Semiconductor structure and method for forming the same
By using alloy layer and alloy mask layer to etch the substrate in the semiconductor process, the problems of insufficient imaging resolution of the photoresist and uneven polymer impurities are solved, and the uniformity of trench morphology and electrical performance are improved.
Patent Information
- Application Number
- CN202010129524.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-02-28
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2040-02-28
AI Technical Summary
In the existing semiconductor processes, insufficient imaging resolution of photoresist leads to the problem of refining the pattern line width of the integrated circuit, and uneven polymer impurities lead to uneven trench morphology, affecting electrical performance.
Using an alloy layer as a mask, by forming a pattern definition layer, an opening and an alloy layer on the alloy mask material layer, removing the pattern definition layer, and etching the substrate with the alloy layer and the alloy mask layer to form separate trenches and spacers. The layer uses the uniform distribution of polymer impurities with metal ions to improve the groove morphology and metal connection quality.
It improves the morphological uniformity of the trench and the quality of metal connections, improves the electrical performance of the semiconductor structure, and meets the demand for refining the pattern line width of the integrated circuit.
Smart Images

Figure CN113327850B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a method for forming the same. Background Art
[0002] As the integration of integrated circuits continues to increase, integrated circuits are rapidly developing towards submicron and deep submicron directions, and their pattern line widths will become increasingly fine, which places higher demands on semiconductor processes. Therefore, in-depth research on how to achieve fine line width patterns to meet the new requirements of semiconductor processes has become an urgent topic.
[0003] Lithography is a key process technology for realizing integrated circuit patterns. In lithography, a photosensitive material (photoresist) is coated on a thin film of a substrate, and light of a wavelength corresponding to the photosensitivity of the photoresist is used to irradiate the surface of the photoresist through a mask with a specific pattern. After development, a photoresist pattern corresponding to the pattern on the mask is formed. In the subsequent process of the integrated circuit, the photoresist pattern is used as a barrier layer to selectively etch the thin film underneath, so that the pattern on the mask can be completely transferred to the thin film of the substrate. The finer the line width of the integrated circuit pattern, the higher the imaging resolution of the photoresist is required, and the imaging resolution of the photoresist is inversely proportional to the wavelength of the exposure light source. Therefore, reducing the wavelength of the exposure light source becomes the main way to achieve fine line width patterns.
[0004] At present, with the development of integrated circuits, lithography technology has gone through the development process of G-line lithography (436nm), I-line lithography (365nm), KrF deep ultraviolet lithography (248nm) and ArF deep ultraviolet lithography (193nm). The types of exposure light sources include near ultraviolet (NearUltra-Violet, NUV), mid ultraviolet (MidUltra-Violet, MUV), deep ultraviolet (DeepUltra-Violet, DUV), extreme ultraviolet (Extreme Ultraviolet Lithography, EUV) and many others. Summary of the invention
[0005] The problem solved by the embodiments of the present invention is to provide a semiconductor structure and a method for forming the same, so as to optimize the electrical performance of the semiconductor structure.
[0006] To solve the above problems, an embodiment of the present invention provides a method for forming a semiconductor structure, comprising: providing a base, the base comprising a substrate and an alloy mask material layer located on the substrate; forming a graphic definition layer on the alloy mask material layer; forming an opening or a plurality of discrete openings in the graphic definition layer, the opening exposing the alloy mask material layer; forming an alloy layer in the opening; after forming the alloy layer, removing the graphic definition layer; etching the alloy mask material layer using the alloy layer as a mask to form an alloy mask layer; etching the substrate using the alloy layer and the alloy mask layer as masks to form a plurality of spaced grooves and a substrate spacer located between the grooves in the substrate.
[0007] Correspondingly, an embodiment of the present invention also provides a semiconductor structure, comprising: providing a base, the base comprising a substrate and an alloy mask material layer located on the substrate; a graphic definition layer located on the alloy mask material layer, the graphic definition layer having one or more openings exposing the alloy mask material layer; and an alloy layer located in the opening.
[0008] Compared with the prior art, the technical solution of the embodiment of the present invention has the following advantages:
[0009] In the method for forming a semiconductor structure provided by an embodiment of the present invention, the alloy mask material layer is etched using the alloy layer as a mask to form an alloy mask layer, and the substrate is etched using the alloy layer and the alloy mask layer as masks to form a plurality of separated grooves in the substrate. In the embodiment of the present invention, the materials of the alloy layer and the alloy mask layer are both alloy materials, and in the process of etching to form the grooves, the polymer impurities generated are all polymer impurities with metal ions, and the obstacles caused by the polymer impurities with metal ions in the etching process are relatively consistent, so that the morphology of the grooves is uniform and better, and accordingly, the quality of the metal wiring subsequently formed in the grooves is better, which is conducive to improving the electrical performance of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figures 1 to 9 It is a schematic structural diagram corresponding to each step in a method for forming a semiconductor structure;
[0011] Figures 10 to 21 It is a schematic structural diagram corresponding to each step in the first embodiment of the method for forming a semiconductor structure according to an embodiment of the present invention. DETAILED DESCRIPTION
[0012] As can be seen from the background technology, the devices currently formed still have the problem of poor performance. The reasons for the poor performance of the devices are now analyzed in combination with a method for forming a semiconductor structure.
[0013] refer to Figures 1 to 9, showing a structural schematic diagram corresponding to each step in a method for forming a semiconductor structure.
[0014] refer to Figure 1 The semiconductor structure includes: a substrate 1, a substrate mask material layer 2 located on the substrate 1, and a pattern definition layer 3 located on the substrate mask material layer 2.
[0015] Combined with reference Figures 1 to 5 , after multiple doping film forming steps, multiple doping layers 9 are sequentially formed in the graphic definition layer 3, and the doping film forming steps include: forming a first mask layer 7 on the graphic definition layer 3; forming an opening 8 exposing the graphic definition layer 3 in the first mask layer 7; doping ions in the graphic definition layer 3 exposed by the opening 8 to form a doping layer 9; after forming the doping layer 9, removing the first mask layer 7; the etching resistance of the doping layer 9 is greater than the etching resistance of the graphic definition layer 3.
[0016] The first mask layer 7 includes: an organic material layer 4 , an anti-reflection coating 5 located on the organic material layer 4 , and a first photoresist layer 6 located on the anti-reflection coating 5 .
[0017] refer to Figure 6 After forming a plurality of the doping layers 9, the pattern definition layer 3 is removed.
[0018] refer to Figure 7 , Figure 7 Based on Figure 6 An isometric view of the structure of the semiconductor device 10 is shown in FIG. 1 . After removing the pattern definition layer 3, a second mask layer 11 is formed, and the second mask layer 11 has a groove 12.
[0019] refer to Figure 8 , using the second mask layer 11 as a mask, the substrate mask material layer 2 is etched to form a substrate mask layer 10 .
[0020] After the substrate mask layer 10 is formed, the second mask layer 11 is removed.
[0021] refer to Fig. 9 After removing the second mask layer 11 , the substrate 1 is etched using the doping layer 9 and the substrate mask layer 10 as masks to form a trench 13 in the substrate 1 .
[0022] Usually, the material of the doping layer 9 is silicon doped with boron ions, and the material of the substrate mask layer 10 is usually alloy materials such as titanium nitride. Correspondingly, in the process of forming the groove 13, the polymer impurities generated by etching the doping layer 9 do not contain metal ions, and the polymer impurities generated by etching the substrate mask layer 10 contain metal ions. The polymer impurities with metal ions and the polymer impurities without metal ions are randomly and unevenly distributed on the surface of the substrate 1. The obstacles caused in the etching process are inconsistent, resulting in poor morphological uniformity of the groove 13. Accordingly, the quality of the metal connection subsequently formed in the groove 13 is poor, resulting in poor electrical performance of the semiconductor structure.
[0023] In order to solve the technical problem, an embodiment of the present invention provides a method for forming a semiconductor structure, comprising: providing a base, the base comprising a substrate and an alloy mask material layer located on the substrate; forming a graphic definition layer on the alloy mask material layer; forming an opening or a plurality of discrete openings in the graphic definition layer, the opening exposing the alloy mask material layer; forming an alloy layer in the opening; after forming the alloy layer, removing the graphic definition layer; etching the alloy mask material layer using the alloy layer as a mask to form an alloy mask layer; etching the substrate using the alloy layer and the alloy mask layer as masks to form a plurality of spaced grooves and a substrate spacer located between the grooves in the substrate.
[0024] In the method for forming a semiconductor structure provided by an embodiment of the present invention, the alloy mask material layer is etched using the alloy layer as a mask to form an alloy mask layer, and the substrate is etched using the alloy layer and the alloy mask layer as masks to form a plurality of separated grooves in the substrate. In the embodiment of the present invention, the materials of the alloy layer and the alloy mask layer are both alloy materials, and in the process of etching to form the grooves, the polymer impurities generated are all polymer impurities with metal ions, and the obstacles caused by the polymer impurities with metal ions in the etching process are relatively consistent, so that the morphology of the grooves is uniform and better, and accordingly, the quality of the metal wiring subsequently formed in the grooves is better, which is conducive to improving the electrical performance of the semiconductor structure.
[0025] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present invention more obvious and easy to understand, specific embodiments of the embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0026] Figures 10 to 21 It is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure according to an embodiment of the present invention.
[0027] refer to Fig.10 , providing a substrate, wherein the substrate includes a substrate 100 and an alloy mask material layer 101 located on the substrate 100 .
[0028] In this embodiment, the material of the substrate 100 includes a dielectric layer. Subsequently, an alloy layer is formed on the substrate 100, and the dielectric layer is etched using the alloy layer as a mask to form a groove in the dielectric layer.
[0029] The material of the dielectric layer is a low-k dielectric material, which is beneficial to reducing the parasitic capacitance between the subsequently formed metal wirings, and further beneficial to reducing the subsequent RC delay.
[0030] Specifically, the material of the dielectric layer includes SiCOH.
[0031] It should be noted that the substrate 100 also includes a transistor, which is usually formed at the bottom of the dielectric layer. The transistor includes a gate structure and source and drain doped regions located on both sides of the gate structure. Contact hole plugs (not shown in the figure) in contact with the source and drain doped regions are also formed in the substrate.
[0032] The alloy mask material layer 101 is used to prepare for the subsequent etching of the dielectric layer. The alloy mask material layer 101 has a high etching resistance. In the subsequent etching process of the dielectric layer, the dielectric layer and the alloy mask material layer 101 have a large etching selectivity.
[0033] In this embodiment, the material of the alloy mask material layer 101 includes one or more of TiN, TiO 2 , HfN, ZrO 2 and Al 2 O 3 .
[0034] Continue to refer Fig.10 , a pattern definition layer 102 is formed on the alloy mask material layer 101.
[0035] The pattern definition layer 102 is used to provide a process platform for the subsequent formation of an alloy layer.
[0036] In this embodiment, the material of the pattern definition layer 102 is amorphous silicon. In other embodiments, the material of the pattern definition layer can also be silicon oxide. Amorphous silicon is a commonly used material in the process, and the formation process is simple, which is conducive to reducing the process cost of the semiconductor structure.
[0037] It should be noted that the graphic definition layer 102 should not be too thick or too thin. If the graphic definition layer 102 is too thick, the aspect ratio of the opening formed in the graphic definition layer 102 is too large, and voids are easily present in the alloy layer formed in the opening by the selective deposition process, resulting in poor quality of the alloy layer; if the graphic definition layer 102 is too thin, the depth of the opening formed in the graphic definition layer 102 is too small, and the depth of the opening will limit the height of the alloy layer. In the subsequent etching of the alloy mask material layer 101 using the alloy layer as a mask to form the alloy mask layer, the alloy layer cannot play a good role as a mask. In this embodiment, in the step of providing the graphic definition layer 102, the thickness of the graphic definition layer 102 is 30 nanometers to 50 nanometers.
[0038] refer to Figures 11 to 16 , forming an opening or a plurality of discrete openings 104 (such as Fig.16 As shown), the opening 104 exposes the alloy mask material layer 101 .
[0039] The opening 104 provides a space for subsequently forming an alloy layer.
[0040] In this embodiment, taking the formation of a plurality of openings 104 in the pattern definition layer 102 as an example, the step of forming the openings 104 in the pattern definition layer 102 to expose the alloy mask material layer 101 includes:
[0041] like Figures 11 to 15 After multiple doping film forming steps, multiple discrete doping layers 105 (such as Fig.15 As shown), the etching resistance of the doping layer 105 is less than the etching resistance of the pattern definition layer 102.
[0042] The etching resistance of the doping layer 105 is lower than that of the pattern definition layer 102 , and in the subsequent step of removing the doping layer 105 , the pattern definition layer 102 is less damaged.
[0043] Specifically, the doping film forming step includes:
[0044] like Fig.11 As shown, a mask layer 103 is formed on the pattern definition layer 102 .
[0045] In this embodiment, the mask layer 103 includes an organic material layer 1031 , an anti-reflective coating layer 1032 located on the organic material layer 1031 , and a photoresist layer 1033 located on the anti-reflective coating layer 1032 .
[0046] In this embodiment, the organic material layer 1031 includes an ODL (organic dielectric layer) material, a DUO (Deep UV Light Absorbing Oxide) material, or a SOC (spin on carbon) material.
[0047] In this embodiment, the material of the anti-reflective coating 1032 includes a BARC (bottom anti-reflective coating) material or a Si-ARC (Silicon anti-reflective coating) material.
[0048] like Fig.12 As shown, a groove 106 exposing the pattern definition layer 102 is formed in the mask layer 103 .
[0049] The groove 106 defines a region to be doped in the pattern definition layer 102 .
[0050] The step of forming the groove 106 includes: exposing the photoresist layer 1033 to form a photoresist groove (not shown in the figure) in the photoresist layer 1033; after the photoresist groove is formed, a dry etching process is used to etch the anti-reflective coating 1032 and the organic material layer 1031 exposed by the photoresist groove to form the groove 106.
[0051] In this embodiment, the dry etching process has the characteristics of anisotropic etching and good etching profile, and can transfer the photoresist groove pattern in the photoresist layer 1033 to the anti-reflective coating 1032 and the organic material layer 1031 .
[0052] It should be noted that, in this embodiment, the photoresist layer 1033, the anti-reflective coating 1032 and the organic material layer 1031 are continuously consumed in the step of forming the groove 106. When the groove 106 is formed, the photoresist layer 1033 has been completely etched away. In other embodiments, when the groove is formed, the photoresist layer may not be completely consumed.
[0053] like Fig.13 As shown, ions are doped into the pattern definition layer 102 exposed by the groove 106 to form a doping layer 105 .
[0054] Ions are doped into the graphic definition layer 102 exposed in the groove 106, so that the material of the graphic definition layer 102 doped with ions is modified, the etching resistance of the doped layer 105 is lower than that of the graphic definition layer 102, and the etching resistance of the doped layer 105 is lower than that of the alloy mask material layer 101. In the subsequent process of removing the doped layer 105, the graphic definition layer 102 and the alloy mask material layer 101 are less damaged.
[0055] In this embodiment, ions are doped into the pattern definition layer 102 exposed in the groove 106 by ion implantation to form a doping layer 105. Ion implantation has the characteristics of simple operation and low process cost.
[0056] Specifically, in the step of doping ions in the pattern definition layer exposed by the groove, the doped ions include phosphorus ions.
[0057] The process parameters of ion implantation include: a doping ion implantation dose of 1.0E19 atoms per square centimeter to 1.0E21 atoms per square centimeter; a doping ion implantation energy of 1Kev to 20Kev, and an angle between the doping ion implantation angle and the surface normal of the substrate 100 is less than 10 degrees.
[0058] It should be noted that the doping ion implantation dose should not be too large or too small. Taking the extension direction perpendicular to the groove 106 as the lateral direction, if the doping ion implantation dose is too large, it will take too much process time, and the formation efficiency of the doping layer 105 is low. If the doping ion implantation dose is too large, the doping ions will diffuse laterally into the graphic definition layer 102 directly below the groove 106 where the organic material layer 1031 is not exposed. In the subsequent process of removing the doping layer 105, the lateral size of the formed opening will be larger than the lateral size of the pre-designed opening, and the lateral size of the alloy layer subsequently formed in the opening will be too large, resulting in the lateral size of the groove formed by etching the substrate 100 using the alloy layer as a mask being too small, which does not meet the process requirements and is not conducive to optimizing the electrical properties of the semiconductor structure. If the doping ion implantation dose is too small, the etching selectivity of the formed doping layer 105 and the pattern definition layer 102 is relatively small. In the subsequent process of removing the doping layer 105, the lateral size of the formed opening is smaller than the lateral size of the pre-designed opening, and the lateral size of the alloy layer subsequently formed in the opening is too small, resulting in the lateral size of the groove formed by etching the substrate 100 based on the alloy layer as a mask being too small, which does not meet the process requirements and is not conducive to optimizing the electrical performance of the semiconductor structure. In this embodiment, the doping ion implantation dose is 1.0E19 atoms per square centimeter to 1.0E21 atoms per square centimeter.
[0059] It should be noted that the implantation energy of the doping ions should not be too large or too small. If the doping ion implantation energy is too large, the doping ions are likely to pass through the graphic definition layer 102 and enter the alloy mask material layer 101. In the process of etching and removing the doping layer 105 to form an opening, the alloy mask material layer 101 is easily damaged. Subsequently, an alloy layer is formed in the opening, and the alloy mask material layer 101 is etched with the alloy layer to form an alloy mask layer. The height of the mask composed of the alloy layer and the alloy mask layer is relatively small, which is not conducive to forming a groove of a specified depth, resulting in poor electrical performance of the semiconductor structure; if the doping ion implantation energy is too small, the doping ions are likely to stay on the surface of the graphic definition layer 102, resulting in a relatively small etching selectivity between the doping layer 105 and the graphic definition layer 102. In the process of etching and removing the doping layer 105, the lateral size of the opening formed is smaller than the lateral size of the pre-designed opening, and then the lateral size of the alloy layer subsequently formed in the opening is too small, resulting in the lateral size of the groove formed by etching the substrate 100 based on the alloy layer as a mask being too small, which does not meet the process requirements and is not conducive to optimizing the electrical performance of the semiconductor structure. In this embodiment, the implantation energy is 1 KeV to 20 KeV.
[0060] The angle between the doping ion implantation direction and the surface normal of the substrate 100 should not be too large. If the angle is too large, in the process of ion implantation of the pattern definition layer 102 exposed by the groove 106, due to the shadow effect, the doping ions are easily implanted into the organic material layer 1031 and the anti-reflective coating 1032. In the subsequent process of removing the doping layer 105, the etching selectivity of the doping layer 105 and the pattern definition layer 102 is relatively small. In the subsequent process of removing the doping layer 105, the lateral size of the formed opening is smaller than the lateral size of the pre-designed opening, and the lateral size of the alloy layer subsequently formed in the opening is too small, resulting in the lateral size of the groove formed by etching the substrate 100 based on the alloy layer as a mask. It is too small, does not meet the process requirements, and causes the electrical performance of the semiconductor structure to be poor. In this embodiment, the angle between the ion implantation direction and the surface normal of the substrate 100 is less than 10 degrees.
[0061] like Fig.14 As shown, after the doping layer 105 is formed, the mask layer 103 is removed.
[0062] In this embodiment, a plurality of openings need to be formed in the pattern definition layer 102, so the mask layer 103 is removed to prepare for the next doping film forming step.
[0063] After the doping layer 105 is formed, the material of the mask layer 103 includes an organic material layer 1031 and an anti-reflection coating 1032 located on the organic material layer 1031 .
[0064] In this embodiment, an ashing process is used to remove the mask layer 103 .
[0065] like Fig.15 As shown, after multiple doping and film-forming steps, a plurality of discrete doping layers 105 are formed in the pattern definition layer 102 .
[0066] In a subsequent process, the doping layer 105 is removed and a plurality of discrete openings are formed in the pattern definition layer 102 .
[0067] like Fig.16 As shown, the doping layer 105 is removed, and a plurality of openings 104 exposing the alloy mask material layer 101 are formed in the pattern definition layer 102 .
[0068] The opening 104 provides a process space for subsequently forming an alloy layer.
[0069] In this embodiment, an isotropic dry etching process is used to remove the doped layer 105. The isotropic dry etching process has the characteristics of high etching efficiency, simple operation, etc., and is not easy to damage the top of the alloy mask material layer 101. The material of the doped layer 105 includes amorphous silicon doped with phosphorus, and the corresponding etching gas includes hydrogen fluoride gas. In other embodiments, an anisotropic dry etching process can also be used to remove the doped layer.
[0070] It should be noted that, in other embodiments, the step of forming an opening in the graphic definition layer to expose the alloy mask material layer includes: forming a mask layer on the graphic definition layer, the mask layer having a plurality of grooves exposing the graphic definition layer; using the mask layer as a mask, doping ions in the graphic definition layer exposed by the grooves to form a plurality of doped layers, the etching resistance of the doped layers being less than that of the graphic definition layer; and removing the doped layers to form a plurality of openings in the graphic definition layer to expose the alloy mask material layer.
[0071] refer to Fig.17 , an alloy layer 107 is formed in the opening 104 .
[0072] Subsequently, the alloy mask material layer 101 is etched using the alloy layer 107 as a mask to form an alloy mask layer, and the substrate 100 is etched using the alloy layer 107 and the alloy mask layer as masks to form a plurality of separated grooves in the substrate 100. In the embodiment of the present invention, the materials of the alloy layer 107 and the alloy mask layer are both alloy materials, and in the process of etching to form the grooves, the polymer impurities generated are all polymer impurities with metal ions, and the obstacles caused by the polymer impurities with metal ions in the etching process are relatively consistent, so that the morphology uniformity of the grooves is better, and accordingly, the quality of the metal wiring subsequently formed in the grooves is better, which is conducive to improving the electrical performance of the semiconductor structure.
[0073] It should be noted that, in the step of etching the alloy mask material layer 101 using the alloy layer 107 as a mask, the etching selectivity ratio between the alloy mask material layer 101 and the alloy layer 107 should not be too small. If the etching selectivity ratio is too small, in the process of etching the alloy mask material layer 101 using the alloy layer 107 as a mask, the alloy layer 107 is easily consumed prematurely, resulting in the alloy layer 107 not being able to play a good role as a mask, and correspondingly, resulting in poor formation quality of the grooves in the dielectric layer. In this embodiment, in the step of etching the alloy mask material layer 101 using the alloy layer 107 as a mask, the etching selectivity ratio between the alloy mask material layer 101 and the alloy layer 107 is greater than 3.
[0074] In this embodiment, the material of the alloy layer includes one or more of TiN, TiO2, HfN, ZrO2 and Al2O3.
[0075] In this embodiment, in the step of forming the alloy layer 107 in the opening 104 , the top surface of the alloy layer 107 is lower than the top surface of the pattern definition layer 102 .
[0076] The top surface of the alloy layer 107 is lower than the top surface of the pattern definition layer 102 , so that in the subsequent step of removing the pattern definition layer 102 , the alloy layer 107 is not likely to block the pattern definition layer 102 , making it difficult for the pattern definition layer 102 to remain.
[0077] It should be noted that the alloy layer 107 should not be too high or too low. If the alloy layer 107 is too high, after the alloy mask material layer 101 is etched using the alloy layer 107 as a mask to form an alloy mask layer, the height of the alloy layer 107 is still too high, and it is easy to spend too much process time to remove the alloy layer 107. If the alloy layer 107 is too low, in the process of etching the alloy mask material layer 101 using the alloy layer 107 as a mask to form an alloy mask layer, the alloy layer 107 is not easy to play the role of an etching mask. In this embodiment, in the step of forming the alloy layer 107 in the opening 104, the thickness of the alloy layer 107 is one-third to two-thirds of the depth of the opening 104. Specifically, the height of the alloy layer 107 is 10 nanometers to 30 nanometers.
[0078] In this embodiment, a selective deposition process is used to form an alloy layer 107 on the alloy mask material layer 101 exposed by the opening 104. The alloy layer 107 is in direct contact with the alloy mask material layer 101.
[0079] The steps of the selective deposition process include: forming hydroxyl groups (not shown in the figure) on the graphic definition layer 102; after the hydroxyl groups are formed, treating the hydroxyl groups with a gas containing a hydrophobic functional group; after treating the hydroxyl groups with a gas containing a hydrophobic functional group, selectively forming an alloy layer 107 on the alloy mask material layer 101 exposed by the opening.
[0080] The step of forming the hydroxyl group on the top of the pattern definition layer 102 includes reacting the top of the pattern definition layer 102 with water to form the hydroxyl group.
[0081] In this embodiment, the material of the pattern definition layer 102 includes amorphous silicon. In the process of amorphous silicon reacting with water to form silicon oxide, the silicon oxide can be provided with hydroxyl groups.
[0082] It should be noted that the method for forming the semiconductor structure also includes: before the top of the graphic definition layer 102 reacts with water, forming a graphic shielding layer (not shown in the figure) in the opening 104, and the graphic shielding layer is lower than the top of the graphic definition layer 102.
[0083] The graphic shielding layer makes it difficult for water to contact the side walls and bottom surface of the opening, thereby making it difficult for water to react with the side walls and bottom surface of the opening, and it is not easy to form hydroxyl groups on the side walls and bottom surface of the opening, so that hydroxyl groups are only formed on the top of the graphic definition layer 102.
[0084] Correspondingly, in the step of reacting the top of the pattern definition layer 102 with water to form the hydroxyl group, the pattern definition layer 102 above the pattern shielding layer is reacted with water to form the hydroxyl group.
[0085] It should be noted that the graphic shielding layer is an organic material. After hydroxyl groups are formed on the top of the graphic definition layer 102, the graphic definition layer 102 and the alloy mask material layer 101 are less damaged during the process of removing the graphic shielding layer.
[0086] In the process of treating the hydroxyl groups with the gas containing the hydrophobic functional group, the process gas containing the hydrophobic functional group contacts the hydroxyl groups on the top of the pattern definition layer 102 .
[0087] The process gas containing hydrophobic functional groups contacts the hydroxyl groups on the top of the pattern definition layer 102. The hydrophobic functional groups replace the hydroxyl groups in the pattern definition layer 102, so that the top of the pattern definition layer 102 is modified, so that the top of the pattern definition layer 102 does not contain adsorption sites for the precursor of the alloy layer, so that in the subsequent step of forming an alloy layer on the alloy mask material layer exposed by the opening, the precursor of the alloy layer will not be formed on the top of the pattern definition layer 102.
[0088] In this embodiment, the process gas containing the hydrophobic functional group includes silicon-containing gas.
[0089] Specifically, the silicon-containing gas includes one or more of alkylsilane, alkoxysilane, alkylalkoxysilane, alkylsiloxane, alkoxysiloxane, alkylalkoxysiloxane, arylsilane, acylsilane, arylsiloxane, acylsiloxane and silazane.
[0090] The step of selectively forming an alloy layer 107 on the alloy mask material layer 101 exposed by the opening 104 includes: selectively forming a precursor of an alloy layer on the alloy mask material layer 101 exposed by the opening 104 , and performing an oxidation-reduction reaction on the precursor of the alloy layer to form the alloy layer 107 .
[0091] It should be noted that, in the process of selectively forming a precursor of the alloy layer on the alloy mask material layer 101 exposed by the opening 104, the precursor of the alloy layer is indiscriminately deposited in the graphic definition layer 102 and in the opening 104 between the graphic definition layer 102. However, because the top of the graphic definition layer 102 contains a hydrophobic functional group, the adsorption force between the precursor of the alloy layer and the top of the graphic definition layer 102 is poor, so that the precursor of the alloy layer is finally formed only in the opening 104.
[0092] In this embodiment, a metal organic chemical vapor deposition (MOCVD) process is used to form the precursor of the alloy layer. The metal organic chemical vapor deposition process is conducive to improving the thickness uniformity of the precursor of the alloy layer, and has good gap filling performance and good step coverage. In other embodiments, an atomic layer deposition process can also be used to form the precursor of the alloy layer.
[0093] Usually, the precursor of the alloy layer contains impurity elements such as C, N, O and S. By performing an oxidation-reduction reaction on the precursor of the alloy layer, it is easy to fully remove the impurity elements in the precursor layer of the alloy layer and improve the purity of the alloy layer 107.
[0094] The method for forming the semiconductor structure further includes: after the gas containing the hydrophobic functional group contacts the hydroxyl group on the top of the pattern definition layer 102, removing the pattern shielding layer.
[0095] It should be noted that, in the process of forming the precursor of the alloy layer on the alloy mask material layer 101 exposed by the opening 104 by using a selective deposition process, the flow rate of the reaction gas should not be too large or too small. If the flow rate of the reaction gas is too large, the formation rate of the precursor of the alloy layer is too fast, and the precursor of the alloy layer is easy to form on the top surface of the pattern definition layer 102. After the precursor of the alloy layer is subjected to oxidation-reduction treatment, after the alloy layer 107 is formed, in the process of removing the pattern definition layer 102, the alloy layer 107 on the top surface of the pattern definition layer 102 is easy to reduce the removal efficiency of the pattern definition layer 102, which is not conducive to improving the formation efficiency of the semiconductor structure; and if the flow rate of the reaction gas is too large, the process controllability and reaction rate uniformity of the precursor of the alloy layer are difficult to control. If the flow rate of the reaction gas is too small, it is easy to cause the formation rate of the precursor of the alloy layer to be too slow, which is correspondingly not conducive to improving the formation rate of the alloy layer 107. In this embodiment, in the step of forming the precursor of the alloy layer by a selective deposition process, the flow rate of the reaction gas is 10 sccm to 1000 sccm.
[0096] It should be noted that, in the process of forming the precursor of the alloy layer on the alloy mask material layer 101 exposed by the opening 104 by using the selective deposition process, the chamber pressure should not be too large or too small. If the chamber pressure is too large, the alloy layer 107 is easily formed on the top surface of the pattern definition layer 102. After the alloy layer 107 is formed, the alloy layer 107 on the top surface of the pattern definition layer 102 is easily reduced in the process of removing the pattern definition layer 102 by oxidation-reduction treatment, which is not conducive to improving the formation efficiency of the semiconductor structure; and if the chamber pressure is too large, the process controllability and reaction rate uniformity of the precursor of the alloy layer are difficult to control. If the chamber pressure is too small, the formation rate of the precursor of the alloy layer is too slow, which is correspondingly not conducive to improving the formation efficiency of the alloy layer 107. In this embodiment, the chamber pressure is 1mTorr to 100mTorr in the process of forming the alloy layer 107 by using the selective deposition process.
[0097] In other embodiments, the step of forming an alloy layer in the opening includes: forming an alloy material layer covering the opening and the graphic definition layer; removing the alloy material layer on the graphic definition layer; after removing the alloy material layer on the graphic definition layer, etching back a portion of the thickness of the alloy material layer in the opening, and the remaining alloy material layer located in the opening serves as the alloy layer.
[0098] Accordingly, the alloy material layer is formed by an atomic layer deposition (ALD) process. The atomic layer deposition process includes performing multiple atomic layer deposition cycles, which is beneficial to improving the thickness uniformity of the alloy material layer. In addition, the atomic layer deposition process has good gap filling performance and step coverage, and voids are not easy to appear in the alloy material layer. In other embodiments, the alloy material layer can also be formed by a chemical vapor deposition process.
[0099] refer to Fig.18 After the alloy layer 107 is formed, the pattern definition layer 102 is removed.
[0100] The pattern definition layer 102 is removed to prepare for the subsequent etching of the alloy mask material layer 101 using the alloy layer 107 as a mask.
[0101] In this embodiment, a wet etching process is used to remove the pattern definition layer 102. The wet etching process has a high etching rate, simple operation and low process cost.
[0102] In this embodiment, the material of the pattern definition layer 102 is amorphous silicon, and the corresponding etching solution for removing the amorphous silicon includes a tetramethylammonium hydroxide (TMAH) solution.
[0103] refer to Fig.19 and Fig. 20 , using the alloy layer 107 as a mask, the alloy mask material layer 101 is etched to form an alloy mask layer 108 .
[0104] In a subsequent process, the substrate 100 is etched using the alloy layer 107 and the alloy mask layer 108 as masks to form a plurality of spaced trenches and substrate spacers between the trenches in the substrate 100 .
[0105] In this embodiment, the alloy mask material layer 101 is etched by dry etching process with the alloy layer 107 as a mask to form an alloy mask layer 108. The dry etching process has anisotropic etching characteristics and good etching profile controllability. Moreover, by changing the etching gas, multiple film layers can be etched in the same etching equipment, simplifying the process steps.
[0106] It should be noted that after removing the graphic definition layer 102, before etching the alloy mask material layer 101 using the alloy layer 107 as a mask, a substrate mask layer 109 is formed on the alloy layer 107 and the alloy mask material layer 101, and the substrate mask layer 109 has a mask opening 110, and the extension direction of the mask opening 110 intersects with the extension direction of the alloy layer 107.
[0107] The extension direction of the mask opening 110 intersects with the extension direction of the alloy layer 107 . Accordingly, during the process of etching the alloy mask material layer 101 , the substrate mask layer 109 and the alloy layer 107 together serve as masks for etching the alloy mask material layer 101 .
[0108] Specifically, the extension direction of the mask opening 110 is perpendicular to the extension direction of the alloy layer 107. The extension direction of the groove formed by subsequently etching the substrate 100 using the substrate mask layer 109 and the alloy layer 107 as masks has high uniformity at both ends, which is beneficial to preventing the metal wires subsequently formed in the groove from being easily bridged together.
[0109] In this embodiment, the material of the substrate mask layer 109 includes an organic material layer 1091 , an anti-reflective coating 1092 on the organic material layer 1091 , and a photoresist layer 1093 on the anti-reflective coating 1092 . The mask opening 110 is located in the photoresist layer 1093 .
[0110] Continue to refer Fig. 20In the step of etching the alloy mask material layer 101 using the alloy layer 107 as a mask to form the alloy mask layer 108 , the alloy mask material layer 101 is etched using the substrate mask layer 109 and the alloy layer 107 as masks to form the alloy mask layer 108 .
[0111] It should be noted that the etching resistance of the substrate mask layer 109 is lower than that of the alloy layer 107. After etching the alloy mask material layer 101 to form the alloy mask layer 108, the alloy layer 107 still has a relatively high thickness, which facilitates the subsequent etching of the substrate 100 using the alloy layer 107 and the alloy mask layer 108 as masks to form grooves in the substrate 100.
[0112] The method for forming a semiconductor structure further includes: after forming the alloy mask layer 108 , removing the substrate mask layer 109 .
[0113] The substrate mask layer 109 does not contain metal ions, so the substrate mask layer 109 is removed to avoid the polymer impurities with metal ions and polymer impurities without metal ions formed simultaneously in the subsequent etching process to form grooves, which are distributed disorderly and unevenly on the surface of the substrate 100. The obstructions caused in the process of etching to form grooves are inconsistent, resulting in poor morphological uniformity of the subsequently formed grooves. Accordingly, the quality of the metal connections subsequently formed in the grooves 13 is poor, resulting in poor electrical performance of the semiconductor structure.
[0114] In this embodiment, an ashing process is used to remove the substrate mask layer 109 .
[0115] refer to Fig.21 After removing the substrate mask layer 109 , the substrate 100 is etched using the alloy layer 107 and the alloy mask layer 108 as masks to form a plurality of spaced trenches 111 and substrate spacers 112 located between the trenches 111 .
[0116] In this embodiment, the materials of the alloy layer 107 and the alloy mask layer 108 both include metal ions. In the process of etching the substrate 100 using the alloy layer 107 and the alloy mask layer 108 as masks to form the groove 111, the polymer impurities generated all carry metal ions. In the process of etching to form the groove 111, the obstruction caused by the polymer impurities carrying metal ions is relatively consistent, so that the morphology of the groove 111 is more uniform. Correspondingly, the quality of the metal connection subsequently formed in the groove 111 is better, and the metal connections in adjacent grooves 111 do not contact each other, which is beneficial to improving the electrical properties of the semiconductor structure.
[0117] In this embodiment, the substrate 100 is etched by dry etching process using the alloy layer 107 and the alloy mask layer 108 as masks to form a plurality of spaced grooves 111 and substrate spacers 112 located between the grooves 111. The dry etching process has anisotropic etching characteristics and good etching profile controllability, which is conducive to making the morphology of the grooves 111 meet process requirements. In addition, the dry etching process is conducive to accurately controlling the formation depth of the grooves 111.
[0118] It should be noted that the trench 111 is formed in the dielectric layer.
[0119] Accordingly, the subsequently formed metal wiring is located in the groove 111, and the material of the dielectric layer is a low-k dielectric material, which is beneficial to reducing the parasitic capacitance between the metal wirings, and further beneficial to reducing the subsequent RC delay.
[0120] Accordingly, an embodiment of the present invention further provides a semiconductor structure. Fig.17 , showing a schematic structural diagram of an embodiment of a semiconductor structure of the present invention.
[0121] The semiconductor structure includes: providing a base, the base including a substrate 100 and an alloy mask material layer 101 located on the substrate 100; a graphic definition layer 102 located on the alloy mask material layer 101, the graphic definition layer 102 having one or more openings 104 exposing the alloy mask material layer 101; and an alloy layer 107 located in the opening 104.
[0122] Subsequently, the alloy mask material layer 101 is etched using the alloy layer 107 as a mask to form an alloy mask layer, and the substrate 100 is etched using the alloy layer 107 and the alloy mask layer as masks to form a plurality of separated grooves in the substrate 100. In the embodiment of the present invention, the materials of the alloy layer 107 and the alloy mask layer are both alloy materials, and in the process of etching to form the grooves, the polymer impurities generated are all polymer impurities with metal ions, and the obstacles caused by the polymer impurities with metal ions in the etching process are relatively consistent, so that the morphology uniformity of the grooves is better, and accordingly, the quality of the metal wiring subsequently formed in the grooves is better, which is conducive to improving the electrical performance of the semiconductor structure.
[0123] In this embodiment, the material of the substrate 100 includes a dielectric layer. Subsequently, a trench is formed in the dielectric layer.
[0124] The material of the dielectric layer is a low-k dielectric material, which is beneficial to reducing the parasitic capacitance between the subsequently formed metal wirings, and further beneficial to reducing the subsequent RC delay.
[0125] Specifically, the material of the dielectric layer includes SiCOH.
[0126] It should be noted that the substrate 100 also includes a transistor, which is usually formed at the bottom of the dielectric layer. The transistor includes a gate structure and source and drain doped regions located on both sides of the gate structure. Contact hole plugs (not shown in the figure) in contact with the source and drain doped regions are also formed in the substrate.
[0127] Subsequently, the alloy mask material layer 101 is etched using the alloy layer 107 as a mask to form an alloy mask layer. After the alloy mask layer is formed, the substrate is etched using the alloy mask layer and the alloy layer as masks to form a groove in the substrate.
[0128] In this embodiment, the alloy mask material layer 101 has a high etching resistance. In the subsequent etching process of the substrate 100 , the materials of the substrate 100 and the alloy mask material layer 101 have a large etching selectivity ratio.
[0129] In this embodiment, the material of the alloy mask material layer 101 includes one or more of TiN, TiO 2 , HfN, ZrO 2 and Al 2 O 3 .
[0130] In this embodiment, the material of the pattern definition layer 102 is amorphous silicon. Amorphous silicon is a commonly used material in the process, and the formation process is simple, which is conducive to reducing the process cost of the semiconductor structure. In other embodiments, the material of the pattern definition layer can also be silicon oxide.
[0131] It should be noted that the graphic definition layer 102 should not be too thick or too thin. The alloy layer 107 is formed in the opening 104 by a selective deposition process. If the graphic definition layer 102 is too thick, the corresponding aspect ratio of the opening 104 is too large, and voids are easily present in the alloy layer 107 formed in the opening 104 by the selective deposition process, resulting in poor formation quality of the alloy layer 107; if the graphic definition layer 102 is too thin, the depth of the opening 104 subsequently formed in the graphic definition layer 102 is too small, and the depth of the opening 104 will limit the formation height of the alloy layer 107. In the subsequent process of etching the alloy mask material layer 101 with the alloy layer 107 as a mask to form the alloy mask layer, the alloy layer 107 cannot play a good role as a mask. In this embodiment, in the step of providing the graphic definition layer 102, the thickness of the graphic definition layer 102 is 30 nanometers to 50 nanometers.
[0132] The semiconductor structure further includes a hydrophobic functional group located on the top of the pattern definition layer 102 .
[0133] The hydrophobic functional group modifies the top of the graphic definition layer 102 so that the top of the graphic definition layer 102 does not contain adsorption sites for the precursor of the alloy layer, thereby preventing the alloy layer 107 from being easily formed on the top of the graphic definition layer 102 during the process of forming the alloy layer 107 using a selective deposition process.
[0134] In this embodiment, the alloy layer 107 is in direct contact with the alloy mask material layer 101. The surface of the alloy mask material layer 101 does not contain hydrophobic functional groups, so the alloy layer 107 formed by the selective deposition process is in direct contact with the alloy mask material layer 101.
[0135] In this embodiment, the material of the alloy layer 107 includes one or more of TiN, TiO 2 , HfN, ZrO 2 and Al 2 O 3 .
[0136] It should be noted that the alloy layer 107 should not be too high or too low. If the alloy layer 107 is too high, after the alloy mask material layer 101 is etched using the alloy layer 107 as a mask to form an alloy mask layer, the height of the alloy layer 107 is still too high, and it is easy to spend too much process time to remove the alloy layer 107. If the alloy layer 107 is too low, in the process of etching the alloy mask material layer 101 using the alloy layer 107 as a mask to form an alloy mask layer, the alloy layer 107 is not easy to play the role of an etching mask. In this embodiment, in the step of forming the alloy layer 107 in the opening 104, the thickness of the alloy layer is one-third to two-thirds of the depth of the opening 104. Specifically, the height of the alloy layer 107 is 10 nanometers to 30 nanometers.
[0137] The semiconductor structure can be formed by the formation method described in the above embodiment, or by other formation methods. For the specific description of the semiconductor structure described in this embodiment, reference can be made to the corresponding description in the above embodiment, and this embodiment will not be repeated here.
[0138] Although the embodiments of the present invention are disclosed above, the embodiments of the present invention are not limited thereto. Any person skilled in the art may make various changes and modifications without departing from the spirit and scope of the embodiments of the present invention. Therefore, the protection scope of the embodiments of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: Providing a substrate, the substrate comprising a substrate and an alloy mask material layer located on the substrate; forming a pattern definition layer on the alloy mask material layer, wherein the material of the pattern definition layer includes amorphous silicon or silicon oxide; forming a plurality of discrete openings in the pattern definition layer, the openings exposing the alloy mask material layer; The step of forming openings in the pattern definition layer to expose the alloy mask material layer comprises: sequentially forming a plurality of discrete doping layers in the pattern definition layer through multiple doping film forming steps, so that the etching resistance of the doping layers is less than that of the pattern definition layer; removing the doping layers, and forming a plurality of openings in the pattern definition layer to expose the alloy mask material layer; Forming an alloy layer on the alloy mask material layer exposed by the opening by a selective deposition process; After forming the alloy layer, removing the pattern definition layer; The alloy mask material layer is etched using the alloy layer as a mask to form an alloy mask layer; the substrate is etched using the alloy layer and the alloy mask layer as masks to form a plurality of spaced grooves and substrate spacers located between the grooves in the substrate.
2. The method for forming a semiconductor structure according to claim 1, wherein: The steps of the selective deposition process include: forming hydroxyl groups on the top of the graphic definition layer; after the hydroxyl groups are formed, treating the hydroxyl groups with a gas containing a hydrophobic functional group; after treating the hydroxyl groups with a gas containing a hydrophobic functional group, selectively forming an alloy layer on the alloy mask material layer exposed by the opening.
3. The method for forming a semiconductor structure according to claim 2, wherein: The formation process of the hydroxyl group includes: reacting the top of the pattern definition layer with water to form the hydroxyl group.
4. The method for forming a semiconductor structure according to claim 2, wherein: The process gas containing hydrophobic functional groups includes silicon-containing gas; The silicon-containing gas includes one or more of alkylsilane, alkoxysilane, alkylalkoxysilane, alkylsiloxane, alkoxysiloxane, alkylalkoxysiloxane, arylsilane, acylsilane, arylsiloxane, acylsiloxane and silazane.
5. The method for forming a semiconductor structure according to claim 1, wherein: The step of selectively forming an alloy layer on the alloy mask material layer exposed by the opening includes: selectively forming a precursor of the alloy layer on the alloy mask material layer exposed by the opening; and performing an oxidation-reduction reaction on the precursor of the alloy layer to form the alloy layer.
6. The method for forming a semiconductor structure according to claim 1, wherein: The alloy mask material layer is etched using the alloy layer as a mask to form the alloy mask layer, wherein an etching selectivity ratio between the alloy mask material layer and the alloy layer is greater than 3.
7. The method for forming a semiconductor structure according to claim 1 or 6, wherein: The material of the alloy layer includes one or more of TiN, TiO2, HfN, ZrO2 and Al2O3.
8. The method for forming a semiconductor structure according to claim 1, wherein: In the step of forming an alloy layer in the opening, the thickness of the alloy layer is one third to two thirds of the depth of the opening.
9. The method for forming a semiconductor structure according to claim 1, wherein: The step of forming an alloy layer in the opening includes: forming an alloy material layer covering the opening and the pattern definition layer; removing the alloy material layer on the pattern definition layer; After removing the alloy material layer on the pattern definition layer, a portion of the alloy material layer in the opening is etched back, and the remaining alloy material layer in the opening serves as the alloy layer.
10. The method for forming a semiconductor structure according to claim 9, wherein: The alloy material layer is formed by an atomic layer deposition process or a metal organic chemical vapor deposition process.
11. The method for forming a semiconductor structure according to claim 1, wherein: The doping film forming step includes: forming a mask layer on the graphic definition layer; forming a groove in the mask layer to expose the graphic definition layer; doping ions in the graphic definition layer exposed by the groove to form a doping layer; after forming the doping layer, removing the mask layer.
12. The method for forming a semiconductor structure according to claim 11, wherein: In the step of doping ions in the pattern definition layer exposed by the groove, the doped ions include phosphorus ions.
13. The method for forming a semiconductor structure according to claim 1, wherein: After removing the pattern definition layer, before etching the alloy mask material layer using the alloy layer as a mask, forming a substrate mask layer on the alloy layer and the alloy mask material layer, wherein the substrate mask layer has a mask opening, and an extension direction of the mask opening intersects with an extension direction of the alloy layer; In the step of etching the alloy mask material layer using the alloy layer as a mask to form the alloy mask layer, the alloy mask material layer is etched using the substrate mask layer and the alloy layer as masks to form the alloy mask layer; After forming the alloy mask layer, removing the substrate mask layer; After removing the substrate mask layer, the substrate is etched using the alloy layer and the alloy mask layer as masks to form a plurality of spaced grooves and substrate spacers located between the grooves.