Measurement method and device for improving the measurement accuracy of prestressed tendon shrinkage

Through the combination of magnet and bow steel flat ruler, combined with jack and semi-spherical measurement base point, the problem of insufficient measurement accuracy of the internal shrinkage of prestressed ribs is solved, high-precision measurement is achieved, the on-site measurement process is simplified, and the field measurement process is simplified, and in three-dimensional space is in Achieve barrier-free measurement.

CN113984528BActive Publication Date: 2024-11-05ARCHITECTURAL SCI RES & DESIGN INST OF HUBEI PROV +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111351482.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-11-16
Publication Date
2024-11-05
Estimated Expiration
2041-11-16

AI Technical Summary

Technical Problem

In the prior art, the measurement accuracy of the internal shrinkage of the prestressed rib is insufficient, and the distance between the deformed surface and the other measurement surface cannot be accurately measured under the limitations of on-site conditions, resulting in increased measurement difficulty.

Method used

The plane to be measured is composed of magnets and arcuate steel flat rulers. By fixing the adsorption magnets and arcuate steel flat rulers, tensioning and oil return measurements are performed using jacks, and combined with the semi-spherical measurement base point, the precise measurement of the length of prestressed ribs is achieved. And improve the measurement accuracy through average calculation.

Benefits of technology

The precise measurement of the internal shrinkage of the prestressed rib is achieved, with an accuracy of 0.01mm, which simplifies the measurement process, avoids inaccuracy caused by changes in the measurement position, and can directly measure in three-dimensional space without being affected by obstacles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113984528B_ABST
    Figure CN113984528B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of construction engineering quality inspection, and provides a method for measuring the shrinkage of prestressed tendons, including seven steps S1 to S7. A device for measuring the shrinkage of prestressed tendons is also provided. The present invention uses a plane to be measured composed of a magnet and a bow-shaped steel ruler to more accurately and simply reflect the deformation of a deformation surface, and only needs to complete 4 measurement values, so that the measurement can be completed quickly; the plane to be measured is a measurement position that does not shift and does not need to be marked or memorized, and there will be no inaccurate measurement value caused by the change of the measurement point position during multiple measurements; the steel ruler leads the measurement point from the interior of the three-dimensional space that is blocked by obstacles in three directions, so that barrier-free direct measurement of the required dimensions can be achieved; the two ends of the bow-shaped steel ruler have semi-spherical measurement base points, and the measurement accuracy is high; the bow-shaped steel ruler is conducive to evenly arranging measurement points around the outer circle of the working anchor, and the measured distance between the deformation surface and another measurement surface is more accurate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of construction engineering quality detection, and in particular to a layout detection method and a device for improving the measurement accuracy of prestressed tendon shrinkage. Background Art

[0002] Prestressed concrete beams are a common form of beam construction in recent years. In order to test the quality of products used in prestressed beams, it is necessary to test parameters such as the shrinkage of prestressed tendons on site. Since prestressed beams in housing construction projects generally adopt a one-end tensioning and one-end buried anchoring method, the detection and measurement of the shrinkage of prestressed tendons in prestressed beams in housing construction projects can only be carried out according to the direct measurement method in Appendix C of GB / T14370-2015 "Anchors, clamps and connectors for prestressed tendons". However, in actual testing, the measurement is difficult because the jack cylinder blocks the anchor plate when the prestressed tendons are tensioned, the anchor plate is often penetrated into the concrete during installation, and the conditions for segmented measurement are not available. Therefore, the direct measurement method in Appendix C of GB / T14370-2015 "Anchors, clamps and connectors for prestressed tendons" can only use 1mm as the standard for the length of the prestressed tendons outside the anchor plate, the length of the prestressed tendons outside the anchor plate when the jack returns oil to an oil pressure of 1Mpa, and the length of the prestressed tendons between the working anchor and the tool anchor. However, the accuracy of the prestressed tendon shrinkage assessment value specified in GB50666-2011 "Concrete Structure Engineering Construction Code" is 1mm, so the accuracy does not meet the requirements of rounding, that is, when the assessment value accuracy is 1mm, the measurement accuracy should reach 0.1mm. At the same time, the anchor plate will deform when the prestressed tendons are tensioned, that is, the step surface of the anchor plate is a deformation surface. In addition, the tensioning construction process is divided into whole-beam tensioning and single-strand tensioning. When a single strand is tensioned, the anchor plate will be locally stressed and deformed. For this situation where the distance between the deformation surface and another measuring surface needs to be measured, the distance between the deformation surface and the other measuring surface is usually measured at ten points in a certain area and the average is used as the distance between the two surfaces. However, due to the narrow space at the detection site and the situation where tensioning and oil return are measured separately, this measurement method cannot be implemented. Therefore, how to overcome the above defects and use a relatively simple method to accurately measure the distance between the deformation surface and the other measuring surface that is restricted by site conditions has become an urgent problem to be solved. Summary of the invention

[0003] The object of the present invention is to provide a layout measurement method and device for improving the measurement accuracy of prestressed tendon shrinkage, which can at least solve some of the defects in the prior art.

[0004] To achieve the above-mentioned purpose, the embodiment of the present invention provides the following technical solution: a layout measurement method for improving the measurement accuracy of prestressed tendon shrinkage, comprising the following steps:

[0005] S1, chisel away the concrete outside the anchor plate that affects the placement of the steel level, and remove the concrete residue on the step surface of the anchor plate;

[0006] S2, adsorbing four identical magnets on the outer step surface of the anchor pad, each of the magnets is divided into two adjacent groups, the two groups of magnets are symmetrically arranged with a line perpendicular to the axis of the working anchor as the symmetry axis, and the shape formed by the four magnets is a square;

[0007] S3, two arched steel rulers are arranged along the circumferential surface of the working anchor, the two arched steel rulers are arranged in parallel and are respectively fixed by two groups of magnets, and the planes with semi-spherical measuring base points at the ends of the ruler surfaces of the two arched steel rulers face the tool anchor side;

[0008] S4, use a jack to tension the prestressed tendons with 80% of their nominal ultimate tensile strength to achieve tension control and hold the load until the elongation is stable;

[0009] S5, using a height micrometer without the base, respectively measure the length L1 of the prestressed tendon outside the arched steel ruler, the length L2 of the prestressed tendon between the working anchor and the tool anchor, and the length L3 of the prestressed tendon between the working anchor and the tool anchor using the semi-spherical vertex at the end of the ruler surface of the arched steel ruler as the reference. j , wherein the tool anchor is located on a side of the jack away from the working anchor;

[0010] S6, when the oil pressure of the jack returns to 1 MPa, use a height micrometer without the base to measure the length L2 of the prestressed tendon outside the bow-shaped steel ruler with the semi-spherical vertex at the end of the ruler surface of the bow-shaped steel ruler as the reference;

[0011] S7, length L1, length L j , length L2, and calculate the average value, and use the average value to calculate the shrinkage of the prestressed tendon.

[0012] Furthermore, the middle part of the arched steel ruler is arched and both ends are straight, and the arc of the arched middle part is consistent with the curvature of the circumferential surface of the working anchor.

[0013] Furthermore, the magnet is a neodymium iron boron magnet.

[0014] Furthermore, the length L1 of the prestressed tendon outside the bow steel ruler and the length L2 of the prestressed tendon between the working anchor and the tool anchor are j , the length L2 of the prestressed tendon outside the bow steel ruler is measured with an accuracy of 0.01mm.

[0015] Furthermore, the calculated shrinkage of the prestressed tendon is rounded off at a rounding interval of 0.1 mm, and the rounded shrinkage of the prestressed tendon is used as the measured value.

[0016] An embodiment of the present invention also provides the following technical solution: a device for measuring the shrinkage of prestressed tendons, comprising an anchor plate partially placed in concrete and on which prestressed tendons can be installed, and a jack for providing tension, a working anchor is provided between the jack and the anchor plate, four identical magnets are adsorbed on the outer step surface of the anchor plate, each of the magnets is divided into two adjacent groups, the two groups of magnets are symmetrically arranged with a line perpendicular to the axis of the working anchor as the axis of symmetry, and the shape formed by the four magnets is a square, two bow-shaped steel rulers are arranged outside the circumferential surface of the working anchor, the two bow-shaped steel rulers are arranged in parallel and the two bow-shaped steel rulers are respectively adsorbed and fixed by the two groups of magnets, and the ends of the ruler surfaces of the two bow-shaped steel rulers have semi-spherical measuring base points.

[0017] Furthermore, a tool anchor is provided on a side of the jack away from the anchor plate.

[0018] Furthermore, a limiting plate is provided between the jack and the working anchor.

[0019] Further, the plane with the semi-spherical measuring base point faces the tool anchor side.

[0020] Furthermore, the middle part of the arched steel ruler is arched and both ends are straight, and the arc of the arched middle part is consistent with the curvature of the circumferential surface of the working anchor.

[0021] Furthermore, the magnet is a neodymium iron boron magnet.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] 1. The plane to be measured composed of magnets and steel rulers can reflect the deformation of the deformation surface more accurately and simply, and only 4 measured values ​​need to be completed, and the measurement can be completed quickly; the plane to be measured is a measurement position that does not shift and does not need to be marked or memorized, and there will be no inaccurate measurement values ​​caused by changes in the position of the measuring points during multiple measurements.

[0024] 2. The steel ruler leads the point to be measured from the interior of the three-dimensional space that is blocked by obstacles in three directions, so as to realize the barrier-free direct measurement of the required dimensions.

[0025] 3. The two ends of the steel ruler are equipped with semi-spherical measuring base points, which ensure high measurement accuracy.

[0026] 4. The bow-shaped steel straightedge is conducive to evenly arranging measuring points around the outer circle of the working anchor, so that the distance measurement between the deformation surface and another measuring surface is more accurate.

[0027] 5. Use a height vernier caliper with the base removed for measurement. The height vernier caliper can be close to the jack cylinder, and the height vernier caliper rod is parallel to the axis of the jack cylinder. The measurement accuracy is high, and it is light and easy to operate. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 A cross-sectional view from a first perspective of a prestressed tendon shrinkage measurement device provided by an embodiment of the present invention;

[0029] Figure 2 A cross-sectional view from a second perspective of the prestressed tendon shrinkage measurement device provided by an embodiment of the present invention;

[0030] In the accompanying drawings: 1-bow steel level; 2-jack; 3-working anchor; 4-magnet; 5-tool anchor; 6-limiting plate; 7-concrete; 8-anchor pad; 9-prestressed tendons. DETAILED DESCRIPTION

[0031] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0032] See also Figure 1 and Figure 2 The embodiment of the present invention provides a layout measurement method for improving the measurement accuracy of the internal shrinkage of prestressed tendons, comprising the following steps: S1, chiseling away the concrete 7 outside the anchor plate 8 that affects the layout of the bow-shaped steel ruler 1, and removing the concrete residue on the step surface of the anchor plate; S2, adsorbing four magnets 4 of equal thickness and specification on the outer step surface of the anchor plate 8, each of the magnets 4 is divided into two adjacent groups, the two groups of magnets 4 are symmetrically arranged with a line perpendicular to the axis of the working anchor 3 as the symmetry axis, and the shape formed by the four magnets is a square; S3, two bow-shaped steel rulers 1 are arranged outside the circumferential surface of the working anchor 3, and the two bow-shaped steel rulers 1 are arranged outside the circumferential surface of the working anchor 3. The rulers 1 are arranged in parallel and the two arched steel rulers 1 are respectively fixed by adsorption by the two groups of magnets 4, and the planes with the semi-spherical measuring base points at the ends of the ruler surfaces of the two arched steel rulers 1 face the tool anchor 5 side; S4, using the jack 2, tensioning is performed with 80% of the nominal ultimate tensile force of the prestressed tendon 9 to achieve the tensioning control force and hold the load until the elongation is stable; S5, using the height micrometer without the base to measure the length L1 of the prestressed tendon 9 outside the arched steel ruler 1 and the length L1 of the prestressed tendon 9 between the working anchor 3 and the tool anchor 5, respectively, with the semi-spherical vertex of the ruler surface end of the arched steel ruler 1 as the reference. j, accurate to 0.01mm, wherein the tool anchor 5 is located on the side of the jack 2 away from the working anchor 3; S6, when the oil pressure of the jack 2 returns to 1Mpa, use the height vernier ruler without the base to measure the length L2 of the prestressed tendon 9 outside the bow-shaped steel ruler 1 with the semi-spherical vertex at the end of the ruler surface of the bow-shaped steel ruler 1 as the reference, accurate to 0.01mm. For the case where the prestressed tendon 9 is in a broken line during single-strand tensioning, it only needs to be measured in two steps to accurately reflect its length change value. If a single-strand tensioning scheme is adopted, the position of the prestressed tendon 9 at the tool anchor 5 is usually in a broken line shape. At this time, a two-stage measurement method should be adopted, that is, the length of the prestressed tendon 9 outside the tool anchor 5 and the length from the tool anchor 5 to the outside of the bow-shaped steel ruler 1 are measured respectively, and the sum is used as the length L1 of the prestressed tendon 9 outside the bow-shaped steel ruler 1; S7, for the length L1 and the length L j , length L2 are averaged respectively, and the shrinkage of the prestressed tendon 9 is calculated with the average value. In this embodiment, some conventional structures are first arranged according to the existing prestress measurement method, such as jack 2, working anchor 3, tool anchor 5, limit plate 6, anchor plate 8, prestressed tendon 9, etc. After chiseling away the concrete outside the anchor plate 8 that affects the placement of the bow-shaped steel ruler 1, the concrete residue on the step surface of the anchor plate 8 needs to be removed. Then the magnet 4 and the bow-shaped steel ruler 1 are arranged. Then measure L1 and L2 twice. j , L2 and then take the average value. When making the second measurement, return the oil in jack 2 to the oil pressure of 1Mpa. Finally, when using the average value for calculation, calculate the shrinkage of prestressed tendon 9 according to the formula of direct measurement method in Appendix C of GB / T14370-2015 "Anchors, clamps and connectors for prestressed tendons 9", accurate to 0.01mm, and use the length of prestressed tendon 9 outside the bow steel ruler 1 to replace the length of prestressed tendon 9 outside the anchor pad 8 in the direct measurement method in Appendix C of GB / T14370-2015 "Anchors, clamps and connectors for prestressed tendons 9". The length of prestressed tendon 9 outside the bow steel ruler 1 when jack 2 returns oil to the oil pressure of 1Mpa replaces the length of prestressed tendon 9 outside the anchor pad 8 when jack 2 returns oil to the oil pressure of 1Mpa. The measurement is simple and there is no difference in the shrinkage calculation results. This calculation method is a conventional technical means, and the specific calculation formula will not be described in detail here. In addition, semi-spherical vertices are provided at the two ends of each of the arched steel rulers 1, and the semi-spherical vertices are used as references, and the two ends of the ruler surface of the arched steel ruler 1 have semi-spherical measurement base points, and the measurement accuracy is high. Preferably, the calculated shrinkage of the prestressed tendon is rounded off at a rounding interval of 0.1 mm, and the rounded shrinkage of the prestressed tendon is used as the measured value.

[0033] As an optimization solution of the embodiment of the present invention, please refer to Figure 1 and Figure 2The arched steel ruler 1 is an arched steel ruler with a raised middle portion and straight ends, and the arc of the raised middle portion is consistent with the curvature of the circumferential surface of the working anchor 3. In this embodiment, the arched steel ruler is used for easy installation.

[0034] As an optimization solution of the embodiment of the present invention, please refer to Figure 1 and Figure 2 , the magnet 4 is a neodymium iron boron magnet. In this embodiment, the suction force of the neodymium iron boron magnet is greater than that of the ordinary magnet 4, which can avoid inaccurate measurement caused by contact during measurement.

[0035] See also Figure 1 and Figure 2 The embodiment of the present invention provides a device for measuring the shrinkage of a prestressed tendon 9, comprising an anchor pad 8 partially placed in concrete 7 and capable of being installed with the prestressed tendon 9, and a jack 2 for providing tension, a working anchor 3 is arranged between the jack 2 and the anchor pad 8, four identical magnets 4 are adsorbed on the outer step surface of the anchor pad 8, each of the magnets 4 is divided into two adjacent groups, the two groups of magnets 4 are symmetrically arranged with a line perpendicular to the axis of the working anchor 3 as a symmetry axis, and the shape formed by the four magnets 4 is a square, two arched steel rulers 1 are arranged outside the circumferential surface of the working anchor 3, the two arched steel rulers 1 are arranged in parallel and the two arched steel rulers 1 are respectively adsorbed and fixed by the two groups of magnets 4, and the ends of the ruler surfaces of the two arched steel rulers 1 have semi-spherical measuring base points. Preferably, a tool anchor 5 is arranged on the side of the jack 2 away from the anchor pad 8. A limit plate 6 is also arranged between the jack 2 and the working anchor 3. The plane with the semi-spherical measuring base point faces the tool anchor 5 side. In this embodiment, some conventional structures are arranged according to the existing prestress measurement method, such as jack 2, working anchor 3, tool anchor 5, limit plate 6, anchor plate 8, prestressed tendon 9, etc. After the concrete outside the anchor plate 8 that affects the placement of the bow steel ruler 1 is chiseled off, the concrete residue on the step surface of the anchor plate 8 needs to be removed. Then the magnet 4 and the bow steel ruler 1 are arranged. Then L1 and L2 are measured twice. j, L2 and then take the average value. When making the second measurement, return the oil in jack 2 to the oil pressure of 1Mpa. Finally, when using the average value for calculation, calculate the shrinkage of prestressed tendon 9 according to the formula of direct measurement method in Appendix C of GB / T14370-2015 "Anchors, clamps and connectors for prestressed tendons 9", accurate to 0.01mm, and use the length of prestressed tendon 9 outside the bow steel ruler 1 to replace the length of prestressed tendon 9 outside the anchor pad 8 in the direct measurement method in Appendix C of GB / T14370-2015 "Anchors, clamps and connectors for prestressed tendons 9". The length of prestressed tendon 9 outside the bow steel ruler 1 when jack 2 returns oil to the oil pressure of 1Mpa replaces the length of prestressed tendon 9 outside the anchor pad 8 when jack 2 returns oil to the oil pressure of 1Mpa. The measurement is simple and there is no difference in the shrinkage calculation results. This calculation method is a conventional technical means, and the specific calculation formula will not be described in detail here. In addition, semi-spherical vertices are provided at the two ends of each of the arcuate steel rulers 1, and the semi-spherical vertices are used as references, and the two ends of the arcuate steel ruler 1 have semi-spherical measurement base points, and the measurement accuracy is high. Preferably, the calculated shrinkage of the prestressed tendon is rounded off at a rounding interval of 0.1 mm, and the rounded shrinkage of the prestressed tendon is used as the measured value.

[0036] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A method for improving the measurement accuracy of prestressed tendon shrinkage, characterized in that: The steps include: S1, chisel away the concrete outside the anchor plate that affects the placement of the bow steel level, and remove the concrete residue on the step surface of the anchor plate; S2, adsorbing four identical magnets on the outer step surface of the anchor pad, each of the magnets is divided into two adjacent groups, the two groups of magnets are symmetrically arranged with a line perpendicular to the axis of the working anchor as the symmetry axis, and the shape formed by the four magnets is a square; S3, two arched steel rulers are arranged along the circumferential surface of the working anchor, the two arched steel rulers are arranged in parallel and are respectively fixed by two groups of magnets, and the planes with semi-spherical measuring base points at the ends of the ruler surfaces of the two arched steel rulers face the tool anchor side; S4, use a jack to tension the prestressed tendons with 80% of their nominal ultimate tensile strength to achieve tension control and hold the load until the elongation is stable; S5, using a height micrometer without the base, respectively measure the length L1 of the prestressed tendon outside the arched steel ruler, the length L2 of the prestressed tendon between the working anchor and the tool anchor, and the length L3 of the prestressed tendon between the working anchor and the tool anchor using the semi-spherical vertex at the end of the ruler surface of the arched steel ruler as the reference. j , wherein the tool anchor is located on a side of the jack away from the working anchor; S6, when the oil pressure of the jack returns to 1 MPa, use a height micrometer without the base to measure the length L2 of the prestressed tendon outside the bow-shaped steel ruler with the semi-spherical vertex at the end of the ruler surface of the bow-shaped steel ruler as the reference; S7, length L1, length L j , length L2, and calculate the average value, and use the average value to calculate the shrinkage of the prestressed tendon.

2. A method for measuring the shrinkage of prestressed tendons according to claim 1, characterized in that: The middle part of the arched steel ruler is arched and the two ends are straight, and the arc of the arched middle part is consistent with the curvature of the circumferential surface of the working anchor.

3. A method for measuring the shrinkage of prestressed tendons according to claim 1, characterized in that: The magnets are neodymium iron boron magnets.

4. A method for measuring the shrinkage of prestressed tendons according to claim 1, characterized in that: The length L1 of the prestressed tendon outside the bow steel ruler and the length L2 of the prestressed tendon between the working anchor and the tool anchor j , the length L2 of the prestressed tendon outside the bow steel ruler is measured with an accuracy of 0.01mm.

5. A prestressed tendon shrinkage measurement device for the layout measurement method according to claim 1, comprising an anchor plate partially placed in concrete and capable of being used for the installation of prestressed tendons, characterized in that: It also includes a jack for providing pulling force, a tool anchor is provided on the side of the jack away from the anchor plate, a working anchor is provided between the jack and the anchor plate, and a limit plate is provided between the jack and the working anchor. Four identical magnets are adsorbed on the outer step surface of the anchor plate, and each of the magnets is divided into two adjacent groups. The two groups of magnets are symmetrically arranged with a line perpendicular to the axis of the working anchor as the symmetry axis, and the shape formed by the four magnets is a square. Two bow-shaped steel rulers are arranged outside the circumferential surface of the working anchor, the two bow-shaped steel rulers are arranged in parallel and are adsorbed and fixed by the two groups of magnets respectively, and the ends of the ruler surfaces of the two bow-shaped steel rulers have semi-spherical measuring base points.

6. A prestressed tendon shrinkage measurement device as claimed in claim 5, characterized in that: The plane with the semi-spherical measuring base point faces the tool anchor side.

7. A prestressed tendon shrinkage measurement device as claimed in claim 5, characterized in that: The middle part of the arched steel ruler is arched and the two ends are straight, and the arc of the arched middle part is consistent with the curvature of the circumferential surface of the working anchor.

8. A prestressed tendon shrinkage measurement device as claimed in claim 5, characterized in that: The magnets are neodymium iron boron magnets.