Method for manufacturing aluminum metal gate
By controlling the deposition temperature and planarization process of the aluminum metal layer, an aluminum metal gate with a hardness gradient is formed, which solves the problems of reduced efficiency of traditional polysilicon gates and dents and scratches on metal gates, and improves the performance of semiconductor components.
Patent Information
- Application Number
- CN202110953380.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-08-19
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2041-08-19
AI Technical Summary
Traditional polysilicon gates in semiconductor devices reduce device performance due to boron penetration and depletion effects, and metal gates are prone to dents or scratches during the manufacturing process, affecting electrical performance.
The physical vapor deposition process is used to control the deposition temperature of the aluminum metal layer to gradually increase from low temperature to high temperature to form an aluminum metal gate, and remove unnecessary metal layers through a planarization process to ensure the grain size and hardness gradient of the aluminum metal layer. , thus avoiding dents and scratches.
It effectively improves the yield rate of aluminum metal gates, avoids dent and scratch problems, and improves the driving ability and electrical performance of semiconductor components.
Smart Images

Figure CN113793803B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for manufacturing an aluminum metal gate, and in particular to a method for controlling the operating temperature of a physical vapor deposition process to deposit aluminum metal from low temperature to high temperature until an aluminum metal gate is formed. Background Art
[0002] In the existing semiconductor industry, polysilicon is widely used in semiconductor devices such as metal oxide semiconductor transistors, becoming a standard gate filling material. However, as the size of MOS transistors continues to shrink, the traditional polysilicon gate has problems such as the boron penetration effect, which leads to reduced device performance and the inevitable depletion effect, which increases the thickness of the equivalent gate dielectric layer and reduces the gate capacitance, thereby leading to the decline of device driving ability. Therefore, the semiconductor industry has tried to replace the traditional polysilicon gate with a new gate filling material, such as metal, as a control gate that matches the high-k gate dielectric layer.
[0003] However, due to the physical properties of metal itself, when making metal gates, the surface of the metal gates often dents or scratches, causing electrical problems in subsequent transistors. Therefore, how to improve the process to increase the yield of metal gates is still an important issue in the industry. Summary of the invention
[0004] In view of this, the present invention provides a new method for manufacturing a metal gate, particularly for manufacturing an aluminum metal gate, to solve the above-mentioned problems of depression and scratches on the metal gate.
[0005] According to a preferred embodiment of the present invention, a method for making an aluminum metal gate includes providing a substrate, a transistor arranged on the substrate, and an interlayer dielectric layer covering the transistor and the substrate, wherein the transistor includes a dummy gate, a gate dielectric layer and two source / drain doped regions, the gate dielectric layer is between the substrate and the dummy gate, the source / drain doped regions are respectively arranged in the substrate on both sides of the dummy gate, the upper surface of the interlayer dielectric layer is flush with the top surface of the dummy gate, then the dummy gate is removed to form a trench, and then a metal stack layer is formed to fill the trench and cover the interlayer dielectric layer, and then, after the metal stack layer is formed, a deposition process is performed to form an aluminum metal layer to fill the trench and cover the interlayer dielectric layer, wherein the deposition process includes: starting to deposit the aluminum metal layer at a first temperature, during the deposition process, the first temperature is gradually increased to a second temperature, the first temperature is less than the second temperature, and finally a planarization process is performed to remove the metal stack layer and the aluminum metal layer outside the trench to form the aluminum metal gate.
[0006] In order to make the above-mentioned objectives, features and advantages of the present invention more clearly understood, the following preferred embodiments are specifically cited and described in detail with reference to the accompanying drawings. However, the following preferred embodiments and drawings are only for reference and explanation, and are not intended to limit the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figures 1 to 4 A schematic diagram of a method for manufacturing an aluminum metal gate according to a preferred embodiment of the present invention;
[0008] Figure 5 yes Figure 4 Top view of the metal gate in .
[0009] Main component symbols
[0010] 10: Base
[0011] 12: Interlayer dielectric layer
[0012] 12a: Upper surface
[0013] 14: Virtual gate
[0014] 14a: Top surface
[0015] 16: Gate dielectric layer
[0016] 18: High dielectric constant layer
[0017] 20: Source / drain doping region
[0018] 22: Gap wall
[0019] 24: Groove
[0020] 26: Metal stack layer
[0021] 26a: Buffer layer
[0022] 26b: Work function layer
[0023] 26c: Buffer layer
[0024] 28:Deposition process
[0025] 30: Aluminum metal layer
[0026] 32: Planarization process
[0027] 100: Transistor
[0028] 126: Metal stack structure
[0029] 130: Aluminum metal gate
[0030] D1: First direction
[0031] D2: Second direction DETAILED DESCRIPTION
[0032] Figures 1 to 4 A method for manufacturing an aluminum metal gate is illustrated according to a preferred embodiment of the present invention. Figure 5 The picture shows Figure 4 Top view of the metal gate in .
[0033] like Figure 1 As shown, first, a substrate 10 is provided, a transistor 100 is arranged on the substrate 10, an interlayer dielectric layer 12 covers the transistor 100 and the substrate 10, the transistor 100 includes a dummy gate 14, a gate dielectric layer 16, two source / drain doped regions 20 and two spacers 22, the two spacers 22 are located on both sides of the dummy gate 14, the gate dielectric layer 16 is between the substrate 10 and the dummy gate 14, a high dielectric constant layer 18 is arranged between the gate dielectric layer 16 and the dummy gate 14, the source / drain doped regions 20 are respectively arranged in the substrate 10 on both sides of the dummy gate 14, the upper surface 12a of the interlayer dielectric layer 12 is aligned with the top surface 14a of the dummy gate 14, and the dummy gate 14 may include a cover layer (not shown). The substrate 10 may include a silicon substrate, a germanium substrate, a gallium arsenide substrate, a silicon germanium substrate, an indium phosphide substrate, a gallium nitride substrate, a silicon carbide substrate, or a silicon on insulator (SOI) substrate. The gate dielectric layer 16 is preferably silicon dioxide. The dummy gate 14 is preferably polysilicon. The high dielectric constant layer 18 includes aluminum oxide, zirconium oxide, barium strontium titanate (BST), lead zirconate titanate (PZT), zirconium silicate (ZrSiO 4 ), hafnium silicon oxide (HfSiO 2 ), hafnium silicon oxynitride (HfSiON), tantalum oxide or a combination of the above materials. The transistor 100 can be a P-type transistor or an N-type transistor, and the source / drain doping region 20 can include a P-type dopant or an N-type dopant. Figure 2 As shown, the dummy gate 14 is removed to form a trench 24 , and the high dielectric constant layer 18 is exposed through the trench 24 .
[0034] like Figure 3As shown, a metal stack layer 26 is formed to conformably fill the trench 24 and cover the interlayer dielectric layer 12. The metal stack layer 26 preferably includes a buffer layer 26a, a work function layer 26b and a buffer layer 26c, which are formed in sequence. The work function layer 26b may include an N-type work function layer, a P-type work function layer, or both an N-type work function layer and a P-type work function layer. The N-type work function layer includes TiN or TaN, and the P-type work function layer includes Ni, Pd, Pt, Be, Ir, Te, Re, Ru, Rh, W, Mo, WN, RuN, MoN, TiN, TaN, WC, TaC, TiC, TiAlN or TaAlN. The buffer layer 26a includes Ti, TiN, or both Ti and TiN. Similarly, the buffer layer 26c includes Ti, TiN, or both Ti and TiN.
[0035] Next, a deposition process 28 is performed to form an aluminum metal layer 30 to conformably fill the trench 24 and cover the interlayer dielectric layer 12. Specifically, the deposition process 28 is preferably physical vapor deposition sputtering (PVD sputtering). The deposition process 28 includes first depositing the aluminum metal layer 30 at a first temperature. During the deposition process 28, the first temperature is gradually increased to a second temperature. The first temperature is lower than the second temperature. According to a preferred embodiment of the present invention, the deposition process 28 starts at the first temperature and ends at the second temperature. It is worth noting that the grains of the aluminum metal layer 30 deposited at a low temperature are smaller, and the grains of the aluminum metal layer 30 deposited at a high temperature are larger. In addition, a first direction D1 is parallel to the upper surface of the substrate 10, and a second direction D2 is perpendicular to the upper surface of the substrate 10. The deposition rate of the aluminum metal layer 30 along the first direction D1 is lower than the deposition rate of the aluminum metal layer along the second direction D2. According to a preferred embodiment of the present invention, the first temperature is between 200°C and 350°C, and the grain size of the aluminum metal layer 30 formed at the first temperature is between 100 microns and 200 microns; the second temperature is between 350°C and 450°C, and the grain size of the aluminum metal layer 30 formed at the second temperature is between 200 microns and 500 microns.
[0036] like Figure 3 and Figure 4 As shown, a planarization process 32 is performed to remove the metal stack layer 26 and the aluminum metal layer 30 outside the trench 24 to form an aluminum metal gate 130 and a metal stack structure 126. The planarization process 32 is preferably chemical mechanical polishing. Since the formation temperature of the aluminum metal layer 30 is increased from a low temperature to a high temperature, and the deposition rate of the aluminum metal layer 30 along the first direction D1 is lower than the deposition rate of the aluminum metal layer 30 along the second direction D2, the lower part of the aluminum metal gate 130 formed finally will contain more aluminum metal layers 30 with small grains, and the upper part of the aluminum metal gate 130 will contain more aluminum metal layers 30 with large grains. Please also refer to Figure 5Only the outermost area of the top surface of the aluminum metal gate 130 is the aluminum metal layer 30 with smaller grains, while the area from the center to the outermost area is the aluminum metal layer 30 with larger grains.
[0037] Since the aluminum metal layer 30 formed at a low temperature has small grains and is relatively hard, if the aluminum metal gate 130 is made entirely of the aluminum metal layer 30 with small grains, scratches will be generated on the surface of the aluminum metal layer 30 during chemical mechanical polishing, and finally the top surface of the aluminum metal gate 130 will also be scratched, affecting the electrical properties of the subsequent transistor 100. On the other hand, since the aluminum metal layer 30 formed at a high temperature has large grains and is relatively soft, if the aluminum metal gate 130 is made entirely of the aluminum metal layer 30 with large grains, a depression will be generated in the center of the aluminum metal layer 30 during chemical mechanical polishing, and finally the center of the aluminum metal gate 130 will also be depressed, affecting the electrical properties of the subsequent transistor 100. Therefore, the present invention specifically regulates the process temperature of the aluminum metal layer 30 so that the lower portion of the aluminum metal gate 130 is the aluminum metal layer 30 with smaller grains and a harder surface, so that the aluminum metal layer 30 can be supported by the lower portion during chemical mechanical polishing without causing depressions, and the area from the center to the periphery of the aluminum metal gate 130 is the aluminum metal layer 30 with larger grains and a softer surface, so that after chemical mechanical polishing, no scratches will remain on the top surface of the aluminum metal gate 130.
[0038] The above descriptions are only preferred embodiments of the present invention. All equivalent changes and modifications made according to the claims of the present invention should fall within the scope of the present invention.
Claims
1. A method for manufacturing an aluminum metal gate, comprising: A substrate is provided, a transistor is arranged on the substrate, an interlayer dielectric layer covers the transistor and the substrate, wherein the transistor comprises: a dummy gate, a gate dielectric layer and two source / drain doped regions, the gate dielectric layer is between the substrate and the dummy gate, the multiple source / drain doped regions are respectively arranged in the substrate at both sides of the dummy gate, and the upper surface of the interlayer dielectric layer is aligned with the top surface of the dummy gate; removing the dummy gate to form a trench; forming a metal stack layer to fill the trench and cover the interlayer dielectric layer; After forming the metal stack layer, a deposition process is performed to form an aluminum metal layer to fill the trench and cover the interlayer dielectric layer, wherein the deposition process comprises: starting to deposit the aluminum metal layer at a first temperature, during the deposition process, the first temperature is gradually increased to a second temperature, wherein the first temperature is between 200° C. and 350° C., and the second temperature is between 350° C. and 450° C.; and A planarization process is performed to remove the metal stack layer and the aluminum metal layer outside the trench to form the aluminum metal gate, wherein at the first temperature, the aluminum metal layer with smaller grains and harder is formed at the lower part of the aluminum metal gate; at the second temperature, the aluminum metal layer with larger grains and softer is formed in the range from the center to near the periphery of the aluminum metal gate. 2 . The method for manufacturing an aluminum metal gate as claimed in claim 1 , wherein the grain size of the aluminum metal layer formed at the first temperature is between 100 microns and 200 microns. 3 . The method for manufacturing an aluminum metal gate as claimed in claim 1 , wherein the grain size of the aluminum metal layer formed at the second temperature is between 200 microns and 500 microns. 4 . The method for manufacturing an aluminum metal gate as claimed in claim 1 , wherein the planarization process is chemical mechanical polishing.
5. The method for manufacturing an aluminum metal gate as described in claim 1, wherein a first direction is parallel to the upper surface of the substrate, a second direction is perpendicular to the upper surface of the substrate, and a deposition rate of the aluminum metal layer along the first direction is less than a deposition rate of the aluminum metal layer along the second direction. 6 . The method for manufacturing an aluminum metal gate as claimed in claim 1 , wherein the deposition process is physical vapor deposition sputtering (PVD sputtering). 7 . The method for manufacturing an aluminum metal gate as claimed in claim 1 , wherein the deposition process starts at the first temperature and ends at the second temperature.
Citation Information
Patent Citations
Process for fabricating a semiconductor device with metallic gate and semiconductor device
CN101043003A
Method for fabricating semiconductor device
CN101714508A
Aluminum metal grid electrode forming method
CN103578940A
Work function layer, metal gate, semiconductor device and manufacturing method thereof
CN109119335A
Method of fabricating metal interconnects using a sacrificial layer to protect seed layer prior to gap fill
US20080113508A1