Combined welding method and combined welding device
The heat generated by the welding gun and the negative electrode sheet melts the tin wire, and is evenly distributed between the pole and terminal by using the wire feeding device, solving the problem that the tin wire cannot be evenly covered and improving the welding strength and stability.
Patent Information
- Application Number
- CN201910091805.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-01-30
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2039-01-30
AI Technical Summary
In battery production, during the welding process of the pole column and terminal, the melted tin wire cannot evenly cover the upper and lower end surfaces of the terminal, affecting the assembly performance.
Using a combined welding method and device, the current between the welding gun and the negative electrode sheet generates heat, melts the tin wire, and continuously replenishes the tin wire through the wire feeding device, so that the molten tin liquid can flow to the upper and lower end surfaces of the terminal, and as the Over time, melt the pole column to ensure that tin liquid is fixed on both sides of the terminal.
The firm connection between the pole column and the terminal is achieved, the connection strength is enhanced, the problem of poor welding is avoided, and the tin distribution is ensured on both sides of the terminal.
Smart Images

Figure CN109623063B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of welding equipment, and in particular to a combined welding method and a combined welding device. Background Art
[0002] In the production of storage batteries, the pole 3 (made of lead, vertically fixed in the battery box 2) and the terminal 1 (i.e., the silver-plated copper sheet) need to be welded together. Before welding the two together, as shown in the attached Figure 1 As shown, during the assembly process of the battery box 2 and the pole 3, the portion of the pole 2 exposed outside the battery box 2 is relatively long. When the terminal 1 is fitted onto the pole 3, a portion of the pole 3 is located above the terminal 1 (relative to the attached Figure 1 In order to ensure that the pole 3 and the terminal 1 can be welded together, the portion of the pole 3 located above the terminal 1 needs to be cut off before welding, and then the terminal 1 and the pole 3 are welded together with a soldering iron tin wire. In the above welding process, the melted tin wire can only cover the upper end surface of the terminal 1, while the lower end surface of the terminal 1 (i.e., the side that fits the battery box 2) cannot be covered by the melted tin wire, which will seriously affect the performance of the battery after assembly. Summary of the invention
[0003] In view of the above problems, the present invention provides a combined welding method and a combined welding device.
[0004] The technical solution adopted by the present invention is as follows:
[0005] A combined welding method comprises the following steps:
[0006] S1: Place the tin wire in the heating area between the welding gun and the negative electrode;
[0007] S2: Power on the welding gun and the negative electrode sheet, and use the heat generated by the current between the welding gun and the negative electrode sheet to melt the tin wire;
[0008] S3: While the tin wire is melting, continuously add tin wire to the heating point between the welding gun and the negative electrode sheet.
[0009] In this welding method, one of the welding gun and the negative electrode is connected to the positive electrode of the power supply, and the other is connected to the negative electrode of the power supply (there is no strict requirement for which one is connected to the positive electrode of the power supply, as long as the welding gun and the negative electrode can generate current), so that the current between the welding gun and the negative electrode will generate a lot of heat. When this method is used to make batteries, the melting point of tin is 231.89 degrees Celsius, and the melting point of lead is 327.502 degrees Celsius, so during the welding process, the tin wire will melt before the pole, and the molten liquid tin will be spread between the pole and the terminal (so that the upper and lower end surfaces of the terminal will be distributed with tin liquid), and as time goes by, the pole will also melt. When the pole melts, stop energizing the welding gun and the negative electrode, and the entire welding process is completed after the lead and tin solidify.
[0010] In the above welding method, the heat generated by the electric current first melts the tin wire, allowing the molten tin liquid to flow to the upper and lower end faces of the terminal, and then the heat is used to melt the pole. After the lead and tin are solidified, the pole and the terminal can be firmly fixed together, and tin is distributed on the upper and lower sides of the terminal.
[0011] At the same time, since the terminal and the pole are melted together, the connection strength between the pole and the terminal is stronger and less likely to fall off.
[0012] A combined welding device comprises a bracket, a wire feeding device, a welding gun and a negative electrode sheet, wherein the wire feeding device is directly or indirectly fixed to the bracket, the welding gun is directly or indirectly fixed to the bracket, and the negative electrode sheet is directly or indirectly fixed to the bracket. The wire feeding device is used to transport tin wire to a heat generating area between the welding gun and the negative electrode sheet, and the welding gun and the negative electrode sheet are used together to melt the tin wire.
[0013] The welding device is suitable for the above welding method. The welding gun can be connected to the positive electrode of the power supply, and the negative electrode sheet is connected to the negative electrode of the power supply. The shapes of the welding gun and the negative electrode sheet can be consistent or inconsistent.
[0014] Optionally, the welding gun is a tubular welding gun, and the wire feeding device is used to feed the tin wire to the bottom of the welding gun.
[0015] The cylindrical welding gun is used to melt the tin wire in the cylindrical welding gun, and then the molten tin liquid drips along the cylindrical welding gun to between the pole and the terminal. The use of the cylindrical welding gun can ensure that the wire feeding device is smoother when conveying the tin wire, and the melted tin wire can slide along the cylindrical welding gun to between the pole and the terminal.
[0016] Optionally, it also includes a first motion mechanism, which is slidably mounted on the bracket, and the welding gun and the negative electrode plate are both mounted on the first motion mechanism, and the first motion mechanism is used to drive the welding gun and the negative electrode plate to move longitudinally and transversely.
[0017] The above structure can be used to adjust the position of the welding gun and the negative electrode sheet on the bracket at any time, so as to better adapt to the welding operation. Since the position of the welding gun and the negative electrode sheet can be adjusted, it can be ensured that the welding gun and the negative electrode sheet can adapt to various welding tasks. The longitudinal movement and the lateral movement here are relative to the position of the slide rail.
[0018] Optionally, the first motion mechanism includes a sliding seat, a mounting seat and a motion rod, the sliding seat is slidably mounted on the bracket, the welding gun and the negative electrode plate are both mounted on the mounting seat, the motion rod is mounted on the sliding seat, the mounting seat is fixedly mounted on the motion rod, and the motion rod is used to drive the mounting seat to move toward or away from the sliding seat.
[0019] Optionally, a slide rail is provided on the bracket, the sliding seat is slidably installed on the slide rail, the moving rod is a screw rod, the moving rod and the sliding seat are matched together through threaded matching, and the moving rod is always perpendicular to the sliding direction of the sliding seat, and the mounting seat is fixed to one end of the moving rod.
[0020] The sliding fit between the sliding seat and the slide rail on the bracket can ensure that the welding gun and the negative electrode sheet can move parallel to the slide rail, and the threaded fit between the moving rod and the sliding seat can ensure that the welding gun and the negative electrode sheet can move perpendicular to the slide rail. The specific position of the sliding seat on the slide rail can be adjusted by setting a motor or manually, and the position relationship between the moving rod and the sliding seat can be adjusted manually or by setting a motor.
[0021] Optionally, the wire feeding device includes a first clamping seat, a first power device, a second clamping seat, a second power device, a third power device and a base, the first power device is installed on the first clamping seat, the second power device is installed on the second clamping seat, the first clamping seat is fixedly installed on the base, the second clamping seat is slidably installed on the base, the third power device is fixedly installed on the base, and the third power device is used to drive the second clamping seat to move on the base; the first clamping seat and the first power device are used together to clamp the tin wire, and the second clamping seat and the second power device are used together to clamp the tin wire from the first clamping seat to the welding gun.
[0022] The working steps of the wire feeding device are as follows: first, the second clamping seat is located in the first working position (i.e., close to one end of the first clamping seat), and the first clamping seat and the first power device are in a loosened state, then the second power device works, and the second power device and the second clamping seat work together to clamp the tin wire, and then the third power device drives the second clamping seat to move to the second working position (i.e., away from the side of the second clamping seat). When the second clamping seat moves to the second working position, the second power device releases the cooperation with the second clamping seat (i.e., no longer clamps the tin wire); then the first power device cooperates with the first clamping seat to clamp the tin wire, and the third power device drives the second clamping seat to move from the second working position to the first working position, waiting for material collection. In this process, the tin wire is clamped by the second clamping seat and the second power device and moves toward the welding gun. The above process is repeated continuously, and the tin wire is continuously added to the welding gun.
[0023] Optionally, the first power device is a first cylinder, and the second power device is a second cylinder. A clamp is installed on each of the first cylinder and the second cylinder. The first cylinder is used to drive the clamp and the first clamp seat to clamp the tin wire together, and the second cylinder is used to drive the clamp and the second clamp seat to clamp the tin wire together.
[0024] The purpose of setting the splint is to better clamp the tin wire.
[0025] Optionally, a sliding rod is provided on the base, a sleeve is provided on the second clamping seat, the second clamping seat is slidably mounted on the sliding rod through the sleeve, the third power device is a third cylinder, the third cylinder is fixedly mounted on the base, and one end of the third cylinder is fixed to the second clamping seat.
[0026] Optionally, the negative electrode sheet is a tubular, columnar or plate-shaped negative electrode sheet.
[0027] The device uses the heat generated by the argon arc welding current to replace the electric soldering iron to melt the tin wire, combines the argon arc welding with the soldering iron tin wire welding, and has a better welding effect.
[0028] The beneficial effect of the present invention is that the heat generated by the electric current first melts the tin wire, so that the molten tin liquid can flow to the upper and lower end faces of the terminal, and then the heat is used to melt the pole. After the lead and tin are solidified, the pole and the terminal can be firmly fixed together, and tin is distributed on the upper and lower sides of the terminal. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is the matching relationship diagram between the pole and the terminal;
[0030] Figure 2 It is a schematic diagram of the structure of the combined welding device;
[0031] Figure 3It is a schematic diagram of the structure of the wire feeding device;
[0032] Figure 4 It is a schematic diagram of the position relationship between the welding gun and the negative electrode sheet;
[0033] Figure 5 Schematic diagram of the installation position relationship of the motion rod.
[0034] The reference numerals in the figure are: 1. terminal, 2. battery box, 3. pole, 4. bracket, 401. slide rail, 5. wire feeding device, 501. base, 5101. first cylinder, 5102. second cylinder, 5103. third cylinder, 5201. first clamping seat, 5202. second clamping seat, 503. clamping plate, 504. sleeve, 505. slide rod, 506. wire unwinding rack, 6. battery positioning device, 7. terminal detection device, 8. welding gun, 9. negative electrode sheet, 10. mounting seat, 11. sliding seat, 1101. adjusting disk, 12. motor, 13. moving rod. DETAILED DESCRIPTION
[0035] The present invention is described in detail below in conjunction with the accompanying drawings.
[0036] The present invention provides a combined welding device, as shown in the attached Figure 2 , Attachment Figure 3 , Attachment Figure 4 And attached Figure 5 As shown, it includes a bracket 4, a wire feeding device 5, a welding gun 8 and a negative electrode sheet 9. The wire feeding device 5 is directly or indirectly fixed to the bracket 4, the welding gun 8 is directly or indirectly fixed to the bracket 4, and the negative electrode sheet 9 is directly or indirectly fixed to the bracket 4. The wire feeding device 5 is used to transport the tin wire to the heat generating area between the welding gun 8 and the negative electrode sheet 9, and the welding gun 8 and the negative electrode sheet 9 are used together to melt the tin wire.
[0037] As attached Figure 2 As shown, a battery positioning device 6 and a terminal detection device 7 are provided on the slide rail 401 on the bracket 1. The battery positioning device 6 is used to clamp the battery, and the terminal detection device 7 is used to detect the battery after welding.
[0038] The welding device is suitable for a combined welding method. The welding gun 8 can be connected to the positive electrode of the power supply, and the negative electrode sheet 9 is connected to the negative electrode of the power supply. The shapes of the welding gun 8 and the negative electrode sheet 9 can be consistent or inconsistent.
[0039] As attached Figure 2 As shown, two slide rails 401 are provided on the bracket 4, and the slide rail 401 installed on the terminal detection device 7 and the battery positioning device 6 is not the same slide rail 401 as the slide rail 401 installed on the sliding seat 11 and the base 501.
[0040] As attached Figure 2 , Attachment Figure 4And attached Figure 5 As shown, the welding gun 8 is a tubular welding gun 8 , and the wire feeding device 5 is used to feed the tin wire to the bottom of the welding gun 8 .
[0041] The cylindrical welding gun 8 is used so that the tin wire is melted in the cylindrical welding gun 8, and then the melted tin liquid drips between the pole and the terminal along the cylindrical welding gun 8. The use of the cylindrical welding gun 8 can ensure that the wire feeding device 5 is smoother when conveying the tin wire, and the melted tin wire can slide smoothly along the cylindrical welding gun 8 to between the pole and the terminal.
[0042] As attached Figure 2 , Attachment Figure 4 And attached Figure 5 As shown, it also includes a first motion mechanism, which is slidably mounted on the bracket 4, and the welding gun 8 and the negative electrode sheet 9 are both mounted on the first motion mechanism. The first motion mechanism is used to drive the welding gun 8 and the negative electrode sheet 9 to move longitudinally and transversely.
[0043] The above structure can be used to adjust the position of the welding gun 8 and the negative electrode sheet 9 on the bracket 4 at any time, so as to better adapt to the welding operation. Since the position of the welding gun 8 and the negative electrode sheet 9 can be adjusted, it can be ensured that the welding gun 8 and the negative electrode sheet 9 can adapt to various welding tasks. The longitudinal movement and the lateral movement here are relative to the position of the slide rail 401.
[0044] As attached Figure 2 , Attachment Figure 4 And attached Figure 5 As shown, the first motion mechanism includes a sliding seat 11, a mounting seat 10 and a motion rod 13. The sliding seat 11 is slidably mounted on the bracket 4, the welding gun 8 and the negative electrode plate 9 are both mounted on the mounting seat 10, the motion rod 13 is mounted on the sliding seat 11, and the mounting seat 10 is fixedly mounted on the motion rod 13. The motion rod 13 is used to drive the mounting seat 10 to move toward or away from the sliding seat 11.
[0045] As attached Figure 2 , Attachment Figure 4 And attached Figure 5 As shown, a slide rail 401 is provided on the bracket 4, and the sliding seat 11 is slidably installed on the slide rail 401. The moving rod 13 is a screw rod. The moving rod 13 and the sliding seat 11 are matched together through threaded matching, and the moving rod 13 is always perpendicular to the sliding direction of the sliding seat 11. The mounting seat 10 is fixed to one end of the moving rod 13.
[0046] The sliding cooperation between the sliding seat 11 and the slide rail 401 on the bracket 4 can ensure that the welding gun 8 and the negative electrode sheet 9 can move relative to and parallel to the slide rail 401. The threaded cooperation between the moving rod 13 and the sliding seat 11 can ensure that the welding gun 8 and the negative electrode sheet 9 can move perpendicular to the slide rail 401. Specifically, the position of the sliding seat 11 on the slide rail 401 can be adjusted by setting a motor 12 or manually, and the position relationship between the moving rod 13 and the sliding seat 11 can be adjusted manually or by setting a motor 12.
[0047] As attached Figure 4 And attached Figure 5 As shown, the sliding seat 11 is provided with an adjustment disk 1101, and when the adjustment disk 1101 is manually rotated, the sliding seat 11 will move on the slide rail 401. Specifically, the sliding seat is provided with a wheel (the wheel and the adjustment disk are meshed together through a gear or other structure, and the wheel rotates when the adjustment disk 1101 is rotated), and the wheel cooperates with the slide rail 401. When the adjustment disk 1101 rotates, the wheel on the sliding seat 11 rolls on the slide rail 401, so that the sliding seat 11 moves on the slide rail 401.
[0048] As attached Figure 2 And attached Figure 3 As shown, the wire feeding device 5 includes a first clamping seat 5201, a first power device, a second clamping seat 5202, a second power device, a third power device and a base 501. The first power device is installed on the first clamping seat 5201, and the second power device is installed on the second clamping seat 5202. The first clamping seat 5201 is fixedly installed on the base 501, and the second clamping seat 5202 is slidably installed on the base 501. The third power device is fixedly installed on the base 501, and the third power device is used to drive the second clamping seat 5202 to move on the base 501; the first clamping seat 5201 and the first power device are used together to clamp the tin wire, and the second clamping seat 5202 and the second power device are used together to clamp the tin wire from the first clamping seat 5201 to the welding gun 8.
[0049] The working steps of the wire feeding device 5 are as follows: first, the second clamping seat 5202 is located at the first working position (i.e., close to one end of the first clamping seat 5201), and the first clamping seat 5201 and the first power device are in a loose state, then the second power device works, and the second power device and the second clamping seat 5202 work together to clamp the tin wire, and then the third power device drives the second clamping seat 5202 to move to the second working position (i.e., away from the side of the second clamping seat), and when the second clamping seat 5202 moves to the second working position, the second power device releases the cooperation with the second clamping seat 5202 (i.e., no longer clamps the tin wire); then the first power device and the first clamping seat 5201 cooperate to clamp the tin wire, and the third power device drives the second clamping seat 5202 to move from the second working position to the first working position, waiting for material collection. In this process, the tin wire is clamped by the second clamping seat 5202 and the second power device and moves toward the welding gun. The above process is continuously repeated, and the tin wire is continuously added to the welding gun.
[0050] First, the second clamping seat 5202 is located at the first working position (i.e., away from one end of the first clamping seat 5201), and the second clamping seat 5202 and the second power device are in a loose state, then the first power device works, the first power device and the first clamping seat 5201 work together to clamp the tin wire, and then the third power device drives the second clamping seat 5202 to move to the second working position (i.e., close to the side of the second clamping seat 5202), when the second clamping seat 5202 moves to the second working position, the first power device releases the cooperation with the first clamping seat 5201 (i.e., no longer clamps the tin wire); then the second power device and the second clamping seat 5202 cooperate to clamp the tin wire, and the third power device drives the second clamping seat 5202 to move from the first working position to the second working position, during which the tin wire is clamped by the second clamping seat 5202 and the second power device and moves toward the welding gun 8. The above process is continuously repeated, and the tin wire is continuously added to the welding gun 8.
[0051] As attached Figure 3 As shown, a wire unwinding rack 506 is provided on the base 501, and the wire unwinding rack 506 is used to set up the tin wire roll.
[0052] As attached Figure 2 And attached Figure 3 As shown, the first power device is the first cylinder 5101, and the second power device is the second cylinder 5102. The first cylinder 5101 and the second cylinder 5102 are each equipped with a clamping plate 503. The first cylinder 5101 is used to drive the clamping plate 503 and the first clamping seat 5201 to clamp the tin wire together, and the second cylinder 5102 is used to drive the clamping plate 503 and the second clamping seat 5202 to clamp the tin wire together.
[0053] The clamping plate 503 is provided to better clamp the tin wire. Figure 3 As shown in FIG. 4 , it is a quadrilateral frame. Figure 2 As shown, it is formed by fixing multiple plates and multiple columns together, but it is a conventional structure and no detailed reference mark is made in this figure. At the same time, the sliding seat 11 is provided with wheels, and the sliding seat is slidably mounted on the slide rail 401 through its own wheels. When the adjustment disk 1101 on the sliding seat 11 is rotated, the wheels on the sliding seat 11 will rotate, so that the sliding seat 11 will move on the slide rail 401. This part also belongs to the existing conventional technology and is not marked in detail in the figure. The mounting seat 10 is composed of multiple plates, columns, bolts and other components. This part also belongs to the existing conventional technology, so the structure of the mounting seat 10 is no longer described in detail in the figure.
[0054] As attached Figure 2 And attached Figure 3 As shown, a sliding rod 505 is provided on the base 501, a sleeve 504 is provided on the second clamping seat 5202, and the second clamping seat 5202 is slidably sleeved on the sliding rod 505 through the sleeve 504. The third power device is a third cylinder 5103, and the third cylinder 5103 is fixedly installed on the base 501, and one end of the third cylinder 5103 is fixed to the second clamping seat 5202.
[0055] As attached Figure 2 And attached Figure 3 As shown, the negative electrode sheet 9 is a tube-shaped, column-shaped, or sheet-shaped negative electrode sheet 9.
[0056] The device uses the heat generated by the argon arc welding current to replace the electric soldering iron to melt the tin wire, combines the argon arc welding with the soldering iron tin wire welding, and has a better welding effect.
[0057] Need to attach Figure 3 , Attachment Figure 4 And attached Figure 5 It is further explained that in order to clearly show the coordination relationship of the main components, some minor components are not drawn in these figures. Figure 3 , Attachment Figure 4 And attached Figure 5 It does not represent the complete structure of the combined welding device. For the complete structure of the combined welding device, please refer to the attached Figure 2 .
[0058] The present invention also provides a combined welding method, comprising the following steps:
[0059] S1: Place the tin wire in the heating area between the welding gun and the negative electrode;
[0060] S2: Power on the welding gun and the negative electrode sheet, and use the heat generated by the current between the welding gun and the negative electrode sheet to melt the tin wire;
[0061] S3: While the tin wire is melting, continuously add tin wire to the heating point between the welding gun and the negative electrode sheet.
[0062] The above description is only a preferred embodiment of the present invention, and does not limit the patent protection scope of the present invention. Any equivalent structural transformation made by using the contents of the present invention and the drawings, directly or indirectly used in other related technical fields, is also included in the protection scope of the present invention.
Claims
1. A combined welding method, characterized in that: The steps include: S1: Place the tin wire in the heating area between the welding gun and the negative electrode; S2: Power on the welding gun and the negative electrode sheet, and use the heat generated by the current between the welding gun and the negative electrode sheet to melt the tin wire; S3: During the melting process of the tin wire, the tin wire is continuously added to the heating part of the welding gun and the negative electrode sheet; The heat generated by the current first melts the tin wire, allowing the molten tin to flow to the upper and lower end faces of the terminal, and then uses the heat to melt the pole. After the lead and tin are solidified, the pole and the terminal are firmly fixed together; Welding is performed using a combined welding device, including a bracket, a wire feeding device, a welding gun and a negative electrode sheet, wherein the wire feeding device is directly or indirectly fixed to the bracket, the welding gun is directly or indirectly fixed to the bracket, and the negative electrode sheet is directly or indirectly fixed to the bracket, the wire feeding device is used to transport the tin wire to the heat generating area between the welding gun and the negative electrode sheet, and the welding gun and the negative electrode sheet are used together to melt the tin wire; The welding gun is a tubular welding gun, and the wire feeding device is used to feed the tin wire to the bottom of the welding gun; The negative electrode sheet is a tube-shaped, column-shaped or sheet-shaped negative electrode sheet; It also includes a first motion mechanism, which is slidably mounted on the bracket, the welding gun and the negative electrode sheet are both mounted on the first motion mechanism, and the first motion mechanism is used to drive the welding gun and the negative electrode sheet to move longitudinally and transversely; The first motion mechanism comprises a sliding seat, a mounting seat and a motion rod, the sliding seat is slidably mounted on the bracket, the welding gun and the negative electrode plate are both mounted on the mounting seat, the motion rod is mounted on the sliding seat, the mounting seat is fixedly mounted on the motion rod, and the motion rod is used to drive the mounting seat to move towards or away from the sliding seat; The bracket is provided with a slide rail, the slide seat is slidably mounted on the slide rail, the movement rod is a screw rod, the movement rod and the slide seat are matched together in the form of threaded matching, and the movement rod is always perpendicular to the sliding direction of the slide seat, and the mounting seat is fixed to one end of the movement rod; The wire feeding device comprises a first clamping seat, a first power device, a second clamping seat, a second power device, a third power device and a base, wherein the first power device is installed on the first clamping seat, the second power device is installed on the second clamping seat, the first clamping seat is fixedly installed on the base, the second clamping seat is slidably installed on the base, the third power device is fixedly installed on the base, and the third power device is used to drive the second clamping seat to move on the base; the first clamping seat and the first power device are used together to clamp the tin wire, and the second clamping seat and the second power device are used together to clamp the tin wire from the first clamping seat to the welding gun; The first power device is a first cylinder, and the second power device is a second cylinder. A clamping plate is installed on each of the first cylinder and the second cylinder. The first cylinder is used to drive the clamping plate to work together with the first clamping seat to clamp the tin wire, and the second cylinder is used to drive the clamping plate to work together with the second clamping seat to clamp the tin wire. A sliding rod is arranged on the base, a sleeve is arranged on the second clamping seat, the second clamping seat is slidably mounted on the sliding rod through the sleeve, the third power device is a third cylinder, the third cylinder is fixedly mounted on the base, and one end of the third cylinder is fixed to the second clamping seat.