A display panel and a method for manufacturing the same
By setting a metal barrier layer in the display panel, the problems of high packaging difficulty and polarization effects are solved, brightness and packaging reliability are improved, product life is extended, and package failure risk is reduced.
Patent Information
- Application Number
- CN202210201499.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-03
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-03-03
AI Technical Summary
In the prior art, the packaging of the O-Cut part of the display panel is difficult, resulting in an increase in the risk of packaging failure, and the polarization effect of the flexible substrate on the TFT affects the brightness drop and the afterimage phenomenon.
A metal barrier layer is provided in the display panel, which is connected to the TFT as a shield layer, which reduces the polarization effect of the flexible substrate on the TFT, and acts as a package barrier layer in the non-display area to improve the stability of O-cut and the package reliability.
It effectively improves the brightness drop and afterimage problems of the display panel, improves product life, and reduces the package failure ratio, and improves the stability and packaging reliability of O-cut.
Smart Images

Figure CN114582945B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of display panels, and in particular to a display panel and a method for preparing the same. Background Art
[0002] Compared with traditional liquid crystal displays, the reliability of TFT in the pixel circuit of organic light emitting diode (OLED) display technology is significantly affected by back channel etching due to the material properties of its flexible substrate PI. The reliability of TFT is a key factor affecting the luminance drop. Usually, image sticking is also one of the main phenomena of luminance drop.
[0003] Through the study of product afterimage, it is found that reducing the polarization effect of the flexible substrate PI on TFT can effectively improve the product life, brightness reduction and afterimage problems. In the prior art, a metal layer is set between the TFT and the PIC layer to form a shielding barrier layer, thereby reducing the polarization effect of the flexible substrate PI on the TFT.
[0004] In addition, the packaging of the O-Cut part of the display panel is difficult to prepare, and the process usually adopts chemical vapor deposition (CVD), but it still faces the risk of packaging failure.
[0005] Therefore, it is necessary to develop a new type of display panel to overcome the defect of high difficulty in packaging the O-Cut part of the prior art. Summary of the invention
[0006] An embodiment of the present invention provides a display panel to solve the technical problem of high difficulty in packaging an O-cut portion of a display panel in the prior art.
[0007] In order to solve the above technical problems, the embodiments of the present invention disclose the following technical solutions:
[0008] On the one hand, a display panel is provided, comprising a non-display area and a display area surrounding the non-display area; and a substrate layer extending from the display area to the non-display area; a metal barrier layer provided on the substrate layer, the metal barrier layer being spaced apart in the non-display area; a functional structure layer provided on the metal barrier layer; a light-emitting device layer provided on the functional structure layer; a slot provided in the non-display area, extending from a side of the light-emitting device layer away from the substrate layer, through the light-emitting device layer and the functional structure layer to the surface of the substrate layer and the metal barrier layer, the metal barrier layer and the substrate layer being exposed in the slot, and the metal barrier layer being located on the peripheral wall of the slot.
[0009] In addition to one or more features disclosed above, or as an alternative, the substrate layer includes a first flexible substrate; a first buffer layer, disposed on the first flexible substrate; a second flexible substrate, disposed on the second buffer layer; a second buffer layer, disposed on the second flexible substrate; and the second buffer layer is exposed in the slot.
[0010] In addition to one or more of the features disclosed above, or as an alternative, the functional structure layer includes a protective layer, which is arranged on the metal barrier layer and extends from the display area to the non-display area; an active layer, which is arranged on the protective layer in the display area; a first gate insulating layer, which is arranged on the active layer and covers the active layer, and extends from the display area to the non-display area; a first gate layer, which is arranged on the first gate insulating layer in the display area; a second gate insulating layer, which is arranged on the first gate layer and covers the first gate layer, and extends from the display area to the non-display area; a second gate layer, which is arranged on the second gate insulating layer in the display area; an interlayer dielectric layer, which is arranged on the second gate layer, and extends from the display area to the non-display area; a source and drain electrode layer, which is arranged on the surface of the interlayer dielectric layer in the display area; and a planarizing layer, which is arranged on the source and drain electrode layer, and extends from the display area to the non-display area.
[0011] In addition to one or more of the features disclosed above, or as an alternative, the functional structure layer also includes a first via, which is arranged in the display area and extends from a side of the interlayer dielectric layer away from the substrate layer to a side of the active layer away from the substrate layer, and the source and drain layer is connected to the active layer through the first via; and a second via is arranged in the display area and extends from a side of the interlayer dielectric layer away from the substrate layer to a side of the metal barrier layer away from the substrate layer, and the source and drain layer is connected to the metal barrier layer through the second via.
[0012] In addition to or as an alternative to one or more features disclosed above, the material filled in the first via hole and the second via hole is the same as the source and drain electrode layer.
[0013] In addition to or as an alternative to one or more of the features disclosed above, in the non-display area, the metal barrier layer includes a first barrier layer and a second barrier layer disposed on the first barrier layer.
[0014] In addition to or as an alternative to one or more features disclosed above, an orthographic projection of the second barrier layer on the substrate layer is larger than an orthographic projection of the first barrier layer on the substrate layer.
[0015] In addition to or as an alternative to one or more of the features disclosed above, the material used for the first barrier layer includes titanium and silver; the material used for the second barrier layer includes molybdenum or indium zinc oxide.
[0016] In addition to or as an alternative to one or more features disclosed above, in the non-display area, the metal barrier layer includes a first barrier layer and a second barrier layer, which are disposed on the first barrier layer; and a third barrier layer, which is disposed on the second barrier layer.
[0017] In addition to one or more features disclosed above, or as an alternative, the orthographic projection of the third barrier layer on the substrate layer is greater than the orthographic projection of the second barrier layer on the substrate layer, and the orthographic projection of the first barrier layer on the substrate layer is greater than or equal to the orthographic projection of the third barrier layer on the substrate layer.
[0018] In addition to or as an alternative to one or more features disclosed above, the material used for the first barrier includes titanium and silver; the material used for the second barrier layer includes aluminum or indium tin oxide; and the material used for the third barrier includes titanium and silver.
[0019] In addition to one or more of the features disclosed above, or as an alternative, the light-emitting device layer includes a pixel definition layer, which is disposed on the flat layer, and the pixel definition layer has an opening; an anode layer, which is disposed in the opening and connected to the source and drain; an OLED layer, which is disposed on the anode layer; and a cathode layer, which is disposed on the OLED layer.
[0020] On the other hand, a preparation method is further disclosed for preparing the display panel of the present invention, wherein the display panel comprises a non-display area and a display area surrounding the non-display area, and the preparation method comprises the following steps:
[0021] Providing a substrate layer, wherein the substrate layer extends from the display area to the non-display area;
[0022] Preparing a metal barrier layer on the substrate layer, wherein the metal barrier layer is disposed at intervals in the non-display area;
[0023] preparing a functional structural layer on the metal barrier layer;
[0024] A slot is prepared in the non-display area, wherein the slot penetrates the functional structure layer from a side of the functional structure layer away from the substrate layer and extends to the surface of the substrate layer and the metal barrier layer, the metal barrier layer and the substrate layer are exposed in the slot, and the metal barrier layer is located on the peripheral wall of the slot;
[0025] A light-emitting device layer is prepared on the functional structure layer, and the slots extend from a side of the light-emitting device layer away from the substrate layer through the light-emitting device layer and the functional structure layer to the surface of the substrate layer and the metal barrier layer.
[0026] One of the above technical solutions has the following advantages or beneficial effects: a metal barrier layer is arranged on the substrate layer. On the one hand, the metal barrier layer in the display area is connected to the source and drain to form a shielding layer, which can weaken the polarization effect of the flexible substrate on the TFT, improve the brightness drop and afterimage problems of the display panel, and thus increase the life of the product; on the other hand, the metal barrier layer in the non-display area serves as a packaging barrier layer, which can improve the stability and packaging reliability of the O-cut and effectively reduce the proportion of packaging failures; in addition, in the process of preparing the display panel, the metal barrier layer in the non-display area can be used as a mask for preparing slots, saving costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The technical solutions and other beneficial effects of the present invention will be made apparent by describing in detail the specific embodiments of the present invention in conjunction with the accompanying drawings.
[0028] Figure 1 A schematic cross-sectional structural diagram of a display panel provided in Embodiment 1 of the present invention;
[0029] Figure 2 A schematic cross-sectional structure diagram of a metal barrier layer in a non-display area provided in Embodiment 1 of the present invention;
[0030] Figure 3 A flow chart of a method for manufacturing a display panel provided in Embodiment 1 of the present invention;
[0031] Figure 4 This is a schematic diagram of the cross-sectional structure of the metal barrier layer in the non-display area provided in Example 2 of the present invention. Description of the drawings:
[0033] Display panel-100; Display area-101;
[0034] Non-display area - 102;
[0035] Substrate layer-110; Functional structure layer-120;
[0036] Light emitting device layer-130; Slot-140;
[0037] Metal barrier layer-150; First flexible substrate-111;
[0038] First buffer layer-112; Second flexible substrate-113;
[0039] Second buffer layer-114; Active layer-121;
[0040] First gate layer-123; First gate insulating layer-122;
[0041] A second gate layer-125; A second gate insulating layer-124;
[0042] Interlayer dielectric layer-126; Source and drain layer-127;
[0043] Flat layer-128; Protective layer-1201;
[0044] First via hole-161; Second via hole-162;
[0045] Pixel definition layer-131; Anode layer-132;
[0046] OLED layer-133; Cathode layer-134;
[0047] A first barrier layer-151; A second barrier layer-152;
[0048] The third barrier layer-153. DETAILED DESCRIPTION
[0049] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention.
[0050] Example 1
[0051] The embodiment of the present invention provides a display panel 100. Figure 1 , Figure 1 The cross-sectional structural schematic diagram of the display panel 100 provided in an embodiment of the present invention, the display panel 100 includes a display area 101 and a non-display area 102 surrounding the display area 101, and the display panel 100 includes a substrate 110, a metal barrier layer 150, a functional structure layer 120, a light-emitting device layer 130 and a slot 140.
[0052] The substrate layer 110 extends from the display area 101 to the non-display area 102, and includes a first flexible substrate 111, a first buffer layer 112, a second flexible substrate 113 and a second buffer layer 114. The first buffer layer 112 is arranged on the first flexible substrate 111, the second flexible substrate 113 is arranged on the first buffer layer 112, and the second buffer layer 114 is arranged on the second flexible substrate 113.
[0053] The metal barrier layer 150 is disposed on the second buffer layer 114 , and the metal barrier layer 150 is disposed at intervals in the non-display area 102 .
[0054] The functional structure layer 120 is disposed on the buffer layer 112, and the functional structure layer 120 extends from the display area 101 to the non-display area 102. The functional structure layer 120 includes a protective layer 1201, an active layer 121, a first gate insulating layer 122, a first gate layer 123, a second gate insulating layer 124, a second gate layer 125, an interlayer dielectric layer 126, a source-drain electrode layer 127, and a planar layer 128. Among them, the protective layer 1201 is disposed on the second buffer layer 114, and extends from the display area 101 to the non-display area 102; the active layer 121 is disposed on the protective layer 1201 in the display area 101; the first gate insulating layer 122 is disposed on the active layer 121, and covers the active layer 121, and extends from the display area 101 to the non-display area 102; the first gate layer 123 is disposed on the first gate insulating layer 122 in the display area 101; the second gate insulating layer 124 is disposed on the first gate layer 123 On, and covering the first gate layer 123, extending from the display area 101 to the non-display area 102; the second gate layer 125 is arranged on the second gate insulating layer 124 of the display area 101; the interlayer dielectric layer 126 is arranged on the second gate layer 125, extending from the display area 101 to the non-display area 102; the source and drain layer 127 is arranged on the surface of the interlayer dielectric layer 126 of the display area 101; the planarization layer 128 is arranged on the source and drain layer 127, extending from the display area 101 to the non-display area 102.
[0055] The functional structure layer 120 further includes a first via hole 161 and a second via hole 162. The first via hole 161 is provided in the display area 101, extending from a side of the interlayer dielectric layer 126 away from the second buffer layer 114 to a side of the active layer 121 away from the second buffer layer 114, and the source-drain electrode layer 127 is connected to the active layer 121 through the first via hole 161. The second via hole 162 is provided in the display area 101, extending from a side of the interlayer dielectric layer 126 away from the second buffer layer 114 to a side of the metal barrier layer 150 away from the second buffer layer 114, and the source-drain electrode layer 127 is connected to the metal barrier layer 150 through the second via hole 162. The materials filled in the first via hole 161 and the second via hole 162 are the same as those in the source-drain electrode layer 127.
[0056] The metal barrier layer 150 in the display area 101 is connected to the source-drain electrode layer 127 to form a shielding layer, which can reduce the polarization effect of the flexible substrate on the TFT, improve the brightness drop and afterimage problems of the display panel, and thus increase the life of the product.
[0057] The light emitting device layer 130 is disposed on the functional structure layer 120; the light emitting device layer 130 includes a pixel definition layer 131, an anode layer 132, an OLED layer 133 and a cathode layer 134. The pixel definition layer 131 is disposed on the flat layer 128, and the pixel definition layer 131 has an opening; the anode layer 132 is disposed in the opening and connected to the source and drain layer 127; the OLED layer 133 is disposed on the anode layer 132; and the cathode layer 134 is disposed on the OLED layer 133.
[0058] The slot 140 is arranged in the non-display area 102, and extends from the side of the light-emitting device layer 130 away from the substrate layer 110, through the light-emitting device layer 130 and the functional structure layer 120 to the surface of the second buffer layer 114 and the metal barrier layer 150. The metal barrier layer 150 and the second buffer layer 114 are exposed in the slot 140, and the metal barrier layer 150 is located on the peripheral wall of the slot 140.
[0059] The slot hole 140 area is the O-cut area of the display panel. The metal barrier layer 150 located on the peripheral wall of the slot hole 140 serves as a packaging barrier layer, which can improve the stability of the O-cut and the packaging reliability and effectively reduce the packaging failure ratio.
[0060] See also Figure 2 , Figure 2 Schematic diagram of the cross-sectional structure of the metal barrier layer in the non-display area. In this embodiment, the metal barrier layer 150 includes a first barrier layer 151 and a second barrier layer 152 disposed on the first barrier layer 151, and the orthographic projection of the second barrier layer 152 on the substrate layer 110 is larger than the orthographic projection of the first barrier layer 151 on the substrate layer 110, which can further improve the stability of the O-cut and the reliability of the packaging.
[0061] In this embodiment, the material of the first barrier layer 151 is titanium, and the material of the second barrier layer 152 is molybdenum; or the material of the first barrier layer 151 is silver, and the material of the second barrier layer 152 is indium zinc oxide.
[0062] The embodiment of the present invention further provides a manufacturing method for manufacturing the display panel 100 of the present invention. Figure 3 , Figure 3 The present invention provides a flow chart of a method for manufacturing a display panel according to an embodiment of the present invention. The method for manufacturing the display panel includes the following steps 1 to 5.
[0063] Step 1: Provide a substrate layer 110 , wherein the substrate layer 110 extends from the display area 101 to the non-display area 102 .
[0064] Specifically, step 1 includes step 11-step 12;
[0065] Step 11 : providing a first flexible substrate 111 , wherein the first flexible substrate 111 extends from the display area 101 to the non-display area 102 .
[0066] Step 12: Prepare a first buffer layer 112 on the first flexible substrate 111 , wherein the first buffer layer 112 extends from the display area 101 to the non-display area 102 .
[0067] Step 13 : preparing a second flexible substrate 113 on the first buffer layer 112 , wherein the second flexible substrate 113 extends from the display area 101 to the non-display area 102 .
[0068] Step 14: Prepare a second buffer layer 114 on the second flexible substrate 113 , wherein the second buffer layer 114 extends from the display area 101 to the non-display area 102 .
[0069] Step 2: Prepare a metal barrier layer 150 on the second buffer layer 114 . The metal barrier layer 150 is disposed at intervals in the non-display area 102 .
[0070] Step 3: Prepare a functional structure layer 120 on the metal barrier layer 150 , wherein the functional structure layer 120 extends from the display area 101 to the non-display area 102 .
[0071] Specifically, step 3 includes steps 31 to 39;
[0072] Step 31 : Prepare a protection layer 1201 on the metal barrier layer 150 . The protection layer 1201 covers the metal barrier layer 150 . The protection layer 1201 extends from the display area 101 to the non-display area 102 .
[0073] Step 32: deposit polysilicon on the protective layer 1201 on the display area 101, prepare a semiconductor layer pattern by photolithography, and form an active layer 121; the thickness of the active layer 121 is
[0074] Step 33: preparing a first gate insulating layer 122 on the active layer 121 and covering the active layer 121 , wherein the first gate insulating layer 122 extends from the display area 101 to the non-display area 102 ;
[0075] Step 34: preparing a first gate layer 123 on the first gate insulating layer 122 of the display area 101;
[0076] Step 35: preparing a second gate insulating layer 124 on the first gate layer 123 and covering the first gate layer 123 , wherein the second gate insulating layer 124 extends from the display area 101 to the non-display area 102 ;
[0077] Step 36: preparing a second gate layer 125 on the second gate insulating layer 124 of the display area 101;
[0078] Step 37: prepare an interlayer dielectric layer 126 on the second gate layer 125, and form a first via hole 161 and a second via hole 162 by photolithography and dry etching;
[0079] Step 38: depositing source and drain electrodes on the surface of the interlayer dielectric layer 126, and connecting them to the active layer 121 through the first via hole 161, and connecting them to the metal barrier layer through the second via hole 162, and preparing source and drain electrode patterns by photolithography and wet etching to form a source and drain electrode layer 127;
[0080] Step 39 : Prepare a planar layer 128 on the source-drain electrode layer 127 , wherein the planar layer 128 extends from the display area 101 to the non-display area 102 .
[0081] Step 4: Prepare a slot 140 in the non-display area 102, the slot 140 extends from the side of the light-emitting device layer 130 away from the substrate layer 110, through the light-emitting device layer 130 and the functional structure layer 120 to the surface of the second buffer layer 114 and the metal barrier layer 150, the metal barrier layer 150 and the second buffer layer 114 are exposed in the slot 140, and the metal barrier layer 150 is located on the peripheral wall of the slot 140.
[0082] Specifically, the metal barrier layer can be used as a mask for preparing slots, saving a mask and thus saving costs.
[0083] Step 5: Prepare the light-emitting device layer 130 on the functional structure layer 120 .
[0084] When the light emitting device layer 130 is prepared, the metal barrier layer 150 in the non-display area 102 is exposed to the air.
[0085] Specifically, step 5 includes step 51 to step 54;
[0086] Step 51: Depositing ITO / Ag / ITO on the source and drain electrode layers to form an anode layer 132;
[0087] Step 52: preparing a pixel definition layer 131 on the planar layer 128, wherein the pixel definition layer 131 has an opening, and the anode layer 132 is located in the opening;
[0088] Step 53: Prepare an OLED layer 133 on the anode layer 132;
[0089] Step 54 : Prepare a cathode layer 134 on the OLED layer 133 .
[0090] Step 6: Etching the first barrier layer 151 and the second barrier layer 152 in the non-display area 102 .
[0091] The second barrier layer 152 located on the upper layer is used as an etching barrier layer to etch the first barrier layer 151 on the lower layer to form a side etching.
[0092] Example 2
[0093] The display panel of this embodiment has a substantially similar structure to that of Embodiment 1. For details, please refer to Embodiment 1. The difference is that the structure of the technical barrier layer in the non-display area is Figure 4 , Figure 4 Schematic diagram of the cross-sectional structure of the metal barrier layer in the non-display area. In this embodiment, the metal barrier layer 150 includes a first barrier layer 151, a second barrier layer 152 disposed on the first barrier layer 151, and a third barrier layer 153 disposed on the second barrier layer 152. The orthographic projection of the third barrier layer 153 on the substrate layer 110 is greater than the orthographic projection of the second barrier layer 152 on the substrate layer 110, and the orthographic projection of the first barrier layer 151 on the substrate layer 110 is greater than or equal to the orthographic projection of the third barrier layer 153 on the substrate layer 110. Compared with Example 1, the stability of the O-cut and the reliability of the packaging can be further improved.
[0094] In this embodiment, the material used for the first barrier layer 151 is titanium, the material used for the second barrier layer 152 is aluminum, and the material used for the third barrier layer 153 is titanium; or the material used for the first barrier layer 151 is silver, the material used for the second barrier layer 152 is indium tin oxide, and the material used for the third barrier layer 153 is silver.
[0095] The above is a detailed introduction to a display panel and a preparation method thereof provided in an embodiment of the present invention. Specific examples are used herein to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the technical solutions and core ideas of the present invention. Ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A display panel, characterized in that: comprising a non-display area and a display area surrounding the non-display area; as well as a substrate layer extending from the display area to the non-display area; A metal barrier layer is disposed on the substrate layer, at least a portion of the metal barrier layer is located in the display area, and the metal barrier layer is disposed at intervals in the non-display area; A functional structure layer is disposed on the metal barrier layer, the functional structure layer comprises a source-drain electrode layer, the source-drain electrode layer is disposed in the display area, and the source-drain electrode layer is connected to the metal barrier layer; A light emitting device layer, disposed on the functional structure layer; A slot is provided in the non-display area, and extends from a side of the light-emitting device layer away from the substrate layer, through the light-emitting device layer and the functional structure layer to the surface of the substrate layer and the metal barrier layer, the metal barrier layer and the substrate layer are exposed in the slot, and the metal barrier layer is located on the peripheral wall of the slot.
2. The display panel according to claim 1, wherein: The substrate layer includes a first flexible substrate; A first buffer layer, disposed on the first flexible substrate; A second flexible substrate, disposed on the first buffer layer; A second buffer layer, disposed on the second flexible substrate; The second buffer layer is exposed in the slot.
3. The display panel according to claim 1, wherein: The functional structural layer includes A protective layer, disposed on the metal barrier layer, extending from the display area to the non-display area; An active layer, disposed on the protective layer of the display area; A first gate insulating layer, disposed on the active layer, covers the active layer, and extends from the display area to the non-display area; A first gate layer, disposed on the first gate insulating layer in the display area; a second gate insulating layer, disposed on the first gate layer, covering the first gate layer, and extending from the display area to the non-display area; A second gate layer, disposed on the second gate insulating layer in the display area; an interlayer dielectric layer, disposed on the second gate layer and extending from the display area to the non-display area; The source-drain electrode layer is disposed on the surface of the interlayer dielectric layer in the display area; The planar layer is disposed on the source and drain electrode layer and extends from the display area to the non-display area.
4. The display panel according to claim 3, wherein: The functional structural layer also includes a first via hole, provided in the display area, extending from a side of the interlayer dielectric layer away from the substrate layer to a side of the active layer away from the substrate layer, wherein the source and drain electrode layer is connected to the active layer through the first via hole; The second via hole is provided in the display area, extending from a side of the interlayer dielectric layer away from the substrate layer to a side of the metal barrier layer away from the substrate layer, and the source and drain electrode layer is connected to the metal barrier layer through the second via hole.
5. The display panel according to claim 4, wherein: The material filled in the first via hole and the second via hole is the same as that of the source and drain electrode layer.
6. The display panel according to claim 1, wherein: In the non-display area, the metal barrier layer includes a first barrier layer and a second barrier layer disposed on the first barrier layer.
7. The display panel according to claim 6, wherein: The orthographic projection of the second barrier layer on the substrate layer is larger than the orthographic projection of the first barrier layer on the substrate layer.
8. The display panel according to claim 1, wherein: In the non-display area, the metal barrier layer includes First barrier layer a second barrier layer, disposed on the first barrier layer; The third barrier layer is disposed on the second barrier layer.
9. The display panel according to claim 8, wherein: The orthographic projection of the third barrier layer on the substrate layer is greater than the orthographic projection of the second barrier layer on the substrate layer, and the orthographic projection of the first barrier layer on the substrate layer is greater than or equal to the orthographic projection of the third barrier layer on the substrate layer.
10. A preparation method, characterized in that: The method for preparing the display panel according to claim 1, wherein the display panel comprises a non-display area and a display area surrounding the non-display area, and the preparation method comprises the following steps: Providing a substrate layer, wherein the substrate layer extends from the display area to the non-display area; Preparing a metal barrier layer on the substrate layer, wherein at least a portion of the metal barrier layer is located in the display area, and the metal barrier layer is disposed at intervals in the non-display area; Preparing a functional structure layer on the metal barrier layer, wherein the functional structure layer includes a source-drain electrode layer, the source-drain electrode layer is arranged in the display area, and the source-drain electrode layer is connected to the metal barrier layer; A slot is prepared in the non-display area, wherein the slot penetrates the functional structure layer from a side of the functional structure layer away from the substrate layer and extends to the surface of the substrate layer and the metal barrier layer, the metal barrier layer and the substrate layer are exposed in the slot, and the metal barrier layer is located on the peripheral wall of the slot; A light-emitting device layer is prepared on the functional structure layer, and the slots extend from a side of the light-emitting device layer away from the substrate layer through the light-emitting device layer and the functional structure layer to the surface of the substrate layer and the metal barrier layer.