Solar cell and photovoltaic module

By introducing a spherical protrusion structure on the surface of the semiconductor conductive layer of a solar cell and combining it with the dielectric layer, the problems of dielectric layer stress and contact resistance are solved, thereby improving the fill factor and photoelectric conversion efficiency of the solar cell.

CN119008728APending Publication Date: 2024-11-22ZHEJIANG JINKO SOLAR CO LTD +1
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202311736380.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-12-15
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing solar cells face limitations in improving photoelectric conversion efficiency and fill factor, particularly in terms of passivation of the film and electrode contact resistance.

Method used

Multiple spherical protrusions are introduced on the surface of the semiconductor conductive layer of a solar cell, and a dielectric layer is covered on top of them. Combined with appropriate deposition processes and electrode design, a monolithic structure is formed to reduce the stress and contact resistance of the dielectric layer.

Benefits of technology

It significantly reduces the phenomenon of dielectric layer bursting, improves the flatness and yield of the dielectric layer, and increases the contact area between the electrode and the semiconductor conductive layer, thereby improving the fill factor and photoelectric conversion efficiency of the solar cell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008728A_ABST
    Figure CN119008728A_ABST
Patent Text Reader

Abstract

The embodiment of the invention relates to a solar cell and a photovoltaic module. The solar cell comprises a substrate; the semiconductor conductive layer is located on the surface of the substrate, the semiconductor conductive layer comprises a first surface which is far away from the substrate along a first direction, and the first surface is provided with a plurality of sphere-like bulge structures; the dielectric layer is positioned on the first surface, and covers the sphere-like bulge structure and the first surface exposed by the sphere-like bulge structure; and the plurality of electrodes are arranged at intervals along a second direction, and the electrodes penetrate through the dielectric layer and are in electric contact with the semiconductor conductive layer. The filling factor and the photoelectric conversion efficiency of the solar cell can be improved at least.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present application relate to the technical field of solar cells, and in particular to a solar cell and a photovoltaic module. Background Art

[0002] Fossil energy causes air pollution and has limited reserves, while solar energy has the advantages of being clean, pollution-free and abundant in resources. Therefore, solar energy is gradually becoming the core clean energy to replace fossil energy. Since solar cells have good photoelectric conversion efficiency, they have become the focus of development of clean energy utilization.

[0003] In order to maximize the efficiency of solar cells and the utilization of incident light, a variety of film layers, cell structures and film layer preparation schemes have emerged to enhance the passivation effect of photovoltaic cells. By forming specific film layers in solar cells, the solar cells have a larger open circuit voltage, smaller recombination losses or smaller parasitic light absorption, thereby improving the photoelectric conversion efficiency of the cells. Summary of the invention

[0004] The embodiments of the present application provide a solar cell and a photovoltaic module, which are at least beneficial to improving the fill factor and photoelectric conversion efficiency of the solar cell.

[0005] An embodiment of the present application provides a solar cell, comprising: a substrate; a semiconductor conductive layer, the semiconductor conductive layer being located on the surface of the substrate, the semiconductor conductive layer comprising a first surface away from the substrate along a first direction, and having a plurality of spherical-like protrusion structures on the first surface; a dielectric layer, the dielectric layer being located on the first surface, covering the spherical-like protrusion structures and the first surface exposed by the spherical-like protrusion structures; a plurality of electrodes, the plurality of electrodes being arranged at intervals along a second direction, and the electrodes penetrating the dielectric layer and being in electrical contact with the semiconductor conductive layer.

[0006] In some embodiments, the density of the spherical protrusion structures on the first surface is 1×10 9 / cm 2 Up to 3×10 11 / cm 2 .

[0007] In some embodiments, a ratio of an area of ​​the first surface covered by the spherical protrusion structure to an area of ​​the first surface is 0.3 to 1.

[0008] In some embodiments, the spherical protrusion structure and the semiconductor conductive layer are an integrally formed structure.

[0009] In some embodiments, along the first direction, a ratio between a thickness of the spherical protrusion structure and a thickness of the semiconductor conductive layer is 0.025 to 0.5.

[0010] In some embodiments, along the first direction, the thickness of the spherical protrusion structure is 5 nm to 100 nm.

[0011] In some embodiments, along the second direction, the width of the spherical protrusion structure is 10 nm to 200 nm.

[0012] In some embodiments, the solar cell further includes: a tunneling dielectric layer, the tunneling dielectric layer is located between the substrate and the semiconductor conductive layer and covers the surface of the substrate facing the semiconductor conductive layer, and the semiconductor conductive layer covers the surface of the tunneling dielectric layer away from the substrate.

[0013] In some embodiments, the substrate includes a front side and a back side opposite to each other along the first direction, the tunneling dielectric layer covers the back side of the substrate, the doping type of the semiconductor conductive layer is the same as the doping type of the substrate, and the doping concentration of the semiconductor conductive layer is greater than the doping concentration of the substrate.

[0014] In some embodiments, the semiconductor conductive layer includes a first doped region and a second doped region alternately arranged along the second direction, one of the first doped region and the second doped region is an N-type doped region, and the other is a P-type doped region; the plurality of electrodes include a first electrode and a second electrode arranged at intervals along the second direction, the first electrode is electrically in contact with the first doped region, and the second electrode is electrically in contact with the second doped region.

[0015] In some embodiments, the semiconductor conductive layer further includes an isolation region that penetrates the thickness of the semiconductor conductive layer, and the isolation region is located between the first doping region and the second doping region.

[0016] In some embodiments, the substrate includes a front side and a back side opposite to each other along the first direction, the semiconductor conductive layer includes a first semiconductor conductive layer located on the front side of the substrate and a second semiconductor conductive layer located on the back side of the substrate, and the solar cell also includes: an intrinsic semiconductor layer, the intrinsic semiconductor layer includes a first intrinsic semiconductor layer and a second intrinsic semiconductor layer; the first intrinsic semiconductor layer covers the front side of the substrate, and the first semiconductor conductive layer covers the surface of the first intrinsic semiconductor layer away from the substrate; the second intrinsic semiconductor layer covers the back side of the substrate, and the second semiconductor conductive layer covers the surface of the second intrinsic semiconductor layer away from the substrate.

[0017] In some embodiments, the semiconductor conductive layer includes electrode regions and non-electrode regions alternately arranged along the second direction, the electrode regions and the non-electrode regions have the same doping type, and the doping concentration of the electrode regions is greater than the doping concentration of the non-electrode regions.

[0018] Correspondingly, an embodiment of the present application also provides a photovoltaic component, comprising: a battery string, the battery string is formed by connecting a plurality of the above-mentioned solar cells; an encapsulation layer, the encapsulation layer is used to cover the surface of the battery string; and a cover plate, the cover plate is used to cover the surface of the encapsulation layer away from the battery string.

[0019] The technical solution provided by the embodiments of the present application has at least the following advantages:

[0020] In the solar cell provided by the embodiment of the present application, the semiconductor conductive layer on the surface of the substrate has a plurality of spherical protrusion structures on the first surface away from the substrate along the first direction, and the dielectric layer is located on the first surface of the semiconductor conductive layer. That is to say, the surface where the semiconductor conductive layer contacts the dielectric layer has a plurality of spherical protrusion structures, and the dielectric layer contacts the surface with a relatively large roughness of the semiconductor conductive layer. Therefore, the stress effect on the dielectric layer during the formation process is greatly reduced, thereby significantly reducing the probability of the dielectric layer having a film burst phenomenon, that is, the probability of randomly distributed pits appearing on the surface of the dielectric layer is reduced, thereby reducing the probability of the dielectric layer having a passivation performance failure or an abnormal appearance, and improving the flatness of the dielectric layer surface and the overall yield of the dielectric layer. The electrode penetrates the dielectric layer and contacts the semiconductor conductive layer. When there are a plurality of spherical protrusions on the first surface of the semiconductor conductive layer, the specific surface area of ​​the electrode in contact with the semiconductor conductive layer is increased, thereby reducing the contact resistance between the electrode and the semiconductor conductive layer, thereby improving the filling factor and photoelectric conversion efficiency of the battery. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] One or more embodiments are exemplarily described by pictures in the corresponding drawings, and these exemplifications do not constitute limitations on the embodiments. Unless otherwise stated, the pictures in the drawings do not constitute proportional limitations.

[0022] Figure 1 A schematic diagram of the overall structure of a solar cell provided in one embodiment of the present application;

[0023] Figure 2 A schematic diagram of the overall structure of another solar cell provided in one embodiment of the present application;

[0024] Figure 3 A top view of a semiconductor conductive layer provided in one embodiment of the present application;

[0025] Figure 4An electron microscope image of a semiconductor conductive layer provided in one embodiment of the present application;

[0026] Figure 5 A schematic diagram of the overall structure of another solar cell provided in one embodiment of the present application;

[0027] Figure 6 A schematic diagram of the overall structure of another solar cell provided in one embodiment of the present application;

[0028] Figure 7 A schematic diagram of the overall structure of another solar cell provided in one embodiment of the present application;

[0029] Figure 8 A schematic diagram of the overall structure of another solar cell provided in one embodiment of the present application;

[0030] Fig. 9 A schematic diagram of the overall structure of another solar cell provided in one embodiment of the present application;

[0031] Fig.10 A schematic diagram of the overall structure of another solar cell provided in one embodiment of the present application;

[0032] Fig.11 A schematic structural diagram of a photovoltaic module provided in another embodiment of the present application. DETAILED DESCRIPTION

[0033] In some embodiments, reference Figure 1 A solar cell generally includes a substrate 1, a first semiconductor conductive layer 2, a second semiconductor conductive layer 3, a first dielectric layer 4, a second dielectric layer 5 and a plurality of electrodes 6, wherein the plurality of electrodes 6 are arranged at intervals, and some of the plurality of electrodes 6 penetrate the first dielectric layer 4 and are in electrical contact with the first semiconductor conductive layer 2, and the remaining electrodes 6 penetrate the second dielectric layer 5 and are in electrical contact with the second semiconductor conductive layer 3.

[0034] In the process of preparing solar cells, the surface of the substrate 1 in contact with the first semiconductor conductive layer 2 and the second semiconductor conductive layer 3 is usually set to a smooth surface, so as to reduce the recombination current generated by the carrier recombination on the surface of the substrate 1 as much as possible, thereby reducing the recombination loss of the solar cell. The first dielectric layer 4 arranged on the surface of the first semiconductor conductive layer 2 away from the substrate 1 can passivate the defects on the surface of the first semiconductor conductive layer 2 through the bonding of the overflowed hydrogen with the material of the first semiconductor conductive layer 2, thereby reducing the carrier recombination on the surface of the first semiconductor conductive layer 2. Similarly, the second dielectric layer 5 can also have a similar passivation effect on the second semiconductor conductive layer 2, thereby significantly reducing the overall carrier recombination loss of the solar cell and significantly improving the photoelectric conversion efficiency.

[0035] An embodiment of the present application provides a solar cell, wherein the semiconductor conductive layer on the surface of the substrate has a plurality of spherical protrusion structures on the first surface away from the substrate in the first direction, and the dielectric layer is located on the first surface of the semiconductor conductive layer. That is, the surface where the semiconductor conductive layer contacts the dielectric layer has a plurality of spherical protrusion structures, and the dielectric layer contacts the surface with a relatively large roughness of the semiconductor conductive layer. Therefore, the stress effect on the dielectric layer during the formation process is greatly reduced, thereby significantly reducing the probability of the dielectric layer having a film burst phenomenon, that is, the probability of randomly distributed pits appearing on the surface of the dielectric layer is reduced, thereby reducing the probability of the dielectric layer having a passivation performance failure or an abnormal appearance, and improving the flatness of the dielectric layer surface and the overall yield of the dielectric layer. The electrode penetrates the dielectric layer and contacts the semiconductor conductive layer. When there are a plurality of spherical protrusions on the first surface of the semiconductor conductive layer, the specific surface area of ​​the electrode in contact with the semiconductor conductive layer is increased, thereby reducing the contact resistance between the electrode and the semiconductor conductive layer, thereby improving the filling factor and photoelectric conversion efficiency of the battery.

[0036] The embodiments of the present application will be described in detail below in conjunction with the accompanying drawings. However, it will be appreciated by those skilled in the art that in each embodiment of the present application, many technical details are provided in order to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solution claimed in the present application can be implemented.

[0037] An embodiment of the present application provides a solar cell, referring to Figure 2 and Figure 3 , Figure 2 is a schematic diagram of the structure of a solar cell, wherein the X direction is a first direction, the Y direction is a second direction, Figure 3 A top view of a semiconductor conductive layer.

[0038] The solar cell includes: a substrate 101; a semiconductor conductive layer 102, the semiconductor conductive layer 102 is located on the surface of the substrate 101, the semiconductor conductive layer 102 includes a first surface 121 away from the substrate 101 along a first direction, and the first surface 121 has a plurality of spherical protrusion structures 122; a dielectric layer 103, the dielectric layer 103 is located on the first surface 121, covers the spherical protrusion structures 122 and the first surface 121 exposed by the spherical protrusion structures 122; a plurality of electrodes 104, the plurality of electrodes are arranged at intervals along a second direction, and the electrodes 104 penetrate the dielectric layer 103 and are in electrical contact with the semiconductor conductive layer 102.

[0039] Among them, the first direction can be regarded as the stacking direction of each functional layer in the solar cell, and can also be regarded as the thickness direction of the substrate 101 itself. The substrate 101 usually has a front side with a higher incident light intensity and a back side with a lower incident light intensity along the thickness direction. In addition, the first direction X and the second direction Y can be perpendicular to each other, or there can be an angle less than 90 degrees, for example, 60 degrees, 45 degrees, 30 degrees, etc., and the first direction X and the second direction Y are not the same direction. For the sake of ease of explanation and understanding, this embodiment is described by taking the example that the first direction X and the second direction Y are perpendicular to each other. In specific applications, the angle setting between the first direction X and the second direction Y can be adjusted according to actual needs and application scenarios, and this embodiment does not limit this.

[0040] In the solar cell, the surface where the substrate 101 and the semiconductor conductive layer 102 contact is a smooth surface, and the carrier recombination on the surface where the substrate 101 and the semiconductor conductive layer 102 contact can be effectively controlled, thereby reducing the recombination current on the surface of the substrate 101. The semiconductor conductive layer 102 has a plurality of spherical protrusion structures 122 on a first surface 121 away from the substrate 101 along a first direction, and the morphology of the first surface 121 can be regarded as a rough surface with a plurality of protrusions. Since the first surface 121 is a rough surface, in the process of forming the dielectric layer 103 covering the spherical protrusion structures 122 and the first surface 121 exposed by the spherical protrusion structures 122, the stress on the dielectric layer 103 is significantly reduced. Therefore, the spherical protrusion structure 122 on the first surface 121 can significantly reduce the probability of film bursting on the surface of the dielectric layer 103, improve the surface morphology of the dielectric layer 103, and avoid the decrease in the passivation effect of the dielectric layer 103 due to film bursting, so that the dielectric layer 103 can effectively passivate the defects on the first surface 121 of the semiconductor conductive layer 102, thereby reducing the recombination current on the surface of the semiconductor conductive layer 102.

[0041] The electrode 104 penetrates the dielectric layer 103 and is in electrical contact with the semiconductor conductive layer 102. When there are multiple spherical protrusion structures 122 on the first surface 121, the specific surface area of ​​the electrode 104 in contact with the semiconductor conductive layer 102 can be increased, thereby reducing the contact resistance between the electrode 104 and the semiconductor conductive layer 102. Therefore, the filling factor and photoelectric conversion efficiency of the solar cell can be effectively improved. Among them, the material of the spherical protrusion structure 122 can be consistent with the semiconductor conductive layer 102, or a material with similar conductive properties to the semiconductor conductive layer 102. The material of the spherical protrusion structure 122 includes at least one of polycrystalline silicon, microcrystalline silicon, amorphous silicon, silicon carbide or titanium nitride.

[0042] In some embodiments, the substrate 101 may be a P-type semiconductor substrate or an N-type semiconductor substrate, wherein the N-type semiconductor substrate is doped with an N-type doping element, and the N-type doping element may be any one of the V-group elements such as phosphorus (P), bismuth (Bi), antimony (Sb), or arsenic (As). The P-type semiconductor substrate is doped with a P-type element, and the P-type doping element may be any one of the III-group elements such as boron (B), aluminum (Al), gallium (Ga), or indium (In).

[0043] It should be understood that the doping type of the semiconductor conductive layer 102 can be P-type or N-type. When the semiconductor conductive layer 102 and the substrate 101 have the same doping type, the ion doping concentration of the semiconductor conductive layer 102 is greater than the ion doping concentration of the substrate 101.

[0044] In some embodiments, the material of the substrate 101 may be an elemental semiconductor material, which is composed of a single element, such as silicon or germanium. The elemental semiconductor material may be single crystal, polycrystalline, amorphous, or microcrystalline (a state having both single crystal and amorphous states is called microcrystalline), for example, silicon may be at least one of single crystal silicon, polycrystalline silicon, amorphous silicon, or microcrystalline silicon.

[0045] In some embodiments, the material of the substrate 101 may also be a compound semiconductor material. Common compound semiconductor materials include, but are not limited to, silicon germanium, silicon carbide, gallium arsenide, indium gallium, perovskite, cadmium telluride, copper indium selenide, etc. The substrate 101 may also be a sapphire substrate, a silicon-on-insulator substrate, or a germanium-on-insulator substrate.

[0046] In some embodiments, the material of the semiconductor conductive layer 102 may be at least one of nanocrystalline silicon, polycrystalline silicon, microcrystalline silicon, amorphous silicon, silicon carbide, titanium nitride, and the like.

[0047] In some embodiments, the material of the electrode 104 may be one of copper, silver, tin, or aluminum, or an alloy of at least two of them.

[0048] In some embodiments, the density of the spherical protrusion structures 122 on the first surface 121 is 1×10 9 / cm 2 Up to 3×10 11 / cm 2 .

[0049] Referring to the above description and analysis of the semiconductor conductive layer 102 and the spherical protrusion structure 122, the main function of the spherical protrusion structure 122 is to reduce the stress on the dielectric layer 103 during the formation process by increasing the roughness of the first surface 121, thereby improving the film quality of the dielectric layer 103, which may reduce the probability of film bursting in the formed dielectric layer 103 and the impact of the film bursting on the quality of the dielectric layer 103.

[0050] The dielectric layer 103 is usually formed on the first surface 121 through a deposition process. When the first surface 121 is a smooth surface, according to the stress analysis during the deposition process, the dielectric layer 103 is subjected to a large stress during the deposition process, and the dielectric layer 103 is prone to film bursting, which in turn affects the film quality of the dielectric layer 103, resulting in a poor appearance of the dielectric layer 103, and even affects the hydrogen overflow of the dielectric layer 103, so that the dielectric layer 103 cannot effectively passivate the defects on the first surface 121. The first surface 121 is a smooth surface, which means that the flatness of the first surface 121 is higher than a certain level, for example, the depression depth of the pits or the protrusion height of the protrusions on the first surface 121 is less than 0.01nm, 0.02nm or 0.05nm.

[0051] The reason why the dielectric layer 103 is subjected to excessive stress is that the dielectric layer 103 is deposited as a whole on a smooth surface with a large area, and the spherical-like protrusion structure 122 reduces the stress on the dielectric layer 103 in that the spherical-like protrusion structure 122 is equivalent to changing the first surface 121 into a rough surface composed of multiple smooth curved surfaces and smooth areas divided into multiple areas by multiple smooth curved surfaces. By dividing the large smooth surface covered by the dielectric layer 103 into multiple small areas and curved surfaces, the stress on the dielectric layer 103 is reduced by means of stress dispersion or offset.

[0052] Therefore, in the process of setting the spherical protrusion structure 122, in order to prevent the spherical protrusion structure 122 from being unable to effectively realize the area division and the surface morphology transformation of the first surface 121, the density of the spherical protrusion structure 122 on the first surface 121 can be set at 1×10 9 / cm 2 Up to 3×10 11 / cm 2 In the range of, for example, 2×10 9 / cm 2 , 3×10 9 / cm 2 , 5×10 9 / cm 2 , 7.5×10 9 / cm 2, 1×10 10 / cm 2 , 2×10 10 / cm 2 , 4×10 10 / cm 2 , 8×10 10 / cm 2 , 1.25×10 11 / cm 2 , 1.75×10 11 / cm 2 or 2.5×10 11 / cm 2 The number of the spherical protrusion structures 122 on the first surface 121 is controlled within an appropriate range, so that there are enough smooth curved surfaces on the first surface 121 , thereby effectively reducing the stress on the dielectric layer 103 and improving the film quality of the dielectric layer 103 .

[0053] In some embodiments, the dielectric layer 103 serves as a passivation film layer or an anti-reflection film layer.

[0054] It should be understood that the distribution of the spherical protrusion structures 122 on the first surface 121 includes mutual spacing and partial overlap, that is, the various spherical protrusion structures 122 may be in a non-contact state, or some of the spherical protrusion structures 122 may partially overlap, and other spherical protrusion structures 122 may be spaced from each other. In addition, all the spherical protrusion structures 122 may partially overlap with at least one other spherical protrusion structure 122. In the embodiment of the present application, Figure 3 In the figure, various spherical protrusion structures are spaced apart from each other as an example. In addition, the spherical protrusion structure 122 may be located only on the first surface 121, or may be located on all surfaces of the semiconductor conductive layer 102 that are not in contact with the substrate 101. The local electron microscope image of the spherical protrusion structure 122 located on multiple surfaces of the semiconductor conductive layer 102 can be referred to. Figure 4 .

[0055] In some embodiments, the ratio of the area of ​​the first surface 121 covered by the spherical protrusion structures 122 to the area of ​​the first surface 121 is 0.3 to 1.

[0056] Referring to the above description and analysis of the influence of the spherical-like protrusion structure 122 on the morphology of the first surface 121, the purpose of setting the spherical-like protrusion structure 122 on the first surface 121 is to convert the surface of the semiconductor conductive layer 102 facing the dielectric layer 103 from the first surface 121, which is a smooth plane with a large area, to a rough surface composed of multiple smooth areas and multiple smooth curved surfaces, thereby reducing the stress on the dielectric layer 103 by means of stress dispersion and offset.

[0057] The spherical protrusion structures 122 on the first surface 121 can be arranged in a partially overlapping manner. Therefore, if various types of spherical protrusion structures 122 are concentrated in a certain area and overlapped, the spherical protrusion structures 122 cannot effectively adjust the morphological characteristics of the first surface 121. The first surface 121 can be regarded as consisting of a larger protrusion structure and a smooth plane that still has a larger area, and the protrusion structure cannot effectively disperse the stress on the dielectric layer 103.

[0058] Therefore, the ratio of the area covered by the spherical protrusion structure 122 on the first surface 121 to the area of ​​the first surface 121 itself can be set in the range of 0.3 to 1, for example, 0.325, 0.345, 0.4, 0.45, 0.55, 0.65, 0.8 or 0.95, etc. The spherical protrusion structure 122 on the first surface 121 has a sufficiently large coverage area, so that the area of ​​the first surface 121 exposed by the spherical protrusion structure 122 can be effectively reduced, thereby reducing the stress on the dielectric layer 103.

[0059] In some embodiments, the spherical protrusion structure 122 and the semiconductor conductive layer 102 are integrally formed.

[0060] In the process of preparing the spherical-like protrusion structure 122, the semiconductor conductive layer 102 may be formed first, so that the first surface 121 of the semiconductor conductive layer 102 is a smooth surface, and then a plurality of spherical-like protrusion structures 122 may be formed on the first surface 121 by a selective deposition process. In the process of preparing the spherical-like protrusion structure 122 in this way, the spherical-like protrusion structure 122 and the first surface 121 will inevitably form a contact cross section directly. When the electrode 104 is in electrical contact with the semiconductor conductive layer 102 through the spherical-like protrusion structure 122, it is easy to affect the contact resistance between the electrode 104 and the semiconductor conductive layer 102, thereby affecting the fill factor of the solar cell.

[0061] Therefore, in the process of preparing the semiconductor conductive layer 102 and the spherical convex structure 122 located on the first surface 121, they can be prepared by an integrated molding method. For example, in the process of forming the semiconductor conductive layer 102 located on the surface of the substrate 101 by a deposition process, the parameters of the deposition process are appropriately modulated so that multiple spherical convex structures 122 can be simultaneously formed on the surface of the semiconductor conductive layer 102 that is not in contact with the substrate 101 during the deposition process. Alternatively, an initial semiconductor conductive layer with a smooth surface is first formed on the surface of the substrate 101 by a deposition process, and then the surface of the initial semiconductor conductive layer away from the substrate 101 is processed by a patterning process and a selective etching method, so that the side of the initial semiconductor conductive layer away from the substrate 101 is formed, which can be regarded as consisting of a smooth first surface 121 and multiple spherical convex structures 122 located on the first surface 121, thereby forming the semiconductor conductive layer 102.

[0062] By setting the spherical protrusion structure 122 and the semiconductor conductive layer 102 as an integrally formed structure, the contact surface between the spherical protrusion structure 122 and the first surface 121 is avoided, and the interference of the contact resistance between the electrode 104 and the semiconductor conductive layer 102 is avoided, thereby reducing the carrier collection loss of the electrode 104 and improving the photoelectric conversion efficiency of the solar cell.

[0063] In addition, in the process of setting the spherical-like protrusion structure 122, the plurality of spherical-like protrusion structures 122 may include a first protrusion structure integrally formed with the semiconductor conductive layer 102 and a second protrusion structure not integrally formed with the semiconductor conductive layer 102. Since the spherical-like protrusion structure 122 on the first surface 121 is located in an area where the semiconductor conductive layer 102 is not in contact with the electrode 104, the second protrusion structure may be set on the first surface 121 corresponding to the area where the semiconductor conductive layer 102 is not in contact with the electrode 104, and the spherical-like protrusion structure 122 located in the area where the semiconductor conductive layer 102 is in contact with the electrode 104 is set to a structure integrally formed with the semiconductor conductive layer 102. The embodiment of the present application does not limit the setting of the spherical-like protrusion structure 122 on the first surface 121.

[0064] In some embodiments, along the first direction, a ratio between the thickness of the spherical protrusion structure 122 and the thickness of the semiconductor conductive layer 102 is 0.025 to 0.5.

[0065] Along the first direction, the thickness of any spherical protrusion structure 122 refers to the interval h1 between the highest point of the spherical protrusion structure 122 protruding from the first surface 121 and the first surface 121, and the thickness of the semiconductor conductive layer 102 refers to the average interval h2 between the surface where the semiconductor conductive layer 102 contacts the substrate 101 and the surface where the semiconductor conductive layer 102 contacts the dielectric layer 103.

[0066] Referring to the above description of the setting of the spherical protrusion structure 122, the purpose of setting the spherical protrusion structure 122 is to reduce the stress on the dielectric layer 103, and the mechanism of action is to adjust the surface morphology of the semiconductor conductive layer 102 toward the dielectric layer 103 to a concave-convex surface composed of multiple smooth areas and multiple smooth areas.

[0067] After the spherical protrusion structure 122 is provided, when the semiconductor conductive layer 102 is an integrally formed structure, it is equivalent to that the surface of the semiconductor conductive layer 102 away from the substrate 101 itself is a concave-convex surface. The greater the degree of concave-convexity of the surface of the semiconductor conductive layer 102 away from the substrate 101, the greater the carrier recombination on the surface of the semiconductor conductive layer 102, which easily leads to excessive recombination current on the surface of the semiconductor conductive layer 102, thereby affecting the photoelectric conversion efficiency of the solar cell. The degree of concave-convexity of the surface of the semiconductor conductive layer 102 away from the substrate 101 can be characterized by the ratio between the protrusion height of the spherical protrusion structure 122 and the thickness of the semiconductor conductive layer 102, that is, by the ratio between the average thickness of various spherical protrusion structures 122 and the thickness of the semiconductor conductive layer 102 along the first direction.

[0068] For the semiconductor conductive layer 102, along the first direction, if the ratio between the average thickness of the various spherical protrusion structures 122 and the thickness of the semiconductor conductive layer 102 is too large, the surface unevenness of the semiconductor conductive layer 102 away from the substrate 101 is too large, and the recombination of carriers on the surface of the semiconductor conductive layer 102 is too large, which will interfere with the filling factor and photoelectric conversion efficiency of the solar cell; if the ratio between the average thickness of the various spherical protrusion structures 122 and the thickness of the semiconductor conductive layer 102 is too small, the set spherical protrusion structures 122 cannot effectively change the morphology of the surface of the semiconductor conductive layer 102 facing the dielectric layer 103, and thus cannot effectively reduce the stress on the dielectric layer 103.

[0069] Therefore, in the process of setting the spherical protrusion structure 122, along the first direction, the ratio between the average thickness of each type of spherical protrusion structure 122 and the thickness of the semiconductor conductive layer 102 can be set in the range of 0.025 to 0.5, for example, 0.03, 0.035, 0.05, 0.075, 0.1, 0.15, 0.2, 0.3 or 0.4, etc. By setting the ratio between the average thickness of the spherical protrusion structure 122 and the thickness of the semiconductor conductive layer 102 in an appropriate range, the stress on the dielectric layer 103 is effectively reduced, the film forming quality of the dielectric layer 103 is improved, and the size of the composite current on the surface of the semiconductor conductive layer 102 facing the dielectric layer 103 is controlled to a small value, so as to avoid excessive negative impact of the spherical protrusion structure 122 on the photoelectric conversion efficiency of the solar cell.

[0070] In some embodiments, along the first direction, the thickness of the spherical protrusion structure 122 is 5 nm to 100 nm.

[0071] Referring to the above analysis and description of the thickness of the spherical protrusion structure 122, the semiconductor conductive layer 102 generally has a thickness in the range of 10nm to 200nm, for example, 15nm, 25nm, 50nm, 75nm, 120nm or 160nm, etc. Therefore, for any spherical protrusion structure 122, along the first direction, the thickness of the spherical protrusion structure 122 can be set in the range of 5nm to 100nm, for example, 5.5nm, 6.5nm, 8nm, 10nm, 12.5nm, 15nm, 20nm, 25nm, 35nm, 45nm, 60nm, 75nm or 90nm, etc. The thickness of each type of spherical protrusion structure 122 is set within an appropriate range to effectively control the composite current on the surface of the semiconductor conductive layer 102 and effectively reduce the stress on the dielectric layer 103. In addition, the thickness of each type of spherical protrusion structure 122 can be the same or different, and the embodiment of the present application does not limit this.

[0072] In some embodiments, along the second direction, the width of the spherical protrusion structure 122 is 10 nm to 200 nm.

[0073] For any spherical protrusion structure 122 , along the second direction, the width of the spherical protrusion structure 122 refers to the maximum interval W between any two points on the surface of the spherical protrusion structure along the second direction.

[0074] For any spherical-like protrusion structure 122, when the width of the spherical-like protrusion structure 122 along the second direction is too small, the surface area of ​​the spherical-like protrusion structure 122 is likely to be small, and the stress dispersion effect that the spherical-like protrusion structure 122 can play is also small, or even cannot play an effective stress dispersion role; when the width of the spherical-like protrusion structure 122 along the second direction is too large, the size of the spherical-like protrusion structure 122 itself is too large, and when adjacent spherical-like protrusion structures 122 partially overlap, the two smooth curved surfaces will form a morphology similar to a smooth plane after combination, which cannot effectively disperse stress and is also likely to cause excessive impact on the composite current on the surface of the semiconductor conductive layer 102.

[0075] Therefore, for any spherical protrusion structure 122, along the second direction, the width of the spherical protrusion structure 122 can be set in the range of 10nm to 200nm, for example, 12.5nm, 15nm, 20nm, 25nm, 35nm, 50nm, 75nm, 100nm, 140nm, 180nm or 190nm, etc. The width of each type of spherical protrusion structure 122 is set in an appropriate range to effectively control the recombination current on the surface of the semiconductor conductive layer 102 and effectively reduce the stress on the dielectric layer 103. In addition, the widths of the various spherical protrusion structures 122 can be the same or different, and the embodiment of the present application does not limit this.

[0076] refer to Figure 5 , Figure 5 Schematic diagram of a solar cell structure, wherein the X direction is the first direction and the Y direction is the second direction. In some embodiments, the solar cell further includes: a tunnel dielectric layer 105, the tunnel dielectric layer 105 is located between the substrate 101 and the semiconductor conductive layer 102, and covers the surface of the substrate 101 facing the semiconductor conductive layer 102, and the semiconductor conductive layer 102 covers the surface of the tunnel dielectric layer 105 away from the substrate 101.

[0077] The photoelectric conversion efficiency of solar cells is affected by the recombination of carriers in the solar cells. In the process of preparing solar cells, a tunnel dielectric layer 105 can be first formed on the surface of the substrate 101, and then a semiconductor conductive layer 102 can be formed on the surface of the tunnel dielectric layer 105 away from the substrate 101. By setting the tunnel dielectric layer 105 and the semiconductor conductive layer 102, the solar cell has a complete passivation contact structure, so that the ability of carriers of different polarities in the substrate 101 to reach the semiconductor conductive layer 102 through the tunnel dielectric layer 105 is significantly different, and the selective transmission of carriers is achieved. At the same time, good passivation is applied to the substrate 101 to reduce the recombination of carriers on the surface of the substrate 101 facing the semiconductor conductive layer 102, thereby reducing the recombination loss of the solar cell, and then improving the photoelectric conversion efficiency of the solar cell.

[0078] The material of the tunnel dielectric layer 105 includes at least one of silicon oxide, silicon nitride, silicon oxynitride, silicon carbide or magnesium fluoride.

[0079] In addition, the material of the dielectric layer 103 includes at least one of silicon oxide, aluminum oxide, silicon nitride, silicon carbide, titanium nitride, magnesium fluoride, or silicon oxynitride. The dielectric layer 103 may be a single-layer structure or a stacked-layer structure. For the stacked-layer structure, each layer is stacked in sequence along the first direction, and the materials of different layers may be different from each other, or the materials of some layers may be the same and different from the materials of other layers. For example, the stacked-layer structure may be a double-layer structure consisting of a stacked silicon nitride layer and an aluminum oxide layer.

[0080] It should be understood that not only can the morphology of the surface of the semiconductor conductive layer 102 away from the substrate 101 be changed by forming a spherical-like protrusion structure 122, but the spherical-like protrusion structure 122 can also be formed on the surface of the tunneling dielectric layer 105 away from the substrate 101, thereby reducing the stress on the semiconductor conductive layer 102 and improving the film forming quality of the semiconductor conductive layer 102. The thickness of the spherical-like protrusion structure 122 formed on the surface of the semiconductor conductive layer 102 along the first direction can be set between 0.025 times and 0.25 times the thickness of the tunneling dielectric layer 105 along the first direction.

[0081] In some embodiments, the substrate 101 includes a front side and a back side opposite to each other along a first direction, the tunneling dielectric layer 105 covers the back side of the substrate 101 , the doping type of the semiconductor conductive layer 102 is the same as the doping type of the substrate 101 , and the doping concentration of the semiconductor conductive layer 102 is greater than the doping concentration of the substrate 101 .

[0082] During the process of setting up solar cells, the two surfaces of the substrate 101 arranged opposite to each other along the first direction can be divided into the front side and the back side according to the design of the light-receiving surface of the solar cell, wherein the front side of the substrate 101 refers to the surface with higher incident light intensity, and the back side refers to the surface with lower incident light intensity.

[0083] A tunnel dielectric layer 105 is disposed on the back side of a substrate 101, and a semiconductor conductive layer 102 is formed on a surface of the tunnel dielectric layer 105 away from the substrate 101, so that the semiconductor conductive layer 102 and the substrate 101 have the same doping type, and the ion doping concentration of the semiconductor conductive layer 102 is higher than the ion doping concentration of the substrate 101, and a back passivation contact structure is formed on the back side of the substrate 101, thereby forming a tunnel dielectric layer passivated contact cell (Tunnel Oxide Passivated Contact solar cell, TOPCon), and the passivation contact structure formed by the tunnel dielectric layer 105 and the semiconductor conductive layer 102 provides good field passivation and surface passivation for the substrate 101, further reduces the carrier recombination loss on the back side of the substrate 101, and improves the photoelectric conversion efficiency of the solar cell.

[0084] In addition, reference Figure 6 The solar cell may further include an emitter 106, a front passivation layer 107 and a front electrode 108 located on the front side of the substrate 101, and the front electrode 108 penetrates the front passivation layer 107 and is in electrical contact with the emitter 106. The emitter 106 may include lightly doped regions and heavily doped regions arranged alternately, the ion doping concentration of the heavily doped regions is greater than the ion doping concentration of the lightly doped regions, and the front electrode 108 penetrates the front passivation layer 107 and is in electrical contact with the heavily doped regions. The surface of the emitter 106 facing the front passivation layer 107 may be a smooth surface, or a rough surface formed by providing a protruding structure similar to the spherical protruding structure 122, so as to improve the film forming quality of the front passivation layer 107, so that the front passivation layer 107 can play a good passivation role on the emitter 106, and further improve the photoelectric conversion efficiency of the solar cell.

[0085] The material of the emitter 106 is similar to that of the semiconductor conductive layer 102 , and the material of the front passivation layer 107 is similar to that of the dielectric layer 103 , which will not be described in detail herein.

[0086] refer to Figure 7 , Figure 7Schematic diagram of a solar cell structure, wherein the X direction is the first direction and the Y direction is the second direction. In some embodiments, the semiconductor conductive layer 202 includes first doping regions 223 and second doping regions 224 alternately arranged along the second direction, one of the first doping regions 223 and the second doping regions 224 is an N-type doping region and the other is a P-type doping region; the plurality of electrodes 204 include first electrodes 241 and second electrodes 242 alternately arranged along the second direction, the first electrode 241 is in electrical contact with the first doping region 223, and the second electrode 242 is in electrical contact with the second doping region 224.

[0087] Another major factor affecting the photoelectric conversion efficiency of solar cells is the light absorption of solar cells. When an electrode is arranged on the front of the solar cell, the electrode on the front of the solar cell will cause a certain degree of light shielding to the solar cell, thereby limiting the light absorption and photoelectric conversion efficiency of the solar cell. Among them, the substrate 201 is similar to the substrate 101 mentioned above, the dielectric layer 203 is similar to the dielectric layer 103 mentioned above, the first surface 221 is similar to the first surface 121, and the spherical protrusion structure 122 is similar to the spherical protrusion structure 222, which will not be repeated here.

[0088] Therefore, the semiconductor conductive layer 102 can be configured to be composed of the first doping region 223 and the second doping region 224 arranged alternately along the second direction, and one of the first doping region 223 and the second doping region 224 is an N-type doping region and the other is a P-type doping region, and then the electrode 204 is configured to be the first electrode 241 and the second electrode 242 arranged alternately in the second direction, the first electrode 241 is in electrical contact with the first doping region 223, and the second electrode 242 is in electrical contact with the second doping region 224, so that the two electrodes for collecting and transmitting carriers with different polarities can be both arranged on the back of the substrate 201, that is, to form an interdigitated back contact (IBC) battery. By arranging the electrodes for transmitting carriers of different polarities on the back of the solar cell, the electrodes are prevented from shielding the light on the front of the solar cell, the light absorption of the solar cell is improved, and the photoelectric conversion efficiency of the solar cell is thereby improved. Figure 7 Taking the example of only one first doping region 223 and one second doping region 224 , in a specific application, the number of the first doping region 223 and the number of the second doping region 224 can also be 2 or more.

[0089] In addition, a tunnel dielectric layer can be formed between the semiconductor conductive layer 202 and the substrate 201, wherein the tunnel dielectric layer is similar to the tunnel dielectric layer 105 mentioned above and will not be described in detail here. By utilizing the tunnel dielectric layer and the first doping region 223 and the second doping region 224, the selective permeability of holes of the portion of the tunnel dielectric layer facing the N-type doping region and the portion facing the P-type doping region are opposite, thereby further reducing the carrier recombination loss of the solar cell.

[0090] In addition, the solar cell may further include an anti-reflection layer located on the surface of the substrate 201 away from the semiconductor conductive layer 202. The anti-reflection layer is similar to the front passivation layer 107 mentioned above and will not be described in detail here. The anti-reflection layer can, on the one hand, passivate the substrate 202, and on the other hand, can also reduce the light reflection of the solar cell, thereby further improving the photoelectric conversion performance of the solar cell.

[0091] refer to Figure 8 , Figure 8 Schematic diagram of a solar cell structure, wherein the X direction is the first direction and the Y direction is the second direction. In some embodiments, the semiconductor conductive layer 302 further includes an isolation region 325 that penetrates the thickness of the semiconductor conductive layer 302 , and the isolation region 325 is located between the first doping region 323 and the second doping region 324 .

[0092] When forming an IBC battery, when the first doping region 323 and the second doping region 324 with different doping types in the semiconductor conductive layer 302 are in direct contact, it will affect the lifetime of the majority carriers and the carrier recombination loss of the solar cell, thereby affecting the lifetime and photoelectric conversion performance of the solar cell.

[0093] Therefore, the semiconductor conductive layer 302 can be configured to be composed of alternatingly arranged first doping regions 323 and second doping regions 324, and an isolation region 325 is provided between the first doping regions 323 and the second doping regions 324. The isolation region 325 can effectively isolate the first doping regions 323 and the second doping regions 324 to avoid carrier recombination between the first doping regions 323 and the second doping regions 324, thereby improving the photoelectric conversion efficiency and service life of the solar cell.

[0094] The isolation region 325 may be directly formed by a groove, or may be formed by filling the groove with a dielectric layer having good isolation capability, and this embodiment of the present application does not impose any limitation on this. Figure 8 In the description, the semiconductor conductive layer 302 includes a first doping region 323, a second doping region 324 and an isolation region 325 as an example. The number of the first doping region 323, the second doping region 324 and the isolation region 325 can also be 2 or more.

[0095] In addition, the solar cell may further include a tunneling dielectric layer formed between the semiconductor conductive layer 302 and the substrate 301, and may further include an anti-reflection layer located on the surface of the substrate 301 away from the semiconductor conductive layer 302, wherein the substrate 301, the tunneling dielectric layer, the electrode 304, the dielectric layer 303 and the anti-reflection layer are respectively similar to the aforementioned substrate 101, the tunneling dielectric layer 105, the electrode 104, the dielectric layer 103 and the front passivation layer 107, and are not described in detail here.

[0096] refer to Fig. 9 , Fig. 9 Schematic diagram of the structure of a solar cell, wherein the X direction is the first direction and the Y direction is the second direction. In some embodiments, the substrate 401 includes a front side and a back side opposite to each other along the first direction, the semiconductor conductive layer 402 includes a first semiconductor conductive layer 426 located on the front side of the substrate and a second semiconductor conductive layer 427 located on the back side of the substrate 401, and the solar cell further includes: an intrinsic semiconductor layer 409, the intrinsic semiconductor layer 409 includes a first intrinsic semiconductor layer 491 and a second intrinsic semiconductor layer 492; the first intrinsic semiconductor layer 491 covers the front side of the substrate, the first semiconductor conductive layer 426 covers the surface of the first intrinsic semiconductor layer 491 away from the substrate 401; the second intrinsic semiconductor layer 492 covers the back side of the substrate 401, and the second semiconductor conductive layer 427 covers the surface of the second intrinsic semiconductor layer 492 away from the substrate 401. The material of the intrinsic semiconductor layer 409 includes one of intrinsic single crystal silicon, intrinsic polycrystalline silicon or intrinsic amorphous silicon.

[0097] Among them, the substrate 401 is similar to the substrate 101 mentioned above, and will not be traced back here. The dielectric layer 403 includes a portion of the first semiconductor conductive layer 426 away from the surface of the substrate 401 and a portion of the second semiconductor conductive layer 427 away from the surface of the substrate 401. The dielectric layer 403 includes a transparent conductive layer formed of materials such as indium tin oxide, and can also be a film layer similar to the dielectric layer 103 mentioned above, which will not be repeated. Some electrodes 404 are in electrical contact with the first semiconductor conductive layer 426, and the remaining electrodes 404 are in contact with the second semiconductor conductive layer 426. The electrodes 404 are similar to the electrodes 104 mentioned above, and will not be repeated. The first semiconductor conductive layer 426 and the second semiconductor conductive layer 427 have different doping types, one is P-type doping and the other is N-type doping.

[0098] When forming a solar cell, an intrinsic semiconductor layer 409 and a first semiconductor conductive layer 426 and a second semiconductor conductive layer 427 having different doping types are used to form a heterojunction structure, thereby forming a heterojunction solar cell. The semiconductor conductive layer 402 is used to improve the film forming quality of the dielectric layer 403, which is beneficial to improving the carrier transmission efficiency and reducing carrier recombination.

[0099] refer to Fig.10 , Fig.10 Schematic diagram of a solar cell structure, wherein the X direction is the first direction and the Y direction is the second direction. In some embodiments, the semiconductor conductive layer 502 includes electrode regions 521 and non-electrode regions 522 alternately arranged along the second direction, the electrode regions 521 and the non-electrode regions 522 have the same doping type, and the doping concentration of the electrode regions 521 is greater than the doping concentration of the non-electrode regions 522.

[0100] The semiconductor conductive layer 502 can also be used as a selective emitter of the solar cell. When the semiconductor conductive layer 502 is set as a selective emitter, the semiconductor conductive layer 502 can be composed of alternately arranged electrode areas 528 and non-electrode areas 529, and the electrode 504 penetrates the dielectric layer 503 and is in electrical contact with the electrode area 528. The semiconductor conductive layer 502 can effectively reduce the stress of the dielectric layer 503, thereby improving the film quality of the dielectric layer 503 and reducing the carrier recombination loss on the front side of the solar cell. Among them, the substrate 501, the electrode 504, and the dielectric layer 503 are similar to the substrate 101, the electrode 104, and the dielectric layer 103 mentioned above, respectively, and will not be repeated here.

[0101] It is worth mentioning that the features in the above-mentioned embodiments can not only exist separately in the solar cell, but also, in the absence of technical conflicts and without exceeding the inventive concept of the embodiments of the present application, the features in the embodiments can also be implemented in combination with each other, and the embodiments of the present application will not be described in detail here.

[0102] In summary, the embodiment of the present application provides a solar cell, wherein the semiconductor conductive layer on the surface of the substrate has a plurality of spherical protrusion structures on the first surface away from the substrate in the first direction, and the dielectric layer is located on the first surface of the semiconductor conductive layer. That is to say, the surface where the semiconductor conductive layer contacts the dielectric layer has a plurality of spherical protrusion structures, and the dielectric layer contacts the surface with a relatively large roughness of the semiconductor conductive layer. Therefore, the stress effect on the dielectric layer during the formation process is greatly reduced, thereby significantly reducing the probability of the dielectric layer having a film burst phenomenon, that is, the probability of randomly distributed pits appearing on the surface of the dielectric layer is reduced, thereby reducing the probability of the dielectric layer having a passivation performance failure or an abnormal appearance, and improving the flatness of the dielectric layer surface and the overall yield of the dielectric layer. The electrode penetrates the dielectric layer and contacts the semiconductor conductive layer. When there are a plurality of spherical protrusions on the first surface of the semiconductor conductive layer, the specific surface area of ​​the electrode in contact with the semiconductor conductive layer is increased, thereby reducing the contact resistance between the electrode and the semiconductor conductive layer, thereby improving the filling factor and photoelectric conversion efficiency of the battery.

[0103] Accordingly, the present application embodiment also provides a photovoltaic assembly, referring to Fig.11 , including a battery string 1101, the battery string 1101 is formed by connecting a plurality of the above-mentioned solar cells and / or the batteries formed by the above-mentioned preparation method; a packaging layer 1102, the packaging layer 1102 is used to cover the surface of the battery string 1101; and a cover plate 1103, the cover plate 1103 is used to cover the surface of the packaging layer 1102 away from the battery string 1101. The solar cells are electrically connected in the form of a whole piece or multiple pieces to form a plurality of battery strings 1101, and the plurality of battery strings 1101 are electrically connected in series and / or in parallel.

[0104] In some embodiments, multiple battery strings 1101 may be electrically connected through a conductive tape 1104. The encapsulation layer 1102 covers the front and back sides of the solar cell. Specifically, the encapsulation layer 1102 may be an organic encapsulation film such as an ethylene-vinyl acetate copolymer (EVA) film, a polyethylene octene co-elastomer (POE) film, or a polyethylene terephthalate (PET) film. In some embodiments, the cover plate 1103 may be a glass cover plate, a plastic cover plate, or the like with a light-transmitting function. The surface of the cover plate 1103 facing the encapsulation layer 1102 may be a concave-convex surface, thereby increasing the utilization rate of the incident light.

[0105] Although the present application is disclosed as above with preferred embodiments, it is not intended to limit the claims. Any technical personnel in this field may make several possible changes and modifications without departing from the spirit and scope of the present application without departing from the concept of the present application. Therefore, the scope of protection of the present application shall be based on the scope defined by the claims of the present application.

Claims

1. A solar cell, characterized in that: include: substrate; A semiconductor conductive layer, the semiconductor conductive layer is located on the surface of the substrate, the semiconductor conductive layer includes a first surface away from the substrate along a first direction, and the first surface has a plurality of spherical protrusion structures; a dielectric layer, the dielectric layer being located on the first surface and covering the spherical protrusion structure and the first surface exposed by the spherical protrusion structure; A plurality of electrodes are arranged at intervals along the second direction, and the electrodes penetrate the dielectric layer and are in electrical contact with the semiconductor conductive layer.

2. The solar cell according to claim 1, characterized in that The density of the spherical protrusion structures on the first surface is 1×10 9 / cm 2 Up to 3×10 11 / cm 2 .

3. The solar cell according to claim 1, characterized in that The ratio of the area of ​​the first surface covered by the spherical protrusion structure to the area of ​​the first surface is 0.3 to 1.

4. The solar cell according to claim 1, characterized in that The spherical protrusion structure and the semiconductor conductive layer are an integrally formed structure.

5. The solar cell according to claim 1, characterized in that: Along the first direction, a ratio between a thickness of the spherical protrusion structure and a thickness of the semiconductor conductive layer is 0.025 to 0.

5.

6. The solar cell according to claim 5, characterized in that: Along the first direction, the thickness of the spherical protrusion structure is 5 nm to 100 nm.

7. The solar cell according to claim 1, characterized in that Along the second direction, the width of the spherical protrusion structure is 10 nm to 200 nm.

8. The solar cell according to claim 1, characterized in that Also includes: A tunneling dielectric layer is located between the substrate and the semiconductor conductive layer and covers a surface of the substrate facing the semiconductor conductive layer. The semiconductor conductive layer covers a surface of the tunneling dielectric layer away from the substrate.

9. The solar cell according to claim 8, characterized in that The substrate includes a front side and a back side opposite to each other along the first direction, the tunnel dielectric layer covers the back side of the substrate, the doping type of the semiconductor conductive layer is the same as the doping type of the substrate, and the doping concentration of the semiconductor conductive layer is greater than the doping concentration of the substrate.

10. The solar cell according to claim 8, characterized in that The semiconductor conductive layer comprises a first doping region and a second doping region alternately arranged along the second direction, one of the first doping region and the second doping region is an N-type doping region, and the other is a P-type doping region; The plurality of electrodes include first electrodes and second electrodes spaced apart along the second direction, the first electrodes are in electrical contact with the first doping region, and the second electrodes are in electrical contact with the second doping region.

11. The solar cell according to claim 10, characterized in that The semiconductor conductive layer further includes an isolation region that penetrates the thickness of the semiconductor conductive layer, and the isolation region is located between the first doping region and the second doping region.

12. The solar cell according to claim 1, characterized in that The substrate comprises a front side and a back side opposite to each other along the first direction, the semiconductor conductive layer comprises a first semiconductor conductive layer located on the front side of the substrate and a second semiconductor conductive layer located on the back side of the substrate, and the solar cell further comprises: an intrinsic semiconductor layer, the intrinsic semiconductor layer comprises a first intrinsic semiconductor layer and a second intrinsic semiconductor layer; The first intrinsic semiconductor layer covers the front surface of the substrate, and the first semiconductor conductive layer covers the surface of the first intrinsic semiconductor layer away from the substrate; The second intrinsic semiconductor layer covers the back side of the substrate, and the second semiconductor conductive layer covers the surface of the second intrinsic semiconductor layer away from the substrate.

13. The solar cell according to claim 1, characterized in that The semiconductor conductive layer includes electrode regions and non-electrode regions alternately arranged along the second direction, the electrode regions and the non-electrode regions have the same doping type, and the doping concentration of the electrode regions is greater than the doping concentration of the non-electrode regions.

14. A photovoltaic module, characterized in that: include: A battery string, wherein the battery string is formed by connecting a plurality of solar cells according to any one of claims 1 to 13; An encapsulation layer, the encapsulation layer is used to cover the surface of the battery string; A cover plate is used to cover a surface of the packaging layer away from the battery string.

Citation Information

Cited By

  • Solar cell and photovoltaic module

    CN119584714A

  • Solar cell and photovoltaic module

    CN120529704A