Test method for improving rock penetration detection effect
By applying strong sealant and vacuum saturation technology to the hot melt pipe, the problem of insufficient sealing in rock permeability test is solved, the accuracy of the test results is improved, and the reuse of the permeability device is realized, reducing the test cost.
Patent Information
- Application Number
- CN202411236444.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-11-26
AI Technical Summary
In the existing rock permeability test, there is a problem that the rock side wall is not tightly sealed and cannot be repeated, resulting in high test costs and large errors in the test results.
By applying strong sealant to the hot melt pipe, the rock sample and the inner wall of the hot melt pipe can be completely sealed, and the samples are efficiently saturated in the vacuum saturation device to form a hot melt layer of the hot melt pipe to achieve early sealing and later disassembly, improving Reusability of penetration devices.
It effectively solves the sealing problem between rock and permeability device, improves the accuracy of permeability coefficient test results, and realizes efficient reuse of permeability device.
Smart Images

Figure CN119023534A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an indoor rock permeability test device, in particular to a test method for improving rock permeability detection effect, and belongs to the technical field of rock hydrogeological parameter testing. Background Art
[0002] Rock permeability is one of the main research contents in rock mechanics teaching, scientific research and engineering practice, and has an important influence on the stress and stability of rocks. The determination of permeability coefficient is of great significance for understanding the permeability of rock and soil, conducting hydrogeological and groundwater calculations, etc. In practical applications, the measurement of permeability coefficient can be obtained through Darcy permeability device, field pumping, water injection and water pressure test. However, since the permeability of rocks is generally low, when testing the permeability of rocks, how to avoid seepage on the side wall of rock samples and ensure the accuracy of rock permeability coefficient test results is the most critical technical issue.
[0003] At present, when measuring the permeability coefficient of rock in indoor tests, the triaxial permeability test is generally used to test the permeability coefficient of rock. By adding a heat shrink tube to the side wall of the rock and applying confining pressure on its periphery, the heat shrink tube and the rock are tightly combined during the entire test process to ensure that no seepage occurs between the side wall of the rock and the heat shrink tube. However, the installation of the rock and the application of confining pressure during the test are relatively complicated. During the test, it is easy for the surrounding hydraulic oil to penetrate into the rock sample or for water to penetrate into the hydraulic oil, resulting in test failure, hydraulic oil pollution and equipment damage, making the cost of conducting rock permeability tests using this method very high.
[0004] In addition, there is also a method designed to test the permeability coefficient of rocks. The rock sample is directly placed in a high-strength sealed penetration device, and a strong glue is used to bond the rock side wall and the sealed container. In this case, the rock sample must be dry to ensure that there is no boundary seepage between the rock side wall and the penetration device, and then its permeability is tested by applying penetration pressure. However, this method still has the following problems: it is difficult to saturate the rock sample after the sample is loaded, and it is difficult to seal the side wall of the wet rock sample with the penetration device. Water will seep along the rock side wall, so there is a large error between the test result and the actual value; even if it can be completely sealed, after the penetration test is completed, due to the high strength of the strong glue, it is difficult to remove the rock sample, and the device cannot be used to repeat the test, which still makes the test cost high.
[0005] Therefore, it is urgent to design a test method for rock penetration detection, which can improve the penetration sealing performance and enable the test device to be used repeatedly and efficiently. Summary of the invention
[0006] The purpose of the present invention is to overcome the problems of poor sealing and inability to repeat the test in the existing rock penetration test in the rock side wall sealing, and to provide a test method for improving the rock penetration detection effect, by applying strong sealant in the hot melt tube to achieve complete sealing between the rock sample and the inner wall of the hot melt tube, and the heat shrink tube and the rock sample can be placed separately in a vacuum saturation device before installation for efficient saturation, thereby effectively solving the sealing problem between the rock and the penetration device and improving the accuracy of the rock permeability coefficient test results; by forming a hot melt layer of the hot melt tube between the hot melt tube and the rock penetration tank body, the early hot melt sealing and later hot melt disassembly between the rock sample and the inner wall of the rock penetration tank body are achieved, and the rock test sample can be efficiently and quickly installed and disassembled, thereby achieving efficient reuse of the penetration device.
[0007] To achieve the above object, the present invention adopts the following technical solution: a test method for improving the rock penetration detection effect, comprising the following steps:
[0008] S1. Install rock samples:
[0009] Select a hot melt tube of corresponding size according to the height and diameter of the rock sample, wherein the inner diameter of the hot melt tube is larger than the diameter of the rock sample, and the height of the hot melt tube is the same as that of the rock sample; wipe the outer surface of the rock sample dry, evenly apply strong sealant on the inner wall of the hot melt tube and the outer wall of the rock sample, and then fill the rock sample into the hot melt tube to make it fully bonded;
[0010] S2. Saturated rock sample:
[0011] Put the hot melt tube of the cemented rock sample into a saturation barrel for vacuum saturation. The vacuum conditions are: vacuum pressure of 100kPa, saturation time of more than 72h, so that the rock sample is fully saturated;
[0012] S3. Assemble and heat the penetration test device:
[0013] Assembly of the penetration test device: The penetration test device includes a rock penetration tank body, in whose inner wall a heating wire connected for heating the hot melt pipe is embedded, and an outlet penetration plate and an inlet penetration plate for penetrating the rock sample are respectively arranged at the upper and lower ends thereof, and an outlet sealing cover and an inlet sealing cover are installed at the two ends thereof to seal the rock penetration tank body; wherein the outlet sealing cover is connected to an outlet pipe connected to the outlet penetration plate, and the inlet sealing cover is connected to an inlet pipe connected to the inlet penetration plate, and an inlet water pressure sensor is installed on the inlet pipe, and an outlet water pressure sensor, an outlet flow meter and an outlet valve are installed on the outlet pipe in sequence from the inside to the outside, and the penetration of the rock sample is along the direction from the inlet pipe to the outlet pipe;
[0014] Heating of the permeability test device: Open the outlet sealing cover and the inlet sealing cover of the permeability test device, remove the outlet permeation plate and the inlet permeation plate, connect the external heating device to make the heating wire start to heat up and heat the inner wall of the rock permeability tank, wherein the horizontal distance between the heating wire and the inner wall of the rock permeability tank is 10-12 mm;
[0015] S4. Install the rock sample to the permeability test device:
[0016] When the heating wire is heated to the melting point of the hot melt tube, its temperature is 240℃~260℃, and the heating time is 15~20min. The rock sample installed in the hot melt tube and saturated is pressed into the penetration test device from the upper part of the penetration test device. During the pressing process, the outer wall of the hot melt tube is heated and melted to form a hot melt layer of the hot melt tube with a thickness of 1~2mm. After the hot melt tube is completely pressed into the penetration device, the external heating device of the heating wire is disconnected to stop heating, and the hot melt layer of the hot melt tube is solidified by the rapid condensation of the penetration test device heated by cooling water. The hot melt layer of the hot melt tube makes the hot melt tube and the inner wall of the rock penetration tank body sealed and connected;
[0017] After the permeability test device is cooled, the residues after the hot melt layer of the hot melt tube formed during the pressing process are cleaned, and the outlet permeation plate and the inlet permeation plate are respectively attached and connected to the upper and lower end surfaces of the rock sample, and the outer end surfaces of the outlet permeation plate and the inlet permeation plate are sealed by the outlet sealing cover and the inlet sealing cover;
[0018] S5. Start the seepage test:
[0019] Apply a predetermined water supply pressure of 0.5MPa or above to the water inlet pipe, and monitor the water pressure in real time through the water inlet water pressure sensor, and simultaneously monitor the flow rate of the water outlet flow meter and the pressure of the water outlet water pressure sensor, and calculate the permeability coefficient of the rock based on the monitoring results and Darcy's law;
[0020]
[0021] Where K is the permeability coefficient of the rock sample (cm / s); V is the volume of the seepage fluid flowing out at time T (cm 3 ); L is the height of the rock (cm); T is the time (s); A is the cross-sectional area of the rock sample (cm 2 ); ΔP is the osmotic pressure difference between the two ends of the rock sample (MPa);
[0022] S6. Remove the rock sample and repeat the next set of tests:
[0023] After the seepage test is completed, remove the upper and lower sealing covers and the upper and lower permeability plates of the permeability test device, and power the heating wire again for heating. When the hot melt tube begins to soften and melt inside the permeability test device, withdraw the rock sample and the hot melt tube together, and clean the inner wall of the permeability test device. After cleaning, replace the next set of rock samples and repeat the above steps to continue the test.
[0024] In step S1, the difference between the inner diameter of the hot melt tube and the diameter of the rock sample is within 1 mm. During the bonding process, the sealing condition between the side wall of the rock sample and the inner wall of the hot melt tube is checked, and strong sealant is further applied to the bonding pores to ensure that the rock sample and the inner wall of the hot melt tube are completely sealed.
[0025] The wall thickness of the hot melt pipe is greater than 5 mm, the hot melt pipe adopts PPR hot melt pipe, and the outer wall diameter of the hot melt pipe is greater than the inner diameter of the rock penetration tank body; the strong sealant adopts strong AB glue that can withstand 800 kg pulling force.
[0026] In step S3, the heating wire in the penetration test device is made of iron-chromium-aluminum alloy, with an inner diameter of 1 mm, and multiple wires are evenly embedded and connected along the vertical direction and parallel to the inner wall of the rock penetration tank, with a spacing of 20 mm between each wire; the heating wire is also connected to a heating wire electrode extending out of the inner wall of the rock penetration tank, and the heating wire electrode is connected to an external power supply to form an external heating device.
[0027] In step S4, during the sealing process of the permeability test device, the outlet permeation plate and the inlet permeation plate are gradually sealed, the outlet sealing ring and the inlet sealing ring are installed on the upper and lower end surfaces of the rock permeability tank body to seal the sealing rings, and the outlet sealing cover and the inlet sealing cover are respectively fastened to the end surface of the rock permeability tank body by the outlet sealing cover screws and the inlet sealing screws to seal the sealing cover, so that the permeability test device is completely sealed.
[0028] In step S4, the outlet permeation plate and the inlet permeation plate are both made of 304 stainless steel with a thickness of 20 mm, and are evenly arranged with a plurality of seepage holes with an inner diameter of 2 mm. The spacing between adjacent seepage holes is 4 mm, and the insides of the seepage holes are interconnected. The cross-sectional area of the outlet permeation plate and the inlet permeation plate is larger than the diameter of the rock sample.
[0029] The beneficial effects of the present invention are:
[0030] 1) In the test method of the present invention, a strong sealant is applied inside the hot melt tube to achieve complete sealing between the rock sample and the inner wall of the hot melt tube, and the heat shrink tube and the rock sample can be placed separately in a vacuum saturation device for efficient saturation before installation. By forming a hot melt layer of the hot melt tube between the hot melt tube and the rock penetration tank body, early hot melt sealing and later hot melt disassembly between the rock sample and the inner wall of the rock penetration tank body can be achieved, thereby effectively solving the sealing problem between the rock and the penetration device and improving the accuracy of the rock permeability coefficient test results; and the rock test sample can be efficiently and quickly installed and disassembled, realizing efficient reuse of the penetration device.
[0031] 2) The difference between the inner diameter of the hot melt tube in the test method of the present invention and the diameter of the rock sample is within 1 mm. At this time, it is easy to completely fill the pores between the outer wall of the rock sample and the inside of the hot melt tube by applying a strong sealant. After the strong sealant is solidified, a good sealing effect can be achieved. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 is a flow chart of the test method of the present invention;
[0033] Figure 2 is a cross-sectional view of a permeation test device used in the test method of the present invention;
[0034] Figure 3 for Figure 2 Cross-section of the rock sample in the hot melt tube after heating;
[0035] Figure 4 for Figure 2 Top view of the rock sample in the hot melt tube after heating.
[0036] In the figure, 1-water outlet valve, 2-water outlet flow meter, 3-water outlet water pressure sensor, 4-water outlet sealing cover screw, 5-water outlet sealing cover, 6-water outlet sealing ring, 7-water outlet penetration plate, 8-rock penetration tank body, 9-heating wire, 10-heating wire electrode, 11-water inlet sealing screw, 12-water inlet sealing ring, 13-water inlet sealing cover, 14-water inlet water pressure sensor, 15-water inlet pipe, 16-water inlet penetration plate, 17-strong sealant, 18-hot melt pipe, 19-rock sample, 20-water outlet pipe, 21-hot melt layer of hot melt pipe. DETAILED DESCRIPTION
[0037] The present invention is further explained below in conjunction with the accompanying drawings and specific embodiments.
[0038] Example: Figure 1 As shown, the present invention provides a test method for improving the rock penetration detection effect, comprising the following steps:
[0039] S1. Install rock samples:
[0040] A hot melt tube 18 of corresponding size is selected according to the height and diameter of the rock sample 19, wherein the inner diameter of the hot melt tube 18 is larger than the diameter of the rock sample 19, and the height of the hot melt tube 18 is the same as that of the rock sample 19; the outer surface of the rock sample 19 is wiped dry, and a strong sealant 17 is evenly applied on the inner wall of the hot melt tube 18 and the outer wall of the rock sample 19, and then the rock sample 19 is filled in the hot melt tube 18 to make it fully bonded.
[0041] The difference between the inner diameter of the hot melt tube 18 and the diameter of the rock sample 19 is within 1 mm. During the bonding process, the sealing condition between the side wall of the rock sample 19 and the inner wall of the hot melt tube 18 is checked, and a strong sealant 17 is further applied to the parts with bonding pores to ensure that the rock sample 19 and the inner wall of the hot melt tube 18 are completely sealed.
[0042] The wall thickness of the hot melt pipe 18 is greater than 5 mm. The hot melt pipe 18 adopts a PPR hot melt pipe. The outer wall diameter of the hot melt pipe 18 is greater than the inner diameter of the rock penetration tank body 8. The strong sealant 17 adopts a strong AB glue that can withstand a tensile force of 800 kg.
[0043] S2. Saturated rock sample:
[0044] The hot melt tube 18 after bonding the rock sample 19 is placed in a saturation barrel for vacuum saturation. The vacuum conditions are: the vacuum pressure is 100kPa. Due to the sealing of the rock side wall, the water inlet area is reduced during saturation. The saturation time is more than 72h, so that the rock sample 19 is fully saturated.
[0045] S3. Assemble and heat the penetration test device:
[0046] Assembly of the penetration test device: Figure 2 As shown, the permeability test device includes a rock permeability tank body 8, in the inner wall of which a heating wire 9 for heating a hot melt pipe 18 is embedded, and an outlet permeation plate 7 and an inlet permeation plate 16 for permeating a rock sample 19 are respectively arranged at the upper and lower ends thereof, and an outlet sealing cover 5 and an inlet sealing cover 13 are installed at the two ends thereof to seal the rock permeability tank body 8; wherein the outlet sealing cover 5 is connected to a water outlet pipe 20 connected to the outlet permeation plate 7, and the inlet sealing cover 13 is connected to a water inlet pipe 15 connected to the inlet permeation plate 16, and the inlet water pressure sensor 14 is installed on the inlet pipe 15, and the outlet water pressure sensor 3, the outlet flow meter 2 and the outlet valve 1 are installed on the outlet pipe 20 from the inside to the outside in sequence, and the penetration of the rock sample 19 is along the direction from the inlet pipe 15 to the outlet pipe 20.
[0047] The heating wire 9 in the penetration test device is made of iron-chromium-aluminum alloy with an inner diameter of 1 mm. There are multiple wires evenly embedded and connected along the vertical direction and parallel to the inner wall of the rock penetration tank 8, and the spacing between each wire is 20 mm. The heating wire 9 is also connected to a heating wire electrode 10 extending out of the inner wall of the rock penetration tank 8, and the heating wire electrode 10 is connected to an external power supply to form an external heating device.
[0048] Heating of the permeability test device: Open the outlet sealing cover 5 and the inlet sealing cover 13 of the permeability test device, remove the outlet permeation plate 7 and the inlet permeation plate 16, and connect the external heating device to make the heating wire 9 start to heat up and heat the inner wall of the rock permeation tank 8, wherein the horizontal distance between the heating wire 9 and the inner wall of the rock permeation tank 8 is 10-12 mm;
[0049] S4. Install the rock sample to the permeability test device:
[0050] like Figure 3 and Figure 4 As shown, when the heating wire 9 is heated to the melting point of the hot melt tube 18, its temperature is 240℃~260℃, and the heating time is 15~20min. The rock sample 19 installed in the hot melt tube 18 and saturated is pressed into the penetration test device from the upper part of the penetration test device. Since the outer wall diameter of the hot melt tube 18 is larger than the inner diameter of the rock penetration tank body 8, the outer wall of the hot melt tube 18 is heated and melted during the pressing process to form a hot melt layer 21 of the hot melt tube with a thickness of 1~2mm. After the hot melt tube 18 is completely pressed into the penetration device, the external heating device of the heating wire 9 is disconnected to stop heating, and the hot melt layer 21 of the hot melt tube is solidified by the cooling water after rapid condensation of the penetration test device after heating. The hot melt layer 21 of the hot melt tube makes the hot melt tube 18 and the inner wall of the rock penetration tank body 8 sealed and connected.
[0051] After the permeability test device has cooled down, clean the residue after the hot-melt layer 21 of the hot-melt tube 18 is formed during the pressing process, and fit the outlet permeation plate 7 and the inlet permeation plate 16 on the upper and lower end surfaces of the rock sample 19 respectively. The outer end surfaces of the outlet permeation plate 7 and the inlet permeation plate 16 are sealed by the outlet sealing cover 5 and the inlet sealing cover 13.
[0052] During the sealing process of the permeability test device, the outlet permeation plate 7 and the inlet permeation plate 16 are sealed step by step, the outlet sealing ring 6 and the inlet sealing ring 12 are installed on the upper and lower end surfaces of the rock permeability tank body 8 to seal the sealing rings, and the outlet sealing cover 5 and the inlet sealing cover 13 are respectively fastened to the end surfaces of the rock permeability tank body 8 by the outlet sealing cover screws 4 and the inlet sealing screws 11 to seal the sealing cover, so that the permeability test device is completely sealed.
[0053] The outlet permeation plate 7 and the inlet permeation plate 16 are both made of 304 stainless steel with a thickness of 20 mm. They are evenly arranged with multiple seepage holes with an inner diameter of 2 mm. The spacing between adjacent seepage holes is 4 mm. The insides of each seepage hole are interconnected, and the cross-sectional area of the outlet permeation plate 7 and the inlet permeation plate 16 is larger than the diameter of the rock sample 19.
[0054] S5. Start the seepage test:
[0055] Apply a predetermined water supply pressure of 0.5 MPa or more to the water inlet pipe 15, and monitor the water pressure in real time through the water inlet water pressure sensor 14, and simultaneously monitor the flow rate of the water outlet flow meter 2 and the pressure of the water outlet water pressure sensor 3, and calculate the permeability coefficient of the rock based on the monitoring results and Darcy's law;
[0056]
[0057] Where K is the permeability coefficient of the rock sample (cm / s); V is the volume of the seepage fluid flowing out at time T (cm 3 ); L is the height of the rock (cm); T is the time (s); A is the cross-sectional area of the rock sample (cm 2 ); ΔP is the osmotic pressure difference between the two ends of the rock sample (MPa).
[0058] S6. Remove the rock sample and repeat the next set of tests:
[0059] After the seepage test is completed, the upper and lower sealing covers and the upper and lower permeability plates of the permeability test device are removed, and the heating wire 9 is powered and heated again. When the hot melt tube 18 begins to soften and melt inside the permeability test device, the rock sample 19 and the hot melt tube 18 are withdrawn together, and the inner wall of the permeability test device is cleaned. After cleaning, the next group of rock samples 19 can be replaced and the above steps can be repeated to continue the test.
[0060] In the test method of the present invention, a strong sealant can be applied inside the hot-melt tube to achieve complete sealing between the rock sample and the inner wall of the hot-melt tube, and the heat shrink tube and the rock sample can be placed separately in a vacuum saturation device for efficient saturation before installation; thereby effectively solving the sealing problem between the rock and the penetration device, improving the sealing performance, and further improving the accuracy of the rock permeability coefficient test results.
[0061] By forming a hot melt layer between the hot melt tube and the rock penetration tank body, early hot melt sealing and later hot melt disassembly between the rock sample and the inner wall of the rock penetration tank body can be achieved, and the rock test sample can be installed and disassembled efficiently and quickly, thereby achieving efficient reuse of the penetration device.
[0062] The above description is only used to illustrate the technical solution of the present invention rather than to limit it. Other modifications or equivalent substitutions made to the technical solution of the present invention by ordinary technicians in this field should be included in the scope of the claims of the present invention as long as they do not depart from the spirit and scope of the technical solution of the present invention.
Claims
1. A test method for improving rock penetration detection effect, characterized in that: The following steps are involved: S1. Install rock samples: Select a hot melt tube of corresponding size according to the height and diameter of the rock sample, wherein the inner diameter of the hot melt tube is larger than the diameter of the rock sample, and the height of the hot melt tube is the same as that of the rock sample; wipe the outer surface of the rock sample dry, evenly apply strong sealant on the inner wall of the hot melt tube and the outer wall of the rock sample, and then fill the rock sample into the hot melt tube to fully bond it; S2. Saturated rock sample: Put the hot melt tube of the cemented rock sample into a saturation barrel for vacuum saturation. The vacuum conditions are: vacuum pressure of 100kPa, saturation time of more than 72h, so that the rock sample is fully saturated; S3. Assemble and heat the penetration test device: Assembly of the penetration test device: The penetration test device includes a rock penetration tank body, in whose inner wall a heating wire connected for heating the hot melt pipe is embedded, and an outlet penetration plate and an inlet penetration plate for penetrating the rock sample are respectively arranged at the upper and lower ends thereof, and an outlet sealing cover and an inlet sealing cover are installed at the two ends thereof to seal the rock penetration tank body; wherein the outlet sealing cover is connected to an outlet pipe connected to the outlet penetration plate, and the inlet sealing cover is connected to an inlet pipe connected to the inlet penetration plate, and an inlet water pressure sensor is installed on the inlet pipe, and an outlet water pressure sensor, an outlet flow meter and an outlet valve are installed on the outlet pipe in sequence from the inside to the outside, and the penetration of the rock sample is along the direction from the inlet pipe to the outlet pipe; Heating of the permeability test device: Open the outlet sealing cover and the inlet sealing cover of the permeability test device, remove the outlet permeation plate and the inlet permeation plate, connect the external heating device to make the heating wire start to heat up and heat the inner wall of the rock permeability tank, wherein the horizontal distance between the heating wire and the inner wall of the rock permeability tank is 10-12 mm; S4. Install the rock sample to the permeability test device: When the heating wire is heated to the melting point of the hot melt tube, its temperature is 240℃~260℃, and the heating time is 15~20min. The rock sample installed in the hot melt tube and saturated is pressed into the penetration test device from the upper part of the penetration test device. During the pressing process, the outer wall of the hot melt tube is heated and melted to form a hot melt layer of the hot melt tube with a thickness of 1~2mm. After the hot melt tube is completely pressed into the penetration device, the external heating device of the heating wire is disconnected to stop heating, and the hot melt layer of the hot melt tube is solidified by the rapid condensation of the penetration test device heated by cooling water. The hot melt layer of the hot melt tube makes the hot melt tube and the inner wall of the rock penetration tank body sealed and connected; After the permeability test device is cooled, the residues after the hot melt layer of the hot melt tube formed during the pressing process are cleaned, and the outlet permeation plate and the inlet permeation plate are respectively attached and connected to the upper and lower end surfaces of the rock sample, and the outer end surfaces of the outlet permeation plate and the inlet permeation plate are sealed by the outlet sealing cover and the inlet sealing cover; S5. Start the seepage test: Apply a predetermined water supply pressure of 0.5MPa or above to the water inlet pipe, and monitor the water pressure in real time through the water inlet water pressure sensor, and simultaneously monitor the flow rate of the water outlet flow meter and the pressure of the water outlet water pressure sensor, and calculate the permeability coefficient of the rock based on the monitoring results and Darcy's law; Where K is the permeability coefficient of the rock sample (cm / s); V is the volume of the seepage fluid flowing out at time T (cm 3 ); L is the height of the rock (cm); T is the time (s); A is the cross-sectional area of the rock sample (cm 2 ); ΔP is the osmotic pressure difference between the two ends of the rock sample (MPa); S6. Remove the rock sample and repeat the next set of tests: After the seepage test is completed, remove the upper and lower sealing covers and the upper and lower permeability plates of the permeability test device, and power the heating wire again for heating. When the hot melt tube begins to soften and melt inside the permeability test device, withdraw the rock sample and the hot melt tube together, and clean the inner wall of the permeability test device. After cleaning, replace the next set of rock samples and repeat the above steps to continue the test.
2. A test method for improving rock penetration detection effect according to claim 1, characterized in that: In step S1, the difference between the inner diameter of the hot melt tube and the diameter of the rock sample is within 1 mm. During the bonding process, the sealing condition between the side wall of the rock sample and the inner wall of the hot melt tube is checked, and strong sealant is further applied to the bonding pores to ensure that the rock sample and the inner wall of the hot melt tube are completely sealed.
3. A test method for improving rock penetration detection effect according to claim 1 or 2, characterized in that: The wall thickness of the hot melt pipe is greater than 5 mm, the hot melt pipe adopts PPR hot melt pipe, and the outer wall diameter of the hot melt pipe is greater than the inner diameter of the rock penetration tank body; the strong sealant adopts strong AB glue that can withstand 800 kg pulling force.
4. A test method for improving rock penetration detection effect according to claim 1, characterized in that: In step S3, the heating wire in the penetration test device is made of iron-chromium-aluminum alloy, with an inner diameter of 1 mm, and multiple wires are evenly embedded and connected along the vertical direction and parallel to the inner wall of the rock penetration tank, with a spacing of 20 mm between each wire; the heating wire is also connected to a heating wire electrode extending out of the inner wall of the rock penetration tank, and the heating wire electrode is connected to an external power supply to form an external heating device.
5. A test method for improving rock penetration detection effect according to claim 1, characterized in that: In step S4, during the sealing process of the permeability test device, the outlet permeation plate and the inlet permeation plate are gradually sealed, the outlet sealing ring and the inlet sealing ring are installed on the upper and lower end surfaces of the rock permeability tank body to seal the sealing rings, and the outlet sealing cover and the inlet sealing cover are respectively fastened to the end surface of the rock permeability tank body by the outlet sealing cover screws and the inlet sealing screws to seal the sealing cover, so that the permeability test device is completely sealed.
6. A test method for improving rock penetration detection effect according to claim 1, characterized in that: In step S4, the outlet permeation plate and the inlet permeation plate are both made of 304 stainless steel with a thickness of 20 mm, and are evenly arranged with a plurality of seepage holes with an inner diameter of 2 mm. The spacing between adjacent seepage holes is 4 mm, and the insides of the seepage holes are interconnected. The cross-sectional area of the outlet permeation plate and the inlet permeation plate is larger than the diameter of the rock sample.
Citation Information
Cited By
Dynamic heat-water-force coupling test device and test method
CN121454037A