A flexible silicon oxide thin film growth device

By designing a silicon oxide film growth device including a reaction cavity and radio frequency electrodes in flexible electronic products, using non-toxic gas sources to quickly grow high-quality silicon oxide films at room temperature, solving the problem of low-temperature growth and gas sources in the existing technology Safety issues provide packaging materials suitable for flexible electronic products.

CN111793791BActive Publication Date: 2024-10-29SHANDONG UNIV
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202010640162.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-07-06
Publication Date
2024-10-29
Estimated Expiration
2040-07-06

AI Technical Summary

Technical Problem

It is difficult to grow high-quality flexible silicon oxide films at low temperatures with existing technology, and the gas source used by conventional equipment is dangerous and cannot meet the packaging needs of flexible electronic products.

Method used

A flexible silicon oxide film growth device including a reaction chamber, gas path system, control system, vacuum system and exhaust gas treatment system is designed. Radio frequency electrodes are used to excite gases for chemical deposition reactions. Non-toxic and non-hazardous Liujia Silicone-based, nitrogen and oxygen gas sources enable thin film growth at room temperature.

Benefits of technology

Silicon oxide films with high density and good mechanical flexibility are rapidly grown at room temperature, which is suitable for flexible electronic packaging. The gas source is safe and high temperature damage to the substrate is avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111793791B_ABST
    Figure CN111793791B_ABST
Patent Text Reader

Abstract

The present invention discloses a flexible silicon oxide-like thin film growth device, including a reaction chamber and a gas circuit system, a control system, a vacuum system and an exhaust gas treatment system connected to the reaction chamber; a radio frequency electrode is suspended and horizontally arranged inside the reaction chamber, the radio frequency electrode is connected to the positive electrode of the radio frequency power supply, and the reaction chamber is connected to the negative electrode of the radio frequency power supply; a gas mixer is arranged below the radio frequency electrode, a substrate for depositing a thin film is fixed on the inner side of the top cover of the reaction chamber, the gas mixer is connected to the gas circuit system, a gas outlet is opened on the reaction chamber to connect the vacuum system; the gas circuit system includes a hexamethylsiloxane storage tank, a nitrogen storage tank, an oxygen storage tank, and a carbon tetrafluoride storage tank, each storage tank is connected to the main pipe at the front end of the reaction chamber through a branch pipeline, and the main pipe is connected to the gas mixer. The device disclosed by the present invention can prepare a flexible silicon oxide-like thin film at room temperature, has good packaging performance, and can be used as a good flexible insulating medium material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a thin film growing device, in particular to a flexible silicon oxide-like thin film growing device. Background Art

[0002] With the rapid development of flexible electronic products, flexible thin film packaging materials have become extremely important. Flexible electronic products require flexible packaging films to be dense to prevent the ingress of oxygen, water and other substances, and to be mechanically flexible. The equipment commonly used for low-temperature growth of dense sealing materials such as aluminum oxide is the atomic layer deposition equipment (ALD). Although ALD can grow dense aluminum oxide, the growth rate is very slow, and the aluminum oxide film is not tough enough. Microcracks are very easy to form during the bending process, and it cannot effectively protect the device from the intrusion of oxygen or water vapor in the environment for a long time.

[0003] In addition to aluminum oxide, dense packaging materials include silicon oxide and silicon nitride, both of which can be grown using ion-enhanced chemical vapor deposition equipment (PECVD). Conventional PECVD needs to be heated to above 300°C to grow high-quality silicon oxide or silicon nitride, but the materials, devices and substrates of flexible electronic products generally cannot withstand high temperatures. Therefore, conventional PECVD basically cannot meet the needs of thin film growth for flexible electronic packaging. Moreover, the gas sources used by conventional PECVD for the growth of dense thin film materials, such as silane, ammonia, and hydrogen, are all very dangerous. Summary of the invention

[0004] In order to solve the above technical problems, the present invention provides a flexible silicon oxide-like film growth device, so as to achieve the purpose of preparing a flexible silicon oxide-like film at room temperature, which has good packaging performance and can be used as a good flexible insulating dielectric material.

[0005] To achieve the above object, the technical solution of the present invention is as follows:

[0006] A flexible silicon oxide-like thin film growth device comprises a reaction chamber and a gas path system, a control system, a vacuum system and an exhaust gas treatment system connected to the reaction chamber;

[0007] A radio frequency electrode is suspended and horizontally arranged inside the reaction chamber, the radio frequency electrode is connected to the positive electrode of the radio frequency power supply, and the reaction chamber is connected to the negative electrode of the radio frequency power supply; a gas mixer is arranged below the radio frequency electrode, a substrate for thin film deposition is fixed on the inner side of the top cover of the reaction chamber, the front side of the substrate faces the radio frequency electrode, the gas mixer is connected to the gas circuit system through the gas inlet on the reaction chamber, and a gas outlet is arranged on the reaction chamber to connect to the vacuum system;

[0008] The gas circuit system includes a hexamethylsiloxane storage tank, a nitrogen storage tank, an oxygen storage tank, and a carbon tetrafluoride storage tank, each storage tank is connected to the main pipe at the front end of the reaction chamber through a branch pipeline, and the main pipe is connected to the gas mixer;

[0009] The end of the vacuum system is connected to the tail gas treatment system.

[0010] In the above scheme, a bypass is provided between the branch pipeline connected to the hexamethylsiloxane storage tank and the branch pipeline connected to the nitrogen storage tank, and a bypass control switch is provided on the bypass.

[0011] In the above solution, the distance from the inner side of the top cover of the reaction chamber to the radio frequency electrode is 5-25 mm.

[0012] In the above scheme, a gas flow meter and a gas flow switch are respectively provided on each branch pipeline.

[0013] In the above scheme, the control system controls the radio frequency power supply, the vacuum system, the gas flow switch and the bypass control switch respectively.

[0014] In the above scheme, the exhaust gas treatment system includes a water pool, the front end of the water pool is connected to the vacuum system through a pipeline, and the end of the water pool is connected to the exhaust gas emission pipeline of the laboratory.

[0015] In the above solution, a temperature sensor is arranged on the top cover of the reaction chamber, and the temperature sensor is connected to a control system.

[0016] In the above solution, a circle of grooves for fixing the sealing ring is provided on the top cover of the reaction chamber.

[0017] In the above solution, a second gas outlet is provided on the side wall of the reaction chamber, and a valve is provided on the second gas outlet.

[0018] In the above solution, the vacuum system includes a mechanical pump, a molecular pump and a vacuum control device, and the vacuum control device is located between the mechanical pump and the reaction chamber.

[0019] Through the above technical solution, the flexible silicon oxide-like thin film growth device provided by the present invention has the following beneficial effects:

[0020] 1. This device grows flexible silicon oxide-like thin films at room temperature, has low high temperature resistance requirements for reaction devices and substrates, and has multiple selectivity;

[0021] 2. This device selects non-toxic and non-hazardous gas sources of hexamethylsiloxane, nitrogen and oxygen, which are mixed through the branch pipeline and the main pipeline and then enter the reaction chamber. After the reaction, they are treated by the exhaust gas treatment system and are harmless to the environment.

[0022] 3. The gas is excited into a plasma state by the radio frequency electrode of the device, and then a chemical deposition reaction occurs to obtain a thin film with a fast growth rate;

[0023] 4. The density of the film prepared by this device is similar to that of thermally oxidized silicon dioxide. Since most of the remaining hexamethylsiloxane after being oxidized by oxygen during the growth process is silicon and oxygen, with very little nitrogen, carbon and hydrogen, a small amount of carbon and hydrogen makes this film have good mechanical flexibility;

[0024] 5. The film prepared by this device can be used as a good flexible film packaging material with good step coverage. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below.

[0026] Figure 1 This is an overall schematic diagram of a flexible silicon oxide-like thin film growth device disclosed in an embodiment of the present invention;

[0027] Figure 2 This is a schematic diagram of the internal structure of the reaction chamber disclosed in an embodiment of the present invention;

[0028] Figure 3 This is a schematic diagram of the top cover structure of the reaction chamber disclosed in an embodiment of the present invention;

[0029] Figure 4 A schematic diagram of the radio frequency electrode structure disclosed in an embodiment of the present invention;

[0030] Figure 5 This is a schematic diagram of the structure of a gas mixer disclosed in an embodiment of the present invention.

[0031] In the figure, 1. reaction chamber; 2. radio frequency electrode; 3. gas mixer; 4. top cover; 5. substrate; 6. gas inlet; 7. gas outlet 1; 8. gas outlet 2; 9. temperature sensor; 10. groove; 11. hexamethylsiloxane storage tank; 12. nitrogen storage tank; 13. oxygen storage tank; 14. carbon tetrafluoride storage tank; 15. branch pipeline; 16. main pipeline; 17. air outlet; 18. bypass; 19. bypass control switch; 20. gas flow meter; 21. gas flow switch; 22. mechanical pump; 23. molecular pump; 24. vacuum control device; 25. water tank; 26. bracket. DETAILED DESCRIPTION

[0032] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings in the embodiments of the present invention.

[0033] The present invention provides a flexible silicon oxide-like thin film growth device, such as Figure 1 As shown, it includes a reaction chamber 1 and a gas circuit system, a control system, a vacuum system and an exhaust gas treatment system connected to the reaction chamber 1.

[0034] like Figure 2 As shown, a radio frequency electrode 2 is suspended horizontally inside the reaction chamber 1, the radio frequency electrode 2 is connected to the positive electrode of the radio frequency power supply, and the reaction chamber 1 is connected to the negative electrode of the radio frequency power supply; a gas mixer 3 is arranged below the radio frequency electrode 2, and a substrate 5 for depositing a thin film is fixed inside the top cover 4 of the reaction chamber 1, and the front side of the substrate 5 faces Figure 4 The RF electrode 2 and the gas mixer 3 shown are connected to the gas circuit system through the gas inlet 6 on the reaction chamber 1, and the bottom of the reaction chamber 1 is provided with a gas outlet 7 connected to the vacuum system. The side wall of the reaction chamber 1 is provided with a gas outlet 8, and a valve is provided on the gas outlet 8. The gas outlet 8 is used to discharge the gas in the reaction chamber 1. When the pressure is too high, it can be discharged through the gas outlet 8. A temperature sensor 9 is provided on the top cover 4 of the reaction chamber 1 to monitor the temperature in the reaction chamber 1. The distance from the inner side of the top cover of the reaction chamber to the RF electrode is 5-25mm.

[0035] The radio frequency electrode 2 and the gas mixer 3 are both mounted on a bracket 26 , and the bottom of the bracket 26 is fixed to the bottom of the reaction chamber 1 .

[0036] like Figure 3 As shown, a circle of grooves 10 for fixing a sealing ring is provided on the top cover 4 of the reaction chamber 1, and the top cover 4 and the reaction chamber 1 are sealed by the sealing ring.

[0037] The gas circuit system includes a hexamethylsiloxane storage tank 11, a nitrogen storage tank 12, an oxygen storage tank 13, and a carbon tetrafluoride storage tank 14, each of which is connected to a main pipe 16 at the front end of the reaction chamber 1 through a branch pipe 15, and the main pipe 16 is connected to a gas mixer 3. The gas mixer 3 is as shown in FIG. Figure 5 As shown, the upper part thereof has a plurality of gas outlet holes 17. A bypass 18 is provided between the branch pipeline 15 connected to the hexamethylsiloxane storage tank 11 and the branch pipeline 15 connected to the nitrogen storage tank 12, and a bypass control switch 19 is provided on the bypass 18. The bypass 18 is provided for nitrogen to purge the residual gas in the branch pipeline 15 connected to the hexamethylsiloxane storage tank 11. A gas flow meter 20 and a gas flow switch 21 are provided on each branch pipeline 15, respectively.

[0038] The vacuum system includes a mechanical pump 22, a molecular pump 23 and a vacuum control device 24. The vacuum control device 24 is located between the mechanical pump 22 and the reaction chamber 1. The vacuum control device 24 can ensure that a certain vacuum is maintained in the reaction chamber 1 during the chemical deposition process. The end of the vacuum system is connected to the exhaust gas treatment system. The exhaust gas treatment system includes a water pool 25, which is used to treat the exhaust gas after the growth gas of the plasma enhanced chemical vapor deposition equipment and the reaction chamber cleaning gas react. The front end of the water pool 25 is connected to the vacuum system through a pipeline, and the end of the water pool is connected to the exhaust gas exhaust pipeline of the laboratory.

[0039] The control system controls the radio frequency power supply, the vacuum system, the gas flow meter 20, the gas flow switch 21, the bypass control switch 19 and the temperature sensor 9 respectively.

[0040] When the device is in use, the substrate 5 is fixed to the inner side of the top cover 4 of the reaction chamber 1 by screws, with the front side facing downward. Figure 3 As shown, the reaction chamber 1 is evacuated by a vacuum system. When the set vacuum degree is reached, the gas flow switch 21 on the branch pipeline 15 connected to the hexamethylsiloxane storage tank 11, the nitrogen storage tank 12, and the oxygen storage tank 13 is turned on, and then the radio frequency power supply is turned on. The radio frequency electrode 2 excites the reaction gas in the reaction chamber 1 to a plasma state, and the plasma of hexamethylsiloxane, nitrogen and oxygen undergoes a chemical deposition reaction, and a thin film begins to grow on the substrate 5;

[0041] When the film grows to the desired thickness, turn off the RF power supply, then turn off the gas flow switches 21 of oxygen, nitrogen and hexamethylsiloxane, turn off the vacuum system, turn on the gas flow switch 21 on the branch pipe 15 connected to the nitrogen storage tank 12, and the bypass control switch 19, inflate the reaction chamber 1, open the top cover 4 of the reaction chamber after reaching atmospheric pressure, take out the sample, cover the top cover 4, open the vacuum system and start vacuuming, turn on the carbon tetrafluoride gas after 10 minutes, turn on the RF power supply, and use the carbon tetrafluoride plasma to etch the silicon oxide deposited in the reaction chamber 1 during the material growth, and clean the reaction chamber 1. After cleaning, turn off the RF power supply first, and then turn off the carbon tetrafluoride gas.

[0042] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A method for growing a flexible silicon oxide-like thin film at room temperature, characterized in that: The method is prepared by using a flexible silicon oxide thin film growth device, which includes a reaction chamber and a gas path system, a control system, a vacuum system and an exhaust gas treatment system connected to the reaction chamber; A radio frequency electrode is suspended and horizontally arranged inside the reaction chamber, the radio frequency electrode is connected to the positive electrode of the radio frequency power supply, and the reaction chamber is connected to the negative electrode of the radio frequency power supply; a gas mixer is arranged below the radio frequency electrode, a substrate for thin film deposition is fixed on the inner side of the top cover of the reaction chamber, the front side of the substrate faces the radio frequency electrode, the gas mixer is connected to the gas circuit system through the gas inlet on the reaction chamber, and a gas outlet is arranged on the reaction chamber to connect to the vacuum system; The gas circuit system includes a hexamethylsiloxane storage tank, a nitrogen storage tank, an oxygen storage tank, and a carbon tetrafluoride storage tank, each storage tank is connected to the main pipe at the front end of the reaction chamber through a branch pipeline, and the main pipe is connected to the gas mixer; The end of the vacuum system is connected to the tail gas treatment system; a bypass is set between the branch pipeline connected to the hexamethylsiloxane storage tank and the branch pipeline connected to the nitrogen storage tank, and a bypass control switch is set on the bypass; a gas flow meter and a gas flow switch are respectively set on each branch pipeline; The distance from the inner side of the top cover of the reaction chamber to the radio frequency electrode is 5-25 mm; A temperature sensor is arranged on the top cover of the reaction chamber, and the temperature sensor is connected to a control system; When the device is used, the substrate is fixed to the inner side of the top cover of the reaction chamber by screws, with the front side facing downward, and then the reaction chamber is evacuated by using a vacuum system. When the set vacuum degree is reached, the gas flow switch on the branch pipeline connected to the hexamethylsiloxane storage tank, the nitrogen storage tank, and the oxygen storage tank is turned on, and then the radio frequency power supply is turned on. The radio frequency electrode excites the reaction gas in the reaction chamber to a plasma state, and the plasma of hexamethylsiloxane, nitrogen and oxygen undergoes a chemical deposition reaction, and a thin film begins to grow on the substrate; When the film grows to the desired thickness, turn off the RF power supply, then turn off the gas flow switches of oxygen, nitrogen and hexamethylsiloxane, turn off the vacuum system, turn on the gas flow switch on the branch pipeline connected to the nitrogen tank, and turn on the bypass control switch to inflate the reaction chamber. After reaching atmospheric pressure, open the top cover of the reaction chamber, take out the sample, cover the top cover, open the vacuum system and start vacuuming. After 10 minutes, turn on the carbon tetrafluoride gas, turn on the RF power supply, and use the carbon tetrafluoride plasma to etch the silicon oxide deposited in the reaction chamber during material growth to clean the reaction chamber. After cleaning, turn off the RF power supply first, and then turn off the carbon tetrafluoride gas.

2. The method for growing a flexible silicon oxide-like thin film at room temperature according to claim 1, characterized in that: The control system controls the radio frequency power supply, the vacuum system, the gas flow switch and the bypass control switch respectively.

3. The method for growing a flexible silicon oxide-like thin film at room temperature according to claim 1, characterized in that: The tail gas treatment system comprises a water pool, the front end of which is connected to a vacuum system via a pipeline, and the rear end of which is connected to a tail gas discharge pipeline of a laboratory.

4. The method for growing a flexible silicon oxide-like thin film at room temperature according to claim 1, characterized in that: A circle of grooves for fixing the sealing ring is arranged on the top cover of the reaction chamber.

5. The method for growing a flexible silicon oxide-like thin film at room temperature according to claim 1, characterized in that: A second gas outlet is provided on the side wall of the reaction chamber, and a valve is arranged on the second gas outlet.

6. The method for growing a flexible silicon oxide-like thin film at room temperature according to claim 1, characterized in that: The vacuum system comprises a mechanical pump, a molecular pump and a vacuum control device, wherein the vacuum control device is located between the mechanical pump and the reaction chamber.

Citation Information

Patent Citations

  • Plasma Processing Method And Plasma Processing Apparatus

    CN103928285A

  • Vacuum reaction device and reaction method

    CN108149225A

  • Method for growing silicon oxide-like flexible film

    CN111893461A

  • Flexible silicon oxide film growth device

    CN212404273U

  • Flexible silicon oxide film large-area growth device

    CN213172560U