A high vacuum flat cavity and production method thereof

By adopting the design of triangular cavity body and reinforcement plate in the vacuum equipment, combined with the single-sided welding process, the vacuum degree and leakage problems of flat cavity are solved, and the improvement of high vacuum degree and strength is achieved.

CN111266809BActive Publication Date: 2024-11-12ZHEJIANG YUCHEN INTELLIGENT EQUIP CO LTD
View PDF 16 Cites 0 Cited by

Patent Information

Application Number
CN202010184283.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-03-17
Publication Date
2024-11-12
Estimated Expiration
2040-03-17

AI Technical Summary

Technical Problem

It is difficult to achieve high vacuum in existing vacuum equipment, and internal gaps and material selection lead to problems such as leakage and high processing costs.

Method used

The triangular cavity body and flange structure are adopted to form a rectangular vacuum chamber through bending edge welding, and reinforcement plates are installed on the outer surface. Single-sided welding and double-sided forming process are adopted, and argon gas protection welding is used to ensure welding. Mass and cavity strength.

Benefits of technology

The high vacuum degree is achieved, which reduces gaps and vacuum time, extends the service life of the equipment, and increases the strength and vacuum degree of the cavity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111266809B_ABST
    Figure CN111266809B_ABST
Patent Text Reader

Abstract

The present invention discloses a high vacuum flat cavity, comprising a triangular cavity body, a first flange and a second flange, wherein the cavity body comprises a first plate body and a second plate body, wherein the first plate body and the second plate body are arranged in parallel and the two side edges are bent toward each other to form a bent edge, wherein the bent edges are welded and sealed to enclose a vacuum chamber, wherein the cross section of the vacuum chamber is a rectangle and the length of the rectangle is much greater than the width; the cavity body has a first opening and a second opening, wherein the first opening and the second opening are respectively located at the bottom and the top of the cavity body, wherein the first flange is fixedly arranged at the first opening and the second flange is fixedly arranged at the second opening; and a production method of a high vacuum flat cavity is also disclosed. The high vacuum flat cavity of the present application has a reasonable structure and high strength, and can well meet the use requirements of the vacuum system; in addition, the present application adopts a single-sided welding and double-sided forming welding process, which directly welds through and does not produce gaps inside.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of vacuum equipment, and in particular relates to a high vacuum flat cavity and a production method thereof. Background Art

[0002] The core of the vacuum system is the vacuum chamber, which is tailor-made for specific applications. It is to reliably separate it from the outside or prevent the environment from being affected by the internal process. Regardless of whether the drying process requires a high vacuum environment, the plasma process needs to be carried out in a medium or high vacuum environment, and the surface research also needs to be carried out in a high vacuum environment. The vacuum chamber must always mechanically withstand the pressure difference between it and the atmosphere. The vacuum chamber needs to reach the vacuum degree of use, which requires a very small outgassing rate in the chamber. There are many factors that affect the vacuum degree: the better the sealing of the vacuum chamber, the lower the leakage rate, and the better the vacuum will be drawn; the outgassing amount of the vacuum chamber material, the outgassing amount of different materials is different, and the vacuum chambers of high vacuum and ultra-high vacuum equipment are generally made of stainless steel; another is the cleanliness of the vacuum chamber. If there are a lot of condensable gases such as oil, alcohol, and water in the vacuum chamber, these components will gasify and decompose when the vacuum degree rises, which has a great impact on the high vacuum equipment. There should be as few gaps as possible inside the chamber. Oil, water, etc. are most likely to accumulate in the gaps. The basic shape of the chamber is usually determined by the application. For the cavity, if possible, a cylindrical tube should be selected, which is conducive to the placement of materials and the stability of the system, but there will inevitably be a demand for a flat vacuum chamber. Since the flat internal space is small, it is difficult to weld and process. If the vacuum side cannot be welded, gaps will be generated, which greatly affects the vacuum degree of the cavity.

[0003] The existing technology often adopts the following methods for production: Option 1, usually in order to ensure that the required vacuum degree is easier to achieve, full internal welding and external intermittent welding are generally adopted. If external welding is used in the cavity welding, gaps will be generated inside due to the inability to weld through. Oil and water stains will remain during the cleaning process, and it is difficult to handle them if they are not clean, which will eventually affect the vacuum pumping time and vacuum degree of the chamber; Option 2, using aluminum alloy that is easier to cut, but the degassing rate of aluminum is higher than that of stainless steel, which affects the vacuum pumping time and vacuum degree, and the overall processing cost is high, the internal space is small, customized tools are required for processing, and deep chip removal is difficult; aluminum is not easy to weld, prone to leakage, and it is difficult to add other interfaces, and it cannot be used for ultra-high vacuum chamber production; aluminum has low strength and cannot meet design requirements. Summary of the invention

[0004] The purpose of the present invention is to provide a high vacuum flat cavity and a production method thereof, which is intended to solve the technical problems existing in the background technology.

[0005] To solve the above technical problems, the purpose of the present invention is achieved as follows:

[0006] A high vacuum flat cavity comprises a triangular cavity body, a first flange and a second flange, wherein the cavity body comprises a first plate body and a second plate body, wherein the first plate body and the second plate body are arranged in parallel and the two side edges are bent toward each other to form bent edges, wherein the bent edges are welded and sealed to enclose a vacuum cavity, wherein the cross section of the vacuum cavity is a rectangle and the length of the rectangle is much greater than the width; wherein the cavity body comprises a first opening and a second opening, wherein the first opening and the second opening are respectively located at the bottom and the top of the cavity body, wherein the first flange is fixed to the first opening, and the second flange is fixed to the second opening.

[0007] On the basis of the above scheme and as a preferred scheme of the above scheme: the outer surfaces of the first plate body and the second plate body are provided with reinforcing ribs, and the reinforcing ribs include multiple vertical ribs and multiple transverse ribs, the vertical ribs are fixedly arranged in parallel on the outer surfaces of the first plate body and the second plate body, and the transverse ribs are located between two adjacent vertical ribs and the transverse ribs are respectively fixedly connected to the two adjacent vertical ribs.

[0008] On the basis of the above solution and as a preferred solution of the above solution: the vertical rib plate is fixed with mounting feet.

[0009] On the basis of the above scheme and as a preferred scheme of the above scheme: a method for producing a high vacuum flat cavity comprises the following steps:

[0010] S1: Cutting the first plate and the second plate;

[0011] S2: Both sides of the first plate and the second plate are bent to form bent edges;

[0012] S3: The outer edge of each bending edge is processed with a groove, the single-side angle of the groove is 30 degrees, and the blunt edge is left with 0.5mm;

[0013] S4: After the bent edges of the first plate and the second plate are joined together, flat welding is used to alternately weld the plates at set lengths, and a gap of 2-3 mm is reserved between the two opposite bent edges during the welding process, and shielding gas is used for protection during the welding process;

[0014] S5: Bottom layer welding: continuous welding is used for welding. During welding, the welding gun swings slightly in a zigzag shape and stays for a while on both sides of the groove. During the welding process, the welding wire is kept at a certain length for continuous welding.

[0015] S6: Surface welding;

[0016] S7: Cavity body molding.

[0017] On the basis of the above scheme and as a preferred scheme of the above scheme: it also includes the step of welding and installing the first flange, the second flange and the reinforcing rib plate to the cavity body.

[0018] On the basis of the above scheme and as a preferred scheme of the above scheme: the protective gas is argon with a purity of 99.99%.

[0019] On the basis of the above scheme and as a preferred scheme of the above scheme: the set length in step S4 is 100 mm.

[0020] Compared with the prior art, the present invention has the following outstanding and beneficial technical effects: the high-vacuum flat cavity of the present invention has a reasonable structure and high strength, and can well meet the use requirements of the vacuum system; in addition, the present invention adopts a single-sided welding and double-sided forming welding process, which directly welds through without generating gaps inside, and can significantly improve the vacuum degree of the flat vacuum cavity and shorten the vacuum pumping time; the welding quality is more reliable, the service life of the chamber is extended, the internal gaps are reduced, the vacuum pumping time is shortened, the vacuum degree is improved, and more time is gained for experiments or production. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a three-dimensional schematic diagram of the overall structure of the present invention;

[0022] Figure 2 It is a GG schematic diagram of the present invention;

[0023] Figure 3 It is a front view of the present invention;

[0024] Figure 4 It is a DD schematic diagram;

[0025] Figure 5 It is a schematic diagram of the weld structure;

[0026] Figure 6 It is a schematic diagram of the internal structure of the present invention. DETAILED DESCRIPTION

[0027] In order to make the purpose, technical solution and advantages of this application clearer, the technical solution in the embodiment will be clearly and completely described below in conjunction with the drawings in the embodiment. Obviously, the described embodiment is only a part of the embodiment of this application, not all embodiments. Based on the given embodiments, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.

[0028] In the description of the present application, it should be understood that the terms "upper", "lower", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0029] In the description of this application, the terms "first", "second", etc. are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features.

[0030] A high vacuum flat cavity comprises a triangular cavity body, a first flange 1 and a second flange 6, wherein the cavity body comprises a first plate body 4 and a second plate body 5, wherein the first plate body 4 and the second plate body 5 are arranged in parallel and the two side edges are bent toward each other to form a bent edge 41 / 51, wherein the bent edges 41 / 51 are welded and sealed to enclose a vacuum chamber 7, wherein the cross section of the vacuum chamber 7 is a rectangle and the length of the rectangle is much greater than the width; the cavity body comprises a first opening 81 and a second opening 82, wherein the first opening 81 and the second opening 82 are respectively located at the bottom and the top of the cavity body, wherein the first flange 1 is fixed to the first opening 81, and the second flange 6 is fixed to the second opening 82.

[0031] In order to strengthen the strength of the cavity body and avoid excessive deformation of the cavity body during the vacuum process, the present embodiment preferably provides reinforcing ribs 3 on the outer surfaces of the first plate body 4 and the second plate body 5, and strengthens the strength of the cavity body by providing the reinforcing ribs 3; specifically, the present embodiment preferably includes a plurality of vertical ribs 31 and a plurality of transverse ribs 32, the vertical ribs 31 are fixedly arranged in parallel on the outer surfaces of the first plate body 4 and the second plate body 5, the transverse ribs 32 are located between two adjacent vertical ribs 31 and the transverse ribs 32 are respectively fixedly connected to the two adjacent vertical ribs 31; the longitudinal strength of the cavity body is strengthened by the vertical ribs 32, and the transverse strength of the cavity body is strengthened by the transverse ribs, thereby greatly enhancing the strength of the cavity body and reducing the deformation of the cavity body during the vacuum process.

[0032] The vertical rib plate 31 is fixed with a mounting foot 2, and the mounting foot 2 is used to fix the cavity body.

[0033] Specifically, when the high vacuum flat chamber in this embodiment is used, the mounting foot 2 is first mounted and fixed to the body, and then the first flange 1 and the second flange 6 are connected to the flange of the external pipeline by bolts to build a vacuum system with other equipment.

[0034] This embodiment also discloses a method for producing a high vacuum flat cavity, comprising the following steps:

[0035] S1: Cutting the first plate body 4 and the second plate body 5, including the step of cutting the stainless steel plate according to the shapes of the first plate body 4 and the second plate body 5; specifically, the plate cutting can be performed by laser cutting, plate cutting machine or other cutting methods.

[0036] S2: using a plate folding machine to bend both sides of the first plate body 4 and the second plate body 5 to form two first bending edges 41 on both sides of the first plate body 4 and two second bending edges 51 on both sides of the second plate body 5 .

[0037] S3: The first plate body 4 and the second plate body 5 are buckled together, and the first bend edge 41 and the corresponding second bend edge 51 are processed into the first bevel 411 and the second bevel 511 on the outer edges respectively. Preferably, the single-side angle of the first bevel 411 and the second bevel 511 is 30 degrees, and the blunt edge 412 / 512 has a length of 0.5 mm.

[0038] S4: After the first bent edge 41 and the second bent edge 51 of the first plate body 4 and the second plate body 5 are spliced ​​together, flat welding is used to perform staggered welding at set lengths. During the welding process, a gap of 2-3mm is reserved between the two opposite bent edges, and shielding gas is used for protection during the welding process; the preferred set length is 100mm, that is, after the first bent edge 41 and the second bent edge 51 of the first plate body 4 and the second plate body 5 are spliced ​​together, flat welding is used to perform staggered welding at intervals of 100mm, so that deformation is small. During assembly, staggered welding is performed at intervals of 100mm to ensure that the root gap is uniform and reasonable with a deviation of less than 1mm. In addition, the shielding gas is preferably argon with a purity of 99.99%.

[0039] S5: Bottom layer welding; continuous welding is adopted for welding. During welding, the welding gun swings horizontally in a small sawtooth shape and stops for a while on both sides of the groove. During the welding process, the welding wire is always kept at a certain length for continuous welding. The welding of the bottom layer weld is the key to the operation. Under the high temperature and blowing force of the arc, the root metal of the first groove and the second groove is melted to form a metal molten pool. A hole slightly larger than the assembly gap between the first groove and the second groove will be generated at the front of the molten pool. The shielding gas can provide a certain protection to the back of the weld through the hole. The bottom layer adopts the continuous welding method. During the welding process, the arc burns continuously and does not extinguish. A narrow groove gap and a small blunt edge are adopted. During the welding process, the welding gun swings horizontally in a small sawtooth shape and stops for a while on both sides of the first groove and the second groove. The welding wire is always kept at a certain length for continuous welding. In this way, the back of the weld is formed more finely and neatly, with good internal quality and stable and excellent mechanical properties.

[0040] S6: Surface welding; pay attention to the welding temperature and the current should be moderate to prevent the tendency of intergranular corrosion caused by overheating.

[0041] S7: Cavity body forming. After this step, the first plate and the second plate are welded to obtain a cavity body with a relatively fine and neat back weld, good internal quality, stable and excellent mechanical properties, more reliable welding quality, extended chamber service life, reduced internal gaps, shortened vacuum time, and improved vacuum degree.

[0042] In addition, after the cavity body is formed, the method further includes welding and installing the first flange 1 , the second flange 6 and the reinforcing rib plate 3 to the cavity body.

[0043] The above embodiments are only preferred embodiments of the present invention and are not intended to limit the protection scope of the present invention. Therefore, any equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for producing a high vacuum flat cavity, characterized in that: The high vacuum flat cavity comprises a triangular cavity body, a first flange and a second flange, the cavity body comprises a first plate body and a second plate body, the first plate body and the second plate body are arranged in parallel and the two side edges are bent toward each other to form a bent edge, the bent edges are welded and sealed to enclose a vacuum cavity, the cross section of the vacuum cavity is a rectangle and the length of the rectangle is much greater than the width; the cavity body has a first opening and a second opening, the first opening and the second opening are respectively located at the bottom and the top of the cavity body, the first flange is fixedly arranged at the first opening, and the second flange is fixedly arranged at the second opening; The outer surfaces of the first plate body and the second plate body are provided with reinforcing ribs, the reinforcing ribs include a plurality of vertical ribs and a plurality of transverse ribs, the vertical ribs are fixedly arranged parallel to the outer surfaces of the first plate body and the second plate body, the transverse ribs are located between two adjacent vertical ribs, and the transverse ribs are respectively fixedly connected to the two adjacent vertical ribs; The following steps are also included: S1: Cutting the first plate and the second plate; S2: Both sides of the first plate and the second plate are bent to form bent edges; S3: The outer edge of each bending edge is processed with a groove, the single-side angle of the groove is 30 degrees, and the blunt edge is left with 0.5mm; S4: After the bent edges of the first plate and the second plate are joined together, flat welding is used to alternately weld the plates at set lengths, and a gap of 2-3 mm is reserved between the two opposite bent edges during the welding process, and shielding gas is used for protection during the welding process; S5: Bottom layer welding: continuous welding is used for welding. During welding, the welding gun swings slightly in a zigzag shape and stays for a while on both sides of the groove. During the welding process, the welding wire is kept at a certain length for continuous welding. S6: Surface welding; S7: Cavity body molding.

2. The method for producing a high vacuum flat cavity according to claim 1, characterized in that: The vertical ribs are fixed with mounting feet.

3. The method for producing a high vacuum flat cavity according to claim 1, characterized in that: The method also includes the step of welding and installing the first flange, the second flange and the reinforcing rib plate to the cavity body.

4. The method for producing a high vacuum flat cavity according to claim 1, characterized in that: The protective gas is argon gas with a purity of 99.99%.

5. The method for producing a high vacuum flat cavity according to claim 1, characterized in that: The set length in step S4 is 100 mm.

Citation Information

Patent Citations

  • Self-positioning vacuum brazing technique for multi-cavity electrical bridge waveguide

    CN103433701A

  • Engine exhaust pipe based on SCR tail gas aftertreatment technology

    CN103982285A

  • Full-automatic 9% Ni steel medium-thin plate vertical butt joint FCAW one-side welding and double-side molding technological method

    CN105081520A

  • Thick-plate single-side welding method

    CN105643066A

  • Novel aluminum fuel tank and method for producing same

    CN105946557A