A clamp for testing the breaking load of a tension wire clamp and a manufacturing method thereof

By designing a tensile wire clip failure load test fixture of polygonal column structure, the problem of steel wire rope falling off and deflection in mechanical performance test is solved, the accuracy and stability of the test results are achieved, and the ductility and insulation of the fixture are enhanced.

CN107677540BActive Publication Date: 2024-11-22JIANGSU SHUANGHUI POWER DEV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201710829791.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2017-09-15
Publication Date
2024-11-22
Estimated Expiration
2037-09-15

AI Technical Summary

Technical Problem

The existing bolt-type tension-resistant wires are clamped in mechanical performance tests. The wire ropes are prone to fall off or deflect due to excessive mechanical load, resulting in inaccurate test results and reduced accuracy.

Method used

Design a tension-resistant wire clamp failure load test fixture including the first clamp sleeve and the second clamp sleeve, stabilize the wire rope through a polygon column structure to avoid falling off and deflection, and use multi-alloy forging and ceramic powder to improve the stability of the fixture and insulation.

Benefits of technology

It improves the accuracy and stability of the test results, reduces power loss, enhances the ductility and insulation of the fixture, and ensures the position stability of the tension clamp and the convenience of the test.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN107677540B_ABST
    Figure CN107677540B_ABST
Patent Text Reader

Abstract

The present invention discloses a clamp for a destructive load test of a tension clamp and a manufacturing and testing method thereof. The device and the testing method belong to the technical field of electric power hardware, and solve the problems of poor accuracy, low convenience, and weak stability of hardware test results in the prior art. The device and the testing method include a first clamping sleeve and a second clamping sleeve. The first clamping sleeve includes a connecting seat fixedly connected to the end of the tension clamp and a fixing sleeve integrally arranged with the connecting seat. The connecting seat is provided with a groove for sleeve-connecting the tension clamp, and the bottom of the groove is provided with an arc-shaped groove matching the end angle of the tension clamp. The fixing sleeve and the second clamping sleeve are both polygonal columns with a through hole for fixing a steel wire rope inside. The present invention utilizes the stable connection between the first clamping sleeve and the tension clamp to ensure that the position of the tension clamp is stable and without deviation, thereby improving the accuracy of the test results. Through the coordinated use of the first clamping sleeve and the second clamping sleeve, the stability and convenience of the destructive load test of the tension clamp are enhanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of electric power hardware, and in particular relates to a clamp for a strain clamp breaking load test and a manufacturing test method thereof. Background Art

[0002] Strain clamps are used to fix conductors to withstand conductor tension and hang conductors on the hardware on tension strings or poles. Strain clamps are used for corner, splice and terminal connections, which are related to the safety of conductors or poles. Therefore, mechanical performance tests are required for strain clamps before operation.

[0003] At present, the mechanical property test of bolt-type tension clamps on the market is mainly carried out by pressing the wire rope through the bolts of the tension clamp, and then applying mechanical loads to the wire rope and the outer end of the tension clamp respectively, so as to test the destructive load of the bolt-type tension clamp. This method has the following shortcomings: when the tightening force between the bolt and the wire rope is less than the applied mechanical load, the position of the wire rope is prone to shift, so that the destructive load of the tension clamp cannot be accurately measured. Moreover, since the wire rope is pressed in the tension clamp, as the mechanical load increases, the placement angle of the tension clamp is prone to deflect, resulting in a decrease in the test accuracy. Summary of the invention

[0004] The present invention aims to provide a clamp for testing the breaking load of a tension clamp, which has high test result accuracy, good convenience and strong stability, and a manufacturing test method thereof.

[0005] In order to achieve the above technical objectives, the technical solutions adopted by the fixture for breaking load test of tension clamp and the manufacturing test method thereof of the present invention are as follows:

[0006] A clamp for a destructive load test of a tension clamp comprises a first clamping sleeve fixedly connected to one end of the tension clamp and a second clamping sleeve arranged at the other end of the tension clamp, the first clamping sleeve comprises a connecting seat fixedly connected to the end of the tension clamp and a fixing sleeve integrally arranged with the connecting seat, the connecting seat is provided with a groove for sleeve-connecting the tension clamp, the bottom of the groove is provided with an arc-shaped groove matching the end angle of the tension clamp, the fixing sleeve and the second clamping sleeve are both polygonal columns with a through hole for fixing a wire rope inside. In the present invention, a test clamp is provided so that the wire rope is firmly crimped into the tension clamp, thereby avoiding the problem of the wire rope falling off from the tension clamp due to excessive mechanical load, and at the same time, the first clamping sleeve generates a reverse force on the wire rope, so that the tension clamp remains stable during the test, thereby ensuring the accuracy of the test.

[0007] Preferably, the polygonal column is a quadrilateral column, a hexagonal column or an octagonal column. The polygonal column is used to reduce the torsion angle of the fixing sleeve and the second clamping sleeve, thereby improving stability.

[0008] Preferably, one end of the steel wire rope is crimped into the first clamping sleeve, and the other end is crimped into the second clamping sleeve. By crimping the steel wire rope into the first clamping sleeve and the second clamping sleeve, the steel wire rope can maintain stability during the tension clamp load test, avoiding deflection due to non-test factors, thereby reducing the test accuracy.

[0009] Preferably, the first clamping sleeve and the second clamping sleeve contain, by weight percentage: 0.6-0.8% silicon, 0.3-0.5% magnesium, 0.5-1% copper, 0.2-0.4% iron, 2-4% chromium, 2-3% titanium, 0.4-0.6% nickel, 0.2-0.5% vanadium, 6-8% ceramic powder, 3-4% aluminum, and the rest is cast steel. To improve the ductility of the clamp, titanium, vanadium and chromium are added during the alloy smelting.

[0010] A method for manufacturing a clamp for a destructive load test of a tension clamp comprises the following steps: by weight percentage: adding 3-4% aluminum blocks into a smelting furnace, heating to 700°C for melting, after the aluminum is melted, raising the temperature to 1500°C, first adding cast steel, then sequentially adding 0.3-0.5% magnesium, 0.5-1% copper, 0.6-0.8% silicon, and then simultaneously adding 0.4-0.6% nickel and 0.2-0.4% iron, raising the temperature to 2000°C, then sequentially adding 2-3% titanium, 2-4% chromium, and 0.2-0.5% vanadium, during which nitrogen is continuously introduced, and when the metal is completely melted, casting is performed to obtain a first clamping sleeve and a second clamping sleeve, and then ceramic powder is added into the groove and through hole of the first clamping sleeve and the through hole of the second clamping sleeve, and the mixture is heated and melted again so that the ceramic powder is completely coated in the groove and the through hole. Nitrogen is introduced to prevent the generation of metal oxides, which in turn reduces the mechanical strength of the alloy. To improve the insulation of the fixture, ceramic powder elements are added to the grooves and through holes to make the fixture insulating and avoid eddy currents generated during electrical performance testing. To make the alloy stronger, nickel and iron are added at the same time so that the structures between the metal elements support each other.

[0011] A method for testing the breaking load of a tension clamp comprises the following steps:

[0012] (1) Control the ambient temperature between 0 and 40°C, crimp one end of the wire rope into the first clamping sleeve, and at the same time, clamp the end angle of the tension clamp into the arc-shaped groove, and crimp the other end of the wire rope into the second clamping sleeve;

[0013] (2) Apply a mechanical load that reaches 50% of the calculated breaking force of the tension clamp as the pre-tension force, and add a ring mark on the surface of the wire rope at the exit of the clamp;

[0014] (3) Continue to apply mechanical load, and the loading rate per minute shall not exceed 10% of the calculated breaking load of the wire clamp;

[0015] (4) When the load reaches the calculated value of the wire clamp, if the wire rope still does not move, continue to increase the load until the wire clamp is damaged, stop the test and record the breaking force value;

[0016] (5) Repeat steps 1 to 3 to reduce the mechanical load. The loading rate per minute should not exceed 10% of the calculated breaking load of the wire clamp. Test the ability of the wire clamp to cope with load changes.

[0017] Compared with the prior art, the present invention has the following beneficial effects:

[0018] 1. The present invention utilizes the stable connection between the first clamping sleeve and the tension clamp, which not only ensures that the tension clamp is in a stable position without deviation, but also fixes one end of the wire rope, thereby facilitating accurate load measurement of the tension clamp and improving the accuracy of the test results;

[0019] 2. The present invention uses the second clamping sleeve to make the other end of the wire rope into a whole strand, avoiding the cumbersomeness of using tape to tie in conventional tests, and improving the convenience of disassembly and installation. At the same time, through the coordinated use of the first clamping sleeve and the second clamping sleeve, the stability and convenience of the tension clamp breaking load test are enhanced;

[0020] 3. The present invention adopts multi-element alloy forging, which not only improves the ductility of the test equipment, but also strengthens the strength of the test equipment, reduces the power loss, and due to the softness of the ceramic powder, it not only fits the steel wire rope, improves the tightness of the device, but also has strong insulation, which provides a basis for power performance testing;

[0021] 4. The present invention utilizes a clamp in conjunction with a tension clamp to perform a mechanical property test, and by first loading the load and then reducing the load, the breaking load of the tension clamp can be accurately measured. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a schematic diagram of the structure of the test of the present invention;

[0023] Figure 2 It is a schematic diagram of the structure of the present invention;

[0024] Figure 3 It is a cross-sectional view of the second jacket of the present invention.

[0025] In the figure: 1. tension clamp; 2. second clamping sleeve; 3. connecting seat; 4. fixing sleeve; 5. groove; 6. arc-shaped groove; 7. through hole. DETAILED DESCRIPTION

[0026] The present invention is further explained below in conjunction with the accompanying drawings and specific implementation methods. It should be understood that these implementation methods are only used to illustrate the present invention and are not used to limit the scope of the present invention. After reading the present invention, various equivalent forms of modifications to the present invention by those skilled in the art all fall within the scope defined by the claims attached to this application.

[0027] like Figure 1 — Figure 3 As shown, a clamp for a destructive load test of a tension clamp comprises a first clamping sleeve fixedly connected to one end of the tension clamp 1 and a second clamping sleeve 2 arranged at the other end of the tension clamp 1, the first clamping sleeve comprises a connecting seat 3 fixedly connected to the end of the tension clamp 1 and a fixing sleeve 4 integrally arranged with the connecting seat 3, the connecting seat 3 is provided with a groove 5 for sleeve-engaging the tension clamp 1, the bottom of the groove 5 is provided with an arc-shaped groove 6 matching the end angle of the tension clamp 1, the fixing sleeve 4 and the second clamping sleeve 2 are both polygonal columns with a through hole 7 for fixing a steel wire rope inside, the polygonal column is a quadrilateral column, a hexagonal column or an octagonal column, one end of the steel wire rope is crimped into the first clamping sleeve, and the other end is crimped into the second clamping sleeve 2. The first clamping sleeve and the second clamping sleeve contain, by weight percentage, 0.6-0.8% silicon, 0.3-0.5% magnesium, 0.5-1% copper, 0.2-0.4% iron, 2-4% chromium, 2-3% titanium, 0.4-0.6% nickel, 0.2-0.5% vanadium, 6-8% ceramic powder, 3-4% aluminum, and the rest is cast steel.

[0028] In the prior art, when the bolt-type tension clamp is subjected to a destructive load test, there is a lack of a test fixture. As the mechanical load on the end of the wire rope increases, the wire rope is prone to fall off the tension clamp, causing the test to be terminated. At the same time, the end of the wire rope crimped in the tension clamp is susceptible to strong tensile force and deflects, thereby driving the deflection of the tension clamp, resulting in a decrease in test accuracy. To solve such problems, the present invention installs fixtures on both sides of the bolt-type tension clamp, one end of the wire rope is crimped into the first clamping sleeve, and the other end is crimped into the second clamping sleeve 2, to ensure It proves that the position of the tension clamp is stable during the load test, and avoids the problem of insufficient crimping strength of the tension clamp bolts and offset position of the wire rope during conventional load tests, which in turn causes inaccurate testing. As the mechanical load at the second clamping sleeve 2 ends increases, the first clamping sleeve generates tension due to the action of the wire rope. Since the first clamping sleeve is firmly connected to the end of the tension clamp, the first clamping sleeve is subjected to reverse tension to achieve force balance, thereby ensuring the stability of the tension clamp placement position, avoiding deflection, and ensuring the test accuracy.

[0029] Among them, the method for making a clamp for a destructive load test of a tension clamp includes the following steps: by weight percentage: adding 3-4% aluminum blocks into a smelting furnace, heating to 700°C to melt, after the aluminum is melted, raising the temperature to 1500°C, first adding cast steel, and then adding 0.3-0.5% magnesium, 0.5-1% copper, 0.6-0.8% silicon in sequence, and then adding 0.4-0.6% nickel and 0.2-0.4% iron at the same time, raising the temperature to 2000°C, and then adding 2-3% titanium, 2-4% chromium, and 0.2-0.5% vanadium in sequence, and continuously introducing nitrogen during the process. When the metal is completely melted, casting is performed to obtain a first clamping sleeve and a second clamping sleeve, and then 6-8% ceramic powder is added to the grooves and through holes of the first clamping sleeve and the through holes of the second clamping sleeve, and heated and melted again to completely coat the ceramic powder in the grooves and through holes. By adding ceramic powder into the fixture, the insulation of the fixture can be improved to avoid eddy currents during power performance testing.

[0030] The method for testing the breaking load of a tension clamp comprises the following steps:

[0031] (1) Control the ambient temperature between 0 and 40°C, crimp one end of the wire rope into the first clamping sleeve, and at the same time clamp the end angle of the tension clamp into the arc-shaped groove, and continue to crimp the wire rope into the second clamping sleeve;

[0032] (2) Apply a mechanical load that reaches 50% of the calculated breaking force of the tension clamp as the pre-tension force, and add a ring mark on the surface of the wire rope at the exit of the clamp;

[0033] (3) Continue to apply mechanical load, and the loading rate per minute shall not exceed 10% of the calculated breaking load of the wire clamp;

[0034] (4) When the load reaches the calculated value of the wire clamp, if the wire rope still does not move, continue to increase the load until the wire clamp is damaged, stop the test and record the breaking force value;

[0035] (5) Repeat steps 1 to 3 to reduce the mechanical load. The loading rate per minute should not exceed 10% of the calculated breaking load of the wire clamp. Test the ability of the wire clamp to cope with load changes.

Claims

1. A clamp for testing the breaking load of a tension clamp. Features: It includes a first clamping sleeve fixedly connected to one end of the tension wire clamp and a second clamping sleeve arranged at the other end of the tension wire clamp, the first clamping sleeve includes a connecting seat fixedly connected to the end of the tension wire clamp and a fixing sleeve integrally arranged with the connecting seat, the connecting seat is provided with a groove for sleeve-connecting the tension wire clamp, the bottom of the groove is provided with an arc-shaped groove matching the end angle of the tension wire clamp, the fixing sleeve and the second clamping sleeve are both polygonal columns with a through hole for fixing a steel wire rope inside, the polygonal column is a quadrilateral column, a hexagonal column or an octagonal column, one end of the steel wire rope is crimped into the first clamping sleeve, and the other end is crimped into the second clamping sleeve, the first clamping sleeve and the second clamping sleeve contain, by weight percentage: 0.6-0.8% silicon, 0.3-0.5% magnesium, 0.5-1% copper, 0.2-0.4% iron, 2-4% chromium, 2-3% titanium, 0.4-0.6% nickel, 0.2-0.5% vanadium, 6-8% ceramic powder, 3-4% aluminum, and the rest is cast steel.

2. A method for manufacturing a clamp for a tension clamp breaking load test according to claim 1, Features: The method comprises the following steps: by weight percentage: adding 3-4% aluminum blocks into a smelting furnace, heating to 700°C for melting, after the aluminum is melted, raising the temperature to 1500°C, first adding cast steel, then sequentially adding 0.3-0.5% magnesium, 0.5-1% copper, 0.6-0.8% silicon, and then simultaneously adding 0.4-0.6% nickel and 0.2-0.4% iron, raising the temperature to 2000°C, then sequentially adding 2-3% titanium, 2-4% chromium, and 0.2-0.5% vanadium, during which nitrogen is continuously introduced, and when the metal is completely melted, casting is performed to obtain a first clamping sleeve and a second clamping sleeve, and then ceramic powder is added into the groove and through hole of the first clamping sleeve and the through hole of the second clamping sleeve, and the ceramic powder is heated and melted again, so that the ceramic powder is completely coated in the groove and the through hole.

3. A method for testing the breaking load of a tension clamp breaking load test fixture according to claim 1, Features: The following steps are involved: Control the ambient temperature at 0-40℃, crimp one end of the wire rope into the first clamping sleeve, and at the same time clamp the end angle of the tension clamp into the arc-shaped groove, and continue to crimp the wire rope into the second clamping sleeve; Apply a mechanical load that reaches 50% of the calculated breaking force of the tension clamp as pre-tension, and add a ring mark on the surface of the wire rope at the clamp outlet; Continue to apply mechanical load, and the loading speed per minute shall not exceed 10% of the calculated breaking load of the wire clamp; When the load reaches the calculated value of the wire clamp, if the wire rope still does not move, continue to increase the load until the wire clamp is broken, stop the test and record the breaking force value; Repeat steps 1 to 3 to reduce the mechanical load. The loading rate per minute should not exceed 10% of the calculated breaking load of the wire clamp to test the wire clamp's ability to cope with load changes.