Electrocatalytic in-situ Mössbauer spectroscopy and in-situ X-ray absorption spectroscopy test sample cell

By designing the electrocatalytic in situ Mussbor spectrum and in situ X-ray absorption spectrum test sample pool, the problem that the existing technology cannot truly observe catalyst changes in the in situ environment is solved, and high-precision sample analysis and high resolution are achieved Spectrum acquisition, suitable for in-situ testing of electrocatalytic reactions.

CN114609165BActive Publication Date: 2024-11-08DALIAN INSTITUTE OF CHEMICAL PHYSICS CHINESE ACADEMY OF SCIENCES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011431535.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-07
Publication Date
2024-11-08
Estimated Expiration
2040-12-07

AI Technical Summary

Technical Problem

The existing electrocatalytic in-situ Mussbor spectral testing technology cannot truly observe the changes in the phase, valence and coordination of the catalyst in the in-situ environment, and the test results are greatly affected by the voltage and sample changes after detachment of the electrolyte. , lacks high precision and high resolution.

Method used

An electrocatalytic in situ Musberg spectrum and in situ X-ray absorption spectrum test sample cell is designed, including the sample cell cavity and a scaffold, equipped with working electrodes, reference electrodes, conductive substrates and lead plates, which can be in situ Under conditions, the Mussbor spectral effect of the sample is observed, and combined with the gas supply device, radioactive source, detector and electrochemical workstation can achieve the acquisition of high-resolution spectra.

Benefits of technology

It realizes high-precision analysis of the composition, structure, adsorption, coordination environment and valence changes of the sample under in situ conditions, can withstand strong acid or strong alkali environments, and has good temperature tolerance and gamma ray shielding, ensuring Test the validity of the signal.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114609165B_ABST
    Figure CN114609165B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of electrocatalytic phase, valence state and coordination testing, specifically, an electrocatalytic in-situ Mössbauer spectroscopy and in-situ X-ray absorption spectroscopy testing sample cell, comprising a sample cell cavity and a bracket, the sample cell cavity is arranged in the bracket, the upper end of the sample cell cavity is sealed and a working electrode is arranged in the middle, a reference electrode and an air inlet are arranged on one side of the upper end of the sample cell cavity, and a counter electrode and an air outlet are arranged on the other side, an electrolyte is arranged in the sample cell cavity, and the lower end of the reference electrode and the lower end of the counter electrode are both inserted into the electrolyte, a conductive substrate is arranged at the lower end of the working electrode and is placed in the electrolyte, a lead plate with a through hole in the middle is arranged on the rear side of the bracket, and the conductive substrate is directly opposite to the lead plate through hole. The present invention can observe the Mössbauer spectroscopy effect or corresponding X-ray of the test sample under any reaction atmosphere under in-situ conditions and obtain a corresponding high-resolution spectrum, and analyze the composition, structure, adsorption, coordination environment, valence state, spin state and other changes of the sample in-situ with high precision.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of electrocatalytic phase, valence state and coordination testing, in particular to an electrocatalytic in-situ Mossbauer spectrum and in-situ X-ray absorption spectrum testing sample cell. Background Art

[0002] The Mössbauer effect is a science that studies the behavior of electrons outside the nucleus by observing the resonance absorption of gamma rays by the atomic nucleus. It is widely used in many chemical fields such as material structure, chemical bonding, and in-situ state analysis. The Mössbauer effect has a very high energy sensitivity, and the energy difference it detects can reach 10 -8 eV, the test signal has a very high resolution, and it is non-destructive, which has advantages over conventional technology characterization for catalyst characterization.

[0003] Domestic electrocatalytic in situ Musspectrographic testing technologies are mostly quasi-in situ Musspectrographic testing, and the testing system is not mature. The test results can show the phase change law of the sample at different reaction stages to a certain extent, but this quasi-in situ testing method cannot avoid the inevitable changes of the catalyst sample when there is no applied voltage and after it is separated from the electrolyte. It cannot truly reflect the changes in the phase, valence state, coordination, etc. of the catalyst sample in the in situ environment. Summary of the invention

[0004] The object of the present invention is to provide an electrocatalytic in-situ Mössbauer spectroscopy and in-situ X-ray absorption spectroscopy test sample cell, which can observe the Mössbauer spectroscopy effect or corresponding X-rays of the test sample in any reaction atmosphere under in-situ conditions and obtain the corresponding high-resolution spectrum, and analyze the changes in the composition, structure, adsorption, coordination environment, valence state, spin state, etc. of the sample in-situ with high precision.

[0005] The objective of the present invention is achieved through the following technical solutions:

[0006] The invention discloses an electrocatalytic in-situ Mössbauer spectroscopy and in-situ X-ray absorption spectroscopy test sample cell, comprising a sample cell cavity and a bracket, wherein the sample cell cavity is arranged in the bracket, the upper end of the sample cell cavity is sealed and a working electrode is arranged in the middle, a reference electrode and an air inlet are arranged on one side of the upper end of the sample cell cavity, and a counter electrode and an air outlet are arranged on the other side, an electrolyte is arranged in the sample cell cavity, and the lower ends of the reference electrode and the counter electrode are both inserted into the electrolyte, a conductive substrate is arranged at the lower end of the working electrode and is placed in the electrolyte, a lead plate with a through hole in the middle is arranged at the rear side of the bracket, and the conductive substrate is directly opposite to the through hole of the lead plate.

[0007] A sealing cover is provided at the upper end of the sample pool cavity, a working electrode is provided in the middle of the sealing cover, a reference electrode and an air inlet are provided on one side of the sealing cover in sequence from the inside to the outside, and a counter electrode and an air outlet are provided on the other side of the sealing cover in sequence from the inside to the outside.

[0008] The sealing cover is provided with a plurality of mounting holes with sealing rings, and the working electrode, reference electrode, air inlet, counter electrode and air outlet are respectively inserted into the corresponding mounting holes.

[0009] The air inlet pipeline enters through the air inlet hole and is inserted into the electrolyte, and the air outlet pipeline is located above the electrolyte liquid level and is led out through the air outlet hole.

[0010] The lower side of the bracket forms a clamping plate.

[0011] A sample cell test system for electrocatalytic in-situ Mössbauer spectroscopy and in-situ X-ray absorption spectroscopy testing comprises a gas supply device, a radiation source, a detector, a Mössbauer spectroscopy control system, an electrochemical workstation and a data analysis device, wherein the gas supply device is connected to the gas inlet via an air inlet pipeline, the radiation source is arranged at the front side of the sample cell cavity, the detector is arranged at the rear side of the sample cell cavity, and the detector is connected to the Mössbauer spectroscopy control system via a line, the reference electrode, the working electrode and the counter electrode are connected to the electrochemical workstation via a line, and the electrochemical workstation is connected to the data analysis device via a line.

[0012] The advantages and positive effects of the present invention are:

[0013] 1. The present invention can observe the Mössbauer spectroscopy effect or corresponding X-ray of the test sample in any reaction atmosphere under in-situ conditions and obtain the corresponding high-resolution spectrum, and analyze the changes in the composition, structure, adsorption, coordination environment, valence state, spin state, etc. of the sample in-situ with high precision.

[0014] 2. The sample cell cavity of the present invention can withstand strong acid or strong alkali (PH = 0 ~ 14) and has good temperature tolerance (0 ~ 140 ° C). In addition, the lead plate arranged on the rear side of the sample cell cavity bracket can effectively block the remaining gamma rays that do not irradiate the sample or scatter, thereby ensuring the effectiveness of the sample signal.

[0015] 3. The present invention is simple and convenient to operate. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a three-dimensional schematic diagram of the present invention,

[0017] Figure 2 for Figure 1 The front view of the present invention,

[0018] Figure 3 for Figure 1 A rear view of the present invention,

[0019] Figure 4 A schematic diagram of a test system using the present invention is shown in FIG.

[0020] Figure 5 The in-situ test results of the NiFe oxyhydroxide oxygen evolution catalyst of the present invention are shown in FIG. Figure 1 ,

[0021] Figure 6 The in-situ test results of the NiFe oxyhydroxide oxygen evolution catalyst of the present invention are shown in FIG. Figure 2 ,

[0022] Figure 7 The in-situ test results of the NiFe oxyhydroxide oxygen evolution catalyst of the present invention are shown in FIG. Figure 3 ,

[0023] Figure 8 The in-situ test results of the NiFe oxyhydroxide oxygen evolution catalyst of the present invention are shown in FIG. Figure 4 ,

[0024] Fig. 9 Schematic diagram of the in-situ test results of the NiFe oxyhydroxide oxygen evolution catalyst of the present invention Figure 5 .

[0025] Among them, 1 is the air inlet; 2 is the air outlet; 3 is the radiation source; 4 is the conductive substrate; 5 is the electrolyte; 6 is the card board; 7 is the reference electrode; 8 is the working electrode; 9 is the counter electrode; 10 is the sealing cover; 11 is the detector; 12 is the bracket; 13 is the lead plate, and 14 is the sample pool cavity. DETAILED DESCRIPTION

[0026] The present invention will be further described below in conjunction with the accompanying drawings.

[0027] like Figures 1 to 4 As shown, the present invention includes a sample cell cavity 14 and a bracket 12, the sample cell cavity 14 is arranged in the bracket 12, and a sealing cover 10 is arranged on the upper side of the sample cell cavity 14, a working electrode 8 is arranged in the middle of the sealing cover 10, a reference electrode 7 and an air inlet 1 are arranged on one side of the sealing cover 10 from the inside to the outside, and a counter electrode 9 and an air outlet 2 are arranged on the other side of the sealing cover 10 from the inside to the outside. An electrolyte 5 is arranged in the sample cell cavity 14, the lower ends of the reference electrode 7 and the counter electrode 9 are both inserted into the electrolyte 5, a conductive substrate 4 is arranged at the lower end of the working electrode 8 and is placed in the electrolyte 5, an air inlet pipeline enters through the air inlet 1 and is inserted into the electrolyte 5, and an air outlet pipeline is located above the liquid level of the electrolyte 5 and is led out from the air outlet 2, as shown in FIG. Figure 3 As shown, a lead plate 13 with a through hole in the middle is provided at the rear side of the bracket 12, and the conductive substrate 4 is directly opposite to the through hole of the lead plate 13. Figure 4As shown, when the present invention is working, the radiation source 3 located at the front side of the sample pool cavity 14 emits gamma rays, and in addition to irradiating the interior of the sample pool cavity 14, the rays also pass through the through hole in the middle of the lead plate 13 and enter the detector 11 on the rear side of the sample pool cavity 14. The lead plate 13 can effectively block the remaining gamma rays that do not irradiate the sample or are scattered, thereby ensuring the validity of the sample signal.

[0028] like Figure 1 As shown, the sealing cover 10 is provided with a plurality of mounting holes with sealing rings, and the working electrode 8, the reference electrode 7, the air inlet 1, the counter electrode 9 and the air outlet 2 are respectively inserted into the corresponding mounting holes.

[0029] like Figure 1 As shown, a card plate 6 is formed on the lower side of the bracket 12, which can be conveniently fixed in a matching card slot on the system, thereby fixing the present invention.

[0030] The sample pool cavity 14 is made of polypropylene or polyethylene, preferably polypropylene (PP), with a wall thickness of 0.2 to 1.5 mm, preferably 0.7 mm. The sample pool cavity 14 can tolerate a pH range of PH = 0 to 14, and a temperature tolerance range of 0 to 140 ° C, which meets the test requirements. At the same time, the sample pool PP material has almost no obstruction to gamma rays and will not affect the test results. In addition, the overall thickness of the sample pool cavity 14 is 3 to 10 mm (preferably 6 mm), which ensures that the catalyst and the electrolyte 5 are effectively in contact and react, and can also ensure that the gamma rays can pass through the sample to obtain an effective signal.

[0031] The reference electrode 7 can be made of materials such as silver chloride electrode, mercuric oxide electrode, saturated calomel electrode, etc., and can be replaced according to the reaction system.

[0032] The counter electrode 9 is made of materials such as platinum wire electrode, platinum sheet electrode, carbon rod, etc., and can be replaced according to the reaction system.

[0033] The working electrode 8 is a copper rod with an open bottom and a diameter of 3 mm.

[0034] The conductive substrate 4 is carbon paper or carbon cloth, and the catalyst is evenly coated on the carbon paper or carbon cloth. A conductive substrate made of other materials may also be used as required.

[0035] The electrolyte 5 in the sample cell cavity 14 can be acidic, alkaline or neutral (or organic or inorganic), and can be changed according to the reaction system.

[0036] The bracket 12 is made of alloy material and has a thickness of 0.5-2 mm, preferably 1 mm.

[0037] The diameter of the middle through hole of the lead plate 13 is 1-30 mm, preferably 15 mm, and the thickness of the lead plate 13 is ≥1 mm, which can effectively shield the gamma rays passing to the outside, while ensuring that the rays from the radiation source 3 can pass stably, and avoiding the absorption of the rays by the surrounding area to interfere with the sample signal.

[0038] A test system using the present invention is as follows Figure 4 As shown, in addition to the sample cell of the present invention, it also includes a gas supply device, a radiation source 3, a detector 11, a Mössbauer spectrum control system, an electrochemical workstation and a data analysis device, wherein the gas supply device is connected to the gas inlet 1 through an air inlet pipeline, the radiation source 3 is arranged at the front side of the sample cell cavity 14, the detector 11 is arranged at the rear side of the sample cell cavity 14, and the detector 11 is connected to the Mössbauer spectrum control system through a line, the reference electrode 7, the working electrode 8 and the counter electrode 9 are connected to the electrochemical workstation through a line, and the electrochemical workstation is connected to the data analysis device through a line. During in-situ testing, the detector 11 can automatically collect data, and only the voltage and current parameters on the electrochemical workstation connected to the three electrodes need to be changed.

[0039] The gas supply device may adopt a gas cylinder, and may adopt reaction gas or protective gas such as carbon dioxide, hydrogen, oxygen, nitrogen, etc., and may adopt a corresponding test atmosphere according to the needs of the test system.

[0040] The detector 11 and the Mössbauer spectroscopy control system are commercially available products. In this embodiment, the Mössbauer spectroscopy control system is MFD-500AV-02. The data analysis device is a computer. The electrochemical workstation and the data analysis device are also commercially available products.

[0041] The working principle of the present invention is:

[0042] like Figure 4 As shown, when the present invention is working, the radiation emitted by the radiation source 3 passes through the conductive substrate 4 in the electrolyte 5, and is emitted from the central through hole of the lead plate 13 to the detector 11. The detector 11 can automatically collect data by simply changing the voltage and current parameters on the electrochemical workstation connected to the three electrodes.

[0043] The working principle of the present invention is further illustrated by taking an application example below.

[0044] Application example 1: In-situ valence change of NiFe oxyhydroxide oxygen evolution catalyst in water electrolysis reaction.

[0045] First, the NiFe hydroxide catalyst was evenly dispersed in the dispersion, and then the slurry was evenly coated on the conductive substrate 4 (carbon paper in this application example) with a loading of 0.5 mg cm -2The conductive substrate 4 is connected to a copper rod with an opening at the bottom as a working electrode 8, and then 1 mol L -1 KOH electrolyte (occupying about two-thirds of the cavity volume), covered with a sealing cover 10, and then the counter electrode 9 and the reference electrode 7 are respectively inserted, the air inlet pipe enters through the air inlet hole 1 and is inserted below the electrolyte 5 liquid surface, and the air outlet pipe is inserted through the air outlet hole 2 and the opening is located above the electrolyte 5 liquid surface.

[0046] like Figure 4 As shown, after the gas line is connected, adjust the gas line, and then continue to introduce oxygen into the sample cell chamber 14 (20mLmin -1 ), after 30 minutes when the oxygen in the electrolyte 5 is fully saturated, the end of the card plate 6 on the lower side of the sample cell cavity 14 is inserted into the corresponding card slot of the test system and fixed, the reference electrode 7, the working electrode 8 and the counter electrode 9 are connected and the gas is continuously introduced, the electrochemical workstation is turned on, the time potential is started, and the constant potential mode is adopted, and the values ​​are 0, 1.42, 1.47, 1.57 V (vs. RHE, relative to the standard hydrogen electrode), and the Mössbauer spectrum control system test software is turned on to start spectrum acquisition.

[0047] Figures 5 to 9 The in-situ test results of the NiFe oxyhydroxide oxygen evolution catalyst using the present invention are as follows: Figure 5 This is the high-resolution Mus spectrum test diagram of the initial sample under the electrocatalytic in-situ Mus spectrum test (OV). Figure 6 This is the high-resolution Mus spectrum test image of the sample transition state-1 under the electrocatalytic in-situ Mus spectrum test (1.42V). Figure 7 This is the high-resolution Mus spectrum test image of the sample transition state-2 under the electrocatalytic in-situ Mus spectrum test (1.47V). Figure 8 This is the high-resolution Mus spectrum test diagram of the transition state-3 of the sample under the electrocatalytic in-situ Mus spectrum test (1.57V). Fig. 9 This is a high-resolution Mus spectroscopy test diagram of the final state of the sample reaction under electrocatalytic in-situ Mus spectroscopy testing.

[0048] Figures 5 to 9 The results show that Figure 5 and Fig. 9 The results of the prepared catalyst before and after the reaction at room temperature show that Fe exists in the form of trivalent iron before and after the reaction. Figures 6 to 8 The change of tetravalent iron content with increasing voltage indicates that the content of tetravalent iron, an active species, gradually increases with increasing applied voltage, which provides practical guidance for the study of the reaction mechanism of NiFe-based catalysts.

[0049] This patent can be used for 57 Fe, 119 Sn, 151The related reactions of Eu and other Mossbauer nuclides are tested in situ in electrocatalytic reactions such as hydrogen evolution in water electrolysis, oxygen evolution reaction, oxygen reduction reaction (metal-air electrode), carbon dioxide reduction, and ammonia synthesis. In addition, Mossbauer spectroscopy (Mossbauer spectroscopy) uses keV-level gamma rays, which still have good signals in 6mm thick electrolytes, so it can detect in-situ changes of samples under liquid phase conditions (alkaline, acidic, neutral or organic, inorganic and other electrolytes). Therefore, the present invention can provide in-situ detection under the real conditions of the reaction and its fine structure can detect the chemical, structural and magnetic changes of Mossbauer elements.

Claims

1. An electrocatalytic in-situ Mössbauer spectroscopy and in-situ X-ray absorption spectroscopy test sample cell, characterized in that: The invention comprises a sample cell cavity (14) and a support (12), wherein the sample cell cavity (14) is arranged in the support (12), the upper end of the sample cell cavity (14) is sealed and a working electrode (8) is arranged in the middle, a reference electrode (7) and an air inlet (1) are arranged on one side of the upper end of the sample cell cavity (14), and a counter electrode (9) and an air outlet (2) are arranged on the other side, an electrolyte (5) is arranged in the sample cell cavity (14), and the lower ends of the reference electrode (7) and the counter electrode (9) are both inserted into the electrolyte (5), a conductive substrate (4) is arranged at the lower end of the working electrode (8) and is placed in the electrolyte (5), and a lead plate (13) with a through hole in the middle is arranged on the rear side of the support (12), and the conductive substrate (4) is directly opposite to the through hole of the lead plate (13); A sealing cover (10) is provided at the upper end of the sample cell cavity (14), a working electrode (8) is provided in the middle of the sealing cover (10), a reference electrode (7) and an air inlet (1) are provided on one side of the sealing cover (10) in sequence from the inside to the outside, and a counter electrode (9) and an air outlet (2) are provided on the other side of the sealing cover (10) in sequence from the inside to the outside; the sample cell cavity (14) is made of polypropylene or polyethylene, and the overall thickness of the sample cell cavity (14) is 3 to 10 mm; The sealing cover (10) is provided with a plurality of mounting holes with sealing rings, and the working electrode (8), the reference electrode (7), the air inlet (1), the counter electrode (9) and the air outlet (2) are respectively inserted into the corresponding mounting holes; During testing, an electrolyte is first injected into the sample cell cavity (14), and then the sealing cover (10) is covered, and then the counter electrode (9) and the reference electrode (7) are respectively inserted, and the air inlet pipeline enters through the air inlet hole (1) and is inserted into the electrolyte (5), and the air outlet pipeline is located above the liquid level of the electrolyte (5) and is discharged from the air outlet hole (2).

2. The electrocatalytic in-situ Mössbauer spectroscopy and in-situ X-ray absorption spectroscopy test sample cell according to claim 1, characterized in that: A clamping plate (6) is formed on the lower side of the bracket (12).

3. An electrocatalytic in-situ Mössbauer spectroscopy and in-situ X-ray absorption spectroscopy test sample cell test system according to claim 1, characterized in that: The invention comprises a gas supply device, a radioactive source (3), a detector (11), a Mössbauer spectrum control system, an electrochemical workstation and a data analysis device, wherein the gas supply device is connected to the gas inlet (1) via a pipeline, the radioactive source (3) is arranged at the front side of the sample cell cavity (14), the detector (11) is arranged at the rear side of the sample cell cavity (14), and the detector (11) is connected to the Mössbauer spectrum control system via a line, the reference electrode (7), the working electrode (8) and the counter electrode (9) are connected to the electrochemical workstation via a line, and the electrochemical workstation is connected to the data analysis device via a line.