Angled Flip-Chip Bump Layout
By designing an angled flip-chip bump layout and non-zero angle gaps on the VCSEL chip, the crack problem caused by mechanical strain in traditional chips is solved, and the performance and reliability of the chip are improved.
Patent Information
- Application Number
- CN202111457928.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-02
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-12-02
AI Technical Summary
Traditional flip-chip VCSEL chips are prone to cracks due to mechanical strain when the pads and bumps are aligned with the crystal cleavage plane, affecting the performance and reliability of the chip.
Design an angled flip-chip bump layout so that the bumps are not aligned with the crystal cleavage plane, and set non-zero angle gaps on the chip to reduce the distribution of mechanical stress along the crystal cleavage plane.
It effectively reduces the mechanical stress generated by the chip along the crystal cleavage plane, reduces the occurrence rate of cracks, and improves the performance and reliability of the chip.
Smart Images

Figure CN114665377B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to U.S. Provisional Patent Application No. 63 / 130,235, filed on December 23, 2020, entitled “ANGLED FLIP CHIP PAD LAYOUT TO REDUCE CRACKING ALONG ACRYSTALCLEAVAGE PLANE,” the contents of which are incorporated herein by reference in their entirety. Technical Field
[0003] The present disclosure relates generally to angled flip-chip bump layouts and, more particularly, to angled vertical cavity surface emitting laser (VCSEL) flip-chip layouts. Background Art
[0004] A vertical emitting device such as a VCSEL is a laser in which the beam is emitted in a direction perpendicular to the substrate surface (e.g., perpendicularly from the surface of a semiconductor wafer). Multiple vertical emitting devices can be arranged in an array with a common substrate associated with one or more crystal axes. Summary of the invention
[0005] In some embodiments, an optical device for mounting in a flip-chip configuration includes a plurality of flip-chip bumps arranged in a pattern on the optical device, wherein the pattern is not aligned with a crystal cleavage plane of a substrate associated with the optical device.
[0006] In some embodiments, an optical device for mounting in a flip-chip structure includes: a primary region; a secondary region; and a gap separating the primary region and the secondary region, wherein at least a portion of a side of the gap is oriented at a non-zero angle relative to a crystal cleavage plane associated with a substrate of the optical device.
[0007] In some embodiments, a chip includes: a plurality of chips including a plurality of chip bumps; and a crystal cleavage plane associated with the chip, wherein: the plurality of chip bumps are arranged in a pattern on the plurality of chips; and the pattern is not aligned with the crystal cleavage plane.
[0008] In some embodiments, a wafer comprises: a plurality of chips comprising a plurality of gaps; and a crystal cleavage plane associated with the wafer, wherein: the plurality of gaps are oriented at a non-zero angle to the crystal cleavage plane. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1A-1B The figure shows a side view of a conventional flip-chip VCSEL device chip.
[0010] Figures 2A-2C is a bottom view of an example chip of an optical device.
[0011] Figures 3A-3C is a bottom view of an example chip of an optical device.
[0012] Figure 4A-4B is a schematic diagram of an example implementation described herein. DETAILED DESCRIPTION
[0013] The following detailed description of example implementations refers to the accompanying drawings.The same reference numbers in different drawings may identify the same or similar elements.
[0014] In a conventional flip chip device, such as a flip chip VCSEL device, the pads of a chip (e.g., a die of a wafer) are connected to a base or a printed circuit board (PCB). For example, the pads may be attached to the base or PCB via a plurality of bumps (e.g., including solder balls or other attachment materials). Typically, the edge of the pad is aligned with the edge of the chip (e.g., the edge of the pad is parallel to the edge of the chip), and / or the bumps associated with the pad are aligned with the edge of the chip (e.g., aligned in one or more rows parallel to the edge of the chip). Therefore, the edge of the pad and / or the bumps associated with the pad are usually aligned with the crystal cleavage plane of the chip (e.g., parallel to the crystal axis of the chip). Therefore, when mechanical strain is introduced on the chip by the pad and / or the bump (which is associated with the pad attaching (e.g., pulling) the chip to the base), the chip will break along one or more cleavage crystal planes. This adversely affects the performance and / or reliability of the chip. For example, one or more VCSELs of a chip located near a crack may not be able to generate light. In addition, cracks may cause the chip to fail to meet durability and / or reliability requirements associated with a particular application.
[0015] For example, Figure 1A-1B The figure shows a side view of a conventional flip-chip VCSEL device chip 100, which includes a gallium arsenide (GaAs) substrate 102 (e.g., an n-GaAS substrate) and an active layer 104 for emitting light 106 perpendicular to a top surface 108 of the chip 100. The substrate 102 may include one or more crystal axes and crystal cleavage planes 110 (shown as being perpendicular to the top surface 108 of the chip 100). Figure 1A-1B The image plane extends along the image plane) may be parallel to one of the crystal axes. Bumps 112 (shown as bumps 112-1 to 112-3) may attach chip 100 to a base ( Figure 1A-1B ), and the crystal cleavage plane 110 may extend between the bumps 112-1 and 112-2. Figure 1A As shown, strain 114 may be formed along crystal cleavage plane 110 due to mechanical stresses generated by bumps 112-1 and 112-2 that respectively pull chip 100 to the base (eg, due to thermal expansion stresses associated with chip 100 and the base). Figure 1AAs further shown in , strain 114 may cause cracks 116 (eg, dislocations, fractures, cracks, etc.) to develop in substrate 102 . Figure 1B A fully formed crack 116 is shown. Thus, the crack 116 may affect the performance and / or reliability of the chip 100.
[0016] Some embodiments described herein provide a chip of an optical device (e.g., for mounting in a flip chip configuration). The chip may include a plurality of bumps arranged in a pattern on the chip that is at a non-zero angle relative to a crystal cleavage plane associated with the chip. This may be referred to as misalignment of the bumps relative to the crystal cleavage plane or non-collinear alignment of the bumps relative to the crystal cleavage plane. In some embodiments, the optical device further includes a gap separating a primary region of the chip and a secondary region of the chip, wherein at least a portion of a side of the gap is oriented at a non-zero angle to the crystal cleavage plane.
[0017] In this way, the non-zero orientation of the bump pattern and / or the gap relative to the crystal cleavage plane reduces the amount of mechanical stress generated along the crystal cleavage plane (e.g., mechanical stress generated by attaching multiple bumps, the first region of the chip, and / or the second region of the chip to a component of another device (such as a base or PCB) rather than using a bump pattern with a zero degree orientation (e.g., oriented parallel to the crystal cleavage plane) and a zero degree oriented gap (e.g., as used in conventional flip chip VCSEL device chip 100). As a result, as described herein, the chip is less likely to crack than conventional chips and therefore has improved performance and / or reliability.
[0018] Figures 2A-2C is a bottom view of an example chip 200 of an optical device (e.g., for mounting in a flip-chip configuration). Figures 2A-2C As shown, the chip 200 may include one or more crystal cleavage planes 202, one or more main regions 204, one or more secondary regions 206, one or more gaps 208, and one or more emitters 210 (e.g., one or more VCSELs). Figure 2B-2C As shown, the chip 200 may include a plurality of bumps 212. These components will be described in detail below.
[0019] In some embodiments, the optical device may be a VCSEL optical device, and the chip 200 may include multiple layers, such as a substrate and an active layer, which emits light perpendicular to a first surface (e.g., a top surface, at the top) of the chip 200 via one or more emitters 210. Figures 2A-2C The chip 200 may include a second surface (eg, Figures 2A-2C), which is configured to mount the chip 200 to a component of another device (e.g., a base, a PCB board, etc.) (e.g., a flip chip configuration). Figures 2A-2C As shown, the chip 200 can be associated with one or more cleavage crystal planes 202. The crystal cleavage planes 202 can be parallel to a crystal axis associated with the chip 200 (e.g., parallel to a crystal axis of the substrate, active layer, and / or one or more other layers of the chip 200). Figures 2A-2C As shown, the crystal cleavage plane 202 may be parallel to a side (eg, an edge) of the chip 200 .
[0020] like Figures 2A-2C As further shown, the second surface of the chip 200 may include one or more main regions 204 (e.g., one or more main pads) and one or more secondary regions 206 (e.g., one or more secondary pads). The one or more main regions 204 may be associated with an anode of the chip 200 (e.g., the main region 204 may be a pad for the anode of the chip 200), and the one or more secondary regions 206 may be associated with a cathode of the chip 200 (e.g., the secondary region 206 may be a pad for the cathode of the chip 200) (or vice versa). Figures 2A-2C As further shown, the second surface may include one or more gaps 208 (e.g., pad gaps, electrode gaps, etc.). The gaps 208 may separate (e.g., electrically insulate) the primary region 204 from the secondary region 206 on the second surface of the chip 200. In some embodiments, the gaps 208 may extend from the first side of the chip 200 to the second side of the chip 200 (e.g., separate the primary region 204 from the secondary region 206). For example, Figures 2A-2C As shown, gap 208 may extend from within a threshold distance of a first side (e.g., top side) of chip 200 to within a threshold distance of a second side (e.g., bottom side) of chip 200. The threshold distance may be a percentage of the distance between the first side and the second side of chip 200, such as 2% of the distance.
[0021] In some embodiments, at least a portion of the side of gap 208 can be oriented at a non-zero angle 214 with respect to crystal cleavage plane 202 of chip 200. Thus, gap 208 can be referred to as having a non-zero orientation with respect to crystal cleavage plane 202. For example, Figure 2A As shown, one or more gaps 208 may extend from the top side of chip 200 to the bottom side of chip 200, respectively, and have sinusoidal sides, wherein at least a portion of the sinusoidal sides are oriented at a non-zero angle 214 relative to a crystal cleavage plane 202 extending from the top side of chip 200 to the bottom side of chip 200. Figure 2AAs shown, a first portion of the sinusoidal side of right gap 208 can be oriented at a non-zero angle 214-1 with respect to crystal cleavage plane 202, and a second portion of the sinusoidal side can be oriented at a non-zero angle 214-2 (e.g., where non-zero angle 214-1 and non-zero angle 214-2 are different from each other). Non-zero angle 214 can be approximately 5 degrees to 15 degrees (e.g., greater than or equal to 5 degrees and less than or equal to 15 degrees). In some embodiments, gap 208 can be configured to intersect crystal cleavage plane 202. For example, as Figure 2A As shown, one or more portions of one side of the right gap 208 may intersect the crystal cleavage plane 202 extending from the top side of the chip 200 to the bottom side of the chip 200 .
[0022] In some embodiments, Figure 2B-2C As shown, the chip 200 may include a plurality of bumps 212 (e.g., a plurality of flip-chip bumps including or associated with pads, solder balls, epoxy resin, etc., for attaching the chip 200 to a component of another device (e.g., a base, a PCB, etc.) on the second surface of the chip 200. Figure 2B-2C As shown, plurality of bumps 212 may be arranged on one or more main regions 204 and / or one or more secondary regions 206 of second surface of chip 200 .
[0023] In some embodiments, the plurality of bumps 212 may be arranged in a pattern (eg, a one-dimensional or two-dimensional array pattern) on the second surface of the chip 200. For example, Figure 2B As shown, the plurality of bumps 212 may be arranged in a non-uniform pattern (e.g., a "random" or pseudo-random pattern), wherein the bumps 212 are located at irregular positions and / or the bumps 212 are not equally spaced from each other. As another example, the plurality of bumps 212 may be arranged in a uniform pattern (formed at a non-zero angle 216 with respect to the crystal cleavage plane 202, as described below), such as Figure 2C Multiple rows of bumps 212 are shown (e.g., a row of bumps 212 includes two or more bumps 212). Within a row of bumps 212, the bumps 212 can be spaced equidistantly (e.g., within a tolerance range) (e.g., each bump 212 in the row of bumps 212 can be spaced the same distance from an adjacent bump 212 in the row of bumps 212).
[0024] In some embodiments, the uniform pattern can be oriented at a non-zero angle 216 with respect to the crystal cleavage plane 202. For example, when the rows of bumps are arranged in multiple rows of bumps 212, such as Figure 2CAs shown, adjacent rows of bumps 212 in the plurality of rows of bumps 212 may be laterally offset from each other (may be referred to as an offset row pattern). Thus, bumps 212 in a first row of bumps 212 from adjacent rows of bumps 212 and corresponding bumps 212 in a second row of bumps 212 from adjacent rows of bumps 212 may be oriented at a non-zero angle 216 with respect to the crystal cleavage plane 202. In some embodiments, the non-zero angle 216 may be approximately 5 degrees to 15 degrees (e.g., greater than or equal to 5 degrees and less than or equal to 15 degrees).
[0025] In this manner, the non-zero orientation of one or more gaps 208 and / or the non-zero orientation of the pattern of bumps 212 results in an amount of mechanical stress along the crystal cleavage plane 202 (e.g., generated by attaching the plurality of bumps 212 to a component of another device (e.g., a base or PCB)) that meets (e.g., is less than) a mechanical stress fracture threshold associated with the chip 200 (e.g., an amount of mechanical stress associated with the generation of cracks in one or more layers of the chip 200 (e.g., a substrate and / or an active layer)). Thus, the amount of mechanical stress along the crystal cleavage plane 202 is less than the mechanical stress generated using gaps 208 having zero orientations and / or a pattern of bumps 212 having zero orientations (as used in conventional flip chip device chips). Thus, the chip 200 is less likely to crack and, therefore, has improved performance and / or reliability compared to conventional flip chip device chips.
[0026] As mentioned above, Figures 2A-2C Provided as an example. Other examples may differ from those for Figures 2A-2C as described.
[0027] Figures 3A-3C is a bottom view of an example chip 300 of an optical device (e.g., for mounting in a flip-chip configuration). Figures 3A-3C As shown. Chip 300 may include one or more crystal cleavage planes 302, one or more main regions 304, one or more secondary regions 306, one or more gaps 308, and one or more emitters 310 (e.g., one or more VCSELs). In some embodiments, as Figure 3B-3C As shown, the chip 300 may include a plurality of bumps 312. These components will be described in detail below.
[0028] In some embodiments, the optical device may be a VCSEL optical device, and the chip 300 may include multiple layers, such as a substrate and an active layer, which emits light perpendicular to a first surface (e.g., Figures 3A-3C The chip 300 may include a second surface (eg, Figures 3A-3C), which is configured to mount the chip 300 to a component of another device (e.g., a base, a PCB, etc.) (e.g., a flip chip configuration). Figures 3A-3C As shown, chip 300 can be associated with one or more cleavage crystal planes 302. Crystal cleavage planes 302 can be parallel to a crystal axis associated with chip 300 (e.g., a crystal axis parallel to the substrate, active layer, and / or one or more other layers of chip 300). In some embodiments, as Figures 3A-3C As shown, crystal cleavage plane 302 may be parallel to a side (eg, an edge) of chip 300 .
[0029] As further shown in FIG. 3 , the second surface of chip 300 may include one or more main regions 304 (e.g., one or more main pads) and one or more secondary regions 306 (e.g., one or more secondary pads). One or more main regions 304 may be associated with an anode of chip 300 (e.g., main regions 304 may be pads for an anode of chip 300), and one or more secondary regions 306 may be associated with a cathode of chip 300 (e.g., secondary regions 306 may be pads for a cathode of chip 300) (or vice versa). Figures 3A-3C As further shown, the second surface may include one or more gaps 308 (e.g., pad gaps, electrode gaps, etc.). The gaps 308 may separate (e.g., electrically insulate) the primary region 304 from the secondary region 306 on the second surface of the chip 300. In some embodiments, the gaps 308 may extend from the first side of the chip 300 to the second side of the chip 300 (e.g., separating the primary region 304 from the secondary region 306). For example, Figures 3A-3C As shown, gap 308 may extend from within a threshold distance of a first side (e.g., top side) of chip 300 to within a threshold distance of a second side (e.g., bottom side) of chip 300. The threshold distance may be a percentage of the distance between the first side and the second side of chip 300, such as 3% of the distance.
[0030] In some embodiments, at least a portion of the side of gap 308 can be oriented at a non-zero angle 314 with respect to the crystal cleavage plane 302 of chip 300. Thus, gap 308 can be considered to have a non-zero orientation with respect to the bulk cleavage plane 302. For example, Figure 3A As shown, one or more gaps 308 may extend from the top side of chip 300 to the bottom side of chip 300, respectively, and may have straight sides having a non-zero angle 314 relative to the crystal cleavage plane 302 extending from the top side of chip 300 to the bottom side of chip 300. Non-zero angle 314 may be approximately 5 degrees to 15 degrees (e.g., greater than or equal to 5 degrees and less than or equal to 15 degrees). In some embodiments, gap 308 may be configured to intersect crystal cleavage plane 302. For example, as Figure 3AAs shown, one or more portions of one side of the right gap 308 may intersect the crystal cleavage plane 302 extending from the top side of the chip 300 to the bottom side of the chip 300 .
[0031] In some embodiments, Figure 3B-3C As shown, the chip 300 may include a plurality of bumps 312 (e.g., a plurality of flip-chip bumps including or associated with pads, solder balls, epoxy resin, etc., for attaching the chip 300 to a component such as a base, a PCB, etc.) on the second surface of the chip 300. Figure 3B-3C As shown, plurality of bumps 312 may be arranged on one or more main regions 304 and / or one or more secondary regions 306 of the second surface of chip 300 .
[0032] In some embodiments, the plurality of bumps 312 may be arranged in a pattern (eg, a one-dimensional or two-dimensional array pattern) on the second surface of the chip 300. For example, Figure 3B As shown, the plurality of bumps 312 may be arranged in a non-uniform pattern, wherein the bumps 312 are located at irregular positions and / or the bumps 312 are not equally spaced from each other. As another example, the plurality of bumps 312 may be arranged in a uniform pattern (formed at a non-zero angle 216 with respect to the crystal cleavage plane 202, as described below), for example Figure 3C Multiple rows of bumps 312 are shown (eg, a row of bumps 312 includes two or more bumps 312). The bumps 312 may be equally spaced within a row of bumps 312 (eg, each bump 312 in a row of bumps 312 may be spaced the same distance from adjacent bumps 312 in the row of bumps 312).
[0033] In some embodiments, the uniform pattern can be oriented at a non-zero angle 316 with respect to the crystal cleavage plane 302. For example, when the bump rows are arranged in multiple rows of bumps 312, such as Figure 3C As shown, adjacent rows of bumps 312 in the plurality of rows of bumps 312 may be laterally offset from each other (e.g., in an offset row pattern). Thus, bumps 312 from a first row of bumps 312 of adjacent rows of bumps 312 and corresponding bumps 312 from a second row of bumps 312 of adjacent rows of bumps 312 may be oriented at a non-zero angle 316 with respect to the crystal cleavage plane 302. In some embodiments, the non-zero angle 316 may be approximately 5 degrees to 15 degrees (e.g., greater than or equal to 5 degrees and less than or equal to 15 degrees).
[0034] In this manner, the non-zero orientation of the pattern of one or more gaps 308 and / or bumps 312 induces an amount of mechanical stress along the crystal cleavage plane 302 (e.g., stress generated by attaching the plurality of bumps 312 to a component of another device such as a base or PCB) to meet (e.g., be less than) a mechanical stress fracture threshold associated with the chip 300 (e.g., an amount of mechanical stress associated with generating cracks in one or more layers of the chip 300 (e.g., a substrate and / or an active layer). Thus, the amount of mechanical stress along the crystal cleavage plane 302 is less than the mechanical stress generated using gaps 308 having zero orientations and / or a pattern of bumps 312 having zero orientations, as used in conventional flip chip device chips. Thus, the chip 300 is less likely to crack and, therefore, has improved performance and / or reliability compared to conventional flip chip device chips.
[0035] As mentioned above, Figure 4A-4B Provided as an example. Other examples may differ from those for Figures 3A-3C as described.
[0036] Figure 4A-4B is a diagram of an example implementation 400 described herein. Figure 4A-4B As shown, embodiment 400 may include processed wafer 402 (e.g., processed semiconductor wafer). For example, processed wafer 402 may be a wafer used to produce a plurality of chips (also referred to as dies), such as a plurality of chips 200 or a plurality of chips 300, for use in an optical device (e.g., a VCSEL optical device). In some embodiments, processed wafer 402 may include a substrate (e.g., a common substrate for a plurality of chips) comprising one or more crystal cleavage planes 404, wherein the crystal cleavage planes 404 may be parallel to a crystal axis associated with the substrate. In some embodiments, one or more masks 406 (e.g., one or more photolithography masks or photomasks used in a photolithography process) may be used to create and / or define (e.g., for manufacturing) a plurality of chips and corresponding components of the plurality of chips. For example, one or more masks 406 may be used to create and / or define a plurality of VCSELs of a chip and / or a plurality of bumps (e.g., one or more flip-chip bumps) of a chip (due to the scale of the diagram being in Figure 4A-4B (not visible in the image).
[0037] like Figure 4AAs shown, one or more masks 406 can be aligned with the crystal cleavage plane 404 (e.g., as shown by edge 408 of one or more masks 406 being parallel to the crystal cleavage plane 404). Thus, one or more masks 406 can create and / or define a plurality of gaps that have no non-zero orientation relative to the crystal cleavage plane 404 and / or a plurality of bumps arranged in a pattern that has no non-zero orientation relative to the crystal cleavage plane 404. For example, one or more masks 406 can create and / or define a pattern of gaps and / or a plurality of non-offset rows of bumps having sides that extend parallel to the crystal cleavage plane 404, wherein groups of a plurality of bumps (e.g., individual rows of bumps) can extend parallel to the crystal cleavage plane 404. In some embodiments, as Figure 4B As shown, one or more masks 406 can be rotated relative to the wafer 402 (e.g., as shown by the non-zero orientation angle 410) (e.g., as shown by the edge 408 of the one or more masks 406 oriented at the orientation angle 410 relative to the crystal cleavage plane 404). Thus, the one or more masks 406 can produce and / or define a non-zero oriented gap and / or a plurality of protrusions arranged in a non-zero oriented pattern. For example, the one or more masks 406 can produce and / or define a gap having a side (which is at a non-zero orientation angle 410 with the crystal cleavage plane 404) and / or a pattern of multiple non-offset rows of protrusions, wherein the words of the multiple protrusions (e.g., individual rows of protrusions) can be at a non-zero orientation angle 410 with the crystal cleavage plane 404 (e.g., due to the rotation of the one or more masks 406 relative to the wafer 402).
[0038] As mentioned above, Figure 4A-4B Provided as an example. Other examples may differ from those for Figure 4A-4B as described.
[0039] The foregoing disclosure provides illustration and description, but is not intended to be exhaustive or to limit the implementation to the precise form disclosed. Modifications and variations may be made based on the foregoing disclosure, or may be obtained from the practice of the implementation. In addition, any implementation described herein may be combined, unless the foregoing disclosure explicitly provides reasons why one or more implementations cannot be combined.
[0040] As used herein, satisfying a threshold may refer to a value greater than a threshold, greater than or equal to a threshold, less than a threshold, less than or equal to a threshold, equal to a threshold, not equal to a threshold, etc., depending on the context.
[0041] Even though specific combinations of features are referenced in the claims and / or disclosed in the specification, these combinations are not intended to limit the disclosure of the various implementations. In fact, many of these features can be combined in ways that are not specifically recited in the claims and / or disclosed in the specification. Although each dependent claim listed below may be directly dependent on only one claim, the disclosure of the various embodiments includes each dependent claim and each other claim in the claim set. As used herein, a phrase referring to "at least one" in a list of items refers to any combination of those items, including single members. For example, "at least one of a, b, or c" is intended to cover any combination of a, b, c, ab, ac, bc, and abc, as well as multiples of the same item.
[0042] Unless explicitly described, the elements, actions or instructions used herein should not be interpreted as key or necessary. In addition, as used herein, the article "one" is intended to include one or more items, and can be used interchangeably with "one or more". In addition, as used herein, the article "the" is intended to include one or more items associated with the article "the", and can be used interchangeably with "the one or more". In addition, as used herein, the term "group" is intended to include one or more items (e.g., a combination of related items, unrelated items, or related and unrelated items), and can be used interchangeably with "one or more". When only one item is intended, the phrase "only one" or similar language is used. In addition, as used herein, the terms "have", "have", "include", etc. are intended to be open terms. In addition, the phrase "based on" is intended to mean "based at least in part", unless otherwise explicitly stated. In addition, as used herein, the term "or" is intended to be included when used in series, and can be used interchangeably with "and / or", unless otherwise explicitly stated (e.g., if used in combination with "either" or "only one of them"). Additionally, for ease of description, spatially relative terms, such as "top," "bottom," "lower," "below," "upper," "above," etc., may be used herein to describe the relationship of one element or feature to another element or feature as depicted in the figures. Spatially relative terms are intended to encompass different orientations of the device, apparatus, and / or element in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein should likewise be interpreted accordingly.
Claims
1. A vertical cavity surface emitting laser (VCSEL) chip for mounting in a flip-chip structure, comprising: Main pad; Secondary welding pad; and The gap separating the primary pad and the secondary pad, where: a first portion of a side of the gap oriented at a first non-zero angle relative to a crystal cleavage plane associated with a substrate of the VCSEL chip; a second portion of the side of the gap is oriented at a second non-zero angle relative to the crystal cleavage plane; The first non-zero angle is different from the second non-zero angle, and Two or more portions of the side surfaces of the gap intersect with the crystal cleavage plane. 2 . The VCSEL chip according to claim 1 , wherein the first non-zero angle is in the range of 5 to 15 degrees. 3 . The VCSEL chip according to claim 1 , further comprising a plurality of flip-chip bumps arranged in a pattern on at least one of the primary pad and the secondary pad. 4 . The VCSEL chip of claim 1 , wherein the primary pad is associated with an anode associated with the VCSEL chip, and the secondary pad is associated with a cathode associated with the VCSEL chip.
5. The VCSEL chip of claim 1 , wherein the orientation of the first portion of the side of the gap results in an amount of mechanical stress along the crystal cleavage plane that is less than a mechanical stress fracture threshold, The amount of mechanical stress is created by attaching the primary and secondary pads to components of another device.
6. The VCSEL chip of claim 1, wherein the gap extends from within a threshold distance of a first side of the VCSEL chip to within a threshold distance of a second side of the VCSEL chip, wherein the threshold distance is 2% or 3% of a distance between the first side and the second side. The VCSEL chip according to claim 3 , wherein the pattern is not aligned with the crystal cleavage plane.
8. The VCSEL chip according to claim 3, wherein the pattern comprises a plurality of rows of flip-chip bumps, Adjacent rows in the plurality of rows are laterally offset from each other.
9. The VCSEL chip according to claim 3, wherein the pattern is a non-uniform pattern. 10 . The VCSEL chip according to claim 1 , wherein the second non-zero angle is in the range of 5 to 15 degrees.
11. The VCSEL chip according to claim 1, wherein: The sides of the gap have a sinusoidal shape.
12. A wafer comprising: A plurality of vertical cavity surface emitting laser (VCSEL) chips, each VCSEL chip comprising a corresponding gap; and The crystal cleavage planes associated with a wafer, where: A first portion of a side of a gap in the plurality of gaps is oriented at a first non-zero angle relative to the crystal cleavage plane; a second portion of the side of the gap is oriented at a second non-zero angle relative to the crystal cleavage plane; The first non-zero angle is different from the second non-zero angle, and Two or more portions of the side surfaces of the gap intersect with the crystal cleavage plane.
13. The wafer of claim 12, wherein each VCSEL chip comprises a plurality of chip bumps, wherein: A plurality of chip bumps are arranged in a pattern on the corresponding VCSEL chip.
14. The wafer according to claim 13, wherein: The pattern of chip bumps is a result of a mask used to fabricate the plurality of chip bumps being rotated relative to the wafer.
15. The wafer according to claim 13, wherein: The pattern includes a non-uniform pattern of chip bumps.
16. The wafer according to claim 13, wherein: The pattern includes multiple rows of chip bumps, Adjacent rows in the plurality of rows are laterally offset from each other.
17. The wafer according to claim 13, wherein: The pattern includes a uniform pattern of chip bumps.
18. The wafer according to claim 12, wherein: The sides of the gap have a sinusoidal shape.
19. The wafer according to claim 12, wherein: At least one of the first non-zero angle or the second non-zero angle is in the range of 5 to 15 degrees.
20. The wafer according to claim 12, wherein: The first portion of the side of the gap is oriented such that an amount of mechanical stress along the crystal cleavage plane is less than a mechanical stress fracture threshold.
Citation Information
Patent Citations
Semiconductor laser device and manufacturing method thereof
CN101136535A
Semiconductor wafer dicing crack prevention using chip peripheral trenches
CN108511514A