Preparation device and method of aviation titanium alloy actuator and composite film layer thereof

By forming a composite film layer on the surface of the titanium alloy cylinder, the problem of insufficient wear resistance of the titanium alloy operating cylinder is solved, and high wear resistance and service life are extended under dry friction and boundary lubrication conditions are achieved.

CN112359392BActive Publication Date: 2024-11-05BEIJING GOLDEN WHEEL SPECIAL MACHINE +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011460673.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-11
Publication Date
2024-11-05
Estimated Expiration
2040-12-11

AI Technical Summary

Technical Problem

The wear resistance of the titanium alloy actuator is insufficient, especially under dry friction and boundary lubrication conditions, resulting in a short service life.

Method used

The composite film layer is formed on the surface of the titanium alloy cylinder, including an oxide film layer and a vapor-deposited film layer. The oxide film layer has a thickness of 20 to 60 μm, and the vapor-deposited film layer is a carbon-based doped film layer with uniformity of more than 70%. The structurally designed tooling improves the density and uniformity of the film layer.

Benefits of technology

The friction coefficient is significantly reduced, the wear resistance is improved, and the service life of the titanium alloy cylinder is extended. The wear resistance of the film layer is greatly improved under dry friction and boundary lubrication conditions, with the difference between the maximum thickness and the minimum thickness of no more than 30%. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112359392B_ABST
    Figure CN112359392B_ABST
Patent Text Reader

Abstract

This invention discloses an apparatus and method for preparing an aerospace titanium alloy actuator cylinder and its composite film layer. Compared with the prior art, this invention reduces the friction coefficient, improves wear resistance, and extends the service life of the titanium alloy cylinder by forming a composite film layer on the inner surface of the titanium alloy cylinder through oxidation and vapor deposition.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of aviation parts, and in particular to a preparation device and a preparation method for an aviation titanium alloy actuator and a composite film layer thereof. Background Art

[0002] Titanium alloy has the characteristics of low density, high specific strength, and good corrosion resistance. It is widely used in the aerospace field with high requirements on weight. In order to reduce the weight of the actuator system while ensuring strength, titanium alloy is used as the cylinder material of the actuator. However, due to the high activity of titanium element and its affinity with oxygen, the low surface hardness of titanium alloy, poor resistance to plastic shear, and especially poor wear resistance, the wide application of titanium alloy actuators is greatly limited. There are many ways to improve the wear resistance of titanium alloy, among which the formation of in-situ oxide film on the surface of titanium alloy is one of the most studied processes. However, the hardness of the titanium alloy oxide film layer is usually low, and improper control of process parameters will cause the film layer to be loose, which in turn causes insufficient wear resistance. The vapor deposition film layer has high hardness, good wear resistance, and good chemical stability. It is prepared on the surface of the oxide film layer to form a composite film layer, which can solve the problem of low hardness and insufficient wear resistance of the oxide film layer.

[0003] When oxidizing a titanium alloy cylinder, the electrolytic cell is usually used as the cathode and the cylinder is used as the anode for film deposition. However, the film thickness on the inner surface of the cylinder prepared in this way is thinner than that on the outer surface of the cylinder, and the film density is poor. When using vapor deposition technology to deposit a film on the inner surface of a titanium alloy cylinder, the plasma inside the cylinder is unevenly distributed due to the electric field shielding effect generated by the cylinder, and the uniformity of the prepared film is poor, with the thickness difference between the thinnest position and the thickest position being greater than 50%. Summary of the invention

[0004] The purpose of the present invention is to provide an aviation titanium alloy actuator and a preparation method thereof. The titanium alloy actuator has high hardness and good wear resistance, can work stably under dry friction and boundary lubrication conditions, and has a long service life.

[0005] To achieve the above object, the present invention provides the following solutions:

[0006] The invention discloses an aviation titanium alloy actuator cylinder, comprising a titanium alloy cylinder body, a stainless steel piston rod and a rubber sealing ring. The surface of the titanium alloy cylinder body is provided with a composite film layer, the composite film layer comprises an oxide film layer deposited on the surface of the titanium alloy cylinder body and a vapor deposition film layer deposited on the oxide film layer, and the vapor deposition film layer is a carbon-based doped film layer with a uniformity greater than 70%.

[0007] Preferably, the thickness of the oxide film layer is 20-60 μm, and the thickness of the vapor deposition film layer is 3-15 μm.

[0008] Preferably, the titanium alloy cylinder has a diameter of 20 to 100 mm and a length of 150 to 400 mm.

[0009] The present invention also discloses a composite film preparation device, which is used to prepare the composite film on the surface of the titanium alloy cylinder, comprising:

[0010] An oxide film preparation device, the oxide film preparation device comprising a blind hole protection seat at the bottom of a cylinder, an insulating ceramic plate, an exhaust pipe, a ceramic pressure cover, a copper alloy gasket and an oxidation power source, the bottom of the blind hole protection seat at the bottom of the cylinder is embedded in the blind hole at the bottom inner side of the titanium alloy cylinder, the insulating ceramic plate is installed on the top of the blind hole protection seat at the bottom of the cylinder, one end of the exhaust pipe is connected to the blind hole protection seat at the bottom of the cylinder, the other end of the exhaust pipe is used to connect to an exhaust pump, the ceramic pressure cover is installed on the top open end of the titanium alloy cylinder, the copper alloy gasket is installed on the exhaust pipe, the copper alloy gasket is used to connect to the cathode of the oxidation power source, and the titanium alloy cylinder is used to connect to the anode of the oxidation power source;

[0011] A device for preparing a vapor deposition film layer, the device for preparing a vapor deposition film layer comprises a vapor deposition vacuum chamber, a blind hole protection seat at the bottom of the cylinder, a gas distribution pipe and a vapor deposition power supply, the titanium alloy cylinder is located in the vapor deposition vacuum chamber, the bottom of the blind hole protection seat at the bottom of the cylinder is embedded in the blind hole at the bottom inner side of the titanium alloy cylinder, the gas distribution pipe passes through the vapor deposition vacuum chamber and partially extends into the titanium alloy cylinder, the part of the gas distribution pipe extending into the titanium alloy cylinder is provided with gas distribution holes, the vapor deposition power supply is located outside the vapor deposition vacuum chamber, the titanium alloy cylinder is used to connect the cathode of the vapor deposition power supply, and the vapor deposition vacuum chamber is used to connect the anode of the vapor deposition power supply.

[0012] Preferably, one end of the air extraction pipe is connected to the blind hole protection seat at the bottom of the cylinder by a screw, and the other end is arranged with an external thread for threaded connection with the air extraction pump.

[0013] Preferably, the ceramic gland is provided with a through hole, into which a support rod extends, and the support rod is used to clamp the titanium alloy cylinder.

[0014] Preferably, the air distribution pipe is U-shaped as a whole, and a portion of the air distribution pipe close to the bottom of the titanium alloy cylinder is spiral.

[0015] Preferably, the air distribution pipe is made of stainless steel, with a diameter of 3-5 mm, the pitch of the spiral part is 6-8 mm, the diameter of the air distribution hole is 0.5-1 mm, and the multiple air distribution holes are equidistantly distributed along the extension direction of the air distribution pipe, with a spacing of 5-8 mm.

[0016] The present invention also discloses a method for preparing a composite film layer, using the above-mentioned composite film layer preparation device, comprising the following steps:

[0017] S1. Place an oxide film preparation device in the titanium alloy cylinder, connect the threaded end of the exhaust pipe to the exhaust pump, connect the copper alloy gasket on the exhaust pipe to the cathode of the power supply, and place the titanium alloy cylinder horizontally in the oxidation electrolytic cell, with the blind hole end high and the open end low. The entire titanium alloy cylinder is at an angle of 10 to 30 degrees to the horizontal direction. During the preparation of the oxide film, ensure that the entire cylinder is completely immersed in the electrolyte;

[0018] The power supply for oxide film preparation adopts bipolar pulse power supply, constant current control, frequency (200~600) Hz, duty cycle (30~50)%, current (2~5) A / dm 2 , termination voltage (400~1000)V, forward current / negative current = 4 / 1~1 / 1, oxidation time 20~90min;

[0019] The oxidation electrolyte is composed of the following components: [Na2SiO3 (10-15g / L) + KOH (1-1.5g / L)] or [Na2B4O7 (3-8g / L) + KOH (0.3-1g / L)] or [NaAlO2 (2-5g / L) + KOH (0.2-1g / L)], and the pH value of the electrolyte is controlled between 10.5 and 12.5;

[0020] S2, mechanically polishing the oxide film layer to a surface roughness Ra < 0.8 μm, and then cleaning it with an ultrasonic cleaner, using an alkaline water-based cleaning agent, an ultrasonic power of 1 kW, cleaning for 10 to 20 minutes, and then keeping it in an oven at 80° C. for 10 to 20 minutes, and then forming a vapor-deposited film layer on the surface of the oxide film layer by a vapor deposition method, the vapor-deposited film layer is a Si-doped carbon-based film layer, the precursors used are acetylene and tetramethylsilane, and the auxiliary gas is argon;

[0021] The conditions for vapor deposition include: vacuum degree 5 to 10 Pa, bias voltage -1200 to -800 V, current 20 to 60 A, ratio of tetramethylsilane to acetylene 1:10 to 1:5, argon flow rate 50 to 300 sccm, and deposition time 30 to 90 min.

[0022] Compared with the prior art, the present invention has achieved the following technical effects:

[0023] The inner surface of the titanium alloy cylinder of the present invention adopts an oxidation and vapor deposition composite film layer, which reduces the friction coefficient, improves the wear resistance, and prolongs the service life of the titanium alloy cylinder. The use of a tool with a special structural design effectively increases the deposition efficiency of the oxide film layer and increases the density of the film layer. A silicon-doped carbon-based film layer is prepared on the surface of the oxide film layer, which further improves the hardness of the film layer, effectively reduces the friction coefficient, and greatly improves the wear resistance of the film layer under dry friction and boundary lubrication conditions. The special gas distribution method during vapor deposition also improves the uniformity of the film layer, ensuring that the difference between the maximum thickness and the minimum thickness is no more than 30%. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0025] Figure 1 This is a schematic diagram of the structure of the oxide film preparation device in this embodiment;

[0026] Figure 2 Schematic diagram of the structure of the vapor deposition film preparation device in this embodiment;

[0027] Explanation of the reference numerals: 1-titanium alloy cylinder; 2-blind hole protection seat at the bottom of the cylinder; 3-insulating ceramic plate; 4-exhaust pipe; 5-ceramic pressure cover; 6-copper alloy gasket; 7-external thread; 8-vapor deposition vacuum chamber; 9-gas distribution pipe; 10-vapor deposition power supply. DETAILED DESCRIPTION

[0028] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0029] The purpose of the present invention is to provide an aviation titanium alloy actuator and a preparation method thereof. The titanium alloy actuator has high hardness and good wear resistance, can work stably under dry friction and boundary lubrication conditions, and has a long service life.

[0030] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0031] like Figure 1-2As shown, this embodiment provides an aviation titanium alloy actuator cylinder, including a titanium alloy cylinder 1, a stainless steel piston rod and a rubber sealing ring. The surface of the titanium alloy cylinder 1 has a composite film layer, which includes an oxide film layer deposited on the surface of the titanium alloy cylinder 1 and a vapor deposition film layer deposited on the oxide film layer, and the vapor deposition film layer is a carbon-based doped film layer with a uniformity greater than 70%.

[0032] In this embodiment, by using an oxidation and vapor deposition composite film layer on the inner surface of the titanium alloy cylinder 1, the friction coefficient is reduced, the wear resistance is improved, and the service life of the titanium alloy cylinder 1 is extended.

[0033] Specifically, in this embodiment, the thickness of the oxide film layer is 20-60 μm, the thickness of the vapor deposition film layer is 3-15 μm, the diameter of the titanium alloy cylinder 1 is 20-100 mm, and the length is 150-400 mm. According to different actual conditions, those skilled in the art may also select other size parameters.

[0034] This embodiment also provides a composite film preparation device for preparing the composite film on the surface of the titanium alloy cylinder 1, including an oxide film preparation device and a vapor deposition film preparation device.

[0035] Among them, the oxide film preparation device includes a blind hole protection seat 2 at the bottom of the cylinder, an insulating ceramic plate 3, an exhaust pipe 4, a ceramic pressure cap 5, a copper alloy gasket 6 and an oxidation power source. The bottom of the blind hole protection seat 2 at the bottom of the cylinder is embedded in the blind hole at the bottom of the inner side of the titanium alloy cylinder 1, and the insulating ceramic plate 3 is installed on the top of the blind hole protection seat 2 at the bottom of the cylinder. One end of the exhaust pipe 4 is connected to the blind hole protection seat 2 at the bottom of the cylinder, and the other end of the exhaust pipe 4 is used to connect to the exhaust pump, and the ceramic pressure cap 5 is installed at the top open end of the titanium alloy cylinder 1. The copper alloy gasket 6 is installed on the exhaust pipe 4, and the copper alloy gasket 6 is used to connect the cathode of the oxidation power source, and the titanium alloy cylinder 1 is used to connect the anode of the oxidation power source.

[0036] The vapor deposition film preparation device includes a vapor deposition vacuum chamber 8, a blind hole protection seat 2 at the bottom of the cylinder, a gas distribution pipe 9 and a vapor deposition power supply 10. The titanium alloy cylinder 1 is located in the vapor deposition vacuum chamber 8, and the bottom of the blind hole protection seat 2 at the bottom of the cylinder is embedded in the blind hole at the bottom of the inner side of the titanium alloy cylinder 1. The gas distribution pipe 9 passes through the vapor deposition vacuum chamber 8 and partially extends into the titanium alloy cylinder 1. The part of the gas distribution pipe 9 extending into the titanium alloy cylinder 1 is provided with a gas distribution hole. The vapor deposition power supply 10 is located outside the vapor deposition vacuum chamber 8, the titanium alloy cylinder 1 is used to connect the cathode of the vapor deposition power supply 10, and the vapor deposition vacuum chamber 8 is used to connect the anode of the vapor deposition power supply 10.

[0037] This embodiment uses a tooling with a special structural design as an oxide film preparation device, which effectively increases the deposition efficiency of the oxide film and increases the density of the oxide film. This embodiment uses a vapor deposition film preparation device to perform vapor deposition, and then prepares a silicon-doped carbon-based film on the surface of the oxide film, which further increases the hardness of the film and effectively reduces the friction coefficient. The wear resistance of the film is greatly improved under dry friction and boundary lubrication conditions.

[0038] There are many ways to connect the air extraction pipe 4, and those skilled in the art can flexibly choose. In this embodiment, one end of the air extraction pipe 4 is connected to the blind hole protection seat 2 at the bottom of the cylinder by screws, and the other end is arranged with an external thread 7 for threaded connection with the air extraction pump.

[0039] During the deposition of the oxide film layer, in order to facilitate clamping, in this embodiment, a through hole is provided on the ceramic gland 5 , into which a support rod is inserted, and the support rod is used to clamp the titanium alloy cylinder 1 .

[0040] During the vapor deposition process, in order to improve the uniformity of the vapor deposited film layer, the gas distribution pipe 9 of this embodiment is U-shaped as a whole, and the bending position of the U-shape is close to the bottom of the titanium alloy cylinder 1, and the bending position is spiral.

[0041] Furthermore, in this embodiment, the air distribution tube 9 is made of stainless steel, with a diameter of 3 to 5 mm, and a pitch of 6 to 8 mm for the spiral portion. The diameter of the air distribution hole is 0.5 to 1 mm, and the plurality of air distribution holes are evenly distributed along the extension direction of the air distribution tube 9, with a spacing of 5 to 8 mm. It should be noted that, according to different actual conditions, those skilled in the art may also select other size parameters.

[0042] This embodiment also provides a method for preparing a composite film layer, using the above-mentioned composite film layer preparation device to prepare the above-mentioned aviation titanium alloy actuator having a composite film layer, which specifically includes the following steps:

[0043] S1. Place an oxide film preparation device in the titanium alloy cylinder 1, connect the threaded end of the exhaust pipe 4 to the exhaust pump, connect the copper alloy gasket 6 on the exhaust pipe 4 to the cathode of the power supply, and place the titanium alloy cylinder 1 horizontally in the oxidation electrolytic cell, with the blind hole end high and the open end low. The entire titanium alloy cylinder 1 is at an angle of 10 to 30 degrees to the horizontal direction. During the preparation of the oxide film, ensure that the entire cylinder is completely immersed in the electrolyte;

[0044] The power supply for oxide film preparation adopts bipolar pulse power supply, constant current control, frequency (200~600) Hz, duty cycle (30~50)%, current (2~5) A / dm 2 , termination voltage (400~1000)V, forward current / negative current = 4 / 1~1 / 1, oxidation time 20~90min;

[0045] The oxidation electrolyte is composed of the following components: [Na2SiO3 (10-15g / L) + KOH (1-1.5g / L)] or [Na2B4O7 (3-8g / L) + KOH (0.3-1g / L)] or [NaAlO2 (2-5g / L) + KOH (0.2-1g / L)], and the pH value of the electrolyte is controlled between 10.5 and 12.5;

[0046] S2, mechanically polishing the oxide film layer to a surface roughness Ra < 0.8 μm, and then cleaning it with an ultrasonic cleaner, using an alkaline water-based cleaning agent, an ultrasonic power of 1 kW, cleaning for 10 to 20 minutes, and then keeping it in an oven at 80° C. for 10 to 20 minutes, and then forming a vapor-deposited film layer on the surface of the oxide film layer by a vapor deposition method, the vapor-deposited film layer is a Si-doped carbon-based film layer, the precursors used are acetylene and tetramethylsilane, and the auxiliary gas is argon;

[0047] The conditions for vapor deposition include: vacuum degree 5 to 10 Pa, bias voltage -1200 to -800 V, current 20 to 60 A, ratio of tetramethylsilane to acetylene 1:10 to 1:5, argon flow rate 50 to 300 sccm, and deposition time 30 to 90 min.

[0048] After testing, the surface oxide film of the titanium alloy cylinder 1 prepared by the above method of this embodiment has a thickness of 50 μm, the vapor deposition film has a thickness of 8 μm, and the composite coating thickness uniformity of the entire cylinder wall can reach 80% after decomposition measurement. After 100 reciprocating motions with the matching piston under dry friction conditions, no scratches or other damage were observed on the inner surface of the cylinder.

[0049] The present specification uses specific examples to illustrate the principles and implementation methods of the present invention. The above examples are only used to help understand the method and core idea of ​​the present invention. At the same time, for those skilled in the art, according to the idea of ​​the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting the present invention.

Claims

1. A composite film preparation device for preparing a composite film on the surface of a titanium alloy cylinder, characterized in that: The composite film layer comprises an oxide film layer deposited on the surface of the titanium alloy cylinder and a vapor deposition film layer deposited on the oxide film layer, wherein the vapor deposition film layer is a carbon-based doped film layer with a uniformity greater than 70%; the oxide film layer has a thickness of 20 to 60 μm, and the vapor deposition film layer has a thickness of 3 to 15 μm; The preparation device of the composite film layer comprises: An oxide film preparation device, the oxide film preparation device comprising a blind hole protection seat at the bottom of a cylinder, an insulating ceramic plate, an exhaust pipe, a ceramic pressure cover, a copper alloy gasket and an oxidation power source, the bottom of the blind hole protection seat at the bottom of the cylinder is embedded in the blind hole at the bottom inner side of the titanium alloy cylinder, the insulating ceramic plate is installed on the top of the blind hole protection seat at the bottom of the cylinder, one end of the exhaust pipe is connected to the blind hole protection seat at the bottom of the cylinder, the other end of the exhaust pipe is used to connect to an exhaust pump, the ceramic pressure cover is installed on the top open end of the titanium alloy cylinder, the copper alloy gasket is installed on the exhaust pipe, the copper alloy gasket is used to connect to the cathode of the oxidation power source, and the titanium alloy cylinder is used to connect to the anode of the oxidation power source; A device for preparing a vapor deposition film layer, the device for preparing a vapor deposition film layer comprises a vapor deposition vacuum chamber, a blind hole protection seat at the bottom of the cylinder, a gas distribution pipe and a vapor deposition power supply, the titanium alloy cylinder is located in the vapor deposition vacuum chamber, the bottom of the blind hole protection seat at the bottom of the cylinder is embedded in the blind hole at the bottom inner side of the titanium alloy cylinder, the gas distribution pipe passes through the vapor deposition vacuum chamber and partially extends into the titanium alloy cylinder, the part of the gas distribution pipe extending into the titanium alloy cylinder is provided with gas distribution holes, the vapor deposition power supply is located outside the vapor deposition vacuum chamber, the titanium alloy cylinder is used to connect the cathode of the vapor deposition power supply, and the vapor deposition vacuum chamber is used to connect the anode of the vapor deposition power supply.

2. The device for preparing the composite film layer according to claim 1, characterized in that: One end of the air extraction pipe is connected to the blind hole protection seat at the bottom of the cylinder by a screw, and the other end is arranged with an external thread for threaded connection with the air extraction pump.

3. The preparation device of the composite film layer according to claim 1, characterized in that: The ceramic gland is provided with a through hole, into which a support rod is inserted, and the support rod is used to clamp the titanium alloy cylinder.

4. The device for preparing a composite film layer according to claim 1, characterized in that: The air distribution pipe is U-shaped as a whole, and the portion of the air distribution pipe close to the bottom of the titanium alloy cylinder is spiral.

5. The device for preparing the composite film layer according to claim 4, characterized in that: The air distribution pipe is made of stainless steel and has a diameter of 3-5 mm. The pitch of the spiral part is 6-8 mm. The diameter of the air distribution hole is 0.5-1 mm. The plurality of air distribution holes are evenly distributed along the extension direction of the air distribution pipe with a spacing of 5-8 mm.

6. The device for preparing a composite film layer according to claim 1, characterized in that: The diameter of the titanium alloy cylinder is 20-100 mm, and the length is 150-400 mm.

7. A method for preparing a composite film layer, using the composite film layer preparation device according to any one of claims 1 to 5, characterized in that: The steps include: S1. Place an oxide film preparation device in the titanium alloy cylinder, connect the threaded end of the exhaust pipe to the exhaust pump, connect the copper alloy gasket on the exhaust pipe to the cathode of the power supply, and place the titanium alloy cylinder horizontally in the oxidation electrolytic cell, with the blind hole end high and the open end low. The entire titanium alloy cylinder is at an angle of 10 to 30 degrees to the horizontal direction. During the preparation of the oxide film, ensure that the entire cylinder is completely immersed in the electrolyte; The power supply for oxide film preparation adopts bipolar pulse power supply, constant current control, frequency 200~600Hz, duty cycle 30~50%, current 2~5A / dm 2 , termination voltage 400~1000V, forward current / negative current = 4 / 1~1 / 1, oxidation time 20~90min; The oxidation electrolyte is composed of the following ingredients: 10~15g / L Na2SiO3 and 1~1.5 g / L KOH, or 3~8g / L Na2B4O7 and 0.3~1g / L KOH, or 2~5g / L NaAlO2 and 0.2~1g / L KOH, and the pH value of the electrolyte is controlled between 10.5~12.5; S2, mechanically polishing the oxide film layer to a surface roughness Ra < 0.8 μm, and then cleaning it with an ultrasonic cleaner, using an alkaline water-based cleaning agent, an ultrasonic power of 1 kW, cleaning for 10 to 20 minutes, and then keeping it in an oven at 80°C for 10 to 20 minutes, and then forming a vapor-deposited film layer on the surface of the oxide film layer by a vapor deposition method, the vapor-deposited film layer is a Si-doped carbon-based film layer, the precursors used are acetylene and tetramethylsilane, and the auxiliary gas is argon; The conditions for vapor deposition include: vacuum degree 5~10Pa, bias voltage -1200~-800V, current 20~60A, ratio of tetramethylsilane to acetylene 1:10~1:5, argon flow rate 50~300sccm, and deposition time 30~90min.