In-situ CVD and ALD coating of chambers with controlled metal contamination
By depositing a protective film on the internal surface of the substrate processing chamber, the problem of component corrosion under high temperature and high pressure is solved, the life of the equipment is extended and maintenance costs are reduced, and stable operation and substrate cleaning processing under high temperature and high pressure are achieved.
Patent Information
- Application Number
- CN201980034219.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-04-12
- Filing Date
- 2019-04-29
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2039-04-29
AI Technical Summary
The internal components of existing substrate processing chambers are prone to corrosion in high-temperature and high-pressure environments, leading to substrate contamination and unstable processing, affecting equipment life and maintenance costs.
Form a protective film on the internal surface of the processing chamber, use ALD or CVD technology to deposit amorphous Si, carbosilane, polysilicon and other materials to form a protective film to prevent corrosion, and remove the film by fluorine or nitrogen trifluoride gas when necessary .
Effectively protect the internal components of the processing chamber, extend the life of the equipment, reduce substrate contamination, ensure stable operation under high temperature and high pressure, and reduce maintenance costs.
Smart Images

Figure CN112154534B_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present disclosure relate generally to apparatus, systems, and methods for processing one or more substrates, and more particularly to apparatus, systems, and methods for processing chamber preparation. Background Art
[0002] Substrate processing chambers may be subjected to high temperatures exceeding 200°C and high pressures exceeding 1 bar, which create a harsh corrosive environment that can cause degradation of the internal components of the processing chamber. The internal components are exposed to these high temperature and high pressure environments, especially in combination with the process gases introduced into the processing chamber during substrate processing. Various coatings and films may be utilized to reduce this corrosion, however, these coatings and films may not be robust enough to withstand the processing conditions and may corrode or degrade during use of the processing chamber. This corrosion may negatively affect the processed substrate, for example by causing the corrosive surface to flake or peel off or separate and land on and contaminate the substrate.
[0003]
[0006] Therefore, there is a need in the art for improved protection of internal components of a processing chamber. Summary of the invention
[0004] Various methods of forming a protective film on a surface including an interior surface of a processing chamber are discussed herein. In one example, the method includes forming a protective film on a plurality of interior components in a processing chamber via ALD or CVD, the interior components including chamber sidewalls, a chamber bottom, a substrate support pedestal, a showerhead, and a chamber top; and after forming the protective film, positioning a substrate on the substrate support pedestal. The substrate contacts a portion of the substrate support pedestal that does not include the protective film.
[0005] In another example, a method for protecting a processing chamber includes: introducing at least one gas into the processing chamber; in response to the positioning of the at least one gas in the processing chamber, removing a first protective film from a plurality of internal components of the processing chamber. The method further includes: forming a second protective film on the plurality of internal components via ALD or CVD in the processing chamber, wherein the second protective film includes amorphous Si, carbosilane, polysilicon, SiC, SiN, SiO2, Al2O3, AlON, HfO2, or Ni3Al. In addition, in this example, the method includes positioning a substrate on a substrate support pedestal after forming the second protective film.
[0006] In another example, a method of processing a substrate includes: introducing at least one gas into a processing chamber; in response to positioning of the at least one gas in the processing chamber, removing a first protective film from a plurality of internal components of the processing chamber. The method further includes: forming a second protective film on the plurality of internal components via ALD or CVD in the processing chamber, wherein the second protective film includes amorphous Si, carbosilane, polysilicon, SiC, SiN, SiO2, Al2O3, AlON, HfO2, or Ni3Al. The method further includes: after forming the second protective film, positioning the substrate on a substrate support pedestal. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1 is a cross-sectional view of an example substrate processing chamber according to certain embodiments of the present disclosure.
[0008] Figure 2 A method for in-situ forming a protective film in a processing chamber according to certain embodiments of the present disclosure. DETAILED DESCRIPTION
[0009] The systems and methods discussed herein relate to the preparation of a substrate processing chamber such that the processing chamber is capable of withstanding processing temperatures in excess of 400° C. without corrosion or other degradation of the internal components of the processing chamber. The internal components of the processing chamber may be formed of materials such as aluminum, stainless steel, nickel-based superalloys, or other materials that may be degraded by high temperatures, high pressures, and / or etching gases in the processing chamber. Degradation of the internal components may cause metallic particulate matter from one or more of the internal components to contaminate one or more substrates positioned in the processing chamber. This contamination negatively impacts both immediate processing and downstream operations in the processing chamber. Furthermore, degradation of the internal processing chamber components reduces the life of the internal components, which increases maintenance and downtime costs.
[0010] The protective film discussed herein protects the internal components of the processing chamber from corrosion and erosion, reducing the pollution incidents of the processing chamber and the substrate manufactured in the processing chamber. The protective film is used to protect the processing chamber (including a high-pressure processing chamber operating at 1 bar or higher pressure) from corrosion. The protective film is formed in situ within the internal chamber body of the processing chamber using chemical vapor deposition (CVD) or atomic layer deposition (ALD). The protective film is formed on some or all exposed surfaces of the internal chamber body, including at least a portion of the internal chamber body wall, the shower head, and the substrate support base. In one example, the shower head of the processing chamber is used to distribute one or more precursors, and the protective film is formed by the one or more precursors. In some embodiments, the protective cover is placed on some or all of the top surfaces of the substrate support base in the processing chamber. The protective cover can be positioned on the substrate support base so that an area on the base equal to or greater than the diameter of the substrate is not coated by the protective film during deposition. The protective cover can be used to protect the back side of the substrate from contamination from the protective film, which can negatively affect downstream operations. In one example, when a substrate is positioned on a substrate support pedestal in a processing chamber after the protective film has been deposited, the substrate does not contact the protective film. In an alternative embodiment, no protective cover is used. In this example, the entire surface of the substrate support pedestal (including where one or more substrates are positioned for processing) is covered by the protective film.
[0011] The protective film may be formed in situ and removed in situ after processing one or more substrates or a batch of substrates in a processing chamber. In contrast, non-in situ coating of a processing chamber can be challenging, such as downtime due to re-coating. Substrate processing in a processing chamber including a protective film or in other chambers after the formation of the protective film may include the deposition of one or more layers. The formation of multiple features of different aspect ratios and / or in some embodiments may include processing the substrate with a hard mask, including a patterned hard mask. In one embodiment, the removal of the protective film may be performed by using one or more gases, including fluorine (F) gas or nitrogen trifluoride (NF3) gas. F or NF3 gas may be ionized into plasma in a remote plasma source (RPS) or in situ in a processing chamber. In one example, the RPS is used to form a NF3 plasma. After removing the protective film, a new protective film of the same or different composition as the previously applied protective film may be applied to the internal chamber body. The protective film is formed of the following materials, including: amorphous silicon (a-Si), carbosilane, polysilicon, silicon carbide (SiC), silicon nitride (SiN), silicon dioxide (SiO2), aluminum oxide (Al2O3), aluminum oxynitride (AlON), hafnium oxide (HfO2), nickel aluminide (Ni3Al), or a combination of the foregoing. The use of the protective film discussed herein thus increases the life of the internal components of the processing chamber and reduces the debris caused by corrosion of these components.
[0012] Figure 1 1 is a cross-sectional view of an example processing chamber 100 according to certain embodiments of the present disclosure. The processing chamber 100 has a protective film 120 formed according to certain embodiments of the present disclosure. The processing chamber 100 includes an outer chamber body 102 formed around an inner chamber body 104. In one embodiment, the outer chamber body 102 includes aluminum and the inner chamber body 104 includes stainless steel. In an alternative embodiment, the outer chamber body 102 includes aluminum and the inner chamber body 104 includes quartz, aluminum, or a The inner chamber body 104 may be defined by chamber walls 122, chamber bottom 124, and chamber top 108A formed by the bottom surface of chamber lid 108. In one embodiment, a vacuum is formed in a space 132 between the outer chamber body 102 and the inner chamber body 104. In one embodiment, the chamber walls 122, chamber bottom 124, chamber top 108A, and additional components discussed herein may be formed of one or more materials, such as stainless steel, quartz, nickel-based superalloys, or aluminum. The inner chamber body 104 is exposed to high temperatures, high pressures, and in some instances, to etching gases, which may corrode and degrade components of the inner chamber body 104. In one example, the processing chamber 100 is coupled to a remote plasma source (RPS) 112, a gas panel 118, a condenser 114, and a steam generator 116.
[0013] In one embodiment, during operation of the processing chamber 100, the processing chamber 100 may be pressurized and have a temperature that is controlled in various ways. In one example, the pressure within the processing space 134 is controlled using a throttle valve 136 located between the inner chamber body 104 and the vacuum pump 138. The temperature at the surface of the chamber wall 122 is controlled using one or more heating elements 128A. The one or more heating elements 128A may be solid elements or liquid-containing elements located in the chamber wall 122 and / or the chamber lid 108 of the inner chamber body 104. In some examples, the one or more heating elements 128A are disposed in the substrate support base 106. In one example, the chamber lid 108 may be heated from 100°C to 300°C. Multiple heating elements 128A may be disposed in the chamber wall 122 of the inner chamber body 104 and electrically coupled to the power supply 128. In Figure 1 In the example of FIG. 1 , the heating elements 128A are shown as two pairs of heating elements 128A disposed in or coupled to the chamber wall 122, one pair of heating elements 128A disposed in or coupled to the substrate support pedestal 106, and one pair of heating elements 128A disposed in or coupled to the chamber lid 108. In alternative embodiments, different from Figure 1More or fewer heating elements 128A as shown may be used in various configurations in the chamber wall 122, in the chamber lid 108, and in some embodiments, within or coupled to the substrate support pedestal 106. In an etching example in the processing chamber 100, chemically reactive ions are released from a plasma, which may be introduced via the RPS 112 or formed in the processing chamber 100 via other means as discussed below. Once released from the plasma, the chemically reactive ions impact a substrate 146 positioned on the substrate support pedestal 106. When the chemically reactive ions impact the substrate, exposed material from the surface of the substrate 146 is removed.
[0014] In another example of the processing chamber 100, a plasma may be generated using an RF source power 140 and an RF bias power 142. Each of the RF source power 140 and the RF bias power 142 is coupled to the processing chamber 100 and configured to apply power (and in some examples, power pulses) to the chamber walls 122 and / or the substrate support pedestal 106. In some examples, a negative bias may also be applied to the substrate support pedestal 106. In one example, a gaseous mixture formed by a gas source (not shown) coupled to the gas panel 118 within the processing volume 134 is ignited into a plasma by applying RF power from the RF source power 140 to a plurality of antenna segments (not shown).
[0015] In addition, in the processing chamber 100, a showerhead 110 is removably coupled to the processing chamber 100 near the chamber top 108A. The showerhead 110 is used to distribute a plurality of gases, for example, gases supplied through the gas panel 118, in the inner chamber body 104. The showerhead 110 can be used to distribute gases and gas mixtures during substrate processing operations, and during the deposition and removal of protective films discussed herein, or other cleaning operations performed inside the processing chamber 100. The showerhead 110 may include a plurality of islands 126 and a plurality of spaces 144 formed between each adjacent pair of islands 126. The islands 126 are connected (not shown here) so that the gas flows through the showerhead 110 and enters the processing space 134, and specifically, the gas flows through the showerhead 110 between the spaces 144 and enters the processing space 134. Thus, when the protective film 120 is formed as discussed herein, since the showerhead 110 is used to form the protective film 120, the protective film is formed on the surface of the showerhead 110 that is exposed to the gaseous component used to form the protective film 120. The protective film 120 is also formed on the exposed surfaces of the inner chamber body 104, including the chamber wall 122. In some examples that may be combined with other examples herein, one or more of the chamber top 108A, the substrate support pedestal 106, and the chamber bottom 124, as well as any other exposed surface, may also have the protective film 120 formed thereon.
[0016] In one embodiment, the controller 130 is coupled to the processing chamber 100 and is configured to execute a plurality of instructions. In one example, the plurality of instructions executed by the controller 130 are associated with substrate processing. The substrate processing may include operations such as layer deposition and patterning, as well as chamber cleaning. In another example, the plurality of instructions executed by the controller 130 are associated with forming a protective film 120 on one or more of the chamber walls 122, the bottom 124, the top 108A, the substrate support pedestal 106, or other exposed surfaces of the inner chamber body 104. In one embodiment, a protective cover (not shown) may be positioned on the substrate support pedestal 106 that covers some or all of the diameter 106A of the substrate support pedestal 106. Thus, optionally, a portion of the substrate support pedestal 106 (shown as an uncoated area 106B in this example) is not coated with the protective film 120 and remains exposed. The protective film 120 may also be formed on the showerhead 110 and may be formed to an average thickness of from 80 nm to 250 nm or from 90 nm to 120 nm. In some examples, the average thickness of the protective film 120 is about 100 nm. In an alternative example that may be combined with other examples herein, a protective cap is not used and the area indicated by the diameter 106A is coated with the protective film 120.
[0017] During operation of the processing chamber 100, after the protective film 120 is formed, the substrate 146 is placed on the substrate support pedestal 106 in the uncoated area 106B of the substrate support pedestal 106. Gaseous components are supplied to the processing chamber 100 from the gas panel 118 through the plurality of islands 126 of the showerhead 110, which serve as inlet ports for the gas. One or more gaseous components are supplied from the gas panel 118 simultaneously, or in an alternating and / or iterative manner, to form a gaseous mixture in the processing space 134. The protective film 120 may be removed by forming a F or NF3 plasma in the processing chamber 100 (or introducing a plasma via the RPS 112), through the showerhead 110 to remove the protective film 120. Removal of the protective film 120 may occur after one or more cycles in the processing chamber, for example, after one or more films (not shown here) are formed on the substrate 146, or after forming a plurality of films, or after patterning a plurality of films, or a combination of the foregoing.
[0018] In one embodiment, the temperature of a substrate 146 positioned in a processing chamber 100 is controlled by stabilizing the temperature of a substrate support pedestal 106 during processing of the substrate 146. Helium or another gas from a gas panel 118 flows into a plenum (not shown) defined between the substrate 146 and a support surface 106C of the substrate support pedestal 106. The substrate 146 is seated in an uncoated area 106B. The helium gas is used to facilitate heat transfer between the substrate 146 and the substrate support pedestal 106. During processing in the processing chamber 100, which may include an etching process, the substrate 146 is gradually heated by the plasma to a steady-state temperature between 200° C. and 600° C. Using temperature control of both the chamber top 108A and the substrate support pedestal 106, and in some cases, the chamber wall 122, the substrate 146 is maintained at a predetermined temperature during processing. When the processing chamber 100 is used at high temperatures and / or pressures, the inner chamber body 104 is exposed to a harsh environment. The presence of etching gases in the processing chamber 100 further provides a harsh environment to which the inner chamber body 104 is subjected. The protective film 120 thus protects the inner chamber body 104 from degradation of one or more of the chamber top 108A, chamber bottom 124, chamber walls 122, showerhead 110, or substrate support pedestal 106.
[0019] Figure 2 is similar to Figure 1 A method 200 for in-situ forming a protective film such as a protective film 120 in a processing chamber of a processing chamber 100 is disclosed. In the method 200, at operation 202, the processing chamber is prepared for in-situ protective film formation. The preparation of the processing chamber at operation 202 may include heating the processing chamber to a temperature from about 300° C. to about 600° C. and establishing a vacuum between an outer chamber body and an inner chamber body using, for example, N2. The preparation at operation 202 may further include establishing a pressure from about 1 Torr to about 600 Torr in the inner chamber body. The preparation at operation 202 may be performed while maintaining a vacuum between the inner chamber body and the outer chamber body.
[0020] At operation 204, after preparing the process chamber at operation 202, a protective film is formed on a plurality of internal components (which may alternatively be referred to as exposed surfaces) of the process chamber. The protective film is formed at operation 204 to a target thickness, which may be from 80 nm to 250 nm, using precursors discussed below. The internal components include at least one of a substrate support base, an internal chamber body wall, a top, a bottom, and a showerhead feature, such as Figure 1As discussed in . In one example, the protective film formed in operation 204 is formed using chemical vapor deposition (CVD). In another example, the protective film formed in operation 204 is formed using atomic layer deposition (ALD). In one embodiment, whether CVD or ALD is used in operation 204, the processing chamber is at a pressure of from 2 Torr to 30 Torr. In another example that may be combined with other examples herein, the temperature of the processing chamber in operation 204 is from 250° C. to 750° C. In yet another example that may be combined with other examples herein, one or more gases such as Si2H6, SiH4, N2, N2O, NH3, Ar, or H2 are present in the processing chamber in operation 204. In an example of using ALD in operation 204, ALD precursors tetrakis(ethylmethylamido)hafnium(IV) (TEMAH) and aluminum trimethanide (TMA) and one or more precursors are used in an ALD chamber to form a protective film having a composition of Al2O3, AlON, HfO2, or Ni3Al. In another embodiment, the protective film formed by ALD in operation 204 is a composition including one or more of amorphous Si, carbosilane, polysilicon, SiC, SiN, or SiO2.
[0021] The protective film formed in operation 204 may be formed to an average thickness of from 80 nm to 250 nm. Operations 202 and 204 are performed without a substrate positioned in a processing chamber. In operation 206, a substrate or a batch of substrates (2 or more substrates) is positioned in a processing chamber and then the substrate is processed in operation 208. The substrate positioned in the processing chamber may be positioned on a substrate support pedestal. In one embodiment, processing the substrate in operation 208 includes forming a plurality of features in the substrate. During the processing of operation 208, the temperature of the processing chamber may be from about 200° C. to about 600° C. or higher, and the pressure of the processing chamber may be from 1 bar to about 250 bar.
[0022] After processing at operation 208, the substrate is removed from the processing chamber at operation 210. In one embodiment, after the substrate is removed at operation 210, the protective film formed at operation 204 is removed at operation 212. The removal of the film may be performed at operation 212 using a fluorine-containing plasma or other suitable cleaning agent. A showerhead of the processing chamber may be used to dispense these components. During the removal of the film at operation 212, the processing chamber may be purged with an inert gas after using the cleaning agent. The protective film protects the interior of the processing chamber from corrosion, which, during processing operations such as those of operation 208, not only degrades the overall components of the processing chamber from a performance perspective. However, the protective film may also pose a risk of contamination during substrate processing, for example, if portions of the film peel off or fall onto the substrate. The film formed at operation 204 may thus be formed and removed after each substrate or batch of substrates are processed at operation 208. Using the systems and methods discussed herein, protective films of different compositions and thicknesses may be formed on the same chamber components. In one embodiment, more than one substrate or a batch of substrates may be processed and removed during operations 208 - 210 prior to removing the film at operation 212 .
[0023] In-situ coating of an apparatus or device such as the processing chamber discussed herein is used herein to provide a uniform thickness of protective coating from within a processing chamber. In some examples, the protective coating discussed herein may be formed on internal components of a processing chamber for high pressure applications of 1 bar or more. Unlike ex-situ coating, ex-situ coating may flake or fall off the coated components for corrosive, high pressure applications. Deterioration of this protective coating may result in frequent re-coating operations.
[0024] While the foregoing is directed to embodiments of the present disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope of the disclosure, and the scope of the disclosure is determined by the appended claims.
Claims
1. A method for processing a substrate, comprising: introducing at least one gas into the processing chamber; removing a first protective film from a plurality of internal components of the processing chamber in response to the introduction of the at least one gas into the processing chamber; forming a second protective film on the plurality of internal components in the processing chamber via ALD or CVD, the internal components including chamber sidewalls, chamber bottom, substrate support pedestal, showerhead, and chamber top, wherein the second protective film and the first protective film are composed of the same material, and the first protective film and the second protective film include Al2O3, AlON, HfO2, or Ni3Al; and After forming the second protective film, a substrate is positioned on the substrate supporting pedestal, wherein the substrate is in contact with a portion of the substrate supporting pedestal that does not include the second protective film.
2. The method of claim 1, further comprising: Prior to the formation of the second protective film, the process chamber is heated to a preheating temperature from 300° C. to 600° C., wherein the formation of the second protective film occurs when the process chamber is at the preheating temperature.
3. The method of claim 1, further comprising: Prior to forming the second protective film, the process chamber is pressurized to a pressure ranging from 1 Torr to 600 Torr.
4. The method of claim 1, further comprising: Prior to positioning the substrate on the substrate support pedestal, a process temperature of the process chamber is set to from 200°C to 600°C.
5. The method of claim 4, further comprising: performing at least one operation in the processing chamber after positioning the substrate; Thereafter, removing the substrate from the processing chamber; and The process chamber is cleaned, wherein the step of cleaning the process chamber removes the second protective film from the plurality of internal components of the process chamber.
6. The method of claim 5, further comprising: The second protective film is removed from the plurality of internal components of the processing chamber using fluorine-containing plasma.
7. A method for protecting a processing chamber, comprising: introducing at least one gas into the processing chamber; removing a first protective film from a plurality of internal components of the processing chamber in response to the introduction of the at least one gas into the processing chamber; forming a second protective film on the plurality of internal components via ALD or CVD in the processing chamber, wherein the first protective film and the second protective film are composed of the same material, the first protective film and the second protective film comprising Al2O3, AloN, Hfo2, or Ni3Al; and After forming the second protective film, the substrate is positioned on a substrate supporting pedestal.
8. The method of claim 7, further comprising: The second protective film is formed to a thickness of from 80 nm to 250 nm.
9. The method of claim 7, further comprising: Prior to forming the second protective film, a cover is positioned on at least a portion of the substrate supporting pedestal such that the second protective film is not formed on the portion of the substrate supporting pedestal.
10. The method of claim 7, further comprising: Prior to forming the second protective film, the processing chamber is heated to a preheating temperature from 300° C. to 600° C., wherein forming the second protective film occurs when the processing chamber is at the preheating temperature.
11. A method for processing a substrate, comprising: introducing at least one gas into the processing chamber; removing a first protective film from a plurality of internal components of the processing chamber in response to the introduction of the at least one gas into the processing chamber; forming a second protective film on the plurality of internal components in the processing chamber via ALD or CVD, the internal components including chamber sidewalls, chamber bottom, substrate support pedestal, showerhead, and chamber top, wherein the first protective film and the second protective film are composed of the same material, the first protective film and the second protective film include Al2O3, AlON, HfO2, or Ni3Al; and After forming the second protective film, positioning a substrate on the substrate supporting pedestal, wherein the second protective film is not formed on a portion of the substrate supporting pedestal, and the substrate contacts the portion of the substrate supporting pedestal that does not include the second protective film.
12. The method of claim 11, further comprising: Prior to forming the second protective film, the processing chamber is heated to a preheating temperature from 300° C. to 600° C., wherein forming the second protective film occurs when the processing chamber is at the preheating temperature.
13. The method of claim 11, further comprising: Prior to positioning the substrate on the substrate support pedestal, a process temperature of the process chamber is set to from 200°C to 600°C.
14. The method of claim 7, wherein the plurality of internal components of the processing chamber comprise stainless steel.
15. The method of claim 7, wherein the at least one gas comprises fluorine.
16. The method of claim 11, further comprising: Before forming the second protection film, the processing chamber is pressurized to from 1 Torr to 600 Torr.
17. The method of claim 11, wherein a process pressure of the chamber is from 1 bar to 250 bar prior to positioning the substrate on the substrate support pedestal.