Laminated iron core and rotating motor

By establishing a bonding area extending along the direction of magnetic flux in the laminated iron core, the problem of iron loss in the bonding area is solved, and the magnetic characteristics and energy efficiency of the rotating electrical machine are improved.

CN113196634BActive Publication Date: 2024-10-18NIPPON STEEL CORPORATION
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN201980083028.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-12-17
Publication Date
2024-10-18
Estimated Expiration
2039-12-17

Smart Images

  • Figure CN113196634B_ABST
    Figure CN113196634B_ABST
Patent Text Reader

Abstract

The laminated iron core includes: a plurality of electromagnetic steel plates stacked on each other; and a bonding portion, which is provided between the electromagnetic steel plates adjacent to each other in the stacking direction, and bonds the electromagnetic steel plates to each other respectively, the electromagnetic steel plates having an annular core back and a plurality of teeth, the plurality of teeth extending from the core back in the radial direction of the core back and arranged at intervals in the circumferential direction of the core back, a bonding area provided with the bonding portion is formed on the core back of the electromagnetic steel plates, the bonding area extending in the direction along the magnetic flux, and the magnetic flux passes through the area of ​​the electromagnetic steel plates in contact with the bonding area.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a laminated core and a rotating electric machine.

[0002] This application claims priority based on Japanese Patent Application No. 2018-235858 filed in Japan on December 17, 2018, and the contents are incorporated herein by reference. Background Art

[0003] Conventionally, there is known a laminated iron core as described in the following Patent Document 1. In this laminated iron core, electromagnetic steel sheets adjacent to each other in the lamination direction are bonded together by an adhesive layer.

[0004] Prior Art Literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Publication No. 2011-023523 Summary of the invention

[0007] Problems to be solved by the invention

[0008] In the above-mentioned conventional laminated core, there is room for improvement in terms of improving magnetic characteristics.

[0009] The present invention has been made in view of the above circumstances, and an object of the present invention is to improve the magnetic characteristics of a laminated core.

[0010] Technical solutions for solving technical problems

[0011] (1) One aspect of the present invention is a laminated iron core, comprising: a plurality of electromagnetic steel sheets stacked on one another; and a bonding portion provided between the electromagnetic steel sheets adjacent to one another in a stacking direction, for bonding the electromagnetic steel sheets to one another, the electromagnetic steel sheets having an annular core back and a plurality of teeth extending from the core back in a radial direction of the core back and arranged at intervals in a circumferential direction of the core back, a bonding region provided with the bonding portion being formed on the core back of the electromagnetic steel sheets, the bonding region extending in a direction along a magnetic flux passing through a region of the electromagnetic steel sheets in contact with the bonding region.

[0012] According to the above configuration, the adhesive portion extends in one direction. By making the adhesive portion extend in one direction, the adhesive area of ​​the adhesive portion can be increased and the adhesive strength can be improved compared to the case where dot-shaped adhesive portions are intermittently provided in the same range.

[0013] Generally, adhesive shrinks when solidifying. Therefore, in the bonding area, which is the area of ​​the electromagnetic steel sheet in contact with the bonding portion, distortion caused by the curing shrinkage of the adhesive occurs, and the iron loss of the electromagnetic steel sheet in this area increases. Here, the area in contact with the bonding area and where the iron loss increases due to distortion is called a deteriorated area. According to the above-mentioned structure, the direction in which the bonding area extends is consistent with the direction of the magnetic flux passing through the deteriorated area. Thereby, the proportion of the deteriorated area in the cross-sectional area of ​​the magnetic flux path can be reduced, and the number of magnetic flux lines passing through the deteriorated area can be suppressed. In addition, by reducing the proportion of the deteriorated area in the cross-sectional area of ​​the magnetic flux path, the magnetic flux can easily bypass the deteriorated area with high magnetic resistance. As a result, it is possible to suppress the deteriorated area from hindering the flow of the magnetic flux that forms the magnetic circuit, and the magnetic properties of the laminated iron core as the stator core can be improved.

[0014] (2) In the laminated iron core of (1), the following structure may be adopted: the back of the iron core has a first portion and a second portion alternately arranged along the circumferential direction, the first portion is connected to the tooth portion in the radial direction on the radial outside of the tooth portion, the second portion is located between the first portions in the circumferential direction, and the bonding area is discretely formed along the circumferential direction in at least one of the first portion and the second portion.

[0015] According to the above configuration, the bonding regions are discretely arranged in the circumferential direction in the core back. Thus, the electromagnetic steel sheets can be fixed to each other in a well-balanced manner. In addition, since the deteriorated regions formed in the electromagnetic steel sheets are discretely arranged, the deteriorated regions are less likely to hinder the flow of magnetic flux.

[0016] (3) In the laminated core described in (2) above, the following configuration may be adopted: in the laminated core, the bonding region is formed at the first portion, and the bonding region is not formed on both sides of the bonding region in the circumferential direction.

[0017] According to the above configuration, regions (non-degraded regions) where iron loss does not increase are provided on both circumferential sides of the degraded region. Therefore, the magnetic flux forming the magnetic path can bypass the non-degraded region, thereby improving the magnetic properties of the laminated core as the stator core.

[0018] (4) In the laminated core described in (3) above, the following configuration may be adopted: in the laminated core, the bonding region extends in a radial direction along a center line of the tooth portion.

[0019] The magnetic flux flowing from the tooth portion to the core back extends radially in the first portion of the core back and branches to both sides in the circumferential direction at the radial middle of the first portion. According to the above configuration, since the bonding area extends radially along the center line of the tooth portion, the direction in which the bonding area extends coincides with the direction in which the magnetic flux extends at the first portion. Therefore, it is possible to suppress the deteriorated area from obstructing the flow of the magnetic flux, and to improve the magnetic properties of the stator core.

[0020] (5) In the laminated core described in (3) or (4), the tooth portion may extend radially inward from the core back, and the bonding region may extend radially inward from the radial outer end of the core back.

[0021] The path for the magnetic flux to flow can easily take the shortest distance with low magnetic resistance. According to the above configuration, since the bonding area extends from the radial outer end of the core back, it is difficult to hinder the flow of the magnetic flux passing through the shortest distance.

[0022] (6) In the laminated core described in (2) above, the bonding region may be provided at the second location, and the bonding region may not be formed on both sides of the bonding region in the radial direction.

[0023] According to the above configuration, the non-degraded regions are provided on both radial sides of the degraded region. Therefore, the magnetic flux forming the magnetic path can bypass and pass through the non-degraded regions, and the magnetic characteristics of the laminated core as the stator core can be improved.

[0024] (7) In the laminated core described in (6) above, the bonding region may extend in the circumferential direction.

[0025] The magnetic flux flowing through the core back flows in the circumferential direction at the second portion. According to the above configuration, since the bonding region extends in the circumferential direction, the deteriorated region is less likely to hinder the flow of the magnetic flux.

[0026] (8) In the laminated core described in (6) or (7), the tooth portion may extend radially inward from the core back, and the bonding region may be arranged radially outward of the core back.

[0027] According to the above configuration, since the bonding region is disposed offset toward the radially outer side of the core back, the flow of the magnetic flux passing through the shortest distance is less likely to be blocked.

[0028] (9) In the laminated iron core described in (2) above, the bonding region may be provided so as to straddle one of the first portion and one of the second portion.

[0029] According to the above configuration, the bonding area is formed asymmetrically with respect to the center line of the tooth portion. Therefore, the magnetic flux density is different on one side and the other side of the circumferential direction with respect to the tooth portion. When such a laminated core is used for a rotating electric machine that rotates only in one direction, the energy efficiency of the rotating electric machine can be improved.

[0030] (10) In the laminated iron core described in any one of (1) to (9), the average thickness of the bonding portion may be 1.0 μm to 3.0 μm.

[0031] (11) In the laminated iron core described in any one of (1) to (10), an average tensile modulus E of the bonding portion may be 1500 MPa to 4500 MPa.

[0032] (12) In the laminated iron core described in any one of (1) to (11), the adhesive portion may be a room temperature adhesive type acrylic adhesive including SGA composed of an acrylic adhesive containing an elastomer.

[0033] (13) A rotating electric machine according to one aspect of the present invention is a rotating electric machine including the laminated iron core described in any one of (1) to (12).

[0034] According to the rotating electric machine having the above-described configuration, since it includes the laminated core having excellent magnetic characteristics, it is possible to improve the energy efficiency of the rotating electric machine.

[0035] Effects of the Invention

[0036] According to the present invention, the magnetic characteristics of the laminated core can be improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 It is a cross-sectional view of a rotating electrical machine according to an embodiment of the present invention.

[0038] Figure 2 yes Figure 1 FIG. 1 is a top view of a stator included in the rotating electrical machine shown.

[0039] Figure 3 yes Figure 1 A front view of a stator included in the rotating electrical machine shown.

[0040] Figure 4 yes Figure 2 and Figure 3 Schematic diagram of the electromagnetic steel plates and bonding areas of the stator shown.

[0041] Figure 5 This is a schematic diagram of the bonding area of ​​the stator according to Modification Example 1.

[0042] Figure 6 It is a schematic diagram of the bonding area of ​​the stator of Modification Example 2.

[0043] Figure 7 This is a schematic diagram of the bonding area of ​​the stator of Modification 3.

[0044] Figure 8 This is a schematic diagram of the bonding area of ​​the stator of Modification Example 4.

[0045] Fig. 9 It is a schematic diagram of the bonding area of ​​the stator of Modification Example 5.

[0046] Fig.10 This is a graph showing the simulation results of the iron loss of Model No. 1 to Model No. 4.

[0047] Fig.11 It is a schematic diagram of the stator core of model No. 4 which is a comparative example. DETAILED DESCRIPTION

[0048] Hereinafter, a rotating electrical machine according to an embodiment of the present invention will be described with reference to the accompanying drawings. In addition, in this embodiment, an electric motor is cited as the rotating electrical machine, specifically an AC motor, more specifically a synchronous motor, and more specifically a permanent magnet excitation type motor as an example for description. Such an electric motor is suitable for use in, for example, electric vehicles, etc.

[0049] like Figure 1 and Figure 2 As shown, the rotary electric machine 10 includes a stator 20, a rotor 30, a housing 50, and a rotating shaft 60. The stator 20 and the rotor 30 are accommodated in the housing 50. The stator 20 is fixed to the housing 50.

[0050] In the rotating electrical machine 10 of the present embodiment, for example, an exciting current having an effective value of 10A and a frequency of 100 Hz is applied to each phase of the stator 20 , and accordingly the rotor 30 and the rotating shaft 60 rotate at a rotation speed of 1000 rpm.

[0051] In the present embodiment, an inner rotor type in which the rotor 30 is located inside the stator 20 is adopted as the rotating electrical machine 10. However, an outer rotor type in which the rotor 30 is located outside the stator 20 may be adopted as the rotating electrical machine 10. In addition, in the present embodiment, the rotating electrical machine 10 is a 12-pole 18-slot three-phase AC motor. However, for example, the number of poles, the number of slots, the number of phases, etc. may be appropriately changed.

[0052] The stator 20 includes a stator core (laminated core) 21 and a winding (not shown).

[0053] The stator core 21 includes an annular core back 22 and a plurality of teeth 23. Hereinafter, the axial direction (the direction of the central axis O of the stator core 21) of the stator core 21 (core back 22) is referred to as the axial direction, the radial direction (the direction orthogonal to the central axis O of the stator core 21) of the stator core 21 (core back 22) is referred to as the radial direction, and the circumferential direction (the direction surrounding the central axis O of the stator core 21) of the stator core 21 (core back 22) is referred to as the circumferential direction.

[0054] The core back 22 is formed in a circular ring shape in a plan view of the stator 20 viewed from the axial direction.

[0055] The plurality of teeth 23 extend radially inward from the core back 22 (along the central axis O of the core back 22 in the radial direction). The plurality of teeth 23 are arranged at equal intervals in the circumferential direction. In the present embodiment, 18 teeth 23 are provided at a center angle of 20 degrees centered on the central axis O. The plurality of teeth 23 are formed in the same shape and size as each other.

[0056] The winding is wound around the teeth 23. The winding may be concentratedly wound or distributedly wound.

[0057] The rotor 30 is arranged radially inward of the stator 20 (stator core 21 ). The rotor 30 includes a rotor core 31 and a plurality of permanent magnets 32 .

[0058] The rotor core 31 is formed in an annular shape (ring shape) arranged coaxially with the stator 20. The rotating shaft 60 is arranged in the rotor core 31. The rotating shaft 60 is fixed to the rotor core 31.

[0059] A plurality of permanent magnets 32 are fixed to the rotor core 31. In the present embodiment, a group of two permanent magnets 32 forms a magnetic pole. The plurality of groups of permanent magnets 32 are arranged at equal intervals in the circumferential direction. In the present embodiment, 12 groups (24 in total) of permanent magnets 32 are provided at a central angle of 30 degrees with the central axis O as the center.

[0060] In the present embodiment, an embedded magnet type motor is used as a permanent magnet excitation type motor. A plurality of through holes 33 are formed on the rotor core 31, which penetrate the rotor core 31 in the axial direction. The plurality of through holes 33 are provided corresponding to the plurality of permanent magnets 32. Each permanent magnet 32 ​​is fixed to the rotor core 31 in a state of being arranged in the corresponding through hole 33. The fixation of each permanent magnet 32 ​​relative to the rotor core 31 can be achieved, for example, by bonding the outer surface of the permanent magnet 32 ​​to the inner surface of the through hole 33 with an adhesive. In addition, as a permanent magnet excitation type motor, a surface magnet type motor can be used instead of an embedded magnet type motor.

[0061] <Laminated Core>

[0062] like Figure 3 As shown in FIG. 1 , the stator core 21 is a laminated core. The stator core 21 is formed by laminating a plurality of electromagnetic steel sheets 40. That is, the stator core 21 includes a plurality of electromagnetic steel sheets 40 laminated in the thickness direction.

[0063] In addition, the stacking thickness of the stator core 21 is, for example, 50.0 mm. The outer diameter of the stator core 21 is, for example, 250.0 mm. The inner diameter of the stator core 21 is, for example, 165.0 mm. However, these values ​​are only examples, and the stacking thickness, outer diameter, and inner diameter of the stator core 21 are not limited to these values. Here, the inner diameter of the stator core 21 is based on the front end of the tooth portion 23 in the stator core 21. That is, the inner diameter of the stator core 21 is the diameter of an imaginary circle inscribed in the front end of all the tooth portions 23.

[0064] Each electromagnetic steel sheet 40 forming the stator core 21 and the rotor core 31 is formed, for example, by punching an electromagnetic steel sheet as a base material. As the electromagnetic steel sheet 40, a known electromagnetic steel sheet can be used. The chemical composition of the electromagnetic steel sheet 40 is not particularly limited. In the present embodiment, a non-oriented electromagnetic steel sheet is used as the electromagnetic steel sheet 40. As the non-oriented electromagnetic steel sheet, for example, a non-oriented electrical steel strip of JIS C 2552:2014 can be used.

[0065] However, a oriented electromagnetic steel sheet may be used instead of a non-oriented electromagnetic steel sheet as the electromagnetic steel sheet 40. As the oriented electromagnetic steel sheet, a oriented electrical steel strip of JIS C 2553:2012 may be used.

[0066] In order to improve the workability of the electromagnetic steel sheet and the iron loss of the laminated core, an insulating film is provided on both sides of the electromagnetic steel sheet 40. As a material constituting the insulating film, for example, (1) an inorganic compound, (2) an organic resin, (3) a mixture of an inorganic compound and an organic resin, etc. can be applied. As an inorganic compound, for example, (1) a complex of dichromate and boric acid, (2) a complex of phosphate and silicon dioxide, etc. can be cited. As an organic resin, epoxy resin, acrylic resin, acrylic styrene resin, polyester resin, silicon resin, fluorine resin, etc. can be cited.

[0067] In order to ensure the insulation performance between the electromagnetic steel sheets 40 stacked on each other, the thickness of the insulating film (the thickness per single surface of the electromagnetic steel sheet 40 ) is preferably 0.1 μm or more.

[0068] On the other hand, as the insulating coating becomes thicker, the insulating effect is saturated. In addition, as the insulating coating becomes thicker, the proportion of the insulating coating in the stator core 21 increases, and the magnetic properties of the stator core 21 decrease. Therefore, the insulating coating is preferably thinner within a range that can ensure the insulating performance. The thickness of the insulating coating (the thickness of each single surface of the electromagnetic steel sheet 40) is preferably 0.1 μm or more and 5 μm or less, and more preferably 0.1 μm or more and 2 μm or less.

[0069] As the electromagnetic steel sheet 40 becomes thinner, the iron loss improvement effect gradually saturates. In addition, as the electromagnetic steel sheet 40 becomes thinner, the manufacturing cost of the electromagnetic steel sheet 40 increases. Therefore, considering the iron loss improvement effect and the manufacturing cost, the thickness of the electromagnetic steel sheet 40 is preferably 0.10 mm or more.

[0070] On the other hand, if the electromagnetic steel sheet 40 is too thick, it becomes difficult to punch the electromagnetic steel sheet 40. Therefore, considering the punching work of the electromagnetic steel sheet 40, the thickness of the electromagnetic steel sheet 40 is preferably 0.65 mm or less.

[0071] In addition, if the thickness of the electromagnetic steel sheet 40 increases, the iron loss increases. Therefore, considering the iron loss characteristics of the electromagnetic steel sheet 40, the thickness of the electromagnetic steel sheet 40 is preferably 0.35 mm or less, and more preferably 0.20 mm or 0.25 mm.

[0072] Considering the above point, the thickness of each electromagnetic steel sheet 40 is, for example, 0.10 mm to 0.65 mm, preferably 0.10 mm to 0.35 mm, and more preferably 0.20 mm or 0.25 mm. The thickness of the electromagnetic steel sheet 40 also includes the thickness of the insulating film.

[0073] The plurality of electromagnetic steel sheets 40 forming the stator core 21 are bonded by bonding portions 41. The bonding portions 41 are provided between the electromagnetic steel sheets 40 adjacent to each other in the stacking direction and are adhesives that are cured without being cut. Among adhesives, for example, thermosetting adhesives based on polymerization bonding are used. As adhesive compositions, those containing (1) acrylic resins, (2) epoxy resins, (3) compositions containing acrylic resins and epoxy resins, etc. can be used. As such adhesives, in addition to thermosetting adhesives, free radical polymerization adhesives, etc. can also be used. From the perspective of productivity, it is preferred to use room temperature curing adhesives. Room temperature curing adhesives cure at 20°C to 30°C. As room temperature curing adhesives, acrylic adhesives are preferred. Representative acrylic adhesives include SGA (Second Generation Acrylic Adhesive). Any of anaerobic adhesives, quick-drying adhesives, and acrylic adhesives containing elastomers can be used within the range that does not impair the effects of the present invention. The adhesive referred to here refers to the state before curing, and the adhesive becomes the adhesive portion 41 after curing.

[0074] The average tensile modulus E of the bonding portion 41 at room temperature (20°C to 30°C) is in the range of 1500MPa to 4500MPa. If the average tensile modulus E of the bonding portion 41 is less than 1500MPa, the rigidity of the laminated core is reduced. Therefore, the lower limit of the average tensile modulus E of the bonding portion 41 is 1500MPa, and more preferably 1800MPa. On the contrary, if the average tensile modulus E of the bonding portion 41 exceeds 4500MPa, the insulating coating formed on the surface of the electromagnetic steel sheet 40 is peeled off. Therefore, the upper limit of the average tensile modulus E of the bonding portion 41 is 4500MPa, and more preferably 3650MPa.

[0075] The average tensile modulus E is measured by a resonance method. Specifically, the tensile modulus is measured in accordance with JIS R 1602:1995.

[0076] More specifically, a sample for measurement (not shown) is first prepared. The sample is obtained by bonding two electromagnetic steel plates 40 with an adhesive of the measurement object and curing the adhesive to form a bonding portion 41. The curing is performed by heating and pressing under actual heating and pressing conditions when the adhesive is a thermosetting type. On the other hand, when the adhesive is a room temperature curing type, it is performed by pressing at room temperature.

[0077] Then, the tensile modulus of the sample is measured by the resonance method. The method for measuring the tensile modulus by the resonance method is performed in accordance with JIS R 1602: 1995 as described above. Then, the tensile modulus of the bonding portion 41 alone can be obtained by calculating the tensile modulus of the sample (measured value) by removing the influence of the electromagnetic steel sheet 40 itself.

[0078] Since the tensile modulus obtained from the sample is equal to the average value of the laminated core as a whole, this value is regarded as the average tensile modulus E. The composition is set so that the average tensile modulus E is almost unchanged at the stacking position along the stacking direction and the circumferential position around the central axis of the laminated core. Therefore, the average tensile modulus E can be set to a value obtained by measuring the cured bonding portion 41 at the upper end position of the laminated core.

[0079] The electric motor generates heat when driven. Therefore, if the melting point of the adhesive portion 41 is low, the heat generated by the engine causes the adhesive portion 41 to melt, thereby changing the shape of the adhesive region 42 and failing to achieve the desired effect. Generally, an insulating coating (enamel coating) is provided on the surface of the winding wound on the stator core 21. The heat-resistant temperature of the coating is, for example, about 180°C. Therefore, a general electric motor is driven in a manner below 180°C. That is, the engine can be heated to about 180°C. In the present embodiment, the melting point of the adhesive portion 41 is preferably above 180°C. Furthermore, considering the safety factor of the local presence of a high-temperature portion, the melting point of the adhesive portion 41 is further preferably above 200°C.

[0080] As a bonding method, for example, a method of applying an adhesive to the electromagnetic steel sheet 40 and then bonding by heating or pressing or both can be adopted. In addition, the heating means can be various means such as heating in a high temperature tank or electric furnace, or directly energizing.

[0081] In order to obtain stable and sufficient adhesive strength, the thickness of the adhesive portion 41 is preferably 1 μm or more.

[0082] On the other hand, if the thickness of the adhesive portion 41 exceeds 100 μm, the adhesive force is saturated. In addition, as the thickness of the adhesive portion 41 increases, the space factor decreases, and the magnetic properties such as the iron loss of the laminated core decrease. Therefore, the thickness of the adhesive portion 41 is preferably 1 μm or more and 100 μm or less, and more preferably 1 μm or more and 10 μm or less.

[0083] Furthermore, in the above description, the thickness of the adhesive portion 41 refers to the average thickness of the adhesive portion 41 .

[0084] The average thickness of the adhesive portion 41 is more preferably not less than 1.0 μm and not more than 3.0 μm. If the average thickness of the adhesive portion 41 is less than 1.0 μm, sufficient bonding strength cannot be ensured as described above. Therefore, the lower limit of the average thickness of the adhesive portion 41 is 1.0 μm, and more preferably 1.2 μm. On the contrary, if the average thickness of the adhesive portion 41 exceeds 3.0 μm and becomes thicker, undesirable conditions such as a significant increase in the amount of distortion of the electromagnetic steel sheet 40 caused by shrinkage during thermal curing occur. Therefore, the upper limit of the average thickness of the adhesive portion 41 is 3.0 μm, and more preferably 2.6 μm.

[0085] The average thickness of the bonding portion 41 is the average value of the entire laminated core. The average thickness of the bonding portion 41 is almost constant at the stacking position along the stacking direction and the circumferential position around the central axis of the laminated core. Therefore, the average thickness of the bonding portion 41 can be set as the average value of the values ​​measured at more than 10 positions in the circumferential direction at the upper end position of the laminated core.

[0086] In addition, the average thickness of the adhesive portion 41 can be adjusted by, for example, changing the amount of adhesive applied. In addition, the average tensile elastic modulus E of the adhesive portion 41 can be adjusted by, for example, changing the heating and pressurizing conditions applied during bonding and one or both of the types of curing agents in the case of a thermosetting adhesive.

[0087] Next, based on Figure 4 , the relationship between the electromagnetic steel sheet 40, the bonding portion 41, and the bonding region 42 will be described.

[0088] like Figure 4 As shown, the electromagnetic steel sheets 40 adjacent to each other in the stacking direction are not bonded to each other over their entire surfaces. These electromagnetic steel sheets 40 are partially bonded to each other. The bonding portion 41 is provided on the plurality of core backs 22 of the electromagnetic steel sheet. The core backs 22 are bonded by the bonding portion 41. That is, the plurality of electromagnetic steel sheets 40 are bonded to each other by the bonding portion 41.

[0089] On the surface of the electromagnetic steel sheet 40 facing the stacking direction (hereinafter referred to as the first surface of the electromagnetic steel sheet 40), an adhesive region 42 and a blank region 43 (non-adhesive region) are formed. The adhesive region 42 refers to the region on the first surface of the electromagnetic steel sheet 40 where the adhesive portion 41 is provided. More specifically, the adhesive region 42 refers to the region on the first surface of the electromagnetic steel sheet 40 where the cured adhesive is provided. The blank region 43 refers to the region on the first surface of the electromagnetic steel sheet where the adhesive portion 41 is not provided.

[0090] Here, the core back 22 of the electromagnetic steel sheet 40 is divided into a first portion 22a and a second portion 22b. The first portion 22a and the second portion 22b are arranged alternately along the circumferential direction. That is, the core back 22 has the first portion 22a and the second portion 22b arranged alternately along the circumferential direction. The boundary line between the first portion 22a and the second portion 22b extends straight in the radial direction. The first portion 22a is connected to the tooth portion 23 on the radial outer side of the tooth portion 23. The second portion 22b is located between the first portions 22a in the circumferential direction.

[0091] The bonding region 42 is provided in the second portion 22b of the core back 22. In addition, the bonding region 42 is not provided in the first portion 22a of the core back 22. One bonding region 42 is provided in one second portion 22b. The bonding region 42 is located at the circumferential center of the second portion 22b. In addition, the bonding region 42 is arranged radially outward in the second portion 22b.

[0092] The bonding area 42 is a generally rectangular shape with the direction perpendicular to the radial direction as the long side direction in a plan view. That is, the bonding area 42 extends along the circumferential direction. According to this embodiment, by setting the bonding area 42 to a shape extending in one direction, the bonding area of ​​the bonding portion 41 can be increased and the bonding strength can be improved compared to the case where dot-shaped bonding areas are intermittently provided within the same range.

[0093] By increasing the width dimension d1 of the bonding portion 41, the bonding portion can be easily formed in the manufacturing process. In addition, by reducing the width dimension d1 of the bonding portion 41, the electromagnetic steel sheet 40 will not be locally deformed significantly due to the compressive stress of the adhesive, and the deterioration of the iron loss of the electromagnetic steel sheet 40 as a whole can be suppressed.

[0094] In addition, the width dimension of the bonding region 42 refers to the dimension in the short side direction of the bonding region 42, and in the present embodiment, it is the dimension in the radial direction of the bonding region 42. In the present embodiment, the bonding region 42 refers to the region where the bonding portion 41 is provided on the first surface of the electromagnetic steel sheet 40, and therefore the width dimension of the bonding region 42 is the same as the width dimension of the bonding portion 41.

[0095] The ratio of the length dimension d2 to the width dimension d1 of the bonding region 42 (d2 / d1, aspect ratio) is preferably 3.5 or more. By setting the aspect ratio of the bonding region 42 to 3.5 or more, the bonding strength between the electromagnetic steel sheets 40 can be ensured while suppressing distortion of the electromagnetic steel sheets 40.

[0096] In the present embodiment, the adhesive shrinks when solidified. Therefore, a distortion caused by the solidification shrinkage of the adhesive occurs in the region of the electromagnetic steel sheet 40 in contact with the adhesive portion 41, and the iron loss of the electromagnetic steel sheet 40 increases in this region. Here, the region in contact with the adhesive portion 41 and in which the iron loss increases due to distortion is referred to as a degraded region 29. The degraded region 29 is a region that overlaps with the adhesive region 42 when viewed from the stacking direction. The degraded region 29 has a higher magnetic resistance than other regions (non-degraded regions).

[0097] In addition, in this specification, the increase in the value of iron loss may be referred to as "deterioration of iron loss".

[0098] When current flows through the winding (not shown) of the stator 20, magnetic flux B is formed in the electromagnetic steel sheet 40. The magnetic flux B forms a magnetic path passing through the teeth 23 and the core back 22. The magnetic flux B extends in the circumferential direction at the second portion 22b of the core back 22.

[0099] According to the present embodiment, the bonding region 42 is located in the second portion 22b and extends in the circumferential direction. That is, the direction in which the bonding region 42 extends coincides with the direction in which the magnetic flux B extends in the second portion 22b. In other words, the bonding region 42 extends in the direction of the magnetic flux B passing through the degraded region 29 of the electromagnetic steel sheet 40 in contact with the bonding region 42. Therefore, the proportion of the degraded region 29 in the cross-sectional area of ​​the path of the magnetic flux B can be reduced, and the number of magnetic flux lines passing through the degraded region 29 can be suppressed. In addition, by reducing the proportion of the degraded region 29 in the cross-sectional area of ​​the path of the magnetic flux, the magnetic flux B can easily bypass the degraded region 29 with high magnetic resistance. As a result, it is possible to suppress the degraded region 29 from obstructing the flow of the magnetic flux B that forms the magnetic path, and the magnetic characteristics of the stator core 21 can be improved compared to the case where the electromagnetic steel sheets are fixed to each other by riveting.

[0100] like Figure 4 As shown, blank areas 43 where no bonding area 42 is provided are provided on the radially outer side of the bonding area 42 and the radially inner side of the bonding area 42, respectively. That is, no bonding area 42 is formed on both circumferential sides of the bonding area 42. The area of ​​the electromagnetic steel sheet 40 overlapping with the blank area 43 is not given stress accompanying the curing shrinkage of the adhesive. Therefore, the iron loss in this area does not increase compared to the degraded area 29. In this specification, the area of ​​the electromagnetic steel sheet 40 that does not produce an increase in iron loss is referred to as a non-degraded area. According to the above-mentioned structure, since non-degraded areas are provided on both radial sides of the degraded area 29, the magnetic flux B that forms the magnetic circuit can detour and pass through the non-degraded area, which can improve the magnetic properties of the stator core 21.

[0101] The magnetic flux B tends to flow through the shortest distance with low magnetic resistance. Therefore, in the core back 22, the magnetic flux density decreases as it moves from the radial inside to the radial outside. In the present embodiment, the bonding area 42 is arranged to be biased toward the radial outside of the core back 22. Therefore, the deteriorated area 29 of the electromagnetic steel sheet 40 can be formed in an area with low magnetic flux density, and the reduction in the magnetic properties of the stator core 21 caused by the provision of the bonding portion 41 can be suppressed.

[0102] According to the present embodiment, the bonding area 42 is provided in the second portion 22b, and is not provided in the first portion 22a. Therefore, the bonding area 42 is discretely arranged in the circumferential direction in the core back 22. As a result, the electromagnetic steel sheets 40 can be fixed to each other in a well-balanced manner. In addition, since the deteriorated areas 29 formed in the electromagnetic steel sheets 40 are discretely arranged, the deteriorated areas 29 are less likely to hinder the flow of the magnetic flux B. In addition, such an effect can be obtained even when the bonding area 42 is provided in the first portion 22a and is not provided in the second portion 22b. That is, as long as the bonding area 42 is discretely provided in the circumferential direction on at least one of the first portion 22a and the second portion 22b, the above effect can be obtained.

[0103] In the present embodiment, the rotor core 31 is a laminated core like the stator core 21. That is, the rotor core 31 has a plurality of electromagnetic steel plates laminated in the thickness direction. In the present embodiment, the laminated thickness of the rotor core 31 is equal to that of the stator core 21, for example, 50.0 mm. The outer diameter of the rotor core 31 is, for example, 163.0 mm. The inner diameter of the rotor core 31 is, for example, 30.0 mm. However, these values ​​are only examples, and the laminated thickness, outer diameter, and inner diameter of the rotor core 31 are not limited to these values.

[0104] In this embodiment, the plurality of electromagnetic steel sheets forming the rotor core 31 are connected by caulking C (pins, see Figure 1 However, the plurality of electromagnetic steel sheets 40 forming the rotor core 31 may be bonded to each other by the same bonding portion as the stator core 21.

[0105] (Variant 1)

[0106] Next, based on Figure 5 The adhesive portion 141 and the adhesive region 142 of Modification 1 that can be adopted in the above embodiment will be described. Note that the same reference numerals are given to components having the same form as those in the above embodiment, and description thereof will be omitted.

[0107] As in the above-described embodiment, an adhesive region 142 having an adhesive portion 141 is formed on the core back 22. The adhesive region 142 of this modified example is provided at the first portion 22a of the core back 22. In addition, the adhesive region 142 is not provided at the second portion 22b of the core back 22. One adhesive region 142 is provided at one first portion 22a. The adhesive region 142 is located at the circumferential center of the first portion 22a.

[0108] The adhesion region 142 is substantially rectangular in plan view with the radial direction as the long side direction. The aspect ratio (d2 / d1) of the adhesion region 142 is the same as in the above embodiment, and is preferably 3.5 or more.

[0109] The bonding area 142 extends radially along the center line CL of the tooth portion 23. The center line CL is an imaginary line that passes radially through the center of the circumferential direction of the tooth portion 23. The radially outer end of the bonding area 142 is located at the radially outer end of the core back 22. That is, the bonding area 142 extends radially inward from the radially outer end of the core back 22. In addition, the radially inner end of the bonding area 142 is located radially outward from the radially inner end of the core back 22.

[0110] When current flows through the winding (not shown) of the stator 20, a magnetic flux B is formed in the electromagnetic steel sheet 40. The magnetic flux B forms a magnetic path passing through the tooth portion 23 and the core back 22. The magnetic flux B extends in the radial direction in the first portion 22a of the core back 22, and branches to both sides in the circumferential direction at the radial middle of the first portion 22a. The magnetic flux B branches in symmetrical directions with respect to the center line CL of the tooth portion 23.

[0111] According to the present modification, the adhesion region 142 is located in the first portion 22a and extends in the radial direction along the center line CL of the tooth portion 23. That is, the direction in which the adhesion region 142 extends coincides with the direction in which at least a portion of the magnetic flux B extends in the first portion 22a. In other words, the adhesion region 142 extends along the direction of at least a portion of the magnetic flux passing through the deteriorated region 129 of the electromagnetic steel sheet 40 in contact with the adhesion region 142. Therefore, the proportion of the deteriorated region 129 in the path cross-sectional area of ​​the magnetic flux B can be reduced, and the number of magnetic flux lines passing through the deteriorated region 129 can be suppressed. In addition, by reducing the proportion of the deteriorated region 129 in the path cross-sectional area of ​​the magnetic flux B, the magnetic flux B easily bypasses the deteriorated region 129 with high magnetic resistance. In addition, in the present modification, since the adhesion region 142 extends along the center line CL of the tooth portion 23, the magnetic flux B branched in the symmetrical direction with respect to the center line CL easily bypasses the deteriorated region 129. As a result, it is possible to suppress the deteriorated region 129 from hindering the flow of the magnetic flux B forming the magnetic path, and the magnetic characteristics of the stator core 21 can be improved compared to the case where the electromagnetic steel sheets are fixed to each other by caulking.

[0112] like Figure 5 As shown, blank areas 143 where no bonding area 142 is provided are provided on both sides of the bonding area 142 in the circumferential direction. In the area of ​​the electromagnetic steel sheet 40 overlapping with the blank area 143, a non-degraded area is formed to which stress accompanying the curing shrinkage of the adhesive is not applied. According to the above configuration, since the non-degraded areas are provided on both sides of the degraded area 129 in the circumferential direction, the magnetic flux B forming the magnetic path can detour and pass through the non-degraded areas, and the magnetic properties of the stator core 21 can be improved.

[0113] The magnetic flux B tends to flow through the shortest distance with low magnetic resistance. Therefore, in the core back 22, the magnetic flux density decreases as it moves from the radial inside to the radial outside. In this modification, the bonding area 142 extends from the radial outer end of the core back 22. Therefore, the deteriorated area 129 of the electromagnetic steel sheet 40 can be formed in an area with low magnetic flux density, and the reduction in the magnetic characteristics of the stator core 21 caused by the provision of the bonding area 142 can be suppressed.

[0114] (Variant 2)

[0115] Next, based on Figure 6The adhesive portion 241 and the adhesive region 242 of Modification 2 that can be adopted in the above embodiment will be described. Note that the same reference numerals are given to components having the same form as those in the above embodiment, and description thereof will be omitted.

[0116] As in the above-described embodiment, an adhesive region 242 having an adhesive portion 241 is formed on the core back 22. The adhesive region 242 of this modified example is provided at the first portion 22a of the core back 22. In addition, the adhesive region 242 is not provided at the second portion 22b of the core back 22. One adhesive region 242 is provided at one first portion 22a. The adhesive region 242 is located at the circumferential center of the first portion 22a. In addition, the adhesive region 242 is arranged radially inward in the first portion 22a.

[0117] The adhesion region 242 is substantially rectangular in plan view, with the longitudinal direction being perpendicular to the radial direction. The aspect ratio (d2 / d1) of the adhesion region 242 is preferably 3.5 or more, similar to the above embodiment.

[0118] When current flows through the winding (not shown) of the stator 20, a magnetic flux B is formed in the electromagnetic steel sheet 40. The magnetic flux B forms a magnetic path passing through the teeth 23 and the core back 22. The magnetic flux B extends in the radial direction in the first portion 22a of the core back 22, and branches to both sides in the circumferential direction at the radial middle of the first portion 22a.

[0119] According to this modification, the bonding area 242 is located in the first portion 22a and extends in the circumferential direction. That is, the direction in which the bonding area 242 extends is partially consistent with the direction of the magnetic flux B that branches in the first portion 22a and extends in the circumferential direction. In other words, at least a portion of the bonding area 242 extends along the direction of the magnetic flux B that passes through the degraded area 229 of the electromagnetic steel sheet 40 that contacts the bonding area 242. Therefore, not only can the proportion of the degraded area 229 in the path cross-sectional area of ​​the magnetic flux B be reduced, but the magnetic flux B can also easily bypass the degraded area 229 with high magnetic resistance. As a result, it is possible to suppress the degraded area 229 from obstructing the flow of the magnetic flux B that forms the magnetic circuit, and the magnetic properties of the stator core 21 can be improved compared to the case where the electromagnetic steel sheets are fixed to each other by riveting.

[0120] like Figure 6 As shown, blank areas 243 where no bonding area 242 is provided are provided on both sides of the bonding area 242 in the circumferential direction. In the area of ​​the electromagnetic steel sheet 40 overlapping with the blank area 243, no non-degraded area to which stress accompanying the curing shrinkage of the adhesive is applied is formed. According to the above configuration, since the non-degraded areas are provided on both sides of the degraded area 229 in the circumferential direction, the magnetic flux B forming the magnetic path can pass through the non-degraded areas, and the magnetic properties of the stator core 21 can be improved.

[0121] (Variant 3)

[0122] Next, based on Figure 7 The adhesive portion 341 and the adhesive region 342 of Modification 3 that can be adopted in the above embodiment will be described. Note that the same reference numerals are given to components having the same form as those in the above embodiment, and description thereof will be omitted.

[0123] As in the above-described embodiment, an adhesive region 342 having an adhesive portion 341 is formed in the core back 22. The adhesive region 342 of this modification is similar in structure to the adhesive region 242 of modification 2. The adhesive region 342 of this modification differs from the adhesive region 242 of modification 2 in that the adhesive region 342 of this modification is arranged radially outward in the first portion 22a.

[0124] Since the magnetic flux B tends to flow through the shortest distance with low magnetic resistance, the magnetic flux density decreases from the radial inside to the radial outside in the core back 22. In this modification, the bonding area 342 is arranged to be biased toward the radial outside of the core back 22. Therefore, the deteriorated area 329 of the electromagnetic steel sheet 40 can be formed in an area with low magnetic flux density, and the reduction in the magnetic characteristics of the stator core 21 due to the provision of the bonding area 342 can be suppressed.

[0125] According to this modification, the adhesion region 342 is arranged radially outward of the first portion 22a and extends in the circumferential direction. Therefore, the adhesion region 342 extends in parallel with the direction of the magnetic flux B branched in the first portion 22a and extending in the circumferential direction over a larger range than the adhesion region 242 of modification 2. Therefore, not only can the proportion of the degraded region 329 in the path cross-sectional area of ​​the magnetic flux B be further reduced, but the magnetic flux B can also more easily bypass the degraded region 329 with high magnetic resistance. As a result, it is possible to suppress the degraded region 329 from obstructing the flow of the magnetic flux B forming the magnetic circuit, and the magnetic properties of the stator core 21 can be further improved compared with modification 2.

[0126] (Variant 4)

[0127] Next, based on Figure 8 The adhesive portion 441 and the adhesive region 442 of Modification 4 that can be adopted in the above-mentioned embodiment will be described. Note that the same reference numerals are given to the same components as those in the above-mentioned embodiment, and description thereof will be omitted.

[0128] As in the above embodiment, an adhesive region 442 having an adhesive portion 441 is formed on the core back 22. The adhesive region 442 of this modification is provided across a first portion 22a and a second portion 22b. In addition, the adhesive region 442 of this modification is arranged to be biased toward the radially outer side of the core back 22 and extends in the circumferential direction.

[0129] In this modification, the bonding area 442 is provided on the boundary line with the second part 22b on one circumferential side relative to one first part 22a, and is not provided on the boundary line with the second part 22b on the other circumferential side. Therefore, the bonding area 442 is formed asymmetrically with respect to the center line CL of the tooth portion 23. The density of the magnetic flux B flowing from the tooth portion 24 to the core back 22 tends to increase on the other circumferential side where the bonding area 442 is not provided, compared with the circumferential side where the bonding area 442 is provided. That is, according to this embodiment, the magnetic flux density is different on one circumferential side and the other side relative to the center line CL. Such a laminated core can improve the energy efficiency of the rotating electrical machine when used for a rotating electrical machine whose rotation direction is limited to one direction.

[0130] (Variant 5)

[0131] Next, based on Fig. 9 The adhesive portion 541 and the adhesive region 542 of the fifth modification example that can be adopted in the above embodiment will be described. Note that the same reference numerals are given to the same components as those in the above embodiment, and the description thereof will be omitted.

[0132] As in the above-mentioned embodiment, an adhesive region 542 having an adhesive portion 541 is formed on the core back 22. The adhesive region 542 of this modification is T-shaped when viewed from above, and can be considered to be a combination of the adhesive region 142 of Modification 1 and the adhesive region 342 of Modification 3. According to this modification, while enjoying the effects of Modification 1 and Modification 3, it is possible to ensure that the adhesive region 542 has a sufficient area and improve the adhesive strength. As shown in this modification, a combination of the configurations of the embodiment and each modification can also be adopted to obtain the combined effect.

[0133] In addition, the technical scope of the present invention is not limited to the above-described embodiment and its modified examples, and various changes can be added without departing from the gist of the present invention.

[0134] In the stator core of the above-mentioned embodiment and its modified example, a plurality of electromagnetic steel sheets are fixed to each other in the bonding area provided at the back of the core. However, the electromagnetic steel sheets may be fixed to each other at the teeth in addition to the back of the core. In this case, rivets may be provided at the teeth, and a bonding area may be provided separately at the teeth. Furthermore, the electromagnetic steel sheets may be fixed to each other by welding in addition to the bonding and fixing by the bonding area.

[0135] In the above embodiment and its modified example, the width dimension of the bonding area is the same throughout the entire length of the bonding area. However, the width dimension of the bonding area may not necessarily be the same. As an example, both ends of the bonding area in the width direction may also be bent and extended along the length direction.

[0136] The shape of the stator core is not limited to the form shown in the above embodiment. Specifically, the outer diameter and inner diameter of the stator core, the stacking thickness, the number of slots, the circumferential and radial dimension ratios of the teeth, the radial dimension ratios of the teeth and the back of the core, etc. can be arbitrarily designed according to the desired characteristics of the rotating electrical machine.

[0137] In the rotor of the embodiment, a set of two permanent magnets 32 forms one magnetic pole, but the present invention is not limited thereto. For example, one permanent magnet 32 ​​may form one magnetic pole, or three or more permanent magnets 32 may form one magnetic pole.

[0138] In the above-described embodiment, a permanent magnet excitation type motor is described as an example of a rotating electrical machine. However, the structure of the rotating electrical machine is not limited to this as exemplified below, and various known structures not exemplified below may be adopted.

[0139] In the above embodiment, a permanent magnet excitation type motor is exemplified as a synchronous motor, but the present invention is not limited thereto. For example, the rotating electric machine may be a reluctance type motor or an electromagnetic excitation type motor (winding excitation type motor).

[0140] In the above embodiment, a synchronous motor is described as an example of an AC motor, but the present invention is not limited to this. For example, the rotating electrical machine may be an induction motor.

[0141] In the above embodiment, an AC motor is described as an example of a motor, but the present invention is not limited to this. For example, the rotating electrical machine may be a DC motor.

[0142] In the above embodiment, an electric motor is described as an example of a rotating electrical machine, but the present invention is not limited to this. For example, the rotating electrical machine may be a generator.

[0143] In the above-described embodiment, the case where the laminated core of the present invention is applied to a stator core is exemplified, but it may also be applied to a rotor core.

[0144] Furthermore, components in the above-described embodiment and its modified examples may be appropriately replaced with well-known components without departing from the gist of the present invention, and the above-described modified examples may be appropriately combined.

[0145] [Example]

[0146] A verification test was carried out to verify the suppression of the degradation of the iron loss of the electromagnetic steel sheet caused by the compressive stress in the bonding portion. In addition, this verification test was carried out by simulation using software. As software, JMAG, a finite element method electromagnetic field analysis software manufactured by JSOL Co., Ltd., was used. As the model used in the simulation, the stator core (laminated core) of Model No. 1 to Model No. 4 described below is assumed. The electromagnetic steel sheet used in each model is an electromagnetic steel sheet produced by punching a thin plate with a thickness of 0.25 mm. The shape of the electromagnetic steel sheet and Figure 2 The shapes shown are the same.

[0147] The stator cores of models No. 1 to No. 3 and model No. 4 have different structures for fixing the electromagnetic steel sheets to each other. In the stator cores of models No. 1 to No. 3, bonding portions are provided between the electromagnetic steel sheets, and the electromagnetic steel sheets are bonded and fixed to each other. On the other hand, the stator core of model No. 4 fixes the electromagnetic steel sheets to each other by caulking.

[0148] The bonding part of model No.1 is equivalent to Figure 4 The bonding portion 41 shown. The bonding region of the bonding portion of Model No. 1 extends in the circumferential direction at the second location of the core back.

[0149] The bonding part of model No.2 is equivalent to Figure 5 The bonding portion 141 shown. The bonding region of the bonding portion of Model No. 2 extends in the radial direction at the first portion of the core back.

[0150] The bonding part of model No.3 is equivalent to Figure 6 The bonding portion 241 shown. The bonding region of the bonding portion of Model No. 3 extends in the circumferential direction at the first portion of the core back.

[0151] The stator core 1021 of model No. 4 is shown in Fig.11 The stator core 1021 is formed by stacking electromagnetic steel sheets 40 of the same shape as the stator core 21 of the above embodiment in the thickness direction. The stator core 1021 is different from the stator core 21 of the above embodiment in that the electromagnetic steel sheets 40 are fixed to each other by rivets 1042 (pins). The rivets 1042 are located at the second portion 22b of the core back 22.

[0152] The calculation results of the iron loss of the electromagnetic steel sheet calculated by the simulation software for each model are shown in FIG. Fig.10 .in addition, Fig.10 In the iron loss (vertical axis) of the calculation results shown, the iron loss of model No. 4 is set to 1.0, and the iron loss of other models is expressed as a ratio to the iron loss of model No. 4.

[0153] like Fig.10 As shown, it was confirmed that the stator cores of Model No. 1 to Model No. 3 had smaller iron loss values ​​than the stator core of Model No. 4.

[0154] The stator core of model No.3 has a larger iron loss than the stator cores of models No.1 and No.2. Figure 6 As shown in FIG. 1 , in the stator core of model No. 3, the bonding area is located near the boundary between the tooth portion and the core back. Therefore, it is considered that the magnetic resistance increases due to the increase in magnetic flux passing through the deteriorated area caused by the bonding area. Therefore, in the stator core of model No. 3, as shown in FIG. Figure 7 As shown, it is considered that the iron loss value can be reduced by arranging the bonding area to be offset toward the radially outer side of the core back.

[0155] Industrial Availability

[0156] According to the present invention, magnetic properties can be improved, and thus the industrial applicability is great.

[0157] Description of Reference Numerals

[0158] 10…rotating electric machine, 20…stator, 21…stator core (laminated core), 22…core back, 22a…first part, 22b…second part, 23…tooth part, 40…electromagnetic steel plate, 41, 141, 241, 341, 441, 541…bonding part, 42, 142, 242, 342, 442, 542…bonding area, 43, 143, 243…blank area, B…magnetic flux, CL…center line.

Claims

1. A laminated core comprising: a plurality of electromagnetic steel plates stacked one on top of the other; as well as a bonding portion provided between the electromagnetic steel sheets adjacent to each other in the stacking direction and bonding the electromagnetic steel sheets to each other; The electromagnetic steel plate has: The annular core back, and a plurality of teeth extending from the core back in a radial direction of the core back and arranged at intervals in a circumferential direction of the core back; A bonding area provided with the bonding portion is formed on the core back of the electromagnetic steel sheet; The bonding region extends in a direction along a magnetic flux passing through a region of the electromagnetic steel sheet in contact with the bonding region; The core back has a first portion and a second portion arranged alternately along the circumferential direction; The first portion is connected to the tooth portion in the radial direction on the radial outer side of the tooth portion; The second portion is located between the first portions in the circumferential direction; The adhesive region is formed only at one of the first portion and the second portion. The boundary line between the first portion and the second portion is an imaginary line that linearly extends from the circumferential end of the tooth portion in the radial direction at the connection portion between the first portion and the tooth portion and passes through the core back portion.

2. The laminated core according to claim 1, wherein: The bonding portion is formed of an adhesive.

3. The laminated core according to claim 1, wherein: In the first part or the second part where the adhesive region is provided, Blank areas where the adhesion area is not formed are arranged on both sides in the circumferential direction and both sides in the radial direction of the adhesion area.

4. The laminated core according to claim 1, wherein: The bonding area is formed at the first portion; The bonding area is not formed on both sides in the circumferential direction of the bonding area.

5. The laminated core according to claim 4, wherein: The bonding area extends in a radial direction along a center line of the tooth.

6. The laminated core according to claim 4, wherein: The tooth portion extends radially inward from the back of the core; The bonding area extends from the radial outer end of the core back to the radial inner side; The radially inner end of the bonding region is located radially outward of the radially inner end of the core back portion.

7. The laminated core according to claim 1, wherein: The bonding area is provided at the second portion; The bonding area is not formed on both sides of the bonding area in the radial direction.

8. The laminated core according to claim 7, wherein: The bonding area extends in the circumferential direction.

9. The laminated core according to claim 7, wherein: The tooth portion extends radially inward from the back of the core; The bonding area is arranged to be biased toward the radial outer side of the core back.

10. The laminated core according to any one of claims 1 to 9, wherein: The average thickness of the adhesive portion is 1.0 μm to 3.0 μm.

11. The laminated core according to any one of claims 1 to 9, wherein: The average tensile elastic modulus E of the bonding portion is 1500 MPa to 4500 MPa.

12. The laminated core according to any one of claims 1 to 9, wherein: The adhesive portion is an acrylic adhesive of a room temperature adhesive type including SGA composed of an acrylic adhesive containing an elastomer.

13. A rotating electric machine comprising the laminated core according to any one of claims 1 to 12.

Citation Information

Patent Citations

  • Electromagnetic steel sheet laminated core which has good thermal conductivity, and method of manufacturing the same

    JP2011023523A

  • Laminated core and manufacturing method thereof

    JP2016073109A

  • Laminated core, method and apparatus for manufacturing laminated core, and stator

    US20090195110A1

  • Permanent magnet-embedded motor, compressor, and refrigerating and air conditioning device

    WO2017033229A1