Method for adjusting oxo acidity

By adjusting the oxo acidity of molten metal hydroxide salts with oxo-acidity control components, the method addresses corrosion issues, enabling efficient use in energy storage and nuclear fission processes.

JP2024538984AInactive Publication Date: 2024-10-28セーアボー アンパーツゼルスカブ
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2024521366
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-07
Filing Date
2022-10-07
Publication Date
2024-10-28
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The corrosive nature of molten metal hydroxide salts limits their effective use in industrial applications, particularly in nuclear fission processes and energy storage systems, due to the lack of methods to control oxo acidity and mitigate corrosion.

Method used

A method to adjust the oxo acidity of molten metal hydroxide salts by introducing an oxo-acidity control component, such as water vapor or metal oxides, to create an optimal oxo-acidity window that minimizes corrosion, allowing for the use of a wide temperature range in energy or heat storage containers.

Benefits of technology

This method enables the efficient use of molten hydroxide salts across a broad temperature range by reducing corrosion, protecting container materials and facilitating large-scale industrial applications like energy storage and nuclear fission reactors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024538984000001_ABST
    Figure 2024538984000001_ABST
Patent Text Reader

Abstract

The present invention relates to a method for adjusting the oxo-acidity of a molten metal hydroxide salt, comprising: 2- and O.H. - estimating at least one target concentration of The present invention relates to a method comprising the steps of: providing an oxo-acidity control component; and contacting the oxo-acidity control component with a molten salt of a metal hydroxide to adjust the oxo-acidity of the molten salt of a metal hydroxide. The method allows for more efficient use of the available temperature range for the molten salt of a metal hydroxide by reducing the corrosiveness of the metal hydroxide.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for adjusting the oxo-acidity of a molten metal hydroxide salt, which allows for more efficient use of the available temperature range for the molten salt of the metal hydroxide by reducing the corrosiveness of the metal hydroxide. [Background technology]

[0002] Although molten salts are generally highly corrosive, the physical and chemical properties of molten salts make them attractive for certain applications. In particular, molten hydroxide salts have potential utility as neutron moderators in nuclear fission processes and can be used over a wider temperature range than molten salts such as chlorides, nitrates, carbonates, etc., that are useful in energy storage, for example.

[0003] Despite the corrosive nature of molten metal hydroxide salts, their use as neutron moderators in nuclear fission processes has been described. For example, WO 2020 / 157247 uses single crystal corundum as a corrosion-resistant material in contact with molten hydroxide moderator salts in a molten salt nuclear fission reactor (MSR). However, single crystal corundum is expensive and therefore its use as a construction material for large-scale systems is limited.

[0004] Molten salts may contain water and other components that contribute to defining the molten salt's property "oxo acidity." In hydroxide-containing molten salts, hydroxide ions can accept protons to form HO and donate protons to form superoxide ions O. 2- The water present in the molten salt reacts according to the following chemical reactions 1 and 2: Chemical reaction formula 1 2H2O⇔H3O + +OH - Chemical reaction formula 2 2OH - ⇔H2O+O 2-

[0005] In this context, we consider pH = -log in aqueous phase chemistry. 10 [H + ] and pOH=-log 10 [OH - ], we define oxo acidity as pH2O=-log 10 [HO] and oxobasicity is defined as pO 2- =-log 10 [O 2- ].

[0006] Oxo acidity helps predict the stability of certain species in molten salts, as described by B.L. Tremillon in Chemistry in Non-Aqueous Solvents, Springer Netherlands, Dordrecht, 1974. doi:10.1007 / 978-94-010-2123-4 and Acid-Base Effects in Molten Electrolytes, in: Molten Salt Chemistry, 1987: pp. 279-303. For example, alumina is an exemplary material that is slightly soluble in acidic and neutral melts and highly soluble in basic melts. In acidic melts, alumina is an AIO + In the basic melt, it dissolves as AIO2 - However, Tremillons points out that the combination of oxidizing species and base stabilizes the system, explaining why easily oxidized species are more stable in basic media. Conversely, oxidizing species are generally much less stable in acidic systems where bases are easily combined with acidic species, resulting in the favoring of reduced species. However, for many metal alloys, there exists an oxo-acidity range within which the alloy can exist in stable equilibrium in oxo-acidic / oxo-basic conditions. Thus, there exists a range of water concentrations in molten hydroxides within which the material is stable enough to be used as a containment material.

[0007] WO 2018 / 229265 similarly discloses an MSR with molten metal hydroxide as moderator salt. The molten moderator salt may contain a redox element, which is a chemical species, e.g., water, that has a greater reduction potential than that of the material in contact with the molten moderator salt or that controls the oxo-acidity of the molten moderator salt. WO 2018 / 229265 suggests bubbling water gas through the molten moderator salt or using an inert cover gas that contains a chemical species that controls the redox potential and / or oxo-acidity of the melt, citing H2O, H2 and HF as exemplary chemical species. However, WO 2018 / 229265 does not disclose how to actually control the oxo-acidity. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] International Publication No. 2020 / 157247 [Patent Document 2] International Publication No. 2018 / 229265 [Non-patent literature]

[0009] [Non-Patent Document 1] Chemistry in Non-Aqueous Solvents, Springer Netherlands, Dordrecht, 1974.doi:10.1007 / 978-94-010-2123-4 [Non-Patent Document 2] Acid-Base Effects in Molten Electrolytes, in:Molten Salt Chemistry, 1987:pp.279~303 Summary of the Invention [Problem to be solved by the invention]

[0010] It is an object of the present invention to provide a method which allows the use of a wide temperature range between the melting point and the boiling point of molten hydroxide salts in industrial applications, and it is a further object to provide a method which allows the use of molten hydroxides on a large scale. [Means for solving the problem]

[0011] The present invention relates to a method for adjusting the oxo-acidity of a molten metal hydroxide salt in an energy or heat storage container in which the hydroxide salt provides a medium for energy or heat storage: 2- and O.H. - providing an oxo-acidity control component; and contacting the oxo-acidity control component with a molten salt of a metal hydroxide to adjust the oxo-acidity of the molten salt of the metal hydroxide. In particular, the oxo-acidity is adjusted to match the corresponding target concentration, e.g., by adjusting the oxo-acidity of HO, O, or H2O to match the corresponding target concentration, e.g., such that the adjustment provides oxo-neutral conditions. 2- and O.H. - The oxo-acidity may be adjusted in relation to the concentration of one or more of the following: Adjusting the oxo-acidity allows for the reduction of corrosion in molten metal hydroxide salts, and therefore the method may also be considered as a method of adjusting oxo-acidity for the reduction of corrosion in molten metal hydroxide salts, or a method of reducing corrosion in molten metal hydroxide salts. In a specific example of the method, the oxo-acidity is adjusted to oxo-neutral conditions, for example for a particular lining material, in a step of contacting the molten salt of the metal hydroxide with an oxo-acidity control component to adjust the oxo-acidity of the molten salt of the metal hydroxide. The metal hydroxide may be any metal hydroxide as desired, but the metal hydroxide is preferably an alkali metal hydroxide, such as, for example, sodium, potassium or lithium hydroxide, or a mixture thereof, or the metal hydroxide may be an alkaline earth metal hydroxide, such as calcium or magnesium. Similarly, the metal hydroxide may be a hydroxide of a different metal.

[0012] The method of adjusting the oxo-acidity of a molten metal hydroxide salt is particularly relevant for energy or heat storage containers in which the hydroxide salt provides energy or heat storage. In another aspect, the invention relates to an energy storage system comprising a container, a heat sink and / or a heat source, and a molten metal hydroxide salt disposed within the container, wherein the molten salt of the metal hydroxide is circulated within the container by forced convection obtained from the heat sink and / or the heat source, as the case may be, configured to create a temperature gradient in the range of 0.1° C. / cm to 10° C. / cm over a distance from the heat sink and / or the heat source to a point in the molten salt of the metal hydroxide. The heat sink and / or the heat source may, for example, be configured to contact the molten salt of the metal hydroxide over a distance in the range of 0 cm to 100 cm from the lining material. In a specific embodiment, the distance from the heat sink and / or the heat source to a point in the molten salt of the metal hydroxide is in the range of 5 cm to 20 cm, as the case may be.

[0013] In one example, a method for adjusting the oxo-acidity of a molten metal hydroxide salt includes the steps of providing a container having an interior surface made of a material of interest, the container containing a molten salt of the metal hydroxide, and the container containing a heat source and / or heat sink configured to create a temperature gradient in the range of 0.1° C. / cm to 10° C. / cm in the molten salt of the metal hydroxide; 2- , and O.H. - and contacting an oxo-acidity control component with a molten salt of a metal hydroxide to adjust the oxo-acidity of the molten salt of the metal hydroxide.

[0014] By adjusting the oxo-acidity of the molten salt of the metal hydroxide, the method allows the oxo-acidity to be adjusted to have an optimal value for the material in contact with the molten salt of the metal hydroxide, thereby minimizing the corrosion of the material that would otherwise be caused by the molten hydroxide salt, and thus the method of the present disclosure can be used in any situation where a molten hydroxide salt is useful or appropriate. For example, the method may be used in a molten salt fission reactor (MSR) where the hydroxide salt serves as a moderator for the nuclear fission process, in an energy or heat storage container where the hydroxide salt provides a medium for energy or heat storage, or in a scrubber unit that operates with a molten hydroxide, e.g., pure molten hydroxide. HO and / or O 2- However, even if the molten salt is a metal hydroxide molten salt, it is still possible to estimate the target concentration of OH, as shown in Equation 1 and Equation 2. - It is relevant to estimate the target concentration of

[0015] The molten salt of the metal hydroxide may be contacted with the oxo acidity control component using any procedure as desired, for example, the oxo acidity control component may be in the form of a gas, liquid or solid that can be directly contacted with the molten salt of the metal hydroxide.

[0016] The method may use a process gas comprising an inert carrier gas and an oxo-acidity control component. For example, the oxo-acidity control component may be provided in a process gas comprising an inert carrier gas, and the method may further comprise contacting the process gas comprising the oxo-acidity control component with the molten salt of the metal hydroxide to adjust the oxo-acidity of the molten salt of the metal hydroxide. In this context, an inert gas is any gas that does not react with the molten salt of the metal hydroxide or the material in contact with the molten salt of the metal hydroxide. Exemplary inert gases include nitrogen (N2) and noble gases, such as helium, neon, argon, and mixtures or combinations thereof. By providing the oxo-acidity control component in the process gas, the amount of the oxo-acidity control component contacted with the molten salt of the metal hydroxide can be easily controlled to adjust and maintain the oxo-acidity of the molten salt of the metal hydroxide within an oxo-acidity window that is optimal for protecting the lining material of the container in which the molten salt of the metal hydroxide is located.

[0017] In this context, the oxo acidity control component is an OH acidity control component in a molten salt, particularly a molten salt of a metal hydroxide. - , O 2- and HO. The chemical may be any chemical, such as an element, molecule, or ion, capable of affecting the concentration of at least one of OH - , O 2- The effect on the concentration of at least one of OH, OH, and HO may be direct or indirect, and the effect may involve, for example, an increase or decrease in concentration according to Equation 1 and Equation 2. In particular, OH - , O 2- and HO are all considered oxo acidity control components in connection with the method, and similarly, OH - Or O 2-and molecules containing the appropriate counterions are also considered oxo acidity control components. Water, H2O, particularly water in the form of steam, is the preferred oxo acidity control component. Water, H2O, can also exist as a hydrate in salts or crystals, and salts containing hydrates may also be used as oxo acidity control components. When a salt contains a hydrate, the number of water molecules in the salt is usually listed as "x·H2O" along with the stoichiometric composition of the salt, and the value of x can be used to determine the amount of salt to adjust the oxo acidity. Other oxo acidity control components are metal oxide salts, for example oxide salts of the same metal as the metal in the molten salt of the metal hydroxide. OH - , O 2- , and / or molecules having the ability to bind HO are also considered oxo acidity control moieties in this context.

[0018] When a treatment gas is utilized, the treatment gas is contacted with the molten salt of the metal hydroxide. Thus, the oxo-acidity control component is also contacted with the molten salt of the metal hydroxide to adjust the oxo-acidity of the molten salt of the metal hydroxide. In general, the amount of the oxo-acidity control component contacted with the molten salt of the metal hydroxide depends on the concentration of the oxo-acidity control component in the treatment gas, the pressure of the treatment gas, and the m of the molten salt of the metal hydroxide contacted with the molten salt of the metal hydroxide, for example. 3 The amount of oxo acidity control component relevant to the specific embodiment of the present method is determined by the amount of OH in the molten salt of the metal hydroxide. - , O 2- and an estimate of the target concentration of at least one of HO, O, and HO present in the molten salt of the selected oxo acidity control component and metal hydroxide. 2- and O.H. - The reaction is determined by the chemical reaction equilibrium between one or more of the

[0019] The oxo acidity control component may also be added to the molten salt of the metal hydroxide without the use of a treatment gas. For example, a solid metal oxide such as lithium oxide or sodium oxide may be added in the form of solid pellets to the molten salt, or HO, O in the molten salt of the metal hydroxide.2- and O.H. - In another example, molten potassium hydroxide hexahydrate can be titrated into a molten salt of a metal hydroxide to obtain HO, O 2- and O.H. - It is also possible to contact an oxide, such as Li2O or Na2O, with a molten salt of a metal hydroxide, with the metal oxide in molten form.

[0020] The molten salt of metal hydroxide may be placed in any kind of container, pipe or tubing when it is contacted with the process gas. In this context, the material in contact with the molten salt of metal hydroxide shall be called the "lining material". The lining material is therefore exposed to the molten salt of metal hydroxide. Generally, the material has an "oxo-acidity window" where the corrosion resistance is optimal, and if the oxo-acidity is too high or too low, the material will be corroded by the molten salt of metal hydroxide too quickly for the lining material to be used in a practical environment. The oxo-acidity corresponding to the oxo-acidity window may be called "oxo-neutral" conditions. The container has an inner surface made of the lining material. The container may be made of any material, such as, for example, a metal, a metal alloy, a ceramic material or a combination thereof, and in this context, this material is called the container material. The inner surface may be a surface of the container material such that the lining material is the container material, or the container material may be coated with a further material to provide the lining material. For example, the container material may be a metal alloy, such as a nickel-based alloy, a nickel-based superalloy, or Hastelloy or nickel. In this context, a nickel-based alloy is an alloy having at least 50% w / w nickel.

[0021] When the molten salt of metal hydroxide is placed in a container, the molten salt of metal hydroxide may be stationary, or the molten salt of metal hydroxide may circulate in the container by natural convection, forced convection or forced circulation. In general, forced circulation involves stirring the molten salt of metal hydroxide. Any kind of stirring may be used in the method. In this context, natural convection is considered to involve motion in the molten salt of metal hydroxide that occurs due to temperature and / or concentration gradients of the components of the molten salt of metal hydroxide without any active steps being taken to affect convection. If no active steps are taken to create a temperature and / or concentration gradient, the molten salt of metal hydroxide is generally considered to be stationary in this context. In contrast, forced convection is considered to involve motion in the molten salt of metal hydroxide that is caused by actively introducing a temperature and / or concentration gradient, in particular temperature gradient. For example, localized heating of a fixed volume of a metal hydroxide molten salt can cause a local expansion of the metal hydroxide molten salt near the heat source, which induces motion in the metal hydroxide molten salt. Similarly, localized cooling of a fixed volume of a metal hydroxide molten salt can cause a local contraction of the metal hydroxide molten salt near the heat sink, which induces motion in the metal hydroxide molten salt. Forced convection and forced circulation allow the oxo-acidity in the metal hydroxide molten salt to be generally uniform, e.g., the oxo-acidity can vary within 30% of the average oxo-acidity throughout the volume of the metal hydroxide molten salt. In this context, forced circulation is expressed in terms of volumetric displacement over time and is expressed in units per time (i.e., h -1 ), for example, the volume displacement may be 0.1 h -1 ~100h -1 , for example 1h -1 ~20h -1 Thus, forced circulation and forced convection are advantageous to avoid situations where local variations in the molten salt of the metal hydroxide create regions where the oxo acidity is outside the oxo acidity window.

[0022] The molten salt of the metal hydroxide is preferably placed in a container, typically with a cover gas above the molten salt of the metal hydroxide, for example the container may have a lid covering the molten salt of the metal hydroxide to provide a closed system, but the lid may also have an opening to control the composition and pressure of the cover gas. The cover gas may be maintained at a pressure higher than ambient pressure, for example in the range of 1 bar to 10 bar. The cover gas may be an inert gas or a process gas containing an oxo acidity control component. The cover gas may contain, for example, water vapor as an oxo acidity control component at a partial pressure in the range of 0.01 bar to 2 bar, for example 0.02 bar to 0.5 bar. If the cover gas contains an oxo acidity control component, the cover gas may be bubbled through the molten salt of the metal hydroxide and recycled to the cover gas, in particular the content of the oxo acidity control component, for example expressed as a partial pressure, may be replenished in the cover gas. For example, the oxo acidity control component may be added directly to a cover gas which may then be bubbled through a molten salt of a metal hydroxide. By using a process gas containing an oxo acidity control component as the cover gas and bubbling the cover gas through the molten salt of a metal hydroxide and recycling the process gas back into the cover gas, a setup is created which is easy to control the oxo acidity of the molten salt of a metal hydroxide.

[0023] In one example, a gas is bubbled through the molten salt of a metal hydroxide. The gas may be an inert gas, i.e., an oxo acidity control component, a treatment gas with an oxo acidity control component, or an inert gas without the oxo acidity control component in gaseous form. If the gas contains an oxo acidity control component, the volume of gas bubbled through the molten salt of the metal hydroxide takes into account the intended amount of oxo acidity control component to be contacted with the molten salt of the metal hydroxide, and the amount of gas bubbled through the molten salt of the metal hydroxide is measured in units per hour (i.e., h -1 The amount of inert gas bubbled through the volume of molten salt of metal hydroxide per unit of time may be expressed as the volume of inert gas relative to the volume of molten salt of metal hydroxide per unit of time such that-1 ~10h -1 , e.g. 0.5h -1 ~2h -1 When gas is bubbled through a molten salt of a metal hydroxide, the bubbles may be in the range of 2h -1 When the temperature is above 1000° C., forced circulation of the molten salt of the metal hydroxide can be created.

[0024] The oxo acidity control component may be present in the metal hydroxide before the salt is melted, and therefore the oxo acidity control component will be present in the metal hydroxide salt once melted. However, due to the high temperatures typically used to melt the salt and possible reactions between the oxo acidity control component and other components, the content of the oxo acidity control component will not be constant over time. For example, the oxo acidity control component may evaporate from the molten salt.

[0025] The method comprises the steps of: 2- and O.H. - The method includes estimating a target concentration of at least one of H2O, O 2- and O.H. - The target concentration of at least one of may be estimated at any temperature at which the metal hydroxide is molten. Generally, at least one temperature is sufficient to provide a useful estimate of the target concentration. However, HO, O 2- and O.H. -is estimated at at least three different temperatures within the melting point and boiling point of the metal hydroxide salt or between the melting point of the metal hydroxide salt and 1000° C. The temperatures, e.g. the at least three temperatures, are preferably selected to be within the intended temperature operating range of the setup. The at least three temperatures are different temperatures, and the different temperatures should be at least 10° C. apart from each other, but the temperatures are preferably distributed over the entire temperature range in which the metal hydroxide salt is molten, e.g. the temperatures may be selected at points at least 50° C., at least 100° C. or at least 200° C. apart from each other. For example, the temperatures may include a first temperature, such as a "nadir temperature" ranging from the melting point of the metal hydroxide salt to the melting point of the metal hydroxide salt plus 100° C., a second temperature, such as a "midpoint temperature" ranging from the midpoint between the melting point and boiling point of the metal hydroxide salt to ±50° C., and a third temperature, such as a "peak temperature" ranging from 100° C. below the boiling point of the metal hydroxide salt to the boiling point of the metal hydroxide salt. 2- and O.H. - is estimated at at least three different temperatures within the melting and boiling points of the metal hydroxide salt, in particular, the temperatures are spaced apart from each other by at least 50° C. or at least 100° C., the inventors have unexpectedly discovered that the estimate of the target concentration is useful over the entire temperature range of the corresponding molten salt of the metal hydroxide. Thus, the method provides a simple approach to use the entire temperature range of the metal hydroxide salt.

[0026] In general, the target concentration represents an oxo-acidity window where corrosion is minimized to optimize the corrosion resistance of the material of the container containing the metal hydroxide molten salt, e.g., the lining material; typically, the target concentration may be a point or a range expressed in mol / L or mol / kg. The target concentration generally depends on the lining material, e.g., the chemical composition and the operating temperature range of the lining material. Theoretical analysis for Ni, Cr and Fe (main components of typical high nickel alloys) highlights their common oxo-acidity window of stability in NaOH at 800°C. For these, the H2O concentration expressed as p(H2O)=-Log[H2O] should be comprised between 2.5 and 5.6, e.g., 2.5 and 3.1. Figure 2 illustrates theoretical potential oxo-acidity diagrams for Ni, Fe and Cr metals, where the theoretical regions of shared stability are highlighted as shaded areas. The thick outline shows the stability window of sodium hydroxide molten salt at 800°C. However, the theoretical potential oxo-acidity diagram of Figure 2 is only valid for pure Ni, Fe and Cr metals. The inventors have found that for alloys currently containing about 90% w / w Ni, the oxo-acidity window for HO is in the range of 0.1-40 mmol HO per kg of molten metal hydroxide, preferably 1-15 mmol HO per kg of molten metal hydroxide. Thus, target concentrations can be defined for a particular lining material. The target concentrations are: HO, O 2- and O.H. - or H2O, O 2- and O.H. - may be expressed in terms of any combination of two or all of the following: H2O, O 2- and O.H. - contributes to oxo acidity, and by contacting a treatment gas containing an oxo acidity control component with a molten salt of a metal hydroxide, HO, O 2- and O.H. -By estimating the target concentration of one, two or all three of these, the oxo-acidity of the molten salt of the metal hydroxide can be adjusted, specifically controlled, for example according to Henry's law, to be within the oxo-acidity window of the lining material. In general, when the oxo-acidity control component is provided in gaseous form, it is assumed that the amount of oxo-acidity control component dissolved in the molten salt of the metal hydroxide is proportional to the partial pressure of the oxo-acidity control component, which is in contact with the molten salt of the metal hydroxide, for example by being above the molten salt of the metal hydroxide (see FIG. 3). In this way, corrosion of the lining material is minimized. In one embodiment, the molten salt of the metal hydroxide is placed in a container having an inner surface made of the lining material, and the molten salt is mixed with H2O, O2, and H2O. 2- and O.H. - At least one target concentration of is defined for the lining material. An empirical correlation discovered by the inventors between the partial pressure of water vapor in the process gas and the concentration of water in the molten salt of sodium hydroxide is shown in FIG.

[0027] Without application of an oxo-acidity control component to the molten metal hydroxide salt, there is only a limited variation in oxo-acidity throughout the volume of the molten metal hydroxide salt, especially when the molten metal hydroxide salt is stationary in a container or when the molten metal hydroxide salt is circulated by natural convection. In general, when the molten metal hydroxide salt is stationary in a container, there may be local variations in the oxo-acidity of the molten metal hydroxide salt, but it is considered that the oxo-acidity of the molten metal hydroxide salt more than 20 cm, for example more than 50 cm or 100 cm, from the container wall has only a limited effect on the influence of the molten metal hydroxide salt on the container wall. However, the risk of corrosion is particularly relevant at the interface between the molten metal hydroxide salt and any material, such as a lining material, that comes into contact with the molten metal hydroxide salt. In one embodiment, the molten salt of the metal hydroxide is placed in a container having an inner surface made of a lining material, and the oxo-acidity control component is contacted with the molten salt of the metal hydroxide placed at a distance in the range of 0 cm to 100 cm, e.g., 0 cm to 50 cm, or 0 cm to 20 cm, from the lining material. In particular, the molten salt of the metal hydroxide placed within 100 cm or within 50 cm or within 20 cm may be contacted with the oxo-acidity control component over the entire distance from the wall of the container, e.g., the inner surface made of the lining material. Thus, the molten salt of the metal hydroxide may be stationary, e.g., in the container, and the molten salt of the metal hydroxide placed at a distance of more than 100 cm, e.g., more than 50 cm or 20 cm, from the lining material does not need to be contacted with the oxo-acidity control component, because the molten salt of the metal hydroxide beyond this distance from the inner wall of the container results in only limited corrosion of the material of the inner wall of the container, e.g., the lining material.For example, the oxo acidity control component, e.g., contained in an inert carrier gas or in gaseous form, may be bubbled through the molten salt of the metal hydroxide at or over a distance in the range of 0 cm to 100 cm, e.g., 0 cm to 50 cm, or 0 cm to 20 cm from a lining material, e.g., a wall of a container storing the molten salt of the metal hydroxide.

[0028] The container may have any size and shape as desired. For example, a container, particularly a storage container, may have a central volume defined by a distance from the container wall. Thus, the container may have a central volume that is at least 20 cm, at least 50 cm, or at least 100 cm away from the container wall. Molten salts of metal hydroxides within the central volume are generally considered not to contribute to corrosion of the container's inner walls. An exemplary container volume is 1 m 3 ~10m 3 In the context of the method, the container may also be a pipe or conduit, for example for adding a salt of a metal hydroxide, for example in molten form, to a storage container.

[0029] Industrial applications of molten salts of metal hydroxides, particularly when the molten salts of metal hydroxides are used for energy storage, may involve being able to add or remove heat from the molten salts of metal hydroxides to take advantage of the large temperature range between the melting point and boiling point of the molten salts of metal hydroxides. Thus, in one example, the molten salts of metal hydroxides are placed in a container, the container including a heat source and / or a heat sink configured to create a temperature gradient in the range of 0.1°C / cm to 100°C / cm, e.g., 0.1°C / cm to 10°C / cm, over a distance in the range of, e.g., 5cm to 50cm, in the molten salt of metal hydroxide. Other relevant temperature gradients are in the range of 0.1°C / cm to 5°C / cm, 0.15°C / cm to 2°C / cm, or 1°C to 5°C / cm. The temperature gradient may be defined in terms of the temperature difference and the distance between the points at which the temperature is measured. Typically, the temperature difference is recorded from a reference point, for example representing the metal hydroxide molten salt, and optionally from a further point representing a heat source and / or a heat sink. The temperature gradient may be expressed in relation to a distance, for example from the heat sink to a point in the metal hydroxide molten salt or from the heat source to a point in the metal hydroxide molten salt, which may be in the range of 1 cm to 100 cm, for example from 10 cm to 50 cm. Thus, in one example, the temperature gradient recorded, for example from the heat sink to a point in the metal hydroxide molten salt or from the heat source to a point in the metal hydroxide molten salt, is in the range of 1° C. over 10 cm to 10° C. over 10 cm, or 10° C. over 50 cm to 100° C. over 50 cm. Typically, heat can be added to or removed from the metal hydroxide molten salt. In particular, heat may be added to or removed from the molten salt of metal hydroxide to create forced convection in the molten salt of metal hydroxide, and thus it is particularly suitable to contact the molten salt of metal hydroxide over a distance of 0 cm to 100 cm or 0 cm to 50 cm from the lining material, e.g. the wall of the container storing the molten salt of metal hydroxide, or to use forced circulation to provide a uniform oxo-acidity of the molten salt of metal hydroxide when the molten salt of metal hydroxide is in contact with a heat source or heat sink.The method is therefore particularly advantageous for large scale use of molten metal hydroxide salts for energy storage, as it allows for protection of the inner walls of the container, e.g., lining material, etc. In one embodiment, the method is aimed at adjusting the oxo-acidity of a molten metal hydroxide salt in an energy storage system having a container in which the molten metal hydroxide salt is disposed, and comprises the steps of: 2- , and O.H. - A target concentration of at least one of is estimated from theoretical calculations, from prior knowledge of a specific material, e.g., a pure metal, or as otherwise described herein, and the molten salt of the metal hydroxide is circulated in the container by resulting forced convection from a heat sink and / or a heat source, as the case may be, configured to create a temperature gradient in the range of 0.1° C. / cm to 10° C. / cm over a distance in the range of 5 cm to 20 cm from the heat source and / or heat sink, to a point in the molten salt of the metal hydroxide. For example, the temperature gradient may be at least 20° C. over a distance of 20 cm.

[0030] Similarly, heating and heat removal are also involved when a molten salt of metal hydroxide is used as a moderator in the MSR. For example, a nuclear fission reaction generates heat, which is removed from the MSR and converted to electricity. When a molten salt of metal hydroxide is used in the MSR, heat is typically removed from the molten salt of metal hydroxide using a heat exchanger, which thus creates forced convection in the molten salt of metal hydroxide, and an oxo acidity control component may be added anywhere in the MSR where the molten salt of metal hydroxide is located. For example, the oxo acidity control component may be steam contained in an inert cover gas, whereby the cover gas corresponds to the process gas, and the cover gas may be bubbled through the molten salt of metal hydroxide in a recirculation loop that may also optionally include a point of addition of steam.

[0031] The method may be advantageous in other applications of molten salts of metal hydroxides as well. Gas stream purification, which operates by contacting a contaminated gas with a molten salt of a metal hydroxide, may be operated in a scrubber unit having a container with a lining material, which may be protected by the techniques disclosed herein. Concurrently with the contaminated gas stream in the container in the scrubber unit, an oxo-acidity control component at a target concentration may be replenished through bubbling to simultaneously determine purification of the gas stream and oxo-acidity adjustment of the molten salt of a metal hydroxide.

[0032] The molten salt of the metal hydroxide may be contacted with a process gas containing an oxo-acidity control component. In one embodiment, the oxo-acidity control component is added to the process gas by sublimating the oxo-acidity control component from the solid state. For example, a metal oxide such as sodium oxide or lithium oxide may be sublimated to generate a partial pressure of gas phase molecular metal oxide which is then mixed with the process gas and used to control the oxo-acidity of the molten salt of the metal hydroxide.

[0033] In another further example, the oxo acidity control component is added to the treatment gas as a liquid via spraying or mist generation. For example, water is sprayed into the treatment gas to dissolve the OH in the molten salt of the metal hydroxide. - , O 2- and / or it is also possible to arrive at a concentration of droplets in the process gas that can provide a target concentration of H2O.

[0034] HO, O in molten metal hydroxide salts 2- and O.H. -The target concentration of may be estimated using any procedure as desired. For pure metals, it may be available from the scientific literature. See FIG. 2. However, the inventors now recognize that as soon as a metal contains other components, such as alloying metals, non-alloying metals and / or non-metallic components, such as carbon, nitrogen, oxygen, boron and / or silicon, even at metal purities up to about 99%, the presence of the other components affects the electrochemical properties compared to the same metal in pure form without the other components, and thus the metal with these components is differently susceptible to corrosion from molten hydroxides than the corresponding pure metal, e.g., more susceptible than the pure metal. The inventors have devised a method to generate accurate data correlating the steady-state concentration of oxo-acidity control components in a molten salt of metal hydroxide with the corrosive attack of the hydroxide on the lining material. In particular, different metal materials have different polarization characteristics as defined by the open circuit potential, breakdown potential and passivation potential of the material. Detection of these electrochemical parameters allows for the identification of the corrosive agent of the material in the environment under study. The method is similar to that used in aqueous corrosion studies, which has been adapted with modifications to study corrosion in molten salts of metal hydroxides. The setup utilized is particularly advantageous since it allows bench-scale analysis of target concentrations for the material of interest. Experimental results for an exemplary nickel alloy containing about 90% w / w nickel are shown in FIG. 4. In this context, a three-electrode arrangement may be used in which three electrodes are in contact with the molten salt of metal hydroxide. This arrangement includes the lining material of interest as the working electrode, a reference electrode, and a counter electrode made of pure nickel or another suitable metal, such as a nickel-based superalloy, which is believed to have excellent resistance to molten hydroxide corrosion. In one example, a beta-alumina sodium reference is used as the reference electrode. The potentials reported in this disclosure are relative to this reference electrode. An exemplary setup includes a high-temperature electrochemical cell including, for example, a metal vessel in which a crucible of inert material, for example, a crucible made of graphite, is placed to contain the molten salt of metal hydroxide.The vessel has a lid to maintain control of the atmosphere of the experiment, for example the atmosphere above the molten salt of metal hydroxide. The lid further has openings to allow the penetration of electrodes, and gas inlets and outlets to add and remove gas, for example the process gas to be analyzed. All openings can be closed and / or opened as required for the experimental setup. The gas inlets may also be used for the addition of non-gaseous components to the molten salt of metal hydroxide. An exemplary electrochemical cell is illustrated in FIG. 1. This arrangement allows for measuring the potential versus current as potentiodynamic polarization, and may include any sensors, computers, etc. for controlling and measuring electrical parameters. For example, the arrangement may include a multi-channel potentiostat / galvanostat controlled by a computer, such as PARSTAT (Princeton Applied Research, Hampshire, UK). This potentiostat / galvanostat may be set up to automatically target a desired potential between the working and reference electrodes by passing an appropriate current between the working and counter electrodes. The polarization of the working electrode may be accomplished potentiodynamically, such that the potential is continuously changed. This change may occur at a sweep rate of 20 mV / s or 50 mV / s. Before a polarization diagram is experimentally constructed, the corrosion potential of the working electrode may be determined relative to a reference electrode in open circuit condition, i.e. with zero applied current. After a few minutes or hours, an approximate constant value of the open circuit potential may be achieved. The working electrode may then be anodically polarized up to the transpassive potential starting from a potential that is 100 mV negative below the open circuit potential. Due to the stochastic nature of the corrosion phenomenon, the polarization test may be repeated at least three times for each material studied and under the test conditions to be used. Moreover, the scale / corrosion products formed during the polarization test on the samples may be metallographically examined using post-mortem analysis, for example, by scanning electron microscopy (SEM) combined with energy dispersive X-ray spectroscopy (EDS), to evaluate whether the material has undergone any microstructural changes at the time of polarization.In an exemplary setup, the test conditions to be investigated may be different target concentrations of the oxo acidity control component in the process gas. In one example, either dry or wet argon may be used as the carrier gas, and wet argon gas as an exemplary process gas may be generated by contacting argon with water in a thermostatic water bath at a temperature ranging from 30° C. to 90° C.

[0035] In another aspect, the present invention provides a method for determining the oxo acidity window of a material comprising: selecting a target material and a metal hydroxide; Providing a crucible of inert material; applying a metal hydroxide into a crucible of inert material and heating the metal hydroxide to provide a molten salt of the metal hydroxide; providing a working electrode made of a material of interest, a reference electrode and a counter electrode made of an inert metal; inserting a working electrode, a reference electrode and a counter electrode into a molten salt of a metal hydroxide; applying a gas above the molten salt of a metal hydroxide and doping the gas with an oxo acidity control component; applying a current between the working and counter electrodes and recording the polarization of the working electrode; determining the oxo acidity window of the material of interest from the polarization of the working electrode; The present invention relates to a method comprising the steps of:

[0036] In one embodiment, the method for determining the oxo acidity window of a material comprises: selecting a target material and a metal hydroxide; Providing a crucible of inert material; applying a metal hydroxide into a crucible of inert material and heating the metal hydroxide to provide a molten salt of the metal hydroxide; Inserting a test piece made of a target material into a molten salt of a metal hydroxide; adding an oxo acidity control component to the treatment gas and contacting the treatment gas with a molten salt of a metal hydroxide; determining the oxo acidity window of the material from the weight loss of the test specimen; A method is provided that includes:

[0037] The two methods for determining the oxo-acidity window of a material are as follows: In the first aspect, i.e., in the method for adjusting the oxo-acidity of a molten salt, H2O, O 2- and O.H. - and the target material may be a lining material of a container for storing a molten salt of a metal hydroxide. The metal hydroxide may be any metal hydroxide, for example an alkali metal or alkaline earth metal hydroxide, and the oxo acidity control component may be as defined above. The inert material may be any material believed to have good resistance to molten hydroxide corrosion, such as graphite.

[0038] The method is suitable for estimating the oxo-acidity window. In a first embodiment, the oxo-acidity window of the material of interest is determined from the polarization of the working electrode. In a second embodiment, this is done by measuring the corrosion rate of the material by measuring the weight loss of a test piece within a certain oxo-acidity range. The metal hydroxide may be any metal hydroxide, for example an alkali metal or an alkaline earth metal hydroxide.

[0039] Thus, for example, the corrosion rate is obtained by measuring the weight difference of a test piece of a selected material before and after exposure to a molten salt of a metal hydroxide contacted with a process gas containing an oxo-acidity control component at a controlled partial pressure. For example, the corrosion rate may be expressed in units of length per time, e.g., mm / year (mm / y), relative to the thickness of the test piece. The oxo-acidity window of the material is then determined as the oxo-acidity, e.g., oxo-acidity range, that provides the lowest corrosion rate. In this context, a corrosion rate of 0.1 mm / y is generally considered acceptable for materials to be used in energy or heat storage containers for MSR or in scrubber units operating with molten hydroxide.

[0040] The counter electrode may be made of any metal believed to have good resistance to molten hydroxide corrosion, such as nickel, e.g., pure nickel, or a metal such as a nickel-based superalloy believed to have good resistance to molten hydroxide corrosion. The reference electrode may be based on alumina, e.g., a beta-alumina sodium reference electrode.

[0041] Thus, by estimating the oxo-acidity of the molten salt of the metal hydroxide and contacting the molten salt of the metal hydroxide with a process gas containing an oxo-acidity control component at a controlled partial pressure, the oxo-acidity can be maintained within the oxo-acidity window, i.e., to provide oxo-neutral conditions for the lining material and minimize corrosion of the lining material by the molten salt of the metal hydroxide. For example, the oxo-acidity control component can be water vapor, which can be added to the process gas to provide a partial pressure of water in the process gas. The molten salt of the metal hydroxide is at a temperature much higher than the boiling point of water even at high pressure, and the water added to the process gas will be in the form of steam regardless of the state of the molten salt of the metal hydroxide. The concentration of water vapor in the process gas can be expressed as a volume percentage, and the concentration of water vapor in the process gas can be freely selected. For example, the concentration of water vapor in the process gas can be in the range of 5% V / V to 95% V / V. Correspondingly, the inert carrier concentration in the process gas may be in the range of 95% V / V to 5% V / V. However, water vapor is generally described in terms of its partial pressure in the process gas. The partial pressure of water vapor may be in the range of, for example, 0.01 bar to 2 bar, for example, 0.02 bar to 0.5 bar. The water vapor partial pressure, and also the process gas amount, suitable for a specific example of the method may depend on the concentration of HO, O in the molten salt of metal hydroxide. 2- and O.H. - The concentration of the at least one of the target concentrations is determined by an estimate of the target concentration of the at least one of the target concentrations.

[0042] In one embodiment, the oxo acidity control component is water vapor, and the water vapor is added to the treatment gas to provide a water pressure in the treatment gas. For example, the water vapor may be added to the treatment gas by contacting the water with the treatment gas. Any method for contacting the water with the treatment gas may be used, and in one example, the treatment gas is bubbled through a water bath, for example, a constant temperature water bath. The treatment gas bubbled through the water bath may be an inert carrier gas without any water content, or the treatment gas may already contain a certain amount of water, for example, a trace amount of water vapor, particularly an amount of water that is lower than the target concentration. After bubbling the treatment gas through the water bath, the treatment gas, now containing water vapor, is contacted with a molten salt of a metal hydroxide. The partial pressure of water vapor in the treatment gas may be controlled by at least one of controlling the temperature of the water bath, controlling the residence time of the treatment gas in the water bath, and controlling the pressure of the treatment gas in the water bath. Typically, the water bath will be at a temperature below the boiling point of water so that the water in the bath is liquid. The optimum temperature range for obtaining an appropriate water partial pressure in the process gas is in the range of 25°C to 90°C, for example 30°C to 50°C.

[0043] Any embodiment of the invention may be used in any aspect of the invention, and any advantage of one specific embodiment applies equally when the embodiment is used in one specific embodiment.

[0044] In the following, the invention will be explained in more detail by means of examples and with reference to the schematic drawings. [Brief description of the drawings]

[0045] [Figure 1] FIG. 1 illustrates an electrochemical cell for estimating a target concentration of at least one of H2O, O2-, and OH- in a molten salt of a metal hydroxide according to the present disclosure. [Diagram 2] FIG. 2 shows the potential oxo acidity diagram for Ni, Fe and Cr. [Diagram 3]FIG. 3 shows the empirical correlation between water pressure in the process gas and the steady-state concentration of H2O in a molten salt of sodium hydroxide. [Figure 4] FIG. 4 shows the potentiodynamic data measured for Ni alloys in molten NaOH at 600° C. [Diagram 5] FIG. 5 shows the corrosion rate for Ni alloys in molten NaOH. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0046] The present invention is not limited to the embodiments illustrated in the drawings. Thus, when features recited in the appended claims are followed by reference signs, it should be understood that such signs are included merely to facilitate comprehension of the claims and do not limit the scope of the claims in any way.

[0047] The term "comprising" as used in the present specification and claims means "consisting at least in part of." When interpreting statements in the present specification and claims containing the term "comprising," features other than those prefaced by the term in each statement may be present as well. Related terms such as "comprise" and "comprised" should be interpreted in the same manner.

[0048] The present invention relates to a method for adjusting the oxo-acidity of a molten metal hydroxide salt, which method is now illustrated in the following non-limiting examples. EXAMPLES

[0049] Example 1 An experiment was set up to determine the correlation between the water vapor pressure in the process gas and the steady-state concentration of H2O in the sodium hydroxide molten salt. Specifically, NaOH was added to a graphite crucible in a vessel made of pure nickel. The vessel had a lid with openings for adding and removing gas so that the composition of the gas above the crucible could be controlled, and the vessel also had openings for a thermometer and a gas analyzer probe. The vessel was placed in a mineral wool container and heated by applying an electric current to a heating wire in the mineral wool, heating the crucible to 600°C to melt the sodium hydroxide. Once the sodium hydroxide was melted, the amount of water vapor in the gas above the crucible was gradually increased to increase the water content in the gas, and the water content in the molten sodium hydroxide was then measured. The results are shown in Figure 3, which shows that a linear correlation was found between the water vapor in the gas and the water content in the molten sodium hydroxide.

[0050] Example 2 Two high Ni content commercial alloys containing more than 70% w / w nickel were analyzed to determine the target concentrations. One alloy contains approximately 90% w / w nickel and iron, manganese, silicon, copper and carbon. Although iron, manganese, silicon, copper and carbon are present in amounts that can be considered trace amounts, these amounts are sufficient to require the alloy to be analyzed to determine the target concentrations. The other alloy contains more than 70% w / w nickel, less than 10% w / w chromium, less than 5% w / w iron and other elements. H2O, O 2- and O.H. - The target concentration of cannot be predicted from the target concentrations of the individual components in their pure form.

[0051] Samples of the two alloys were analyzed in graphite reference crucibles using sodium hydroxide as an exemplary metal hydroxide salt. Analyses were performed at temperatures within the melting point of sodium hydroxide and 900° C. Water vapor was used as the oxo acidity control component, and the amount of water in the molten salt of sodium hydroxide was obtained from the correlation shown in FIG. 3.

[0052] Specifically, the two alloys were analyzed in an electrochemical cell 1 as illustrated in FIG. 1. The alloy containing more than 90% w / w nickel was supplied by Q-metal as 1 mm diameter wire, and the alloy containing more than 70% w / w nickel was supplied by Merck as 1 mm diameter wire. The electrochemical cell 1 had a vessel 2 made of pure nickel containing a graphite crucible 20. Pellets of NaOH were added to the crucible 20, and the vessel 2 with the crucible 20 was placed in a container of mineral wool as insulating material 23 and heated by applying an electric current to a copper heating wire 231 to melt the NaOH and provide a molten salt of metal hydroxide 3. The NaOH was obtained from Honeywell with a nominal purity of 98% or higher at 600° C.

[0053] The vessel 2 had a lid 21 assembled on a cell support 24, which had openings 22 for the working electrode 11, reference electrode 12, counter electrode 13 and thermocouple 14, as well as for a gas inlet 41 and a gas outlet 42. It should be understood that the openings 22 may be used for any item or device that will be in suitable contact with the molten salt of metal hydroxide 3. The gas inlet 41 and gas outlet 42 housed stainless steel piping and pumps for adding / removing the process gases to be analyzed.

[0054] The working electrode 11 was made of one of the alloys to be analyzed, and the reference electrode 12 and counter electrode 13 were made of pure nickel. The reference electrode 12 was housed in a membrane 121 of beta-alumina 121. The electrodes 11, 12, 13 were connected to a PARSTAT multichannel potentiostat / galvanostat (not shown) controlled by a computer (not shown). The potentiostat / galvanostat was set up to maintain a potential between the working and reference electrodes by passing a direct current between the working electrode 11 and the counter electrode 13, and the potential was continuously changed to analyze the polarization of the working electrode 11. Specifically, the change was made at a sweep rate of 20 mV / s or 50 mV / s.

[0055] Before constructing the experimental polarization diagrams, the corrosion potential of the working electrode 11 was determined under open circuit conditions, i.e. against the reference electrode 12 where the applied current was zero. An approximate constant value of the open circuit potential was usually reached after a few minutes. The working electrode 11 was then anodically polarized starting from a potential 100 mV negative below the open circuit potential up to the transpassive potential. Due to the stochastic nature of the corrosion phenomenon, the polarization test was repeated three times for each of the working electrode 11 materials.

[0056] Moreover, the formation of scale / corrosion products during polarization tests on the test alloys was metallographically examined using post mortem analysis using Scanning Electron Microscopy coupled with Energy Dispersive X-ray Spectroscopy (SEM / EDS) to evaluate whether the materials had undergone any microstructural changes after polarization.

[0057] Argon was used as the carrier gas and an exemplary process gas, wet argon, was generated by bubbling argon through water baths (not shown) at temperatures of 36° C., 50° C. or 90° C. Wet argon was introduced into vessel 2 via gas inlet 41. Excess gas was removed from vessel 2 via gas outlet 42 to maintain the pressure at ambient pressure.

[0058] The results of this practical example show the technique for finding the optimal oxo acidity window for a given material, but the results are not exhaustive. For accurate evaluation of the oxo acidity window, multiple test conditions can be assessed. Furthermore, while one temperature of the molten salt was used in the examples, multiple temperatures can be adequately evaluated to define a suitable oxo acidity window in a practical commercial setup to take into account temperature transients.

[0059] The results for a nickel alloy containing about 90% w / w nickel are shown in Figure 4, which shows the variation of the determined current versus potential. Different electrochemical responses were obtained for the same type of sample at different partial pressures of water (ppH2O) in the process gas used to adjust the steady-state concentration of water in the molten salt. By comparing the different profiles, the inventors defined the target oxo-acidity conditions to be used in the oxo-acidity control of the full-scale setup. Figure 4 shows a clear corrosion reduction for ppH2O = 5.5968% in cover gas at 1 atm total pressure. Two main features in the plot indicate the improvement by adjusting the water pressure. First, the peak in the potential region between 0.4 V and 1.2 V is assigned to the corrosion potential region. The higher the potential, the more corrosion resistant the material is at the operating conditions. The black line, corresponding to the absence of water addition in the molten salt, showed the worst performance, with a corrosion potential peak at 0.6 V. The salt was very oxobasic and easily corroded the samples. Notably, excessive amounts of ppH2O in the treatment gas also reduced the corrosion of the samples, albeit to a lesser extent. The blue and green lines correspond to the oxoacidic conditions of the salt, determining a corrosion potential of around 0.77 V. Finally, the red line shows the corrosion reduction that can be achieved by careful control of the target oxoacidity. Under these conditions, the inventors believe that the molten salt is in oxo-neutral conditions, i.e., between oxobasic and oxoacidic for the selected lining material. Within this oxoacidity window, the corrosion potential peak can increase significantly, reaching a value of 1.1 V.

[0060] Furthermore, another region of the plot shows the corrosion mitigation achieved with the correct water target concentration. In the potential region between 1.2V and 2V, a protective passivation layer can be observed. The lower the current, the stronger the protective passivation. When the target concentration of the lining material is correct, the surface chemistry on the material is stable, allowing the formation of a stable metal oxide on the surface, similar to the Cr oxide passivation layer obtained on conventional stainless steels exposed to air / moisture, which protects the uncorroded material layer below the surface. In this region of the plot, it can again be observed that the first ppH2O (red line) performs best in protecting against corrosion, while the oxo-basic regime (black line) is the worst in promoting the formation of a stable oxide layer on the material, while the second (green) and third (blue) ppH2O concentrations determine oxo-acidic conditions and similar protective effects.

[0061] Example 3 An experiment was set up to analyze the 90% nickel alloy also used in Example 2. Samples of the alloy were analyzed in an alumina crucible with sodium hydroxide as an exemplary metal hydroxide salt. The analysis was performed at temperatures within the melting point of sodium hydroxide and 900°C. Water vapor was used as the oxo acidity control component, and the amount of water in the molten salt of sodium hydroxide was obtained from the correlation plotted in Figure 3.

[0062] Specifically, pellets of NaOH were added to an alumina crucible, the crucible was placed in a container of mineral wool as an insulating material, and heated by applying an electric current to a copper heating wire wrapped around the crucible to melt the NaOH and provide a molten salt of the metal hydroxide. The NaOH was obtained from Honeywell, with a nominal purity of 98% or greater at 600°C.

[0063] The alloys were supplied by Q-metal as test specimens 3 mm thick, 20 mm long and 7 mm wide. The specimens were washed and dried before being weighed and then inserted into molten NaOH. After one week the specimens were removed from the molten NaOH and any molten NaOH residue was removed from the surface of the specimen before cooling the specimen to ambient temperature and weighing. The weight loss of each specimen was recorded and expressed in mg / cm2 as a function of the surface area (i.e. length x width) of the specimen. 2 From the duration of exposure to molten NaOH, the corrosion rate was calculated and expressed in mm / year (mm / y) in relation to the thickness of the specimen. The results are shown in Figure 5, which shows the weight change and corrosion rate at different oxo-acidity levels determined at a corrosion rate of ±0.1 mm / y. Different corrosion rates were obtained for the same type of specimen at different partial pressures of water (ppH2O) in the process gas used to adjust the steady-state concentration in the molten salt. Figure 5 shows the results obtained from the weight change and the inductively coupled plasma optical emission spectroscopy (ICP-OES) results. The lowest corrosion rate from the weight change calculation is found to be 0 mm / y at a p[H2O] of 2.27. [Explanation of symbols]

[0064] 1. Electrochemical cell 2 containers 20 Crucible 21 Lid 22 Opening 23 Insulating materials 231 Heating wire 24 Cell Support 3 Molten salts of metal hydroxides 11 Working electrode 12 Reference electrode 121 Membrane 13 Counter electrode 14 Thermocouple 41 Gas inlet 42 Gas outlet

Claims

1. 1. A method for adjusting the oxo-acidity of a molten metal hydroxide salt in an energy or heat storage container, wherein the hydroxide salt provides a medium for energy or heat storage, comprising: H in molten metal hydroxides 2 O, O 2- and O.H. - estimating at least one target concentration of providing an oxo acidity control component; contacting said oxo-acidity control component with said molten salt of a metal hydroxide to adjust the oxo-acidity of said molten salt of a metal hydroxide.

2. 2. The method of claim 1, wherein the oxo-acidity control component is provided in a process gas comprising an inert carrier gas, and the method further comprises the step of contacting the process gas comprising the oxo-acidity control component with the molten salt of a metal hydroxide to adjust the oxo-acidity of the molten salt of a metal hydroxide.

3. 3. The method of adjusting the oxo-acidity of a molten salt as claimed in claim 2, wherein the oxo-acidity control component is water vapor, and the water vapor is added to the process gas to provide a partial pressure of water in the process gas.

4. The water vapor is added to the process gas by bubbling the process gas through a water bath, and the partial pressure of the water vapor in the process gas is: controlling the temperature of the water bath; controlling the residence time of the treatment gas in the water bath; and controlling the pressure of the treatment gas in the water bath; The method for adjusting the oxo acidity of a molten salt according to claim 3, wherein the oxo acidity is controlled by at least one of the following:

5. 3. The method of adjusting the oxo-acidity of a molten salt according to claim 2, wherein the oxo-acidity control component is added to the process gas by sublimating the oxo-acidity control component from the solid state.

6. 3. The method of adjusting the oxo-acidity of a molten salt according to claim 2, wherein the oxo-acidity control component is added to the process gas as a liquid via spraying or mist generation.

7. The molten salt of metal hydroxide is placed in a container having an inner surface made of a lining material, and the OH - , O 2- , and H 2 7. The method for adjusting the oxo-acidity of a molten salt according to claim 1, wherein the target concentration of at least one of O is defined for the lining material.

8. 8. The method for adjusting the oxo-acidity of a molten salt according to claim 7, wherein the molten salt of a metal hydroxide is stationary or circulated within the container by forced convection or forced circulation.

9. 9. The method for adjusting the oxo-acidity of a molten salt according to claim 7 or 8, wherein the oxo-acidity control component is contacted with the molten salt of a metal hydroxide located at a distance in the range of 0 cm to 100 cm from the lining material.

10. 10. A method for adjusting the oxo-acidity of a molten salt according to any one of claims 1 to 9, wherein heat is added to or removed from the molten salt of a metal hydroxide.

11. 10. The method of adjusting the oxo-acidity of a molten salt according to any one of claims 7 to 9, wherein the container comprises a heat source and / or a heat sink configured to create a temperature gradient in the range of 0.1 °C / cm to 10 °C / cm in the molten salt of a metal hydroxide.

12. 12. A method for adjusting the oxo-acidity of a molten salt according to any one of claims 1 to 11, wherein a cover gas above the molten salt of metal hydroxide is maintained at a pressure higher than ambient pressure.

13. 13. The method for adjusting the oxo-acidity of a molten salt according to claim 12, wherein the cover gas is the process gas.

14. 14. A method for adjusting the oxo-acidity of a molten salt according to any one of claims 2 to 13, wherein the process gas is bubbled through the molten salt of a metal hydroxide.

15. The H 2 O, O 2- and O.H. - 15. The method for adjusting the oxo-acidity of a molten salt according to claim 1 , wherein the target concentration of at least one of the above is estimated at at least three different temperatures within the range of the melting point and boiling point of the salt of a metal hydroxide.

16. A method for determining the oxo acidity window of a material comprising: selecting a target material and a metal hydroxide; Providing a crucible of inert material; applying the metal hydroxide into the crucible of inert material and heating the metal hydroxide to provide a molten salt of the metal hydroxide; providing a working electrode made of the material of interest, a reference electrode and a counter electrode made of an inert metal; inserting the working electrode, the reference electrode and the counter electrode into the molten salt of the metal hydroxide; applying a gas above the molten salt of the metal hydroxide and doping the gas with an oxo acidity control component; applying a current between the working electrode and the counter electrode and recording the polarization of the working electrode; determining an oxo-acidity window of the material of interest from the polarization of the working electrode; The method includes:

17. 1. A method for determining the oxo acidity window of a material, comprising: selecting a target material and a metal hydroxide; Providing a crucible of inert material; applying the metal hydroxide into the crucible of inert material and heating the metal hydroxide to provide a molten salt of the metal hydroxide; inserting a test specimen of the material of interest into the molten salt of the metal hydroxide; adding an oxo acidity control component to a process gas and contacting said process gas with said molten salt of said metal hydroxide; determining the oxo-acidity window of the material from the weight loss of the test specimen; The method includes:

18. 1. An energy storage system comprising a container, a heat sink and / or a heat source, and a molten metal hydroxide salt disposed within the container, wherein the molten salt of metal hydroxide is circulated within the container by forced convection obtained from the heat sink and / or the heat source, the heat sink and / or the heat source being configured to create a temperature gradient in the range of 0.1° C. / cm to 10° C. / cm over a distance from the heat sink and / or the heat source, as the case may be, to a point in the molten salt of metal hydroxide.

19. 20. The energy storage system of claim 18, wherein the heat sink and / or the heat source are configured to contact the molten salt of metal hydroxide over a distance in the range of 0 cm to 100 cm from the lining material.

20. 20. An energy storage system according to claim 18 or 19, wherein the distance from the heat sink and / or heat source as the case may be to the point in the molten salt of metal hydroxide is in the range of 5cm to 20cm.

21. 21. The energy storage system of claim 18, wherein the oxo-acidity of the molten metal hydroxide salt is adjusted using a method according to any one of claims 1 to 15.

Citation Information

Patent Citations

  • Molten salt reactor

    WO2018229265A1

  • Structural material for molten salt reactors

    WO2020157247A1