A magnetic effervescent tablet based on magnetic graphene oxide and preparation method thereof
Through magnetic effervescent tablets based on magnetic graphene oxide, combined with effervescent micro-extraction technology, the problem of polycyclic aromatic hydrocarbons removal in water is solved, efficient and low-cost pollutant removal and detection is achieved, the operation process is simplified, and the removal efficiency is improved. and adsorption capacity.
Patent Information
- Application Number
- CN202111187228.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-10-12
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2041-10-12
AI Technical Summary
It is difficult to remove polycyclic aromatic hydrocarbon pollutants in water efficiently and at low cost with existing technology, and traditional methods require dispersants and complex dispersion methods, resulting in low operating efficiency.
Magnetic effervescent tablets based on magnetic graphene oxide are prepared through effervescent microextraction technology, using magnetic graphene oxide, citric acid, sodium bicarbonate, 1-octyl-3-methylimidazole chloride, and bistrifluoromethane Lithium sulfonylimide is combined into a magnetic effervescent tablet to achieve efficient adsorption and removal of polycyclic aromatic hydrocarbons.
It achieves efficient, low-cost, simple-to-operate removal of polycyclic aromatic hydrocarbons, has strong adsorption capacity, and does not require dispersants or complex dispersion methods. The magnetic effervescent tablet is stable and easy to separate, and is suitable for the detection and removal of polycyclic aromatic hydrocarbons in water samples.
Smart Images

Figure CN113976079B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of detection and removal of pollutants in water, and relates to a method for preparing a magnetic effervescent tablet based on magnetic graphene oxide and application of the magnetic effervescent tablet in the removal of polycyclic aromatic hydrocarbons. Background Art
[0002] Effervescent tablet-assisted microextraction (ETE), also known as effervescent-assisted microextraction, has been introduced as a new solvent-free dispersion technology. This technology promotes phase homogenization by adding proton donors and carbon sources to the matrix to form bubbles in situ, replacing the use of dispersed solvents and auxiliary extraction methods such as ultrasound and vortex. Effervescent microextraction can add a variety of extractants, such as ionic liquids and nanomaterials, or combine proton donors, carbon sources and extractants into extraction devices or effervescent tablets to facilitate operation. At present, effervescent microextraction technology has been widely used in environmental sample analysis.
[0003] Magnetic graphene oxide (MGO) is a graphene-based composite material with magnetism and oxygen-containing functional groups. Based on the physicochemical properties brought by its oxygen-containing functional groups, the material has good dispersibility and stability in aqueous solution and its adsorption capacity is better than other conventional adsorbents. Therefore, it is used to detect or remove trace toxic pollutants from aqueous solutions.
[0004] Polycyclic aromatic hydrocarbons (PAHs) are a class of persistent organic pollutants that mainly come from human activities, including motor vehicle exhaust, fossil fuels, and incomplete combustion of wood. Due to their high solubility in lipids, they can be distributed in a variety of animal tissues. Long-term exposure to PAHs can easily cause damage to the eyes, kidneys, and liver. In addition, PAHs also have serious toxicological effects such as mutagenicity, carcinogenicity, teratogenicity, and gene mutation. Since PAHs can enter surface water and infiltrate into drinking water sources to cause health hazards, it is necessary to develop low-cost and effective technologies to remove PAHs from water to ensure water safety. Obviously, magnetic effervescent tablets prepared using effervescent microextraction technology and magnetic graphene oxide will be expected to achieve convenient and efficient removal of PAHs. Summary of the invention
[0005] The object of the present invention is to provide an effervescent tablet based on magnetic graphene oxide and a preparation method thereof, and verify the effect of removing polycyclic aromatic hydrocarbons. The method has the advantages of simple operation, high accuracy, good sensitivity, small matrix effect, and environmental friendliness. Compared with traditional pollutant removal methods, this technology can remove polycyclic aromatic hydrocarbons in environmental water samples without dispersants or complex dispersion methods, greatly improving operating efficiency.
[0006] Technical solution: To achieve the above purpose, the present invention adopts the following technical solution:
[0007] A magnetic effervescent tablet based on magnetic graphene oxide is prepared from magnetic graphene oxide, citric acid, sodium bicarbonate, 1-octyl-3-methylimidazolium chloride and lithium bis(trifluoromethanesulfonyl)imide.
[0008] A method for preparing a magnetic effervescent tablet based on magnetic graphene oxide comprises the following steps:
[0009] (1) Synthesis of magnetic graphene oxide: Take graphene oxide and water, stir under nitrogen protection, and heat from room temperature to 60-80 °C; then add a solution consisting of FeCl3·6H2O, FeCl2·4H2O and water, continue stirring and then add a solution consisting of NaOH and water. After continuing the reaction, cool the mixture to room temperature and pour it into a beaker. Use an external magnet to adsorb the synthesized magnetic material, then wash the magnetic material with water and ethanol, dry it, and grind it into powder to obtain magnetic graphene oxide;
[0010] (2) Synthesis of magnetic effervescent tablets: Accurately weigh citric acid, sodium bicarbonate, 1-octyl-3-methylimidazolium chloride, lithium bis(trifluoromethanesulfonyl)imide and the magnetic graphene oxide obtained in step (1); grind the solid-liquid mixture in a mortar until the powder is uniform and fine; then, use an infrared tablet press to press the mixed uniform powder into a magnetic effervescent tablet.
[0011] As a preferred embodiment, the method for preparing the magnetic effervescent tablet based on magnetic graphene oxide described above comprises the following steps:
[0012] (1) Synthesis of magnetic graphene oxide: Take graphene oxide and water, stir under nitrogen protection, and heat from room temperature to 60-80 °C; then add a solution consisting of 0.5-3 g FeCl3·6H2O, 0.5-3 g FeCl2·4H2O and 10-50 ml water, continue stirring and then add a solution consisting of NaOH and water. After continuing the reaction, cool the mixture to room temperature and pour it into a beaker. Use an external magnet to adsorb the synthesized magnetic material, then wash the magnetic material with water and ethanol, dry it, and grind it into powder to obtain magnetic graphene oxide;
[0013] (2) Synthesis of magnetic effervescent tablets: Accurately weigh 200-300 mg of citric acid, 100-150 mg of sodium bicarbonate, 10-50 μL of 1-octyl-3-methylimidazolium chloride, 20-40 mg of lithium bis(trifluoromethanesulfonyl)imide and 1-30 mg of the magnetic graphene oxide obtained in step (1); grind the solid-liquid mixture in a mortar until the powder is uniform and fine; then, use an infrared tablet press to press the mixed uniform powder into a magnetic effervescent tablet.
[0014] As a preferred embodiment, in the method for preparing the magnetic effervescent tablet based on magnetic graphene oxide described above, after the temperature is raised from room temperature to 70°C in step (1), a solution consisting of 2.16g FeCl3·6H2O, 0.8g FeCl2·4H2O and 40ml water is added.
[0015] As a preferred embodiment, in the method for preparing the magnetic effervescent tablet based on magnetic graphene oxide described above, the dosage ratio of citric acid, sodium bicarbonate, 1-octyl-3-methylimidazolium chloride, lithium bis(trifluoromethanesulfonyl)imide, and magnetic graphene oxide in step (2) is 278 mg: 121 mg: 30 μL: 32 mg: 10 mg.
[0016] The invention provides a method for detecting 4-benzopyrene and anthracene by adsorption of a magnetic effervescent tablet based on magnetic graphene oxide. The method comprises the following steps: placing the magnetic effervescent tablet based on magnetic graphene oxide in a centrifuge tube, respectively adding aqueous solutions of BaP and Ant into the centrifuge tube, and when the effervescent tablet is completely disintegrated, keeping an external magnet next to the outer wall of the centrifuge tube to separate the magnetic graphene oxide from the aqueous phase, aspirating and discarding the supernatant using a dropper, eluting the residual magnetic nanomaterial of 3,4-benzopyrene adsorbed with 400-2000 μL of toluene or acetone for 1-6 times; and eluting the residual magnetic nanomaterial of anthracene adsorbed with 400-2000 μL of toluene or acetone for 1-6 times; and then transferring the mixed elution solution to a quartz cuvette with a cover, and recording the fluorescence intensity using a fluorescence spectrophotometer.
[0017] As a preferred embodiment, the present invention provides a method for detecting 4-benzopyrene and anthracene by adsorption using a magnetic effervescent tablet based on magnetic graphene oxide, wherein the eluent for 3,4-benzopyrene (BaP) and anthracene (Ant) is acetone, the elution amount should be 400 μL, the optimal elution times for BaP are 3 times, the optimal elution times for Ant are 4 times, and the optimal pH of the matrix solution is 7.
[0018] Compared with the existing method, the present invention has the following beneficial effects:
[0019] (1) The present invention has screened through a large number of experiments and found that magnetic graphene oxide, citric acid, sodium bicarbonate, 1-octyl-3-methylimidazolium chloride, and lithium bis(trifluoromethanesulfonyl)imide can be used to prepare magnetic graphene oxide effervescent tablets with good adsorption performance. All raw materials are indispensable.
[0020] (2) The effervescent microextraction technology is used. The preparation method is simple, reliable and low-cost. It can efficiently remove pollutants without dispersants or complex dispersion methods. The use of magnetic graphene oxide can easily separate it from the matrix and has stronger adsorption capacity. The finished product of the technology is in the form of effervescent tablets, which are easy to carry, simple to use, and have good effects. It can be used in the detection and removal of polycyclic aromatic hydrocarbons.
[0021] (3) The magnetic effervescent tablets designed in the present invention are stable in nature and have obvious magnetism. After disintegration in water, the target substance can be quickly separated and recovered from the liquid phase using a magnet. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 In the embodiment, (a) the Fourier transform infrared (FTIR) spectrum of GO; (b) the FTIR spectrum of MGO;
[0023] Figure 2 In the examples, (a) a scanning electron microscope (SEM) image of GO; (b) a SEM image of MGO; (c) a transmission electron microscope (TEM) image of GO; (d) a TEM image of MGO;
[0024] Figure 3 The following are (a) the nanomaterial selection survey diagram in the examples; (b) the material dosage survey diagram; (c) the ionic liquid type survey diagram; (d) the ionic liquid dosage survey diagram; (e) the ion exchange agent selection survey diagram; (f) the effervescent tablet ingredient survey diagram;
[0025] Figure 4 These are (a) the sample solution pH investigation diagram in the examples; (b) the eluent selection investigation diagram; (c) the eluent dosage investigation diagram; and (d) the elution time investigation diagram. DETAILED DESCRIPTION
[0026] The following is a further detailed description of the claims of the present invention in conjunction with specific implementation methods, but does not constitute any limitation to the present invention. Any limited modifications made within the scope of protection of the claims of the present invention are still within the scope of protection of the claims of the present invention.
[0027] Example 1
[0028] A method for preparing a magnetic effervescent tablet based on magnetic graphene oxide comprises the following steps:
[0029] (1) Solution preparation: Take appropriate amounts of 3,4-benzopyrene (BaP) and anthracene (Ant) standards, accurately weigh them, place them in 10 mL brown volumetric flasks, and dilute them with methanol to a concentration of 1 mg mL -1 The standard stock solution was stored at 4 °C in the dark. The stock solution was diluted with methanol and diluted step by step to the required concentration when used.
[0030] (2) Sample collection and preparation: Environmental water was collected from the local suburbs. The water samples were filtered through a 0.45 μm syringe filter and placed in a 4 ℃ refrigerator for later use. 5 mL of water sample was taken and 100 μL of BaP or Ant standard stock solution was added for subsequent analysis.
[0031] (3) Synthesis of magnetic graphene oxide: 0.5 g of graphene oxide and 100 mL of water were added to a three-necked flask, mechanically stirred under nitrogen protection, and heated from room temperature to 70 °C. Then, a solution consisting of 2.16 g of FeCl3·6H2O, 0.80 g of FeCl2·4H2O, and 40 mL of water was added. After stirring for 10 min, a solution consisting of 7 g of NaOH and 70 mL of water was added. After the reaction was continued for 1 h, the mixture was cooled to room temperature and poured into a glass container. The synthesized magnetic material was adsorbed by an external magnet, washed three times with water and ethanol respectively, dried in a vacuum oven at 60 °C for 8 h, and ground into powder.
[0032] (4) Synthesis of magnetic effervescent tablets: Precisely weigh the tablet precursor, including 278 mg of citric acid, 121 mg of sodium bicarbonate, 30 μL of 1-octyl-3-methylimidazolium chloride, 32 mg of lithium bis(trifluoromethanesulfonyl)imide and 10 mg of magnetic graphene oxide obtained in step (3). Grind the solid-liquid mixture in a mortar until the powder is uniform and fine. Subsequently, use an infrared tablet press to press the mixed uniform powder into magnetic effervescent tablets (8 mm diameter × 2 mm thickness), package them in a sealed bag, and place them in a desiccator for subsequent use.
[0033] (5) Conducting a magnetic effervescent tablet-assisted microextraction experiment: First, the effervescent tablet was placed in a centrifuge tube, each containing 5 mL of an aqueous solution (pH = 7) containing BaP and Ant obtained by the preparation method in step (2). After about a few minutes, the effervescent tablet was observed to completely disintegrate. Subsequently, an external magnet was kept next to the outer wall of the centrifuge tube to separate the magnetic graphene oxide (MGO) from the aqueous phase. Finally, the supernatant was aspirated and discarded using a dropper, and the magnetic nanomaterials (MNPs) with residual BaP adsorption were eluted with 400 μL of acetone for 3 minutes; for the MNPs with residual Ant adsorption, they were eluted with 400 μL of acetone for 4 minutes. The mixed elution solution was transferred to a quartz cuvette with a lid, and the fluorescence intensity was recorded using a fluorescence spectrophotometer. The adsorption recoveries of BaP and Ant reached 98.6% and 87.1%, respectively, showing strong adsorption performance.
[0034] The properties of the obtained magnetic graphene oxide (MGO) and graphene oxide (GO) were characterized by Figure 1 It can be seen that the FT-IR spectrum of MGO has a peak at 584.5 cm -1 The absorption peak at , which is attributed to the vibration of Fe-O bonds, indicates the successful formation of covalent bonds between magnetic nanoparticles and graphene oxide. Figure 2 (a / b) It can be seen that GO has a smooth sheet structure and is evenly distributed. The surface of MGO is relatively rough, which indicates that the FeO nanoparticles are well distributed and successfully bonded to the surface of graphene oxide, indicating the successful synthesis of magnetic graphene oxide. Figure 2 (c / d) It can be seen that GO is in the form of flakes with high transparency. The Fe3O4 nanoparticles appear as black spots on the cross section of MGO and are evenly bonded to the GO surface, confirming the successful synthesis of MGO.
[0035] Example 2 Screening of the composition of magnetic effervescent tablets is an experimental study
[0036] 1. Taking the removal of two PAHs as indicators, Figure 3 The composition of the effervescent tablet was determined, including (a) selecting magnetic graphene oxide as the adsorption material; (b) selecting 10 mg as the amount of adsorption material with good removal effect and small material dosage; (c) selecting 1-octyl-3-methylimidazolium chloride as the ionic liquid; (d) selecting 30 μL as the amount of ionic liquid; (e) selecting lithium bis(trifluoromethanesulfonyl)imide as the ion exchanger; and (f) determining that the nanomaterial, ionic liquid and ion exchanger should all exist in the composition for optimal results.
[0037] 2. The adsorption-elution process conditions were investigated, with the removal of two PAHs as the index. Figure 4The adsorption-elution process conditions were clarified, including (a) selecting pH=7 as the matrix pH value; (b) selecting acetone as the elution solvent; (c) selecting 400 μL as the elution dose; and (d) selecting 3 min and 4 min as the elution time of BaP and Ant.
[0038] The above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable people familiar with the technology to understand the content of the present invention and implement it accordingly, and they cannot be used to limit the protection scope of the present invention. Any equivalent changes or modifications made according to the spirit of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for preparing a magnetic effervescent tablet based on magnetic graphene oxide, characterized in that: The steps include: (1) Synthesis of magnetic graphene oxide: graphene oxide and water are stirred under nitrogen protection and heated from room temperature to 60-80°C; then a solution consisting of 0.5-3 g FeCl3·6H2O, 0.5-3 g FeCl2·4H2O and 10-50 mL water is added, and after continued stirring, a solution consisting of NaOH and water is added. After continued reaction, the mixture is cooled to room temperature and poured into a beaker. The synthesized magnetic material is adsorbed by an external magnet, and then the magnetic material is washed with water and ethanol in sequence, dried, and ground into powder to obtain magnetic graphene oxide; (2) Synthesis of magnetic effervescent tablets: accurately weigh 278 mg of citric acid, 121 mg of sodium bicarbonate, 30 μL of 1-octyl-3-methylimidazolium chloride, 32 mg of lithium bis(trifluoromethanesulfonyl)imide and 10 mg of the magnetic graphene oxide obtained in step (1); grind the solid-liquid mixture in a mortar until the powder is uniform and fine; then, use an infrared tablet press to press the mixed uniform powder into the magnetic effervescent tablet.
2. The method for preparing a magnetic effervescent tablet based on magnetic graphene oxide according to claim 1, characterized in that: In step (1), after the temperature is raised from room temperature to 70°C, a solution consisting of 2.16 g FeCl3·6H2O, 0.8 g FeCl2·4H2O and 40 mL water is added.
3. Application of the magnetic effervescent tablet based on magnetic graphene oxide prepared by the preparation method according to claim 1 in the adsorption and removal of 3,4-benzopyrene or anthracene.
4. A method for detecting 3,4-benzopyrene or anthracene by adsorption of a magnetic effervescent tablet based on magnetic graphene oxide prepared by the preparation method according to claim 1, characterized in that: The method comprises the following steps: placing a magnetic effervescent tablet based on magnetic graphene oxide into a centrifuge tube, adding an aqueous solution of 3,4-benzopyrene or anthracene into the centrifuge tube respectively, and when the effervescent tablet is completely disintegrated, keeping an external magnet next to the outer wall of the centrifuge tube to separate the magnetic graphene oxide from the aqueous phase, and using a dropper to absorb and discard the supernatant; eluting the magnetic nanomaterial with residual adsorption of 3,4-benzopyrene with 400-2000 μL of toluene or acetone for 1-6 times; eluting the magnetic nanomaterial with residual adsorption of anthracene with 400-2000 μL of toluene or acetone for 1-6 times; and then transferring the mixed elution solution into a quartz cuvette with a cover, and recording the fluorescence intensity with a fluorescence spectrophotometer.
5. The method according to claim 4, characterized in that The eluent for 3,4-benzopyrene or anthracene is acetone, the elution amount is 400 μL, the elution times for 3,4-benzopyrene is 3 times, the elution times for anthracene is 4 times, and the pH value of the matrix solution is 7.
Citation Information
Patent Citations
Graphene aerogel microsphere with gradient pore structure as well as preparation method and application thereof
CN111977641A