A method for preparing a stepped semi-copper via PCB

By using the split plating and drilling methods in the preparation process of step hole PCB, the high-temperature glue sticking process is eliminated, and the problems of complex production and low yield in the existing technology are solved, and the product quality and efficiency are improved.

CN114401595BActive Publication Date: 2024-11-29VICTORY GIANT TECH HUIZHOU CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202210000805.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-04
Publication Date
2024-11-29
Estimated Expiration
2042-01-04

AI Technical Summary

Technical Problem

When making step-hole PCBs, the existing technology is difficult to meet customers' high requirements for Stub residual piles and signal design, and the production process is complex, the yield is low, and there are problems with low efficiency of applying high-temperature glue and product quality.

Method used

Using the method of split plating and drilling, the outer sealing pattern and pattern plating holes are performed respectively during the preparation process of L1-L4 and L5-L6 layers, and the first and second drilling is performed before and after the copper plate is submerged. The high-temperature glue paste process has been cancelled and the production process has been simplified.

Benefits of technology

It improves product yield and quality, simplifies production processes, improves production efficiency, and avoids the in-depth and residual problems of potions caused by applying high-temperature glue.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to a preparation method of a stepped semi-copper hole PCB, which adopts a separate plating and a separate drilling method to prepare the stepped semi-copper hole, and comprises the following steps: S1: including copper plated board and inner layer pattern, performing outer layer sealing pattern after copper plated board and before inner layer pattern, while sealing the outer layer, exposing the hole to be copper plated, then performing pattern plating on the exposed hole, thickening the hole copper, and no need to apply high temperature glue after the inner layer pattern; S2: performing inner layer pattern making on L5-L6 layers respectively; S3: pressing the L1-L4 laminated semi-finished product obtained in steps S1 and S2, and the L5 and L6 layers with inner layer patterns together, and performing the first drilling and the second drilling respectively before and after copper plated board, without applying high temperature glue before copper plated board, and performing forming gong groove, laser drilling, and outer layer circuit pattern in sequence after the second drilling to obtain a stepped semi-copper hole PCB. The preparation method of the stepped semi-copper via PCB of the present invention has the advantages of good product quality, high yield rate and high production efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of PCB preparation, and in particular to a method for preparing a stepped semi-copper via PCB. Background Art

[0002] With the development of 5G products, the design requirements for PCB signals are getting higher and higher. In order to meet the conduction and model requirements of the products, back drilling and other methods are often needed to meet the product needs. Back drilling has Stub stumps. The existing Stub drilling capacity is 5-8mil. When the customer's interlayer thickness is less than 5mil, or the Stub requirement is 0mil, the existing back drilling method cannot meet the needs. Other production methods are needed to meet this.

[0003] At present, for the production of stepped hole PCB, taking the 6-layer board as an example, the L1-L4 layer holes require copper plating, and the L4 layer stepped groove position, the L4 layer needs to retain the PAD, and the L4-L6 layer position is designed without copper. The existing pulse hole plating method cannot meet the demand due to the large aspect ratio of the L1-L4 layer, and the back drilling method has stub residues. The existing practice adopts back drilling or split plating, which has a complex production process and low yield. In addition, when the L1-L4 layer is produced, it is necessary to apply high-temperature glue to the L1-L4 layer position before pressing. In addition, when the L1-L6 layer is produced, it is necessary to apply high-temperature glue to the back-drilled hole position of the L1-L4 layer after drilling. Since the high-temperature glue cannot be applied by machine, manual glue application will have low operation efficiency and problems such as crooked application and scrapping. In addition, the subsequent glue removal will corrode the colloid, which is easy to cause the liquid to penetrate deeply and cause residue, thus affecting the product quality and resulting in low yield. Summary of the invention

[0004] The present invention provides a method for preparing a stepped semi-copper via PCB with good product quality, high yield and high production efficiency.

[0005] In order to achieve the above purpose, the following technical solutions are adopted.

[0006] A method for preparing a stepped semi-copper via PCB, which adopts a separate plating and a separate drilling method to prepare the stepped semi-copper via, specifically comprising the following steps:

[0007] S1: Preparation of L1-L4 layers, including copper-plated board and inner layer patterning, outer layer sealing patterning after copper-plated board and before inner layer patterning, while sealing the outer layer, the holes to be copper-plated are exposed, and then the exposed holes are plated with patterns to thicken the hole copper, and no high-temperature glue is required after the inner layer patterning to obtain L1-4 layer laminated semi-finished products; the outer layer sealing pattern and pattern plated holes are added after copper-plated board, and after the inner layer patterning is made, it is not necessary to seal the L1-L4 layer positions with high-temperature glue, which effectively ensures the sealing quality, reduces the problem of residual copper biting caused by the sealing of the holes with high-temperature glue in the prior art, and effectively improves the product yield;

[0008] S2: Preparation of L5-L6 layer, making inner layer pattern of L5 layer, obtaining L5-L6 layer with inner layer pattern;

[0009] S3: Overall preparation of L1-L6 layers, pressing together the L1-L4 laminated semi-finished products obtained in steps S1 and S2, and the L5 and L6 layers with inner layer patterns, and performing the first drilling and the second drilling respectively before and after the copper plate is electroplated, without the need to apply high-temperature glue before the copper plate is electroplated, and after the second drilling, forming gong grooves, laser drilling, and outer layer circuit patterns are performed in sequence to obtain a stepped semi-copper hole PCB. The first drilling and the second drilling before and after the copper plate in this step make it unnecessary to apply high-temperature glue in the preparation process, and the high-temperature glue application process before the copper plate is electroplated and the high-temperature glue tearing process after the copper plate is electroplated are cancelled, which effectively avoids the problems of hole position height difference, glue flow holes, and uneven board thickness after pressing in the prior art, and effectively improves product quality.

[0010] Furthermore, in step S1, the copper plating thickness of the copper plate in the electroplating process is 25 μm.

[0011] Furthermore, the pattern hole plating process in step S1 thickens the hole copper by 25 μm.

[0012] Furthermore, step S1 also includes film stripping and resin plugging processes between the pattern plated holes and the inner layer patterns.

[0013] Furthermore, the resin plugging is to plug the blind holes of the L1-L4 layers with resin ink, and then grind them flat with a sanding belt.

[0014] Furthermore, in step S3, the first drilling is to drill the via holes, and the second drilling is to drill the holes at the L1-L4 positions, and the drill bit is 0.05 mm smaller than the drill bit for the first drilling.

[0015] Furthermore, the forming gong groove in step S3 uses a controlled depth gong to drill the L4-L6 layer stepped holes with controlled depth, leaving a bottom thickness of 3mil to 4mil.

[0016] Furthermore, the laser drilling in step S3 is used to remove the residual thickness of the forming gong groove process.

[0017] Compared with the prior art, the method for preparing the stepped semi-copper via PCB of the present invention has the following beneficial effects:

[0018] First, the product yield is high. In the preparation method of the stepped semi-copper hole PCB of the present invention, an outer layer sealing pattern and a pattern plated hole are added between the copper plate and the inner layer pattern in step S1. After the outer layer sealing pattern and the pattern plated hole are added to the copper plate, there is no need to apply high temperature glue to seal the L1-L4 layer positions after the inner layer pattern is made, which effectively ensures the sealing quality and reduces the problem of residual copper biting caused by the high temperature glue sealing in the prior art, thereby effectively improving the product yield.

[0019] Second, the product quality is good. In the preparation method of the stepped semi-copper hole PCB of the present invention, the drilling process before the copper plate is electroplated is divided into two drilling processes in step S3, and the drilling processes are respectively performed before and after the copper plate is electroplated. The high-temperature glue sticking process before the copper plate is electroplated and the high-temperature glue tearing process after the copper plate is electroplated are cancelled, which effectively avoids the problems of the hole position height difference, the glue flow hole, and the uneven board thickness after the pressing in the prior art, and effectively improves the product quality;

[0020] Third, the production efficiency is high. The preparation method of the stepped semi-copper hole PCB of the present invention adds an outer layer sealing hole pattern and a pattern plated hole between the copper plate and the inner layer pattern in step S1, and splits the drilling process before the copper plate into two drilling processes in step S3, and performs them before and after the copper plate, thereby eliminating two high-temperature glue sticking processes in the prior art that cannot be machine-operated and can only be manually operated, thereby effectively improving the production efficiency and yield rate, and improving the production quality.

[0021] The preparation method of the stepped semi-copper via PCB of the present invention can meet the requirements and reduce the production cost without affecting the customer's functions by improving and optimizing the production process, thereby improving the problems of residual piles and residual glue in the stepped semi-copper vias and effectively improving the product quality and yield. DETAILED DESCRIPTION

[0022] The preparation method of the stepped half copper via PCB of the present invention will be further described in detail below in conjunction with specific embodiments.

[0023] A method for preparing a stepped semi-copper via PCB. The present invention takes a 6-layer board as an example. In this embodiment, a step semi-copper via is prepared by a separate plating and a separate drilling method, which specifically includes the following steps:

[0024] S1: Preparation of L1-L4 layers. In this embodiment, the process flow of this step is pre-process → lamination → drilling → copper plate electroplating → outer layer sealing pattern → pattern plated hole → film stripping → resin plugging → inner layer pattern → post-process. Specifically, after the pre-process, the L1-L4 layer board is first pressed, and then drilled through the drilling process. In this embodiment, the required holes are pre-enlarged by 0.1mm based on the hole diameter required by the customer for drilling. After drilling, copper plating is performed. In this embodiment, the copper plating thickness of the copper plating process is 25μm. After copper plating, the outer layer sealing pattern is performed before the inner layer pattern. While the outer layer is sealed, the holes that need to be copper plated are exposed, and then the exposed holes are plated with patterns to thicken the hole copper. In this embodiment, the pattern hole plating process thickens the hole copper by 25μm to meet customer requirements; after the pattern hole plating and before the inner layer pattern, it also includes sequentially arranged film stripping and resin plugging processes, wherein the resin plugging is to plug the blind holes of the L1-L4 layers with resin ink, and then grind them with a sanding belt; the inner layer pattern is used to make the L4 layer pattern. After the inner layer pattern, post-processing is performed to obtain the L1-4 layer laminated semi-finished product. In the present embodiment, the outer layer sealing pattern and the pattern plated holes are added to the copper plate, and after the inner layer pattern is produced, there is no need to apply high temperature glue to seal the L1-L4 layers, thereby effectively ensuring the quality of the sealing holes and reducing the problem in the prior art of the medicine penetrating into the holes due to the application of high temperature glue to seal the holes, causing residues and causing the copper to be bitten and scrapped, thereby effectively improving the product yield.

[0025] S2: Preparation of L5-L6 layer, firstly performing pre-processing, then making inner layer pattern of L5 layer, obtaining L5-L6 layer with inner layer pattern, and then performing post-processing on L5-L6 layer.

[0026] S3: Overall preparation of L1-L6 layers. In this embodiment, the process flow of this step is pre-process → lamination → outer layer drilling → copper plate electroplating → outer layer drilling → forming gong groove → laser drilling → outer layer circuit pattern → post-process. Specifically, after the pre-process, the L1-L4 laminated semi-finished products obtained in steps S1 and S2, and the L5-L6 layers with inner layer patterns are stacked together in sequence, and the L1-L6 layer boards are first pressed; then the first drilling and the second drilling are performed before and after the copper plate electroplating. In this embodiment, the first drilling and the second drilling are set before and after the copper plate electroplating. The first drilling and the second drilling are both outer layer drilling. Specifically, the first drilling will drill the via hole, and the second drilling will drill the L1-L4 position hole, and the drill tip is 0.05mm smaller than the first drilling tip. In this embodiment, the drilling process of the prior art is changed to the drilling process of the present invention, which is completed in two times and is respectively arranged before and after the copper plate is electroplated, so that the preparation process does not need to carry out the high-temperature glue sticking process before the copper plate is electroplated, and the high-temperature glue sticking process before the copper plate is electroplated and the high-temperature glue tearing process after the copper plate is electroplated are cancelled, which effectively avoids the problems of hole position height difference, glue flow hole, and uneven board thickness after pressing in the prior art, and effectively improves the product quality; moreover, in this embodiment, after the second drilling, the forming gong groove, laser drilling, and outer layer circuit pattern are successively carried out, wherein the forming gong groove adopts a controlled depth gong to control the depth of the L4-L6 layer stepped holes, and a bottom thickness of 3mil to 4mil is reserved to ensure the formation of the stepped holes and avoid glue flow, and laser drilling is carried out after the forming gong groove to remove the residual thickness of the forming gong groove process, and finally the outer layer circuit pattern and the post-process are carried out to obtain the L1-L6 PCB with stepped semi-copper holes.

[0027] Compared with the prior art, the preparation method of the stepped semi-copper hole PCB of the present invention has the following beneficial effects: in the preparation method of the stepped semi-copper hole PCB of the present invention, an outer layer sealing pattern and a pattern plated hole are added between the copper plate and the inner layer pattern in step S1, and the outer layer sealing pattern and the pattern plated hole are added after the copper plate. After the inner layer pattern is made, it is not necessary to apply high-temperature glue to seal the L1-L4 layer positions, which effectively ensures the sealing quality, reduces the problem of residual copper biting caused by the high-temperature glue sealing in the prior art, and effectively improves the product yield; in the preparation method of the stepped semi-copper hole PCB of the present invention, the drilling process before the copper plate is applied is divided into two drilling processes in step S3. The process of applying high temperature glue before copper plate electroplating and removing high temperature glue after copper plate electroplating are cancelled, and the problems of hole position height difference, glue flow hole, and uneven board thickness after pressing in the prior art are effectively avoided, and the product quality is effectively improved; the preparation method of the stepped semi-copper hole PCB of the present invention adds an outer layer sealing hole pattern and a pattern plated hole between the copper plate electroplating and the inner layer pattern in the S1 step, and splits the drilling process before copper plate electroplating into two drilling processes in the S3 step, and the drilling processes are placed before and after the copper plate electroplating, and the two high temperature glue applying processes in the prior art that cannot be operated by machine and can only be operated manually are cancelled, and the production efficiency and yield are effectively improved.

[0028] The above embodiments are only specific embodiments of the present invention, and their descriptions are relatively specific and detailed, but they cannot be understood as limiting the scope of the present invention. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, and these obvious replacement forms all belong to the protection scope of the present invention.

Claims

1. A method for preparing a stepped half-copper via PCB, characterized in that: The step semi-copper via is prepared by using a separate plating and drilling method, which specifically includes the following steps: S1: Preparation of L1-L4 layers, including copper-plated board and inner layer patterning, outer layer sealing patterning after copper-plated board and before inner layer patterning, while sealing the outer layer, the holes that need to be copper-plated are exposed, and then the exposed holes are pattern-plated to thicken the hole copper, and no high-temperature glue is required after the inner layer patterning to obtain L1-L4 layer lamination semi-finished products; S2: Preparation of L5-L6 layer, making inner layer pattern of L5 layer, obtaining L5-L6 layer with inner layer pattern; S3: Overall preparation of L1-L6 layers, laminating the semi-finished L1-L4 layers obtained in steps S1 and S2, and the L5-L6 layers with inner layer patterns together, and performing the first drilling and the second drilling respectively before and after the copper plate is electroplated, so as to change the drilling process in the prior art from completing the drilling in one step to completing the drilling in two steps, namely the first drilling and the second drilling. By performing the drilling once before and after the copper plate is electroplated, there is no need to apply high temperature glue before the copper plate is electroplated, and after the second drilling, forming gong grooves, laser drilling, and outer layer circuit patterns are performed in sequence to obtain a stepped semi-copper hole PCB.

2. The method for preparing a stepped half copper via PCB according to claim 1, characterized in that: The copper plating thickness of the copper plate in the electroplating process in step S1 is 25 μm.

3. The method for preparing a stepped half copper via PCB according to claim 1, characterized in that: The pattern hole plating process in step S1 thickens the hole copper by 25 μm.

4. The method for preparing a stepped half copper via PCB according to claim 1, characterized in that: The S1 step is between the pattern plated holes and the inner layer patterns, and also includes the film stripping and resin plugging processes.

5. The method for preparing a stepped half copper via PCB according to claim 4, characterized in that: The resin plugging method is to plug the blind holes of the L1-L4 layers with resin ink and then grind them flat with a sanding belt.

6. The method for preparing a stepped half copper via PCB according to claim 1, characterized in that: In step S3, the first drilling is to drill the via holes, and the second drilling is to drill the holes at the L1-L4 positions, and the drill tip is 0.05 mm smaller than the drill tip used in the first drilling.

7. The method for preparing a stepped half copper via PCB according to claim 1, characterized in that: The forming gong groove described in step S3 uses a controlled depth gong to drill the L4-L6 layer stepped holes with controlled depth, leaving a bottom thickness of 3mil to 4mil.

8. The method for preparing a stepped half copper via PCB according to claim 5, characterized in that: The laser drilling described in step S3 is used to remove the residual thickness of the forming gong groove process.

Citation Information

Patent Citations

  • Method for manufacturing multi-layer circuit board with internal connecting finger

    CN103249264A

  • Manufacturing process of thick copper plate capable of preventing no-copper condition in hole

    CN109640546A

  • Stepped blind slotted hole mixed-pressing high-frequency microwave printed circuit board and processing method thereof

    CN112040674A

  • Processing method for improving interconnection and separation of through holes of PTFE circuit board

    CN113873758A

  • Manufacture of wiring board

    JP1998270844A