A four-corner single-side dovetail groove tile back mold core and the tile made thereof

By designing a four-corner single-sided dovetail groove tile back mold core, the problem of uneven tile back texture density is solved by utilizing the expansion and deformation of the tile body during demolding, achieving a back texture with uniform depth and high bonding strength.

CN112248197BActive Publication Date: 2024-11-19陈锐
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011323506.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-11-23
Publication Date
2024-11-19
Estimated Expiration
2040-11-23

AI Technical Summary

Technical Problem

In existing tile production processes, the back texture structure of tiles leads to uneven density, resulting in problems such as sintering through to the bottom and insufficient bonding strength.

Method used

The back mold core of the ceramic tile adopts a four-corner single-sided dovetail groove design. The single-sided dovetail groove convex pattern is located at the four corners of the back mold core. The convex pattern forms an obtuse angle and an acute angle structure with the back mold core plane. By utilizing the expansion and deformation characteristics of the ceramic tile body during demolding, a deep and symmetrical dovetail groove back pattern is formed.

Benefits of technology

It improves the depth and flatness of the tile's back texture, enhances adhesive strength, prevents detachment, forms a rigid mortise and tenon structure, and improves the tile's safety performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112248197B_ABST
    Figure CN112248197B_ABST
Patent Text Reader

Abstract

A four-corner single-sided dovetail groove ceramic tile back mold core, the surface of the back mold core vulcanized rubber includes convex and concave patterns that are integrally formed and pasted on the iron substrate of the back mold core, the single-sided dovetail groove convex patterns of the ceramic tile back mold core are located at the four corners of the ceramic tile back mold core, the single-sided dovetail groove convex patterns are grid patterns or stripes, the side of the single-sided dovetail groove convex pattern close to the center of the back mold core forms an obtuse angle with the plane of the back mold core, and the side far from the center of the back mold core forms an acute angle with the plane of the back mold core; during the pressing process of the ceramic tile blank, the acute angle of the convex pattern far from the center forms a single-sided dovetail groove on the ceramic tile back pattern, and during the demolding link of the ceramic tile blank, the outward deformation movement of the ceramic tile blank when releasing self-stress is utilized, and the single-sided dovetail groove formed by the ceramic tile blank moves laterally away from the acute angle of the convex pattern so as to be demolded smoothly; a four-corner single-sided dovetail groove back pattern ceramic tile, the four corner areas of the ceramic tile are single-sided dovetail groove concave patterns with grid patterns or stripes, and each grid pattern or each stripe has a pattern side with an inverted acute angle that is less than 1 / 2 of the pattern circumference.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of ceramic production, and more specifically, to a ceramic tile back mold core with four-corner single-side dovetail grooves and a ceramic tile made therefrom. Background Art

[0002] In the existing ceramic tile production process, the ceramic tile embryo is formed by powder through ultra-high pressure pressing. The ceramic tile embryo is molded by mechanical equipment with fixed upper and lower molds. In order to increase the bonding area, various patterns of back patterns are arranged on the back of the ceramic tile. In the existing ceramic tile back mold core process, especially in molds with a size of more than 300*300mm, most of them are checkered patterns, arc-shaped broom patterns, random patterns, convex dot patterns, etc. The common point of all existing back mold cores is that the connecting edges between the convex patterns and the concave patterns have a positive demoulding slope, that is, the upper mouth of the convex pattern is smaller than the lower mouth and the center lines of the upper and lower mouths coincide. This structural structure determines that an effective dovetail groove cannot be formed.

[0003] During the pressing process of the tile body, the thickness of the pressed body is generally 35%~40% of the thickness of the arranged powder. The height difference between the convex and concave patterns on the back pattern of the tile back mold core leads to different density of the tile body at the corresponding position. The tile body with different density shrinks at different rates during sintering, resulting in insufficient flatness of the tile surface and defective products with sintered bottom. The tile has to reduce the depth of the back pattern and reduce the bonding strength.

[0004] During the pressing process of the tile blank, when the tile blank is pressed and formed, it is pressed by the upper and lower dies on six sides in the mold cavity. At the final pressing, the tile blank has the same internal stress of the reaction force. In the demolding process of the tile blank, especially for the demolding of tiles with a size of 300*300mm or more, the upper and lower dies clamp the formed tile blank and float out of the lower mold cavity first. At this time, the pressure on the four sides of the tile blank is released first, and the volume of the tile blank expands to the four sides to release the internal stress. As the upper die is further lifted upward, the whole tile blank expands evenly to release the internal stress. The side length of the expanded tile blank increases by about 0.5%-1.5%. The tile blank after expansion and enlargement no longer matches the back pattern of the tile back mold core. When expanded and deformed, the tile blank slides from the center from the inside to the outside along the demolding slope position of the back mold core back pattern and is demolded. Summary of the invention

[0005] The problem to be solved by the present invention is to prevent the phenomenon of ceramic tiles being sintered through during the production of ceramic tile blanks, to make the pressed ceramic tiles have a sufficiently deep back pattern and a dovetail groove structure, to make full use of the characteristic of the ceramic tiles expanding and deforming when demolding, and to provide a four-corner single-sided dovetail groove ceramic tile back mold core; and to use the four-corner single-sided dovetail groove ceramic tile back mold core of the present invention to make a four-corner single-sided dovetail groove back pattern ceramic tile.

[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a four-corner single-sided dovetail groove ceramic tile back mold core, comprising a back mold core iron matrix and a vulcanized rubber on the back mold core surface, wherein the vulcanized rubber on the back mold core surface comprises convex patterns and concave patterns integrally formed and pasted on the back mold core iron matrix, wherein the single-sided dovetail groove convex patterns of the ceramic tile back mold core are located at the four corners of the ceramic tile back mold core, the single-sided dovetail groove convex patterns are lattice patterns or stripes, the side of the single-sided dovetail groove convex patterns close to the back mold core center forms an obtuse angle with the back mold core plane, and the side far from the back mold core center forms an acute angle with the back mold core plane;

[0007] When the convex pattern of the single-sided dovetail groove is a checkered pattern, it is a two-step convex pattern. The first-level flat step with a height of 0.5mm~1.0mm is raised based on the concave pattern of the back mold core. The second-level step is raised 0.3mm~3mm from the first-level flat step and the width of the top plane of the step is less than 1mm. The riser of the formed step forms an obtuse angle of 110 degrees to 150 degrees with the plane of the back mold core on the side close to the center of the back mold core; the side of the convex pattern of the single-sided dovetail groove far from the center of the back mold core forms an acute angle of 55 degrees to 89 degrees with the plane of the back mold core from the top of the second step to the concave pattern surface;

[0008] When the convex pattern of the single-sided dovetail groove is a stripe, it is a first-level step convex pattern. The side close to the center of the back mold core forms a slope or arc slope at 110 degrees to 150 degrees from the concave surface to form a step with a height of 1mm to 5mm, and the plane width of the top of the step is less than 1mm. The side of the convex pattern of the single-sided dovetail groove far from the center of the back mold core forms an acute angle of 55 to 89 degrees from the top of the step to the concave surface.

[0009] A four-corner single-sided dovetail groove ceramic tile back mold core, wherein the single-sided dovetail groove convex pattern of the ceramic tile back mold core is located at the four corners outside the back mold core center radius of 100mm and outside the 5mm width of the central vertical line of the four sides, and other patterns except the single-sided dovetail groove convex pattern are checkered or striped patterns with a height of 0.5mm~1.2mm and an obtuse angle of 110 degrees to 150 degrees formed with the back mold core plane on all sides.

[0010] A four-corner single-sided dovetail groove ceramic tile back mold core, wherein an isostatic layer can be arranged between the back mold core iron matrix and the vulcanized rubber on the back mold core surface; an exhaust system can be arranged between the back mold core iron matrix and the vulcanized rubber on the back mold core surface, the exhaust port is located at the obtuse slope surface of the convex pattern of the single-sided dovetail groove or the first-level step plane of the lattice pattern, and the exhaust pipe is located in the back mold core iron matrix.

[0011] A four-corner single-sided dovetail groove back-patterned ceramic tile can be obtained by producing a four-corner single-sided dovetail groove ceramic tile back mold core using the technology of the present invention, wherein the four corner areas of the ceramic tile are single-sided dovetail groove concave patterns with grids or stripes, each grid or each stripe has a grain side with a chamfered acute angle that is less than 1 / 2 of the grain circumference, the grain side with the chamfered acute angle forms an angle of 55 to 89 degrees with the back plane of the ceramic tile, and the grain side of the remaining part except the chamfered acute angle forms an angle of 110 to 150 degrees with the back plane of the ceramic tile.

[0012] The invention provides a four-corner single-sided dovetail groove ceramic tile back mold core and a ceramic tile made thereof. The four-corner single-sided dovetail groove ceramic tile back mold core has a vulcanized rubber on the surface of the back mold core, including convex patterns and concave patterns, which are integrally formed and pasted on the iron substrate of the back mold core. The convex patterns of the single-sided dovetail groove of the ceramic tile back mold core are located at the four corners of the ceramic tile back mold core. The convex patterns of the single-sided dovetail groove are lattice patterns or stripes. The side of the convex patterns of the single-sided dovetail groove close to the center of the back mold core forms an obtuse angle with the plane of the back mold core, and the side far from the center of the back mold core forms an acute angle with the plane of the back mold core. During the pressing process of the tile body, the acute angle of the convex pattern far from the center forms a single-sided dovetail groove on the back pattern of the tile. During the demolding process of the tile body, the outward deformation movement of the tile body when releasing self-stress is utilized, and the single-sided dovetail groove formed by the tile body moves laterally away from the acute angle of the convex pattern, thereby smoothly demolding. A four-corner single-sided dovetail groove back pattern tile, the four corner areas of the tile are single-sided dovetail groove concave patterns with grids or stripes, and each grid or each stripe has a pattern side with an inverted acute angle that is less than 1 / 2 of the pattern circumference.

[0013] Compared with the prior art, the four-corner single-sided dovetail groove ceramic tile back mold core and the ceramic tile made by implementing the present invention have the following beneficial effects: simple and firm structure, the four-corner single-sided dovetail groove convex pattern is integrally formed and covered on the back mold core iron matrix by vulcanization molding; it is convenient to further optimize the addition of isostatic pressing system and exhaust system; the produced ceramic tiles have deep back patterns and smooth surfaces, the formed single-sided dovetail groove back patterns are centrally symmetrical or axially symmetrical, and the symmetrical patterns form double-sided dovetail grooves with excellent structural strength; after the ceramic tiles are pasted, a rigid mortise and tenon structure is formed with the adhesive layer to prevent the ceramic tiles from falling off, thereby greatly improving the safety performance of the ceramic tiles. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a plan view of the single-sided dovetail groove lattice back mold core of the present invention.

[0015] Figure 2 It is a plan view of the single-sided dovetail groove stripe back mold core of the present invention.

[0016] Figure 3 This is a partial large-scale diagram A of the checkered back mold core of the present invention.

[0017] Figure 4 It is a CC cross-sectional view of the local large-scale drawing A of the present invention.

[0018] Figure 5 This is the striped back mold core pattern B of the present invention.

[0019] Figure 6 It is a DD cross-sectional view of the local large-scale drawing B of the present invention.

[0020] Figure 7 It is a plan view of another single-sided dovetail groove stripe mold core of the present invention.

[0021] Among them: 1. The second step of the single-sided dovetail groove grid pattern; 101. The chamfered sharp edge of the single-sided dovetail groove grid pattern; 102. The obtuse bevel of the second step of the single-sided dovetail groove grid pattern; 2. The first step of the single-sided dovetail groove grid pattern; 201. The obtuse bevel of the first step of the single-sided dovetail groove grid pattern; 3. The traditional convex grid pattern of the back mold core; 4. The concave pattern of the back mold core; 5. The cutting edge of the iron matrix of the back mold core; 6. The vertical line of the center of the four sides of the back mold core; 7. The stripes of the single-sided dovetail groove; 701. The chamfered sharp edge of the stripes of the single-sided dovetail groove; 702. The obtuse bevel of the stripes of the single-sided dovetail groove; 8. The traditional convex stripes of the back mold core; 9. The iron matrix of the back mold core. DETAILED DESCRIPTION

[0022] The technical solution of the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0023] like Figure 1-7 As shown, a four-corner single-sided dovetail groove ceramic tile back mold core comprises a back mold core iron substrate 9 and a vulcanized rubber on the back mold core surface, wherein the vulcanized rubber on the back mold core surface comprises convex patterns and concave patterns integrally formed and pasted on the back mold core iron substrate, wherein the single-sided dovetail groove convex patterns of the ceramic tile back mold core are located at the four corners of the ceramic tile back mold core, the single-sided dovetail groove convex patterns are checkered or striped, the side of the single-sided dovetail groove convex patterns close to the center of the back mold core forms an obtuse angle with the plane of the back mold core, and the side far from the center of the back mold core forms an acute angle with the plane of the back mold core.

[0024] There are two types of convex patterns on the single-sided dovetail groove: checkered or striped. One of them is a two-step convex pattern when the convex pattern of the single-sided dovetail groove is a checkered pattern. The first-level flat step with a height of 0.5mm~1.0mm is raised based on the concave pattern of the back mold core. This step is the first-level step 2 of the single-sided dovetail groove checkered pattern. The second-level step is the second-level step 1 of the single-sided dovetail groove checkered pattern, which is raised 0.3mm~3mm from the first-level step 2 of the single-sided dovetail groove checkered pattern and the width of the top plane of the step is less than 1mm. The stepped riser forms an obtuse angle of 110 to 150 degrees with the plane of the back mold core on the side close to the center of the back mold core, the riser formed by the first step is the obtuse angle bevel 201 of the first step of the single-sided dovetail groove lattice, and the riser formed by the second step is the obtuse angle bevel 102 of the second step of the single-sided dovetail groove lattice; the side of the single-sided dovetail groove convex pattern far from the back mold core center forms an acute angle of 55 to 89 degrees from the top of the second step to the concave surface, and this side is the chamfered acute angle edge 101 of the single-sided dovetail groove lattice.

[0025] Another type of single-sided dovetail groove convex pattern, when the single-sided dovetail groove convex pattern is a stripe, the single-sided dovetail groove convex pattern with a stripe is a first-level step convex pattern, and the step convex pattern is a single-sided dovetail groove stripe 7. The side close to the center of the back mold core forms a slope or arc slope at 110 degrees to 150 degrees from the concave surface, and the step height is 1mm to 5mm, and the plane width of the top of the step is less than 1mm. The slope or arc slope formed on this side is the obtuse angle bevel 702 of the single-sided dovetail groove stripe, and the side of the single-sided dovetail groove convex pattern far from the back mold core center forms an acute angle of 55 to 89 degrees from the top of the step to the concave surface, and this side is the single-sided dovetail groove stripe inverted acute angle edge 701.

[0026] A four-corner single-sided dovetail groove ceramic tile back mold core, wherein the single-sided dovetail groove convex pattern of the ceramic tile back mold core is located in the four corner areas outside the back mold core center radius of 100mm and outside the 5mm width of the central vertical line of the four sides, the central vertical line of the four sides is the central vertical line 6 of the four sides of the back mold core, and the other patterns except the single-sided dovetail groove convex pattern are grid patterns or stripes with a height of 0.5mm~1.2mm and an obtuse angle of 110 degrees to 150 degrees formed with the plane of the back mold core on all sides, wherein the grid pattern is the traditional convex grid pattern 3 of the back mold core and the stripes are the traditional convex stripes 8 of the back mold core.

[0027] A four-corner single-sided dovetail groove ceramic tile back mold core, wherein an isostatic layer can be arranged between the back mold core iron matrix 9 and the vulcanized rubber on the back mold core surface; an exhaust system can be arranged between the back mold core iron matrix 9 and the vulcanized rubber on the back mold core surface, the exhaust port is located at the obtuse slope surface of the convex pattern of the single-sided dovetail groove or the first-level step plane of the lattice pattern, and the exhaust pipe is located inside the back mold core iron matrix 9.

[0028] A four-corner single-sided dovetail groove back-patterned ceramic tile can be obtained by producing a four-corner single-sided dovetail groove ceramic tile back mold core using the technology of the present invention, wherein the four corner areas of the ceramic tile are single-sided dovetail groove concave patterns with grids or stripes, each grid or each stripe has a grain side with a chamfered acute angle that is less than 1 / 2 of the grain circumference, the grain side with the chamfered acute angle forms an angle of 55 to 89 degrees with the back plane of the ceramic tile, and the grain side of the remaining part except the chamfered acute angle forms an angle of 110 to 150 degrees with the back plane of the ceramic tile.

[0029] A processing and manufacturing method for a back mold core of a four-corner single-sided dovetail groove tile comprises a back mold core iron substrate 9 and a vulcanized rubber on the surface of the back mold core. First, according to the back pattern and shape of the designed back mold core of the four-corner single-sided dovetail groove tile, the same convex pattern is carved on an aluminum plate by a CNC machine tool. The outer side length of the aluminum plate is 4mm larger than the designed back mold core. The completed aluminum mold is called a mother mold I. Another iron plate or aluminum plate is prepared, the outer side length of which is 2mm smaller than the mother mold I. After leaving a cutting edge of about 1.3mm on all sides, a groove with a depth of 2-6mm is milled on the front panel, and the groove is sandblasted. , apply primer, pour liquid polyurethane glue and cover with mother mold I coated with release agent, close the mold, heat and vulcanize, demould the mother mold I to obtain mother mold II; the front surface of the back mold core iron matrix 9 is processed into an inner groove with a cutting edge of 0.2mm~0.8mm thickness on all sides, the cutting edge is the cutting edge 5 of the back mold core iron matrix, the surface of the inner groove is sandblasted, coated with primer, poured with liquid polyurethane glue and then covered with mother mold II coated with release agent, close the mold, heat and vulcanize, demould the mother mold II to obtain a four-corner single-sided dovetail groove tile back mold core as required by the design.

[0030] The working process and working principle of a four-corner single-sided dovetail groove tile back mold core are supplemented, and the reverse-hitting process with the surface mold core at the bottom is used as an example. Before work, the surface mold core descends to the feeding height in the lower mold cavity, and the tile powder is spread and scraped flat. The press machine presses the four-corner single-sided dovetail groove tile back mold core into the lower mold cavity, and squeezes the tile powder to obtain a compacted tile body. After the pressure is applied, the four-corner single-sided dovetail groove tile back mold core and the surface mold core sandwich the tile body and rise to the upper plane of the lower mold cavity. At this time, the pressure constraints on the four sides of the tile body disappear, and the tile body begins to expand and deform on all sides to release internal stress. Then, with the further lifting of the four-corner single-sided dovetail groove tile back mold core, the upper and lower pressure constraints disappear, and the tile body further deforms and expands to release internal stress. Practical tests show that after the tile body is fully expanded and the pressure is released, the side length is about 0.8% longer than the side length in the lower mold cavity, and most of them are between 0.5% and 1.5%. Different powders have different The expansion rates of pressure processes are different. The expansion of the tile body is based on the center of the tile body and extends to the surrounding areas with the same expansion rate. The center of the tile body expands less, and the expansion increases as it goes outward. When the tile body expands and deforms, due to the structural characteristics of the four-corner single-sided dovetail groove tile back mold core: the side of the single-sided dovetail groove convex pattern close to the center of the back mold core forms an obtuse angle with the back mold core plane and the side far from the center of the back mold core forms an acute angle with the back mold core plane, and the obtuse angle is 110~150 degrees. Due to the interaction with the obtuse angle, when the tile body expands and deforms, it moves horizontally and longitudinally at the same time to lift the tile body out of the back mold core. The convex pattern on the other side is an acute angle of 55~89 degrees to form a single-sided dovetail groove. It leaves the suspension during expansion movement, effectively protecting the single-sided dovetail groove formed by the tile body. Furthermore, in the reverse punching process, the four-corner single-sided dovetail groove tile back mold core and the tile body are smoothly demolded due to the self-weight of the tile body.

[0031] The single-sided dovetail groove back pattern is applied to the four corners of the back mold core, making full use of the position with larger deformation amount. In the grid dovetail groove convex pattern, the grid pattern includes triangles, quadrilaterals, polygons and other polygons, and also includes circular, random convex irregular convex patterns, but the obtuse bevel edge 102 of the second step of the single-sided dovetail groove grid pattern and the single-sided dovetail groove grid pattern chamfered sharp edge 101 must be on the side far from the center of the tile back mold core and cannot exceed half of the convex pattern; when using single-sided dovetail groove stripes, the shape can be straight, C-shaped, L-shaped, S-shaped and other shapes, but the side dovetail groove grid pattern chamfered sharp edge 101 must be on the side far from the center of the tile back mold core and cannot exceed half of the convex pattern; and in the central part of the back mold core and the central vertical line position of the four sides, although the expansion rate of the tile blank is consistent with the four corners, the deformation is relatively small, so except for the four corners, the traditional back mold core traditional convex grid pattern 3 or the back mold core traditional convex stripe 8 is retained.

[0032] A four-corner single-sided dovetail groove back-patterned ceramic tile can be obtained by producing a four-corner single-sided dovetail groove ceramic tile back mold core using the technology of the present invention, wherein the four corner areas of the ceramic tile are single-sided dovetail groove concave patterns with grids or stripes, each grid or each stripe has a grain side with a chamfered acute angle that is less than 1 / 2 of the grain circumference, the grain side with the chamfered acute angle forms an angle of 55 to 89 degrees with the back plane of the ceramic tile, and the grain side of the remaining part except the chamfered acute angle forms an angle of 110 to 150 degrees with the back plane of the ceramic tile.

[0033] Combined with the existing traditional technology of ceramic tile mold back mold core, the ceramic tile back mold core with four corners and single side dovetail groove of the present invention is particularly suitable for ceramic tiles with a size of 300*300 and above. It can also add an exhaust system and an isostatic pressure layer according to the requirements of specific tiles, change the back pattern characteristics of traditional ceramic tile back mold core, and make full use of the deformation movement of the ceramic tile blank when releasing the internal stress during demolding, so that the ceramic tile forms a four-corner single side dovetail groove back pattern, and the back pattern of the whole tile is a centrally symmetrical or axially symmetrical geometric pattern. After pasting, it forms a rigid mortise and tenon structure of a rigid double-sided dovetail groove with the hardened adhesive layer, which greatly improves the safety performance of ceramic tile pasting and can produce unexpected industrial effects.

[0034] For those skilled in the art, various other corresponding changes and deformations can be made according to the technical solutions and concepts described above, and all of these changes and deformations should fall within the scope of protection of the patent claims of the present invention.

Claims

1. A four-corner single-side dovetail groove ceramic tile back mold core, comprising a back mold core iron matrix and a back mold core surface vulcanized rubber, the back mold core surface vulcanized rubber including convex and concave patterns integrally formed and pasted on the back mold core iron matrix, characterized in that: The single-sided dovetail groove convex pattern of the ceramic tile back mold core is located at the four corners of the ceramic tile back mold core, the single-sided dovetail groove convex pattern is a checkered pattern or a stripe, the side of the single-sided dovetail groove convex pattern close to the back mold core center forms an obtuse angle with the back mold core plane and the side far from the back mold core center forms an acute angle with the back mold core plane; When the unilateral dovetail groove convex pattern is a checkered pattern, it is a two-stage step convex pattern, with the first-stage plane step raised by 0.5mm~1.0mm in height based on the concave pattern of the back mold core, the second-stage step is raised by 0.3mm~3mm from the first-stage plane step and the plane width of the top of the step is less than 1mm, and the riser of the formed step forms an obtuse angle of 110 degrees to 150 degrees with the plane of the back mold core on the side close to the center of the back mold core; the side of the unilateral dovetail groove convex pattern far from the center of the back mold core forms an acute angle of 55 degrees to 89 degrees with the plane of the back mold core from the top of the second-stage step to the concave pattern surface; The single-sided dovetail groove convex pattern is a first-level step convex pattern when it is a stripe. The side close to the center of the back mold core forms a slope or arc slope at 110 degrees to 150 degrees from the concave surface to form a step with a height of 1mm to 5mm, and the plane width of the top of the step is less than 1mm. The side of the single-sided dovetail groove convex pattern far from the center of the back mold core forms an acute angle of 55 to 89 degrees from the top of the step to the concave surface.

2. A four-corner single-side dovetail groove ceramic tile back mold core according to claim 1, characterized in that: The single-sided dovetail groove convex pattern of the tile back mold core is located outside the center radius of 100mm of the back mold core and the four corner areas outside the 5mm width of the central vertical line of the four sides. Except for the single-sided dovetail groove convex pattern, the other patterns are checkered or stripes with a height of 0.5mm~1.2mm and an obtuse angle of 110 degrees to 150 degrees formed with the plane of the back mold core.

3. A four-corner single-side dovetail groove ceramic tile back mold core according to claim 1, characterized in that: An isostatic layer can be arranged between the back mold core iron matrix and the vulcanized rubber on the back mold core surface; an exhaust system can be arranged between the back mold core iron matrix and the vulcanized rubber on the back mold core surface, the exhaust port is located at the obtuse slope surface of the convex pattern of the single-sided dovetail groove or the first-level step plane of the lattice pattern, and the exhaust pipe is located in the back mold core iron matrix.

4. A four-corner single-side dovetail groove back pattern tile, characterized in that: It is formed by pressing a four-corner single-sided dovetail groove ceramic tile back mold core as described in any one of claims 1-3, and the four corner areas of the ceramic tile are single-sided dovetail groove concave patterns with grids or stripes, and each grid or each stripe has a grain side with a chamfered acute angle less than 1 / 2 of the grain circumference, and the angle formed by the grain side with the back plane of the ceramic tile is 55 to 89 degrees, and the angle formed by the grain side of the remaining part except the chamfered acute angle with the back plane of the ceramic tile is 110 to 150 degrees.