Preparation method of PBT silver-ion antibiotic moisture-absorption deodorization fibre
A silver ion and fiber technology is applied in the field of preparation of PBT silver ion antibacterial, moisture-absorbing and deodorizing fibers, which can solve problems such as no reports on PBT silver-ion antibacterial, moisture-absorbing and deodorizing fibers, and achieve excellent chemical resistance, good durability, Good durability
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2010-06-30
- Estimated Expiration
- Not applicable · inactive patent
Smart Images
Figure 1 Figure 2
Abstract
Description
technical field
[0001] The invention belongs to the technical field of fiber preparation, in particular to a method for preparing a PBT silver ion antibacterial, moisture-absorbing and deodorizing fiber. Background technique
[0002] Many metal ions have bactericidal and anti-mildew effects. The antibacterial mechanism is generally divided into two categories: one is to destroy the structure of bacteria, and the other is to affect metabolism and physiological activities. Silver ions can kill bacteria by destroying the plasma membrane of bacteria. In addition, silver ions can destroy the three-dimensional conformation of proteases by combining with the sulfhydryl group (-SH) of proteins and kill microorganisms. Therefore, silver fibers (silver ions) provide dual functions of antibacterial and deodorizing. Bacterial growth will cause body odor. Coincidentally, qualitatively altered proteins will also produce odor on clothes and socks. The silver component on the surface of s...
Examples
preparation example Construction
[0013] In conjunction with accompanying drawing, the preparation method of a kind of PBT silver ion antibacterial hygroscopic deodorant fiber of the present invention comprises the following steps:
[0014] Step 1. Pre-crystallize the material, which is a mixture of PBT slices and silver ion SHT antibacterial plastic masterbatch; specifically, dry hot air is used for pre-crystallization; when the material is pre-crystallized, the pre-crystallization temperature is 120-125°C , The temperature of the dry hot air is 130-135°C, the air dew point is less than or equal to -60°C, the moisture content of the material is 30ppm, and the drying time is 8-10 hours.
[0015] Step 2. Material screw feeding: first dry the color masterbatch with hot air, then feed the mixed material of the color masterbatch and PBT chips into the screw extruder through a special color masterbatch feeder that can measure the color masterbatch Middle; when the material is screw-fed, the material is a mixture of...
Embodiment 1
[0020] A preparation method of PBT silver ion antibacterial, moisture-absorbing and deodorant fiber, comprising the following steps:
[0021] Step 1. Pre-crystallize the material, which is a mixture of PBT slices and silver ion SHT antibacterial plastic masterbatch; specifically, dry hot air is used for pre-crystallization; when the material is pre-crystallized, the pre-crystallization temperature is 120 ° C, and the The temperature of the hot air is 130°C, the air dew point is -60°C, the moisture content of the material is 30ppm, and the drying time is 8 hours.
[0022] Step 2. Material screw feeding: first dry the color masterbatch with hot air, then feed the mixed material of the color masterbatch and PBT chips into the screw extruder through a special color masterbatch feeder that can measure the color masterbatch Middle; when the material is screw-fed, the material is a mixture of PBT (polybutylene terephthalate) slices and silver ion SHT (nano silver inorganic antibacter...
Embodiment 2
[0026] A preparation method of PBT silver ion antibacterial, moisture-absorbing and deodorant fiber, comprising the following steps:
[0027] Step 1. Pre-crystallize the material, which is a mixture of PBT slices and silver ion SHT antibacterial plastic masterbatch; specifically, dry hot air is used for pre-crystallization; when the material is pre-crystallized, the pre-crystallization temperature is 125 ° C, and the drying The temperature of the hot air is 135°C, the air dew point is -55°C, the moisture content of the material is 30ppm, and the drying time is 10 hours.
[0028] Step 2. Material screw feeding: first dry the color masterbatch with hot air, then feed the mixed material of the color masterbatch and PBT chips into the screw extruder through a special color masterbatch feeder that can measure the color masterbatch Middle; when the material is screw-fed, the material is a mixture of PBT (polybutylene terephthalate) slices and silver ion SHT (nano silver inorganic an...