Pretreatment method of azobisisobutyronitrile and determination method of trace element content
Pretreatment of azobisisobutyronitrile by ashing method solves the problem of safety and accuracy of trace element content determination, realizes the application of ICP-OES method, ensures the safety and accuracy of measurement, and fills the gap Domestic technology gaps.
Patent Information
- Application Number
- CN202111519282.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-13
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2041-12-13
AI Technical Summary
The existing technology cannot safely and quickly determine the trace element content in azobisisobutyronitrile, especially K, Na, Ca, Mg, Fe and other elements, and the ICP-OES method cannot be directly applied to water-insoluble azobis. Isobutyronitrile samples have the risk of explosion, fire and toxic properties.
Azobisisobutyronitrile is pre-treated by ashing method, and converted into ashing residue by heating to 85-95°C and ashing for 7-8 hours, and the trace element content is measured by ICP-OES method, combined with Container preparation and weighing paper prevent sticking and ensure measurement accuracy and safety.
It achieves safe, rapid pre-treatment and accurate trace element content determination of azobisisobutyronitrile, fills the domestic gap, improves product quality control capabilities, is simple to operate, fast in analysis, low in detection limits, and accurate in test results.
Smart Images

Figure CN114199667B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of detection technology, in particular to a pretreatment method of azobisisobutyronitrile and a method for determining the content of trace elements. Background Art
[0002] The content of trace elements such as K, Na, Ca, Mg, and Fe in azobisisobutyronitrile will directly affect the quality of polyacrylonitrile solution, and further affect the quality of carbon fiber products. Therefore, a simple, fast, and accurate method for determining the content of trace elements in azobisisobutyronitrile is needed.
[0003] At present, there are few domestic manufacturers producing azobisisobutyronitrile, and the amount used by enterprises is also small. Because azobisisobutyronitrile is insoluble in water, releases nitrogen and organic cyanide containing -(CH2)2-C-CN group when decomposed by heat, and decomposes rapidly at a temperature of 100°C, which can cause explosion and fire, is flammable and toxic, and the organic cyanide released by decomposition is harmful to the human body, there are not many related studies on the determination of trace element content in azobisisobutyronitrile in China. At present, there is only a method of using colorimetry to determine the Fe ion content, and this method cannot accurately give the accurate value of the Fe ion content, and cannot meet the requirements for the detection of trace metal ion content in raw and auxiliary materials in the carbon fiber production process. In summary, it is particularly important to develop a method for determining the content of trace elements in azobisisobutyronitrile to fill the domestic gap.
[0004] ICP-OES refers to an inductively coupled plasma emission spectrometer, which can be used for qualitative and quantitative analysis of more than 70 metal elements and some non-metal elements in samples in geology, environmental protection, chemical industry, biology, medicine, food, metallurgy, agriculture, etc. When using ICP-OES for detection, the sample is required to be a completely dissolved, clear and bright liquid. When two or more organic substances are mixed together, it is impossible to quantitatively analyze one of the organic substances.
[0005] Since azobisisobutyronitrile is insoluble in water (it can only be dissolved in organic solvents such as methanol, ethanol, acetone, and mixtures of two or more organic solvents cannot be directly measured by ICP), it does not meet the conditions for direct dissolution and quantitative detection by ICP-OES. Therefore, azobisisobutyronitrile must be pre-treated (digested) before ICP-OES can be used for trace element determination.
[0006] However, due to the above characteristics of azobisisobutyronitrile (such as decomposition upon heat, explosion, ignition, flammability, toxicity, etc.), how to pre-treat (digest) azobisisobutyronitrile safely and quickly is a technical problem. Summary of the invention
[0007] In view of this, the present invention provides a pretreatment method of azobisisobutyronitrile and a method for determining the content of trace elements. The main purpose is to provide a safe and rapid pretreatment method of azobisisobutyronitrile. After pretreatment, the contents of trace elements such as K, Na, Ca, Mg, Fe, etc. in the azobisisobutyronitrile sample can be determined by ICP-OES method.
[0008] In order to achieve the above object, the present invention mainly provides the following technical solutions:
[0009] On the one hand, an embodiment of the present invention provides a pre-treatment method of azobisisobutyronitrile, which comprises the following steps:
[0010] Sample adding step: placing a set mass of azobisisobutyronitrile sample at the bottom of a container to obtain a container containing the sample;
[0011] Ashing step: heating the container containing the sample to an ashing treatment temperature to ashed the azobisisobutyronitrile sample in the container to obtain an ashed residue; wherein the ashing treatment temperature is 85-95° C. and the ashing treatment time is 7-8 hours;
[0012] Preferably, in the sample adding step, the set mass of azobisisobutyronitrile is spread evenly on the bottom of the container.
[0013] Preferably, in the sample adding step: before adding the azobisisobutyronitrile sample to the container, a detachable measuring paper is attached to the inner wall of the container to ensure that when the azobisisobutyronitrile sample is added to the container, the azobisisobutyronitrile sample will not stick to the side wall of the container; preferably, in the container containing the sample: there is a set distance between the azobisisobutyronitrile sample and the side wall of the container; preferably, the set distance is 2-5mm; preferably, the sample is added to the container by multiple sample additions until the mass of the azobisisobutyronitrile sample in the container is the set mass; preferably, the sample adding step is specifically as follows: placing the container on a balance, pressing the tare key, rolling the weighing paper into a cylinder, and placing it in the container so that it is adsorbed on the inner wall of the container; using a sampling spoon to spread the sample to the bottom of the container by multiple sampling and adding; when the mass displayed on the balance is the first mass, stop sampling, pull out the weighing paper, and finally read the mass of the sample as the set mass.
[0014] Preferably, before the sample adding step, the method further comprises: a step of pre-treating the container: sequentially soaking, cleaning and calcining the container in nitric acid; preferably, after soaking the container in nitric acid, cleaning the soaked container with deionized water and ultrapure water, and then calcining the cleaned container to constant weight; preferably, the calcination temperature is 600-900°C; preferably, the calcination step is performed in a muffle furnace.
[0015] Preferably, in the sample adding step: the set mass is 1.000-1.015 g.
[0016] Preferably, the container is made of quartz glass.
[0017] Preferably, in the ashing step: the container containing the sample is placed on an electric heating device, heated to the ashing temperature, and ashing is performed until the white granular azobisisobutyronitrile at the bottom of the container is decomposed and ashed to become colorless and transparent to obtain an ashed residue; preferably, the electric heating device is a temperature-controllable electric heating plate; preferably, when heating the container containing the sample, the temperature of the electric heating device is first set to 85-86°C, and when the temperature is raised to 85-86°C, it is heated at this temperature for 1.5-2.5 hours, and then the temperature of the electric heating device is set to 90-95°C, and heating is continued until the white granular azobisisobutyronitrile sample is completely decomposed; preferably, under the same ashing conditions, a container without a sample is heated to serve as a blank sample.
[0018] On the other hand, an embodiment of the present invention provides a method for determining the content of trace elements in azobisisobutyronitrile, comprising the following steps:
[0019] A sample pretreatment step, pretreating the azobisisobutyronitrile sample using any of the azobisisobutyronitrile pretreatment methods described above;
[0020] Determination steps: preparing a sample solution from the ash residue obtained in the sample pretreatment step; preparing a standard mixed solution; setting the instrument working conditions of the inductively coupled plasma emission spectrometer; selecting a spectral curve; drawing a standard curve; and using the inductively coupled plasma emission spectrometer to measure the sample solution to determine the content of trace elements in the azobisisobutyronitrile sample.
[0021] Preferably, the trace elements include one or more of K, Na, Ca, Mg, and Fe.
[0022] Preferably, the determining step comprises:
[0023] Dissolving the ashing residue with nitric acid to obtain a dissolving solution; and fixing the dissolving solution to obtain a sample solution;
[0024] Prepare multiple standard mixed solutions, select working conditions and spectral curves, and draw standard curves;
[0025] The content of trace elements in azobisisobutyronitrile was determined using the same working conditions and spectral lines as those used to draw the standard curve.
[0026] Preferably, the sample solution is transparent and clear.
[0027] Preferably, the mass fraction of the nitric acid is 2-5%.
[0028] Preferably, the nitric acid is prepared from UPS electronic grade standard acid.
[0029] Preferably, after constant volume, the volume of the sample solution is 10-20 mL.
[0030] Preferably, the concentrations of the elements to be tested in the multiple standard mixed solutions increase in sequence; wherein the elements to be tested include one or more of K, Na, Ca, Mg, and Fe; preferably, eight standard mixed solutions are prepared; wherein the concentration of the elements to be tested in the first standard mixed solution is 0 mg / L, the concentration of each element to be tested in the second standard mixed solution is 0.5 mg / L, the content of each element to be tested in the third standard mixed solution is 1 mg / L, the content of each element to be tested in the fourth standard mixed solution is 2 mg / L, the content of each element to be tested in the fifth standard mixed solution is 4 mg / L, the content of each element to be tested in the sixth standard mixed solution is 6 mg / L, the content of each element to be tested in the seventh standard mixed solution is 8 mg / L, and the content of each element to be tested in the eighth standard mixed solution is 10 mg / L. (Here, the concentration of the standard mixed solution can also be prepared according to the content range of each trace element in the actual sample and the concentration difference can be selected).
[0031] Preferably, the working conditions of the inductively coupled plasma emission spectrometer are set as follows: the power is set to 1500W; the observation height is set to 12mm; the peristaltic pump speed is set to 45r / min; the auxiliary device is set to 0.5L / min; the nebulizer is set to 0.6L / min; and the injection cleaning time is set to 30s. Here, the instrument working conditions can be appropriately adjusted according to the actual instrument model.
[0032] Preferably, the spectral lines are selected as follows: K, 766.491 nm; Na, 589.592 nm; Ca, 422.673 nm; Mg, 285.213 nm, Fe, 238.204 nm.
[0033] Preferably, a standard curve is drawn with the mass concentration of the element to be determined in the standard mixed solution in mg / L as the abscissa and the emission intensity as the ordinate, and the correlation coefficient of the standard curve is greater than 0.999.
[0034] Compared with the prior art, the pretreatment method of azobisisobutyronitrile and the method for determining the content of trace elements of the present invention have at least the following beneficial effects:
[0035] On the one hand, an embodiment of the present invention provides a pretreatment method of azobisisobutyronitrile, in which azobisisobutyronitrile is pretreated by an ashing method. The present invention proposes requirements for the sample addition step (i.e., spreading a set mass of azobisisobutyronitrile sample on the bottom of a container) and conditions for the ashing step (i.e., the ashing temperature is 85-95° C., and the ashing time is 7-8 hours). This not only can safely and quickly pretreat azobisisobutyronitrile, but also can ensure the accuracy of subsequent ICP-OES determination of its trace elements.
[0036] Furthermore, in a pretreatment method of azobisisobutyronitrile provided in an embodiment of the present invention, before adding a sample to a container, a weighing paper is attached to the inner wall of the container, so as to prevent the sample from adhering to the inner wall of the container and avoid incomplete decomposition of the sample adhering to the inner wall of the container in the subsequent ashing step (because the temperature of the inner wall of the container is lower than the temperature of the bottom). Furthermore, when adding the sample, the sample should be laid flat in an area of about 2-5 mm from the side wall to avoid bringing the sample to the inner wall of the container when the weighing paper is removed.
[0037] Furthermore, the pretreatment method of azobisisobutyronitrile provided in an embodiment of the present invention further includes a step of pretreating the container before the sample adding step. By pretreating the container (immersing, cleaning, and calcining to constant weight in nitric acid), moisture and impurities adsorbed by the container can be eliminated to eliminate the systematic error of subsequent measurements.
[0038] Furthermore, in the pretreatment method of azobisisobutyronitrile provided in an embodiment of the present invention, a quartz beaker is selected as the container, so as to facilitate observation of the decomposition and ashing of the sample in the subsequent ashing step.
[0039] Further, in a pretreatment method of azobisisobutyronitrile provided by an embodiment of the present invention, in the ashing step, when heating the container containing the sample, the temperature of the electric heating device is first set to 85-86°C, and when the temperature is raised to 85-86°C, it is heated at this temperature for 1.5-2.5 hours, and then the temperature of the electric heating device is set to 90-95°C, and the heating is continued until the white granular azobisisobutyronitrile sample is completely decomposed. Regarding the above steps, the heating decomposition is first carried out at a slightly lower temperature of 85-86°C, the purpose of which is to ensure that the accumulated samples are slowly decomposed, to avoid local rapid decomposition caused by excessive heating, and to cause splashing, explosion and the like; after decomposing for 1.5-2.5 hours, a part of the accumulated samples is decomposed, and the samples become thinner, and the temperature can be appropriately increased without causing the above phenomenon.
[0040] On the other hand, the embodiment of the present invention provides a method for determining the content of trace elements in azobisisobutyronitrile, comprising the following steps: pre-treating the azobisisobutyronitrile sample using the pre-treatment method of the azobisisobutyronitrile described above; preparing the ashing residue obtained by the sample pre-treatment step into a sample solution, preparing a standard mixed solution, and measuring it using an inductively coupled plasma emission spectrometer to measure the content of trace elements in the azobisisobutyronitrile sample. Here, on the one hand, by pre-treating the azobisisobutyronitrile sample using the pre-treatment method of the azobisisobutyronitrile described above, azobisisobutyronitrile can be determined by ICP-OES method The content of trace elements (including K, Na, Ca, Mg, Fe) in azobisisobutyronitrile, and the setting of the working conditions of the subsequent inductively coupled plasma emission spectrometer, the selection of spectral lines, the preparation of standard mixed solutions, etc., ensures the measurement accuracy of trace elements.
[0041] In summary, the present invention adopts ICP-OES method for the first time to determine the content of trace elements such as K, Na, Ca, Mg, and Fe in azobisisobutyronitrile samples, which fills the domestic gap and helps manufacturers using the raw materials to fully understand the purity of the raw materials and improve the quality control ability of the products. The sample detection operation steps using this method are safe, simple, fast, the detection limit is low, and the detection results are accurate.
[0042] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention and implement it according to the contents of the specification, the following is a detailed description of the preferred embodiments of the present invention in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] Figure 1 It is a schematic diagram of an operation of adding an azobisisobutyronitrile sample into a container (quartz beaker) provided by an embodiment of the present invention;
[0044] Figure 2It is a burning curve diagram of the quartz beaker provided in the embodiment of the present invention. DETAILED DESCRIPTION
[0045] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention application are described in detail below in conjunction with the accompanying drawings and preferred embodiments. In the following description, different "one embodiment" or "embodiment" does not necessarily refer to the same embodiment. In addition, specific features, structures, or characteristics in one or more embodiments may be combined in any suitable form.
[0046] For azobisisobutyronitrile, when using ICP-OES method to determine its trace element content, the azobisisobutyronitrile sample needs to be pre-treated first. However, because azobisisobutyronitrile is insoluble in water, it will release nitrogen and organic cyanide containing -(CH2)2-C-CN group when decomposed by heat, and it will decompose rapidly at 100°C, which can cause explosion and fire, and it is flammable and toxic. The organic cyanide released by decomposition is very harmful to the human body. Therefore, how to pre-treat it safely and quickly is particularly important.
[0047] Based on the above technical problems, the present invention proposes a pretreatment method of azobisisobutyronitrile, which specifically comprises the following steps:
[0048] Sample adding step: spread a set mass of azobisisobutyronitrile sample evenly on the bottom of the container to obtain a container containing the sample.
[0049] Specifically, in this step, the azobisisobutyronitrile sample is first stirred evenly, shrunk, and accurately weighed, and the sample is spread on the bottom of the container. The sample should be fully stirred, shrunk, and 0.1g of sample should be weighed to an accuracy of 0.1mg; preferably, the mass of each sample is 1.000-1.015g (it should be noted here that the purpose of controlling each sample in this range is: (1) Under the premise of ensuring a certain sample amount, the sample spread on the bottom of the beaker is as small and thin as possible to shorten the heating decomposition time; (2) Under the condition that the mass of parallel samples is basically the same, the repeatability of the test results is better, and the sample amount can be appropriately relaxed). Preferably, there are 2-3 parallel samples. Among them, if Figure 1 As shown, before adding the sample to the container 1, a layer of weighing paper 2 should be added to the inner wall of the container 1 in advance to ensure that the inner wall of the container is not stained with the azobisisobutyronitrile sample. Further, when adding the sample, the sample 3 should be evenly spread to the bottom of the container 1 and at a certain distance from the side wall. Preferably, the sample is spread in an area 2-5 mm away from the side wall to avoid the sample being taken away from the side wall when the weighing paper is removed (to avoid the phenomenon of incomplete ashing of the sample stained with the side wall due to the temperature of the container side wall being lower than the bottom temperature).
[0050] More specifically, you should first take a prepared container, place it on the balance, and press the tare button. Roll the weighing paper into a tube and place it in the container so that it sticks to the inner wall of the container. This is to prevent the sample from adhering to the inner wall of the container when it is added to the container. Furthermore, add the sample in small amounts and multiple times; use a sampling spoon to take a small amount of sample and insert it into the container from the upper side, gently shake the sampling spoon, and evenly spread the sample to the bottom of the container. Furthermore, the sample should be added to the middle of the container first, and then slowly spread to the sides (see Figure 1 As shown). Further, when the balance shows the first mass (about 1.005-1.018g), stop adding the sample. At this time, gently pull up the weighing paper, roll it up while pulling, and quickly pull it out of the container. Further, after the balance is stable, read the sample mass as the set mass (1.000-1.015g).
[0051] In addition, after the first sample is weighed, two other parallel samples are weighed according to the above method (ie, multiple containers containing samples are prepared).
[0052] Preferably, the container in the present invention is a quartz beaker, so as to facilitate observation of the decomposition and ashing of the sample during the ashing step.
[0053] Preferably, before the step of adding the sample, the step of pre-treating the container is also included: soaking the container in nitric acid, washing it, and burning it to constant weight. Specifically, soak the container in (1+1) nitric acid for 24 hours or soak it in concentrated nitric acid for 6 hours. Further, clean it with deionized water or ultrapure water ultrasonically, and then burn it in a muffle furnace to constant weight (burning temperature is 600-900°C) for later use (wherein, the burning curve is as shown in Figure 2 As shown). In addition, after the test, first use acetone or ethanol to ultrasonically clean it once, then repeat the above cleaning steps and set it aside. It should be noted here that the container (quartz beaker) will absorb a certain amount of water and other impurities when placed at room temperature. Under high temperature conditions, the adsorbed water and other impurities will volatilize or burn away, eliminating systematic errors. Therefore, before quantitative analysis, it is generally necessary to dry or burn it to constant weight to eliminate systematic errors.
[0054] Ashing step: heating the container containing the sample to an ashing treatment temperature to ashed the azobisisobutyronitrile sample in the container to obtain an ashed residue; wherein the ashing treatment temperature is 85-95°C and the ashing treatment time at the ashing treatment temperature is 7-8 hours.
[0055] The specific step is: place the container (quartz beaker) containing the sample in the middle of an electric heating device (preferably a temperature-controllable electric heating plate), open the fume hood, set the heating temperature, and slowly heat until the white granular azobisisobutyronitrile sample at the bottom of the container is completely decomposed and ashed, and there is no white granule at the bottom of the container.
[0056] Preferably, multiple containers containing samples (parallel samples) and empty containers without samples (blank samples) are placed in the middle of the electric heating device, the fume hood is turned on, the temperature of the electric heating device is first set to 85-86°C, and the timing is started when the electric heating plate is heated to this temperature. After 1.5-2.5 hours (preferably 2 hours), the heating temperature is adjusted to 90-95°C, and the heating is continued slowly. Further, after the heating time reaches 7-8 hours (starting from the start of the timing), it is observed that all the white granular azobisisobutyronitrile samples at the bottom of the container are completely decomposed, the ashing is completed, and the heating is stopped. Let it cool.
[0057] Preferably, when the temperature of the electric heating device rises above 90°C, the ashing of the sample should be observed every half an hour, so that timely emergency treatment can be facilitated when unexpected situations such as rapid decomposition of the sample occur.
[0058] On the other hand, an embodiment of the present invention provides a method for determining the content of trace elements in azobisisobutyronitrile, comprising the following steps:
[0059] In the sample pretreatment step, the azobisisobutyronitrile sample is pretreated by the azobisisobutyronitrile pretreatment method described above.
[0060] Determination step: prepare the ash residue obtained in the sample pretreatment step into a sample solution; prepare a standard mixed solution; set the instrument working conditions of the inductively coupled plasma emission spectrometer; select a spectral curve; draw a standard curve; use the inductively coupled plasma emission spectrometer to measure the sample solution and determine the content of trace elements in the azobisisobutyronitrile sample. Among them, the trace elements are one or more of K, Na, Ca, Mg, and Fe.
[0061] Among them, the step of preparing the sample solution: It can be known from the above-mentioned pre-treatment method of azobisisobutyronitrile that after the ashing step is completed, the azobisisobutyronitrile sample in the container is converted into a residue after ashing. In this step, nitric acid is used to dissolve the residue after ashing to obtain a dissolved solution. Then the dissolved solution in the container is transferred to a plastic centrifuge tube and fixed to a set volume to obtain a sample solution. Further, this step is specifically: after the ashing step in the above-mentioned pre-treatment method of azobisisobutyronitrile is completed for a few minutes (about 10 minutes), when the container is touchable, pour about 3mL of nitric acid with a concentration of 2-5% into the container to dissolve the residue after ashing, and then use nitric acid with a concentration of 2-5% to clean the bottom and inner wall of the container 2-3 times, and transfer the dissolved solution to a 10-20mL plastic centrifuge tube. Finally, nitric acid with a concentration of 2-5% is fixed to the scale line. Further, the obtained sample solution is transparent and clear. Further, the nitric acid used is prepared by UPS electronic grade standard acid. In addition, the container after use should be ultrasonically cleaned once with acetone or ethanol, then rinsed with deionized water, ultrasonically cleaned once with ultrapure water, and dried in a muffle furnace at 600-900°C to constant weight for use.
[0062] In this step, the steps of preparing the standard mixed solution are as follows: first, single element standard solutions of K, Na, Ca, Mg, Fe, etc., each with a content of 1000 mg / L, are used to prepare mixed standard working solutions of K, Na, Ca, Mg, Fe with contents of 0 mg / L, 0.5 mg / L, 1.0 mg / L, 2.0 mg / L, 4.0 mg / L, 6.0 mg / L, 8.0 mg / L, and 10.0 mg / L, respectively (i.e., standard mixed solutions), and transfer them into plastic bottles or centrifuge test tubes for later use. That is, the content of each element to be measured in the first standard mixed solution is 0 mg / L, the content of each element to be measured in the second standard mixed solution is 0.5 mg / L, the content of each element to be measured in the third standard mixed solution is 1 mg / L, the content of each element to be measured in the fourth standard mixed solution is 2 mg / L, the content of each element to be measured in the fifth standard mixed solution is 4 mg / L, the content of each element to be measured in the sixth standard mixed solution is 6 mg / L, the content of each element to be measured in the seventh standard mixed solution is 8 mg / L, and the content of each element to be measured in the eighth standard mixed solution is 10 mg / L.
[0063] In addition, the standard mixed solution can also be prepared according to the method of GB / T602; or the concentration range of the standard mixed solution can be selected according to the content of each element to be measured in the sample to be measured, and the single element standard solution can be selected according to the type of element to be measured.
[0064] In this step: the working conditions of the inductively coupled plasma emission spectrometer are set, the spectral lines are selected, the standard curve is drawn, and the content of trace elements in azobisisobutyronitrile in the sample is determined using the same working conditions and spectral lines.
[0065] The instrument working conditions of the inductively coupled plasma emission spectrometer are set as follows: power is set to 1500W; observation height is set to 12mm; peristaltic pump speed is set to 45r / min; auxiliary device is set to 0.5L / min; nebulizer is set to 0.6L / min; injection cleaning time is set to 30s. Here, the instrument working conditions can be appropriately adjusted according to the actual instrument model.
[0066] Among them, the spectral lines (recommended wavelengths) are selected as: 766.491nm (K), 589.592 (Na), 422.673 (Ca), 285.213 (Mg), 238.204 (Fe).
[0067] Among them, the mass concentration of the element to be measured in the standard mixed solution is mg / L as the horizontal axis, and the emission intensity is the vertical axis to draw the standard curve of the corresponding element. Furthermore, the correlation coefficient of the standard curve should be greater than 0.999. Finally, according to the working conditions of the instrument, the contents of trace elements such as K, Na, Ca, Mg, and Fe in the azobisisobutyronitrile sample solution were determined respectively.
[0068] The present invention is further described below by specific experimental examples:
[0069] Example 1
[0070] In this embodiment, the azobisisobutyronitrile samples of ××× batches were pre-treated, and then the contents of trace elements such as K, Na, Ca, Mg, and Fe in the azobisisobutyronitrile samples were determined using an inductively coupled plasma emission spectrometer. Specifically, the following steps are included:
[0071] 1) Pre-treatment of the container: Take 4 unused 50 mL quartz beakers (i.e., the container in this embodiment is a quartz beaker), soak them in (1+1) nitric acid for 24 hours, rinse them with tap water and deionized water for several times, and then ultrasonically clean them with ultrapure water. Then, Figure 2 The cleaned quartz beaker was burned in a muffle furnace to constant weight according to the heating curve. Finally, it was taken out and placed in a desiccator to cool for later use.
[0072] 2) Sample addition steps:
[0073] a) Stir the azobisisobutyronitrile sample thoroughly and evenly, and reduce the sample by quartering method until it is reduced to about 2-3g, and set aside.
[0074] b) Take a quartz beaker, place it on the balance, and press the tare button. Figure 1 As shown, roll the weighing paper 2 into a tube and place it in the container 1 (quartz beaker) so that it is attached to the inner wall of the container 1 (quartz beaker); use a sampling spoon to take a small amount of samples from the shrunk sample multiple times, insert it into the quartz beaker from the upper side, and gently shake the sampling spoon to evenly spread a layer of the sample to the bottom of the quartz beaker. When loading the sample, pay attention to adding the sample to the middle of the quartz beaker first, and then slowly spread it to the edge. When the balance shows a mass of 1.004g, stop adding quartz. Tap the outer wall of the weighing paper while quickly pulling it out of the quartz beaker. After the balance stabilizes, read the mass of the sample as 1.002g.
[0075] Similarly, weigh another two parallel samples of 1.002g and 1.001g respectively according to the above method.
[0076] 3) Ashing step: Place the quartz beaker containing the sample in the middle of a temperature-controlled electric hot plate. At the same time, take an empty quartz beaker and place it in the middle of the electric hot plate as a blank sample. Open the fume hood, set the temperature of the hot plate to 85°C, start timing when the hot plate heats up to 85°C, set the temperature of the hot plate to 93°C after 2 hours, and continue to heat slowly. During this period, observe the decomposition of the sample every half an hour. After 7.8 hours from the start of timing, it was observed that all the white granular azobisisobutyronitrile samples at the bottom of the quartz beaker were completely decomposed, and the sample at the bottom of the quartz beaker became colorless and transparent. Stop heating and let it dry for 10 minutes.
[0077] 4) Steps for preparing the sample solution: add 3 mL of 2% nitric acid to each of the four quartz beakers to dissolve the residue after ashing, then wash the bottom and inner wall of the quartz beakers 2-3 times with 2% nitric acid, transfer the sample solution to a 15 mL plastic centrifuge test tube, and finally dilute to the mark with 2% nitric acid to obtain a transparent and clear sample solution.
[0078] 5) Determination steps (ICP detection steps):
[0079] a) First, use single element standard solutions of K, Na, Ca, Mg, Fe, etc., each with a content of 1000 mg / L, to prepare mixed standard working solutions of K, Na, Ca, Mg, Fe with contents of 0 mg / L, 0.5 mg / L, 1.0 mg / L, 2.0 mg / L, 4.0 mg / L, 6.0 mg / L, 8.0 mg / L, and 10.0 mg / L, respectively (i.e., standard mixed solutions), and transfer them into centrifuge test tubes for later use.
[0080] That is, the content of each element to be measured in the first standard mixed solution is 0 mg / L, the content of each element to be measured in the second standard mixed solution is 0.5 mg / L, the content of each element to be measured in the third standard mixed solution is 1 mg / L, the content of each element to be measured in the fourth standard mixed solution is 2 mg / L, the content of each element to be measured in the fifth standard mixed solution is 4 mg / L, the content of each element to be measured in the sixth standard mixed solution is 6 mg / L, the content of each element to be measured in the seventh standard mixed solution is 8 mg / L, and the content of each element to be measured in the eighth standard mixed solution is 10 mg / L.
[0081] b) Set the instrument working conditions of the inductively coupled plasma emission spectrometer: the power is set to 1500 W; the observation height is set to 12 mm; the peristaltic pump speed is set to 45 r / min; the auxiliary device is set to 0.5 L / min; the nebulizer is set to 0.6 L / min; the injection cleaning time is set to 30 s.
[0082] c) The standard curve of the corresponding element was drawn with the mass concentration of the element to be determined in the standard mixed solution in mg / L as the abscissa and the emission intensity as the ordinate. The correlation coefficient of the standard curve was 0.9998.
[0083] d) Finally, according to the working conditions of the instrument, the contents of trace metal elements such as K, Na, Ca, Mg, and Fe in the azobisisobutyronitrile sample solution were measured at wavelengths of 766.491 nm (K), 589.592 (Na), 422.673 (Ca), 285.213 (Mg), and 238.204 (Fe). The measurement results are shown in Table 1.
[0084] Table 1
[0085]
[0086] In summary, the pre-treatment method of azobisisobutyronitrile and the determination method of trace element content provided by the embodiment of the present invention fill the domestic method blank of accurately measuring the content of trace elements in azobisisobutyronitrile. In addition, compared with the current domestic detection method of measuring the content of Fe ions in azobisisobutyronitrile using colorimetry, the present invention has the advantages of high safety, low sample blank, low detection limit and high accuracy.
[0087] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention still falls within the scope of the technical solution of the present invention.
Claims
1. A pre-treatment method for azobisisobutyronitrile, characterized in that: The steps include: The sample adding step is as follows: placing a set mass of azobisisobutyronitrile sample at the bottom of a container to obtain a container containing the sample; wherein the set mass is 1.000-1.015 g; the set mass of azobisisobutyronitrile is spread flat on the bottom of the container; in the container containing the sample: there is a set distance between the azobisisobutyronitrile sample and the side wall of the container; the set distance is 2-5 mm; wherein the sample adding step is specifically as follows: placing the container on a balance, pressing the tare key, rolling the weighing paper into a cylinder, placing it in the container so that it is adsorbed on the inner wall of the container; using a sampling spoon to spread the sample to the bottom of the container in a manner of multiple sampling and adding; when the mass displayed on the balance is the first mass, stopping sampling, pulling out the weighing paper, and finally reading the mass of the sample as the set mass; Ashing step: heating the container containing the sample to an ashing treatment temperature to ashed the azobisisobutyronitrile sample in the container to obtain an ashed residue; wherein the ashing treatment temperature is 85-95° C. and the ashing treatment time is 7-8 hours; Wherein, in the ashing step: placing the container containing the sample on an electric heating device, heating it to the ashing temperature, and performing an ashing process until the white granular azobisisobutyronitrile at the bottom of the container is decomposed and ashed to become colorless and transparent, thereby obtaining an ashing residue; When heating the container containing the sample, first set the temperature of the electric heating device to 85-86°C. When the temperature reaches 85-86°C, heat at this temperature for 1.5-2.5 hours. Then, set the temperature of the electric heating device to 90-95°C and continue heating until the white granular azobisisobutyronitrile sample is completely decomposed.
2. A pre-treatment method of azobisisobutyronitrile according to claim 1, characterized in that, Before the sample adding step, the method further comprises: The steps of pre-treating the container are as follows: soaking, cleaning and burning the container in nitric acid in sequence.
3. A pre-treatment method of azobisisobutyronitrile according to claim 2, characterized in that, After the container is soaked in nitric acid, the soaked container is cleaned with deionized water and ultrapure water, and then the cleaned container is burned to a constant weight.
4. A pre-treatment method of azobisisobutyronitrile according to claim 3, characterized in that, The temperature of the calcination treatment is 600-900°C.
5. A pre-treatment method of azobisisobutyronitrile according to claim 3, characterized in that, The calcination step is carried out in a muffle furnace.
6. A pre-treatment method of azobisisobutyronitrile according to any one of claims 1 to 5, characterized in that: In the sample loading step: The container is a quartz beaker.
7. A pre-treatment method for azobisisobutyronitrile according to any one of claims 1 to 5, wherein in the ashing step: Under the same ashing conditions, heat the container without sample to serve as a blank sample.
8. A method for determining the content of trace elements in azobisisobutyronitrile, characterized in that: It includes the following steps: A sample pretreatment step, pretreating the azobisisobutyronitrile sample using the azobisisobutyronitrile pretreatment method according to any one of claims 1 to 7; Determination steps: preparing a sample solution from the ash residue obtained in the sample pretreatment step; preparing a standard mixed solution; setting the instrument working conditions of the inductively coupled plasma emission spectrometer; selecting a spectral curve; drawing a standard curve; and using the inductively coupled plasma emission spectrometer to measure the sample solution to determine the content of trace elements in the azobisisobutyronitrile sample.
9. The method for measuring the content of trace elements in azobisisobutyronitrile according to claim 8, characterized in that: The trace elements include one or more of K, Na, Ca, Mg and Fe.
10. The method for determining the content of trace elements in azobisisobutyronitrile according to claim 8, characterized in that: The measuring step comprises: Dissolving the ashing residue with nitric acid to obtain a dissolving solution; and fixing the dissolving solution to obtain a sample solution; Prepare standard mixed solutions of multiple concentrations, select working conditions and spectral curves, and draw standard curves; The content of trace elements in azobisisobutyronitrile was determined using the same working conditions and spectral lines as those used to draw the standard curve.
11. The method for determining the content of trace elements in azobisisobutyronitrile according to claim 10, characterized in that: The sample solution is transparent and clear; and / or The mass fraction of the nitric acid is 2-5%; and / or The nitric acid is prepared from UPS electronic grade standard acid; and / or After constant volume, the volume of the sample solution is 10-20 mL.
12. The method for determining the content of trace elements in azobisisobutyronitrile according to claim 10, characterized in that: The concentrations of the elements to be tested in the multiple standard mixed solutions increase in sequence; wherein the elements to be tested include one or more of K, Na, Ca, Mg, and Fe.
13. The method for determining the content of trace elements in azobisisobutyronitrile according to claim 12, characterized in that: Eight standard mixed solutions are prepared; wherein the concentration of the element to be measured in the first standard mixed solution is 0 mg / L, the concentration of each element to be measured in the second standard mixed solution is 0.5 mg / L, the content of each element to be measured in the third standard mixed solution is 1 mg / L, the content of each element to be measured in the fourth standard mixed solution is 2 mg / L, the content of each element to be measured in the fifth standard mixed solution is 4 mg / L, the content of each element to be measured in the sixth standard mixed solution is 6 mg / L, the content of each element to be measured in the seventh standard mixed solution is 8 mg / L, and the content of each element to be measured in the eighth standard mixed solution is 10 mg / L.
14. The method for determining the content of trace elements in azobisisobutyronitrile according to claim 10, characterized in that: The working conditions of the inductively coupled plasma emission spectrometer are set as follows: the power is set to 1500W; the observation height is set to 12mm; the peristaltic pump speed is set to 45r / min; the auxiliary device is set to 0.5L / min; the nebulizer is set to 0.6L / min; the injection cleaning time is set to 30s; and / or The spectral lines are selected as follows: K, 766.491nm; Na, 589.592nm; Ca, 422.673nm; Mg, 285.213nm, Fe, 238.204nm; and / or A standard curve was drawn with the mass concentration of the measured element in the standard mixed solution in mg / L as the abscissa and the emission intensity as the ordinate. The correlation coefficient of the standard curve was greater than 0.999.