An Ion Source That Reduces the Escape Rate of Electrons
An escape rate and ion source technology, applied in the field of ion sources that can reduce the electron escape rate, can solve the problems of shortening the maintenance period of the cathode magnetic pole piece, pollution, and increasing the etching of the cathode magnetic pole piece.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Publication Date
- 2020-05-05
Smart Images

Figure 1 
Figure 2
Abstract
Description
technical field
[0001] The invention relates to the technical field of ion source equipment, in particular to an ion source capable of reducing the escape rate of electrons. Background technique
[0002] An anode layer plasma source is usually used in the PECVD (Plasma Enhanced Chemical Vapor Deposition) reaction. In the DLC deposition process, it is used to ionize inert gases such as argon, or directly ionize acetylene, acetone, etc. The deposition gas makes it form an ion flow and injects it into the reaction vacuum chamber, and increases the ionization rate of the deposition reaction gas, thereby increasing the proportion of SP3 in the DLC coating and the deposition rate, so as to improve the quality of the deposited film and the deposition time shortening.
[0003] The anode layer ion source was originally developed from a closed drift ion thruster used in space engines. An annular gap is opened on the cathode plate, an annular anode is set under the annular gap, and a ...
Examples
Embodiment Construction
[0018] Such as figure 1 and figure 2 As shown, the ion source that can reduce the escape rate of electrons provided by this embodiment includes a discharge chamber composed of an anode ring 4, an inner cathode 1 and an outer cathode 2, and the anode ring 4 is located between the inner cathode 1 and the outer cathode 2, The anode ring 4, the inner cathode 1 and the outer cathode 2 are all axisymmetric structures, and the entire discharge chamber is symmetrical about the central axis 6. Specifically, a soft magnetic column 7 is fixed in the middle of the yoke of the outer cathode 2, and the soft magnetic One end of the column 7 passes through the center of the inner hole of the anode ring 4 and is connected to the middle part of the inner cathode 1, and the yoke of the outer cathode 2 is provided with two permanent magnets 3, which are symmetrical about the soft magnetic column 7, By adding a permanent magnet 3, two independent magnetic circuits can be formed in the whole ion ...