Semiconductor devices and electronic equipment

By optimizing the semiconductor device structure of the liquid crystal display and utilizing the area where oxide semiconductor films overlap on the insulating film to arrange transistors, the problems of low aperture ratio, low integration density, and high power consumption were solved, achieving high definition and high-speed operation.

CN113314545BActive Publication Date: 2024-10-29SEMICON ENERGY LAB CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202110383436.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2016-04-11
Publication Date
2024-10-29
Estimated Expiration
2036-04-11

AI Technical Summary

Technical Problem

In the existing technology, liquid crystal displays have low pixel aperture ratio, low integration, high power consumption, and insufficient transistor on-state current, making it difficult to achieve high-speed operation.

Method used

A semiconductor device structure including a first wiring, a second wiring, a third wiring, a first driving circuit, a second driving circuit, and a unit array is adopted. Transistors are arranged in the area where the oxide semiconductor film overlaps on the insulating film. The circuit design is optimized by connecting the second wiring and the third wiring, thereby improving the current driving capability of the transistors.

Benefits of technology

The increased aperture ratio of the pixel section enhances the high definition and integration of the display device, reduces power consumption, and increases the on-state current of the transistor, enabling high-speed operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113314545B_ABST
    Figure CN113314545B_ABST
Patent Text Reader

Abstract

One of the purposes of one embodiment of the present invention is to provide a semiconductor device with an improved aperture ratio. In addition, a semiconductor device capable of reducing power consumption is provided. One embodiment of the present invention is a semiconductor device, comprising: a first wiring, a second wiring, a third wiring, a first drive circuit, a second drive circuit, and a cell array, wherein the cell array includes a plurality of cells including transistors and storage capacitors. The first wiring is electrically connected to the first drive circuit, the second wiring is electrically connected to the second drive circuit, the transistor is arranged above the second wiring, the second wiring includes a region serving as a first gate electrode of the transistor in a region overlapping with the transistor, the third wiring is arranged above the transistor and includes a region overlapping with the second wiring, and the second wiring is electrically connected to the third wiring in a region outside the cell array.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of the following invention patent application:

[0002] Invention name: Semiconductor device and electronic device; Application date: April 11, 2016; Application number: 201680023158.8. Technical Field

[0003] One embodiment of the present invention relates to a semiconductor device. Note that one embodiment of the present invention is not limited to the above-mentioned technical field. The technical field of one embodiment of the invention disclosed in this specification and the like relates to an object, a method or a manufacturing method. Alternatively, one embodiment of the present invention relates to a process, a machine, a product or a composition of matter. Therefore, more specifically, as examples of the technical field of one embodiment of the present invention disclosed in this specification, semiconductor devices, display devices, liquid crystal display devices, light-emitting devices, power storage devices, imaging devices, storage devices and methods for driving these devices or methods for manufacturing these devices can be cited. Background Art

[0004] In recent years, flat panel displays such as liquid crystal displays (LCDs) have become widely popular. In display devices such as flat panel displays, pixels arranged in row and column directions are provided with transistors as switching elements, liquid crystal elements electrically connected to the transistors, and capacitor elements connected in parallel to the liquid crystal elements.

[0005] As a semiconductor material for a semiconductor film constituting the transistor, a silicon semiconductor such as amorphous silicon or polycrystalline silicon is generally used.

[0006] In addition, metal oxides that exhibit semiconductor properties (hereinafter also referred to as oxide semiconductors) are also semiconductor materials that can be used as semiconductor films of transistors. For example, a technology for manufacturing transistors using zinc oxide or In-Ga-Zn-based oxide semiconductors has been disclosed (see Patent Documents 1 and 2). In addition to display devices, oxide semiconductors are also used in various devices such as memory and CPU (see Patent Document 3).

[0007] [References]

[0008] [Patent Document]

[0009] [Patent Document 1] Japanese Patent Application Publication No. 2014-63141

[0010] [Patent Document 2] Japanese Patent Application Publication No. 2014-199402

[0011] [Patent Document 3] Japanese Patent Application Publication No. 2012-257187 Summary of the invention

[0012] One of the purposes of one embodiment of the present invention is to provide a display device including a pixel portion with a high aperture ratio. In addition, one of the purposes of one embodiment of the present invention is to provide a high-definition display device. In addition, one of the purposes of one embodiment of the present invention is to provide a semiconductor device with a high degree of integration. In addition, one of the purposes of one embodiment of the present invention is to provide a semiconductor device with low power consumption. In addition, one of the purposes of one embodiment of the present invention is to provide a semiconductor device including a transistor with a high on-state current. In addition, one of the purposes of one embodiment of the present invention is to provide a semiconductor device that operates at a high speed.

[0013] In addition, one of the purposes of one embodiment of the present invention is to provide a novel semiconductor device. In addition, one of the purposes of one embodiment of the present invention is to provide a module including the semiconductor device. In addition, one of the purposes of one embodiment of the present invention is to provide an electronic device including the semiconductor device or the module. In addition, one of the purposes of one embodiment of the present invention is to provide a method for manufacturing the semiconductor device.

[0014] Note that the recording of these purposes does not prevent the existence of other purposes. One mode of the present invention does not need to achieve all of the above purposes. In addition, the description of the specification, drawings, claims, etc. clearly contains purposes other than the above purposes, and the purposes other than the above purposes can be obtained from the description of the specification, drawings, claims, etc.

[0015] One embodiment of the present invention is a semiconductor device, which includes a first wiring, a second wiring, a third wiring, a first driving circuit, a second driving circuit, and a cell array. The cell array includes a plurality of cells including transistors and storage capacitors. The transistor includes a first insulating film, an oxide semiconductor film, and a second insulating film. The oxide semiconductor film includes a region overlapping the second wiring across the first insulating film and a region overlapping the third wiring across the second insulating film. The first wiring is electrically connected to the first driving circuit, and the second wiring is electrically connected to the second driving circuit. The transistor is arranged above the second wiring, and the second wiring includes a region serving as a first gate electrode of the transistor in a region overlapping with the transistor. In addition, the third wiring is arranged above the transistor and includes a region serving as a second gate electrode of the transistor in a region overlapping with the transistor. Furthermore, the third wiring includes a region overlapping with the second wiring, and the second wiring is electrically connected to the third wiring in a region outside the cell array.

[0016] The second wiring and the third wiring may be electrically connected in at least one cell.

[0017] One embodiment of the present invention is a semiconductor device, which includes a first wiring, a second wiring, a third wiring, a first driving circuit, a second driving circuit, a third driving circuit and a cell array. A cell array is arranged between the second driving circuit and the third driving circuit. The cell array includes a plurality of cells including transistors and storage capacitors. The transistor includes a first insulating film, an oxide semiconductor film and a second insulating film. The oxide semiconductor film includes a region overlapping the second wiring across the first insulating film and a region overlapping the fourth wiring across the second insulating film. The first wiring is electrically connected to the first driving circuit, and the second wiring is electrically connected to the second driving circuit or the third driving circuit. The transistor is arranged above the second wiring, and the second wiring includes a region serving as a first gate electrode of the transistor in a region overlapping with the transistor. In addition, the third wiring is arranged above the transistor and includes a region serving as a second gate electrode of the transistor in a region overlapping with the transistor. Furthermore, the third wiring includes a region overlapping with the second wiring, and the second wiring is electrically connected to the third wiring in a region outside the cell array.

[0018] The second wiring and the third wiring may be electrically connected in a region between the cell array and the second driver circuit.

[0019] The width of the second wiring in the connection portion between the second wiring and the third wiring may be larger than the width of the second wiring in the region overlapping with the cell.

[0020] The resistance of the third wiring may be lower than the resistance of the second wiring.

[0021] The third wiring may also include copper.

[0022] In addition, the unit may be a pixel, and the unit array may be a pixel unit.

[0023] One embodiment of the present invention is an electronic device including the above-mentioned semiconductor device.

[0024] According to one embodiment of the present invention, a display device including a pixel portion with a high aperture ratio can be provided. In addition, a high-definition display device can be provided. In addition, a semiconductor device with a high degree of integration can be provided. In addition, a semiconductor device with low power consumption can be provided. In addition, a semiconductor device including a transistor with a high on-state current can be provided. In addition, a semiconductor device that operates at a high speed can be provided.

[0025] In addition, a novel semiconductor device can be provided. In addition, a module including the semiconductor device can be provided. In addition, an electronic device including the semiconductor device or the module can be provided. In addition, a method for manufacturing the semiconductor device can be provided.

[0026] In addition, one embodiment of the present invention does not necessarily have all of the above effects. Effects other than the above effects are obvious from the description of the specification, drawings, claims, etc., and effects other than the above effects can be extracted from the description. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 is a top view showing one aspect of a display device;

[0028] Figure 2 is a top view showing one aspect of a display device;

[0029] Figure 3 is a top view showing one aspect of a display device;

[0030] Figure 4 A top view and a cross-sectional view showing one embodiment of a semiconductor device;

[0031] Figure 5 A top view and a cross-sectional view showing one embodiment of a semiconductor device;

[0032] Figure 6 A top view and a cross-sectional view showing one embodiment of a semiconductor device;

[0033] Figure 7 A top view and a cross-sectional view showing one embodiment of a semiconductor device;

[0034] Figure 8 A top view and a cross-sectional view showing one embodiment of a semiconductor device;

[0035] Fig. 9 is a diagram illustrating the band structure;

[0036] Fig.10 A diagram illustrating structural analysis of CAAC-OS and a single crystal oxide semiconductor using XRD and a diagram showing a selected area electron diffraction pattern of CAAC-OS;

[0037] Fig.11 The cross-sectional TEM image, planar TEM image, and analysis image of CAAC-OS;

[0038] Fig.12 is a diagram showing an electron diffraction pattern of nc-OS and a cross-sectional TEM image of nc-OS;

[0039] Fig.13 is the cross-sectional TEM image of a-like OS;

[0040] Fig.14 is a diagram showing changes in the crystal part of In-Ga-Zn oxide due to electron irradiation;

[0041] Fig.15 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0042] Fig.16 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0043] Fig.17 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0044] Fig.18 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0045] Fig.19 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0046] Fig. 20 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0047] Fig.21 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0048] Fig. 22 is a cross-sectional view showing one embodiment of a semiconductor device;

[0049] Fig.23 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0050] Fig.24 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0051] Fig.25 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0052] Fig.26 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0053] Fig. 27 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0054] Fig.28 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0055] Fig.29 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0056] Fig.30 is a plan view and a cross-sectional view showing an example of a manufacturing process of a semiconductor device;

[0057] Fig.31 is a cross-sectional view showing one embodiment of a display device;

[0058] Fig.32 is a circuit diagram showing one embodiment of a storage device;

[0059] Fig.33 is a circuit diagram showing one embodiment of a storage device;

[0060] Fig.34 is a cross-sectional view showing one embodiment of a storage device;

[0061] Fig.35 is a cross-sectional view showing one embodiment of a storage device;

[0062] Fig.36 is a cross-sectional view showing one embodiment of a storage device;

[0063] Fig.37 is a diagram illustrating a display module;

[0064] Fig.38 It is a diagram for explaining an electronic device. DETAILED DESCRIPTION

[0065] Below, the embodiments of the present invention will be described with reference to the accompanying drawings. However, the present invention is not limited to the following description. A person skilled in the art can easily understand that the mode and details can be transformed into various forms without departing from the purpose and scope of the present invention. Therefore, the present invention should not be interpreted as being limited to the contents described in the embodiments shown below. Note that when describing the structure of the present invention with reference to the accompanying drawings, the same reference numerals are used in common in different drawings to represent the same constituent elements.

[0066] In the accompanying drawings, for the sake of clarity, the size, thickness of the layer or the region are sometimes exaggerated. Therefore, the present invention is not necessarily limited to the above-mentioned dimensions. In addition, in the accompanying drawings, ideal examples are schematically shown, so the present invention is not limited to the shapes or numerical values ​​shown in the accompanying drawings.

[0067] The terms “first”, “second”, “third” to “n” (n is a natural number) etc. used in the present specification are used to avoid confusion among constituent elements and are not used to limit the number.

[0068] In this specification, for convenience, words and phrases such as "upper" and "lower" indicating configuration are used to explain the positional relationship of the components with reference to the drawings. In addition, the positional relationship of the components is appropriately changed according to the direction in which each component is described. Therefore, the words and phrases described in this specification are not limited and can be appropriately replaced according to the situation.

[0069] In this specification, etc., a transistor refers to an element including at least three terminals: a gate, a drain, and a source. A transistor has a channel region between a drain (drain terminal, a drain region, or a drain electrode) and a source (source terminal, a source region, or a source electrode), and current can flow through the drain, the channel region, and the source. Note that in this specification, etc., a channel region refers to a region where current mainly flows.

[0070] When transistors with different polarities are used or when the direction of current changes during circuit operation, the functions of the source and the drain may be interchanged. Therefore, in this specification, etc., the source and the drain may be interchanged.

[0071] In this specification, "electrical connection" includes connection through "an element having some kind of electrical function". Here, "an element having some kind of electrical function" is not particularly limited as long as it can transmit and receive electrical signals between the connected objects. For example, "an element having some kind of electrical function" includes not only electrodes and wiring, but also switching elements such as transistors, resistors, inductors, capacitors, and other elements having various functions.

[0072] Depending on the situation or condition, the words "film" and "layer" may be interchanged. For example, "conductive layer" may be replaced by "conductive film". Also, "insulating film" may be replaced by "insulating layer".

[0073] In this specification and the like, the oxide conductive film may be referred to alternatively as an oxide semiconductor film having high carrier density and low resistance, an oxide semiconductor film having conductivity, or an oxide semiconductor film having high conductivity.

[0074] In this specification, a pixel portion refers to a region that includes a scan line, a signal line, a transistor serving as a selection switch, a storage capacitor, a pixel electrode, and a counter electrode and is used to optically modulate an RGB image.

[0075] In addition, depending on the situation or circumstances, the words "pixel" and "pixel portion" may be interchanged.

[0076] In addition, in this specification, the words "pixel" and "unit" can be interchanged depending on the situation or condition. In addition, the words "pixel portion" and "unit array" can be interchanged depending on the situation or condition.

[0077] Implementation Method 1

[0078] In this embodiment, the following reference Figures 1 to 3 An example of a semiconductor device including a transistor will be described.

[0079] Figure 1 A is a plan view showing an example of a semiconductor device. Figure 1 The semiconductor device 700 shown in A includes a first substrate 701, a pixel portion 702, a source driver 704, a second substrate 705, a gate driver 706, an FPC terminal portion 708 (FPC: Flexible Printed Circuit), a wiring 710, a sealant 712, an FPC 716, a scan line 717, a wiring 718, a contact hole 719 and a signal line 720.

[0080] A pixel portion 702, a source driver 704, a gate driver 706, an FPC terminal portion 708, a wiring 710, an FPC 716, a scanning line 717, and a signal line 720 are provided over the first substrate 701. In addition, a second substrate 705 is provided so as to face the first substrate 701. Note that Figure 1 Although not shown in FIG. 1A, a display element is provided between the first substrate 701 and the second substrate 705. The first substrate 701 and the second substrate 705 are sealed by a sealant 712. That is, the pixel portion 702, the source driver 704, and the gate driver 706 are sealed by the first substrate 701, the sealant 712, and the second substrate 705.

[0081] The pixel portion 702 includes a plurality of pixels 703 arranged in a matrix of p rows and q columns (p and q are integers greater than or equal to 2), and although not shown, transistors serving as selection switches for the pixels 703 are arranged on the scan lines 717. In addition, the wiring 718 is provided so as to overlap with the scan lines 717.

[0082] The FPC terminal portion 708 is electrically connected to the pixel portion 702, the source driver 704, and the gate driver 706. In addition, the FPC terminal portion 708 is connected to the FPC 716, and various signals and the like are supplied to the pixel portion 702, the source driver 704, and the gate driver 706 through the FPC 716. In addition, the pixel portion 702, the source driver 704, the gate driver 706, and the FPC terminal portion 708 are each connected to the wiring 710. Various signals and the like supplied by the FPC 716 are supplied to the pixel portion 702, the source driver 704, the gate driver 706, and the FPC terminal portion 708 through the wiring 710.

[0083] The scan line 717 is connected to the gate driver 706 , and the signal line 720 is connected to the source driver 704 .

[0084] The scan line 717 and the wiring 718 are electrically connected through a contact hole 719 provided in a region outside the pixel portion 702. Thus, there is no need to provide a contact hole for electrically connecting the scan line 717 and the wiring 718 to the pixel 703, and the aperture ratio of the pixel portion 702 can be increased.

[0085] Note that although the contact hole 719 is provided in the region 722 between the pixel portion 702 and the wiring 710 , the present invention is not limited to this. For example, the contact hole 719 may be provided in the region 721 between the pixel portion 702 and the gate driver 706 .

[0086] Figure 1 B shows Figure 1 A is an enlarged view of the area 730. In addition, Figure 1 C shows the position of the contact hole 719 and Figure 1 A. Figure 1 B is an enlarged view of region 730 under different conditions. Figure 1 In B, the pixel 703 is separated from the contact hole 719, but it can also be Figure 1 As shown in C, the pixel 703 is in contact with the contact hole 719.

[0087] The scanning line 717 is used as a first gate electrode of a transistor which is provided in the pixel 703 and has a function of selecting a switch, and the wiring 718 is used as a second gate electrode. The details will be described in Embodiment 2. By forming the second gate electrode, the current driving capability of the transistor is improved, thereby obtaining a high on-state current characteristic. In addition, since the on-state current can be increased, the transistor can be miniaturized.

[0088] The scanning line 717 and the wiring 718 can be formed using a metal element selected from chromium (Cr), copper (Cu), aluminum (Al), gold (Au), silver (Ag), zinc (Zn), molybdenum (Mo), tantalum (Ta), titanium (Ti), tungsten (W), manganese (Mn), nickel (Ni), iron (Fe), cobalt (Co), an alloy containing the above metal elements, or an alloy combining the above metal elements.

[0089] In addition, the scanning line 717 and the wiring 718 may have a single-layer structure or a stacked structure of two or more layers. For example, there can be cited: a single-layer structure of an aluminum film containing silicon; a two-layer structure in which a titanium film is stacked on an aluminum film; a two-layer structure in which a titanium film is stacked on a titanium nitride film; a two-layer structure in which a tungsten film is stacked on a titanium nitride film; a two-layer structure in which a tungsten film is stacked on a tantalum nitride film or a tungsten nitride film; and a three-layer structure in which a titanium film, an aluminum film, and a titanium film are stacked in sequence; etc. In addition, an alloy film or a nitride film formed by combining aluminum with one or more selected from titanium, tantalum, tungsten, molybdenum, chromium, neodymium, and scandium can also be used.

[0090] Alternatively, a Cu-X alloy film (X is Mn, Ni, Cr, Fe, Co, Mo, Ta, or Ti) may be used. By using the Cu-X alloy film, wiring resistance can be reduced.

[0091] In addition, light-transmitting conductive materials such as indium tin oxide, indium tungsten oxide, indium zinc tungsten oxide, indium titanium oxide, indium tin titanium oxide, indium zinc oxide, and indium tin silicon oxide may also be used. In particular, light-transmitting conductive materials such as indium tungsten oxide, indium zinc tungsten oxide, indium titanium oxide, indium tin titanium oxide, indium tin oxide (ITO), indium zinc oxide, and indium tin silicon oxide (ITSO) may be used.

[0092] Furthermore, a low-resistance oxide semiconductor film may be used. As the oxide semiconductor film, zinc oxide or an In-Ga-Zn-based oxide semiconductor film may be used. In addition, the same material as the oxide semiconductor film described in Embodiment 2 may be used. As a method of reducing resistance, a method of forming an insulating film containing a large amount of hydrogen in contact with the oxide semiconductor film may be cited. Since the oxide semiconductor film can be used as a transparent electrode, the aperture ratio does not decrease when the oxide semiconductor film is used for wiring 718.

[0093] The scanning line 717 and the wiring 718 may be formed of the same material or different materials. However, since signal delay occurs when the scanning line 717 and the wiring 718 have different resistances, it is preferable to adjust the width of the scanning line 717 and the wiring 718 so that their resistances are equal. Alternatively, the wiring 718 may have a lower resistance than the scanning line 717.

[0094] In addition, if Figure 2 As shown in FIG. 1A , signal delay can be reduced by providing a plurality of contact holes 719 for electrically connecting the scan line 717 and the wiring 718. For example, a contact hole 719a and a contact hole 719b can be provided, that is, a contact hole 719a can be provided in the region 721, and a contact hole 719b can be provided in the region 722.

[0095] Furthermore, in the pixel portion 702, a contact hole other than the contact hole 719a and the contact hole 719b may be provided. Figure 2 B is a top view of the semiconductor device 700 in the following case: in addition to the contact holes 719a and 719b, a contact hole 719c is provided in the pixel 703[2,n] of the pixel portion 702. The contact hole 719c can be provided at any position as long as it is provided at a position where the scanning line 717 overlaps with the wiring 718. Note that in this specification, for example, the pixel 703 in the mth row (m is a natural number less than p) and the nth column (n is a natural number less than q) is described as a pixel 703[m,n].

[0096] In addition, in addition to the contact holes 719a and the contact holes 719b, contact holes may be provided in each plurality of pixels. For example, contact holes may be provided in any m rows of pixels 703 [m, n]. For example, contact holes may be provided in all odd rows of pixels 703 [(odd numbers such as 1, 3, 5), n] or in all even rows of pixels 703 [(even numbers such as 2, 4, 6), n]. Furthermore, for example, contact holes may be provided in all rows of pixels 703 [(multiples of 3 such as 3, 6, 9), n]. Furthermore, for example, contact holes may be provided in all rows of pixels 703 [(multiples of 4 such as 4, 8, 12), n]. Furthermore, for example, contact holes can be set in pixels 703 [(x, 2x, 3x, etc., multiples of x), n] in all rows of multiples of x (x is a natural number less than p), and contact holes can be set in pixels 703 [(x+y, 2x+y, 3x+y, etc.), n] in all rows of "multiples of x + y" (x is a natural number less than p, y is a natural number less than x).

[0097] In addition, the formation positions of the above-mentioned contact holes may be combined. For example, contact holes may be provided in all pixels 703 in rows that are multiples of 3 or rows that are multiples of 4 [(3, 4, 6, 8, 9, 12, etc., multiples of 3 or multiples of 4), n].

[0098] Since the shorter the distance between the contact holes, the smaller the signal delay, by providing contact holes in addition to the contact holes 719a and the contact holes 719b in the pixel portion 702, the signal delay of the scanning line 717 and the wiring 718 can be reduced compared to the case where no contact holes are provided in the pixel portion 702. Since the greater the number of contact holes, the shorter the distance between the contact holes, the signal delay can be reduced. Note that the distances between the contact holes are preferably as equal as possible, but they may be different.

[0099] In one embodiment of the present invention, since contact holes for electrically connecting the scan lines 717 and the wirings 718 are not provided in all pixels 703 , providing contact holes in the pixel portion 702 can also improve the aperture ratio of the pixel portion 702 compared to the case where contact holes are provided in all pixels 703 .

[0100] In addition, if Figure 3As shown, a plurality of gate drivers may be provided in the semiconductor device 700. For example, a gate driver 706a and a gate driver 706b may be provided. For example, by connecting the scanning line 717a connected to the pixels 703 of odd rows [(1, 3, 5, etc. odd numbers), n] to the gate driver 706a and connecting the scanning line 717b connected to the pixels 703 of even rows [(2, 4, 6, etc. even numbers), n] to the gate driver 706b, the area of ​​the contact hole 719 may be enlarged. Note that Figure 2 Likewise, a plurality of contact holes 719 may be provided.

[0101] In addition, Figure 3 In the embodiment, the width of the scan line 717 and the wiring 718 around the contact hole 719 is larger than the width of the portion outside the contact hole 719. On the other hand, by increasing only the width of the scan line 717 around the contact hole 719, the width of the wiring 718 around the contact hole 719 can be made equal to the width of the wiring 718 outside the contact hole 719.

[0102] In addition, as the semiconductor device 700, although an example is shown in which the source driver 704 and the gate driver 706 are formed on the same first substrate 701 as the pixel portion 702, the present invention is not limited to this structure. For example, only the gate driver 706 may be formed on the first substrate 701. Alternatively, only the source driver 704 may be formed on the first substrate 701. In this case, a structure in which a substrate having a source driver circuit or a gate driver circuit (for example, a driver circuit substrate formed of a single crystal semiconductor film or a polycrystalline semiconductor film) is mounted on the first substrate 701 may be adopted. In addition, there is no particular limitation on the connection method of the separately formed driver circuit substrate, and a COG (Chip On Glass) method, a wire bonding method, or the like may be adopted.

[0103] The pixel portion 702 , the source driver 704 , and the gate driver 706 included in the semiconductor device 700 include a plurality of transistors, and these transistors can be applied as transistors of the semiconductor device of one embodiment of the present invention.

[0104] In addition, the semiconductor device 700 can be used in various ways or have various display elements. As display elements, for example, liquid crystal elements, EL (electroluminescent) elements (EL elements including organic and inorganic materials, organic EL elements or inorganic EL elements) including LEDs (white LEDs, red LEDs, green LEDs, blue LEDs, etc.), transistors (transistors that emit light according to current), electron emission elements, electrophoretic elements, display elements using micro-electromechanical systems (MEMS) such as grating light valves (GLV), digital micromirror devices (DMDs), digital micro shutters (DMS) elements, MIRASOL (registered trademark) displays, interferometric modulation (IMOD) elements, piezoelectric ceramic displays, etc., electrowetting (electrowetting) elements, etc. In addition, display media that change due to electrical or magnetic effects such as contrast, brightness, reflectivity, and transmittance can also be included. In addition, quantum dots can also be used as display elements. As examples of display devices using liquid crystal elements, there are liquid crystal displays (transmissive liquid crystal displays, semi-transmissive liquid crystal displays, reflective liquid crystal displays, direct-view liquid crystal displays, and projection liquid crystal displays). As an example of a display device using EL elements, there are EL displays, etc. As an example of a display device using electron emission elements, there are field emission displays (FED) or SED flat-panel displays (SED: Surface-conduction Electron-emitter Display: surface-conduction electron emission display), etc. As an example of a display device using quantum dots, there are quantum dot displays, etc. As an example of a display device using electronic ink or electrophoretic elements, there are electronic paper, etc. Note that when a semi-transmissive liquid crystal display or a reflective liquid crystal display is implemented, part or all of the pixel electrode can function as a reflective electrode. For example, part or all of the pixel electrode can contain aluminum, silver, etc. In addition, at this time, a storage circuit such as SRAM can also be set under the reflective electrode. Thereby, power consumption can be further reduced.

[0105] As a display mode of the semiconductor device 700, a progressive scanning mode or an interlaced scanning mode can be adopted. In addition, the color element controlled in the pixel when performing color display is not limited to the three colors of RGB (R represents red, G represents green, and B represents blue). For example, it can be composed of four pixels of R pixel, G pixel, B pixel and W (white) pixel. Alternatively, as in the PenTile arrangement, a color element can be composed of two colors in RGB, and two different colors can be selected according to the color element. Alternatively, one or more colors such as yellow, cyan, magenta, etc. can be added to RGB. In addition, the size of the display area of ​​each color element point can be different. However, the disclosed invention is not limited to a display device for color display, but can also be applied to a display device for black and white display.

[0106] In addition, in order to use white light (W) for backlight (organic EL element, inorganic EL element, LED, fluorescent lamp, etc.) to enable the display device to display in full color, a coloring layer (also called a filter) can also be used. As a coloring layer, for example, red (R), green (G), blue (B), yellow (Y), etc. can be used in appropriate combinations. By using a coloring layer, the color reproducibility can be further improved compared to the case where a coloring layer is not used. At this time, it is also possible to directly use white light in the area that does not include the coloring layer for display by setting an area including the coloring layer and an area that does not include the coloring layer. By partially setting an area that does not include the coloring layer, when displaying a bright image, the brightness reduction caused by the coloring layer can sometimes be reduced and the power consumption can be reduced by about 20% to 30%. However, when using self-luminous elements such as organic EL elements or inorganic EL elements for full-color display, R, G, B, Y, and white (W) can also be emitted from elements with each luminous color. By using a self-luminous element, power consumption can sometimes be further reduced compared to the case where a coloring layer is used.

[0107] The structure described in this embodiment mode can be implemented in combination with the structures described in other embodiment modes as appropriate.

[0108] Implementation Method 2

[0109] In this embodiment, refer to Figures 4 to 30 A semiconductor device and a method for manufacturing the semiconductor device according to one embodiment of the present invention will be described.

[0110] <Structural Example of Semiconductor Device>

[0111] Figure 4 A is a top view of a transistor 500 as a semiconductor device according to one embodiment of the present invention. Figure 4 B is equivalent to following Figure 4 A is a cross-sectional view of the cut surface along the dot-dash line X1-X2, Figure 4 C is equivalent to following Figure 4 A is a cross-sectional view of a section taken along the dashed line Y1 - Y2 .

[0112] In addition, Figure 4 In A, for the sake of convenience, some components of transistor 500 (such as an insulating film used as a gate insulating film) are omitted. In addition, the dot-dash line X1-X2 direction is sometimes referred to as the channel length direction, and the dot-dash line Y1-Y2 direction is sometimes referred to as the channel width direction. Note that sometimes the top view of the transistor below is also the same as Figure 4 A Similarly, part of the components are omitted.

[0113] The transistor 500 includes a substrate 502, a conductive film 504, an insulating film 506, an insulating film 507, an oxide semiconductor film 508, a conductive film 512a, a conductive film 512b, an insulating film 514, an insulating film 516, an insulating film 518, a conductive film 520a, and a conductive film 520b. In addition, the oxide semiconductor film 508 includes an oxide semiconductor film 508a on one side of the conductive film 504 and an oxide semiconductor film 508b on the oxide semiconductor film 508a.

[0114] The conductive film 504 is arranged on the substrate 502, the insulating film 506 is arranged on the substrate 502 and the conductive film 504, the insulating film 507 is arranged on the insulating film 506, the oxide semiconductor film 508 is arranged on the insulating film 507, the conductive film 512a is arranged on the insulating film 507 and the oxide semiconductor film 508, the conductive film 512b is arranged on the insulating film 507 and the oxide semiconductor film 508, the insulating film 514 is arranged on the oxide semiconductor film 508, the conductive film 512a, and the conductive film 512b, the insulating film 516 is arranged on the insulating film 514, the insulating film 518 is arranged on the insulating film 516, and the conductive film 520b is arranged on the insulating film 518. In addition, the conductive film 520a is arranged on the conductive film 512b and the insulating film 518 via a contact hole 542c provided in the insulating film 514, the insulating film 516, and the insulating film 518 and reaching the conductive film 512b.

[0115] The oxide semiconductor film 508 is electrically connected to the conductive film 512a and the conductive film 512b. In addition, the conductive film 520a is electrically connected to the conductive film 512b.

[0116] The conductive film 504 has a function of a first gate electrode, and the conductive film 520b has a function of a second gate electrode (also referred to as a back gate electrode). In addition, the conductive film 512a has a function of one of a source electrode and a drain electrode, and the conductive film 512b has a function of the other of the source electrode and the drain electrode. In addition, the conductive film 520a has a function of, for example, a pixel electrode for a display device.

[0117] In addition, as described in Embodiment Mode 1, the conductive film 504 is Figures 1 to 3 The conductive film 520b is a portion of the scanning line 717 shown in FIG. Figures 1 to 3 A portion of wiring 718 is shown.

[0118] Here, as a comparative example, Figure 5 A contact hole is shown for each pixel to open to electrically connect the first gate electrode and the second gate electrode of the transistor 570 .

[0119] In transistor 500, the conductive film 504 and the conductive film 520b are electrically connected in a region other than the pixel portion, so that the potentials of the conductive film 504 and the conductive film 520b are equal. On the other hand, in transistor 570, the conductive film 504 and the conductive film 520b are electrically connected by contact holes 542a and 542b, so that the potentials of the conductive film 504 and the conductive film 520b are equal. Since only transistor 500 does not include contact holes 542a and 542b, the aperture ratio of transistor 500 is higher than that of transistor 570.

[0120] In addition, the oxide semiconductor film 508 included in the transistor 500 and the transistor 570 is located at a position opposite to the conductive film 504 and the conductive film 520b, and is sandwiched between the two conductive films used as gate electrodes. The length of the conductive film 520b in the channel length direction and the length of the channel width direction are both greater than the length of the oxide semiconductor film 508 in the channel length direction and the length of the channel width direction, and the conductive film 520b covers the entire oxide semiconductor film 508 via the insulating films 514, 516, and 518.

[0121] By adopting the above structure, the oxide semiconductor film 508 included in the transistor 500 and the transistor 570 is electrically surrounded by the electric field of the conductive film 504 and the conductive film 520b. As shown in the transistor 500 and the transistor 570, the device structure of the transistor in which the oxide semiconductor film having the channel region is electrically surrounded by the electric field of the first gate electrode and the second gate electrode can be called a surrounded channel (s-channel) structure.

[0122] Since the transistor 500 and the transistor 570 have an s-channel structure, an electric field for inducing a channel can be effectively applied to the oxide semiconductor film 508 using the conductive film 504, whereby, as described in Embodiment 1, the current driving capability of the transistor 500 and the transistor 570 is improved compared to the case where the conductive film 520 b is not included, thereby obtaining a high on-state current characteristic. In addition, since the on-state current can be increased, the transistor 500 and the transistor 570 can be miniaturized.

[0123] Figure 6A transistor 600 is shown as a modified example of this embodiment. The transistor 600 includes a substrate 602, a conductive film 604, an insulating film 606, an oxide semiconductor film 608, a conductive film 612a, a conductive film 612b, an insulating film 614, a conductive film 616, and an insulating film 618. In addition, the oxide semiconductor film 608 includes an oxide semiconductor film 608a on the side of the conductive film 604 and an oxide semiconductor film 608b on the oxide semiconductor film 608a.

[0124] The conductive film 604 is disposed on the substrate 602, the insulating film 606 is disposed on the substrate 602 and the conductive film 604, the oxide semiconductor film 608 is disposed on the insulating film 606, the conductive film 612a is disposed on the insulating film 606 and the oxide semiconductor film 608, the conductive film 612b is disposed on the insulating film 606 and the oxide semiconductor film 608, the insulating film 614 is disposed on the oxide semiconductor film 608, the conductive film 612a, and the conductive film 612b, the conductive film 616 is disposed on the insulating film 614, and the insulating film 618 is disposed on the insulating film 606, the conductive film 612a, and the conductive film 612b. In addition, the oxide semiconductor film 608 is electrically connected to the conductive film 612a and the conductive film 612b, the conductive film 612a has the function of one of a source electrode and a drain electrode, and the conductive film 612b has the function of the other of the source electrode and the drain electrode.

[0125] The transistor 600 has a top gate structure in which a conductive film 604 serving as a second gate electrode (also referred to as a back gate electrode) is formed below a conductive film 616 serving as a first gate electrode.

[0126] The oxide semiconductor film 608 is located at a position opposite to the conductive film 616 and the conductive film 604 and is sandwiched between the conductive film 616 and the conductive film 604. That is, the transistor 600 has the above-described s-channel structure. Therefore, high on-state current characteristics can be obtained.

[0127] In addition, the conductive film 616 is Figures 1 to 3 The conductive film 604 is a portion of the scanning line 717 shown in FIG. Figures 1 to 3 A portion of the wiring 718 is shown. That is, the wiring 718 is formed below the scanning line 717.

[0128] Transistor 600 may also have Figure 7 The structure shown in FIG. 1 is a self-aligned structure in which there is no region where the conductive film 616 overlaps with the conductive film 612a and the conductive film 612b. A transistor with a self-aligned structure is suitable for high-speed operation because the parasitic capacitance between the conductive film used as the source electrode or the drain electrode and the conductive film used as the first gate electrode is extremely small.

[0129] Alternatively, transistor 600 may also have Figure 8In this structure, the insulating film 614 and the conductive film 616 are provided in a contact hole provided in the insulating film 618 and reaching the oxide semiconductor film 608 b and the insulating film 606 .

[0130] Compared with the structure of the above transistor, Figure 8 In the structure of the transistor 600 shown in FIG. 1 , the conductive film used as the source electrode or the drain electrode overlaps the conductive film used as the first gate electrode in a small area, thereby reducing the parasitic capacitance. Therefore, the transistor is suitable for a component of a circuit that requires high-speed operation. In addition, although it is preferred that the top surface of the transistor be Figure 8 B and Figure 8 As shown in C, planarization is performed by a CMP (Chemical Mechanical Polishing) method or the like, but a structure in which planarization is not performed may also be employed.

[0131] Next, components included in the transistor 500 are described in detail. Note that the conductive film 504 and the conductive film 520b can be made of the same materials as those of the scan line 717 and the wiring 718 described in Embodiment 1, respectively.

[0132] <Substrate>

[0133] As the substrate 502, for example, a substrate having heat resistance at least capable of withstanding subsequent heat treatment, such as a glass substrate, a ceramic substrate, a quartz substrate, a sapphire substrate, etc., can be used. In addition, a single crystal semiconductor substrate or a polycrystalline semiconductor substrate made of silicon or silicon carbide, a compound semiconductor substrate made of silicon germanium, etc., an SOI (Silicon On Insulator) substrate, etc. can be used, and a substrate having a semiconductor element provided on these substrates can also be used as the substrate 502. When a glass substrate is used as the substrate 502, a large display device can be manufactured by using a large-area substrate of the 6th generation, 7th generation, 8th generation, 9th generation, 10th generation, etc. The use of such a large-area substrate is preferred because the manufacturing cost can be reduced. A flexible substrate can also be used as the substrate 502.

[0134] <Insulating Film Serving as First Gate Insulating Film>

[0135] As the insulating film 506 and the insulating film 507 used as the first gate insulating film of the transistor 500, one or more insulating films including a silicon oxide film, a silicon oxynitride film, a silicon nitride oxide film, a silicon nitride film, an aluminum oxide film, a hafnium oxide film, a yttrium oxide film, a zirconium oxide film, a gallium oxide film, a tantalum oxide film, a magnesium oxide film, a lanthanum oxide film, a cerium oxide film, and a neodymium oxide film formed by a plasma enhanced chemical vapor deposition (PECVD) method, a sputtering method, etc. can be used. Note that a single layer or three or more insulating films selected from the above materials may be used instead of using a stacked structure of the insulating film 506 and the insulating film 507.

[0136] The insulating film 506 has a function as a barrier film that suppresses oxygen permeation. For example, when excessive oxygen is supplied to the insulating film 507, the insulating film 514, the insulating film 516, and / or the oxide semiconductor film 508, the insulating film 506 can suppress oxygen permeation.

[0137] The insulating film 507 in contact with the oxide semiconductor film 508 serving as the channel region of the transistor 500 is preferably an oxide insulating film, and more preferably includes a region containing oxygen exceeding the stoichiometric composition (oxygen excess region). In other words, the insulating film 507 is an insulating film capable of releasing oxygen.

[0138] In addition, when hafnium oxide is used as the insulating film 507, the following effects are exerted. The relative dielectric constant of hafnium oxide is higher than that of silicon oxide or silicon oxynitride. Therefore, the thickness of the insulating film 507 can be made larger than that of using silicon oxide, thereby reducing the leakage current caused by the tunnel current. In other words, a transistor with a small off-state current can be realized. Furthermore, compared with hafnium oxide having an amorphous structure, the relative dielectric constant of hafnium oxide having a crystalline structure is higher. Therefore, in order to form a transistor with a small off-state current, it is preferred to use hafnium oxide including a crystalline structure. As examples of crystalline structures, monoclinic system or cubic system can be cited. Note that one embodiment of the present invention is not limited to this.

[0139] Note that in this embodiment, a silicon nitride film is formed as the insulating film 506, and a silicon oxide film is formed as the insulating film 507. Compared with a silicon oxide film, a silicon nitride film has a higher relative dielectric constant and requires a greater thickness to obtain an electrostatic capacitance equivalent to that of a silicon oxide film. Therefore, by making the gate insulating film of the transistor 500 include a silicon nitride film, the physical thickness of the insulating film can be increased. Therefore, by suppressing a decrease in the dielectric withstand voltage of the transistor 500 and increasing the dielectric withstand voltage, electrostatic breakdown of the transistor 500 can be suppressed.

[0140] <Oxide Semiconductor Film>

[0141] The above materials can be used as the oxide semiconductor film 508. When the oxide semiconductor film 508 is In-M-Zn oxide, the atomic number ratio of the metal element of the sputtering target used to form the In-M-Zn oxide preferably satisfies In≥M (the number of In atoms is greater than the number of M atoms) and Zn≥M (the number of Zn atoms is greater than the number of M atoms). The atomic number ratio of the metal element of such a sputtering target is preferably In:M:Zn=1:1:1, In:M:Zn=1:1:1.2, In:M:Zn=2:1:3, In:M:Zn=3:1:2, In:M:Zn=4:2:4.1. In addition, when the oxide semiconductor film 508 is In-M-Zn oxide, a target containing polycrystalline In-M-Zn oxide is preferably used as the sputtering target. By using a target containing polycrystalline In-M-Zn oxide, it is easy to form an oxide semiconductor film 508 having crystallinity. Note that the atomic number ratio of the formed oxide semiconductor film 508 includes an error within the range of ±40% of the atomic number ratio of the metal element in the above-mentioned sputtering target. For example, when the atomic number ratio of In:Ga:Zn=4:2:4.1 is used as the sputtering target, the atomic number ratio of the formed oxide semiconductor film 508 is sometimes In:Ga:Zn=4:2:3 or so.

[0142] For example, the oxide semiconductor film 508a can be formed using the sputtering target materials such as In:M:Zn=2:1:3, In:M:Zn=3:1:2, In:M:Zn=4:2:4.1, etc. The atomic number ratio of the oxide semiconductor film 508a is preferably In:M:Zn=4:α1(1.5≤α1≤2.5)(α1 is greater than or equal to 1.5 and less than or equal to 2.5):α2(2.5≤α2≤3.5)(α2 is greater than or equal to 2.5 and less than or equal to 3.5).

[0143] In addition, the oxide semiconductor film 508b can be formed using the above-mentioned sputtering targets such as In:M:Zn=1:1:1, In:M:Zn=1:1:1.2. The atomic number ratio of the oxide semiconductor film 508b is preferably In:M:Zn=1:β1(0.8≤β1≤1.2)(β1 is greater than 0.8 and less than 1.2):β2(0.8≤β2≤1.2)(β2 is greater than 0.8 and less than 1.2). In addition, the atomic number ratio of the metal element used as the sputtering target for the oxide semiconductor film 508b does not necessarily have to satisfy In≥M (the number of In atoms is greater than the number of M atoms) and Zn≥M (the number of Zn atoms is greater than the number of M atoms) at the same time, and may also satisfy In<M and / or Zn<M. Specifically, In:M:Zn=1:3:2, In:M:Zn=1:3:4, In:M:Zn=1:3:6, etc. are mentioned.

[0144] The energy gap of the oxide semiconductor film 508 is greater than 2 eV, preferably greater than 2.5 eV, and more preferably greater than 3 eV. In this way, by using an oxide semiconductor with a wider energy gap, the off-state current of the transistor 500 can be reduced. In particular, an oxide semiconductor film with an energy gap of greater than 2.0 eV, preferably greater than 2.0 eV and less than 3.0 eV, is used as the oxide semiconductor film 508a, and an oxide semiconductor film with an energy gap of greater than 2.5 eV and less than 3.5 eV is used as the oxide semiconductor film 508b. In addition, it is preferred that the energy gap of the oxide semiconductor film 508b is greater than the energy gap of the oxide semiconductor film 508a.

[0145] The thickness of the oxide semiconductor film 508 a and the oxide semiconductor film 508 b are each greater than or equal to 3 nm and less than or equal to 200 nm, preferably greater than or equal to 3 nm and less than or equal to 100 nm, and more preferably greater than or equal to 3 nm and less than or equal to 50 nm.

[0146] In addition, an oxide semiconductor film having a low carrier density is used as the oxide semiconductor film 508 a. For example, the carrier density of the oxide semiconductor film 508 a can be less than 8×10 11 / cm 3 , preferably less than 1×10 11 / cm 3 , more preferably less than 1×10 10 / cm 3 , and is 1×10 -9 / cm 3 In addition, an oxide semiconductor film having a low carrier density is used as the oxide semiconductor film 508 b. For example, the carrier density of the oxide semiconductor film 508 b may be 1×10 17 / cm 3 Below, preferably 1×10 15 / cm 3 Below, more preferably 1×10 13 / cm 3 Below, more preferably 1×10 11 / cm 3 the following.

[0147] The present invention is not limited to the above description, and a material having an appropriate composition can be used according to the desired semiconductor characteristics and electrical characteristics (field effect mobility, threshold voltage, etc.) of the transistor. In addition, it is preferred to appropriately set the carrier density, impurity concentration, defect density, atomic ratio of metal elements to oxygen, interatomic distance, density, etc. of the oxide semiconductor film 508a and the oxide semiconductor film 508b to obtain the desired semiconductor characteristics of the transistor.

[0148] By using an oxide semiconductor film with a low impurity concentration and a low defect state density as the oxide semiconductor film 508a and the oxide semiconductor film 508b, a transistor with better electrical characteristics can be manufactured, so it is preferred. Here, the state of low impurity concentration and low defect state density (few oxygen defects) is referred to as "high purity intrinsic" or "substantially high purity intrinsic". Because the high purity intrinsic or substantially high purity intrinsic oxide semiconductor film has fewer carrier generation sources, the carrier density can be reduced. Therefore, a transistor having a channel region formed in the oxide semiconductor film rarely has an electrical characteristic of a negative threshold voltage (also called a normally-on characteristic). Because the high purity intrinsic or substantially high purity intrinsic oxide semiconductor film has a lower defect state density, it is possible to have a lower trap state density. The off-state current of the high purity intrinsic or substantially high purity intrinsic oxide semiconductor film is significantly low, even if the channel width is 1×10 6 For a device with a channel length of 10 μm and a source-drain voltage of 1 V to 10 V, the off-state current can be below the measurement limit of the semiconductor parameter analyzer, that is, 1×10 -13 A or below.

[0149] Therefore, a transistor having a channel region formed in the above-mentioned high-purity intrinsic or substantially high-purity intrinsic oxide semiconductor film can be a transistor with small changes in electrical characteristics and high reliability. In addition, it takes a long time for the charge captured by the trap energy level of the oxide semiconductor film to disappear, and sometimes it acts like a fixed charge. Therefore, sometimes the electrical characteristics of a transistor having a channel region formed in an oxide semiconductor film with a high trap state density are unstable. Impurities include hydrogen, nitrogen, alkali metals or alkaline earth metals.

[0150] The hydrogen contained in the oxide semiconductor film reacts with the oxygen bonded to the metal atom to generate water, and at the same time, an oxygen defect is formed in the lattice where oxygen detachment occurs (or the portion where oxygen detachment occurs). When hydrogen enters the oxygen defect, electrons are sometimes generated as carriers. In addition, sometimes electrons are generated as carriers because a portion of the hydrogen is bonded to the oxygen bonded to the metal atom. Therefore, transistors using oxide semiconductor films containing hydrogen tend to have normally-on characteristics. Therefore, it is preferred to reduce the amount of hydrogen in the oxide semiconductor film 508 as much as possible. Specifically, in the oxide semiconductor film 508, the hydrogen concentration measured by SIMS (Secondary Ion Mass Spectrometry) is 2×10 20 atoms / cm 3 Below, preferably 5×10 19 atoms / cm 3 Below, more preferably 1×10 19 atoms / cm 3Below, more preferably 5×10 18 atoms / cm 3 Below, more preferably 1×10 18 atoms / cm 3 Below, more preferably 5×10 17 atoms / cm 3 Below, more preferably 1×10 16 atoms / cm 3 the following.

[0151] Note that the oxide semiconductor film 508a preferably includes a portion having a lower hydrogen concentration than the oxide semiconductor film 508b. When the oxide semiconductor film 508a includes a portion having a lower hydrogen concentration than the oxide semiconductor film 508b, a highly reliable semiconductor device can be provided.

[0152] In addition, when the oxide semiconductor film 508a contains silicon or carbon, which is one of the elements of Group 14, oxygen vacancies increase in the oxide semiconductor film 508a, causing the oxide semiconductor film 508a to become n-type. Therefore, the concentration of silicon or carbon in the oxide semiconductor film 508a and the concentration of silicon or carbon near the interface with the oxide semiconductor film 508a (concentration measured by SIMS analysis) are 2×10 18 atoms / cm 3 Below, preferably 2×10 17 atoms / cm 3 the following.

[0153] In addition, the concentration of the alkali metal or alkaline earth metal in the oxide semiconductor film 508a measured by SIMS analysis is 1×10 18 atoms / cm 3 Below, preferably 2×10 16 atoms / cm 3 When an alkali metal or alkaline earth metal is bonded to an oxide semiconductor, carriers are generated and the off-state current of the transistor is increased. Therefore, the concentration of the alkali metal or alkaline earth metal in the oxide semiconductor film 508a is preferably reduced.

[0154] When nitrogen is contained in the oxide semiconductor film 508a, electrons are generated as carriers, and the carrier density increases, resulting in the n-type of the oxide semiconductor film 508a. As a result, a transistor using an oxide semiconductor film containing nitrogen tends to have a normally-on characteristic. Therefore, it is preferable to reduce the nitrogen in the oxide semiconductor film as much as possible. For example, the nitrogen concentration measured by SIMS analysis is preferably 5×10 18 atoms / cm 3 the following.

[0155] The oxide semiconductor film 508a and the oxide semiconductor film 508b may each have a non-single-crystal structure. The non-single-crystal structure includes, for example, the following CAAC-OS (C Axis Aligned Crystalline Oxide Semiconductor: c-axis oriented crystalline oxide semiconductor), a polycrystalline structure, a microcrystalline structure, or an amorphous structure. Among the non-single-crystal structures, the defect state density of the amorphous structure is the highest, while the defect state density of the CAAC-OS is the lowest.

[0156] Here, refer to Fig. 9 The energy band structures of the oxide semiconductor film 508 and the insulating film in contact with the oxide semiconductor film 508 are described.

[0157] Fig. 9 1 is an example of an energy band structure in the film thickness direction of a stacked structure including an insulating film 507, an oxide semiconductor film 508a, an oxide semiconductor film 508b, and an insulating film 514. In the energy band structure, for easy understanding, the conduction band bottom energy levels (Ec) of the insulating film 507, the oxide semiconductor film 508a, the oxide semiconductor film 508b, and the insulating film 514 are shown.

[0158] exist Fig. 9 In the energy band diagram shown, a silicon oxide film is used as the insulating film 507 and the insulating film 514, an oxide semiconductor film formed using a metal oxide target having an atomic ratio of metal elements of In:Ga:Zn=4:2:4.1 is used as the oxide semiconductor film 508a, and a metal oxide film formed using a metal oxide target having an atomic ratio of metal elements of In:Ga:Zn=1:1:1.2 is used as the oxide semiconductor film 508b.

[0159] like Fig. 9 As shown in FIG. 1 , in the oxide semiconductor film 508 a and the oxide semiconductor film 508 b, the conduction band bottom energy level changes smoothly. In other words, the conduction band bottom energy level changes continuously or is continuously connected. In order to achieve such an energy band structure, impurities that form defect energy levels such as trap centers or recombination centers are not present at the interface between the oxide semiconductor film 508 a and the oxide semiconductor film 508 b.

[0160] In order to form a continuous junction between the oxide semiconductor film 508 a and the oxide semiconductor film 508 b , a multi-chamber film formation apparatus (sputtering apparatus) including a load lock chamber may be used so that each film is continuously stacked without being exposed to the atmosphere.

[0161] It can be seen that by adopting Fig. 9 In the structure shown in FIG. 1 , the oxide semiconductor film 508 a functions as a well. In a transistor using the stacked structure described above, a channel region is formed in the oxide semiconductor film 508 a .

[0162] In addition, when the oxide semiconductor film 508b is not formed, a trap level may be formed in the oxide semiconductor film 508a. On the other hand, by adopting the above-mentioned stacked structure, the trap level may be formed in the oxide semiconductor film 508b. Therefore, the trap level can be kept away from the oxide semiconductor film 508a.

[0163] In addition, sometimes the trap energy level is farther from the vacuum energy level than the bottom energy level (Ec) of the conduction band of the oxide semiconductor film 508a used as the channel region, and electrons are easily accumulated in the trap energy level. When electrons accumulate in the trap energy level, they become negative fixed charges, causing the threshold voltage of the transistor to drift in the positive direction. Therefore, it is preferred to adopt a structure in which the trap energy level is closer to the vacuum energy level than the bottom energy level (Ec) of the conduction band of the oxide semiconductor film 508a. By adopting the above structure, electrons are not easily accumulated in the trap energy level, so the on-state current of the transistor can be increased, and the field effect mobility can also be improved.

[0164] exist Fig. 9 In the embodiment, the conduction band bottom energy level of the oxide semiconductor film 508b is closer to the vacuum level than that of the oxide semiconductor film 508a. Typically, the difference between the conduction band bottom energy level of the oxide semiconductor film 508a and the conduction band bottom energy level of the oxide semiconductor film 508b is 0.15 eV or 0.5 eV and 2 eV or 1 eV. In other words, the difference between the electron affinity of the oxide semiconductor film 508b and the electron affinity of the oxide semiconductor film 508a is 0.15 eV or 0.5 eV and 2 eV or 1 eV.

[0165] By adopting the above structure, the oxide semiconductor film 508a becomes the main path of the current and is used as a channel region. Since the oxide semiconductor film 508b includes one or more of the metal elements contained in the oxide semiconductor film 508a forming the channel region, interface scattering is not easily generated at the interface between the oxide semiconductor film 508a and the oxide semiconductor film 508b. As a result, since the movement of carriers in the interface is not hindered, the field effect mobility of the transistor is improved.

[0166] In order to prevent the oxide semiconductor film 508b from being used as part of the channel region, the oxide semiconductor film 508b uses a material with sufficiently low conductivity. Alternatively, the oxide semiconductor film 508b uses a material whose electron affinity (difference between the vacuum energy level and the conduction band bottom energy level) is lower than that of the oxide semiconductor film 508a and whose conduction band bottom energy level is different from that of the oxide semiconductor film 508a (band offset). In addition, in order to suppress the difference between the threshold voltages caused by the drain voltage value, it is preferred to use a material whose conduction band bottom energy level of the oxide semiconductor film 508b is closer to the vacuum energy level by more than 0.2 eV, preferably more than 0.5 eV, than that of the conduction band bottom energy level of the oxide semiconductor film 508a.

[0167] It is preferable that the oxide semiconductor film 508b does not include a spinel-type crystal structure. When the oxide semiconductor film 508b includes a spinel-type crystal structure, the constituent elements of the conductive film 512a and the conductive film 512b may diffuse into the oxide semiconductor film 508a at the interface between the spinel-type crystal structure and other regions. Note that in the case where the oxide semiconductor film 508b is a CAAC-OS described later, the properties of the constituent elements such as copper that block the conductive film 512a and the conductive film 512b are improved, so it is preferable.

[0168] The thickness of the oxide semiconductor film 508b is greater than or equal to a thickness that can suppress diffusion of constituent elements of the conductive film 512a and the conductive film 512b into the oxide semiconductor film 508b and less than a thickness that suppresses supply of oxygen from the insulating film 514 to the oxide semiconductor film 508b. For example, when the thickness of the oxide semiconductor film 508b is greater than or equal to 10 nm, diffusion of constituent elements of the conductive film 512a and the conductive film 512b into the oxide semiconductor film 508a can be suppressed. In addition, when the thickness of the oxide semiconductor film 508b is less than or equal to 100 nm, oxygen can be effectively supplied from the insulating film 514 and the insulating film 516 to the oxide semiconductor film 508a.

[0169] <Structure of Oxide Semiconductor>

[0170] Next, the structure of the oxide semiconductor is described.

[0171] In this specification, "parallel" refers to a state where the angle formed by two straight lines is greater than -10° and less than 10°. Therefore, it also includes a state where the angle is greater than -5° and less than 5°. In addition, "approximately parallel" refers to a state where the angle formed by two straight lines is greater than -30° and less than 30°. In addition, "perpendicular" refers to a state where the angle formed by two straight lines is greater than 80° and less than 100°. Therefore, it also includes a state where the angle is greater than 85° and less than 95°. "Approximately perpendicular" refers to a state where the angle formed by two straight lines is greater than 60° and less than 120°.

[0172] In addition, in this specification, the hexagonal crystal system includes the trigonal crystal system and the rhombohedral crystal system.

[0173] Oxide semiconductors are classified into single crystal oxide semiconductors and non-single crystal oxide semiconductors. Examples of non-single crystal oxide semiconductors include CAAC-OS (c-axis-aligned crystalline oxide semiconductor), polycrystalline oxide semiconductor, nc-OS (nanocrystalline oxide semiconductor), a-like OS (amorphous-like oxide semiconductor), and amorphous oxide semiconductor.

[0174] From another viewpoint, oxide semiconductors are classified into amorphous oxide semiconductors and crystalline oxide semiconductors. Examples of crystalline oxide semiconductors include single crystal oxide semiconductors, CAAC-OS, polycrystalline oxide semiconductors, and nc-OS.

[0175] Generally speaking, an amorphous structure has the following characteristics: it is isotropic but not inhomogeneous; it is in a metastable state and the configuration of atoms is not fixed; the bond angle is not fixed; it has short-range order but not long-range order; etc.

[0176] That is to say, a stable oxide semiconductor cannot be called a completely amorphous oxide semiconductor. In addition, an oxide semiconductor that does not have isotropy (for example, a periodic structure in a tiny area) cannot be called a completely amorphous oxide semiconductor. On the other hand, a-like OS does not have isotropy but has an unstable structure with voids. In terms of instability, a-like OS is close to amorphous oxide semiconductors in terms of physical properties.

[0177] <caac-os>

[0178] First, CAAC-OS is described.

[0179] CAAC-OS is a type of oxide semiconductor including a plurality of c-axis-aligned crystal parts (also referred to as grains).

[0180] The following describes the situation when CAAC-OS is analyzed using an X-ray diffraction (XRD) device. For example, when the structure of CAAC-OS including InGaZnO4 crystals classified into the space group R-3m is analyzed using the out-of-plane method, as shown in FIG. Fig.10 As shown in A, a peak appears near the diffraction angle (2θ) of 31°. Since this peak originates from the (009) plane of the InGaZnO4 crystal, it can be confirmed that the crystallization in CAAC-OS has a c-axis orientation, and the c-axis is oriented in a direction roughly perpendicular to the surface (also referred to as the formed surface) or the top surface of the film forming CAAC-OS. Note that in addition to the peak near 2θ of 31°, a peak sometimes appears near 2θ of 36°. The peak near 2θ of 36° is caused by a crystal structure classified as the space group Fd-3m. Therefore, it is preferred that this peak does not appear in CAAC-OS.

[0181] On the other hand, when the structure of CAAC-OS is analyzed using the in-plane method in which X-rays are incident on the sample from a direction parallel to the formed surface, a peak appears near 2θ of 56°. This peak originates from the (110) plane of the InGaZnO4 crystal. Furthermore, even when 2θ is fixed at around 56° and the sample is rotated with the normal vector of the sample surface as the axis (φ axis), the analysis (φ scan) is still the same. Fig.10 No clear peak is observed as shown in B. On the other hand, when single crystal InGaZnO4 is scanned with 2θ fixed at around 56°, Fig.10 As shown in C, six peaks derived from a crystal plane equivalent to the (110) plane were observed. Therefore, it was confirmed from the structural analysis using XRD that there was no regularity in the orientation of the a-axis and the b-axis in CAAC-OS.

[0182] Next, the CAAC-OS analyzed by electron diffraction is described. For example, when an electron beam with a beam diameter of 300 nm is incident on a CAAC-OS including InGaZnO4 crystals in a direction parallel to the surface on which the CAAC-OS is formed, it is possible that Fig.10 D shows a diffraction pattern (also called a selected area electron diffraction pattern). The diffraction pattern contains spots caused by the (009) plane of InGaZnO4 crystal. Therefore, electron diffraction also shows that the particles contained in CAAC-OS have c-axis orientation, and the c-axis is oriented in a direction roughly perpendicular to the formed surface or top surface. On the other hand, Fig.10 E shows the diffraction pattern of the same sample when an electron beam with a beam diameter of 300 nm is incident on the sample in a direction perpendicular to the sample surface. Fig.10 E observed a ring-shaped diffraction pattern. Therefore, electron diffraction using an electron beam with a beam diameter of 300 nm also shows that the a-axis and b-axis of the particles included in CAAC-OS have no orientation. Fig.10 The first ring in E originates from the (010) and (100) planes of the InGaZnO4 crystal. Fig.10 The second ring in E originates from the (110) plane, etc.

[0183] In addition, in a composite analysis image (also called a high-resolution TEM image) of a bright field image and a diffraction pattern of CAAC-OS obtained by observation using a transmission electron microscope (TEM), multiple particles can be observed. However, even in a high-resolution TEM image, a clear boundary between particles, i.e., a grain boundary, is sometimes not observed. Therefore, it can be said that in CAAC-OS, a decrease in electron mobility due to grain boundaries is not likely to occur.

[0184] Fig.11 A shows a high-resolution TEM image of a cross section of the CAAC-OS obtained by observing from a direction roughly parallel to the sample surface. The high-resolution TEM image is obtained using the spherical aberration corrector function. In particular, the high-resolution TEM image obtained using the spherical aberration correction function is called a Cs-corrected high-resolution TEM image. For example, the Cs-corrected high-resolution TEM image can be observed using an atomic resolution analytical electron microscope JEM-ARM200F manufactured by JEOL Ltd.

[0185] from Fig.11 A can confirm particles in which metal atoms are arranged in layers. And it can be seen that the size of a particle is greater than 1 nm or greater than 3 nm. Therefore, the particles can also be called nanocrystals (nc: nanocrystal). In addition, CAAC-OS can also be called an oxide semiconductor with CANC (C-Axis Aligned nanocrystals: c-axis oriented nanocrystals). The particles reflect the convexity and concavity of the formed surface or top surface of CAAC-OS and are parallel to the formed surface or top surface of CAAC-OS.

[0186] in addition, Fig.11 B and Fig.11 C shows a Cs-corrected high-resolution TEM image of the plane of the CAAC-OS acquired by observing from a direction substantially perpendicular to the sample surface. Fig.11 D and Fig.11 E is achieved through Fig.11 B and Fig.11 The image is obtained by performing image processing on C. The image processing method is described below. First, Fig.11 B performs fast Fourier transform (FFT) processing to obtain an FFT image. Next, the FFT image obtained is retained to obtain the region 2.8 nm from the origin. -1 Up to 5.0nm -1 The masking is performed in a manner of a range of . Next, the masked FFT image is subjected to an inverse fast Fourier transform (IFFT) to obtain a processed image. The acquired image is called an FFT filtered image. The FFT filtered image is an image of periodic components extracted from the Cs-corrected high-resolution TEM image, which shows the lattice arrangement.

[0187] exist Fig.11 In D, the dotted line shows the part where the lattice arrangement is disrupted. The area surrounded by the dotted line is a particle. And the part shown by the dotted line is the connection between particles. The dotted line is hexagonal, which shows that the particle is hexagonal. Note that the shape of the particle is not limited to a regular hexagon, and there are many cases where it is not a regular hexagon.

[0188] exist Fig.11 In E, the dotted lines show the part where the direction of the lattice arrangement between the area with consistent lattice arrangement and other areas with consistent lattice arrangement changes, and the dotted lines show the change in the direction of the lattice arrangement. No clear grain boundaries can be confirmed near the dotted lines. When the lattice points around the lattice points near the dotted lines are connected, distorted hexagons, pentagons and / or heptagons can be formed. In other words, it can be seen that the formation of grain boundaries can be suppressed by distorting the lattice arrangement. This may be because CAAC-OS can tolerate distortions caused by the following reasons: low density of atomic arrangement in the ab plane direction, changes in the bonding distance between atoms due to substitution of metal elements, etc.

[0189] As described above, CAAC-OS has c-axis alignment, and its multiple particles (nanocrystals) are linked in the ab plane direction, and the crystal structure has distortion. Therefore, CAAC-OS can also be called CAA crystal (c-axis-aligned ab-plane-anchored crystal).

[0190] CAAC-OS is an oxide semiconductor with high crystallinity. Since the crystallinity of an oxide semiconductor may be reduced due to the incorporation of impurities or the generation of defects, this means that CAAC-OS is an oxide semiconductor with few impurities or defects (oxygen defects, etc.).

[0191] In addition, impurities refer to elements other than the main components of oxide semiconductors, such as hydrogen, carbon, silicon, and transition metal elements. For example, elements such as silicon that have a stronger bonding force with oxygen than the metal elements that constitute the oxide semiconductor will take away oxygen from the oxide semiconductor, thereby disrupting the atomic arrangement of the oxide semiconductor, resulting in a decrease in crystallinity. In addition, since heavy metals such as iron or nickel, argon, carbon dioxide, etc. have large atomic radii (or molecular radii), they will disrupt the atomic arrangement of the oxide semiconductor, resulting in a decrease in crystallinity.

[0192] <nc-os>

[0193] Next, nc-OS is described.

[0194] The following describes the analysis of nc-OS using an XRD device. For example, when the structure of nc-OS is analyzed using the out-of-plane method, no peak indicating orientation appears. In other words, the crystals of nc-OS do not have orientation.

[0195] For example, when nc-OS containing InGaZnO4 crystals was thinned and an electron beam with a beam diameter of 50 nm was incident on a region with a thickness of 34 nm in a direction parallel to the formed surface, the following was observed: Fig.12 A shows a ring-shaped diffraction pattern (nanobeam electron diffraction pattern). Fig.12 B shows the diffraction pattern (nanobeam electron diffraction pattern) when an electron beam with a beam diameter of 1 nm is incident on the same sample. Fig.12 B. Multiple spots were observed in the ring-shaped region. Therefore, the nc-OS had no order when the incident electron beam had an incident beam diameter of 50 nm, but had order when the incident electron beam had an incident beam diameter of 1 nm.

[0196] In addition, when an electron beam with a beam diameter of 1 nm is incident on a region with a thickness of less than 10 nm, Fig.12 As shown in Figure 3, electron diffraction patterns in which spots are arranged in quasi-regular hexagons are sometimes observed. This shows that nc-OS contains highly ordered regions, i.e., crystals, within a thickness range of less than 10 nm. Note that because the crystals are oriented in various directions, there are also regions where regular electron diffraction patterns are not observed.

[0197] Fig.12 D shows a Cs-corrected high-resolution TEM image of a cross section of nc-OS observed from a direction roughly parallel to the formed surface. In the high-resolution TEM image of nc-OS, there are areas where crystalline parts can be observed, such as the parts shown by the auxiliary lines, and areas where no clear crystalline parts can be observed. The size of the crystalline part contained in nc-OS is greater than 1nm and less than 10nm, and in particular, most of them are greater than 1nm and less than 3nm. Note that oxide semiconductors whose crystalline parts are greater than 10nm and less than 100nm are sometimes called microcrystalline oxide semiconductors. For example, in the high-resolution TEM image of nc-OS, grain boundaries are sometimes not clearly observed. Note that the source of the nanocrystals may be the same as the particles in CAAC-OS. Therefore, the crystalline parts of nc-OS are sometimes referred to as particles below.

[0198] Thus, in nc-OS, the atomic arrangement in a tiny region (e.g., a region between 1 nm and 10 nm, especially a region between 1 nm and 3 nm) is periodic. In addition, in nc-OS, no regularity of crystal orientation is observed between different particles. Therefore, no orientation is observed in the entire film. Therefore, sometimes nc-OS is no different from a-like OS or amorphous oxide semiconductors in some analysis methods.

[0199] In addition, since there is no regularity in crystal orientation between particles (nanocrystals), nc-OS may also be referred to as an oxide semiconductor including RANC (Random Aligned nanocrystals) or an oxide semiconductor including NANC (Non-Aligned nanocrystals).

[0200] nc-OS is an oxide semiconductor with higher regularity than amorphous oxide semiconductors. Therefore, the defect state density of nc-OS is lower than that of a-like OS or amorphous oxide semiconductors. However, the regularity of crystal orientation is not observed between different particles in nc-OS. Therefore, the defect state density of nc-OS is higher than that of CAAC-OS.

[0201] <a-like OS>

[0202] An a-like OS is an oxide semiconductor having a structure between an nc-OS and an amorphous oxide semiconductor.

[0203] Fig.13 A high-resolution cross-sectional TEM image of an a-like OS is shown. Fig.13 A shows a high-resolution cross-sectional TEM image of the a-like OS at the start of electron irradiation. Fig.13 B shows irradiation of 4.3×10 8 e - / nm 2 The electron (e - ) after the high-resolution cross-sectional TEM image of a-likeOS. Fig.13 A and Fig.13 B shows that a-like OS is observed as a stripe-shaped bright area extending in the longitudinal direction from the start of electron irradiation. In addition, it can be seen that the shape of the bright area changes after electron irradiation. The bright area is estimated to be a void or a low-density area.

[0204] Since a-like OS contains voids, its structure is unstable. In order to prove that a-like OS has an unstable structure compared with CAAC-OS and nc-OS, the structural changes caused by electron irradiation are shown below.

[0205] As samples, a-like OS, nc-OS, and CAAC-OS were prepared. Each sample was In-Ga-Zn oxide.

[0206] First, a high-resolution cross-sectional TEM image of each sample was obtained. From the high-resolution cross-sectional TEM image, it was found that each sample had a crystal part.

[0207] It is known that the unit lattice of InGaZnO4 crystal has a structure in which three In-O layers and six Ga-Zn-O layers, a total of nine layers, are stacked in layers in the c-axis direction. The spacing between these layers close to each other is almost equal to the lattice surface spacing (also called d value) of the (009) plane, and its value is 0.29nm obtained by crystal structure analysis. Therefore, the portion where the spacing of the lattice fringes is greater than 0.28nm and less than 0.30nm can be regarded as the InGaZnO4 crystal portion. The lattice fringes correspond to the ab plane of the InGaZnO4 crystal.

[0208] Fig.14 The example of the average size of the crystal part (22 to 30 positions) of each sample is shown. Note that the crystal part size corresponds to the length of the lattice fringes described above. Fig.14 It can be seen that in a-like OS, the crystal part gradually increases in size according to the cumulative irradiation of electrons in obtaining TEM images, etc. Fig.14 It can be seen that in the observation using TEM, the initial size of the crystal part (also called the initial crystal nucleus) is about 1.2nm in size. - ) is 4.2×10 8 e - / nm 2 On the other hand, it can be seen that the cumulative irradiation dose of nc-OS and CAAC-OS from the start of electron irradiation to 4.2×10 8 e - / nm 2 The size of the crystal part does not change within the range of Fig.14 It can be seen that regardless of the cumulative electron irradiation dose, the crystal size of nc-OS and CAAC-OS is about 1.3nm and 1.8nm, respectively. In addition, electron beam irradiation and TEM observation were performed using a Hitachi transmission electron microscope H-9000NAR. As electron beam irradiation conditions, the acceleration voltage was 300kV; the current density was 6.7×10 5 e - / (nm 2 ·s), and the diameter of the irradiated area is 230nm.

[0209] Thus, electron irradiation sometimes causes the growth of crystal parts in a-like OS. On the other hand, in nc-OS and CAAC-OS, there is almost no growth of crystal parts caused by electron irradiation. In other words, a-like OS has an unstable structure compared with CAAC-OS and nc-OS.

[0210] In addition, since a-like OS contains voids, its density is lower than that of nc-OS and CAAC-OS. Specifically, the density of a-like OS is 78.6% or more and less than 92.3% of a single crystal oxide semiconductor having the same composition. The density of nc-OS and the density of CAAC-OS are 92.3% or more and less than 100% of a single crystal oxide semiconductor having the same composition. Note that it is difficult to form an oxide semiconductor whose density is less than 78% of the density of a single crystal oxide semiconductor.

[0211] For example, in an oxide semiconductor where the atomic ratio satisfies In:Ga:Zn=1:1:1, the density of single crystal InGaZnO4 having a rhombohedral structure is 6.357 g / cm 3 Therefore, for example, in an oxide semiconductor with an atomic ratio of In:Ga:Zn=1:1:1, the density of a-like OS is 5.0 g / cm 3 Above and less than 5.9g / cm 3 In addition, for example, in an oxide semiconductor having an atomic ratio of In:Ga:Zn=1:1:1, the density of nc-OS and the density of CAAC-OS are 5.9 g / cm 3 Above and less than 6.3g / cm 3 .

[0212] Note that when there are no single crystal oxide semiconductors with the same composition, the density of a single crystal oxide semiconductor with a desired composition can be estimated by combining single crystal oxide semiconductors with different compositions in an arbitrary ratio. The density of a single crystal oxide semiconductor with a desired composition can be estimated using a weighted average according to the combination ratio of single crystal oxide semiconductors with different compositions. Note that it is preferable to estimate the density by reducing the types of single crystal oxide semiconductors combined as much as possible.

[0213] As described above, oxide semiconductors have various structures and various characteristics. Note that the oxide semiconductor may be, for example, a stacked film including two or more of an amorphous oxide semiconductor, an a-like OS, a nc-OS, and a CAAC-OS.

[0214] <Carrier Density of Oxide Semiconductor>

[0215] Next, the carrier density of the oxide semiconductor is described.

[0216] Factors that affect the carrier density of an oxide semiconductor include oxygen vacancies (Vo) in the oxide semiconductor and impurities in the oxide semiconductor.

[0217] When the number of oxygen defects in an oxide semiconductor increases, hydrogen bonds with the oxygen defects (this state can also be referred to as VoH) to increase the defect state density. In addition, when the number of impurities in an oxide semiconductor increases, the defect state density also increases. Thus, the carrier density of the oxide semiconductor can be controlled by controlling the defect state density in the oxide semiconductor.

[0218] Next, a transistor using an oxide semiconductor for a channel region will be described.

[0219] In the case where the purpose is to suppress the negative drift of the threshold voltage of the transistor or to reduce the off-state current of the transistor, it is preferred to reduce the carrier density of the oxide semiconductor. In the case where the purpose is to reduce the carrier density of the oxide semiconductor, the impurity concentration in the oxide semiconductor can be reduced to reduce the defect state density. In this specification, etc., the state of low impurity concentration and low defect state density is referred to as "high-purity intrinsic" or "substantially high-purity intrinsic". The carrier density of a high-purity intrinsic oxide semiconductor is less than 8×10 15 cm -3 , preferably less than 1×10 11 cm -3 , more preferably less than 1×10 10 cm -3 , and is 1×10 -9 cm -3 That’s all.

[0220] On the other hand, in the case where the purpose is to increase the on-state current of the transistor or to improve the field effect mobility of the transistor, it is preferred to increase the carrier density of the oxide semiconductor. In the case where the purpose is to increase the carrier density of the oxide semiconductor, the impurity concentration of the oxide semiconductor can be slightly increased, or the defect state density of the oxide semiconductor can be slightly increased. Alternatively, it is preferred to narrow the band gap of the oxide semiconductor. For example, in the range of the on / off ratio of the Id-Vg characteristic of the transistor, an oxide semiconductor with a slightly higher impurity concentration or a slightly higher defect state density can be regarded as substantially intrinsic. In addition, an oxide semiconductor with an increased density of thermally excited electrons (carriers) due to a large electron affinity and a small band gap can be regarded as substantially intrinsic. In addition, when an oxide semiconductor with a greater electron affinity is used, the threshold voltage of the transistor is lower.

[0221] The oxide semiconductor with improved carrier density is slightly converted to n-type. Therefore, the oxide semiconductor with improved carrier density can also be called "Slightly-n".

[0222] The carrier density of a substantially intrinsic oxide semiconductor is preferably 1×10 5 cm -3 More than and less than 1×10 18 cm -3 , more preferably 1×10 7 cm -3 Above and 1×10 17 cm -3 Below, more preferably 1×10 9 cm -3 Above and 5×10 16 cm -3 Below, more preferably 1×10 10 cm -3 Above and 1×10 16 cm -3 Below, more preferably 1×10 11 cm -3 Above and 1×10 15 cm -3 the following.

[0223] <Insulating Film Serving as Protective Insulating Film and Second Gate Insulating Film of Transistor>

[0224] The insulating film 514 and the insulating film 516 have a function of supplying oxygen to the oxide semiconductor film 508. The insulating film 518 has a function of a protective insulating film and a second gate insulating film of the transistor 500. The insulating film 514 and the insulating film 516 contain oxygen. The insulating film 514 is an insulating film that allows oxygen to pass through. Note that the insulating film 514 also serves as a film that mitigates damage to the oxide semiconductor film 508 when the insulating film 516 is formed later.

[0225] As the insulating film 514 , silicon oxide, silicon oxynitride, or the like can be used with a thickness of 5 nm to 150 nm, preferably 5 nm to 50 nm.

[0226] Furthermore, the number of defects in the insulating film 514 is preferably small. Typically, the spin density of a signal at g=2.001 due to dangling bonds of silicon measured by ESR (Electron Spin Resonance) is preferably 3×10 17 spins / cm 3 This is because, if the defect density of the insulating film 514 is high, oxygen is bonded to the defects, and the oxygen permeability in the insulating film 514 is reduced.

[0227] In the insulating film 514, sometimes all of the oxygen that enters the insulating film 514 from the outside does not move to the outside of the insulating film 514, but a part of it remains inside the insulating film 514. In addition, sometimes, when oxygen enters the insulating film 514, oxygen contained in the insulating film 514 moves to the outside of the insulating film 514, and oxygen movement occurs in the insulating film 514. When an oxide insulating film that allows oxygen to pass is formed as the insulating film 514, oxygen separated from the insulating film 516 provided on the insulating film 514 can be moved to the oxide semiconductor film 508 via the insulating film 514.

[0228] Alternatively, the insulating film 514 may be formed using an oxide insulating film having a low state density due to nitride oxide. Note that the state density due to nitride oxide may be formed at the energy (E) of the valence band top of the oxide semiconductor film. V_OS ) and the energy of the conduction band bottom of the oxide semiconductor film (E C_OS As the oxide insulating film, a silicon oxynitride film with a small amount of nitride oxide released or an aluminum oxynitride film with a small amount of nitride oxide released can be used.

[0229] In addition, in thermal desorption spectrum analysis, the silicon oxynitride film with a small amount of nitrogen oxide release is a film that releases more ammonia than nitrogen oxide. Typically, the amount of ammonia molecules released is 1×10 18 Molecules / cm 3 Above and 5×10 19 Molecules / cm 3 Note that the amount of ammonia released is the amount released when the film surface temperature is heated to a temperature of 50° C. to 650° C., preferably 50° C. to 550° C.

[0230] Nitrogen oxides (NO x , x is greater than or equal to 0 and less than or equal to 2, preferably greater than or equal to 1 and less than or equal to 2), typically NO2 or NO forms an energy level in the insulating film 514 or the like. This energy level is located in the energy gap of the oxide semiconductor film 508. Therefore, when nitrogen oxide diffuses to the interface between the insulating film 514 and the oxide semiconductor film 508, sometimes this energy level captures electrons on one side of the insulating film 514. As a result, the captured electrons remain near the interface between the insulating film 514 and the oxide semiconductor film 508, thereby causing the threshold voltage of the transistor to drift in the positive direction.

[0231] In addition, when heat treatment is performed, nitrogen oxide reacts with ammonia and oxygen. When heat treatment is performed, nitrogen oxide contained in the insulating film 514 reacts with ammonia contained in the insulating film 516, thereby reducing nitrogen oxide contained in the insulating film 514. Therefore, electrons are not easily captured at the interface between the insulating film 514 and the oxide semiconductor film 508.

[0232] By using the above-described oxide insulating film as the insulating film 514 , a drift in the threshold voltage of the transistor can be reduced, thereby reducing variations in electrical characteristics of the transistor.

[0233] By performing a heat treatment in the manufacturing process of the transistor, typically a heat treatment at a temperature lower than 400°C or lower than 375°C (preferably at a temperature of 340°C or higher and 360°C or lower), in the spectrum of the insulating film 514 measured by ESR at 100K or lower, a first signal having a g value of 2.037 or higher and 2.039 or lower, a second signal having a g value of 2.001 or higher and 2.003 or lower, and a third signal having a g value of 1.964 or higher and 1.966 or lower are observed. In the ESR measurement of the X band, the split width between the first signal and the second signal and the split width between the second signal and the third signal are approximately 5 mT. In addition, the sum of the spin densities of the first signal having a g value of 2.037 or higher and 2.039 or lower, the second signal having a g value of 2.001 or higher and 2.003 or lower, and the third signal having a g value of 1.964 or higher and 1.966 or lower is less than 1×10 18 spins / cm 3 , typically 1×10 17 spins / cm 3 Above and below 1×10 18 spins / cm 3 .

[0234] In the ESR spectrum below 100K, the first signal with a g value of 2.037 to 2.039, the second signal with a g value of 2.001 to 2.003, and the third signal with a g value of 1.964 to 1.966 correspond to the emission of nitrogen oxides (NO x , x is greater than or equal to 0 and less than or equal to 2, preferably greater than or equal to 1 and less than or equal to 2). Typical examples of nitrogen oxides include nitrogen monoxide and nitrogen dioxide. That is, the smaller the total number of spin densities of the first signal having a g value of greater than or equal to 2.037 and less than or equal to 2.039, the second signal having a g value of greater than or equal to 2.001 and less than or equal to 2.003, and the third signal having a g value of greater than or equal to 1.964 and less than or equal to 1.966, the less the content of nitrogen oxides in the oxide insulating film.

[0235] The nitrogen concentration of the oxide insulating film measured by SIMS was 6×10 20 atoms / cm 3 the following.

[0236] By forming the oxide insulating film by a PECVD method using silane and nitrous oxide at a substrate temperature of 220° C. to 350° C., a dense film with high hardness can be formed.

[0237] The insulating film 516 is formed using an oxide insulating film whose oxygen content exceeds the stoichiometric composition. The oxide insulating film whose oxygen content exceeds the stoichiometric composition is heated, and part of its oxygen is released. According to TDS analysis, the amount of oxygen released from the oxide insulating film whose oxygen content exceeds the stoichiometric composition is 1.0×10 19 atoms / cm 3 Above, preferably 3.0×10 20 atoms / cm 3 Note that the surface temperature of the film during the above TDS analysis is preferably 100° C. or higher and 700° C. or lower, or 100° C. or higher and 500° C. or lower.

[0238] As the insulating film 516 , a silicon oxide film, a silicon oxynitride film, or the like can be used with a thickness of greater than or equal to 30 nm and less than or equal to 500 nm, preferably greater than or equal to 50 nm and less than or equal to 400 nm.

[0239] Furthermore, it is preferable to reduce the number of defects in the insulating film 516. Typically, the spin density of the signal at g = 2.001 due to dangling bonds of silicon measured by ESR is less than 1.5×10 18 spins / cm 3 , more preferably 1×10 18 spins / cm 3 Since the insulating film 516 is farther from the oxide semiconductor film 508 than the insulating film 514 , the defect density of the insulating film 516 can also be higher than that of the insulating film 514 .

[0240] In addition, since the insulating film 514 and the insulating film 516 can be formed using the same type of material, the interface between the insulating film 514 and the insulating film 516 may not be clearly confirmed. Therefore, in this embodiment, the interface between the insulating film 514 and the insulating film 516 is shown by a dotted line. Note that in this embodiment, although a two-layer structure of the insulating film 514 and the insulating film 516 is described, the present invention is not limited to this. For example, the insulating film 514 or the insulating film 516 may also have a single-layer structure.

[0241] The insulating film 518 has a function of blocking oxygen, hydrogen, water, alkali metals, alkaline earth metals, and the like. By providing the insulating film 518, oxygen can be prevented from diffusing from the oxide semiconductor film 508 to the outside, and oxygen contained in the insulating film 514 and the insulating film 516 can be prevented from diffusing to the outside, and hydrogen, water, and the like can be prevented from invading the oxide semiconductor film 508 from the outside. As the insulating film 518, for example, a nitride insulating film can be used. As the nitride insulating film, there are silicon nitride, silicon nitride oxide, aluminum nitride, aluminum nitride oxide, and the like. In particular, when silicon nitride oxide or a silicon nitride film is used as the insulating film 518, it is preferred because oxygen diffusion to the outside can be suppressed.

[0242] Alternatively, an oxide insulating film having a barrier effect on oxygen, hydrogen, water, etc. may be provided as the insulating film 518 instead of the nitride insulating film having a barrier effect on oxygen, hydrogen, water, alkali metals, alkaline earth metals, etc. Examples of the oxide insulating film having a barrier effect on oxygen, hydrogen, water, etc. include an aluminum oxide film, an aluminum oxynitride film, a gallium oxide film, a gallium oxynitride film, a yttrium oxide film, an yttrium oxynitride film, a hafnium oxide film, and a hafnium oxynitride film. As the oxide insulating film having a barrier effect on oxygen, hydrogen, water, etc., aluminum oxide, hafnium oxide, or yttrium oxide is particularly preferably used.

[0243] <Method 1 for manufacturing semiconductor device>

[0244] Next, refer to Figures 15 to 30 A method for manufacturing the transistor 500 of the semiconductor device according to one embodiment of the present invention will be described in detail.

[0245] First, a conductive film is formed over a substrate 502, and the conductive film is processed by a photolithography step and an etching step to form a conductive film 504 serving as a gate electrode. Next, an insulating film 506 and an insulating film 507 serving as a gate insulating film are formed over the conductive film 504 (see FIG. 1 ). Fig.15 ).

[0246] Next, for example, an oxide semiconductor film 509 is formed on the insulating film 507 by a sputtering method or the like at a first temperature. In addition, as the oxide semiconductor film 509, an insulating film 509a is formed, and then an oxide semiconductor film 509b is formed (see Fig.16 ).

[0247] The first temperature for forming the oxide semiconductor film 509 is above room temperature and below 340°C, preferably above room temperature and below 300°C, more preferably above 100°C and below 250°C, and further preferably above 100°C and below 200°C. By heating to form the oxide semiconductor film 509, the crystallinity of the oxide semiconductor film 509 can be improved. On the other hand, when a large glass substrate (for example, the 6th to 10th generation) is used as the substrate 502, the substrate 502 sometimes deforms when the first temperature is above 150°C and below 340°C. Therefore, when using a large glass substrate, the deformation of the glass substrate can be suppressed by setting the first temperature to above 100°C and below 150°C.

[0248] The substrate temperatures during the formation of the insulating film 509a and the oxide semiconductor film 509b may be the same or different, but preferably, the insulating film 509a and the oxide semiconductor film 509b are formed at the same substrate temperature because manufacturing costs can be reduced.

[0249] In the case of forming the oxide semiconductor film 509 by sputtering, as the sputtering gas, a rare gas (typically argon), oxygen, or a mixed gas of a rare gas and oxygen is appropriately used. In addition, when a mixed gas is used, it is preferred to increase the proportion of oxygen gas relative to the rare gas. In addition, the sputtering gas needs to be highly purified. For example, as a sputtering gas, oxygen gas or argon gas is used, and a high-purity gas with a dew point of less than -40°C, preferably less than -80°C, more preferably less than -100°C, and further preferably less than -120°C is used, thereby preventing moisture and the like from mixing into the oxide semiconductor film 509 as much as possible.

[0250] In addition, in the processing chamber of the sputtering device, it is preferable to use an adsorption type vacuum pump such as a cryopump to perform high vacuum evacuation (evacuation to 5×10 -7 Pa or more and 1×10 -4 Pa or less) to remove as much water and the like which are impurities to the oxide semiconductor film 509 as possible. Alternatively, it is preferable to combine a turbomolecular pump and a cold trap to prevent gas, especially gas containing carbon or hydrogen, from flowing back into the processing chamber from the exhaust system.

[0251] Next, the oxide semiconductor film 509 is processed to form an island-shaped oxide semiconductor film 508. Note that the insulating film 509a becomes the island-shaped oxide semiconductor film 508a, and the oxide semiconductor film 509b becomes the island-shaped oxide semiconductor film 508b (see Fig.17 ).

[0252] Next, a conductive film 512 to be a source electrode and a drain electrode is formed over the insulating film 507 and the oxide semiconductor film 508 without performing a step at a temperature higher than the first temperature (see Fig.18 ).

[0253] Next, masks 536a and 536b are formed in desired regions on the conductive film 512 (see Fig.19 ).

[0254] In this embodiment, a photosensitive resin film is applied on the conductive film 512 and the photosensitive resin film is patterned by a photolithography process, thereby forming the mask 536 a and the mask 536 b .

[0255] Next, the conductive film 512 is processed from above the conductive film 512, the mask 536a, and the mask 536b using an etchant 538, thereby forming the conductive film 512a and the conductive film 512b separated from each other (see FIG. 5A ). Fig. 20 ).

[0256] In this embodiment, the conductive film 512 is processed using a dry etching device. However, the processing method of the conductive film 512 is not limited to this. For example, a chemical solution may be used for the etchant 538 and a wet etching device may be used to process the conductive film 512 and the oxide semiconductor film 508b. Note that, compared with the case where the conductive film 512 is processed using a wet etching device, a finer pattern can be formed by processing the conductive film 512 using a dry etching device. On the other hand, compared with the case where the conductive film 512 is processed using a dry etching device, processing the conductive film 512 using a wet etching device can reduce manufacturing costs.

[0257] Next, the surface of the oxide semiconductor film 508b is cleaned from above the oxide semiconductor film 508b, the conductive film 512a, the conductive film 512b, the mask 536a, and the mask 536b using an etchant 539 (see Fig.21 ).

[0258] As the above-mentioned washing method, for example, washing using a chemical solution such as phosphoric acid can be cited. By washing using a chemical solution such as phosphoric acid, impurities attached to the surface of the oxide semiconductor film 508b (for example, elements contained in the conductive film 512a and the conductive film 512b) can be removed. Note that this washing is not necessarily required. Depending on the situation, this washing may not be performed.

[0259] Note that when the conductive films 512a and 512b are formed and / or in the above-described cleaning step, a region of the oxide semiconductor film 508b exposed from the conductive films 512a and 512b may become thinner than the oxide semiconductor film 508a.

[0260] In addition, when the conductive films 512a and 512b are formed and / or in the above-mentioned cleaning step, the region of the oxide semiconductor film 508b exposed from the conductive films 512a and 512b may not be thinned. Fig. 22 An example of this is shown below. Fig. 22 is a cross-sectional view showing an example of a semiconductor device. Fig. 22 A and Fig. 22 B is Figure 4 1 is an example of a case where the oxide semiconductor film 508b of the transistor 500 is not thinned. Fig. 22 C and Fig. 22 As shown in FIG. 2 , the oxide semiconductor film 508 b may be formed thinner than the oxide semiconductor film 508 a in advance, and the thickness of the region exposed from the conductive film 512 a and the conductive film 512 b may be set to be equal to Figure 4 The transistor 500 shown is equal. Fig. 22 E and Fig. 22 As shown in FIG. 5F, the oxide semiconductor film 508b may be formed thinner than the oxide semiconductor film 508a in advance, and an insulating film 519 may be formed on the oxide semiconductor film 508b and the insulating film 507. At this time, a contact hole for electrically connecting the oxide semiconductor film 508b to the conductive film 512a and the conductive film 512b is formed in the insulating film 519. The insulating film 519 may be formed using the same material and the same formation method as the insulating film 514.

[0261] Next, the mask 536a and the mask 536b are removed, so that the conductive film 512a serving as the source electrode and the conductive film 512b serving as the drain electrode are formed over the oxide semiconductor film 508b. The oxide semiconductor film 508 has a stacked-layer structure of the oxide semiconductor film 508a and the oxide semiconductor film 508b (see Fig.23 ).

[0262] Next, insulating films 514 and 516 are formed over the oxide semiconductor film 508, the conductive films 512a, and the conductive films 512b, and then a barrier film 531 is formed (see Fig.24 ).

[0263] In addition, it is preferable that the insulating film 516 is continuously formed without being exposed to the atmosphere after the insulating film 514 is formed. After the insulating film 514 is formed, the insulating film 516 is continuously formed without being exposed to the atmosphere by adjusting one or more of the flow rate, pressure, high-frequency power, and substrate temperature of the source gas, thereby reducing the concentration of impurities derived from atmospheric components at the interface between the insulating film 514 and the insulating film 516, and oxygen contained in the insulating film 514 and the insulating film 516 can be moved to the oxide semiconductor film 508, so that the amount of oxygen vacancies in the oxide semiconductor film 508 can be reduced.

[0264] For example, as the insulating film 514, a silicon oxynitride film can be formed by the PECVD method. At this time, as the source gas, it is preferred to use a deposition gas containing silicon and an oxidizing gas. Typical examples of deposition gases containing silicon are silane, disilane, trisilane, fluorinated silane, and the like. As oxidizing gases, there are nitrous oxide, nitrogen dioxide, and the like. In addition, the insulating film 514 containing nitrogen and having a small amount of defects can be formed by the PECVD method under the following conditions: the flow rate of the oxidizing gas is greater than 20 times and less than 100 times the flow rate of the above-mentioned deposition gas, preferably greater than 40 times and less than 80 times; and the pressure in the processing chamber is less than 100 Pa, preferably less than 50 Pa.

[0265] As the insulating film 516, for example, a silicon oxide film or a silicon oxynitride film is formed under the following conditions: the temperature of the substrate in a vacuum-evacuated processing chamber installed in a PECVD device is maintained at 180° C. or higher and 350° C. or lower, a source gas is introduced into the processing chamber and the pressure in the processing chamber is set to 100 Pa or higher and 250 Pa or lower, preferably 100 Pa or higher and 200 Pa or lower, and 0.17 W / cm2 is supplied to an electrode provided in the processing chamber. 2 Above 0.5W / cm 2 Below, more preferably 0.25W / cm 2 Above and 0.35W / cm 2 The following high frequency power.

[0266] In the film formation conditions of the insulating film 516, the high frequency power having the above power density is supplied in the reaction chamber having the above pressure, thereby improving the decomposition efficiency of the source gas in the plasma, increasing the oxygen radicals, and promoting the oxidation of the source gas, so that the oxygen content in the insulating film 516 exceeds the stoichiometric composition. On the other hand, in the film formed at the above substrate temperature, since the bonding force between silicon and oxygen is weak, part of the oxygen in the film is released by the heat treatment in the subsequent step. As a result, an oxide insulating film whose oxygen content exceeds the stoichiometric composition and part of the oxygen is released by heating can be formed.

[0267] In the step of forming the insulating film 516, the insulating film 514 is used as a protective film for the oxide semiconductor film 508. Therefore, the insulating film 516 can be formed using high-frequency power with high power density while reducing damage to the oxide semiconductor film 508.

[0268] In addition, in the film formation conditions of the insulating film 516, by increasing the flow rate of the deposition gas containing silicon relative to the oxidizing gas, the amount of defects in the insulating film 516 can be reduced. Typically, an oxide insulating film with a small amount of defects can be formed in which the spin density of the signal at g=2.001 due to the dangling bonds of silicon measured by ESR is less than 6×10 17 spins / cm 3 , preferably 3×10 17 spins / cm 3 Below, more preferably 1.5×10 17 spins / cm 3 As follows. This can improve the reliability of the transistor.

[0269] Alternatively, heat treatment may be performed after the insulating film 514 and the insulating film 516 are formed (in other words, after the insulating film 516 is formed and before the barrier film 531 is formed). By this heat treatment, nitrogen oxides included in the insulating film 514 and the insulating film 516 can be reduced. Also, by this heat treatment, part of oxygen included in the insulating film 514 and the insulating film 516 can be moved to the oxide semiconductor film 508 to reduce the amount of oxygen vacancies in the oxide semiconductor film 508.

[0270] The temperature of the heat treatment performed on the insulating film 514 and the insulating film 516 is typically set to be lower than 400°C, preferably lower than 375°C, more preferably higher than 150°C and lower than 360°C, and further preferably higher than 350°C and lower than 360°C. The heat treatment can be performed in an atmosphere of nitrogen, oxygen, ultra-dry air (air with a water content of less than 20 ppm, preferably less than 1 ppm, and more preferably less than 10 ppb) or a rare gas (argon, helium, etc.). The above-mentioned nitrogen, oxygen, ultra-dry air or rare gas preferably does not contain hydrogen, water, etc. The heat treatment can be performed using an electric furnace, an RTA device, etc.

[0271] The barrier film 531 contains oxygen and a metal (at least one selected from indium, zinc, titanium, aluminum, tungsten, tantalum, molybdenum, hafnium, and yttrium). When indium tin oxide (also called ITO (Indium Tin Oxide)), indium tin silicon oxide (also called ITSO), or indium oxide is used as the barrier film 531, the coverage of the uneven surface is good, so it is preferred.

[0272] In addition, the barrier film 531 can be formed by, for example, a sputtering method. When the barrier film 531 is very thin, it is sometimes difficult to suppress oxygen that may be released from the insulating film 516 to the outside. On the other hand, when the barrier film 531 is very thick, oxygen may not be properly added to the insulating film 516. Therefore, the thickness of the barrier film 531 is preferably not less than 1 nm and not more than 20 nm, and more preferably not less than 2 nm and not more than 10 nm. In this embodiment, ITSO with a thickness of 5 nm is formed as the barrier film 531.

[0273] Next, oxygen 540 is added to the insulating film 516 via the barrier film 531. Note that in the drawings, oxygen added to the insulating film 516 is schematically represented as oxygen 540a (see Fig.25 ). In addition, oxygen 540 is sometimes added to the insulating film 514.

[0274] As a method of adding oxygen 540 to the insulating film 516 via the barrier film 531, there are ion doping, ion implantation, plasma treatment, etc. In addition, as oxygen 540, excess oxygen or oxygen radicals can be cited. In addition, when adding oxygen 540, oxygen 540 can be effectively added to the insulating film 516 by applying a bias voltage to the substrate side. As the above-mentioned bias voltage, for example, the power density is set to 1 W / cm 2 Above and 5W / cm 2 By providing the barrier film 531 over the insulating film 516 to add oxygen, the barrier film 531 can be used as a protective film for suppressing the release of oxygen from the insulating film 516. Therefore, more oxygen can be added to the insulating film 516.

[0275] Next, the blocking film 531 or a portion of the blocking film 531 and a portion of the insulating film 516 are removed by an etchant 542 (see Fig.26 ).

[0276] As a method for removing a portion of the blocking film 531 and the insulating film 516, a dry etching method, a wet etching method, or a method combining the dry etching method and the wet etching method can be cited. Note that when the dry etching method is used, the etchant 542 is an etching gas, and when the wet etching method is used, the etchant 542 is a chemical solution. In this embodiment, the blocking film 531 is removed by the wet etching method. As a method for removing the blocking film 531, the wet etching method is preferably used because it can reduce the manufacturing cost.

[0277] Next, an insulating film 518 is formed on the insulating film 516 (see Fig. 27 ).

[0278] When the insulating film 518 is formed by the PECVD method, the substrate temperature is lower than 400° C., preferably lower than 375° C., and more preferably 340° C. to 360° C. When the substrate temperature is set to the above range when the insulating film 518 is formed, the excess oxygen or the oxygen radicals can be diffused into the oxide semiconductor film 508. When the substrate temperature is set to the above range when the insulating film 518 is formed, a dense film can be formed, which is preferred.

[0279] For example, when a silicon nitride film is formed as an insulating film 518 by a PECVD method, a deposition gas containing silicon, nitrogen, and ammonia are preferably used as source gases. By using a small amount of ammonia compared to nitrogen, ammonia dissociates in the plasma to generate active species. The active species cuts the bond between silicon and hydrogen and the triple bond of nitrogen contained in the deposition gas containing silicon. As a result, the bonding between silicon and nitrogen can be promoted, and a silicon nitride film with fewer bonds between silicon and hydrogen, fewer defects, and a dense structure can be formed. On the other hand, when the amount of ammonia is large relative to nitrogen, the decomposition of the deposition gas containing silicon and nitrogen does not progress, and the bond between silicon and hydrogen remains, resulting in the formation of a silicon nitride film with more defects and less density. Therefore, in the source gas, the flow ratio of nitrogen to ammonia is set to be greater than 5 times and less than 50 times, preferably greater than 10 times and less than 50 times.

[0280] Alternatively, heat treatment may be performed after forming the insulating film 518. Furthermore, by performing heat treatment after forming the insulating film 518, excess oxygen or oxygen radicals in the insulating film 516 can be diffused into the oxide semiconductor film 508, thereby filling oxygen vacancies in the oxide semiconductor film 508. Alternatively, by forming the insulating film 518 by heating, excess oxygen or oxygen radicals in the insulating film 516 can be diffused into the oxide semiconductor film 508, thereby filling oxygen vacancies in the oxide semiconductor film 508.

[0281] Next, a mask is formed on the insulating film 518 by a photolithography process, and a contact hole 542c reaching the conductive film 512b is formed in a desired region of the insulating film 514, the insulating film 516, and the insulating film 518 (see FIG. 5A ). Fig.28 ).

[0282] Next, a conductive film 520 is formed on the insulating film 518 so as to cover the contact hole 542c (see Fig.29 ).

[0283] Next, a mask is formed on the conductive film 520 by a photolithography process, and the conductive film 520 is processed into a desired shape to form the conductive film 520a and the conductive film 520b (see FIG. 1 ). Fig.30 ) As a method for forming the conductive film 520a and the conductive film 520b, a dry etching method, a wet etching method, a method combining a dry etching method and a wet etching method, or the like can be cited.

[0284] Although the various films such as the conductive film, insulating film, and oxide semiconductor film described above can be formed by, for example, a thermal CVD (Chemical Vapor Deposition: metal organic chemical vapor deposition) method or an atomic layer deposition (ALD: atomic layer deposition) method in addition to the methods described above, an MOCVD (Metal Organic Chemical Vapor Deposition: metal organic chemical vapor deposition) method can be cited as an example of the thermal CVD method.

[0285] Since the thermal CVD method is a film forming method that does not use plasma, it has an advantage that defects due to plasma damage do not occur.

[0286] Film formation using thermal CVD can be performed by supplying a source gas and an oxidant simultaneously into a chamber, setting the pressure in the chamber to atmospheric pressure or reduced pressure, and causing them to react near or on a substrate to deposit on the substrate.

[0287] In addition, film formation using the ALD method can also be performed in the following method: the pressure in the chamber is set to atmospheric pressure or reduced pressure, the source gas used for the reaction is introduced into the chamber in sequence, and the gas is repeatedly introduced in this order. For example, by switching each switch valve (also called a high-speed valve) to supply two or more source gases into the chamber in sequence, in order to prevent the mixing of multiple source gases, an inert gas (argon or nitrogen, etc.) is introduced at the same time or after the first source gas is introduced, and then the second source gas is introduced. Note that when the first source gas and the inert gas are introduced at the same time, the inert gas is used as a carrier gas. In addition, the inert gas can be introduced at the same time as the second source gas. In addition, the first source gas can be discharged by vacuum pumping without introducing an inert gas, and then the second source gas is introduced. The first source gas adheres to the surface of the substrate to form a first layer, and the second source gas introduced thereafter reacts with the first layer, thereby stacking the second layer on the first layer to form a thin film. By repeatedly introducing gases in this order until the desired thickness is obtained, a thin film with good step coverage can be formed. Since the thickness of the thin film can be adjusted by the number of times the gas is introduced in sequence, the ALD method can accurately adjust the thickness and is suitable for manufacturing micro FETs.

[0288] Various films such as the conductive film, insulating film, oxide semiconductor film, and metal oxide film described in the above embodiments can be formed by a thermal CVD method such as an MOCVD method. For example, when an In-Ga-ZnO film is formed, trimethyl indium, trimethyl gallium, and dimethyl zinc are used. The chemical formula of trimethyl indium is In(CH3)3. The chemical formula of trimethyl gallium is Ga(CH3)3. In addition, the chemical formula of dimethyl zinc is Zn(CH3)2. In addition, without being limited to the above combination, triethyl gallium (chemical formula is Ga(C2H5)3) can be used instead of trimethyl gallium, and diethyl zinc (chemical formula is Zn(C2H5)2) can be used instead of dimethyl zinc.

[0289] For example, when forming a hafnium oxide film using a film forming apparatus utilizing the ALD method, the following two gases are used: a source gas obtained by gasifying a liquid containing a solvent and a hafnium precursor compound (hafnium alkoxide, hafnium tetrakis dimethylamide (TDMAH) and other hafnium amides); and ozone (O3) used as an oxidant. The chemical formula of hafnium tetrakis dimethylamide is Hf[N(CH3)2]4. In addition, other material liquids include hafnium tetrakis (ethylmethylamide) and the like.

[0290] For example, when an aluminum oxide film is formed using a film forming apparatus using the ALD method, the following two gases are used: a source gas obtained by gasifying a liquid containing a solvent and an aluminum precursor compound (trimethylaluminum (TMA) or the like); and H2O used as an oxidant. In addition, the chemical formula of trimethylaluminum is Al(CH3)3. In addition, as other material liquids, there are tris(dimethylamide)aluminum, triisobutylaluminum, aluminum tris(2,2,6,6-tetramethyl-3,5-heptanedione), and the like.

[0291] For example, when a silicon oxide film is formed using a film forming apparatus utilizing the ALD method, hexachlorodisilane is attached to the film-forming surface to remove chlorine contained in the deposits, and radicals of an oxidizing gas (O2, nitrous oxide) are supplied to react with the deposits.

[0292] For example, when a tungsten film is formed using a film forming apparatus using the ALD method, WF6 gas and B2H6 gas are repeatedly introduced in sequence to form an initial tungsten film, and then WF6 gas and H2 gas are used to form a tungsten film. Note that SiH4 gas may be used instead of B2H6 gas.

[0293] For example, when an oxide semiconductor film such as an In-Ga-ZnO film is formed using a film forming apparatus utilizing the ALD method, In(CH3)3 gas and O3 gas are repeatedly introduced in sequence to form an In-O layer, then Ga(CH3)3 gas and O3 gas are used to form a GaO layer, and then Zn(CH3)2 gas and O3 gas are used to form a ZnO layer. Note that the order of these layers is not limited to the above example. In addition, these gases may also be mixed to form mixed compound layers such as an In-Ga-O layer, an In-Zn-O layer, a Ga-Zn-O layer, and the like. Note that although H2O gas obtained by bubbling with an inert gas such as Ar may be used instead of O3 gas, it is preferred to use O3 gas that does not contain H. In addition, In(C2H5)3 gas may be used instead of In(CH3)3 gas. In addition, Ga(C2H5)3 gas may be used instead of Ga(CH3)3 gas. In addition, Zn(CH3)2 gas may also be used.

[0294] Through the above process, it can be manufactured Figure 4 Transistor 500 is shown.

[0295] <Method 2 for manufacturing semiconductor device>

[0296] Next, Figures 15 to 30 Different manufacturing methods of the transistor 500 shown will be described below.

[0297] First, similarly to <Semiconductor device manufacturing method 1>, Figures 15 to 24 Then, no Figure 25 to Figure 27 The process shown is carried out Figures 28 to 30 The process shown.

[0298] At this time, a metal oxide film is used as the barrier film 531, and as the metal oxide film, aluminum oxide, hafnium oxide, or yttrium oxide is preferably formed.

[0299] When aluminum oxide, hafnium oxide, or yttrium oxide is formed by sputtering as the barrier film 531, the sputtering gas preferably contains at least oxygen. When forming the barrier film 531, by using oxygen as the sputtering gas, the oxygen becomes oxygen radicals in the plasma, and sometimes either or both of the oxygen and the oxygen radicals are added to the insulating film 516. Therefore, it is not necessary to perform sputtering. Fig.25 In other words, when the barrier film 531 is formed, the oxygen addition process and the formation of the barrier film 531 can be performed simultaneously. In addition, when the first barrier film is formed (especially in the initial stage of formation), the barrier film 531 has the function of adding oxygen, and after the barrier film 531 is formed, the barrier film 531 has the function of blocking oxygen.

[0300] When aluminum oxide is formed as the barrier film 531 by sputtering, for example, a mixed layer may be formed near the interface between the insulating film 516 and the barrier film 531. When the insulating film 516 is a silicon oxynitride film, Al2O3 may be formed as the mixed layer. x Si y O z .

[0301] In addition, when aluminum oxide, hafnium oxide, or yttrium oxide is used as the barrier film 531, aluminum oxide, hafnium oxide, and yttrium oxide have high insulation and high oxygen barrier properties. Fig.26 The process of removing the barrier film 531 is shown as well as Fig. 27 Therefore, the barrier film 531 has the same function as the insulating film 518.

[0302] In addition, by heating the barrier film 531 at a substrate temperature lower than 400° C., preferably lower than 375° C., and more preferably 340° C. or higher and 360° C. or lower during film formation, excess oxygen or oxygen radicals added to the insulating film 516 can be diffused into the oxide semiconductor film 508. Alternatively, when heat treatment is performed at a temperature lower than 400° C., preferably lower than 375° C., and more preferably 340° C. or higher and 360° C. or lower after the barrier film 531 is formed, excess oxygen or oxygen radicals added to the insulating film 516 can be diffused into the oxide semiconductor film 508.

[0303] In this way, by using aluminum oxide, hafnium oxide, or yttrium oxide as the barrier film 531, the manufacturing process of the semiconductor device can be shortened, thereby reducing the manufacturing cost.

[0304] The structure and method described in this embodiment can be used in combination with the structure and method described in other embodiment as appropriate.

[0305] Implementation 3

[0306] In this embodiment, a structure of a display device using a liquid crystal element as a display element is described.

[0307] Fig.31 yes Figure 1 A is a cross-sectional view between the dot-dash line QR. Fig.31 The semiconductor device 700 shown includes: a routing wiring portion 711; a region 722; a pixel portion 702; a source driver 704; and an FPC terminal portion 708. In addition, the routing wiring portion 711 includes a wiring 710. In addition, the pixel portion 702 includes a transistor 750 and a capacitor 790. In addition, the source driver 704 includes a transistor 752. The FPC terminal portion 708 includes a connection electrode 760, an anisotropic conductive film 780, and an FPC 716.

[0308] As the transistor 750 and the transistor 752 , the transistors described in Embodiment 2 can be used.

[0309] Transistor 750 is set at Figures 1 to 3 The scanning line 717 is shown in FIG. 717 . A portion of the scanning line 717 functions as a first gate electrode of the transistor 750 . In addition, a portion of the wiring 718 provided so as to overlap with the scanning line 717 functions as a second gate electrode of the transistor 750 .

[0310] The scan line 717 and the wiring 718 are electrically connected via a contact hole 719 formed in the region 722 .

[0311] The transistor used in this embodiment includes a highly purified oxide semiconductor film in which the formation of oxygen defects is suppressed. The transistor can reduce the current value in the off state (off-state current value). Therefore, the retention time of electrical signals such as image signals can be extended, and the write interval can also be extended in the state where the power is turned on. Therefore, the frequency of refresh work can be reduced, thereby achieving the effect of suppressing power consumption.

[0312] In addition, the transistor used in this embodiment can obtain a higher field effect mobility and can therefore be driven at high speed. For example, by using such a transistor capable of high-speed driving in a liquid crystal display device, a transistor in a pixel portion and a transistor in a drive circuit portion can be formed on the same substrate. In other words, since a semiconductor device formed of a silicon wafer or the like does not need to be used separately as a drive circuit, the number of components of the semiconductor device can be reduced. In addition, a high-quality image can also be provided in the pixel portion by using a transistor capable of high-speed driving.

[0313] The capacitor 790 has a structure having a dielectric between a pair of electrodes. More specifically, one electrode of the capacitor 790 uses a conductive film formed by the same process as the scanning line 717, and the other electrode of the capacitor 790 uses a conductive film used as a source electrode and a drain electrode of the transistor 750. In addition, the dielectric sandwiched between the pair of electrodes uses an insulating film used as a gate insulating film of the transistor 750.

[0314] In addition, Fig.31 In the embodiment, an insulating film 764 , an insulating film 766 , an insulating film 768 , and a planarizing insulating film 770 are provided over the transistor 750 , the transistor 752 , and the capacitor 790 .

[0315] The insulating film 764, the insulating film 766, and the insulating film 768 can be formed using the same material and manufacturing method as the insulating film 514, the insulating film 516, and the insulating film 518 described in Embodiment 2. As the planarization insulating film 770, a heat-resistant organic material such as a polyimide resin, an acrylic resin, a polyimide amide resin, a benzocyclobutene resin, a polyamide resin, an epoxy resin, etc. can be used. In addition, the planarization insulating film 770 can also be formed by stacking a plurality of insulating films formed of these materials. In addition, a structure in which the planarization insulating film 770 is not provided can also be adopted.

[0316] The wiring 710 is formed in the same process as a conductive film which functions as a source electrode and a drain electrode of the transistor 750 and the transistor 752. When a material including copper is used as the wiring 710, wiring resistance can be reduced.

[0317] The connection electrode 760 is formed in the same process as a conductive film used as a source electrode and a drain electrode of the transistor 750 and the transistor 752. The connection electrode 760 and a terminal included in the FPC 716 are electrically connected via an anisotropic conductive film 780.

[0318] A structure 778 is provided between the first substrate 701 and the second substrate 705. The structure 778 is a columnar spacer obtained by selectively etching an insulating film and is used to control the distance (cell gap) between the first substrate 701 and the second substrate 705. Alternatively, a spherical spacer may be used as the structure 778.

[0319] In this embodiment, the structure 778 is provided on the first substrate 701 side, but the present invention is not limited to this. For example, the structure 778 may be provided on the second substrate 705 side or on both the first substrate 701 and the second substrate 705.

[0320] On the second substrate 705 side, a light-shielding film 738 serving as a black matrix, a coloring layer 736 serving as a color filter, and an insulating film 734 in contact with the light-shielding film 738 and the coloring layer 736 are provided.

[0321] The semiconductor device 700 includes a liquid crystal element 775. The liquid crystal element 775 includes a conductive film 772, a conductive film 774, and a liquid crystal layer 776. The conductive film 774 is provided on the second substrate 705 side and is used as a counter electrode. The semiconductor device 700 can display an image by changing the orientation state of the liquid crystal layer 776 by applying a voltage to the conductive film 772 and the conductive film 774, thereby controlling the transmission and non-transmission of light. A protrusion 744 is provided on the conductive film 774.

[0322] The conductive film 772 is connected to the conductive film used as the source electrode and the drain electrode of the transistor 750. The conductive film 772 is formed on the planarization insulating film 770 and used as a pixel electrode, that is, an electrode of the display element. In addition, the conductive film 772 has a function as a reflective electrode. The semiconductor device 700 is a so-called reflective color liquid crystal display device in which external light is reflected by the conductive film 772 and displayed through the coloring layer 736.

[0323] In addition, as the conductive film 772, a conductive film that is translucent to visible light or a conductive film that is reflective to visible light can be used. As the conductive film that is translucent to visible light, for example, a material containing one selected from indium (In), zinc (Zn), and tin (Sn) is preferably used. As the conductive film that is reflective to visible light, for example, a material containing aluminum or silver is preferably used. In this embodiment, a conductive film that is reflective to visible light is used as the conductive film 772.

[0324] In addition, when a conductive film that is reflective to visible light is used, the conductive film 772 may also have a stacked structure. For example, an aluminum film having a thickness of 100 nm is formed as a lower layer, and a silver alloy film (e.g., an alloy film containing silver, palladium, and copper) having a thickness of 30 nm is formed as an upper layer. By adopting the above structure, the following excellent effects are exerted.

[0325] The above-mentioned excellent effects are as follows: (1) the adhesion between the base film and the conductive film 772 can be improved; (2) the aluminum film and the silver alloy film can be etched together using a chemical solution; (3) the cross-sectional shape of the conductive film 772 can be made into a good shape (for example, a tapered shape). The reason for (3) is considered to be as follows: when etching is performed using a chemical solution, the etching speed of the aluminum film is slower than that of the silver alloy film, or when the lower aluminum film is exposed after etching the upper silver alloy film, electrons are extracted from the metal that is cheaper than the silver alloy film, in other words, aluminum with a high ionization tendency, so that the etching of the silver alloy film is suppressed, and the etching speed of the lower aluminum film is accelerated.

[0326] In addition, as Fig.31 The semiconductor device 700 shown in the figure is a reflective color liquid crystal display device, but the display device 700 is not limited to this. For example, a transmissive color liquid crystal display device using a conductive film having light transmittance to visible light as the conductive film 772 may also be used. In the case where the semiconductor device 700 is a transmissive liquid crystal display device, a pair of electrodes included in the capacitor element 790 is set at a position that does not overlap with the conductive film 772. In addition, each layer provided in the path of light incident from the substrate 701 through the liquid crystal element 775 and the coloring layer 736 is preferably a layer having light transmittance to visible light.

[0327] In addition, although Fig.31 Although not shown in the figure, optical components (optical substrates) such as polarization components, phase difference components, and anti-reflection components may be appropriately provided. For example, circular polarization using a polarization substrate and a phase difference substrate may also be used. In addition, backlight, side light, etc. may also be used as a light source.

[0328] The structure described in this embodiment mode can be implemented in combination with the structures described in other embodiment modes as appropriate.

[0329] Implementation 4

[0330] In this embodiment, refer to Figure 32 to Figure 36 A memory device including a semiconductor device according to one embodiment of the present invention will be described.

[0331] Fig.32 A is a circuit diagram of a cell 1000 included in the memory device in this embodiment, including a transistor 1200 , a transistor 600 , and a capacitor 1400 .

[0332] As shown in Embodiment 2, since the transistor 600 uses an oxide semiconductor, the off-state current of the transistor 600 is small. Therefore, a specific node of the semiconductor device can maintain storage content for a long period of time. That is, since a refresh operation is not required or the frequency of the refresh operation can be made extremely low, a semiconductor device with low power consumption can be realized.

[0333] In the cell 1000, the first wiring 1001 is electrically connected to one of the source electrode and the drain electrode of the transistor 1200, and the second wiring 1002 is electrically connected to the other of the source electrode and the drain electrode of the transistor 1200. In addition, the third wiring 1003 is electrically connected to one of the source electrode and the drain electrode of the transistor 600, and the fourth wiring 1004 is electrically connected to the first gate electrode of the transistor 600. Furthermore, the gate electrode of the transistor 1200 and the other of the source electrode and the drain electrode of the transistor 600 are electrically connected to one electrode of the capacitor 1400, and the fifth wiring 1005 is electrically connected to the other electrode of the capacitor 1400. In addition, the sixth wiring 1006 is electrically connected to the second gate electrode (also called the back gate electrode) of the transistor 600.

[0334] The memory device including the cell 1000 has a feature of being able to hold the potential of the gate of the transistor 1200, and thus can write, hold, and read information as described below.

[0335] The writing and holding of information are described. First, the potential of the fourth wiring 1004 is set to a potential that makes the transistor 600 in a conducting state, so that the transistor 600 is in a conducting state. Thus, the potential of the third wiring 1003 is applied to the node FG electrically connected to the gate of the transistor 1200 and an electrode of the capacitor 1400. In other words, a predetermined charge is applied to the gate of the transistor 1200 (writing). Here, any one of two different levels of charge (hereinafter referred to as low-level charge and high-level charge) is applied. Then, the transistor 600 is placed in a non-conducting state by setting the potential of the fourth wiring 1004 to a potential that makes the transistor 600 in a non-conducting state, so that the node FG retains the charge (maintains).

[0336] Since the off-state current of the transistor 600 is small, the charge of the node FG is retained for a long time.

[0337] Next, the reading of information is described. When a proper potential (reading potential) is applied to the fifth wiring 1005 while a predetermined potential (constant potential) is applied to the first wiring 1001, the second wiring 1002 has a potential corresponding to the amount of charge held in the node FG. This is because, when the transistor 1200 is an n-channel transistor, the apparent threshold voltage V when a high-level charge is applied to the gate of the transistor 1200 is th_H is lower than the apparent threshold voltage V when a low level charge is applied to the gate of transistor 1200 th_L Here, the apparent threshold voltage refers to the potential of the fifth wiring 1005 required to turn the transistor 1200 into the "on state". th_H With V th_L The potential V0 between the fifth wiring 1005 and the fifth wiring 1006 can distinguish the charge applied to the node FG. For example, when the node FG is supplied with a high-level charge during writing, if the potential of the fifth wiring 1005 is V0 (> V th_H ), the transistor 1200 is in the “on state”. On the other hand, when the node FG is supplied with low-level charges, even if the potential of the fifth wiring 1005 is V0 (<V th_L ), the transistor 1200 also maintains the "non-conductive state". Therefore, by identifying the potential of the second wiring 1002, the information stored in the node FG can be read.

[0338] Note that the information of the desired cell must be read when reading. In the memory cell where the information is not to be read, a potential that causes the transistor 1200 to be in a "non-conductive state" regardless of the charge applied to the node FG is applied to the fifth wiring 1005, that is, a potential lower than V th_H Alternatively, a potential higher than V is applied to the fifth wiring 1005, which makes the transistor 1200 "on" regardless of the charge applied to the node FG. th_L The potential of , that’s it.

[0339] Fig.32 The cell 1100 shown in B is different from the cell 1000 in that it does not include the transistor 1200. In this case as well, the data writing and holding operations can be performed by the same operations as the cell 1000.

[0340] The data readout in the cell 1100 is described. When the transistor 600 is turned on, the third wiring 1003 and the capacitor 1400 in the floating state are turned on, and the charge is redistributed between the third wiring 1003 and the capacitor 1400. As a result, the potential of the third wiring 1003 changes. The amount of change in the potential of the third wiring 1003 has different values ​​depending on the potential of one electrode of the capacitor 1400 (or the charge accumulated in the capacitor 1400).

[0341] For example, when the potential of one electrode of the capacitor 1400 is V, the capacitance of the capacitor 1400 is C, the capacitance component of the third wiring 1003 is CB, and the potential of the third wiring 1003 before the redistribution of the charge is VB0, the potential of the third wiring 1003 after the redistribution of the charge is (CB×VB0+CV) / (CB+C). Therefore, assuming that the unit is in a state where the potential of one electrode of the capacitor 1400 is two states, namely V1 and V0 (V1>V0), it can be known that the potential of the third wiring 1003 when the potential V1 is maintained (=(CB×VB0+CV1) / (CB+C)) is higher than the potential of the third wiring 1003 when the potential V0 is maintained (=(CB×VB0+CV0) / (CB+C)).

[0342] Furthermore, by comparing the potential of the third wiring 1003 with a predetermined potential, data can be read.

[0343] In addition, since the storage device including the unit 1000 or the unit 1100 does not require a high voltage when writing data, it is not easy for the element to deteriorate. For example, unlike the existing non-volatile memory, it is not necessary to inject electrons into the floating gate or extract electrons from the floating gate, so the problem of insulation film degradation does not occur. In other words, in the storage device of one embodiment of the present invention, the number of rewrites that is a problem in the existing non-volatile memory is not limited, and its reliability is greatly improved. Furthermore, data is written according to the on state / off state of the transistor, so high-speed operation can be performed.

[0344] Fig.33 Show that Fig.32 The cells 1000 shown in A are arranged in a matrix-shaped cell array 1010. The wirings 1001 and 1003 are connected to the wiring 1011, the wiring 1002 is connected to the wiring 1012, the wiring 1004 is connected to the wiring 1014, the wiring 1005 is connected to the wiring 1015, and the wiring 1006 is connected to the wiring 1016. That is, the wiring 1014 is electrically connected to the first gate electrode of the transistor 600, and the wiring 1016 is electrically connected to the second gate electrode of the transistor 600.

[0345] like Fig.33 As shown, when the wiring 1014 and the wiring 1015 are electrically connected by the wiring 1017 in the area outside the cell array 1010, there is no need to provide a contact hole for electrically connecting the wiring 1014 and the wiring 1015 to the cell 1000, thereby improving the density of the cell 1000.

[0346] In addition, a contact hole may be provided in a part of the cell 1000 to electrically connect the wiring 1014 and the wiring 1015. For example, a contact hole may be provided in the cell 1000 in each chip. By providing the contact hole in the area outside the cell array 1010 and in the cell 1000, the distance between the contact holes can be reduced. Therefore, the signal delay between the wiring 1014 and the wiring 1015 can be reduced. Note that, although the distance between the contact holes is preferably as equal as possible, it may be different.

[0347] Even when contact holes for electrically connecting the wiring 1014 and the wiring 1015 are provided in a part of the cells 1000 , the density of the cells 1000 can be increased compared to the case where contact holes are provided in all the cells 1000 .

[0348] Fig.34 is corresponding to Fig.32 A cross-sectional view of unit 1000. Note that Fig.34 A. Fig.34 B and Fig.34 C is a cross-sectional view of different parts.

[0349] Fig.34 The semiconductor device shown includes a transistor 1200 , a transistor 600 , and a capacitor 1400 . The transistor 600 and the capacitor 1400 are disposed above the transistor 1200 .

[0350] The transistor 1200 is a transistor using a semiconductor substrate 450 . The transistor 1200 includes a region 472 a in the semiconductor substrate 450 , a region 472 b in the semiconductor substrate 450 , an insulating film 462 , and a conductive film 454 .

[0351] In the transistor 1200, the region 472a and the region 472b function as a source region and a drain region. In addition, the insulating film 462 functions as a gate insulating film. In addition, the conductive film 454 functions as a gate electrode. Therefore, the resistance of the channel formation region can be controlled by the potential applied to the conductive film 454. In other words, the conduction / non-conduction between the region 472a and the region 472b can be controlled by the potential applied to the conductive film 454.

[0352] The semiconductor substrate 450 may be, for example, a single material semiconductor substrate made of silicon or germanium, or a compound semiconductor substrate made of silicon carbide, silicon germanium, gallium arsenide, indium phosphide, zinc oxide, or gallium oxide. Preferably, a single crystal silicon substrate is used as the semiconductor substrate 450 .

[0353] A semiconductor substrate containing an impurity imparting n-type conductivity is used as the semiconductor substrate 450. Note that a semiconductor substrate containing an impurity imparting p-type conductivity may also be used as the semiconductor substrate 450. In this case, a well containing an impurity imparting n-type conductivity may be provided in the region where the transistor 1200 is formed. Alternatively, the semiconductor substrate 450 may be i-type.

[0354] The top surface of the semiconductor substrate 450 preferably has a (110) plane. This can improve the on-state characteristics of the transistor 1200.

[0355] The region 472a and the region 472b are regions containing an impurity imparting p-type conductivity. Thus, the transistor 1200 has a p-channel structure.

[0356] Note that the transistor 1200 is separated from an adjacent transistor by a region 460 or the like. The region 460 has an insulating property.

[0357] Fig.34 The unit 1000 shown includes an insulating film 464, an insulating film 466, an insulating film 468, an insulating film 422, a conductive film 480a, a conductive film 480b, a conductive film 480c, a conductive film 478a, a conductive film 478b, a conductive film 478c, a conductive film 476a, a conductive film 476b, a conductive film 474a, a conductive film 474b, a conductive film 474c, a conductive film 496a, a conductive film 496b, a conductive film 496c, a conductive film 496d, a conductive film 498a, a conductive film 498b, a conductive film 498c, a conductive film 498d, an insulating film 490, an insulating film 492, an insulating film 428, an insulating film 409 and an insulating film 494.

[0358] Here, the insulating film 422, the insulating film 428, and the insulating film 409 are insulating films having a barrier property. Fig.34 The semiconductor device shown has a structure in which the transistor 600 is surrounded by an insulating film having a barrier property. Note that any one or more of the insulating film 422, the insulating film 428, and the insulating film 409 may not be included.

[0359] The insulating film 464 is disposed on the transistor 1200. The insulating film 466 is disposed on the insulating film 464. The insulating film 468 is disposed on the insulating film 466. The insulating film 490 is disposed on the insulating film 468. The transistor 600 is disposed on the insulating film 490. The insulating film 492 is disposed on the transistor 600. The insulating film 494 is disposed on the insulating film 492.

[0360] The insulating film 464 includes a contact hole reaching the region 472a, a contact hole reaching the region 472b, and a contact hole reaching the conductive film 454. The conductive film 480a, the conductive film 480b, or the conductive film 480c is filled in each contact hole.

[0361] The insulating film 466 includes a contact hole reaching the conductive film 480a, a contact hole reaching the conductive film 480b, and a contact hole reaching the conductive film 480c. The conductive film 478a, the conductive film 478b, or the conductive film 478c is filled in each contact hole.

[0362] The insulating film 468 and the insulating film 422 include a contact hole reaching the conductive film 478b and a contact hole reaching the conductive film 478c. The conductive film 476a or the conductive film 476b is filled in each contact hole.

[0363] The insulating film 490 includes a contact hole overlapping with the channel formation region of the transistor 600, a contact hole reaching the conductive film 476a, and a contact hole reaching the conductive film 476b. The conductive film 474a, the conductive film 474b, or the conductive film 474c is filled in each contact hole.

[0364] The conductive film 474a may also function as a second gate electrode (also referred to as a back gate electrode) of the transistor 600. That is, the transistor 600 has the s-channel structure described in Embodiment 2. Thus, the on-state current of the transistor 600 can be increased. In addition, since the punch-through phenomenon can be suppressed, the electrical characteristics of the transistor 600 in the saturation region can be stabilized.

[0365] The insulating film 409 and the insulating film 492 include a contact hole reaching a conductive film 617 overlapping with a conductive film 612a serving as one of the source electrode and the drain electrode of the transistor 600 via an insulating film 615, a contact hole reaching a conductive film 616 serving as a gate electrode of the transistor 600, a contact hole reaching a conductive film 474b through a conductive film 612b serving as the other of the source electrode and the drain electrode of the transistor 600, and a contact hole reaching a conductive film 474c through a conductive film 612a serving as one of the source electrode and the drain electrode of the transistor 600. The conductive film 496a, the conductive film 496b, the conductive film 496c, or the conductive film 496d is filled in each of the contact holes. Note that each contact hole may sandwich a contact hole included in any of the components such as the transistor 600.

[0366] The insulating film 494 includes a contact hole reaching the conductive film 496a, a contact hole reaching the conductive film 496b, a contact hole reaching the conductive film 496c, and a contact hole reaching the conductive film 496d. The conductive film 498a, the conductive film 498b, the conductive film 498c, or the conductive film 498d is filled in each contact hole.

[0367] As the insulating films 464, 466, 468, 490, 492, and 494, for example, a single layer or a stacked layer of an insulating film containing boron, carbon, nitrogen, oxygen, fluorine, magnesium, aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zirconium, lanthanum, neodymium, hafnium, or tantalum can be used. For example, as the insulating film 401, aluminum oxide, magnesium oxide, silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, neodymium oxide, hafnium oxide, or tantalum oxide can be used.

[0368] One or more of the insulating film 464 , the insulating film 466 , the insulating film 468 , the insulating film 490 , the insulating film 492 , and the insulating film 494 preferably includes an insulating film having a barrier property.

[0369] As an insulating film having the function of blocking impurities such as hydrogen and oxygen, for example, a single layer or a stack of insulating films containing boron, carbon, nitrogen, oxygen, fluorine, magnesium, aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zirconium, lanthanum, neodymium, hafnium or tantalum can be used.

[0370] As the conductive film 480a, the conductive film 480b, the conductive film 480c, the conductive film 478a, the conductive film 478b, the conductive film 478c, the conductive film 476a, the conductive film 476b, the conductive film 474a, the conductive film 474b, the conductive film 474c, the conductive film 496a, the conductive film 496b, the conductive film 496c, the conductive film 496d, the conductive film 498a, the conductive film 498b, the conductive film 498c and the conductive film 498d, for example, a single layer or a stacked layer of a conductive film containing one or more of boron, nitrogen, oxygen, fluorine, silicon, phosphorus, aluminum, titanium, chromium, manganese, cobalt, nickel, copper, zinc, gallium, yttrium, zirconium, molybdenum, ruthenium, silver, indium, tin, tantalum and tungsten can be used. For example, an alloy or a compound may be used, and a conductive film including aluminum, a conductive film including copper and titanium, a conductive film including copper and manganese, a conductive film including indium, tin, and oxygen, a conductive film including titanium and nitrogen, etc. may be used. At least one of the conductive films 480a, 480b, 480c, 478a, 478b, 478c, 476a, 476b, 474a, 474b, 474c, 496a, 496b, 496c, 496d, 498a, 498b, 498c, and 498d preferably includes a conductive film having a barrier property.

[0371] The source electrode or the drain electrode of the transistor 1200 is electrically connected to the conductive film 612b serving as the other of the source electrode and the drain electrode of the transistor 600 through the conductive film 480b, the conductive film 478b, the conductive film 476a, the conductive film 474b, and the conductive film 496c. Further, the conductive film 454 serving as the gate electrode of the transistor 1200 is electrically connected to the conductive film 612a serving as one of the source electrode and the drain electrode of the transistor 600 through the conductive film 480c, the conductive film 478c, the conductive film 476b, the conductive film 474c, and the conductive film 496d.

[0372] The capacitor 1400 includes an insulating film 615 and a conductive film 617. Note that the insulating film 615 can be formed by the same process as the insulating film 614 used as the gate insulating film of the transistor 600, thereby improving productivity, which is sometimes preferred. In addition, when a layer formed by the same process as the conductive film 616 used as the gate electrode of the transistor 600 is used as the conductive film 617, productivity can be improved, which is sometimes preferred. However, these films may also be formed by different processes.

[0373] Notice, Fig.35 The unit 1000 shown is Fig.34 The cell 1000 shown differs only in the structure of transistor 1200. Fig.35 The unit 1000 shown, with reference to Fig.34 Specifically, in Fig.35 In the unit 1000 shown, the transistor 1200 is a Fin type. By making the transistor 1200 a Fin type, the effective channel width is increased, so that the on-characteristics of the transistor 1200 can be improved. In addition, since the influence of the electric field of the gate electrode can be increased, the off-characteristics of the transistor 1200 can be improved. Note that Fig.35 A. Fig.35 B and Fig.35 C is a cross-sectional view of different parts.

[0374] in addition, Fig.36 The unit 1000 shown is Fig.34 The cell 1000 shown differs only in the structure of transistor 1200. Fig.36 The unit 1000 shown, with reference to Fig.34 Specifically, in Fig.36 In the illustrated cell 1000 , the transistor 1200 is disposed on a SOI substrate. Fig.36 The structure in which the region 456 and the semiconductor substrate 450 are separated by the insulating film 452 is shown. By using an SOI substrate, a punch-through phenomenon can be suppressed, so that the off characteristics of the transistor 1200 can be improved. Note that the insulating film 452 can be formed by insulating a part of the semiconductor substrate 450. For example, silicon oxide can be used as the insulating film 452. Note that Fig.36 A. Fig.36 B and Fig.36 C is a cross-sectional view of different parts.

[0375] exist Figure 34 to Figure 36 In the unit 1000 shown, since a p-channel transistor is formed using a semiconductor substrate and an n-channel transistor is formed thereon, the area occupied by the element can be reduced. In other words, the integration of the semiconductor device can be improved. In addition, compared with the case where an n-channel transistor and a p-channel transistor are formed using the same semiconductor substrate, the manufacturing process can be simplified, so the productivity of the semiconductor device can be improved. In addition, the yield of the semiconductor device can be improved. In addition, the p-channel transistor can sometimes omit complex processes such as the formation of the LDD (Lightly Doped Drain) region, the formation of a shallow trench (Shallow Trench) structure, or the bending design. Therefore, compared with the unit 1000 in which an n-channel transistor is formed using a semiconductor substrate, Figure 34 to Figure 36 The illustrated unit 1000 can sometimes improve productivity and yield.

[0376] In this embodiment, the case where the transistor 1200 is a p-channel transistor is described; however, the transistor 1200 may be an n-channel transistor.

[0377] Note that in this embodiment, the transistor 600 may also be the transistor 500 .

[0378] The structure described in this embodiment mode can be implemented in combination with the structures described in other embodiment modes as appropriate.

[0379] Implementation method 5

[0380] In this embodiment, refer to Fig.37 and Fig.38 A display module and an electronic device including a semiconductor device according to one embodiment of the present invention will be described.

[0381] Fig.37 The display module 8000 shown includes a touch panel 8004 connected to an FPC 8003 , a display panel 8006 connected to an FPC 8005 , a backlight 8007 , a frame 8009 , a printed circuit board 8010 , and a battery 8011 between an upper cover 8001 and a lower cover 8002 .

[0382] The semiconductor device of one embodiment of the present invention can be used for the display panel 8006, for example.

[0383] The shapes and sizes of the upper cover 8001 and the lower cover 8002 may be appropriately changed according to the sizes of the touch panel 8004 and the display panel 8006 .

[0384] The touch panel 8004 may be a resistive film touch panel or an electrostatic capacitive touch panel, and may be formed in a manner overlapping with the display panel 8006. In addition, the opposing substrate (sealing substrate) of the display panel 8006 may also have a touch panel function. In addition, a light sensor may be provided in each pixel of the display panel 8006 to form an optical touch panel.

[0385] Backlight 8007 includes light source 8008. Note that although Fig.37 2 shows a structure in which the light source 8008 is arranged on the backlight 8007, but the present invention is not limited thereto. For example, the light source 8008 may be arranged at the end of the backlight 8007, and a light diffusion plate may be used. When a self-luminous light-emitting element such as an organic EL element is used, or when a reflective panel is used, a structure in which the backlight 8007 is not arranged may be adopted.

[0386] The frame 8009 has a function of protecting the display panel 8006 and also has an electromagnetic shielding function for blocking electromagnetic waves generated by the operation of the printed circuit board 8010. In addition, the frame 8009 may also have a function of a heat sink.

[0387] The printed circuit board 8010 includes a power supply circuit and a signal processing circuit for outputting a video signal and a clock signal. As a power supply for supplying power to the power supply circuit, either an external commercial power supply or a separately provided battery 8011 can be used. When a commercial power supply is used, the battery 8011 can be omitted.

[0388] In addition, components such as a polarizing plate, a phase difference plate, and a prism sheet may also be provided in the display module 8000 .

[0389] Fig.38 A to Fig.38 G is a diagram showing electronic devices. These electronic devices may include a housing 5000, a display unit 5001, a speaker 5003, an LED lamp 5004, an operation key 5005 (including a power switch or an operation switch), a connection terminal 5006, a sensor 5007 (having a function of measuring the following factors: force, displacement, position, speed, acceleration, angular velocity, rotation speed, distance, light, liquid, magnetism, temperature, chemical substance, sound, time, hardness, electric field, current, voltage, electricity, radiation, flow, humidity, inclination, vibration, smell or infrared), a microphone 5008, etc.

[0390] Fig.38 A shows a mobile computer, which may include a switch 5009, an infrared port 5010, etc. in addition to the above. Fig.38 B shows a portable image reproduction device (for example, a DVD reproduction device) equipped with a recording medium. In addition to the above, the portable image reproduction device may further include a second display unit 5002, a recording medium reading unit 5011, and the like. Fig.38 C shows a goggles-type display, which may include a second display portion 5002, a support portion 5012, earphones 5013, and the like in addition to the above. Fig.38 D shows a portable game machine, which may include a recording medium reading unit 5011 and the like in addition to the above. Fig.38 E shows a digital camera having a television reception function, which may include an antenna 5014, a shutter button 5015, an image receiving unit 5016, and the like in addition to the above. Fig.38 F shows a portable game machine, which may include a second display portion 5002, a recording medium reading portion 5011, and the like in addition to the above. Fig.38 G shows a portable television receiver, which may include a charger 5017 capable of transmitting and receiving signals, etc. in addition to the above.

[0391] Fig.38 A to Fig.38 The electronic device shown in G may have various functions. For example, it may have the following functions: displaying various data (static images, dynamic images, text images, etc.) on the display unit; touch panel; displaying calendar, date or time, etc.; controlling processing by using various software (programs); performing wireless communications; connecting to various computer networks by using the wireless communication function; sending or receiving various data by using the wireless communication function; reading out programs or data stored in a recording medium to display them on the display unit, etc. Furthermore, in an electronic device having multiple display units, it may have the following functions: one display unit mainly displays image data, while another display unit mainly displays text data; or, images that take parallax into account are displayed on multiple display units to display stereoscopic images, etc. Furthermore, in an electronic device having an image receiving unit, it may have the following functions: shooting static images; shooting dynamic images; automatically or manually correcting the shot images; storing the shot images in a recording medium (external or built-in to the camera); displaying the shot images on the display unit, etc. Note that, Fig.38 A to Fig.38 The functions that the electronic device indicated by G can have are not limited to the above functions, but can have various functions.

[0392] The semiconductor device described in Embodiments 1 to 4 can be applied to the electronic device described in this embodiment.

[0393] The structure described in this embodiment mode can be implemented in combination with the structures described in other embodiment modes as appropriate.

[0394] Explanation of symbols

[0395] 401 Insulation Film

[0396] 409 Insulation Film

[0397] 422 Insulation film

[0398] 428 Insulation film

[0399] 450 Semiconductor Substrate

[0400] 452 Insulation film

[0401] 454 Conductive film

[0402] 456 Area

[0403] 460 Area

[0404] 462 Insulation film

[0405] 464 Insulation film

[0406] 466 Insulation film

[0407] 468 Insulation film

[0408] 472a Area

[0409] 472b Zone

[0410] 474a Conductive film

[0411] 474b Conductive film

[0412] 474c Conductive film

[0413] 476a Conductive film

[0414] 476b Conductive film

[0415] 478a Conductive film

[0416] 478b Conductive film

[0417] 478c Conductive film

[0418] 480a Conductive film

[0419] 480b Conductive film

[0420] 480c Conductive film

[0421] 490 Insulation film

[0422] 492 Insulation film

[0423] 494 Insulation film

[0424] 496a Conductive film

[0425] 496b Conductive film

[0426] 496c Conductive film

[0427] 496d Conductive film

[0428] 498a Conductive film

[0429] 498b Conductive film

[0430] 498c Conductive film

[0431] 498d Conductive film

[0432] 500 transistors

[0433] 502 substrate

[0434] 504 Conductive film

[0435] 506 Insulation film

[0436] 507 Insulation Film

[0437] 508 Oxide semiconductor film

[0438] 508a Oxide semiconductor film

[0439] 508b Oxide semiconductor film

[0440] 509 Oxide semiconductor film

[0441] 509a Insulation film

[0442] 509b Oxide semiconductor film

[0443] 512 Conductive film

[0444] 512a Conductive film

[0445] 512b Conductive film

[0446] 514 Insulation film

[0447] 516 Insulation film

[0448] 518 Insulation film

[0449] 519 Insulation Film

[0450] 520 Conductive film

[0451] 520a Conductive film

[0452] 520b Conductive film

[0453] 531 Barrier Film

[0454] 536a Mask

[0455] 536b Mask

[0456] 538 Etching Agent

[0457] 539 Etching Agent

[0458] 540 Oxygen

[0459] 540a Oxygen

[0460] 542 Etching Agent

[0461] 542a Contact hole

[0462] 542b Contact hole

[0463] 542c Contact hole

[0464] 570 transistors

[0465] 600 transistors

[0466] 602 Substrate

[0467] 604 Conductive film

[0468] 606 Insulation Film

[0469] 608 Oxide semiconductor film

[0470] 608a Oxide semiconductor film

[0471] 608b Oxide semiconductor film

[0472] 612a Conductive film

[0473] 612b Conductive film

[0474] 614 Insulation film

[0475] 615 Insulation film

[0476] 616 Conductive film

[0477] 617 Conductive film

[0478] 618 Insulation film

[0479] 700 Semiconductor devices

[0480] 701 Substrate

[0481] 702 Pixel Department

[0482] 703 Pixel Department

[0483] 704 Source Driver

[0484] 705 substrate

[0485] 706 Gate Driver

[0486] 706a Gate Driver

[0487] 706b Gate Driver

[0488] 708 FPC terminal

[0489] 710 Wiring

[0490] 711 Wiring Department

[0491] 712 Sealant

[0492] 716 FPC

[0493] 717 scan lines

[0494] 717a Scan Line

[0495] 717b scan lines

[0496] 718 Wiring

[0497] 719 Contact hole

[0498] 719a Contact hole

[0499] 719b Contact hole

[0500] 719c Contact hole

[0501] 720 signal line

[0502] 721 Area

[0503] 722 Area

[0504] 730 Area

[0505] 734 Insulation film

[0506] 736 Coloring Layer

[0507] 738 shading film

[0508] 744 Protrusion

[0509] 750 transistors

[0510] 752 transistors

[0511] 760 Connecting electrodes

[0512] 764 Insulation film

[0513] 766 Insulation film

[0514] 768 Insulation film

[0515] 770 Planarization insulation film

[0516] 772 Conductive film

[0517] 774 Conductive film

[0518] 775 Liquid crystal element

[0519] 776 Liquid crystal layer

[0520] 778 Structure

[0521] 780 Anisotropic Conductive Film

[0522] 790 Capacitor Components

[0523] 1000 units

[0524] 1001 Wiring

[0525] 1002 Wiring

[0526] 1003 Wiring

[0527] 1004 Wiring

[0528] 1005 Wiring

[0529] 1006 Wiring

[0530] 1010 cell array

[0531] 1011 Wiring

[0532] 1012 Wiring

[0533] 1014 Wiring

[0534] 1015 Wiring

[0535] 1016 Wiring

[0536] 1017 Wiring

[0537] 1100 units

[0538] 1200 transistors

[0539] 1400 Capacitor Components

[0540] 5000 Housing

[0541] 5001 Display

[0542] 5002 Display unit

[0543] 5003 Speaker

[0544] 5004 LED Light

[0545] 5005 Operation keys

[0546] 5006 Connection Terminals

[0547] 5007 Sensor

[0548] 5008 Microphone

[0549] 5009 Switch

[0550] 5010 Infrared port

[0551] 5011 Recording medium reading unit

[0552] 5012 Support

[0553] 5013 Headphones

[0554] 5014 Antenna

[0555] 5015 Shutter button

[0556] 5016 Image Receiving Unit

[0557] 5017 Charger

[0558] 8000 Display Module

[0559] 8001 Cover

[0560] 8002 Lower cover

[0561] 8003 FPC

[0562] 8004 Touch Panel

[0563] 8005 FPC

[0564] 8006 Display Panel

[0565] 8007 Backlight

[0566] 8008 Light Source

[0567] 8009 Framework

[0568] 8010 Printed Circuit Board

[0569] 8011 Battery

Claims

1. A display device, comprising: A pixel portion including a plurality of pixels, at least one of the plurality of pixels including: Transistors, including: a first gate electrode; an oxide semiconductor film on the first gate electrode; and a second gate electrode on the oxide semiconductor film, wherein the oxide semiconductor film contains indium, gallium and zinc, wherein a first wiring including a region serving as the first gate electrode of the transistor and a second wiring including a region serving as the second gate electrode of the transistor overlap with each other, wherein the first wiring and the second wiring are electrically connected to a gate driver, wherein, in a plan view, a first end portion of the first wiring is electrically connected to a first end portion of the second wiring through a contact hole in a first region outside the pixel portion, wherein the second end of the first wiring and the second end of the second wiring are located in a second region outside the pixel portion, wherein no contact hole for electrically connecting the first wiring and the second wiring is provided in the second region, and wherein the pixel portion is located between the first region and the second region.

2. A display device, comprising: A pixel portion including a plurality of pixels, at least one of the plurality of pixels including: Transistors, including: a first gate electrode; a gate insulating film on the first gate electrode; an oxide semiconductor film on the gate insulating film; a source electrode and a drain electrode electrically connected to the oxide semiconductor film; and a second gate electrode on the oxide semiconductor film; and a capacitor including a first electrode and a second electrode, wherein the oxide semiconductor film contains indium, gallium and zinc, wherein a first wiring including a region serving as the first gate electrode of the transistor and a second wiring including a region serving as the second gate electrode of the transistor overlap with each other, wherein the first wiring and the second wiring are electrically connected to a gate driver, wherein, in a plan view, a first end portion of the first wiring is electrically connected to a first end portion of the second wiring through a contact hole in a first region outside the pixel portion, wherein the second end of the first wiring and the second end of the second wiring are located in a second region outside the pixel portion, wherein no contact hole for electrically connecting the first wiring and the second wiring is provided in the second region, wherein the pixel portion is located between the first region and the second region, and Here, one of the source electrode and the drain electrode of the transistor is used as the first electrode of the capacitor.

3. A display device, comprising: A pixel portion including a plurality of pixels, at least one of the plurality of pixels including: The first transistor comprises: Silicon semiconductors; and a gate electrode on the silicon semiconductor; A second transistor on the first transistor, the second transistor comprising: a first gate electrode; an oxide semiconductor film on the first gate electrode; a source electrode and a drain electrode electrically connected to the oxide semiconductor film; and a second gate electrode on the oxide semiconductor film; and a capacitor including a first electrode and a second electrode, wherein the oxide semiconductor film contains indium, gallium and zinc, wherein a first wiring including a region serving as the first gate electrode of the second transistor and a second wiring including a region serving as the second gate electrode of the transistor overlap with each other, wherein the first wiring and the second wiring are electrically connected to a gate driver, wherein, in a plan view, a first end portion of the first wiring is electrically connected to a first end portion of the second wiring through a contact hole in a first region outside the pixel portion, wherein the second end of the first wiring and the second end of the second wiring are located in a second region outside the pixel portion, wherein no contact hole for electrically connecting the first wiring and the second wiring is provided in the second region, The pixel portion is located between the first region and the second region. wherein one of the source electrode and the drain electrode of the second transistor is used as the first electrode of the capacitor, and The channel of the second transistor does not overlap with the channel of the first transistor.

4. The display device according to any one of claims 1 to 3, wherein: The oxide semiconductor film has a thickness of 3 nm to 50 nm.

5. The display device according to any one of claims 1 to 3, wherein: The oxide semiconductor film includes nanocrystals.

6. The display device according to any one of claims 1 to 3, wherein: The first gate electrode and the second gate electrode include the same conductive material. 7 . The display device according to claim 1 , further comprising an organic EL element.

Citation Information

Patent Citations

  • Semiconductor integrated circuit

    JP2012257187A

  • Semiconductor device

    JP2014063141A

  • Semiconductor device

    JP2014199402A

  • Array substrate for display device and method of fabricating the same

    KR1020140082368A

  • Semiconductor device

    US20150084047A1