Aromatic hydrocarbon transalkylation method and system
By hydrocracking pretreatment of the mixed raw materials of aromatic hydrocarbons and toluene, the problems of reduced activity and short life of the alkyl transfer unit catalyst in the aromatic hydrocarbon combined device are solved, and the catalyst life is extended and the reaction efficiency is improved. .
Patent Information
- Application Number
- CN202011129315.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-21
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2040-10-21
AI Technical Summary
In the aromatic hydrocarbon combined device, the deterioration of raw materials of the alkyl transfer unit leads to the problem of decreasing catalyst activity and short service life, mainly due to the existence of polycyclic aromatic hydrocarbons, heavy fused aromatic hydrocarbons, unsaturated aromatic hydrocarbons and other impurities.
The pretreatment step is used to carry out hydrocracking reaction of the mixed raw materials of C9 aromatic hydrocarbons and toluene to remove impurities, including polycyclic aromatic hydrocarbons, fused ring heavy aromatic hydrocarbons, unsaturated aromatic hydrocarbons and other impurities, and extend the service life of the alkyl transfer catalyst. The pretreatment step uses a specific catalyst, including an oxide support, the first active component and the second active component, combined with a molecular sieve, to perform a hydrogenation reaction, optimizing reaction conditions such as pressure, temperature and hydrogen-hydrogen molar ratio.
It effectively reduces the impurity content in the feed of the alkyl transfer reactor, extends the service life of the catalyst, improves the total conversion rate and selectivity of the reaction, and extends the operating cycle of the catalyst under high bromine index conditions.
Smart Images

Figure CN114456035B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of aromatic hydrocarbon alkyl transfer, and in particular relates to a method and system for aromatic hydrocarbon alkyl transfer. Background Art
[0002] The aromatics complex is the core unit for producing PX. It mainly uses straight-run naphtha as raw material to produce aromatic products such as benzene, para-xylene and o-xylene. It usually includes catalytic reforming, aromatics extraction, xylene separation, alkyl transfer, adsorption separation and xylene isomerization. In the traditional aromatics complex, the aromatics raw materials generated by reforming are split and extracted by the deheptanizer tower, and benzene and toluene are separated as raw materials to enter the alkyl transfer unit; and the bottom components of the tower are separated into C8 aromatics by the xylene unit, and heavy aromatics (C9 + A) is used as a raw material to enter the alkyl transfer unit, undergoes an alkyl transfer reaction with benzene or toluene to produce xylene; benzene or toluene is used to react with heavy aromatics (C9 + A) Transalkylation reaction to increase xylene production is an effective method to increase xylene production by utilizing heavy aromatics.
[0003] As the quality of upstream raw materials deteriorates and the severity of the reforming process increases, the raw materials benzene or toluene used in the transalkylation unit and heavy aromatics (C9 + A) The impurity content is increasing day by day. The main impurity types are polycyclic aromatic hydrocarbons, heavy condensed aromatic hydrocarbons, unsaturated aromatic hydrocarbons and other impurities such as moisture, carbon oxides, etc. Polycyclic aromatic hydrocarbons are easily adsorbed on the catalyst surface and cover the reaction active center. The coke generated after the reaction is deposited on the catalyst surface, which has a great influence on the catalyst activity; heavy condensed aromatic hydrocarbons will accelerate the coking of the catalyst surface and affect the catalyst life; the unsaturated bonds on the unsaturated aromatic hydrocarbons are easy to condense on the catalyst surface to form coke, and free water is easy to cause high-temperature water to remove the skeleton atoms in the molecular sieve crystal structure, causing the catalyst activity to be permanently reduced or lost, affecting the catalyst activity and stability; carbon oxides are easy to adsorb on the catalyst active center, poisoning the catalyst, affecting the catalyst activity, affecting the product quality, and causing corrosion and damage to the equipment. Therefore, it is generally necessary to pretreat the aromatic raw materials.
[0004] In traditional aromatics complexes, the reformed oil is subjected to a de-olefination process before entering the aromatics conversion and separation process. The main purpose of this process is to provide olefin-free raw materials for the adsorption separation of paraxylene in the paraxylene production process. During the processing, the aromatic raw materials generated by reforming are separated into C7 - and C8 + Components, including C8 + After the olefins are removed from the components in the white clay tower, they enter the xylene tower for separation, and the C8A enters the PX adsorption separation unit for separation. -After extraction to remove non-aromatic hydrocarbons, trace olefins are removed through a bleaching clay tower. The benzene or toluene after olefin removal is used as the raw material for the transalkylation unit reaction. The adsorption separation unit has extremely high restrictions on olefins. In the process of removing olefins, bleaching clay is usually used as an adsorbent. Olefins undergo polymerization reactions on its surface and are adsorbed and removed. The disadvantage of bleaching clay adsorbent is that it has a short service life and must be replaced frequently. Abandoned bleaching clay will cause serious environmental pollution during the landfill process. In recent years, with the breakthrough of key issues such as the large-scale crystallization separation equipment, PX crystallization separation technology has developed rapidly. Due to the advantages of low energy consumption, simple operation, and stable products, crystallization separation has been increasingly widely used and is one of the future development directions of PX separation technology.
[0005] Since PX crystallization separation technology does not involve the use of adsorbents, it has no strict restrictions on the olefin components in the raw materials. Therefore, it is not necessary to de-olefinize the reformed oil in the process, which can greatly reduce waste solid emissions. In the new generation of aromatics production process, the separation of paraxylene adopts a crystallization process, which has a higher tolerance to olefins. Therefore, the process of de-olefinizing the reformed oil seems unnecessary. Therefore, when the requirements for olefins in the new process of paraxylene adsorption separation are reduced, it is bound to weaken the original de-olefinization process, resulting in the deterioration of the raw materials of the alkyl transfer unit.
[0006] CN1282733C discloses a catalyst for selective hydrogenation and deolefination of reforming oil, the main purpose of which is to provide high-quality raw materials for subsequent units and reduce the content of olefins in the raw materials. It contains 0.1-1.0wt% of precious metals and 0.05-0.50wt% of alkali metals or alkaline earth metals as additives. Under hydrogen reaction conditions, the reaction temperature is 150-250℃, the pressure is 1.5-3.0MPa, and the volume space velocity is 2.0-4.0h -1 Under the above conditions, the bromine index of the product is less than 100mgBr / 100g oil, and the loss of aromatics is less than 0.5wt%. The above-mentioned deolefination catalyst is only for the removal of olefins in the C8 component, just to ensure that the bromine index of the PX adsorption separation feed is qualified. In order to extend its service life, the removal of olefins in C9 and above components and C7 and below components is often ignored, resulting in the subsequent carbon deposition of the catalyst and the rapid decrease in activity after the C9 heavy aromatics enter the alkyl transfer unit. Summary of the invention
[0007] In order to overcome the problems existing in the prior art, the present invention provides a method for aromatic hydrocarbon transalkylation, which mainly solves the problem of poor operating stability and short life of toluene transalkylation catalyst caused by increased raw material deterioration in the transalkylation unit in the existing xylene production process. In the aromatic refining unit widely used in the latest generation of aromatics equipment, there is often a problem of high content of polycyclic aromatic hydrocarbons, heavy condensed aromatic hydrocarbons, unsaturated aromatic hydrocarbons and other impurities such as moisture and carbon oxides in the raw materials of the transalkylation unit. The material with a high impurity content often causes the catalyst activity to drop rapidly after entering the transalkylation unit.
[0008] One of the objects of the present invention is to provide a method for aromatic hydrocarbon transalkylation, the method comprising the following steps:
[0009] Step 1, mixing C9 aromatic hydrocarbons and toluene to obtain mixed raw material 1, and further mixing the mixed raw material 1 with hydrogen to obtain mixed raw material 2;
[0010] Step 2, reacting the mixed raw material 2 in the presence of a transalkylation catalyst to obtain a mixed product containing benzene and C8 aromatics;
[0011] Step 3: The mixed product obtained in step 2 is heat exchanged with the mixed raw material 2 obtained in step 1, and then cooled and gas-liquid separated in sequence, the hydrogen obtained in the gas phase is recycled back to step 1, and the liquid is stripped;
[0012] Before performing step 2, a pretreatment catalyst is used to pretreat the C9 aromatics and / or the mixed feedstock 1 and / or the mixed feedstock 2 before heat exchange and / or the mixed feedstock 2 after heat exchange.
[0013] In the present invention, the C9 aromatics are obtained as follows: heavy aromatics from a paraxylene unit enter a heavy aromatics tower to obtain C9 + A (used to adjust gasoline), and C9 aromatics.
[0014] In a preferred embodiment, the pretreatment conditions are: operating pressure 0.1-6.0 MPa, reaction temperature 100-420°C, reaction weight hourly space velocity 0.5-30.0 h -1 , the hydrogen-to-hydrocarbon molar ratio is 0.5-5.0.
[0015] In a further preferred embodiment, the pretreatment conditions are: operating pressure 2.0-4.0 MPa, reaction temperature 340-450°C, reaction weight hourly space velocity 5-20 h -1 , the hydrogen-to-hydrocarbon molar ratio is 3 to 5.
[0016] Among them, during the raw material pretreatment process, hydrocracking reactions of polycyclic aromatic hydrocarbons, hydrocracking reactions of condensed-ring heavy aromatic hydrocarbons, hydrocracking and / or cracking reactions of non-aromatic hydrocarbons, hydrogenation reactions of unsaturated aromatic hydrocarbons, etc. can occur simultaneously, mainly involving the removal of polycyclic aromatic hydrocarbons, condensed-ring heavy aromatic hydrocarbons, non-aromatic hydrocarbons and unsaturated aromatic hydrocarbons, solving the problem of high levels of impurities such as polycyclic aromatic hydrocarbons, condensed-ring heavy aromatic hydrocarbons, non-aromatic hydrocarbons and unsaturated aromatic hydrocarbons in the feed of the aromatic alkyl transfer unit, reducing the influence of impurities on the alkyl transfer catalyst, and achieving the goal of extending the life of the alkyl transfer catalyst.
[0017] In a preferred embodiment, the pretreatment catalyst comprises an oxide support, a first active component, a second active component and an optional molecular sieve, wherein the first active component is selected from at least one of Group VIII metals, and the second active component is selected from at least one (e.g., at least two or at least three) of Group VIB, Group VB, Group VIIB, Group IIB and Group VA metals.
[0018] Wherein, the first active component and the second active component exist independently in at least one form of a simple substance, an oxide and a complex.
[0019] In a preferred embodiment, the first active component is selected from at least one of cobalt, nickel, palladium, platinum, rhodium and iridium.
[0020] In a further preferred embodiment, the first active component is selected from cobalt and / or nickel.
[0021] In a preferred embodiment, the second active component is selected from at least one of zinc, rhenium, molybdenum, bismuth and chromium.
[0022] In a further preferred embodiment, the second active component is selected from at least one of rhenium, molybdenum and bismuth.
[0023] In a preferred embodiment, the mass ratio of the first active component to the second active component is (0.01-40):1, preferably (0.1-20):1, and more preferably (0.1-10):1, calculated by the mass of the metal element.
[0024] For example, 0.5:1, 1:1, 2:1, 3:1, 4:1, 5:1, 8:1, 10:1, 15:1, 20:1, 30:1, etc.
[0025] In a preferred embodiment, the molecular sieve contains 6-12 ring structures. Preferably, the molecular sieve is at least one selected from MFI molecular sieve, FER molecular sieve, PTY molecular sieve, MEI molecular sieve, MEL molecular sieve, MOR molecular sieve, FAU molecular sieve, STF molecular sieve, ITQ molecular sieve, BEA molecular sieve, MTW molecular sieve, MFI / MEL molecular sieve, MOR / MFI molecular sieve, MOR / MEL molecular sieve, MFI / FAU molecular sieve, BEA / MFI molecular sieve, and FAU / MEL molecular sieve.
[0026] In a further preferred embodiment, the molecular sieve is a mixture of a molecular sieve with a maximum circular ring structure of 8 to 10 rings and a molecular sieve with a maximum circular ring structure of 12; preferably, the mass ratio of the molecular sieve with a maximum circular ring structure of 8-10 rings to the molecular sieve with a maximum circular ring structure of 12 rings is (0.1-5):1, preferably (0.3-2):1.
[0027] Wherein, the topological structure of the molecular sieve is a single topological structure and / or a mixed topological structure.
[0028] In a further preferred embodiment, in the pretreatment catalyst, the external specific surface area of the molecular sieve is higher than 30 m 2 / g (preferably 50-300m 2 / g), pore volume of 0.15~0.5cm 3 / g, micropores (micropores are 2nm) account for more than 40% of the total pore volume.
[0029] In a preferred embodiment, the carrier is selected from at least one of α-alumina, γ-alumina, silicon dioxide, silica gel, and silicon carbide.
[0030] In a further preferred embodiment, the carrier is a calcined carrier.
[0031] In a further preferred embodiment, the calcination temperature is 350-900°C, preferably 500-800°C, more preferably 550-700°C; and / or the calcination time is 2-12h, preferably 2-12h, more preferably 4-10h.
[0032] In a preferred embodiment, in the pretreated catalyst, the weight content of each component is as follows: 5-99% of the carrier, 0-90% of the molecular sieve, 0.05-20% of the first active component, and 0.05-30% of the second active component.
[0033] In a further preferred embodiment, in the pretreatment catalyst, the weight content of each component is as follows: 10-95% of the carrier, 4-80% of the molecular sieve, 0.08-10% of the first active component, and 0.1-20% of the second active component.
[0034] In a preferred embodiment, in step 1, the mass ratio of C9 aromatics to toluene is 100 / 0 to 0 / 100, preferably 20 / 70 to 80 / 20, and more preferably 60 / 40-40 / 60.
[0035] In a preferred embodiment, in step 1, the molar ratio of hydrogen to mixed raw material 1 is 10:1 to 0.5:1, preferably 5:1 to 1:1, and more preferably 3.5:1-2:1.
[0036] In a preferred embodiment, the reaction in step 2 is carried out as follows: reaction pressure 1.0-6.0 MPa, reaction temperature 300-550°C, hydrogen-to-hydrocarbon molar ratio 1-20, feed weight space velocity 1.0-100 h -1 Next proceed.
[0037] In a further preferred embodiment, the reaction in step 2 is carried out as follows: the reaction pressure is 2.0-4.0 MPa, the reaction temperature is 340-450°C, the hydrogen-to-hydrocarbon molar ratio is 3-10, and the feed weight space velocity is 5-20 h -1 Next proceed.
[0038] In a preferred embodiment, in step 1, the hydrogen is optionally pretreated before being mixed with the mixed feedstock.
[0039] In a further preferred embodiment, the pretreatment is carried out in the presence of a molecular sieve and / or the pretreatment catalyst, mainly for removing carbon oxides (such as carbon monoxide).
[0040] The molecular sieve may be selected from at least one of 4A molecular sieve, 5A molecular sieve and 4X molecular sieve. The pretreatment may be directly carried out at room temperature and pressure without strictly controlling the conditions.
[0041] In a preferred embodiment, the method further comprises step 5: performing optional pretreatment on the mixture of benzene and toluene from the aromatic extraction unit, and then mixing it with the liquid product after the gas stripping treatment in step 3 or entering the bleaching clay tower, benzene tower and toluene tower in sequence independently of each other.
[0042] The above means that the mixture of benzene and toluene can be mixed with the liquid product after the gas stripping treatment in step 3 and then enter the bleaching tower together; or the mixture of benzene and toluene and the liquid product after the gas stripping treatment in step 3 can enter the bleaching tower separately and independently and be mixed in the bleaching tower.
[0043] In a further preferred embodiment, the benzene product is obtained by a benzene tower, and the C8 + A product (paraxylene removal unit) and toluene product.
[0044] In a further preferred embodiment, the mixture of benzene and toluene is pretreated in the presence of molecular sieve and / or the pretreatment catalyst, mainly for removing water. The pretreatment is carried out at a temperature higher than 100°C and a pressure>2MPa, but in actual application, the operating temperature and pressure do not need to be specially controlled, because the heat exchange and pressurization (pressure 2.0-3.0MPa and temperature>200 degrees Celsius) of the previous equipment have been completed when the logistics flows through this place, and the lower limit of the condition can meet the dehydration.
[0045] The mixture of benzene and toluene may be pretreated before and / or after mixing with the liquid product after the stripping treatment in step 3. The molecular sieve may be selected from at least one of 4A molecular sieve, 5A molecular sieve and 4X molecular sieve.
[0046] The method of the present invention can be used to solve the problem of high content of polycyclic aromatic hydrocarbons, heavy condensed aromatic hydrocarbons, unsaturated aromatic hydrocarbons and other impurities such as moisture and carbon oxides in the feed of the transalkylation reactor, play a role in protecting the transalkylation catalyst and extending its service life.
[0047] The second object of the present invention is to provide an aromatic hydrocarbon alkyl transfer system for carrying out the method described in one of the objects of the present invention, wherein the system comprises a toluene tower, a heavy aromatic hydrocarbon tower, a feed buffer tank, an inlet and outlet heat exchanger, a feed heating furnace, and an aromatic hydrocarbon alkyl transfer reactor, wherein the toluene tower and the heavy aromatic hydrocarbon tower are both connected to the feed buffer tank, an inlet and outlet heat exchanger is provided between the feed buffer tank and the aromatic hydrocarbon alkyl transfer reactor, and a material pretreatment device I is provided before the aromatic hydrocarbon alkyl transfer reactor.
[0048] In a preferred embodiment, the material pretreatment device I is arranged between the toluene tower (preferably the toluene tower top reflux tank) and the feed buffer tank, and / or between the heavy aromatics tower (preferably the heavy aromatics tower top reflux tank) and the feed buffer tank, and / or between the feed buffer tank and the inlet and outlet heat exchanger, and / or between the inlet and outlet heat exchanger and the feed heating furnace, and / or between the feed heating furnace and the aromatics alkyl transfer reactor.
[0049] Among them, the material pretreatment device I includes a material pipeline, product separation equipment required by the working conditions, gas / liquid boosting equipment and other ancillary equipment, such as feed and discharge pumps, compressors, etc.
[0050] In a further preferred embodiment, the material pretreatment device I is filled with the pretreatment catalyst.
[0051] The pretreatment catalyst described herein has the same definition as the pretreatment catalyst described in one of the objectives of the present invention.
[0052] In a preferred embodiment, along the material flow direction, a cooler, a gas-liquid separator (such as a high separation tank), a stripping tower, a bleaching clay tower, and a benzene tower are further arranged after the inlet and outlet heat exchangers.
[0053] In a further preferred embodiment, the benzene tower is connected to the toluene tower along the material flow direction. The benzene product is separated by the benzene tower, and the C8 + A product (paraxylene removal unit) and toluene product.
[0054] In a preferred embodiment, the bleaching clay tower is further connected to an aromatics extraction device for introducing a mixture containing benzene and toluene in the aromatics extraction device into the bleaching clay tower.
[0055] In a further preferred embodiment, a material pretreatment device II is optionally provided between the bleaching clay tower and the aromatics extraction device, in which a molecular sieve and / or the pretreatment catalyst is loaded, mainly for removing water.
[0056] The molecular sieve may be selected from at least one of 4A molecular sieve, 5A molecular sieve and 4X molecular sieve.
[0057] In a preferred embodiment, the system further comprises a circulating hydrogen compressor.
[0058] In a further preferred embodiment, one end of the circulating hydrogen compressor is connected to the gas-liquid separator, and the other end is connected to the feed buffer tank.
[0059] In a further preferred embodiment, an optional material pretreatment device III is provided between the circulating hydrogen compressor and the feed buffer tank, in which a molecular sieve and / or the pretreatment catalyst are loaded, mainly for removing carbon oxides (such as carbon monoxide).
[0060] The molecular sieve may be selected from at least one of 4A molecular sieve, 5A molecular sieve and 4X molecular sieve.
[0061] The endpoints and any values of the scope disclosed in the present invention are not limited to the precise scope or value, and these scopes or values should be understood to include values close to these scopes or values. For numerical ranges, the endpoint values of each scope, the endpoint values of each scope and the individual point values, and the individual point values can be combined with each other to obtain one or more new numerical ranges, which should be regarded as specifically disclosed in this article. Hereinafter, in principle, each technical solution can be combined with each other to obtain a new technical solution, which should also be regarded as specifically disclosed in this article.
[0062] Compared with the prior art, the present invention has the following beneficial effects: the method and system of the present invention can be used to solve the problem of high content of polycyclic aromatic hydrocarbons, heavy condensed aromatic hydrocarbons, unsaturated aromatic hydrocarbons and other impurities such as moisture and carbon oxides in the feed of the transalkylation reactor, play a role in protecting the transalkylation catalyst and extending its service life. BRIEF DESCRIPTION OF THE DRAWINGS
[0063] Figure 1 The systems used in Example 1, Example 2 and Comparative Examples 2 to 7 are shown;
[0064] Figure 2 The system used in Comparative Examples 1 and 8 to 10 is shown;
[0065] Figure 3 The system used in Example 3 is shown;
[0066] Figure 4 A system adopted in Example 4 is shown.
[0067] 1-toluene tower; 2-heavy aromatics tower; 3-feed buffer tank; 4-inlet and outlet heat exchanger; 5-alkyl transfer reactor; 6-cooler; 7-gas-liquid separator; 8-stripping tower; 9-white clay tower; 10-benzene tower; 11-paraxylene unit; 12-aromatics extraction unit; 13-circulating hydrogen compressor; I-material pretreatment unit I; II-material pretreatment unit II; III-material pretreatment unit III.
[0068] S1-supplemental hydrogen (from catalytic reforming); S2-mixture of benzene and toluene; S3-heavy aromatics; S4-C9 + A aromatics; S5-benzene products; S6-C8 + A aromatic hydrocarbons; S7-toluene; S8-C9 aromatic hydrocarbons; S9-mixed feedstock 1; S10-mixed feedstock 2; S11-mixed product containing benzene and C8 aromatic hydrocarbons; S12-circulating hydrogen. DETAILED DESCRIPTION
[0069] The present invention is described in detail below in conjunction with specific embodiments. It is necessary to point out that the following embodiments are only used to further illustrate the present invention and cannot be understood as limiting the scope of protection of the present invention. Some non-essential improvements and adjustments made to the present invention by those skilled in the art based on the contents of the present invention still fall within the scope of protection of the present invention.
[0070] It should also be noted that the various specific technical features described in the following specific embodiments can be combined in any suitable manner without contradiction. To avoid unnecessary repetition, the present invention will not further describe various possible combinations.
[0071] In addition, the various embodiments of the present invention may be arbitrarily combined as long as they do not violate the concept of the present invention. The technical solutions thus formed belong to part of the original disclosure of this specification and also fall within the protection scope of the present invention.
[0072] The raw materials used in the examples and comparative examples, unless otherwise specified, are disclosed in the prior art, for example, they can be directly purchased or prepared according to the preparation methods disclosed in the prior art.
[0073]
[0074] [Example 1]
[0075] use Figure 1 The system shown carries out an aromatic hydrocarbon transalkylation reaction, wherein a material pretreatment device I is added between the feed heating furnace and the transalkylation reactor 5.
[0076] The mixed raw material S10 after the circulating hydrogen S12, the supplementary hydrogen S1 and the mixed raw material S9 enters the feed heat exchanger 4. After heat removal, the mixed material enters the material pretreatment device I to undergo a raw material refining reaction. This reaction is a hydrocracking reaction, and its main purpose is to reduce the polycyclic aromatic hydrocarbons in the alkylation feed. After pretreatment, the raw material enters the feed heating furnace ( Figure 1 The product S11 after the reaction is heat exchanged with the mixed raw material S10, and then enters the cooler 6, the gas-liquid separator 7, and the stripping tower 8 in sequence to obtain a liquid product.
[0077] The mixed material containing benzene and toluene from the aromatics extraction device 12 is mixed with the liquid phase product from the stripping tower 8 and then enters the clay tower 9, the benzene tower 10 and the toluene tower 1 in sequence. Among them, the benzene product S5 is separated from the benzene tower, and the C8 is separated from the toluene tower. + Aromatic hydrocarbon S6 and toluene S7 are obtained at the same time.
[0078] Heavy aromatics from the paraxylene unit 11 enter the heavy aromatics tower 2 to separate C9 + Aromatic hydrocarbons S4 are used to adjust gasoline, and C9 aromatic hydrocarbons S8 are obtained at the same time. The C9 aromatic hydrocarbons S8 are mixed with toluene S7 and then enter the feed buffer tank 3.
[0079] The material pretreatment device I is filled with a pretreatment catalyst A1, which is prepared as follows: 41 g of alumina (calcined at 500° C. for 6 h) and 39 g of ammonium ZSM-5 / FAU molecular sieve (mass ratio 0.2) are mixed evenly, 5.24 g of zinc chloride and 71.53 g of cobalt sulfate heptahydrate are dissolved in a small amount of distilled water and added to the mixed powder, followed by adding 5 g of sesbania powder and 10 mL of nitric acid solution, kneading and extruding, calcining at 500° C. for 3 h, and then reducing at 400° C. and 3 MPa for 4 h to obtain catalyst A1. The catalyst properties are shown in Table 1.
[0080] The reaction conditions in the material pretreatment device I and the reaction conditions in the alkane transfer reactor are shown in Table 3.
[0081] [Comparative Example 1]
[0082] use Figure 2 The system is carried out without the material pretreatment device I. The specific process is repeated in Example 1, except that the material pretreatment is not performed. The reaction conditions in the material pretreatment device I and the reaction conditions in the alkane transfer reactor are shown in Table 3.
[0083] The performance comparison of Example 1 and Comparative Example 1 after different running times is shown in Table 4.
[0084] [Comparative Example 2]
[0085] The process of Example 1 was repeated, except that:
[0086] The material pretreatment device I is filled with a pretreatment catalyst D1, which is prepared as follows: 41 g of alumina (calcined at 500° C. for 6 h) and 39 g of ammonium-type SFN molecular sieve (mass ratio 0.2) are mixed evenly, 5.24 g of zinc chloride and 57.22 g of cobalt sulfate heptahydrate are dissolved in a small amount of distilled water and added to the mixed powder, followed by adding 5 g of sesbania powder and 10 mL of nitric acid solution, kneading and extruding, calcining at 500° C. for 3 h, and then reducing at 400° C. and 3 MPa for 4 h to obtain catalyst D1. The catalyst properties are shown in Table 1.
[0087] [Comparative Example 3]
[0088] The process of Example 1 was repeated, except that:
[0089] The material pretreatment device I is filled with a pretreatment catalyst D2, and the pretreatment catalyst D2 is prepared as follows: 41g of alumina (untreated) and 39g of ammonium ZSM-5 / FAU molecular sieve (mass ratio 0.2) are mixed evenly, 5.24g of zinc chloride and 57.22g of cobalt sulfate heptahydrate are dissolved in a small amount of distilled water and added to the mixed powder, and then 5g of sesbania powder and 10mL of nitric acid solution are added, kneaded and extruded, and calcined at 500°C for 3 hours, and then reduced at 400°C and a pressure of 3MPa for 4 hours to obtain catalyst D2. The catalyst properties are shown in Table 1.
[0090] [Comparative Example 4]
[0091] The process of Example 1 was repeated, except that:
[0092] The material pretreatment device I is filled with a pretreatment catalyst D3, and the pretreatment catalyst D3 is prepared as follows: 41g of alumina (calcined at 500°C for 6h) and 39g of ammonium ZSM-5 / FAU molecular sieve (mass ratio 0.2) are mixed evenly, 5.24g of zinc chloride and 0.048 of cobalt sulfate heptahydrate are dissolved in a small amount of distilled water and added to the mixed powder, and then 5g of sesbania powder and 10mL of nitric acid solution are added, kneaded and extruded, and calcined at 500°C for 3 hours, and then reduced at 400°C and a pressure of 3MPa for 4 hours to obtain catalyst D3. The catalyst properties are shown in Table 1.
[0093] [Comparative Example 5]
[0094] The process of Example 1 was repeated, except that:
[0095] The material pretreatment device I is filled with a pretreatment catalyst D4, which is prepared as follows: 41 g of alumina (calcined at 500° C. for 6 h) and 39 g of ammonium ZSM-5 / FAU molecular sieve (mass ratio 0.2) are mixed evenly, 0.524 g of zinc chloride and 57.22 g of cobalt sulfate heptahydrate are dissolved in a small amount of distilled water and added to the mixed powder, followed by adding 5 g of sesbania powder and 10 mL of nitric acid solution, kneading and extruding, calcining at 500° C. for 3 h, and then reducing at 400° C. and 3 MPa for 4 h to obtain catalyst D4. The catalyst properties are shown in Table 1.
[0096] [Comparative Example 6]
[0097] The process of Example 1 was repeated, except that:
[0098] The material pretreatment device I is filled with a pretreatment catalyst D5, which is prepared as follows: 41 g of alumina (calcined at 500° C. for 6 h) and 39 g of ammonium ZSM-5 / FAU molecular sieve (mass ratio 10) are mixed evenly, 5.24 g of zinc chloride and 57.22 g of cobalt sulfate heptahydrate are dissolved in a small amount of distilled water and added to the mixed powder, followed by adding 5 g of sesbania powder and 10 mL of nitric acid solution, kneading and extruding, calcining at 500° C. for 3 h, and reducing at 400° C. and 3 MPa for 4 h to obtain catalyst D5. The catalyst properties are shown in Table 1.
[0099] [Comparative Example 7]
[0100] The process of Example 1 was repeated, except that:
[0101] The material pretreatment device I is filled with a pretreatment catalyst D6, and the pretreatment catalyst D6 is prepared as follows: 41g of alumina (calcined at 500°C for 6h) and 39g of ammonium ZSM-5 / FAU molecular sieve (mass ratio 0.2) are mixed evenly, 5.24g of zinc chloride and 57.22g of cobalt sulfate heptahydrate are dissolved in a small amount of distilled water and added to the mixed powder, followed by adding 5g of sesbania powder and 10mL of nitric acid solution, kneading and extruding, calcining at 500°C for 3 hours, and then reducing at 400°C and 3MPa for 4 hours to obtain catalyst D6. The catalyst properties are shown in Table 1.
[0102] Table 2: Properties of the molecular sieves used in the catalysts prepared in Example 1 and Comparative Example 7
[0103]
[0104] Table 3 Comparison of operating parameters of Example 1 and Comparative Examples 1 to 7
[0105]
[0106]
[0107]
[0108]
[0109]
[0110] It can be seen from Table 3 and Table 4 that at the initial stage of operation, the operating conditions of the transalkylation reactors in Example 1 and Comparative Examples 1 to 7 are similar, and the content of unsaturated aromatics in the feedstock is different. In Example 1, the unsaturated aromatics in the transalkylation feed after the feedstock pretreatment unit are significantly reduced. The performance of the transalkylation catalysts of the two are similar at the initial stage of the reaction, but after a long period of operation, the transalkylation catalyst in Example 1 with the addition of a feedstock pretreatment reactor has a higher total reaction conversion rate and selectivity under the same feedstock conditions, which means that the feedstock pretreatment unit can extend the operation cycle of the transalkylation catalyst under high bromine index conditions and achieve higher conversion efficiency and selectivity.
[0111] [Example 2]
[0112] use Figure 1 The system is carried out, and the specific process repeats Example 1, and the hydrogenation reaction occurs in the material pretreatment device I. The reaction conditions in the material pretreatment device I and the reaction conditions in the alkane transfer reactor are shown in Table 5.
[0113] The material pretreatment device I is filled with a pretreatment catalyst A2, which is prepared as follows: 25 g of aluminum oxide (calcined at 350° C. for 12 h), 70 g of silicon oxide, 15.57 g of nickel nitrate and 2.35 g of rhenium trichloride are dissolved in a small amount of distilled water and added to the mixed powder, followed by adding 5 g of sesbania powder and 10 mL of nitric acid solution, kneading and extruding, calcining at 500° C. for 3 hours, and then reducing at 400° C. and 3 MPa for 4 hours to obtain catalyst A2. The catalyst properties are shown in Table 1.
[0114] [Comparative Example 8]
[0115] use Figure 2 The system is carried out without the material pretreatment device I. The specific process is repeated in Example 2, except that the material pretreatment is not performed. The reaction conditions in the material pretreatment device I and the reaction conditions in the alkane transfer reactor are shown in Table 5.
[0116] The performance comparison of Example 2 and Comparative Example 8 after different running times is shown in Table 5.
[0117] Table 5 Comparison of operating parameters of Example 2 and Comparative Example 8
[0118]
[0119] Table 6 Performance comparison of Example 2 and Comparative Example 8 after different running time
[0120]
[0121] It can be seen from Tables 5 and 6 that at the initial stage of operation, the operating conditions of the transalkylation reactors in Example 2 and Comparative Example 8 are similar, and the content of polycyclic aromatic hydrocarbons in the raw materials is different. In Example 2, the polycyclic aromatic hydrocarbons in the transalkylation feed after the raw material pretreatment unit are significantly reduced. The performance of the transalkylation catalysts of the two is similar at the initial stage of the reaction. After long-term operation, the transalkylation catalyst in Example 2 with the addition of a raw material pretreatment reactor has a higher total reaction conversion rate and selectivity under the same raw material conditions, which means that the raw material pretreatment unit can extend the operation cycle of the transalkylation catalyst under high bromine index conditions and achieve higher conversion efficiency and selectivity.
[0122] [Example 3]
[0123] use Figure 3 The system shown carries out an aromatic hydrocarbon transalkylation reaction, wherein a material pretreatment device I is added between the heavy aromatic hydrocarbon tower 2 and the feed buffer tank 3.
[0124] Heavy aromatics from the paraxylene unit 11 enter the heavy aromatics tower 2 to separate C9 + Aromatic hydrocarbons S4 are used to adjust gasoline, and C9 aromatic hydrocarbons S8 are obtained at the same time. The C9 aromatic hydrocarbons S8 enter the material pretreatment device I for pretreatment (specifically, hydrocracking reaction). The pretreated C9 aromatic hydrocarbons S8 are mixed with toluene S7 and enter the feed buffer tank 3.
[0125] The mixed raw material 2 S10 after the circulating hydrogen S12, the supplementary hydrogen S1 and the mixed raw material 1 S9 are mixed enters the inlet and outlet heat exchanger 4, and after heat removal, the mixed material enters the transalkylation reactor 5 for reaction. The product S11 after the reaction exchanges heat with the mixed raw material 2 S10, and then enters the cooler 6, the gas-liquid separator 7, and the stripping tower 8 in sequence to obtain a liquid product.
[0126] The mixed material containing benzene and toluene from the aromatics extraction device 12 is mixed with the liquid phase product from the stripping tower 8 and then enters the clay tower 9, the benzene tower 10 and the toluene tower 1 in sequence. Among them, the benzene product S5 is separated from the benzene tower, and the C8 is separated from the toluene tower. + Aromatic hydrocarbon S6 and toluene S7 are obtained at the same time.
[0127] The material pretreatment device I is filled with two beds connected in series, the first bed is filled with a physical mixture of 5A molecular sieve and carrier alumina, with a mass ratio of 5:1; the second bed is filled with a pretreatment catalyst A3, which is prepared as follows: 7g of silicon oxide (calcined at 500°C for 8h) and 88g of ammonium type MOR / ZSM-11 (MOR / MEL structure, mass ratio 1 / 6) are mixed evenly, 0.50g of palladium chloride and 9.20g of ammonium heptamolybdate are dissolved in a small amount of distilled water and added to the mixed powder, followed by adding 5g of sesbania powder and 10mL of nitric acid solution, fully kneading and extruding, calcining at 500°C for 3 hours, and then reducing at 400°C and 3MPa for 4 hours to obtain catalyst A3.
[0128] The reaction conditions in the material pretreatment device I and the reaction conditions in the alkane transfer reactor are shown in Table 7.
[0129] [Comparative Example 9]
[0130] use Figure 2 The system is carried out without the material pretreatment device I. The specific process is repeated in Example 3, except that the material pretreatment is not performed. The reaction conditions in the material pretreatment device I and the reaction conditions in the alkane transfer reactor are shown in Table 7.
[0131] The performance comparison of Example 3 and Comparative Example 9 after different running times is shown in Table 8.
[0132] Table 7 Comparison of operating parameters in Example 3
[0133]
[0134] Table 8 Performance comparison of Example 3 and Comparative Example 9 after different running times
[0135]
[0136] It can be seen from Tables 7 and 8 that at the initial stage of operation, the operating conditions of the transalkylation reactors in Example 3 and Comparative Example 9 are similar, and the content of heavy condensed aromatic hydrocarbons in the raw materials is different. In Example 3, the content of heavy condensed aromatic hydrocarbons in the transalkylation feed after the raw material pretreatment unit is significantly reduced. The performance of the transalkylation catalysts of the two is similar at the initial stage of the reaction. After long-term operation, the transalkylation catalyst in Example 3 with the addition of a raw material pretreatment reactor has a higher total reaction conversion rate and selectivity under the same raw material conditions, which means that the raw material pretreatment unit can extend the operation cycle of the transalkylation catalyst under high bromine index conditions and achieve higher conversion efficiency and selectivity.
[0137] [Example 4]
[0138] use Figure 4The system shown in the figure performs an aromatic transalkylation reaction, wherein a material pretreatment device I is added between the heavy aromatic tower 2 and the feed buffer tank 3. At the same time, benzene and toluene are pretreated before entering the bleaching earth tower, that is, a material pretreatment device II is set between the aromatic extraction device and the bleaching earth tower, which is mainly used to remove water from the mixed material containing benzene and toluene; a material pretreatment device III is set between the circulating hydrogen compressor 13 and the material buffer tank 3, which is mainly used to remove carbon oxides in the circulating hydrogen.
[0139] Heavy aromatics from the paraxylene unit 11 enter the heavy aromatics tower 2 to separate C9 + Aromatic hydrocarbons S4 are used to adjust gasoline, and C9 aromatic hydrocarbons S8 are obtained at the same time. The C9 aromatic hydrocarbons S8 enter the material pretreatment device I for pretreatment (specifically, hydrocracking reaction). The pretreated C9 aromatic hydrocarbons S8 are mixed with toluene S7 and enter the feed buffer tank 3.
[0140] The mixed raw material 2 S10 after the circulating hydrogen S12, the supplementary hydrogen S1 and the mixed raw material 1 S9 are mixed enters the inlet and outlet heat exchanger 4, and after heat removal, the mixed material enters the transalkylation reactor 5 for reaction. The product S11 after the reaction exchanges heat with the mixed raw material 2 S10, and then enters the cooler 6, the gas-liquid separator 7, and the stripping tower 8 in sequence to obtain a liquid product.
[0141] The mixed material containing benzene and toluene from the aromatics extraction device 12 is mixed with the liquid phase product from the stripping tower 8 and then enters the clay tower 9, the benzene tower 10 and the toluene tower 1 in sequence. Among them, the benzene product S5 is separated from the benzene tower, and the C8 is separated from the toluene tower. + Aromatic hydrocarbon S6 and toluene S7 are obtained at the same time.
[0142] The material pretreatment device I is filled with a pretreatment catalyst A4, which is prepared as follows: 51 g of alumina (calcined at 550° C. for 3 h) and 45 g of ammonium FER / MTW molecular sieve (mass ratio 1 / 2) are mixed evenly, 4.66 g of iridium chloride and 0.69 g of chromium nitrate are dissolved in a small amount of distilled water and added to the mixed powder, and then 5 g of sesbania powder and 10 ml of nitric acid solution are added, fully kneaded and extruded, and the mixture is calcined at 500° C. for 3 h and then reduced at 400° C. and a pressure of 3 MPa for 4 h to obtain catalyst A4.
[0143] The material pretreatment device II and the material pretreatment device III are both filled with molecular sieves.
[0144] The reaction conditions in the material pretreatment unit I and the reaction conditions in the alkane transfer reactor are shown in Table 9.
[0145] [Comparative Example 10]
[0146] use Figure 2The system is carried out without material pretreatment device I, material pretreatment device II, and material pretreatment device III. The specific process is repeated in Example 4, except that material pretreatment is not performed. The reaction conditions in the material pretreatment device I and the reaction conditions in the alkane transfer reactor are shown in Table 9.
[0147] The performance comparison of Example 4 and Comparative Example 4 after different running times is shown in Table 10.
[0148] Table 9 Comparison of operating parameters of Example 4 and Comparative Example 10
[0149]
[0150] Table 10 Performance comparison of Example 4 and Comparative Example 10 after different running times
[0151]
[0152]
[0153] It can be seen from Tables 9 and 10 that in the initial stage of operation, the operating conditions of the transalkylation reactors in Example 4 and Comparative Example 10 are similar, and the carbon monoxide and water contents of the raw materials are different. In Example 4, the carbon monoxide and water contents in the transalkylation feed after the raw material pretreatment unit are significantly reduced. The catalyst performance of the two is similar in the initial stage of the reaction. After long-term operation, the transalkylation catalyst in Example 4 with the addition of a raw material pretreatment reactor has a higher total reaction conversion rate and selectivity under the same raw material conditions, which means that the raw material pretreatment unit can extend the operation cycle of the transalkylation catalyst under high bromine index conditions and achieve higher conversion efficiency and selectivity.
[0154] The present invention has been described in detail above in conjunction with specific implementations and exemplary examples, but these descriptions cannot be understood as limiting the present invention. Those skilled in the art understand that, without departing from the spirit and scope of the present invention, a variety of equivalent substitutions, modifications or improvements may be made to the technical solution of the present invention and its implementation methods, all of which fall within the scope of the present invention. The scope of protection of the present invention shall be subject to the attached claims.
Claims
1. A method for aromatic hydrocarbon transalkylation, the method comprising the following steps: Step 1, mixing C9 aromatic hydrocarbons and toluene to obtain mixed raw material 1, and further mixing the mixed raw material 1 with hydrogen to obtain mixed raw material 2; Step 2, reacting the mixed raw material 2 in the presence of a transalkylation catalyst to obtain a mixed product containing benzene and C8 aromatics; Step 3: The mixed product obtained in step 2 is heat exchanged with the mixed raw material 2 obtained in step 1, and then cooled and gas-liquid separated in sequence, the hydrogen obtained in the gas phase is recycled back to step 1, and the liquid is stripped; Before performing step 2, a pretreatment catalyst is used to pretreat C9 aromatics and / or mixed raw material 1 and / or mixed raw material 2 before heat exchange and / or mixed raw material 2 after heat exchange; the pretreatment catalyst comprises an oxide carrier, a first active component, a second active component and a molecular sieve, the carrier is a calcined carrier, the first active component is selected from at least one of cobalt, nickel, palladium, platinum, rhodium and iridium, the second active component is selected from at least one of zinc, rhenium, molybdenum, bismuth and chromium, and the mass ratio of the first active component to the second active component is (0.1-40):1 based on the mass of the metal element; the molecular sieve is a mixture of a molecular sieve with a maximum ring structure of 10 members and a molecular sieve with a maximum ring structure of 12 members, and the mass ratio of the molecular sieve with a maximum ring structure of 10 members to the molecular sieve with a maximum ring structure of 12 members is (0.1-0.2):1; the external specific surface area of the molecular sieve is higher than 30 m 2 / g, pore volume is 0.15~0.5 cm 3 / g, the percentage of micropores in the total pore volume is more than 40%; the carrier is selected from at least one of α-alumina, γ-alumina and silica.
2. The method according to claim 1, characterized in that The pretreatment conditions are: operating pressure 0.1-6.0 MPa, reaction temperature 100-420°C, reaction weight hourly space velocity 0.5-30.0 h -1 , the hydrogen-to-hydrocarbon molar ratio is 0.5-5.
0.
3. The method according to claim 2, characterized in that The pretreatment conditions are: operating pressure 2.0-4.0 MPa, reaction temperature 340-420°C, reaction weight hourly space velocity 5-20 h -1 , the hydrogen-to-hydrocarbon molar ratio is 3~5.
4. The method according to claim 1, characterized in that: Calculated by the mass of metal elements, the mass ratio of the first active component to the second active component is (0.1-20):
1.
5. The method according to claim 1, characterized in that The molecular sieve is at least one selected from MFI molecular sieve, MEI molecular sieve, MEL molecular sieve, MOR molecular sieve, FAU molecular sieve, STF molecular sieve, ITQ molecular sieve, BEA molecular sieve, MTW molecular sieve, MFI / MEL molecular sieve, MOR / MFI molecular sieve, MOR / MEL molecular sieve, MFI / FAU molecular sieve, BEA / MFI molecular sieve, and FAU / MEL molecular sieve.
6. The method according to claim 1, characterized in that The calcination temperature is 350-900°C.
7. The method according to claim 1, characterized in that The calcination temperature is 500-800°C.
8. The method according to claim 1, characterized in that In the pre-treated catalyst, the weight content of each component is as follows: 10-95% of the carrier, 4-80% of the molecular sieve, 0.08-10% of the first active component, and 0.1-20% of the second active component.
9. The method according to claim 1, characterized in that In step 1, the mass ratio of C9 aromatics to toluene is 100 / 0 to 0 / 100; and / or In step 1, the molar ratio of hydrogen to mixed raw material 1 is 10:1 to 0.5:1; and / or The reaction in step 2 is carried out as follows: reaction pressure 1.0-6.0 MPa, reaction temperature 300-550°C, hydrogen-to-hydrocarbon molar ratio 1-20, feed weight space velocity 1.0-100 h -1 Next proceed.
10. The method according to claim 9, characterized in that In step 1, the mass ratio of C9 aromatics to toluene is 20 / 70 to 80 / 20; and / or In step 1, the molar ratio of hydrogen to mixed raw material 1 is 5:1 to 1:
1.
11. The method according to any one of claims 1 to 10, characterized in that: The hydrogen may be optionally pretreated prior to mixing with the mixed feed.
12. The method according to claim 11, characterized in that The pretreatment is carried out in the presence of a molecular sieve and / or the pretreatment catalyst.
13. The method according to claim 11, characterized in that The method further comprises: performing optional pretreatment on the mixture of benzene and toluene from the aromatics extraction unit, and then mixing it with the liquid phase product after the gas stripping treatment in step 3 or entering the bleaching clay tower, benzene tower and toluene tower in sequence independently of each other.
14. The method according to claim 13, characterized in that The mixed material of benzene and toluene is pretreated in the presence of the molecular sieve and / or the pretreatment catalyst.
Citation Information
Patent Citations
Method for converting polycyclic aromatic hydrocarbons into monocyclic aromatic hydrocarbons to produce more dimethylbenzene
CN103121907A
Method for disproportionation and transalkylation of toluene and heavy aromatic hydrocarbon
CN105272803A
Method for producing p-xylene, o-xylene and 1,2,4-trimethylbenzene from coal-based raw materials
CN107473918A
Pre-treatment method for aromatic hydrocarbon
CN1377866A