Automobile interior composite material and manufacturing process thereof
By using a combination process of textured natural or imitation natural stone layer, PV or UV coating and injection molding layer in automotive interior materials, the problems of existing materials are solved, and rich visual and tactile sense are achieved Experience and low cost production.
Patent Information
- Application Number
- CN202411308162.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-19
- Publication Date
- 2024-11-29
AI Technical Summary
The existing automotive interior materials are not diverse enough, the experience is not rich enough, and it is difficult to meet personalized production needs at low cost.
Using natural or imitation natural stone layers with textures, combined with PV or UV coating and injection molding layer, the composite material is formed through the injection molding process, which not only retains the beautiful texture of the stone, but also overcomes the problems of easy wear and cracking, and uses convex texture. Layers enhance touch and visual effects.
It realizes diversified and rich visual and tactile experiences of automotive interior materials, reduces production costs, simplifies production processes, and improves the wear resistance and environmental protection of the materials.
Smart Images

Figure CN119036955A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of automobile decorative materials, and in particular to an automobile interior composite material and a manufacturing process thereof. Background Art
[0002] With the development of the times, cars have evolved from simple means of transportation to mobile spaces for people's lives, so people's requirements for the interior space of cars are also developing accordingly. Therefore, automotive interior materials have gradually evolved from traditional materials such as leather to various composite materials, because only composite materials can meet the diversified and personalized demand trends. For automotive interior materials, they must meet the different aesthetic requirements of different users, including high-end, luxurious, simple, and colorful. Accordingly, people not only have requirements for the visual beauty of automotive interior materials, but also for the sense of touch. Existing automotive interior materials cannot meet the needs of these new trends, or the production cost of meeting these personalized requirements is particularly high. Summary of the invention
[0003] In view of this, the technical problem to be solved by the present application is to provide a composite material for automotive interior and a manufacturing process thereof, so as to solve the problems of insufficient diversity and insufficient experience of automotive interior products in the prior art, as well as the problem of not being able to produce personalized interior composite materials at a relatively low cost.
[0004] To this end, the present application proposes a manufacturing process for a composite material for automotive interior, comprising the following steps:
[0005] A. Select a natural or imitation natural stone layer with texture, the thickness of the stone layer is between 0.1-3mm, and cut it into the required shape;
[0006] B. Coat the upper surface of the stone layer with a PV or UV coating, the thickness of the coating is 0.002-1.2mm. After the coating is cured, continue to put the stone layer into the injection mold for back skeleton injection molding to form the basic thickness and strength of the composite material; or put the stone layer into the injection mold for back skeleton injection molding to form the basic thickness and strength of the composite material, and then coat the upper surface of the stone layer with a PV or UV coating, the thickness of the coating is 0.002-1.2mm.
[0007] Another aspect of the present application provides an automotive interior composite material, comprising: a stone layer, which is a natural or simulated natural material with patterns, and the thickness of the stone layer is between 0.1 and 3 mm; a protective layer, which is a PV or UV coating coated on the upper surface of the stone layer, and the thickness of the coating is between 0.002 and 1.2 mm; and an injection molding layer, which is arranged on the lower surface of the stone layer to form the basic thickness and strength of the composite material, wherein the stone layer is fixed to the injection molding layer by injection molding.
[0008] The automotive interior composite material and its manufacturing process provided by the present application use a natural stone layer or an imitation natural stone layer with texture as the basic layer, and then set a coating on the stone layer and an injection molding layer below. This composite structure has the characteristics of beautiful texture of natural stone, and overcomes the shortcomings of easy wear and easy breakage of stone. The use of imitation natural stone also has the advantage of low cost; and the manufacturing process is simple. After the coating is set on the stone layer, it can protect the natural stone or imitation natural stone from damage during the injection molding process and resist wear in daily use; the stone layer and the injection molding layer are fixed by injection molding, the processing procedure is simple and more environmentally friendly, and can quickly meet the individual aesthetic requirements for automotive interior. The convex and concave texture layer enhances the three-dimensional sense of the automotive interior composite material, providing users with a strong tactile experience, and the protrusions on the surface of the material combined with the pattern inside the material can further enhance the aesthetic effect of the pattern, providing users with a rich visual and tactile experience. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 Shown is a schematic diagram of a process for manufacturing a composite material for automotive interior according to one embodiment of the present application.
[0010] Figure 2 Shown is a cross-sectional view of a composite material for automotive interior according to one embodiment of the present application. DETAILED DESCRIPTION
[0011] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application clearer and more understandable, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0012] Words related to directions in the present application, such as up, down, top, bottom, inside, outside, high, and low, are based on the position of the composite material under normal use.
[0013] In this application, the term PV, the full name of Polyvinyl, is a polyvinyl chloride material.
[0014] In order to provide a personalized automotive interior composite material with high production efficiency that meets personalized aesthetic needs, the present application provides a manufacturing process for an automotive interior composite material, comprising the following steps:
[0015] A. Select a natural or imitation natural stone layer with texture and cut it into the required shape. The thickness of the stone layer is between 0.1-3mm;
[0016] B. PV or UV coating is applied on the upper surface of the stone layer, and the thickness of the coating is 0.002-1.2mm. After the coating is cured, the stone layer is placed in the injection mold for back skeleton injection molding to form the basic thickness and strength of the composite material; or the stone layer is placed in the injection mold for back skeleton injection molding to form the basic thickness and strength of the composite material, and then PV or UV coating is applied on the upper surface of the stone layer, and the thickness of the coating is 0.002-1.2mm. A natural stone layer or an imitation natural stone layer with texture is used as the basic layer, and then a coating is set above the stone layer and an injection molding layer is set below. This composite structure has the characteristics of beautiful texture of natural stone, and overcomes the shortcomings of easy wear and easy breakage of natural stone or imitation natural stone. The use of imitation natural stone also has the advantage of low cost; and the production process is simple, which can quickly meet the individual aesthetic requirements for car interiors. The imitation natural stone layer is made of stone powder, resin, non-woven fabric or imitation stone grain material.
[0017] In at least one embodiment, the PV coating has a thickness of 0.01 mm to 1.2 mm.
[0018] In at least one embodiment, the thickness of the UV coating is 0.01 mm-0.5 mm.
[0019] In at least one embodiment, after step B, the step of performing multi-layer screen printing with UV ink on the upper surface of the coating and forming a convex-concave texture layer after drying is further included, and the thickness of the convex-concave texture layer is greater than 0.05 mm.
[0020] In at least one embodiment, the pattern of the convex-concave texture layer corresponds to the grain pattern of a natural or simulated-natural stone layer.
[0021] In at least one embodiment, the thickness of the convex-concave texture layer is between 0.05 mm and 0.2 mm.
[0022] Another aspect of the present application provides an automotive interior composite material, comprising:
[0023] The stone layer is a natural or natural-like material with patterns, and the thickness of the stone layer is between 0.1 and 3 mm;
[0024] The protective layer is a PV or UV coating applied on the upper surface of the stone layer, and the thickness of the coating is 0.002-1.2 mm; and
[0025] The injection molding layer is arranged on the lower surface of the stone layer to form the basic thickness and strength of the composite material; wherein the stone layer is fixed together with the injection molding layer by injection molding.
[0026] In at least one embodiment, the thickness of the PV coating is 0.01 mm-1.2 mm, and the thickness of the UV coating is 0.01 mm-0.5 mm.
[0027] In at least one embodiment, the upper surface of the coating includes a convex-concave texture layer formed by multi-layer screen printing, and the thickness of the convex-concave texture layer is greater than 0.05 mm; the convex-concave texture layer is a UV ink layer.
[0028] In at least one embodiment, the pattern of the convex-concave texture layer corresponds to the grain pattern of a natural or simulated-natural stone layer.
[0029] In at least one embodiment, the thickness of the convex-concave texture layer is between 0.05 mm and 0.2 mm.
[0030] The specific implementation process of the embodiments of the present application will be described in detail below with reference to the accompanying drawings:
[0031] like Figure 1 FIG. 1 is a schematic diagram of a process for manufacturing a composite material for automobile interior decoration according to one embodiment of the present invention, which includes the following steps:
[0032] A. First, select a natural or imitation natural stone layer with texture and cut it into the required shape. The thickness of the stone layer is between 0.1-3mm;
[0033] The stone layer also preferably has a thickness of 0.2 mm, 0.5 mm, 1 mm, 1.5 mm, 2 mm, 2.5 mm, etc.
[0034] B. Then, a PV or UV coating is applied on the upper surface of the stone layer, and the coating thickness is 0.002-1.2 mm. After the coating is cured, the stone layer is placed in the injection mold for back skeleton injection molding to form the basic thickness and strength of the composite material; or the stone layer is placed in the injection mold for back skeleton injection molding to form the basic thickness and strength of the composite material, and then a PV or UV coating is applied on the upper surface of the stone layer, and the coating thickness is 0.002-1.2 mm.
[0035] In one embodiment, after step B, the method further includes: performing multi-layer screen printing with UV ink on the upper surface of the coating and drying to form a convex-concave texture layer, wherein the thickness of the convex-concave texture layer is greater than 0.05 mm.
[0036] If a convex-concave texture layer formed by UV ink printing is provided on the upper surface of the coating, the convex-concave texture layer is UV cured after the injection molding layer is completed to enhance the strength of the convex-concave texture layer, but avoid the pattern formed by the UV ink from falling off.
[0037] In one embodiment, after completing step B, glue is applied to the edge of the composite material to further reinforce the composite material and prevent delamination of the composite material during a subsequent cleaning process.
[0038] The present application uses a natural or natural-like stone layer with texture as part of the composite material, and sets a coating on its surface and an injection molding layer on the bottom surface, so that the composite material used for automobile interior has the high-grade feeling of natural stone, but overcomes the shortcomings of the natural or natural-like stone layer such as easy wear, easy breakage, poor plasticity, etc. The natural-like stone layer further has the advantage of low cost. The UV curing time and sequence of the pattern layer formed after UV ink printing are arranged after the injection molding layer is formed, which can form the convex and concave feeling on the surface of the stone layer, effectively ensure the firmness of the UV ink pattern, and avoid the UV ink pattern from falling off.
[0039] like Figure 2 Another aspect of the present application is a cross-sectional view of a composite material for automotive interior, comprising: a stone layer 2, which is a natural or natural-like material with texture, and the thickness of the stone layer is between 0.1-3 mm. The upper surface of the stone layer 2 includes a PV or UV coating 1, and the thickness of the coating 1 is 0.002-1.2 mm; an injection molding layer 3 is also provided below the stone layer 2, which is the skeleton structure of the composite material for automotive interior to form the basic thickness and strength of the composite material, wherein the stone layer is fixed to the injection molding layer by injection molding. In one embodiment, a convex-concave texture layer formed by multi-layer screen printing and drying with UV ink is also provided above the coating 1, and its thickness is between 0.05 mm-0.2 mm, such as 0.1 mm, 0.15 mm, 0.18 mm, etc.; the convex-concave texture layer forms a convex-concave feeling on the upper surface of the stone layer 1, which enhances the feel of the composite material for automotive interior. The pattern texture of the convex-concave texture layer preferably corresponds to the texture of the stone layer, so that the composite material forms a unique three-dimensional sense of space.
[0040] The preferred embodiments of the present invention are described above with reference to the accompanying drawings, but the scope of the present invention is not limited thereby. A person skilled in the art may implement the present invention in a variety of variations without departing from the scope and essence of the present invention, such as using a feature of one embodiment to obtain another embodiment. Any modification, equivalent substitution and improvement made within the technical concept of the present invention shall be within the scope of the present invention.
Claims
1. A process for producing a composite material for automobile interior decoration, comprising the following steps: A. Select a natural or simulated natural stone layer with texture, the thickness of which is between 0.1-3 mm, and cut it into the required shape; B. Coating a PV or UV coating on the upper surface of the stone layer, the coating thickness is 0.002-1.2 mm, and after the coating is cured, the stone layer is further placed in the injection mold for back skeleton injection molding to form the basic thickness and strength of the composite material; or placing the stone layer in the injection mold for back skeleton injection molding to form the basic thickness and strength of the composite material, and then coating a PV or UV coating on the upper surface of the stone layer, the coating thickness is 0.002-1.2 mm.
2. The manufacturing process according to claim 1, characterized in that: The thickness of the PV coating is 0.01 mm-1.2 mm.
3. The manufacturing process according to claim 1, characterized in that: The thickness of the UV coating is 0.01 mm-0.5 mm.
4. The manufacturing process according to claim 1, characterized in that: The method further comprises the following steps after step B: performing multi-layer screen printing with UV ink on the upper surface of the coating and forming a convex-concave texture layer after drying, wherein the thickness of the convex-concave texture layer is greater than 0.05 mm.
5. The manufacturing process according to claim 4, characterized in that: The pattern of the convex-concave texture layer corresponds to the grain pattern of the natural or simulated-natural stone layer.
6. The manufacturing process according to claim 4, characterized in that: The thickness of the convex-concave texture layer is between 0.05 mm and 0.2 mm.
7. A composite material for automobile interior decoration, characterized in that include: The stone layer is a natural or natural-like material with patterns, and the thickness of the stone layer is between 0.1 and 3 mm; The protective layer is a PV or UV coating applied on the upper surface of the stone layer, and the thickness of the coating is 0.002-1.2 mm; as well as An injection molding layer is disposed on the lower surface of the stone layer to form a basic thickness and strength of the composite material; Wherein, the stone layer is fixed together with the injection molding layer by injection molding.
8. The composite material for automobile interior decoration according to claim 7, characterized in that: The thickness of the PV coating is 0.01 mm-1.2 mm, and the thickness of the UV coating is 0.01 mm-0.5 mm.
9. The composite material for automobile interior decoration according to claim 7, characterized in that: The upper surface of the coating comprises a convex-concave texture layer formed by multi-layer screen printing, the thickness of the convex-concave texture layer is greater than 0.05 mm; the convex-concave texture layer is a UV ink layer.
10. The composite material for automobile interior decoration according to claim 9, characterized in that: The pattern of the convex-concave texture layer corresponds to the grain pattern of the natural or simulated-natural stone layer.
Citation Information
Patent Citations
Composite material for automotive trim and manufacturing method
CN115610028A
Interior trim panel, interior trim part and interior trim system
CN220180707U
Automotive trim composite material
CN223327090U
Slate assembly having accommodating groove for fixing means
KR1020110138454A
Automobile-use interior material and method for manufacturing same
WO2016195213A1