Cylindrical lithium thionyl chloride primary battery with high reliability and safety
The cylindrical lithium thionyl chloride primary battery addresses voltage hysteresis and passivation issues by using a stainless steel shell and porous carbon electrodes, ensuring high energy density, reliability, and safety for marine survey and monitoring equipment.
Patent Information
- Application Number
- CN202420982503.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-08
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-05-08
AI Technical Summary
Lithium-ion batteries used in marine survey and monitoring equipment face challenges with high energy density, reliability, safety, small size, long service life, maintainability, multifunctional integration, and explosion-proof functions, particularly due to voltage hysteresis and passivation issues that affect performance and capacity.
A cylindrical lithium thionyl chloride primary battery design featuring a stainless steel shell, porous carbon package electrodes, and a diaphragm made of non-woven glass cloth, with a gas-tight structure and vacuum injection process to ensure reliable ion and electron conduction, minimizing passivation effects.
The battery achieves high energy density (35Ah), reliability, safety, small size, long service life, and stable voltage, meeting the requirements for marine survey and monitoring equipment with improved maintainability and explosion-proof capabilities.
Smart Images

Figure CN222106770U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of lithium battery chemistry, in particular to a cylindrical lithium thionyl chloride primary battery with high reliability and safety. Background Art
[0002] With the development of microelectronics technology in the 20th century, the number of miniaturized devices has increased, which has put forward high requirements on power supply. As a result, lithium batteries have entered the stage of large-scale practical use.
[0003] The earliest application was the lithium ion battery, which was used in cardiac pacemakers. Since the self-discharge rate of lithium ion batteries is extremely low and the discharge voltage is very gentle, it makes it possible to implant pacemakers in the human body for long-term use.
[0004] Li / SOCl2 batteries consist of a lithium negative electrode, a carbon positive electrode, and a non-aqueous SOCl2:LiAlCl4 electrolyte. Thionyl chloride is both the electrolyte and the positive electrode active material. Other electrolyte salts, such as LiAlCl4, have been used in specially designed batteries, but different electrolyte formulations have different electrode performance. The composition of the negative electrode, positive electrode, and SOCl2 is selected by the manufacturer based on the expected performance of the battery. The generally accepted overall reaction mechanism is:
[0005] 4Li+2SOCl2→4LiCl+S↓+SO2
[0006] Nowadays, lithium-ion batteries have been widely used in smart electricity meters, water meters, heat meters, gas meters, memory backup, clock power supplies, data backup power supplies, smoke alarms, temperature monitors, positioning devices, marine remote controls, tire pressure monitoring systems, ETC (non-stop toll collection systems), automated instruments and equipment, oil wells, mines, medical equipment, anti-theft alarms, wireless communications, marine lifesaving, aviation, aerospace, marine electronics, land and air weapons, etc. They are also used in marine survey and monitoring equipment, but there are higher requirements for batteries for marine survey and monitoring equipment: The batteries for marine survey and monitoring equipment have the following requirements:
[0007] (1) High energy density: Marine survey and monitoring equipment needs to work on the seabed for a long time, so the battery is required to have a high energy density to ensure the endurance of the equipment.
[0008] (2) High reliability: The seabed environment is complex, and batteries need to withstand various tests, including temperature, pressure, salinity, corrosion and other factors, so the batteries are required to have high reliability.
[0009] (3) Safety: The seabed environment is prone to safety issues, so the battery is required to have high safety and will not affect the safe use of the equipment due to leakage, explosion and other problems.
[0010] (4) Small size: The size of marine survey and monitoring equipment is limited, so the battery must be small in size so that it can carry more power.
[0011] (5) Long service life: Marine survey and monitoring equipment needs to be used multiple times, so the battery is required to have a long service life and be able to withstand the test of multiple charging and discharging.
[0012] (6) Good maintainability: Marine survey and monitoring equipment requires regular maintenance and battery replacement during operation, so the battery must be maintainable and easy to replace.
[0013] (7) Multifunctional integration: The battery should have multiple functions, such as built-in protection, monitoring, power control and battery conditioning, to meet the use requirements of the equipment in various environments.
[0014] (8) Explosion-proof function: Batteries used in flameproof enclosures should be protected from flammable mixtures formed by electrolytic gases (usually hydrogen and oxygen). Batteries that may release electrolytic gases during normal use should not be used in flameproof enclosures.
[0015] In short, the batteries for marine survey and monitoring equipment need to have many advantages, such as high energy density, high reliability, safety, small size, long service life, good maintainability, multi-functional integration and explosion-proof function. These requirements are to ensure that the equipment can operate reliably and conduct effective detection and monitoring in the complex environment of the seabed.
[0016] However, the lithium-ion battery produced by the prior art has the following disadvantages:
[0017] 1. The voltage hysteresis caused by the passivation of lithium-ion batteries after long-term non-operation may cause the load to work under voltage or fail to start. The voltage hysteresis phenomenon is most obvious when the battery is discharged at low temperature after long-term storage at high temperature;
[0018] 2. The batteries for marine survey and monitoring equipment need to have many advantages such as high energy density, high reliability, safety, small size, long service life, good maintainability, multi-functional integration and explosion-proof function. The battery model ER341245 (nominal capacity: 35Ah, size: diameter 34mm Max, height 124.5mmMax) that is closest to the existing lithium-ion cylindrical battery does not meet the small size requirement, while the nominal capacity of other models of lithium-ion batteries cannot reach 35Ah.
[0019] The lithium-ion battery produced by the prior art has the following disadvantages:
[0020] The hysteresis of lithium-thionyl chloride battery is due to the reaction of Li and SOCl2 after long-term storage, which will produce a dense passivation film on the surface of metallic lithium. The passivation film can prevent Li and SOCl2 from further reacting. Therefore, when the battery is connected to the load for the first time after storage, voltage hysteresis will occur. However, as the battery discharges, the passivation film will gradually be eliminated, and the load voltage will gradually rise. Battery hysteresis has both advantages and disadvantages: the advantage is that the reaction of Li and SOCl2 can produce a dense passivation film to prevent the reaction from further proceeding, so the storage time of lithium-thionyl chloride battery can reach more than 10 years; the disadvantage is that after long-term storage of lithium-thionyl chloride battery, the battery passivation will reduce the large current pulse output capability, so that the instantaneous minimum voltage of the battery may be lower than the cut-off voltage of the application.
[0021] Therefore, developing a lithium-ion battery with high capacity, small size and appropriate weight has become a new trend. Utility Model Content
[0022] The purpose of the utility model is to meet the requirements of the battery of the seabed detection and monitoring equipment with high energy density, high reliability, safety, small size, long service life, good maintainability, multi-functional integration and explosion-proof function. The cylindrical high-reliability and safety cylindrical lithium thionyl chloride primary battery (model: ER41720, nominal capacity: 35Ah, size: diameter 43mm Max, height 73mm Max, weight: 245g Max) of the utility model just meets the requirements of seabed detection; although battery passivation is inevitable, its influence can be minimized to meet the use requirements.
[0023] In order to achieve the above technical objectives, the utility model adopts the following technical solutions:
[0024] A highly reliable and safe cylindrical lithium thionyl chloride primary battery comprises an inner and outer part. The outer part comprises an outer shell, a cover assembly and a sealing nail. The positive electrode and the negative electrode of the inner part are separated by a diaphragm. Plastic sheets are attached to the top and the bottom. The negative electrode is made of a lithium sheet and leans against the inner wall of the outer shell. The diaphragm is made of non-woven glass cloth. The positive electrode is composed of a carbon bag and contacts the diaphragm. The internal current collecting part is spot welded by a positive electrode column, a current collecting ring and a current collecting nickel needle spot welding machine.
[0025] Furthermore, the shell is a stainless steel shell.
[0026] Furthermore, the shell is formed by welding a stainless steel tube and a bottom cover, and the welding process is argon arc welding.
[0027] Furthermore, the dimensions of the stainless steel tube are: outer diameter Φ42.65±0.1mm, inner diameter Φ40.46-0.06mm, length Φ70.5±0.1mm; the dimensions of the bottom cover are: diameter Φ40.5±0.04mm, thickness Φ2±0.05mm.
[0028] Furthermore, the cover assembly is formed by sintering a cover plate, a positive electrode column, and insulating glass.
[0029] Furthermore, the dimensions of the cover assembly are: diameter Φ40.5±0.04mm, thickness Φ2±0.05mm, and injection hole diameter Φ1.1+0.03mm.
[0030] Furthermore, the stainless steel pipe, the bottom cover and the cover plate are all cut by a lathe, and the material is all SUS304.
[0031] Furthermore, the plastic sheet is a polytetrafluoroethylene plastic sheet.
[0032] Furthermore, the dimensions of the collecting ring are: outer diameter Φ21±0.1 mm, inner diameter Φ20.2±0.1 mm, and thickness Φ4±0.2 mm.
[0033] Furthermore, the dimensions of the current collecting nickel needle are: length Φ57.5±0.5mm, diameter Φ1.2±0.05mm.
[0034] Compared with the prior art, the utility model has the following advantages:
[0035] Compared with the existing lithium-ion battery, the utility model has the advantages of high energy density (nominal capacity of 35Ah), high reliability and safety (passed UL, CE, SGS, ISO9001 quality management system certification), small size, long service life, wide operating temperature range (-60℃~+85℃), stable high operating voltage (at room temperature, open circuit voltage ≥3.64V, load voltage ≥3.35V), constant current discharge test with 100mA current on the discharge equipment, and can discharge a capacity of more than 23000mAh. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 The dimensional diagram of the cylindrical lithium thionyl chloride primary battery with high reliability and safety of the utility model;
[0037] Figure 2 The utility model is a schematic diagram of the basic structure of a cylindrical lithium thionyl chloride primary battery with high reliability and safety. DETAILED DESCRIPTION
[0038] The utility model is further described below in conjunction with the accompanying drawings.
[0039] like Figure 1 , 2 As shown, the utility model has a high reliability and safety cylindrical lithium thionyl chloride primary battery, which consists of two parts, the inner and outer parts. The outer part consists of a stainless steel shell (steel tube + bottom cover), a cover assembly and a sealing nail. The outer steel shell is welded by a stainless steel tube and a bottom cover, and the welding process is argon arc welding. The cover assembly is sintered by a cover plate, a positive pole and an insulating glass. The stainless steel tube, the bottom cover and the cover plate are cut by a lathe, and the material is SUS304. The positive and negative electrodes inside are separated by a diaphragm, and polytetrafluoroethylene (PTFE) plastic sheets are attached to the top and bottom. The negative electrode in the battery preparation under this process is made of a lithium sheet (sprayed with a coating liquid) and leans against the inner wall of the stainless steel shell. The diaphragm is made of non-woven glass cloth (glass fiber), and the positive electrode is composed of positive electrode particles with a polytetrafluoroethylene binder component (hereinafter referred to as "carbon package"), which has an extremely high porosity. During assembly, the positive electrode can directly enter the interior of the battery shell and contact the diaphragm, and occupy most of the volume of the battery to promote ion conduction. This process can give full play to the advantages of the integrated molding process; the battery is a gas-tight structure, and the positive electrode column of the cover group adopts a glass-metal sealing insulator; under the vacuum injection process, the positive electrode structure of the battery will not be affected when the shell is evacuated, thereby avoiding the fracture problem caused by the misalignment of the positive electrode; in the porous structure of the carbon package, the battery cell is filled with free electrolyte to ensure that the positive electrode part can always be in an infiltrated state, realizing rapid conduction between electrons and ions and ensuring the performance of the battery.
[0040] exist Figure 2 The basic structure of the cylindrical lithium thionyl chloride primary battery with high reliability and safety is shown in the relevant information. From top to bottom, the dimensions are as follows:
[0041] The dimensions of the cover assembly 1 are: diameter Φ40.5±0.04mm, thickness Φ2±0.05mm, and injection hole diameter Φ1.1+0.03mm;
[0042] The dimensions of the steel pipe 2 are: outer diameter Φ42.65±0.1mm, inner diameter Φ40.46-0.06mm, length Φ70.5±0.1mm;
[0043] The dimensions of the PTFE upper film 3 are: diameter Φ31*2±0.1mm, thickness Φ0.2±0.02mm;
[0044] The dimensions of the glass fiber cover film 4 are: diameter Φ44±0.1mm, thickness Φ0.2±0.02mm;
[0045] The dimensions of the collector ring 5 are: outer diameter Φ21±0.1mm, inner diameter Φ20.2±0.1mm, thickness Φ4±0.2mm;
[0046] The dimensions of the current collecting nickel needle 6 are: length Φ57.5±0.5mm, diameter Φ1.2±0.05mm;
[0047] The dimensions of the lithium ribbon 7 are: length Φ114.5+1mm, width Φ58+0.5mm, thickness Φ2.6±0.02mm, and weight 9.2-9.5g;
[0048] The dimensions of the glass fiber edge film 8 are: length Φ130+1mm, width Φ67+0.5mm, thickness Φ0.3±0.02mm;
[0049] The dimensions of the glass fiber bottom film 9 are: diameter Φ47±0.1mm, thickness Φ0.2±0.02mm;
[0050] The dimensions of the PTFE base film 10 are: diameter Φ33±0.1mm, thickness Φ0.2±0.02mm;
[0051] The dimensions of the bottom cover 11 are: diameter Φ40.5±0.04 mm, thickness Φ2±0.05 mm.
[0052] In order to achieve the design goal of a cylindrical lithium thionyl chloride primary battery with high reliability and safety, the key processes used in this utility model include:
[0053] a. The selected battery positive electrode is a carbon package (7-8 mesh, diameter: 1.5-2.5mm, weight 9.3-9.4g), the material composition is composed of acetylene black, RW, alcohol, pure water (conductivity ≤1μS) and binder polytetrafluoroethylene. This material has low installation difficulty and high strength; at the same time, due to the porous structure of the carbon package, the material can maintain contact with the battery separator after being loaded into the shell, and the design of the porous loose structure can enhance the battery pulse capability. Under ideal room temperature conditions, the negative voltage value of the battery is maintained above 3.35V.
[0054] b. The selected cover group 1 is sintered by a cover plate, a positive pole, and an insulating glass, and is penetrated with a polytetrafluoroethylene upper film 3. The current collector is welded by a current collector ring 5 and six equidistant nickel needles 6. The connection between the cover group 1 and the current collector is made by two pure nickel strips (length 48 mm) folded in half into an eight-shaped shape, with the heads spot welded to the positive pole of the cover group 1, and the tails of the four nickel strips are symmetrically spot welded to the current collector ring. The fixed connection process is spot welding with a spot welding machine.
[0055] The manufacturing method of the high-performance lithium thionyl chloride battery pack of the utility model comprises the following steps:
[0056] (i) Negative electrode shelling: After the lithium ribbon 7 is cut, it is placed on the lithium winding rod, manually rolled into a cylindrical shape, and placed in the steel shell.
[0057] (ii) Installing the polytetrafluoroethylene bottom membrane 10 and the glass fiber bottom membrane 9. After the polytetrafluoroethylene bottom membrane 10 and the glass fiber bottom membrane 9 are cut out by a cutting machine, they are pressed into the bottom position of the steel shell respectively.
[0058] (iii) When installing the diaphragm sheet 8, a glass fiber membrane of appropriate length can be cut out on a cutting machine, and then the material is manually rolled into a cylindrical shape and loaded into the negative electrode steel shell.
[0059] (iv) Install the carbon package, put the carbon package into the shell and press it, at this time the carbon package and the negative electrode lithium 7 are separated by the diaphragm. Previously, when preparing the carbon package, acetylene black, RW, alcohol, pure water and binder polytetrafluoroethylene can be prepared, and after being evenly mixed in a powder mixer according to an appropriate ratio, the materials are extruded and shot blasted. After the formed carbon package is left to stand, it is placed in a baking oven for baking. RW: RW used in carbon black is a coupling agent (additive) used to improve the interfacial interaction between carbon black and the polymer matrix, thereby improving the mechanical and electrical properties of the composite material.
[0060] (V) In installing the glass fiber cover film 4, it can be prepared into a specific specification according to the processing technology and then stamped on the top surface of the carbon package.
[0061] (VI) When installing the cover assembly 1 and adding the current collector, the steel shell can be fixed on the fixture, and its current collector nickel needle 6 can be inserted into the carbon bag under the glass fiber cover film 4.
[0062] (VII) Setting the sealing cover. After the positive pole current collecting ring 5 and the current collecting nickel needle 6 are connected by spot welding, they are compressed and sealed, and finally sealed by argon arc welding.
[0063] (VIII) Injecting electrolyte: Injecting electrolyte through full vacuum liquid injection equipment, such as the process described in the utility model using lithium aluminum tetrachloride thionyl chloride solution.
[0064] (IX) Install the sealing nails. After the injection hole is compacted with the sealing nails, assemble the battery cells, and finally clean the assembled battery cells.
[0065] (10) Static aging. After the semi-finished battery cells are assembled, they are left to stand and age. After aging, the battery cells are packaged with film to make finished batteries.
[0066] In order to make the present invention more fully disclosed, it is described below through more specific embodiments.
[0067] Example 1
[0068] like Figure 2 As shown, the basic structure and dimensions of a cylindrical lithium thionyl chloride primary battery with high reliability and safety are as follows:
[0069] Cover set 1: diameter 40.46mm, thickness 2.01mm, injection hole diameter 1.11mm;
[0070] Steel pipe 2: outer diameter 42.70mm, inner diameter 40.45mm, length 70.60mm;
[0071] PTFE upper film 3: diameter 31.26mm, thickness 0.22mm;
[0072] Glass fiber cover film 4: diameter 44.02mm, thickness 0.22mm;
[0073] Collector ring 5: outer diameter 20.94mm, inner diameter 20.15mm, thickness 3.89mm;
[0074] Current collecting nickel needle 6: length 57.91mm, diameter 1.18mm;
[0075] Lithium belt 7: length 114.57mm, width 58.42mm, thickness 2.62mm, weight 9.36g;
[0076] Glass fiber edge film 8: length 130.23mm, width 67.45mm, thickness 0.31mm;
[0077] Glass fiber bottom film 9: diameter 47.06mm, thickness 0.22mm;
[0078] PTFE bottom film 10: diameter 33.03mm, thickness 0.22mm;
[0079] Bottom cover 11: diameter 40.47mm, thickness 1.91mm.
[0080] The method for manufacturing a cylindrical lithium thionyl chloride primary battery pack with high reliability and safety comprises the following steps:
[0081] (I) Negative electrode into the shell. After the lithium ribbon 7 is cut, it is placed on the lithium winding rod, manually rolled into a cylindrical shape, and placed into the steel shell. At this time, the height × thickness of the lithium ribbon 7 = 114.57 mm × 2.62 mm.
[0082] (ii) Installing the polytetrafluoroethylene bottom membrane 10 and the glass fiber bottom membrane 9. After the polytetrafluoroethylene bottom membrane 10 and the glass fiber bottom membrane 9 are cut out by a cutting machine, they are pressed into the bottom position of the steel shell respectively.
[0083] (iii) When installing the diaphragm sheet 8, first cut a glass fiber membrane of appropriate length on a cutting machine, and then manually roll the material into a cylindrical shape and load it into the negative electrode steel shell.
[0084] (IV) Install the carbon package, put the carbon package into the shell and press it, at this time, the carbon package and the negative electrode lithium 7 are separated by the diaphragm. Before preparing the carbon package, acetylene black, RW, alcohol, pure water (conductivity is 1μS) and binder polytetrafluoroethylene are prepared, and according to the appropriate ratio (the mass ratio of acetylene black, RW, alcohol, pure water, binder polytetrafluoroethylene = 18:2:60:24:3) are evenly mixed in the powder mixer, and then the materials are extruded and shot blasted. After the formed carbon package is left to stand, it is baked in the baking oven.
[0085] (V) Installing the glass fiber cover film 4, after it is prepared into a specific specification (diameter 44.02mm, thickness 0.22mm) according to the processing technology, it is stamped on the top surface of the carbon package.
[0086] (VI) When installing the cover assembly 1 and adding the current collector, fix the steel shell on the fixture, and insert the current collector nickel needle 6 into the carbon bag under the glass fiber cover film 4. The insertion depth of the current collector nickel needle 6 is 53 mm.
[0087] (VII) Setting the sealing cover. After the positive pole current collecting ring 5 and the current collecting nickel needle 6 are connected by spot welding, they are compressed and sealed, and finally sealed by argon arc welding.
[0088] (VIII) Injecting electrolyte: Inject electrolyte through full vacuum liquid injection equipment, the electrolyte is lithium aluminum tetrachloride thionyl chloride solution, and the specification of the solution is 15 mol / L.
[0089] (IX) Install the sealing nails. After the injection hole is compacted with the sealing nails, assemble the battery cells, and finally clean the assembled battery cells.
[0090] (10) Static aging. After the semi-finished battery cells are assembled, they are left to stand and age. After aging, the battery cells are packaged with film to make finished batteries.
[0091] Example 2
[0092] like Figure 2 As shown, the basic structure dimensions of a cylindrical lithium thionyl chloride primary battery with high reliability and safety are as follows: Cover group 1: diameter 40.51mm, thickness 2.00mm, injection hole diameter 1.12mm;
[0093] Steel pipe 2: outer diameter 42.74mm, inner diameter 40.46mm, length 70.41mm;
[0094] PTFE upper film 3: diameter 31.18mm, thickness 0.20mm;
[0095] Glass fiber cover film 4: diameter 44.08mm, thickness 0.21mm;
[0096] Collector ring 5: outer diameter 20.97mm, inner diameter 20.12mm, thickness 3.82mm;
[0097] Current collecting nickel needle 6: length 57.67mm, diameter 1.19mm;
[0098] Lithium belt 7: length 114.86mm, width 58.10mm, thickness 2.60mm, weight 9.27g;
[0099] Glass fiber edge film 8: length 130.65mm, width 67.12mm, thickness 0.32mm;
[0100] Glass fiber bottom film 9: diameter 47.02mm, thickness 0.21mm;
[0101] PTFE bottom film 10: diameter 33.04mm, thickness 0.20mm;
[0102] Bottom cover 11: diameter 40.44mm, thickness 1.92mm.
[0103] The method for manufacturing a cylindrical lithium thionyl chloride primary battery pack with high reliability and safety comprises the following steps:
[0104] (I) Negative electrode into the shell. After the lithium ribbon 7 is cut, it is placed on the lithium winding rod, manually rolled into a cylindrical shape, and placed into the steel shell. At this time, the height × thickness of the lithium ribbon 7 = 114.86 mm × 2.60 mm.
[0105] (ii) Installing the polytetrafluoroethylene bottom membrane 10 and the glass fiber bottom membrane 9. After the polytetrafluoroethylene bottom membrane 10 and the glass fiber bottom membrane 9 are cut out by a cutting machine, they are pressed into the bottom position of the steel shell respectively.
[0106] (iii) When installing the diaphragm sheet 8, first cut a glass fiber membrane of appropriate length on a cutting machine, and then manually roll the material into a cylindrical shape and load it into the negative electrode steel shell.
[0107] (IV) Install the carbon package, put the carbon package into the shell and press it, at this time, the carbon package and the negative electrode lithium 7 are separated by the diaphragm. Before preparing the carbon package, acetylene black, RW, alcohol, pure water (conductivity is 1μS) and binder polytetrafluoroethylene are prepared, and according to the appropriate ratio (the mass ratio of acetylene black, RW, alcohol, pure water, binder polytetrafluoroethylene = 18:2:60:24:3) are evenly mixed in the powder mixer, and then the materials are extruded and shot blasted. After the formed carbon package is left to stand, it is baked in the baking oven.
[0108] (V) Installing the glass fiber cover film 4, after it is prepared into a specific specification (diameter 44.08 mm, thickness 0.21 mm) according to the processing technology, it is stamped on the top surface of the carbon package.
[0109] (VI) When installing the cover assembly 1 and adding the current collector, fix the steel shell on the fixture, and insert the current collector nickel needle 6 into the carbon bag under the glass fiber cover film 4. The insertion depth of the current collector nickel needle 6 is 54 mm.
[0110] (VII) Setting the sealing cover. After the positive pole current collecting ring 5 and the current collecting nickel needle 6 are connected by spot welding, they are compressed and sealed, and finally sealed by argon arc welding.
[0111] (VIII) Injecting electrolyte: Inject electrolyte through full vacuum liquid injection equipment, the electrolyte is lithium aluminum tetrachloride thionyl chloride solution, and the specification of the solution is 15 mol / L.
[0112] (IX) Install the sealing nails. After the injection hole is compacted with the sealing nails, assemble the battery cells, and finally clean the assembled battery cells.
[0113] (10) Static aging. After the semi-finished battery cells are assembled, they are left to stand and age. After aging, the battery cells are packaged with film to make finished batteries.
[0114] The above description is only the preferred embodiment of the utility model, and is not intended to limit the utility model. For those skilled in the art, the utility model can have various modifications and changes. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the utility model shall be included in the protection scope of the utility model.
Claims
1. A cylindrical lithium thionyl chloride primary battery with high reliability and safety, characterized in that: It consists of two parts, the outer part includes an outer shell, a cover group and a sealing nail. The positive and negative electrodes of the inner part are separated by a diaphragm. Plastic sheets are attached to the top and the bottom. The negative electrode is made of a lithium sheet and leans against the inner wall of the outer shell. The diaphragm is made of non-woven glass cloth. The positive electrode is composed of a carbon package and is in contact with the diaphragm. The internal current collecting part is spot welded by a positive electrode column, a current collecting ring and a current collecting nickel needle spot welding machine.
2. The cylindrical lithium thionyl chloride primary battery with high reliability and safety according to claim 1, characterized in that: The shell is a stainless steel shell.
3. The highly reliable and safe cylindrical lithium thionyl chloride primary battery according to claim 2, characterized in that: The shell is formed by welding a stainless steel tube and a bottom cover, and the welding process is argon arc welding.
4. The highly reliable and safe cylindrical lithium thionyl chloride primary battery according to claim 3, characterized in that: The dimensions of the stainless steel tube are: outer diameter Φ42.65±0.1mm, inner diameter Φ40.46-0.06mm, length Φ70.5±0.1mm; the dimensions of the bottom cover are: diameter Φ40.5±0.04mm, thickness Φ2±0.05mm.
5. The highly reliable and safe cylindrical lithium thionyl chloride primary battery according to claim 1, characterized in that: The cover assembly is formed by sintering a cover plate, a positive pole and insulating glass.
6. The highly reliable and safe cylindrical lithium thionyl chloride primary battery according to claim 5, characterized in that: The dimensions of the cover assembly are: diameter Φ40.5±0.04mm, thickness Φ2±0.05mm, and injection hole diameter Φ1.1+0.03mm.
7. The highly reliable and safe cylindrical lithium thionyl chloride primary battery according to claim 5, characterized in that: The stainless steel tube, bottom cover and cover plate are all cut by lathe, and the material is SUS304.
8. The highly reliable and safe cylindrical lithium thionyl chloride primary battery according to claim 1, characterized in that: The plastic sheet is a polytetrafluoroethylene plastic sheet.
9. The highly reliable and safe cylindrical lithium thionyl chloride primary battery according to claim 1, characterized in that: The dimensions of the collecting ring are: outer diameter Φ21±0.1mm, inner diameter Φ20.2±0.1mm, and thickness Φ4±0.2mm.
10. The highly reliable and safe cylindrical lithium thionyl chloride primary battery according to claim 1, characterized in that: The dimensions of the current collecting nickel needle are: length Φ57.5±0.5mm, diameter Φ1.2±0.05mm.