A deep cryogenic temperature sensor based on multi-layer quantum well structure and its preparation method

By using a deep cryogenic temperature sensor with a multi-layer quantum well structure, the limitations of existing cryogenic thermometers in achieving high-precision measurement in different cryogenic ranges are overcome, realizing high-sensitivity and high-precision temperature measurement and adapting to the temperature measurement needs of different cryogenic environments.

CN113739949BInactive Publication Date: 2024-11-08LASER FUSION RES CENT CHINA ACAD OF ENG PHYSICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111039736.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-09-06
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing low-temperature thermometers, such as platinum resistance thermometers, germanium resistance thermometers, and silicon diode thermometers, have limitations in high-precision measurement across different low-temperature ranges. They cannot be flexibly adapted, and their large sensor size and slow response speed make it difficult to meet the requirements of high-precision measurement.

Method used

The cryogenic temperature sensor employing a multilayer quantum well structure includes a heat transfer layer, a substrate layer, a buffer layer, a temperature-sensitive layer, and a contact layer. The epitaxial wafer is prepared using solid-source molecular beam epitaxy, and an alloyed ohmic contact layer and an oxygen-free copper heat sink are used to achieve precise control of the electron transport process, enabling high-precision temperature measurement in different cryogenic ranges.

Benefits of technology

It significantly improves the relative sensitivity and high-precision temperature measurement capability of the sensor in various low-temperature ranges, enabling flexible high-precision measurement in different low-temperature ranges, and improving the structural stability and response speed of the sensor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113739949B_ABST
    Figure CN113739949B_ABST
Patent Text Reader

Abstract

The present invention discloses a deep cryogenic temperature sensor based on a multi-layer quantum well structure and a preparation method thereof, comprising: a heat transfer layer, a substrate layer, a buffer layer with a lower electrode, a temperature sensitive layer composed of a plurality of quantum well periods, and a contact layer with an upper electrode, which are arranged in sequence from bottom to top; each of the quantum well periods is composed of multiple layers of Al2O3 with different thicknesses. 0.15 Ga 0.85 The present invention provides a multi-layer quantum well structure based on the GaAs material system, which can accurately control the transport process of electrons in the multi-layer quantum well structure in a deep low temperature environment, thereby significantly improving the relative sensitivity of the device in various low temperature ranges; at the same time, according to the needs of high-precision temperature measurement in different low temperature ranges, the multi-layer structure of the quantum well can be flexibly grown and cut to achieve high-precision temperature measurement in different low temperature ranges.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor processing for deep cryogenic detection, and in particular to a deep cryogenic temperature sensor based on a multi-layer quantum well structure and a preparation method thereof. Background Art

[0002] The application of cryogenic technology is very extensive, from people's daily life to industrial and agricultural production processes, from medical technology to scientific research, all are inseparable from cryogenic technology. The various physical and chemical characteristics of materials in low temperature environments are very important for superconductivity research, aerospace, biomedicine, and new energy development. In the research and development of cryogenic technology applications, low temperature acquisition and low temperature measurement are two important directions in this field. In low temperature environments, such as liquid oxygen (90.2K), liquid nitrogen (77K), liquid hydrogen (20.3K), and liquid helium (0.8K), temperature is the most basic thermodynamic quantity, and the precise measurement of temperature is an important indicator for analyzing system performance and reliability.

[0003] At present, there are many types of low-temperature thermometers, mainly including diode thermometers and resistance thermometers, such as platinum resistance thermometers, germanium resistance thermometers, silicon diode thermometers, etc. Platinum metal is easy to process and has stable physical and chemical properties. It is a standard thermometer in the temperature range of 13.8-429.7K (International ITS-90 temperature scale). However, platinum resistance thermometers generally use spiral platinum wires as sensitive elements, which are stress-free packaging technology. Therefore, the sensor size is large and the response speed is slow. As a secondary standard temperature measurement, the germanium resistance thermometer has good long-term stability. However, this thermometer also requires stress-free packaging technology, has a magnetoresistance effect, and cannot be used in a magnetic field environment. Silicon diode thermometers have good interchangeability, but the measurement accuracy is limited and is not suitable for high-precision measurement. In addition, the above temperature sensors are limited by the material type and cannot flexibly adapt to the needs of high-precision temperature measurement in different low-temperature temperature ranges. At the same time, the temperature measurement accuracy is limited by the low-temperature characteristics of the material type itself, and it is difficult to further improve. Summary of the invention

[0004] An object of the present invention is to solve at least the above problems and / or defects and to provide at least the advantages described below. In order to achieve these objects and other advantages according to the present invention, a deep cryogenic temperature sensor based on a multi-layer quantum well structure and a preparation method thereof are provided, comprising: a heat transfer layer, a substrate layer, a buffer layer with a lower electrode, a temperature sensitive layer composed of a plurality of quantum well periods, and a contact layer with an upper electrode, each of which is composed of multiple layers of Al2O3 with different thicknesses. 0.15 Ga 0.85 As and GaAs are composed alternately.

[0005] Preferably, the heat transfer layer comprises a Ti / Au thermal contact layer with a thickness of 50nm to 70nm; the upper end of the Ti / Au thermal contact layer is connected to the substrate layer, and the lower end is provided with an oxygen-free copper heat sink with a thickness of 2mm to 5mm and a purity greater than 99.9%.

[0006] Preferably, the substrate layer is a semi-insulating GaAs substrate with a thickness of 180 μm to 200 μm.

[0007] Preferably, the buffer layer is specifically a layer with a thickness of 700 nm, a doping element of Si, and a doping concentration of 2.5×10 18 cm -3 of heavily doped layers.

[0008] Preferably, each of the quantum well periods is composed of eight layers of Al with different thicknesses. 0.15 Ga 0.85 As and GaAs are composed alternately.

[0009] Preferably, the contact layer is specifically a layer with a thickness of 70 nm, a doping element of Si, and a doping concentration of 5.0×10 18 cm -3 of heavily doped layers.

[0010] Preferably, the lower electrode and the upper electrode are both AU electrodes with a thickness of 100 nm, and alloyed ohmic contact layers 7 are provided between the buffer layer and the contact layer respectively.

[0011] Preferably, in step 1, the epitaxial wafer is prepared by a solid source molecular beam epitaxy method;

[0012] Step S11: grow a 700nm thick Si-doped layer on the substrate layer with a doping concentration of 2.5×10 18 cm -3 A heavily doped layer as a buffer layer;

[0013] Step S12: growing a multi-layer quantum well structure consisting of 50 to 80 quantum well periods on the buffer layer as a temperature sensitive layer; each quantum well period consists of eight layers of Al with different thicknesses, the minimum thickness being 1.7 nm and the maximum thickness being 17.0 nm. 0.15 Ga 0.85 As and GaAs are grown alternately;

[0014] Step S13: grow a 70nm thick layer on the temperature sensitive layer, with Si as the doping element and a doping concentration of 5.0×10 18 cm -3 The heavily doped layer is used as a contact layer to complete the preparation of the epitaxial wafer;

[0015] Step 2: preparing an alloyed ohmic contact layer by electron beam deposition;

[0016] Step S21, taking an epitaxial wafer of size 5 mm×10 mm, using acetone and ethanol to clean the surface of the epitaxial wafer in sequence, then rinsing it with deionized water, and finally drying it with high-purity N2;

[0017] Step S22, etching a stripe structure with a designed ridge width of 800 μm on the epitaxial wafer, and etching to a depth reaching the buffer layer of the epitaxial wafer;

[0018] Step S23, using an electron beam to sequentially deposit Ge, Au, Ni, Au and other multi-layer metal films between the lower electrode and the buffer layer and between the upper electrode and the contact layer, and then rapidly annealing and alloying, thereby achieving ohmic contact between the lower electrode and the buffer layer and between the upper electrode and the contact layer; and completing the preparation of the alloyed ohmic contact layer;

[0019] Step 3: Preparation and sintering of oxygen-free copper heat sink;

[0020] Step S31, performing thermal evaporation plating of indium on the oxygen-free copper base material, with a coating thickness of 15 μm; completing the preparation of the oxygen-free copper heat sink;

[0021] Step S32, installing an oxygen-free copper heat sink on a fixture, placing the epitaxial wafer on the oxygen-free copper heat sink, and then sintering in a vacuum sintering furnace;

[0022] Step 4: Use the gold wire ball bonding method to lead out the lower electrode 41 and the upper electrode 61.

[0023] The present invention has at least the following beneficial effects:

[0024] The present invention provides a multi-layer quantum well structure based on a GaAs material system, which can accurately control the transport process of electrons in the multi-layer quantum well structure in a deep cryogenic environment, thereby significantly improving the relative sensitivity of the device in various low-temperature ranges; at the same time, the multi-layer structure of the quantum well can be flexibly grown and cut according to the needs of high-precision temperature measurement in different low-temperature ranges, thereby realizing high-precision temperature measurement in different low-temperature ranges;

[0025] Other advantages, objectives and features of the present invention will be embodied in part through the following description, and in part will be understood by those skilled in the art through study and practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a cross-sectional view of the overall structure of the present invention;

[0027] Figure 2 A structural cross-sectional view of each quantum well period of the present invention;

[0028] Figure 3 It is a functional change relationship diagram of resistance and temperature under the test environment of the present invention;

[0029] Figure 4 A diagram showing the relationship between the resistance sensitivity function under the test environment of the present invention;

[0030] Figure 5 The quantum well energy level calculation flow chart of the present invention; DETAILED DESCRIPTION

[0031] The present invention is further described in detail below in conjunction with the accompanying drawings so that those skilled in the art can implement the invention with reference to the description.

[0032] It should be understood that the terms such as “having”, “including” and “comprising” used herein do not exclude the existence or addition of one or more other elements or combinations thereof.

[0033] It should be noted that in the description of the present invention, the orientation or positional relationship indicated by the terms is based on the orientation or positional relationship shown in the drawings, and is only for the convenience of describing the present invention and simplifying the description. It does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0034] In the description of the present invention, unless otherwise clearly stipulated and limited, the terms "installed", "provided with", "mounted / connected", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection. It can be a mechanical connection or an electrical connection. It can be a direct connection or an indirect connection through an intermediate medium. It can be the internal connection of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0035] In addition, in the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature.

[0036] Figure 1-5 An implementation form of the present invention is shown, including:

[0037] The heat transfer layer 1, the substrate layer 2, the buffer layer 4 with the lower electrode 41, the temperature sensitive layer 5 composed of a plurality of quantum well periods 50, and the contact layer 6 with the upper electrode 61 are arranged in sequence from bottom to top; each of the quantum well periods 50 is composed of multiple layers of Al with different thicknesses. 0.15 Ga 0.85 As and GaAs are composed alternately.

[0038] Working principle:

[0039] When using the present invention, the device is placed in a deep low temperature detection environment and an electric field strength is applied. When the heat transfer layer 1 contacts the measured object, the temperature sensitive layer 5 will quickly reach temperature equilibrium with the measured object. At this time, in one of the quantum well periods 50 of the temperature sensitive layer 5, the lower energy level 52 of the lasing forms a resonance with the lower energy level 54 of the e-LO resonance transition. Although it is higher than the upper energy level 53 of the e-LO resonance transition, it is close to the energy of the upper energy level 53 of the e-LO resonance transition, forming a microband, thereby forming a particle number inversion; the injected state 55 and the next The lasing upper energy level 51 of each quantum well period 50 produces a resonance effect, which makes the injection efficiency higher; under the combined action of these two effects, the electrons can become mainly tunneling current when passing through the structure, and the resistance of the quantum well period 50 in the temperature-sensitive layer 5 will increase rapidly with temperature changes; in order to increase the stability of the temperature-sensitive layer 5 and achieve the overall resistance value that can be measured by conventional technology, we adopt the method of repeatedly growing multiple quantum well periods 50, so that the resistance value and sensitivity of the entire temperature-sensitive layer 5 can meet actual needs in a deep low temperature test environment.

[0040] In this technical solution, each quantum well period 50 in the temperature sensitive region 5 is composed of multiple layers of Al with different thicknesses. 0.15 Ga 0.85As and GaAs are alternately composed to form a double phonon resonance four-well structure. In this special structure, the quantum confinement effect forms sub-energy levels in the quantum well, which can effectively control the electron transport process and realize that the electron has a high probability of passing through the multi-layer quantum well barrier structure through the resonant tunneling effect at deep low temperature; specifically, in each quantum well period 50, the first thin quantum well effectively promotes the effective resonant coupling between the previous electron injection ground state and the high-energy excited state 56, ensuring the injection efficiency of the high-energy excited state 56 while reducing the non-resonant transfer of the electron injection region to the lasing lower energy level 52; a quantum well behind the lasing lower energy level 52 forms two sub-bands with a spacing close to the LO phonon energy below the low energy state of the electron transition. This double phonon resonance design greatly improves the extraction speed of low-energy state electrons while maintaining almost the same electron injection efficiency and electron transition matrix elements between sub-bands, and the particle number inversion is significantly improved. In order to further improve the accuracy and repeatability of the electron transport process and meet the reasonable range of device resistance required in actual testing, the double phonon resonance four-well structure is repeated for multiple cycles. By effectively controlling the electron transport process as described above, when the test temperature is lower than the preset temperature, the resistance of the temperature-sensitive layer will show a quantitative relationship of rapid linear increase as the temperature drops, and the corresponding relative sensitivity also meets actual needs.

[0041] In the above technical solution, the heat transfer layer 1 includes a Ti / Au thermal contact layer 11 with a thickness of 50nm to 70nm; the upper end of the Ti / Au thermal contact layer 11 is connected to the substrate layer 2, and the lower end is provided with an oxygen-free copper heat sink 12 with a thickness of 2mm to 5mm and a purity greater than 99.9%. The advantage of this arrangement is that the oxygen-free copper heat sink 12 has a very high thermal conductivity and a thin thickness at deep low temperatures, and the temperature-sensitive layer 5 can quickly reach temperature equilibrium with the measured object while ensuring the mechanical installation strength; the Ti / Au thermal contact layer 11 can achieve a close connection between the substrate layer 2 and the oxygen-free copper heat sink 12, thereby improving the support and stability of the overall structure.

[0042] In the above technical solution, the substrate layer 2 is specifically a semi-insulating GaAs substrate with a thickness of 180 μm to 200 μm. The advantage of this arrangement is that the GaAs substrate has high electron mobility and a large bandgap, and is suitable as a substrate for the growth of the material system of the device.

[0043] In the above technical solution, the buffer layer 4 is specifically a layer with a thickness of 700 nm, a doping element of Si, and a doping concentration of 2.5×10 18 cm -3The advantage of this arrangement is that heavily doping Si in the buffer layer 4 can increase the critical capacity of generating dislocations in the material, reduce the dislocation density in the material, and improve the integrity of the crystal according to the hardening effect of impurities; at the same time, it can increase the carrier concentration in the buffer layer 4 and improve the conductivity of the buffer layer 4.

[0044] In the above technical solution, each of the quantum well periods 50 is composed of eight layers of Al with different thicknesses. 0.15 Ga 0.85 As and GaAs are alternately composed. The advantage of this arrangement is that it can maintain almost the same electron injection efficiency and inter-subband electron transition matrix elements, while greatly improving the extraction speed of low-energy state electrons and significantly improving the population inversion.

[0045] In the above technical solution, the contact layer 6 is specifically a layer with a thickness of 70 nm, a doping element of Si, and a doping concentration of 5.0×10 18 cm -3 The advantage of this arrangement is that heavily doped Si in the contact layer can provide a larger tunnel current, can better adapt to the upper electrode to make ohmic contact, and reduce the overall volume resistivity.

[0046] In the above technical solution, the lower electrode 41 and the upper electrode 61 are both AU electrodes with a thickness of 100 nm, and an alloyed ohmic contact layer 7 is respectively provided between the buffer layer 4 and the contact layer 6. The advantage of such a setting is that the use of the alloyed ohmic contact layer 7 and the AU electrode can reduce the contact resistance, be more conducive to the electron injection into the temperature sensitive layer 5, and improve the overall detection performance of the device.

[0047] In the above technical solution,

[0048] Step 1: preparing epitaxial wafers by solid source molecular beam epitaxy method;

[0049] Step S11: grow a 700 nm thick Si-doped layer on the substrate layer 2 with a doping concentration of 2.5×10 18 cm -3 A heavily doped layer as a buffer layer 4;

[0050] Step S12: growing a multi-layer quantum well structure consisting of 50 to 80 quantum well periods 50 on the buffer layer 4 as the temperature sensitive layer 5; each quantum well period 50 consists of eight layers of Al with different thicknesses, the minimum thickness being 1.7 nm and the maximum thickness being 17.0 nm. 0.15 Ga 0.85 As and GaAs are grown alternately;

[0051] Step S13: grow a 70nm thick layer on the temperature sensitive layer 5, with Si as the doping element and a doping concentration of 5.0×10 18 cm -3 The heavily doped layer is used as the contact layer 6; the preparation of the epitaxial wafer is completed;

[0052] In step one, the solid source molecular beam epitaxy method is used to prepare the epitaxial wafer, which makes the epitaxial growth temperature lower, reduces the epitaxial self-doping and external diffusion, and is beneficial to improving the purity and integrity of the epitaxial wafer. At the same time, the surface morphology is good, the finished product area is large, and it is uniform and stable.

[0053] Step 2: preparing an alloyed ohmic contact layer by electron beam deposition;

[0054] Step S21, taking an epitaxial wafer of size 5 mm×10 mm, using acetone and ethanol to clean the surface of the epitaxial wafer in sequence, then rinsing it with deionized water, and finally drying it with high-purity N2;

[0055] Step S22, etching a stripe structure with a designed ridge width of 800 μm on the epitaxial wafer, and etching to a depth reaching the buffer layer 4 of the epitaxial wafer;

[0056] Step S23, using an electron beam to sequentially deposit Ge, Au, Ni, Au and other multi-layer metal films between the lower electrode 41 and the buffer layer 4, and between the upper electrode 61 and the contact layer 6, and then rapidly annealing and alloying, thereby achieving ohmic contact between the lower electrode 41 and the buffer layer 4, and between the upper electrode 61 and the contact layer 6; and completing the preparation of the alloyed ohmic contact layer 7;

[0057] In step two, the cleanliness of the epitaxial wafer can be significantly improved, the etching processing quality can be improved, the mobility can be guaranteed, the contact resistance can be effectively reduced, and the overall test performance of the device can be improved; since the electron beam can be precisely controlled, the growth structure and deposition accuracy of the alloyed ohmic contact layer 7 reach a high level, the deposition efficiency is high, the electron beam is easy to adjust, and the processing efficiency is significantly improved.

[0058] Step 3: Preparation and sintering of oxygen-free copper heat sink 12;

[0059] Step S31, thermal evaporation indium is plated on the oxygen-free copper base material, and the coating thickness is 15 μm; the preparation of the oxygen-free copper heat sink 12 is completed;

[0060] Step S32, mounting the oxygen-free copper heat sink 12 on a fixture, placing the epitaxial wafer on the oxygen-free copper heat sink 12, and then sintering in a vacuum sintering furnace;

[0061] In step three, the oxygen-free copper heat sink 12 can further improve its thermal conductivity in a deep low temperature environment at a relatively thin thickness; at the same time, the mechanical installation strength of the entire oxygen-free copper heat sink 12 is enhanced, so that the temperature-sensitive layer 5 can quickly reach temperature equilibrium with the measured object;

[0062] Step 4: Use the gold wire ball welding method to lead out the lower electrode and the upper electrode.

[0063] In step four, the packaging method of gold wire ball welding is adopted. Since gold wire has high electrical conductivity and corrosion resistance, the durability of the device is improved. At the same time, the processing is convenient and flexible, the solder joints are firm and stable, the piezoelectric area is large and non-directional, and automated high-speed welding can be achieved, thereby improving the overall processing efficiency of the device and achieving high-density packaging of the device.

[0064] Embodiment 1:

[0065] like Figure 3 , Figure 4 As shown, the test was carried out under the conditions of an initial test temperature of 50K and an external electric field strength of 9.6kV / cm; it can be seen that after the temperature is lower than 40K, the resistance of the device achieves a quantitative relationship of rapid linear increase with decreasing temperature, and the corresponding relative sensitivity reaches 15%, which meets the use requirements in deep low temperature environments.

[0066] Embodiment 2:

[0067] The envelope function method is used to calculate the energy level, which divides the electrons into the wave function of the rapidly oscillating atomic-electronic structure and the envelope function that changes relatively slowly in space. 0.15 Ga 0.85 As / GaAs composition, its lattice constant is almost the same, the lattice interface stress is very small, the Al component is continuously adjustable, the conduction band difference can be finely adjusted, and the sub-level structure is highly stable. The non-parabolic characteristics of GaAs and AlGaAs are ignored during the calculation process, that is, the relationship between effective mass and energy is ignored. The Hamiltonian of the system can be described by an effective mass model that is independent of energy:

[0068]

[0069] In the formula, H sc is all scattering terms including phonons, impurities, interfaces, and electrons, z is the growth direction, m e (z), Ec(z) is the effective mass of the electron of different material components and the energy of the conduction band bottom, k is the two-dimensional wave vector of the electron in the transverse xy plane, e is the charge of the electron, F is the strength of the external electric field, V c(z) is the Coulomb potential caused by the doped ions and electron distribution, which is determined by the Poisson equation. In the specific calculation, the Hamiltonian is decomposed into three parts: the first part describes the envelope wave function (referred to as wave function) in the pure z direction, which includes the first, third, fourth, and fifth terms, and the remaining two terms are perturbation terms. The second part describes the lateral xy part, that is, the second term, which is related to z. The effective mass is treated according to the quantum mechanical expectation value. The third part is the scattering term, which is the electron decoherence mechanism, and the semiclassical Fermi golden rule can be used.

[0070] In order to obtain the current density under different electric fields, it is usually necessary to find the eigenvalues ​​and eigenstates of the Hamiltonian under different electric fields, and then further calculate the scattering rates of various interactions to obtain the time lifetimes of different eigenstates and their corresponding particle number distributions, and finally obtain the current density. The corresponding calculation scheme is:

[0071] (a) Calculate the bound eigenenergy of the modified single quantum well Hamiltonian without electric field and without considering the Coulomb potential, and fit an empirical formula with very small error;

[0072] (b) Based on the empirical formula of the single quantum well energy level, the eigenenergy {E i}, eigenstate {ψ i (z)} constitute a set of orthogonal normalized basis vectors;

[0073] (c) Numerical calculation of the matrix z of the basis vector ij =<ψ i |z|ψ j >、Electron distribution ψ i (z)ψ j The Coulomb potential Mc of (z) ij (z) and V cijkl =<ψ k |V cij |ψ1> and the conduction band potential function matrix <ψ i |Ec|ψ j >

[0074] (d) Iteratively calculate the eigenenergy and eigenstates with applied electric field and Coulomb potential correction, and calculate the shape factor of the possible scattering matrix without electric field;

[0075] (e) Using the results of the first two steps, the shape factors under various electric fields are expressed semi-analytically, and then the scattering rates, energy level lifetimes, and decoherence times of various mechanisms are calculated. The waveguide loss and confinement factor of the device are calculated, and the photoelectric transport characteristics are obtained using rate equations, Monte Carlo methods, or density matrix methods. The entire calculation flow chart is shown below. Figure 5 As shown:

[0076] In the above calculation, the potential barriers on both sides of the single quantum well are infinitely wide. When the quantum wells are close to each other, the two interact with each other. At this time, the wave functions of the two quantum wells are used as the ground state, and the coupling of the two wells is used to calculate the intrinsic energy of the two quantum wells. By expanding the Hamiltonian based on the bound state of the two potential wells, the following parameters can be obtained:

[0077] r=<ψ L |ψ R >

[0078] S L =<ψ L |(V R (z)-V b )Θ(z R )|ψ L >

[0079] S R =<ψ R |(V L (z)-(V b ))Θ(z L )|ψ L >

[0080] In the formula, ψ L / R is the wave function of the single quantum wells on both sides. The parameter r represents the overlap factor of the two wave functions, which describes the strength of the coupling between the two sub-energy levels. The parameter S L / R It represents the energy shift between two states, V L / R (z) is the single quantum well potential function on both sides, Θ(z L / R ) is the characteristic area function of the left (right) potential well, which is equal to 1 only in the left (right) potential well and 0 elsewhere. The above calculation can be extended to the case where there are multiple sub-energy levels on both sides. In this case, the parameters r, S L / R They are all matrices.

[0081] Based on the above calculations, we can flexibly tailor the multilayer structure of quantum well period 50 according to the needs of high-precision temperature measurement in different cryogenic temperature ranges (15-40K, 50-60K, 70-90K, etc.) to meet the needs of high-precision temperature measurement in different cryogenic temperature ranges.

[0082] The number of devices and processing scales described here are used to simplify the description of the present invention. Applications, modifications and variations of the present invention are obvious to those skilled in the art. Although the embodiments of the present invention have been disclosed as above, they are not limited to the applications listed in the specification and the implementation mode. They can be applied to various fields suitable for the present invention. For those familiar with the art, other modifications can be easily realized. Therefore, without departing from the general concept defined by the claims and the equivalent scope, the present invention is not limited to the specific details and the legends shown and described here.

Claims

1. A deep cryogenic temperature sensor based on a multi-layer quantum well structure, characterized in that: include: The heat transfer layer, substrate layer, buffer layer with lower electrode, temperature sensitive layer composed of multiple quantum well periods, and contact layer with upper electrode are arranged in sequence from bottom to top; each quantum well period is composed of eight layers of Al with different thicknesses. 0.15 Ga 0.85 As and GaAs are composed alternately; Energy level calculation using envelope function method In the formula, is all scattering terms including phonons, impurities, interfaces, and electrons, z is the growth direction, m e (z), Ec(z) is the effective mass of the electron of different material components and the energy of the conduction band bottom, k is the two-dimensional wave vector of the electron in the transverse xy plane, e is the charge of the electron, F is the strength of the external electric field, V c (z) is the Coulomb potential caused by the distribution of doped ions and electrons; The buffer layer has a thickness of 700 nm, a doping element of Si, and a doping concentration of 2.5×10 18 cm -3 A heavily doped layer; The contact layer has a thickness of 70 nm, a doping element of Si, and a doping concentration of 5.0×10 18 cm -3 of heavily doped layers.

2. A deep cryogenic temperature sensor based on a multi-layer quantum well structure as claimed in claim 1, characterized in that: The heat transfer layer comprises a Ti / Au thermal contact layer with a thickness of 50nm-70nm; the upper end of the Ti / Au thermal contact layer is connected to the substrate layer, and the lower end is provided with an oxygen-free copper heat sink with a thickness of 2mm-5mm and a purity greater than 99.9%.

3. A deep cryogenic temperature sensor based on a multi-layer quantum well structure as claimed in claim 1, characterized in that: The substrate layer is specifically a semi-insulating GaAs substrate with a thickness of 180 μm to 200 μm.

4. A deep cryogenic temperature sensor based on a multi-layer quantum well structure as claimed in claim 1, characterized in that: The lower electrode and the upper electrode are both AU electrodes with a thickness of 100 nm, and alloyed ohmic contact layers are respectively arranged between the buffer layer and the contact layer.

5. A method for preparing a deep cryogenic temperature sensor based on a multi-layer quantum well structure according to any one of claims 1 to 4, characterized in that: The following steps are involved: Step 1: preparing epitaxial wafers by solid source molecular beam epitaxy method; Step S11: grow a 700nm thick Si-doped layer on the substrate layer with a doping concentration of 2.5×10 18 cm -3 A heavily doped layer as a buffer layer; Step S12: growing a multi-layer quantum well structure consisting of 50 to 80 quantum well periods on the buffer layer as a temperature sensitive layer; each quantum well period consists of eight layers of Al with different thicknesses, the minimum thickness being 1.7 nm and the maximum thickness being 17.0 nm. 0.15 Ga 0.85 As and GaAs are grown alternately; Step S13: grow a 70nm thick layer on the temperature sensitive layer, with Si as the doping element and a doping concentration of 5.0×10 18 cm -3 The heavily doped layer is used as a contact layer to complete the preparation of the epitaxial wafer; Step 2: preparing an alloyed ohmic contact layer by electron beam deposition; Step S21, taking an epitaxial wafer of size 5 mm×10 mm, using acetone and ethanol to clean the surface of the epitaxial wafer in sequence, then rinsing it with deionized water, and finally drying it with high-purity N2; Step S22, etching a stripe structure with a designed ridge width of 800 μm on the epitaxial wafer, and etching to a depth reaching the buffer layer of the epitaxial wafer; Step S23, using an electron beam to sequentially deposit Ge, Au, Ni, Au and other multi-layer metal films between the lower electrode and the buffer layer and between the upper electrode and the contact layer, and then rapidly annealing and alloying, thereby achieving ohmic contact between the lower electrode and the buffer layer and between the upper electrode and the contact layer; and completing the preparation of the alloyed ohmic contact layer; Step 3: Preparation and sintering of oxygen-free copper heat sink; Step S31, performing thermal evaporation plating of indium on the oxygen-free copper base material, with a coating thickness of 15 μm; completing the preparation of the oxygen-free copper heat sink; Step S32, installing an oxygen-free copper heat sink on a fixture, placing the epitaxial wafer on the oxygen-free copper heat sink, and then sintering in a vacuum sintering furnace; Step 4: Use the gold wire ball welding method to lead out the lower electrode and the upper electrode.