A tire capsule mold
By dividing the oil chamber chamber into multiple sub-oil chambers in the tire capsule mold and setting up a communication channel, the problems of slow flow and uneven heating of the existing mold heating medium are solved, faster heating and more uniform heating are achieved, and faster heating is achieved, improving The vulcanization effect is achieved.
Patent Information
- Application Number
- CN201810410613.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-05-02
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2038-05-02
AI Technical Summary
The heating medium of existing tire capsule molds flows slowly, resulting in slower temperature rise and uneven heat treatment, affecting the vulcanization effect.
Design a tire capsule mold, which divides it into multiple sub-oil chambers distributed in the height direction of the mold by setting a transverse plate in the oil chamber cavity, and connects adjacent sub-oil chambers through a communication channel to ensure that the heating medium is from the lower end Enter and gradually fill the upper end to improve the flow rate and uniformity of the heating medium.
It improves the heating speed and heating uniformity of the mold, and significantly improves the quality and service life of the vulcanized capsules.
Smart Images

Figure CN108381824B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of tire mold structures, in particular to a tire bladder mold. Background Art
[0002] The production methods of curing bladders are mainly compression molding and injection molding. The tire bladder molds of these two methods are composed of an upper outer mold, a lower outer mold, an upper core mold, and a lower core mold. The upper outer mold, the lower outer mold, and the upper core mold are divided into several heating spaces, and the heating medium enters the heating space to vulcanize the bladder.
[0003] Figure 1 Schematic diagram of the structure of a tire bladder mold 10 in the prior art. Figure 2 This is a structural diagram from another perspective of the figure.
[0004] Please refer to Figure 1 and Figure 2 As can be seen from the figure, the outer mold includes an upper outer mold 111 and a lower outer mold 112 that cooperate with each other. Further, the cylindrical upper outer mold 111 has an oil chamber 12 for accommodating a heating medium. A first partition 141 is arranged in the oil chamber 12, and the periphery of the first partition 141 is arranged on the inner wall of the oil chamber 12 to completely separate the oil chamber 12. The oil inlet 131 and the oil outlet 132 are both arranged through the side wall of the oil chamber 12, and the oil inlet 131 and the oil outlet 132 are symmetrically arranged on both sides of the first partition 141.
[0005] A plurality of second partitions 142 are also provided in the oil chamber 12, and the first partition 141 and the plurality of second partitions 142 are circumferentially arrayed on the upper outer mold 111. The first partition 141 and the plurality of second partitions 142 divide the oil chamber 12 into a plurality of closed heating spaces 150. The second partition 142 is provided with a through hole 151, and the through hole 151 is used to connect the heating spaces 150 adjacent to the second partition 142.
[0006] However, in this structure, the heating medium flows slowly in the oil chamber 12, resulting in a slow temperature rise of the mold and uneven heating, thereby affecting the vulcanization effect of the product. Summary of the invention
[0007] The object of the present invention is to provide a tire bladder mold, which improves the problem of uneven heating of the existing mold, thereby ensuring the vulcanization effect of the tire product.
[0008] The embodiments of the present invention are implemented by the following technical solutions:
[0009] The tire bladder mold includes a mold body, an oil chamber cavity, a transverse plate and a partition. The oil chamber cavity is a hollow and closed annular structure distributed along the circumference of the mold body; the transverse plate divides the oil chamber cavity into at least two annular sub-oil chambers, and the multiple sub-oil chambers are distributed along the height direction of the mold body; an oil inlet is provided on the side wall of the sub-oil chamber near the lower end; an oil outlet is provided on the side wall of the sub-oil chamber near the upper end; a connecting channel connecting adjacent sub-oil chambers is provided on the transverse plate; and a partition is provided on the inner wall of the sub-oil chamber, and the partition is configured to separate the sub-oil chambers.
[0010] The inventors found that the existing tire bladder mold divides the oil chamber into multiple heating spaces, and heats the entire mold by entering the heating medium (usually medium oil) from the oil inlet and discharging from the oil outlet. However, the prior art divides the oil chamber into multiple heating spaces arranged circumferentially. Although this heating method divides the larger oil chamber into smaller heating spaces for heating, it is helpful to improve the inconvenience and slow heating rate caused by direct heating of the entire oil chamber. However, this heating method makes it impossible for the heating medium to fill the entire heating space well, and this heating method requires that multiple (generally more than 6) heating spaces be filled in sequence. The heating medium flows slowly in the oil chamber, resulting in a slow temperature rise of the mold, and the heating is mostly uneven, thereby affecting the vulcanization effect of the product.
[0011] Based on this, the inventor invented a tire bladder mold, which sets a horizontal plate on the oil chamber cavity, and then divides the oil chamber cavity into at least two sub-oil chambers distributed in the height direction of the mold body. The connecting channel on the horizontal plate is used to connect the adjacent sub-oil chambers in the upper and lower directions. At the same time, an oil inlet is set on the side wall of the sub-oil chamber near the lower end; an oil outlet is set on the side wall of the sub-oil chamber near the upper end. In this way, the heating medium enters the sub-oil chamber from the oil inlet at the lower end of the mold body, and after the heating medium fills the sub-oil chamber at the lower end, it flows upward in sequence until it is discharged from the oil outlet of the sub-oil chamber at the upper end of the mold body. This arrangement ensures that the oil chamber cavity can be filled with the heating medium, ensuring the uniformity of heating; from the lower end to the upper end of the mold body, the heating medium gradually fills the corresponding sub-oil chamber, and this method also ensures the flow channel speed of the heating medium in the sub-oil chamber, thereby increasing the heating rate of the mold. The partition provided in the sub-oil chamber further defines the space of the sub-oil chamber, thereby ensuring the stability and uniformity of the movement of the heating medium in the sub-oil chamber, and further adjusting the uniformity and stability of the temperature rise of the mold.
[0012] In summary, such a tire bladder mold has a simple structure and is easy to operate. It can significantly increase the flow rate of the heat medium in the oil chamber cavity, slow down the temperature rise of the mold, ensure uniform heating of the mold body, and thus improve the vulcanization effect of the product.
[0013] Further, in the sub-oil chamber near the lower end, the oil inlet and the communication channel are located on both sides of the partition respectively;
[0014] In the sub-oil chamber near the upper end, the oil outlet and the communication channel are respectively located on both sides of the partition.
[0015] Further, the tire bladder mold includes at least three sub-oil chambers;
[0016] A sub-oil chamber located in the middle position has two sub-oil chambers adjacent to each other in the height direction;
[0017] The sub-oil chamber located in the middle position is connected with the adjacent sub-oil chambers through two connecting passages respectively;
[0018] The two communication channels are respectively arranged on both sides of the partition plate of the sub-oil chamber located in the middle position;
[0019] Preferably, the two communicating channels are adjacent to the partition;
[0020] Furthermore, the plurality of partitions are located in the same plane up and down.
[0021] Further, the partition is radially arranged on the inner wall of the sub-oil chamber;
[0022] Preferably, the plurality of partitions are all located in a radial direction with the oil chamber cavity as the center;
[0023] Preferably, the number of the partitions is the same as the number of the oil sub-chambers.
[0024] Furthermore, the communication channels are symmetrically arranged on both sides of the partition.
[0025] Furthermore, from the bottom of the oil chamber cavity to the top of the oil chamber cavity, the radial widths of the plurality of sub-oil chambers gradually increase.
[0026] Further, a plurality of sub-oil chambers are concentrically arranged;
[0027] Furthermore, the outer diameters of the plurality of oil sub-chambers are the same.
[0028] Further, the tire bladder mold includes an outer mold and a core mold that cooperate with each other, and the outer mold includes an upper outer mold and a lower outer mold that cooperate with each other;
[0029] At least one of the upper outer mold, the lower outer mold and the core mold is provided with an oil chamber cavity.
[0030] Further, the oil inlet is arranged on the side wall of the sub-oil chamber;
[0031] The oil inlet is located near the bottom of the sub-oil chamber.
[0032] Furthermore, the oil inlet and the oil outlet are both arranged on the outer peripheral surface of the mold body.
[0033] The technical solution of the embodiment of the present invention has at least the following advantages and beneficial effects:
[0034] The tire bladder mold provided by the embodiment of the present invention includes a mold body, an oil chamber cavity, a horizontal plate and a partition. The heating medium enters the sub-oil chamber from the oil inlet at the lower end of the mold body. After the heating medium fills the sub-oil chamber at the lower end, it flows upward in sequence until it is discharged from the oil outlet of the sub-oil chamber at the upper end of the mold body. This arrangement ensures that the oil chamber cavity can be filled with the heating medium, ensuring the uniformity of heating; from the lower end to the upper end of the mold body, the heating medium gradually fills the corresponding sub-oil chamber, and this arrangement also ensures the flow channel speed of the heating medium in the sub-oil chamber, thereby increasing the heating speed of the mold. The partition arranged in the sub-oil chamber further limits the space of the sub-oil chamber, thereby ensuring the stability and uniformity of the movement of the heating medium in the sub-oil chamber, thereby adjusting the uniformity and stability of the mold heating. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0036] Figure 1 It is a structural schematic diagram of a tire bladder mold in the prior art;
[0037] Figure 2 for Figure 1 A schematic diagram of the structure from another perspective;
[0038] Figure 3 A schematic structural diagram of a tire bladder mold provided by an embodiment of the present invention;
[0039] Figure 4 for Figure 3 A schematic diagram of the structure from another perspective;
[0040] Figure 5 for Figure 4 A partial schematic diagram of
[0041] Figure 6 for Figure 3 A first partial schematic diagram of;
[0042] Figure 7 for Figure 3 A second partial schematic diagram of;
[0043] Figure 8 This is another structural schematic diagram of the tire bladder mold provided in this embodiment of the present invention.
[0044] Icons: 10-tire bladder mold; 111-upper outer mold; 112-lower outer mold; 12-oil chamber; 131-oil inlet; 132-oil outlet; 141-first partition; 142-second partition; 150-heating space; 151-through hole; 20-tire bladder mold; 210-mold body; 220-oil chamber cavity; 221-sub-oil chamber; 2211-first sub-oil chamber; 2212-second sub-oil chamber; 2213-third sub-oil chamber; 230-cross plate; 231-connecting channel; 2311-first connecting channel; 2312-second connecting channel; 241-oil inlet; 242-oil outlet; 250-partition; 261-upper outer mold; 262-lower outer mold; 270-core mold. DETAILED DESCRIPTION
[0045] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0046] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0047] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.
[0048] In the description of the present invention, it should be noted that if the terms "vertical", "horizontal", "inside", "outside", etc. indicate an orientation or positional relationship based on the orientation or positional relationship shown in the drawings, or the orientation or positional relationship in which the product of the invention is usually placed when in use, it is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.
[0049] In addition, the use of terms such as "vertical" does not mean that the component is absolutely suspended, but can be slightly inclined. In the description of the present invention, it should also be noted that unless otherwise clearly specified and limited, the use of terms such as "set", "install", "connect", and "connect" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected, or indirectly connected through an intermediate medium, or it can be internal communication between two components. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0050] Example 1
[0051] Figure 3 A schematic structural diagram of a tire bladder mold 20 provided in an embodiment of the present invention. Figure 4 for Figure 3 Schematic diagram of the structure from another perspective. Figure 5 for Figure 4 Please refer to the partial schematic diagram of Figure 3-Figure 5 A tire bladder mold 20 includes a mold body 210, an oil chamber cavity 220, a cross plate 230 and a partition 250.
[0052] The oil chamber cavity 220 is a hollow and closed annular structure distributed along the circumference of the mold body 210. The transverse plate 230 divides the oil chamber cavity 220 into at least two annular sub-oil chambers 221, and the multiple sub-oil chambers 221 are distributed along the height direction of the mold body 210. An oil inlet 241 is provided on the side wall of the sub-oil chamber 221 near the lower end; an oil outlet 242 is provided on the side wall of the sub-oil chamber 221 near the upper end. A connecting channel 231 connecting adjacent sub-oil chambers 221 is provided on the transverse plate 230.
[0053] The partition plate 250 is disposed on the inner wall of the sub-oil chamber 221 , and the partition plate 250 is configured to partition the sub-oil chamber 221 .
[0054] The inventors found that the existing tire bladder mold 20 divides the oil chamber into multiple heating spaces, and heats the entire mold through the heating medium (usually medium oil) that enters from the oil inlet 241 and is discharged from the oil outlet 242. However, the prior art divides the oil chamber into multiple heating spaces arranged circumferentially. Although this heating method divides the larger oil chamber into smaller heating spaces for heating, it is helpful to improve the inconvenience and slow heating rate caused by direct heating of the entire oil chamber. However, this heating method makes it impossible for the heating medium to fill the entire heating space well, and this heating method requires that multiple (generally more than 6) heating spaces be filled in sequence. The heating medium flows slowly in the oil chamber, resulting in a slow temperature rise of the mold, and the heating is mostly uneven, thereby affecting the vulcanization effect of the product.
[0055] The oil chamber cavity 220 of the tire bladder mold 20 in this embodiment is provided with a transverse plate 230, thereby dividing the oil chamber cavity 220 into at least two sub-oil chambers 221 distributed in the height direction of the mold body 210. The connecting channel on the transverse plate 230 is used to connect the adjacent sub-oil chambers 221 in the upper and lower directions. At the same time, an oil inlet 241 is provided on the side wall of the sub-oil chamber 221 near the lower end; and an oil outlet 242 is provided on the side wall of the sub-oil chamber 221 near the upper end. In this way, the heating medium enters the sub-oil chamber 221 from the oil inlet 241 at the lower end of the mold body 210, and after the heating medium fills the sub-oil chamber 221 at the lower end, it flows upward in sequence until it is filled and discharged from the oil outlet 242 of the sub-oil chamber 221 at the upper end of the mold body 210. This arrangement ensures that the oil chamber cavity 220 can be filled with the heating medium, ensuring the uniformity of heating; from the lower end to the upper end of the mold body 210, the heating medium gradually fills the corresponding sub-oil chamber 221, and this arrangement also ensures the flow speed of the heating medium in the sub-oil chamber 221, thereby increasing the heating speed of the mold. The partition 250 arranged in the sub-oil chamber 221 further limits the space of the sub-oil chamber 221, thereby ensuring the stability and uniformity of the movement of the heating medium in the sub-oil chamber 221, thereby adjusting the uniformity and stability of the mold heating.
[0056] Further, the tire bladder mold 20 includes an outer mold and a core mold that cooperate with each other, and the outer mold includes an upper outer mold 261 and a lower outer mold 262 that cooperate with each other; at least one oil chamber cavity 220 needs to be provided in the upper outer mold 261, the lower outer mold 262 and the core mold. It can also be seen from the figure that the structural schematic diagram of the outer mold (including the upper outer mold 261 and the lower outer mold 262) shown here. The outer mold is cylindrical. The upper outer mold 261 is provided with 3 sub-oil chambers 221, and the lower outer mold 262 is provided with 2 sub-oil chambers 221.
[0057] It can be seen from the figure that the number of the partitions 250 is the same as the number of the sub-oil chambers 221, and the partitions 250 are radially arranged on the inner wall of the sub-oil chambers 221. This is just an example, and in other embodiments, it is not limited to this.
[0058] Furthermore, the multiple sub-oil chambers 221 are all concentrically arranged; and the multiple sub-oil chambers 221 have the same outer diameter. It should be noted here that the three sub-oil chambers 221 of the upper outer mold 261 have the same outer diameter and are concentrically arranged. The two sub-oil chambers 221 of the lower outer mold 262 are concentrically arranged, but have different outer diameters. This is mainly designed to adapt to the different heating temperatures and different heating rates required at different parts of the outer mold.
[0059] It can also be seen from the figure that the radial widths of the multiple sub-oil chambers 221 gradually increase from the bottom of the oil chamber cavity 220 to the top of the oil chamber cavity 220. Further, from the bottom to the top of the upper outer mold 261, the radial thickness of the upper outer mold 261 gradually increases, and the radial widths of the three sub-oil chambers 221 of the upper outer mold 261 gradually increase, so that the above-mentioned sub-oil chambers 221 are at the same distance from the inner side wall of the upper outer mold 261, thereby ensuring the uniformity of heating of the inner side wall of the upper outer mold 261 (the inner side wall is the vulcanization working surface) and improving the tire vulcanization effect.
[0060] It is understandable that the radial widths of the plurality of sub-oil chambers 221 may be arranged in other ways. In this embodiment, the radial thickness of the lower outer mold 262 gradually decreases from the bottom to the top, and the radial widths of the two sub-oil chambers 221 of the lower outer mold 262 gradually decrease, and the purpose of this is also to ensure the uniformity of heating of the inner side wall of the lower outer mold 262 (the inner side wall is the vulcanization working surface) and improve the tire vulcanization effect.
[0061] It can also be seen from the figure that in this embodiment, the outer diameters of the two sub-oil chambers 221 of the lower outer mold 262 are not equal. Because the lower outer mold 262 has a larger volume, without increasing the sub-oil chambers 221 of the lower outer mold 262, such a setting can ensure the uniformity of heating of the lower outer mold 262, reduce the use of heating medium, and improve heating efficiency.
[0062] Further, in the sub-oil chamber 221 near the lower end, the oil inlet 241 and the communication channel 231 are respectively located on both sides of the partition 250; in the sub-oil chamber 221 near the upper end, the oil outlet 242 and the communication channel 231 are respectively located on both sides of the partition 250. Preferably, the two communication channels 231 are adjacent to the partition 250.
[0063] In this embodiment, the oil inlet 241 and the communication channel 231 are respectively adjacent to the partition 250 of the lower sub-oil chamber 221, and the oil outlet 242 and the communication channel 231 are also respectively adjacent to the partition 250 of the upper sub-oil chamber 221. In this way, the flow of the medium heating medium between different sub-oil chambers 211 is facilitated, and the heating efficiency is improved.
[0064] In this way, when the heating medium enters the sub-oil chamber 221 near the lower end of the mold body 210 from the oil inlet 241, the heating medium moves along the annular inner cavity from the oil inlet 241 away from the partition 250 until the entire sub-oil chamber 221 is filled, and then it can enter the adjacent sub-oil chamber 221 from the connecting channel 231. This ensures that the heating medium can fill the sub-oil chamber 221, thereby ensuring the heating efficiency (the heating medium is supplied from bottom to top in the height direction of the mold body 210); because the heating medium fills the entire sub-oil chamber 221, the heating uniformity of the mold body 210 is guaranteed.
[0065] Furthermore, the tire bladder mold 20 includes at least three sub-oil chambers 221; a sub-oil chamber 221 located in the middle position has two sub-oil chambers 221 adjacent to each other in the height direction; the sub-oil chamber 221 located in the middle position is connected to the adjacent sub-oil chambers 221 through two connecting channels 231 respectively; the two connecting channels 231 are respectively arranged on both sides of the partition 250 of the sub-oil chamber 221 located in the middle position. Optionally, the two connecting channels 231 are adjacent to the partition 250 of the sub-oil chamber 221 located in the middle position, and the multiple partitions 250 are located in the same plane in the height direction. In this way, it is ensured that the heating medium can quickly enter the next sub-oil chamber 211 after filling one sub-oil chamber 211, thereby improving the heating efficiency; and such a setting method is convenient for processing and manufacturing, and also improves the convenience of repairing the partition 250 (because the partition 250 is located in the same plane, the partition 250 can be inspected and repaired at the same position).
[0066] It is understandable that in other embodiments of the present invention, the connecting channel 231 may maintain a preset interval with the partition 250; and the plurality of partitions 250 may not be located in the same plane in the height direction, which is not limited here.
[0067] As shown in the figure, in this embodiment, the upper mold body 210 includes a first sub-oil chamber 2211, a second sub-oil chamber 2212 and a third sub-oil chamber 2213 arranged from bottom to top. The second sub-oil chamber 2212 has a first sub-oil chamber 2211 and a third sub-oil chamber 2213 adjacent to each other in the height direction. The upper mold body 210 also includes two connecting channels 231, a first connecting channel 2311 and a second connecting channel 2312, wherein the first connecting channel 2311 is used to connect the first sub-oil chamber 2211 and the second sub-oil chamber 2212, and the second connecting channel 2312 is used to connect the second sub-oil chamber 2212 and the third sub-oil chamber 2213.
[0068] The first connecting channel 2311 and the second connecting channel 2312 are respectively disposed on both sides of the partition plate 250 of the second sub-oil chamber 2212 (see Figure 5). Further, the first sub-oil chamber 2211 is provided with an oil inlet 241, and the oil inlet 241 and the first connecting channel 2311 are respectively provided on both sides of the partition 250 of the first sub-oil chamber 2211; the third sub-oil chamber 2213 is provided with an oil outlet 242, and the oil outlet 242 and the second connecting channel 2312 are respectively provided on both sides of the partition 250 of the third sub-oil chamber 2213. In this way, the heating medium enters the cavity of the first sub-oil chamber 2211 from one side of the partition 250 of the first sub-oil chamber 2211, moves along the annular cavity of the first sub-oil chamber 2211 for one circle, fills the entire first sub-oil chamber 2211, and then enters the second sub-oil chamber 2212 from the first connecting channel 2311 on the other side of the partition 250 of the first sub-oil chamber 2211; the heating medium entering the second sub-oil chamber 2212 fills the entire second sub-oil chamber 2212, and then enters the third sub-oil chamber 2213 through the second connecting channel 2312 from the other side of the partition 250 of the second sub-oil chamber 2212 away from the first connecting channel 2311; the heating medium entering the third sub-oil chamber 2213 fills the entire third sub-oil chamber 2213, and then is discharged from the oil outlet 242 on the other side of the partition 250 of the third sub-oil chamber 2213 away from the second connecting channel 2312. In this way, the heating medium evenly fills the entire oil chamber cavity 220 from bottom to top, thereby achieving three-dimensional circulation of the heating medium in each sub-oil chamber 221, thereby ensuring the uniformity and stability of the heating of the upper mold body 210.
[0069] Optionally, the first connecting channel 2311 and the second connecting channel 2312 are symmetrically arranged on both sides of the partition 250. In this way, it is ensured that the heating medium can completely fill the entire sub-oil chamber 211, ensuring the heating efficiency. It is understandable that in other embodiments, the first connecting channel 2311 and the second connecting channel 2312 can also be asymmetrically arranged, as long as the connecting channel 231 can connect adjacent sub-oil chambers 211.
[0070] Furthermore, the partition 250 is radially arranged on the inner wall of the sub-oil chamber 221; preferably, the multiple partitions 250 are all located in the radial direction with the oil chamber cavity 220 as the center; preferably, the number of the partitions 250 is the same as the number of the sub-oil chambers 221.
[0071] It can also be seen from the figure that in this embodiment, a plurality of partitions 250 are located in the radial direction with the oil chamber cavity 220 as the center. This makes the tire bladder mold 20 have better neatness and is easy to manufacture and repair.
[0072] Furthermore, the oil inlet 241 is disposed on the side wall of the sub-oil chamber 221 and is located near the bottom of the sub-oil chamber 221. In this way, the heating medium can smoothly enter the sub-oil chamber 221, ensuring the uniformity of heating of the mold body 210 and the flow rate of the heating medium.
[0073] Furthermore, the oil inlet 241 and the oil outlet 242 are both arranged on the outer peripheral surface of the mold body 210. In this way, the arrangement of the oil inlet and outlet 242 is facilitated, the structure is simplified, and it is beneficial to manufacture and processing.
[0074] As an optional implementation, please refer to Figure 6 , Figure 6 for Figure 3 A first partial schematic diagram of .
[0075] As can be seen from the figure, in this embodiment, the upper mold body 210 includes 3 sub-oil chambers 221, namely a first sub-oil chamber 2211, a second sub-oil chamber 2212 and a third sub-oil chamber 2213 arranged from bottom to top; the first connecting channel 2311 is used to connect the first sub-oil chamber 2211 and the second sub-oil chamber 2212, and the second connecting channel 2312 is used to connect the second sub-oil chamber 2212 and the third sub-oil chamber 2213.
[0076] The partitions 250 in the three sub-oil chambers 221 are respectively arranged in a staggered manner, and further, the three partitions 250 are all located on the same oblique line.
[0077] In the height direction of the oil chamber cavity, the oil inlet 241 and the first connecting channel 2311 are arranged on both sides of the partition 250 of the first sub-oil chamber 2211. The first connecting channel 2311 communicating with the first sub-oil chamber 2211 and the second connecting channel 2312 communicating with the third sub-oil chamber 2213 are arranged on both sides of the partition 250 of the second sub-oil chamber 2212; and the partition 250 of the second sub-oil chamber 2212 is located in a direction away from the partition 250 of the first sub-oil chamber 2211 (also away from the first connecting channel 2311). The oil outlet 242 and the second connecting channel 2312 are arranged on both sides of the partition 250 of the third sub-oil chamber 2213; the partition 250 is located in a direction away from the partition 250 of the second sub-oil chamber 2212 (also away from the second connecting channel 2312). In this way, efficient and uniform heating of the mold can also be achieved.
[0078] Furthermore, in this embodiment, the oil outlet 242 or the communication channel 231 may be directly opposite to the partition plate 250 , and a communication groove (not shown in the figure) communicating with the sub-oil chamber 221 is provided in the partition plate 250 .
[0079] As another optional implementation, please refer to Figure 7 , Figure 7 for Figure 3 As can be seen from the figure, in this embodiment, the partitions 250 in the three sub-oil chambers 221 are arbitrarily arranged, and further, the three sub-oil chambers 221 are neither located in the same plane nor in the same straight line.
[0080] Optionally, in the height direction of the oil chamber cavity, the oil inlet 241 and the first connecting channel 2311 are arranged on both sides of the partition plate 250 of the first sub-oil chamber 2211 .
[0081] The first connecting channel 2311 communicating with the first sub-oil chamber 2211 and the second connecting channel 2312 communicating with the third sub-oil chamber 2213 are respectively arranged on both sides of the partition 250 of the second sub-oil chamber 2212; and the partition 250 of the second sub-oil chamber 2212 is located in a direction close to the partition 250 of the first sub-oil chamber 2211. Furthermore, the partition 250 of the second sub-oil chamber 2212 is located slightly above the partition 250 of the first sub-oil chamber 2211.
[0082] The oil outlet 242 and the second connecting channel 2312 are arranged on both sides of the partition 250 of the third sub-oil chamber 2213; the partition 250 is located away from the partition 250 of the second sub-oil chamber 2212 (also away from the second connecting channel 2312). In this way, the oil inlet 241 and the oil outlet 242 are located on the same side. In this way, efficient and uniform heating of the mold can be achieved.
[0083] In other embodiments of the present invention, the oil inlet 241 and the oil outlet 242 may be arranged in other ways, and this is just an example.
[0084] Example 2
[0085] Please refer to Figure 8 , Figure 8 A schematic structural diagram of a tire bladder mold 20 provided in this embodiment of the present invention.
[0086] Figure 8 2 shows a schematic diagram of the structure of the core mold 270, and the structure of the core mold 270 is similar to that of the outer mold. The oil chamber cavity 220 of the core mold 270 is provided with a plurality of sub-oil chambers 221 from bottom to top, and adjacent sub-oil chambers 221 are connected through a connecting channel 231. Unlike the outer mold, the oil inlet 241 of the sub-oil chamber 221 at the lower end of the mold body 210 is introduced from the axial direction of the center of the mold body 210; the oil outlet 242 of the sub-oil chamber 221 at the upper end of the mold body 210 is led out from the axial direction of the center of the mold body 210.
[0087] The tire bladder mold 20 of this embodiment of the present invention has at least the following advantages:
[0088] After the heating medium enters from the oil inlet 241, it flows to the next sub-oil chamber 221 after filling one sub-oil chamber 221, passes through each sub-oil chamber 221 in turn, and finally flows out from the oil outlet 242. At the same time, each sub-oil chamber 221 has a partition 250, so as to realize the unidirectional spiral circulation flow of the heating medium inside the sub-oil chamber 221.
[0089] Furthermore, such a tire bladder mold 20 increases the flow rate and heat transfer coefficient, improves the problem of uneven temperature of the heating medium in the oil chamber 220 caused by poor flow of the heating medium at the dead angle formed by the partition 250 and the mold body 210; on the other hand, the tire bladder mold 20 can improve the thermal energy utilization rate of the heating medium, the heating temperature is balanced, the mold is heated evenly, and the product is vulcanized uniformly. After multiple actual production verifications, after using the outer mold of the present invention, the temperature of the upper and lower outer molds 262 is uniform, and the mold heating time can be reduced by about 1 hour compared with before. In addition, the thickness of the vulcanization bladder is more balanced and the service life is longer.
[0090] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A tire bladder mold, characterized in that: include: Model, An oil chamber cavity, wherein the oil chamber cavity is a hollow and closed annular structure distributed along the circumference of the mold body; A transverse plate, wherein the transverse plate divides the oil chamber into at least two annular sub-oil chambers, and the plurality of sub-oil chambers are distributed along the height direction of the mold body; An oil inlet is provided on the side wall of the sub-oil chamber near the lower end; an oil outlet is provided on the side wall of the sub-oil chamber near the upper end; The transverse plate is provided with a communication channel connecting the adjacent sub-oil chambers; a partition plate, the partition plate being radially arranged on the inner wall of the sub-oil chamber, the partition plate being configured to partition the sub-oil chamber; In the sub-oil chamber near the lower end, the oil inlet and the communication channel are respectively located on both sides of the partition plate; In the sub-oil chamber near the upper end, the oil outlet and the communication channel are respectively located on both sides of the partition.
2. The tire bladder mold according to claim 1, characterized in that: The tire bladder mold includes at least three sub-oil chambers; One of the sub-oil chambers located in the middle position has two sub-oil chambers that are adjacent to each other in the vertical direction; The sub-oil chamber located in the middle position is communicated with the adjacent sub-oil chambers through the two communication channels respectively; The two communication channels are respectively arranged on both sides of the partition plate of the sub-oil chamber located at the middle position.
3. The tire bladder mold according to claim 2, characterized in that: The two communication channels are adjacent to the partition plate.
4. The tire bladder mold according to claim 1, characterized in that: A plurality of partitions are located in the same plane up and down.
5. The tire bladder mold according to claim 1, characterized in that: The plurality of partitions are all located in a radial direction with the oil chamber cavity as the center.
6. The tire bladder mold according to claim 1, characterized in that: The number of the partition plates is the same as the number of the sub-oil chambers.
7. The tire bladder mold according to claim 2, characterized in that: The communication channels are symmetrically arranged on both sides of the partition.
8. The tire bladder mold according to any one of claims 1 to 7, characterized in that: From the bottom of the oil chamber cavity to the top of the oil chamber cavity, radial widths of the plurality of sub-oil chambers gradually increase.
9. The tire bladder mold according to any one of claims 1 to 7, characterized in that: A plurality of said sub-oil chambers are concentrically arranged; Furthermore, the outer diameters of the plurality of oil sub-chambers are the same.
10. The tire bladder mold according to any one of claims 1 to 7, characterized in that: The tire bladder mold comprises an outer mold and a core mold that cooperate with each other, and the outer mold comprises an upper outer mold and a lower outer mold that cooperate with each other; At least one of the upper outer mold, the lower outer mold and the core mold is provided with the oil chamber cavity.
11. The tire bladder mold according to any one of claims 1 to 7, characterized in that: The oil inlet is arranged on the side wall of the sub-oil chamber; And the oil inlet is located near the bottom of the sub-oil chamber.