second features are in direct contact, and may also include embodiments in which additional features are formed between the first and second features, such that the first and second features may not be in direct contact.
[0050] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0051] Embodiment 1:
[0052] This embodiment provides a semiconductor process method, the semiconductor process method comprising:
[0053] Step 1: providing a structure to be etched, on which a first hard mask layer, a second hard mask layer, a third hard mask layer and a patterned photoresist are sequentially stacked from bottom to top;
[0054] Step 2: etching the third hard mask layer through the patterned photoresist to obtain the patterned third hard mask layer;
[0055] Step 3: Filling the first hard mask material in the gap of the patterned third hard mask layer by atomic layer deposition, wherein the first hard mask material completely fills the gap of the third hard mask layer, and the filled first hard mask material constitutes a first spacer layer;
[0056] Step 4: removing the third hard mask layer to obtain the patterned first spacer layer;
[0057] Step 5: Using the first spacer layer as a mask, a self-aligned double imaging process is continued downward on the second hard mask layer, the first hard mask layer and the structure to be etched to obtain a patterned structure to be etched.
[0058] The semiconductor process method of the present invention will be described in detail below with reference to the accompanying drawings. It should be noted that the above sequence does not strictly represent the sequence of the semiconductor process method protected by the present invention, and those skilled in the art may change it according to the actual preparation steps.
[0059] First, if Figure 1 As shown, step 1 is performed to provide a structure to be etched 1, on which a first hard mask layer 2, a second hard mask layer 3, a third hard mask layer 4 and a patterned photoresist 5 are sequentially stacked from bottom to top.
[0060] In one embodiment, Figure 1 As shown, a stop layer 6 is arranged between the structure to be etched 1 and the first hard mask layer 2, a stop layer 6 is arranged between the first hard mask layer 2 and the second hard mask layer 3, a stop layer 6 is arranged between the second hard mask layer 3 and the third hard mask layer 4, and a stop layer 6 is arranged between the photoresist 5 and the third hard mask layer 4; the stop layer 6 includes a nitrogen-free dielectric anti-reflective coating.
[0061] By providing the stop layer 6, the present invention can control the etching of only the target hard mask layer without etching the non-target hard mask layer downward, thereby improving the accuracy of the obtained pattern.
[0062] In one embodiment, the material of the first hard mask layer 2 , the second hard mask layer 3 and / or the third hard mask layer 4 is amorphous carbon.
[0063] The present invention makes the etching speed of the stop layer 6 much lower than that of the hard mask layer during the etching process by coordinating the material selection of the stop layer 6 and the hard mask layer, thereby controlling the etching of the non-target hard mask layer and improving the etching rate of the target hard mask layer. Specifically, the thickness of the stop layer 6 is much smaller than the thickness of the hard mask layer.
[0064] Specifically, the materials of the stop layer 6 , the first hard mask layer 2 , the second hard mask layer 3 , and the third hard mask layer 4 may also be other appropriate materials.
[0065] Then, if Figure 2 As shown, step 2 is performed to etch the third hard mask layer 4 through the patterned photoresist 5 to obtain the patterned third hard mask layer 4.
[0066] Then, if Figure 3 As shown, step 3 is performed to fill the gaps in the patterned third hard mask layer 4 with the first hard mask material by atomic layer deposition. The first hard mask material completely fills the gaps in the third hard mask layer 4 , and the filled first hard mask material constitutes a first spacer layer 7 .
[0067] In the prior art, when pattern multiplication is performed by self-aligned double imaging technology, the following method is often used: providing a structure to be etched that is the same as that in the present embodiment, on which a first hard mask layer, a second hard mask layer and a third hard mask layer are stacked in sequence from bottom to top; firstly setting a patterned photoresist on the third hard mask layer; etching the third hard mask layer below by the patterned photoresist to obtain a patterned third hard mask layer; depositing a first spacer layer on the side wall of the patterned third hard mask layer; removing the third hard mask layer to obtain a patterned first spacer layer; using the patterned first spacer layer as a mask to etch the second hard mask layer to obtain a patterned second hard mask layer; depositing a second spacer layer on the side wall of the patterned second hard mask layer; removing the second hard mask layer to obtain a patterned second spacer layer; using the patterned second spacer layer as a mask to etch the first hard mask layer to obtain a patterned first hard mask layer; etching the structure to be etched by using the patterned first hard mask layer as a mask to obtain a patterned structure to be etched. In this process, since the first spacer layer and the second spacer layer are both deposited on the sidewall of the patterned hard mask layer, there are the following edges at the edges of the first spacer layer and the second spacer layer: Figure 4 The closed pattern 92 shown in the figure, the closed pattern 92 causes the first spacing layer and the second spacing layer to be separated from each other, and the spacing patterns that are originally required to be obtained are still connected, resulting in that the final pattern circuit does not meet the requirements; to solve this problem, in the prior art, after obtaining the first spacing layer and the second spacing layer with the closed pattern 92, use Figure 5The additional mask 91 shown is used to remove the closed pattern of the first spacer layer and the second spacer layer, thereby obtaining Figure 6 The spacer patterns 93 are shown as being separated from each other. However, this step requires the additional preparation of a mask plate and an additional etching and removal step, which reduces the overall process efficiency and increases the overall process cost.
[0068] like Figure 3 As shown, the present invention uses atomic layer deposition to fill the gaps between the patterned third hard mask layers 4 when forming the first spacer layer 7. Since the atomic layer deposition method only fills the gaps in the third hard mask layer 4 and does not deposit on the edges of the third hard mask layer 4, the obtained first spacer layer 7 does not form a closed pattern 92, and no additional mask plate 91 is required for additional etching process. Therefore, on the premise of obtaining the preset spacer pattern 93, the overall process efficiency is improved and the process cost is reduced. At the same time, atomic layer deposition can achieve a good deposition effect in a gap of tiny size, so that the process can be applied to the pattern preparation process of high-density circuits, which is conducive to adapting to the application scenarios of high-density, high-integration, and small-size semiconductor devices.
[0069] In one embodiment, Figure 1 As shown, the photoresist 5 is a negative photoresist 51 .
[0070] In the prior art, during self-aligned double imaging, since the graphic density that can be achieved by the positive photoresist itself after exposure is lower than the graphic density that can be achieved by the negative photoresist, a good photoresist pattern cannot be obtained by exposing and developing the positive photoresist using a photoresist mask of a corresponding circuit density given by the circuit design. Therefore, it is necessary to perform optical proximity correction (OPC) on the matching photoresist mask to reduce the graphic density of the photoresist mask so that the graphic obtained after the positive photoresist is exposed and developed is half of the circuit density of the circuit design. Then, the circuit density is doubled by depositing a spacer layer on the sidewall so that the final graphic density meets the requirements of the circuit design. However, the step of performing OPC on the photoresist mask will reduce the process efficiency.
[0071] The negative photoresist 51 used in the present invention can obtain a pattern with a higher density than the positive photoresist pattern, so that the photoresist 5 can be directly exposed and developed through a photoresist mask corresponding to the circuit density of the circuit design without the need to perform OPC operations on the photoresist mask, thereby improving process efficiency; using negative photoresist 51 in self-aligned dual imaging technology in combination with the method of atomic layer deposition to fill the pattern gap instead of the sidewall deposition method can improve process efficiency and reduce process costs in smaller size and higher density application environments.
[0072] In one embodiment, the first hard mask material is oxide.
[0073] Specifically, the present invention sets a large material etching selectivity ratio between the first hard mask material and the first hard mask layer 2, thereby improving the accuracy of the obtained pattern.
[0074] Specifically, the first hard mask material may also be other suitable materials.
[0075] In one embodiment, when the first hard mask material is filled in the gap of the patterned third hard mask layer 4 by atomic layer deposition, Figure 7 As shown, the first hard mask material also covers the upper surface of the third hard mask layer 4. Figure 3 As shown, the first hard mask material on the upper surface of the third hard mask layer 4 is removed, so that the first spacer layer 7 is flush with the upper surface of the third hard mask layer 4 .
[0076] In one embodiment, the first hard mask material on the upper surface of the third hard mask layer 4 is removed by etching or chemical mechanical polishing.
[0077] Then, if Figure 8 As shown, step 4 is performed to remove the third hard mask layer 4 to obtain the patterned first spacer layer 7.
[0078] Finally, if Figure 9-12 As shown, step 5 is performed, using the first spacer layer 7 as a mask to continue to perform a self-aligned double imaging process on the second hard mask layer 3, the first hard mask layer 2 and the structure to be etched 1 to obtain a patterned structure to be etched 1.
[0079] In one embodiment, a method for performing a self-aligned double imaging process on the second hard mask layer 3, the first hard mask layer 2 and the structure to be etched 1 includes:
[0080] like Fig. 9 As shown, the second hard mask layer 3 is etched using the first spacer layer 7 as a mask to obtain a patterned second hard mask layer 3;
[0081] like Fig.10 As shown, a second hard mask material is deposited on the sidewall of the patterned second hard mask layer 3, and the second hard mask material on the sidewall constitutes a second spacer layer 8;
[0082] like Fig.11 As shown, the second hard mask layer 3 is removed to obtain the patterned second spacer layer 8;
[0083] like Fig.12As shown, the first hard mask layer 2 is etched using the second spacer layer 8 as a mask to obtain a patterned first hard mask layer 2;
[0084] The structure to be etched 1 is etched using the patterned first hard mask layer 2 as a mask to obtain the patterned structure to be etched 1 .
[0085] In one embodiment, the second hard mask material is oxide.
[0086] Specifically, the present invention sets a large material etching selectivity ratio between the second hard mask material and the second hard mask layer 3, thereby improving the accuracy of the obtained pattern.
[0087] Specifically, the second hard mask material may also be other suitable materials.
[0088] Specifically, the first hard mask material and the second hard mask material may be the same, or may be other suitable hard mask materials.
[0089] In one embodiment, after obtaining the patterned second spacer layer 8, a closed pattern 92 exists at the edge of a spacer pattern 93 included in the formed second spacer layer 8. The closed pattern 92 of the second spacer layer 8 is removed through a mask to obtain the second spacer layer 8 without connection between adjacent spacer patterns 93.
[0090] Specifically, this example forms the second spacer layer 8 by sidewall deposition to better improve the pattern density preset by the self-aligned double imaging process, and the closed pattern 92 at the edge of the second spacer layer 8 can be subsequently removed by a mask to obtain a preset pattern.
[0091] Specifically, the drawings in this embodiment mark the corresponding dimensions in the corresponding structures, and the units are nanometers; the dimensions of the drawings marked in this embodiment are only the graphic dimensions obtained in an experiment to illustrate the dimensional changes in the process; different dimensional specifications can also be designed according to different processes, devices and dimensional requirements, all of which are within the scope of protection of the present invention.
[0092] Embodiment 2:
[0093] The present invention provides a semiconductor structure, which is the structure to be etched in any one of the semiconductor process methods described in the first embodiment, and the semiconductor structure is patterned by using any one of the semiconductor process methods described in the first embodiment.
[0094] The present invention uses the semiconductor process method of the first embodiment to perform self-aligned double imaging technology, and finally obtains a semiconductor structure with doubled pattern density, thereby improving process efficiency and reducing process cost while ensuring the pattern density of the obtained semiconductor structure.
[0095] In summary, the semiconductor process method and semiconductor structure of the present invention can fill the patterned third hard mask layer gap through atomic layer deposition to replace the first sidewall deposition step in the self-aligned double imaging technology, thereby avoiding the formation of closed patterns and eliminating the step of removing the closed patterns obtained at the edges after sidewall deposition with a mask, thereby improving preparation efficiency and saving process costs; at the same time, atomic layer deposition is used to fill and form the first spacer layer to achieve high-density pattern gap filling, which is beneficial for application in high-density circuits; in addition, higher-density patterns can be obtained by exposure and development with negative photoresist, thereby eliminating the need for optical proximity effect correction of the photoresist mask when using positive photoresist, thereby improving process efficiency.
[0096] Therefore, the present invention effectively overcomes various shortcomings in the prior art and has high industrial utilization value.
[0097] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A semiconductor process method, It is characterized in that The semiconductor process method comprises: Providing a structure to be etched, on which a first hard mask layer, a second hard mask layer, a third hard mask layer and a patterned photoresist are sequentially stacked from bottom to top; Etching the third hard mask layer through the patterned photoresist to obtain the patterned third hard mask layer; Filling the first hard mask material in the gap of the patterned third hard mask layer by atomic layer deposition, wherein the first hard mask material completely fills the gap of the third hard mask layer, and the filled first hard mask material constitutes a first spacer layer; removing the third hard mask layer to obtain the patterned first spacer layer; The first spacer layer is used as a mask to continuously perform a self-aligned double imaging process on the second hard mask layer, the first hard mask layer and the structure to be etched, so as to obtain a patterned structure to be etched.
2. The semiconductor process method according to claim 1, It is characterized in that The photoresist is a negative photoresist.
3. The semiconductor process method according to claim 1, It is characterized in that A stop layer is arranged between the structure to be etched and the first hard mask layer, a stop layer is arranged between the first hard mask layer and the second hard mask layer, a stop layer is arranged between the second hard mask layer and the third hard mask layer, and a stop layer is arranged between the photoresist and the third hard mask layer; the stop layer includes a nitrogen-free dielectric anti-reflective coating.
4. The semiconductor process according to claim 1 or 3, It is characterized in that The material of the first hard mask layer, the second hard mask layer and / or the third hard mask layer is amorphous carbon.
5. The semiconductor process method according to claim 1, It is characterized in that The first hard mask material is oxide.
6. The semiconductor process method according to claim 1, It is characterized in that The method of performing a self-aligned double imaging process on the second hard mask layer, the first hard mask layer and the structure to be etched comprises: Using the first spacer layer as a mask, etching the second hard mask layer to obtain a patterned second hard mask layer; Depositing a second hard mask material on the sidewalls of the patterned second hard mask layer, wherein the second hard mask material on the sidewalls constitutes a second spacer layer; removing the second hard mask layer to obtain the patterned second spacer layer; Using the second spacer layer as a mask, etching the first hard mask layer to obtain a patterned first hard mask layer; The structure to be etched is etched using the patterned first hard mask layer as a mask to obtain the patterned structure to be etched.
7. The semiconductor process method according to claim 6, It is characterized in that The second hard mask material is oxide.
8. The semiconductor process method according to claim 6, It is characterized in that After the patterned second spacer layer is obtained, the edges of the spacer patterns included in the formed second spacer layer have closed patterns, and the closed patterns of the second spacer layer are removed by a mask to obtain the second spacer layer without connection between adjacent spacer patterns.
9. The semiconductor process method according to claim 1, It is characterized in that When the first hard mask material is filled in the gap of the patterned third hard mask layer using atomic layer deposition, the first hard mask material also covers the upper surface of the third hard mask layer. The first hard mask material on the upper surface of the third hard mask layer is removed to make the first spacer layer flush with the upper surface of the third hard mask layer.
10. A semiconductor structure, It is characterized in that The semiconductor structure is the structure to be etched in the semiconductor process method described in any one of claims 1 to 9, and the semiconductor structure is patterned using the semiconductor process method described in any one of claims 1 to 9.