A high stability CT tube
By using a combined structure of rhenium-tungsten alloy, metal molybdenum and graphite layer on the anode target disc of the CT ball tube, combined with the optimized bearing design and sealing process, the problem of poor heat dissipation ability of the anode target disc at high speed rotation and high temperature is solved. , improves the stability and service life of CT tube.
Patent Information
- Application Number
- CN201811158807.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-09-30
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2038-09-30
AI Technical Summary
The anode target disc of the CT ball tube is difficult to operate stably for a long time under high-speed rotation and high temperature conditions, and has poor heat dissipation ability, resulting in a short service life.
Anode target disk with a combined structure of scattering layer made of rhenium tungsten alloy, a thermal conductivity layer made of metal molybdenum and a heat dissipation layer made of graphite, combined with optimized bearing design and sealing process, improves the heat dissipation ability of the anode target disk and stability.
It effectively improves the working stability and service life of the CT ball tube, ensures that the anode target disc can dissipate heat in time when rotating at high speed, and extends the service life of the equipment.
Smart Images

Figure CN109243948B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a CT tube, in particular to a high-stability CT tube. Background Art
[0002] CT machine is a fully functional disease detection instrument. With the development of technology, CT machine has been popularized with high resolution and intuitive and accurate diagnosis effect, and has been widely used in the medical field. CT tube, also known as X-ray tube, is the core component of CT machine, used to generate X-rays. The technical perfection of CT tube directly affects the working effect of CT machine. X-ray tube mainly includes anode, cathode and glass shell. Anode includes rotor, bearing, fixed sleeve and anode target disk, and cathode includes filament, cathode head and cathode core column. Its working principle is: filament made of tungsten wire can emit a sufficient number of electrons at high temperature as an electron source; under the action of strong electric field formed by high voltage of tens of kilovolts to hundreds of kilovolts between anode and cathode, electrons are accelerated and high-speed electron flow is formed; the role of anode is to attract and accelerate electrons, and make high-speed electrons bombard the target surface of the target disk, and the target surface is bombarded by electrons so that it is sharply blocked to produce X-rays.
[0003] The electrode system of the entire X-ray tube is encapsulated in a high-vacuum glass shell, which is used to support the cathode and anode and provide the vacuum environment necessary for the high-speed electron flight and the normal operation of the high-temperature filament. Since the anode target of the CT tube needs to be hit by high-speed electron flow under high temperature, high-speed rotation and vacuum conditions, cracks usually appear on the target surface of the anode target. At the same time, only 1% of the energy of the high-speed electron flow after bombarding the anode target is converted into X-rays and emitted, and the remaining 99% of the energy is converted into heat or other forms of energy. The current anode target is generally made of rhenium-tungsten alloy as a whole, with poor heat dissipation capacity, unable to dissipate the generated heat in time, making it difficult for the anode target to work stably for a long time and having a short service life. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a high-stability CT tube, which enables the anode target plate to bear greater heat when rotating at high speed and dissipate heat in time, thereby improving the working stability of the CT tube and extending its service life. The technical solution adopted is as follows:
[0005] A high-stability CT tube comprises an anode, a cathode and a glass shell; the cathode is mounted on the top of the inner cavity of the glass shell; the anode comprises a rotor, a rotating shaft, a bearing, an anode kovar and an anode target disk; the anode target disk is in the shape of an inverted disc; the annular inclined surface of the anode target disk in the circumferential direction is the anode target surface; the bearing is mounted on the bottom of the inner cavity of the glass shell through the anode kovar; the rotating shaft is connected to the bearing; the rotor is fixedly connected to the rotating shaft; a center hole is opened in the middle of the anode target disk; the anode target disk is fixedly mounted on the rotor through the center hole; the characteristic is that the anode target disk comprises a scattering layer made of rhenium-tungsten alloy, a heat-conducting layer made of metal molybdenum and a heat-dissipating layer made of graphite; the scattering layer is arranged on the upper surface of the heat-conducting layer; and the heat-dissipating layer is arranged on the lower surface of the heat-conducting layer.
[0006] As a preferred embodiment of the present invention, the inclination angle of the anode target surface is 10° to 15°. The inclination angle of the anode target surface is the angle between the impact surface of the high-speed electron flow (i.e., the target surface of the anode target disk) and the vertical plane of the X-ray tube axis. In theory, the larger the inclination angle of the anode target surface of the anode target disk, the larger the actual focal area and effective focal area of the high-speed electron flow impacting on the anode target surface, thereby reducing the clarity of the obtained image. Therefore, the angle of the anode target surface of the anode target disk is selected to be 10° to 15°. In a specific embodiment, it is further preferred that the inclination angle of the anode target surface is 12°.
[0007] As a preferred embodiment of the present invention, the bearing is an integrated bearing, which includes a bearing sleeve, an inner sleeve, a first ball bearing and a second ball bearing. An inner cavity is provided at the lower part of the rotor; the bearing sleeve is installed at the bottom of the glass shell through the anode; the first ball bearing, the inner sleeve and the second ball bearing are arranged in the bearing sleeve from top to bottom, and the two ends of the inner sleeve are respectively connected to the inner rings of the first ball bearing and the second ball bearing, and the outer rings of the first ball bearing and the second ball bearing are respectively connected to the inner wall of the bearing sleeve; the rotating shaft passes through the first ball bearing, the inner sleeve and the second ball bearing from top to bottom, and the rotating shaft is connected to the inner rings of the first ball bearing and the second ball bearing, and the upper end connecting part of the rotating shaft is exposed outside the first ball bearing; the bearing sleeve extends into the inner cavity of the rotor, and the shoulder shaft of the rotor is fixedly connected to the upper end connecting part of the rotating shaft.
[0008] As a preferred embodiment of the present invention, the cathode includes a tray, a cathode head, a cathode core, a cathode ring, a cathode tube, a cathode kovar and a filament with a lead; the cathode head is installed on one side of the tray, the cathode core is installed on the cathode head, the filament with a lead is installed on the cathode core, and the cathode ring is sleeved on the outside of the cathode head; the cathode tube is installed on the tray and connected to the cathode head, the lower end of the cathode kovar is fixedly installed on the cathode tube, and the upper end of the cathode kovar is connected to the glass shell.
[0009] As a further preferred embodiment of the present invention, the cathode kovar includes a cathode fixed end and a cathode sealing member, the cathode sealing member is fixedly installed in the cathode tube, the lower end of the cathode fixed end extends into the cathode tube and is connected to the cathode sealing member, and the upper end of the cathode fixed end is connected to the glass shell.
[0010] As a further preferred embodiment of the present invention, the leaded filament comprises a first lead, a second lead and a filament, the first end of the filament is connected to the first lead, and the second end of the filament is connected to the second lead; the filament is made of rhenium tungsten wire; the first lead and the second lead both comprise a cathode segment made of molybdenum, a welding segment made of an iron-nickel-cobalt alloy and an outer lead segment made of a copper stranded wire, the cathode segment, the welding segment and the outer lead segment are connected in sequence, the cathode segment is connected to the corresponding end of the filament, the welding segment is welded to the glass shell, and the outer lead segment is outside the glass shell.
[0011] The anode kovar and cathode kovar are generally made of iron-nickel-cobalt alloy, but may also be made of other metal materials.
[0012] As a further preferred embodiment of the present invention, the sealing process of the anode kovar / cathode kovar and the glass housing comprises the following steps:
[0013] (1) Clean the glass rod, glass shell, anode kovar / cathode kovar used for sealing respectively;
[0014] (2) Carry out hydrogen burning treatment on the anode kovar / cathode kovar;
[0015] (3) Winding molten glass around the opening of the anode kovar / cathode kovar: heating the end of a glass rod to a molten state at 550-800°C, and heating the opening of the anode kovar / cathode kovar to a nearly molten state at 750-900°C, and then using the glass rod with the end heated to a molten state to wind a layer of molten glass around the inner and outer edges of the opening of the anode kovar / cathode kovar;
[0016] (4) Butt joint of the anode kovar / cathode kovar with the glass shell: Heat the opening of the glass shell at 500-650℃ until the opening of the glass shell softens, then butt joint the edge of the glass tube opening with the molten glass at the edge of the anode kovar / cathode kovar opening, and then heat at 600-960℃ for 20-30min to fully fuse the glass at the opening of the glass shell and the glass at the anode kovar / cathode kovar opening;
[0017] (5) Sintering annealing: gradually lower the sintering temperature at the opening of the glass shell and the opening of the anode kovar / cathode kovar to room temperature, completing the sealing of the anode kovar / cathode kovar and the glass shell;
[0018] (6) Remove the residual oxide layer on the surface of the anode kovar / cathode kovar opening.
[0019] The above-mentioned treatment to remove the residual oxide layer on the surface of the anode kovar / cathode kovar opening can be carried out by chemical treatment or by manual polishing.
[0020] In the above step (1), anhydrous ethanol is used as a cleaning liquid to clean the inner and outer walls of the glass rod and the glass shell, and acetone is used as a cleaning liquid to clean the inner and outer walls of the anode kovar / cathode kovar. The cleaning removes oxides, grease and dust on the surface of the glass rod, the glass shell and the anode kovar / cathode kovar.
[0021] In the above step (2), the hydrogen burning treatment is to place the anode kovar / cathode kovar in a hydrogen furnace and calcine it with hydrogen, and then anneal it under the condition of continuous input of hydrogen. The entire calcination and annealing process of the anode kovar / cathode kovar in the hydrogen furnace is carried out under the protection of hydrogen flow, which is beneficial to the decarburization of the surface layer of the anode kovar / cathode kovar. Due to the diffusion of hydrogen atoms at high temperature, hydrogen replaces other gases inside the anode kovar / cathode kovar, plays the role of exhaust, so that the sealing position is firmly bonded and has good airtightness.
[0022] Compared with the prior art, the present invention has the following advantages:
[0023] This high-stability CT tube, because the anode target plate adopts a structure composed of a scattering layer, a thermal conductive layer and a heat dissipation layer, can not only withstand the impact of high-speed electron flow, but also quickly dissipate heat, thereby improving the working stability of the CT tube and extending its service life. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a structural schematic diagram of a preferred embodiment of the present invention;
[0025] Figure 2 is a schematic diagram of the structure of the anode;
[0026] Figure 3 is a schematic diagram of the cathode structure;
[0027] Figure 4 yes Figure 3 Section along AA;
[0028] Figure 5 It is a schematic diagram of the structure of a filament with leads;
[0029] Figure 6 is a schematic diagram of the structure of the first lead and the second lead;
[0030] Figure 7 It is a schematic diagram of anode Kovar / cathode Kovar winding molten glass;
[0031] Figure 8It is a schematic diagram of the connection between the anode kovar / cathode kovar and the opening of the glass shell;
[0032] Fig. 9 It is a schematic diagram of annealing after sealing. DETAILED DESCRIPTION
[0033] The following is a further description of the preferred embodiments of the present invention in conjunction with the accompanying drawings.
[0034] like Figure 1 As shown, this high stability CT tube includes an anode 1, a cathode 2 and a glass shell 3; the cathode 2 is installed on the top of the inner cavity of the glass shell 3; Figure 2 As shown, the anode 1 includes a rotor 101, a rotating shaft 102, a bearing 103, an anode kovar 104 and an anode target plate 105. The anode target plate 105 is in the shape of an inverted disc. The annular inclined surface of the anode target plate 105 in the circumferential direction is an anode target surface 1051. The inclination angle of the anode target surface 1051 is 12° (10° to 15° is also possible). The bearing 103 is installed at the bottom of the inner cavity of the glass shell 3 through the anode kovar 104. The rotating shaft 102 is connected to the bearing 103. The rotor 101 The anode target plate 105 is fixedly connected to the rotating shaft 102, and a center hole 1052 is opened in the middle of the anode target plate 105. The anode target plate 105 is fixedly installed on the rotor 102 through the center hole 1052; the anode target plate 105 includes a scattering layer 1053 made of rhenium-tungsten alloy, a heat-conducting layer 1054 made of metal molybdenum and a heat-dissipating layer 1055 made of graphite, the scattering layer 1053 is arranged on the upper surface of the heat-conducting layer 1054, and the heat-dissipating layer 1055 is arranged on the lower surface of the heat-conducting layer 1054.
[0035] like Figure 2 As shown, the bearing 103 is an integrated bearing, which includes a bearing sleeve 1031, an inner sleeve 1032, a first ball bearing 1033 and a second ball bearing 1034. The lower part of the rotor 101 is provided with an inner cavity 1011; the bearing sleeve 1031 is installed at the bottom of the glass shell 3 through the anode 104; the first ball bearing 1033, the inner sleeve 1032 and the second ball bearing 1034 are arranged in the bearing sleeve 1031 from top to bottom, and the two ends of the inner sleeve 1032 are respectively connected to the inner rings of the first ball bearing 1033 and the second ball bearing 1034. The outer rings of the bearing 1033 and the second ball bearing 1034 are respectively connected to the inner wall of the bearing sleeve 1031; the rotating shaft 102 passes through the first ball bearing 1033, the inner sleeve 1032, and the second ball bearing 1034 from top to bottom, and the rotating shaft 102 is connected to the inner rings of the first ball bearing 1033 and the second ball bearing 1034, and the upper end connecting portion 1021 of the rotating shaft 102 is exposed outside the first ball bearing 1033; the bearing sleeve 1031 extends into the inner cavity 1011 of the rotor 101, and the shoulder shaft 1012 of the rotor 101 is fixedly connected to the upper end connecting portion 1021 of the rotating shaft 102.
[0036] like Figure 3 , Figure 4 As shown, the cathode 2 comprises a tray 201, a cathode head 202, a cathode core 203, a cathode ring 204, a cathode cylinder 205, a cathode ferrule 206 and a filament with a lead 207 (hidden in the cathode core 203, see Figure 5 ); the cathode head 202 is mounted on one side of the tray 201, the cathode core 203 is mounted on the cathode head 202, the lead filament 207 is mounted on the cathode core 203, and the cathode ring 204 is sleeved on the outside of the cathode head 202; the cathode cylinder 205 is mounted on the tray 201 and connected to the cathode head 202, the lower end of the cathode kovar 206 is fixedly mounted on the cathode cylinder 205, and the upper end of the cathode kovar 206 is connected to the glass shell 3. Among them, the cathode kovar 206 includes a cathode fixed end 2061 and a cathode sealing member 2062, the cathode sealing member 2062 is fixedly mounted in the cathode cylinder 205, the lower end of the cathode fixed end 2061 extends into the cathode cylinder 205 and is connected to the cathode sealing member 2062, and the upper end of the cathode fixed end 2061 is connected to the glass shell 3.
[0037] like Figure 5 , Figure 6 As shown, the leaded filament 207 comprises a first lead 2071, a second lead 2072 and a filament 2073. The first end of the filament 2073 is connected to the first lead 2071, and the second end of the filament 2073 is connected to the second lead 2072. The diameter of the filament 2073 is 0.22 mm. The filament 2073 is a spiral filament, and the core shaft diameter of the spiral filament 2073 is 1.20 mm. The filament 2073 is made of rhenium tungsten wire. 2071 and the second lead 2072 each include a cathode segment 20711 made of molybdenum, a welding segment 20712 made of an iron-nickel-cobalt alloy, and an outer lead segment 20713 made of a copper stranded wire. The cathode segment 20711, the welding segment 20712, and the outer lead segment 20713 are connected in sequence. The cathode segment 20711 is connected to the corresponding end of the filament 2073, the welding segment 20712 is connected (welded) to the glass shell 3, and the outer lead segment 20713 is outside the glass shell 3.
[0038] The anode kovar 104 and the cathode kovar 206 are generally circular sealing connectors, which are generally made of iron-nickel-cobalt alloy, and other metal materials may also be used.
[0039] The anode target disk 105 is set to a structure composed of a scattering layer 1053, a heat-conducting layer 1054 and a heat-dissipating layer 1055, wherein the scattering layer 1053 is made of a rhenium-tungsten alloy, which has high hardness and high stability and strength at high temperatures, so that the scattering layer 1053 can withstand the impact of high-speed electron flow multiple times under the conditions of high temperature, high vacuum and high-speed rotation; the heat-conducting layer 1054 is made of metal molybdenum, which has a high melting point, high hardness, small expansion coefficient, good thermal conductivity, and good plasticity at high temperatures. By using metal molybdenum as the heat-conducting layer 1054 of the anode target disk 105, the heat absorbed by the scattering layer 1053 can be effectively transferred to the heat-dissipating layer 1055, and deformation is not likely to occur; the heat-dissipating layer 1055 is made of graphite, which is resistant to high temperatures and has good thermal conductivity, and can quickly dissipate the heat of the anode target disk 105, and no cracks will be generated when it is cooled after use in a high-temperature environment.
[0040] In addition, by providing an inner cavity 1011 on the rotor 101, that is, hollowing out the lower part of the rotor 101, and then extending the integrated bearing 103 into the inner cavity 1011 of the rotor 101, the height of the anode target plate 105 is greatly reduced, almost just the height of the rotor 101, so that the center of gravity of the anode target plate 105 is greatly reduced, and its high-speed rotation stability is improved; on the other hand, the fixed sleeve and bearing in the prior art are replaced with the integrated bearing 103, and the first ball bearing 1033, the inner sleeve 1032, the second ball bearing 1034 are connected to the rotating shaft 102, so that the rotating shaft 102 is limited, and the limited length of the rotating shaft 102 is greatly increased, and the vibration of the rotating shaft 102 during high-speed rotation is avoided, so that the anode target plate 105 has a higher rotation speed and stability, and the imaging quality is improved.
[0041] In addition, by setting the cathode kovar 206 as a cathode fixed end 2061 and a cathode sealing member 2062, wherein the cathode sealing member 2062 is directly set to the middle and lower part of the cathode tube 205, a better sealed connection is achieved, and the cathode fixed end 2061 used for welding with the glass shell 3 can be made wider, thereby increasing the connection area between the cathode kovar 206 and the glass shell 3 and improving the structural stability; and because the cathode kovar 206 extends into the interior of the cathode tube 205, the center of gravity of the cathode 2 moves up after the connection, closer to the connection between the cathode kovar 206 and the glass shell 3, so that the moment of the center of gravity of the cathode 2 becomes smaller, avoiding excessive moment causing cracks or even ruptures at the connection between the cathode kovar 206 and the glass shell 3, thereby further improving the structural stability and extending the service life.
[0042] In addition, the filament 2073 made of rhenium tungsten wire is used as the cathode. The rhenium tungsten wire is an alloy material made of rhenium and tungsten. It can emit a sufficient number of electrons at high temperatures and serve as an electron source. The rhenium tungsten wire has a high resistivity, good surface oxidation resistance, higher plasticity at low temperatures, is easy to manufacture and shape, has good processing performance and weldability, and has high stability and strength at high temperatures. After long-term use and cooling, the material will not become brittle. The first lead 2071 and the second lead 2072 are divided into a cathode section 20711, a welding section 20712 and an outer lead section 20713. The cathode section 20711 is made of molybdenum, so that the cathode section 20711 has the characteristics of high temperature resistance, making it suitable for connection with the corresponding end of the filament 2073; the welding section 20712 is made of iron-nickel-cobalt alloy, so that the welding section 20712 has the strength and hardness of glass. After being connected (welded) to the glass shell 3, it is not easy to be rotated and twisted by external forces, thereby avoiding damage. The original sealing interface avoids the X-ray tube from leaking and failing; the expansion coefficient of the material of the welding section 20712 is close to that of the glass. After being connected (welded) to the glass shell 3, it can avoid glass cracks or breakages caused by temperature changes in the glass shell 3, so as to achieve the purpose of improving the vacuum degree; the outer lead section 20713 is made of copper stranded wire, so that the outer lead section 20713 has good electrical conductivity and is located outside the glass shell 3 to connect the filament power supply; thereby further improving the adaptability of the lead part of the filament in a high temperature environment.
[0043] The sealing process of the anode kovar / cathode kovar and the glass shell comprises the following steps:
[0044] (1) Cleaning the glass rod, glass shell 3, anode Kovar 104 / cathode Kovar 206 used for sealing respectively;
[0045] (2) Carry out hydrogen burning treatment on the anode Kovar 104 / cathode Kovar 206;
[0046] (3) If Figure 7 As shown, the opening of the anode kovar 104 / cathode kovar 206 is wound with molten glass 100: the end of the glass rod is heated to a molten state at 550-800° C., and the opening of the anode kovar 104 / cathode kovar 206 is heated to a nearly molten state at 750-900° C., and then a layer of molten glass 100 is wound around the inner and outer edges of the opening of the anode kovar 104 / cathode kovar 206 using the glass rod whose end is heated to a molten state;
[0047] (4) If Figure 8As shown, the anode kovar 104 / cathode kovar 206 is butted with the glass shell 3: the opening of the glass shell 3 is heated at 500-650°C until the opening of the glass shell 3 is softened, and then the edge of the opening of the glass shell 3 is butted with the molten glass at the edge of the opening of the anode kovar 104 / cathode kovar 206, and then heated at 600-960°C for 20-30 minutes to fully melt the glass 100 at the opening of the glass shell 3 and the opening of the anode kovar 104 / cathode kovar 206;
[0048] (5) Fig. 9 As shown, sintering annealing: gradually lowering the sintering temperature at the opening of the glass shell 3 and the opening of the anode kovar 104 / cathode kovar 206 to room temperature, completing the sealing of the anode kovar 104 / cathode kovar 206 and the glass shell 3;
[0049] (6) Remove the oxide layer remaining on the surface of the anode Kovar 104 / cathode Kovar 206 opening.
[0050] The above-mentioned sealing process firstly wraps molten glass 100 around the inner and outer edges of the opening of the anode kovar 104 / cathode kovar 206, and then seals the anode kovar 104 / cathode kovar 206 and the glass shell 3 together by connecting and fusing the glass of the opening of the anode kovar 104 / cathode kovar 206 through the glass shell 3, effectively reducing the difficulty of sealing the anode kovar 104 / cathode kovar 206 and the glass shell 3. At the same time, the sealing part of the anode kovar 104 / cathode kovar 206 and the glass shell 3 is smooth and integrated, with high degree of fusion and strength, thereby effectively improving the service life of the CT tube; in addition, before sealing, the anode kovar 104 / cathode kovar 206 is subjected to hydrogen burning treatment to decarbonize the surface of the anode kovar 104 / cathode kovar 206, thereby avoiding the generation of black at the sealing position during subsequent high-temperature sealing. points and destroy the overall firmness and sealing; when the inner and outer edges of the opening of the anode kovar 104 / cathode kovar 206 are wrapped around the glass 100, the opening of the anode kovar 104 / cathode kovar 206 is heated to a state close to the molten state (the state close to the molten state is a transitional state between the solid and the molten state). In this state, the formation of an oxide layer at this position can be avoided, and the metal atoms at this position are made quite active, which can penetrate each other with the molten glass 100, and the anode kovar 104 / cathode kovar 206 is easier to combine with the molten glass, and the combination is tighter after annealing, further improving the firmness and sealing after sealing; and after the sealing is completed, the oxide layer remaining on the surface of the opening of the anode kovar 104 / cathode kovar 206 is removed to avoid the glass at the sealing position being peeled off due to the shedding of the oxide layer.
[0051] In the above step (1), anhydrous ethanol is used as a cleaning liquid to clean the inner and outer walls of the glass rod and the glass shell 3, and acetone is used as a cleaning liquid to clean the inner and outer walls of the anode kovar 104 / cathode kovar 206. The cleaning removes oxides, grease and dust on the surfaces of the glass rod, the glass shell 3 and the anode kovar 104 / cathode kovar 206.
[0052] In the above step (2), the hydrogen burning treatment is to place the anode kovar 104 / cathode kovar 206 in a hydrogen furnace and calcine it with hydrogen, and then perform annealing treatment under the condition of continuous input of hydrogen. The entire calcination and annealing process of the anode kovar 104 / cathode kovar 206 in the hydrogen furnace is carried out under the protection of hydrogen flow, which is beneficial to the decarburization of the surface layer of the anode kovar 104 / cathode kovar 206. Due to the diffusion of hydrogen atoms at high temperature, hydrogen replaces other gases inside the anode kovar 104 / cathode kovar 206, plays the role of exhaust, so that the sealing position is firmly bonded and has good airtightness.
[0053] In addition, it should be noted that the names of the various parts of the specific embodiments described in this specification may be different, and any equivalent or simple changes made based on the structure, features and principles described in the patent concept of the present invention are included in the protection scope of the patent of the present invention. The technicians in the technical field of the present invention can make various modifications or supplements to the specific embodiments described or replace them in a similar manner, as long as they do not deviate from the structure of the present invention or exceed the scope defined by the claims, they should all fall within the protection scope of the present invention.
Claims
1. A high-stability CT tube, comprising an anode, a cathode and a glass shell; the cathode is mounted on the top of the inner cavity of the glass shell; the anode comprises a rotor, a rotating shaft, a bearing, an anode kovar and an anode target disk, the anode target disk is an inverted disc, the annular inclined surface of the anode target disk in the circumferential direction is the anode target surface, the inclination angle of the anode target surface is 10° to 15°, the bearing is mounted on the bottom of the inner cavity of the glass shell through the anode kovar, the rotating shaft is connected to the bearing, the rotor is fixedly connected to the rotating shaft, a center hole is opened in the middle of the anode target disk, and the anode target disk is fixedly mounted on the rotor through the center hole; the characteristics are: The anode target plate includes a scattering layer made of rhenium-tungsten alloy, a heat-conducting layer made of metal molybdenum and a heat-dissipating layer made of graphite, the scattering layer is arranged on the upper surface of the heat-conducting layer, and the heat-dissipating layer is arranged on the lower surface of the heat-conducting layer; the cathode includes a tray, a cathode head, a cathode core, a cathode ring, a cathode tube, a cathode kovar and a filament with a lead; the cathode head is installed on one side of the tray, the cathode core is installed on the cathode head, the filament with a lead is installed on the cathode core, and the cathode ring is sleeved on the outside of the cathode head; the cathode tube is installed on the tray and connected to the cathode head, and the lower end of the cathode kovar is fixedly installed Installed on the cathode tube, the upper end of the cathode is connected to the glass shell; the lead filament includes a first lead, a second lead and a filament, the first end of the filament is connected to the first lead, and the second end of the filament is connected to the second lead; the filament is made of rhenium tungsten wire; the first lead and the second lead both include a cathode segment made of molybdenum, a welding segment made of iron-nickel-cobalt alloy and an outer lead segment made of copper stranded wire, the cathode segment, the welding segment and the outer lead segment are connected in sequence, the cathode segment is connected to the corresponding end of the filament, the welding segment is welded to the glass shell, and the outer lead segment is outside the glass shell.
2. The high stability CT tube according to claim 1, characterized in that: The bearing is an integrated bearing, which includes a bearing sleeve, an inner sleeve, a first ball bearing and a second ball bearing. An inner cavity is provided at the lower part of the rotor; the bearing sleeve is installed at the bottom of the glass shell through the anode; the first ball bearing, the inner sleeve and the second ball bearing are arranged in the bearing sleeve from top to bottom, and the two ends of the inner sleeve are respectively connected to the inner rings of the first ball bearing and the second ball bearing, and the outer rings of the first ball bearing and the second ball bearing are respectively connected to the inner wall of the bearing sleeve; the rotating shaft passes through the first ball bearing, the inner sleeve and the second ball bearing from top to bottom, and the rotating shaft is connected to the inner rings of the first ball bearing and the second ball bearing, and the upper end connecting part of the rotating shaft is exposed outside the first ball bearing; the bearing sleeve extends into the inner cavity of the rotor, and the shoulder shaft of the rotor is fixedly connected to the upper end connecting part of the rotating shaft.
3. The high stability CT tube according to claim 1, characterized in that: The cathode kovar comprises a cathode fixing end and a cathode sealing member, the cathode sealing member is fixedly installed in the cathode tube, the lower end of the cathode fixing end extends into the cathode tube and is connected to the cathode sealing member, and the upper end of the cathode fixing end is connected to the glass shell.
4. The high stability CT tube according to claim 1, characterized in that: The sealing process of the anode kovar / cathode kovar and the glass shell comprises the following steps: (1) Clean the glass rod, glass shell, anode kovar / cathode kovar used for sealing respectively; (2) Perform hydrogen burning treatment on the anode kovar / cathode kovar; (3) Winding molten glass around the opening of the anode kovar / cathode kovar: heating the end of a glass rod to a molten state at 550-800°C, and heating the opening of the anode kovar / cathode kovar to a nearly molten state at 750-900°C, and then using the glass rod with the end heated to a molten state to wind a layer of molten glass around the inner and outer edges of the opening of the anode kovar / cathode kovar; (4) Butt joint of the anode kovar / cathode kovar and the glass shell: Heat the opening of the glass shell at 500-650℃ until the opening of the glass shell softens, then butt joint the edge of the opening of the glass shell with the molten glass at the edge of the opening of the anode kovar / cathode kovar, and then heat at 600-960℃ for 20-30min to fully fuse the glass of the opening of the glass shell and the glass of the opening of the anode kovar / cathode kovar; (5) Sintering annealing: gradually lower the sintering temperature at the opening of the glass shell and the opening of the anode kovar / cathode kovar to room temperature, completing the sealing of the anode kovar / cathode kovar and the glass shell; (6) Remove the residual oxide layer on the surface of the anode kovar / cathode kovar opening.