A method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials, a device and application thereof
The linear polarization laser pulse splitting technology detects photomagnetization and ultrafast demagnetization of non-magnetic materials, which solves the shortcomings in the research on photomagnetization and ultrafast demagnetization of non-magnetic materials in the prior art, and realizes the Ultrafast magnetization manipulation and detection provide new methods for ultrafast information processing and storage.
Patent Information
- Application Number
- CN202011599752.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-12-29
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-12-29
AI Technical Summary
The existing technology has failed to effectively study and detect photomagnetization and ultrafast demagnetization of non-magnetic materials, especially the lack of detailed research on the detection and regulation of ultrafast demagnetization time of non-magnetic materials, which limits its ultrafast information processing and Applications in the storage field.
Linear polarization laser pulses are divided into pump optical paths and detection optical paths. Through a single wavelength circularly polarized pump optical light and a circularly polarized detection light with a spectrum, the photomagnetization intensity of non-magnetic materials is detected by spin selection rules, and the photomagnetization intensity of non-magnetic materials is detected by The ultrafast demagnetization relaxation time is fitted to realize the detection and regulation of photomagnetization and ultrafast demagnetization of non-magnetic materials.
Magnetization manipulation and detection of non-magnetic materials on picosecond or even femtosecond time scales is achieved, and the use of external magnetic fields is avoided. It has the advantages of stability, efficiency and ease of realization, and is used for ultrafast optical magnetic switches and ultrafast optical control storage. Providing possibilities.
Smart Images

Figure CN114690091B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of nano-optics and magnetism, and in particular to a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials, a device thereof and an application thereof. Background Art
[0002] With the rapid development of science and technology, people have a huge demand for the rapid development of information recording and processing, especially how to manipulate the magnetism of materials at ultrafast time scales. Studies have shown that under the action of femtosecond laser pulses, the magnetism of materials will drop sharply in a very short time, which is called ultrafast demagnetization. However, the current research objects on ultrafast demagnetization are limited to magnetic materials, such as ferromagnetic materials, ferrimagnetic materials and paramagnetic materials, and the size of the materials is mainly at the micron level. Therefore, breaking through the restrictions on the magnetic requirements of materials and nano-scaling devices has important guiding significance and application value.
[0003] In recent years, the inverse Faraday effect has made it possible to magnetize non-magnetic materials, that is, circularly polarized electromagnetic waves can be used to induce magnetic fields, referred to as photoinduced magnetization, and in the field of ultrafast information processing and storage, the response time of ultrafast demagnetization is an important application indicator. However, the existing technology has not conducted detailed research on the photoinduced magnetization and ultrafast demagnetization of non-magnetic materials, especially the detection and regulation of ultrafast demagnetization time.
[0004] Therefore, there is an urgent need to develop a method and device for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials, so as to provide the possibility for using non-magnetic materials for ultrafast photomagnetic switching or ultrafast light-controlled storage. Summary of the invention
[0005] In view of the problems existing in the prior art, the present invention provides a detection method for photoinduced magnetization and ultrafast demagnetization of non-magnetic materials, a device and an application thereof, wherein a linearly polarized laser pulse is divided into a pump light path and a detection light path, and then the linearly polarized laser pulse of the pump light path is processed to obtain a circularly polarized pump light of a single wavelength, so as to realize in-band excitation of the non-magnetic material, and the linearly polarized laser pulse of the detection light path is processed to obtain a delayed circularly polarized detection light with a spectrum, which is used to detect the transient spectrum of excited and unexcited non-magnetic materials, and the spin selection rule is used to reflect the photoinduced magnetization intensity of the non-magnetic material by detecting the transient absorption difference of the circularly polarized detection light with different polarization states, and further adjust the delay time Δt corresponding to the circularly polarized detection light, and use the change of the photoinduced magnetization intensity to fit the ultrafast demagnetization relaxation time of the non-magnetic material, so as to provide the possibility for the non-magnetic material to be used for ultrafast photomagnetic switching or ultrafast optically controlled storage.
[0006] To achieve this object, the present invention adopts the following technical solutions:
[0007] One of the purposes of the present invention is to provide a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials, the detection method comprising the following contents:
[0008] The linearly polarized laser pulse is divided into two paths: a pump light path and a detection light path;
[0009] The linearly polarized laser pulses of the pump optical path are sequentially adjusted through optical parameter amplification and polarization rotation to obtain circularly polarized pump light of a single wavelength, and the circularly polarized pump light is irradiated on the non-magnetic material sample to form a light spot a and realize in-band excitation;
[0010] The linearly polarized laser pulse of the detection light path is sequentially subjected to delay adjustment, white light generation adjustment and polarization rotation adjustment to obtain a circularly polarized detection light with a spectrum, and then the circularly polarized detection light is divided into a circularly polarized detection light I and a circularly polarized detection light II, the circularly polarized detection light I is irradiated on the light spot a to achieve light spot overlap, the circularly polarized detection light II is irradiated on the non-magnetic material sample to form a light spot b, and the light spot a does not overlap with the light spot b;
[0011] The circularly polarized pump light is fixed to be right-handed circularly polarized pump light, and the circularly polarized detection light is adjusted to be left-handed circularly polarized detection light and right-handed circularly polarized detection light, respectively. The change of the light spot a compared with the light spot b is detected at the same time, and the left-handed transient absorption signal ΔA(L) and the right-handed transient absorption signal ΔA(R) are obtained respectively, and then the net spin state accumulation ΔA(L)-ΔA(R) is obtained, which is the photoinduced magnetization intensity ΔA(L)-ΔA(R) of the non-magnetic material, and the delay time Δt corresponding to the circularly polarized detection light is further adjusted, and the ultrafast demagnetization relaxation time of the non-magnetic material is obtained by fitting the change of the photoinduced magnetization intensity ΔA(L)-ΔA(R);
[0012] The circularly polarized pump light is fixed to be left-handed circularly polarized pump light, and its detection method is the same as the detection method corresponding to the case where the circularly polarized pump light is right-handed circularly polarized pump light.
[0013] The detection method of the present invention adjusts the polarization state of a linearly polarized laser pulse to realize the generation of circularly polarized pump light or circularly polarized probe light. Based on the inverse Faraday effect, the circularly polarized pump light can realize the photoinduced magnetization of a non-magnetic material, and the plasmon resonance can enhance the magnetization. By using the spin selection rule, the difference in the number of spin states (net spin state accumulation) is reflected by detecting the transient absorption difference of circularly polarized probe light with different polarization states, which is the photoinduced magnetization intensity of the non-magnetic material. The delay time Δt corresponding to the circularly polarized probe light is further adjusted, and the ultrafast demagnetization relaxation time of the non-magnetic material is obtained by fitting the change of the photoinduced magnetization intensity. Moreover, by changing the polarization state of the circularly polarized pump light, the detection difference signal of different circularly polarized probe lights can be reversed, reflecting the controllability of the direction of the photoinduced magnetization (spin state), and can be used for ultrafast optical magnetic switching or ultrafast optically controlled storage.
[0014] The method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials described in the present invention can not only realize magnetization manipulation and detection on a picosecond or even femtosecond time scale, but also has the advantages of being easy to implement, requiring no external magnetic field, and being more stable and efficient.
[0015] As a preferred technical solution of the present invention, the non-magnetic material includes gold nanorods.
[0016] Gold nanorods have the characteristics of strong surface plasmon resonance effect, structural diversity, biocompatibility and good stability. They are widely used in optics, sensing, catalysis and biological detection, and show great application prospects. Under ultrafast time scale, the plasmon-induced hot electrons corresponding to gold nanorods can excite strong transient optical signals, and their induced intensity and lifetime can be regulated by the size and shape of gold nanorods. In addition, the anisotropic electron cloud of gold nanorods can oscillate along the short axis and long axis respectively, resulting in two different types of resonance signals in different optical bands, which has important research and application value. By replacing the magnetic field, using light to directly magnetize the sample, and studying the internal photoinduced magnetization and ultrafast demagnetization process and physical mechanism, the magnetization (spin state) direction can be regulated, which has extremely important development value and research significance.
[0017] The non-magnetic material in the detection method of the present invention is gold nanorods, which can also realize the combination of photoinduced magnetization and plasmon resonance advantages of gold nanorods under light excitation, and has the advantages of enhancement effect, band controllability and hot electrons accelerating demagnetization relaxation time, which is more conducive to the demonstration of detection methods for photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. The realized magnetization excitation and magnetization (spin state) direction control are of great significance to the design and application of ultrafast photomagnetic switches or ultrafast light-controlled storage devices.
[0018] Preferably, the aspect ratio of the gold nanorods is 2-2.5, such as 2, 2.1, 2.2, 2.3, 2.4 or 2.5, but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0019] Preferably, the long axis of the gold nanorod is 30-50 nm, for example, 30 nm, 35 nm, 40 nm, 45 nm or 50 nm, and the short axis is 15-20 nm, for example, 15 nm, 16 nm, 17 nm, 18 nm, 19 nm or 20 nm, but is not limited to the listed values, and other unlisted values within the above numerical range are also applicable.
[0020] As a preferred technical solution of the present invention, the gold nanorods are prepared by the following method:
[0021] First, sodium borohydride is used to reduce chloroauric acid to prepare a seed solution, and then a mixed solution of chloroauric acid, hexadecyltrimethylammonium bromide, silver nitrate and ascorbic acid is used as a growth solution. Finally, the seed solution is added to the growth solution for growth to obtain the gold nanorod solution.
[0022] As a preferred technical solution of the present invention, the method for preparing the seed solution comprises: mixing a chloroauric acid solution with a hexadecyltrimethylammonium bromide solution, adding a newly prepared sodium borohydride solution, and keeping warm in a water bath at 30°C for 10-15h to obtain the seed solution; wherein the molar ratio of the chloroauric acid, hexadecyltrimethylammonium bromide, sodium borohydride and water is controlled to be 1:(200-400):(2-3):(200-250).
[0023] Preferably, the preparation method of the growth solution comprises: mixing a chloroauric acid solution with a hexadecyltrimethylammonium bromide solution, first adding a silver nitrate solution, and then adding an ascorbic acid solution, until the color of the system becomes colorless, to obtain the growth solution; wherein the molar ratio of the chloroauric acid, hexadecyltrimethylammonium bromide, silver nitrate, ascorbic acid and water is controlled to be 1:(190-210):(0.1-0.13):(0.012-0.013):(950-1050).
[0024] The method for preparing the gold nanorods of the present invention can prepare gold nanorods with different aspect ratios by adjusting the amount of silver nitrate.
[0025] In the method for preparing gold nanorods of the present invention, the mixing method of the components in the growth solution is not particularly limited and can be any method commonly used in the art, that is, the components can be directly mixed with water, or the components can be dissolved in water in advance and then mixed in the form of a solution.
[0026] Preferably, the volume ratio of the seed solution to the growth solution is (1-1.4) μL:1 mL, for example, 1 μL:1 mL, 1.1 μL:1 mL, 1.2 μL:1 mL, 1.3 μL:1 mL or 1.4 μL:1 mL, etc., but is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0027] The preparation method of the gold nanorods of the present invention also includes centrifugally washing the gold nanorod solution with deionized water at least twice, with a centrifugal speed of 10000r / min and a centrifugal time of 20min, and finally re-dispersing the centrifugally washed gold nanorod solution in deionized water to obtain a washed gold nanorod solution.
[0028] As a preferred technical solution of the present invention, the pulse width of the linearly polarized laser pulse is 10-50fs, for example, 10fs, 20fs, 30fs, 40fs or 50fs, and the repetition frequency is 0.5-1.5kHz, for example, 0.5kHz, 0.7kHz, 0.9kHz, 1kHz, 1.2kHz, 1.4kHz or 1.5kHz, but is not limited to the listed values, and other values not listed within the above numerical range are also applicable.
[0029] As a preferred technical solution of the present invention, the delay time Δt is 0.2-15ps, for example 0.2ps (200fs), 1ps, 5ps, 10ps or 15ps, etc., but is not limited to the listed values, and other unlisted values within the above numerical range are also applicable.
[0030] As a preferred technical solution of the present invention, the wavelength of the circularly polarized pump light is 750-800nm, for example, 750nm, 760nm, 770nm, 780nm, 790nm or 800nm, but is not limited to the listed values, and other unlisted values within the above numerical range are also applicable.
[0031] The wavelength of the circularly polarized pump light of the present invention is determined by the intra-band excitation of the non-magnetic material. For example, when gold nanorods are selected as the non-magnetic material, the wavelength of the circularly polarized pump light is 780nm, and the intra-band excitation of the gold nanorods can be achieved.
[0032] Preferably, the spectrum of the circularly polarized detection light is 350-1600 nm.
[0033] The second object of the present invention is to provide a device for the detection method described in the first object, the device comprising: a laser, a beam splitter, an optical parametric amplifier, a pump light polarization rotation element, a non-magnetic material sample element, a plane reflector, an electric delay line, a white light generator, a detection light polarization rotation element, a curved reflector and a transient spectrometer;
[0034] The linearly polarized laser pulse emitted by the laser is divided into a pump light path and a detection light path by a beam splitter; the linearly polarized laser pulse of the pump light path passes through an optical parametric amplifier and a pump light polarization rotation element in sequence to obtain a circularly polarized pump light of a single wavelength, and the circularly polarized pump light is irradiated on a non-magnetic material sample element to form a light spot a and realize in-band excitation; the linearly polarized laser pulse of the detection light path is first delayed and adjusted by a plane reflector and an electric delay line, and then passes through a white light generator and a detection light polarization rotation element in sequence to obtain a circularly polarized detection light with a spectrum, and then the circularly polarized detection light is divided into a circularly polarized detection light I and a circularly polarized detection light II by a beam splitter, the circularly polarized detection light I is irradiated on the light spot a by a curved reflector to realize light spot overlap, and the circularly polarized detection light II is irradiated on the non-magnetic material sample element by a curved reflector to form a light spot b, and the light spot a does not overlap with the light spot b; a transient spectrometer is used to detect the change of the light spot a compared with the light spot b to obtain a transient absorption signal.
[0035] The preparation of the non-magnetic material sample element of the present invention includes first injecting a solution containing a non-magnetic material (such as a gold nanorod solution) into the gap between two quartz plates, controlling the seal by a rubber ring, and then installing the sealed quartz plate into the element slot. Moreover, during the actual detection process, the non-magnetic material sample element is electrically controlled to achieve uniform rotation to ensure that the solution containing the non-magnetic material inside is evenly dispersed, thereby offsetting the effect of gravity on the gold nanorods.
[0036] As a preferred technical solution of the present invention, the laser is a femtosecond laser, and the transient spectrometer is a femtosecond transient spectrometer.
[0037] A third object of the present invention is to provide an application of the detection method described in the first object, wherein the detection method is used for ultrafast optical magnetic switching or ultrafast optically controlled storage.
[0038] Compared with the prior art solutions, the present invention has at least the following beneficial effects:
[0039] (1) The detection method of the present invention generates circularly polarized light by loading a polarization rotation element (λ / 4), and utilizes the inverse Faraday effect to realize the magnetization of non-magnetic materials, thereby replacing the external magnetic field required for traditional magnetization, achieving more stable and more efficient excitation, and not easily damaging the sample;
[0040] (2) Compared with the limitation of conventional femtosecond pump-probe technology that can only detect ultrafast optical signals, the detection method of the present invention applies the photomagnetic effect to it, thereby realizing photoinduced magnetization and detecting photoinduced magnetic effect signals;
[0041] (3) The detection method of the present invention is simple to operate, easy to implement, and the detection process is fast;
[0042] (4) The detection method of the present invention can realize spin manipulation on a picosecond or even femtosecond time scale, with high sensitivity, breaking the time limit of adding magnetic field pulses to manipulate magnetization in conventional methods;
[0043] (5) The present invention uses gold nanorods as non-magnetic materials to achieve the combination of photoinduced magnetization and the plasmon resonance of gold nanorods under light excitation, which has the advantages of enhanced effect, adjustable wavelength and accelerated demagnetization relaxation time by hot electrons;
[0044] (6) The detection method of the present invention reflects the photoinduced magnetization intensity of the non-magnetic material by detecting the transient absorption difference of circularly polarized detection light with different polarization states, further adjusting the delay time Δt corresponding to the circularly polarized detection light, and fitting the change of the photoinduced magnetization intensity to obtain the ultrafast demagnetization relaxation time of the non-magnetic material, thereby providing the possibility for non-magnetic materials to be used for ultrafast optical magnetic switching or ultrafast optically controlled storage. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Figure 1 It is a schematic diagram of a device corresponding to the detection method of photoinduced magnetization and ultrafast demagnetization of non-magnetic materials according to the present invention;
[0046] In the figure: 1-laser; 2-beam splitter (including 2a, 2b); 3-optical parametric amplifier; 4-pump light polarization rotation element; 5-non-magnetic material sample element; 6-plane reflector (including 6a, 6b, 6c, 6d); 7-electric delay line; 8-white light generator; 9-detection light polarization rotation element; 10-curved reflector (including 10a, 10b); 11-transient spectrometer;
[0047] Figure 2 is the left-handed transient absorption signal ΔA(L) obtained in Examples 1-5 of the present invention;
[0048] Figure 3 is the right-handed transient absorption signal ΔA(R) obtained in Examples 6-10 of the present invention;
[0049] Figure 4 It is the photoinduced magnetization intensity ΔA(L)-ΔA(R) corresponding to the gold nanorod when the delay time Δt is 200fs under the in-band excitation of circularly polarized pump light in different polarization states as described in Examples 1, 6, 11 and 16 of the present invention. DETAILED DESCRIPTION
[0050] The technical solution of the present invention is further described below with reference to the accompanying drawings and through specific implementation methods.
[0051] To better illustrate the present invention and facilitate understanding of the technical solution of the present invention, typical but non-limiting embodiments of the present invention are as follows:
[0052] The non-magnetic materials used in the embodiments of the present invention are all gold nanorods, with an aspect ratio of 2.3, a major axis of 40.3 nm, and a minor axis of 17.3 nm, and are prepared by the following method:
[0053] Seed solution: 0.25 mL of 10 mM chloroauric acid solution was added to 7.5 mL of 100 mM hexadecyltrimethylammonium bromide solution, and then 1.65 mL of deionized water and 0.6 mL of 10 mM newly prepared low-temperature sodium borohydride solution were quickly injected into the above solution under vigorous stirring and stirred for 1 min, and kept in a water bath at 30° C. for 12 h to obtain the seed solution; wherein the molar ratio of the chloroauric acid, hexadecyltrimethylammonium bromide, sodium borohydride and water was controlled to be 1:300:2.4:250;
[0054] Growth solution: 0.5 mL of 10 mM chloroauric acid solution was added to 10 mL of 100 mM hexadecyltrimethylammonium bromide solution, 50 μL of 10 mM silver nitrate solution was added first, and 0.6 μL of 100 mM ascorbic acid solution was added while vigorously stirring at 30° C. until the color of the system turned colorless to obtain the growth solution; wherein the molar ratio of the chloroauric acid, hexadecyltrimethylammonium bromide, silver nitrate, ascorbic acid and water was controlled to be 1:200:0.1:0.012:1000;
[0055] Growth: 12 μL of the seed solution was quickly injected into the above growth solution, and the obtained mixed solution was allowed to stand at 30° C. for 12 h to allow it to grow, thereby obtaining the gold nanorod solution.
[0056] according to Figure 1 The device corresponding to the detection method of photoinduced magnetization and ultrafast demagnetization of non-magnetic materials is shown, wherein the laser 1 is a titanium sapphire femtosecond laser (emitting laser 800nm, Coherent Laser Company), and the transient spectrometer 11 is a femtosecond transient spectrometer (Russian CDP2022).
[0057] Fix the circularly polarized pump light to be right-handed circularly polarized pump light
[0058] Example 1
[0059] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials, and the detection method includes the following contents:
[0060] The linearly polarized laser pulse (pulse width of 30 fs, repetition frequency of 1 kHz) emitted by laser 1 is divided into two paths, a pump light path and a detection light path, by beam splitter 2a;
[0061] The linearly polarized laser pulse of the pump light path first passes through the optical parametric amplifier 3 to obtain a single wavelength pump light tuned to 780nm, and then passes through the pump light polarization rotation element 4 to fix the rotation angle of the single wavelength pump light to 45° to obtain a single wavelength right-handed circularly polarized pump light. The right-handed circularly polarized pump light is irradiated on the non-magnetic material sample to form a light spot a and realize in-band excitation. No external magnetic field assistance is required, and the photoinduced magnetization of the non-magnetic material can be realized through the inverse Faraday effect.
[0062] The linearly polarized laser pulse of the detection light path is first delayed and adjusted by the plane reflector 6 (including 6a, 6b, 6c, and 6d) and the electric delay line 7, and the delay time Δt is fixed to 200fs. Then, it passes through the white light generator 8 to obtain a detection light with a spectrum (the wavelength corresponds to 350-1600nm). Then, the rotation angle of the detection light is fixed to 315° by the detection light polarization rotation element 9 to obtain a left-handed circularly polarized detection light with a spectrum. Then, the left-handed circularly polarized detection light is divided into a left-handed circularly polarized detection light I and a left-handed circularly polarized detection light II by a beam splitter 2b. The left-handed circularly polarized detection light I is irradiated on the light spot a by a curved reflector 10a to achieve light spot overlap. The left-handed circularly polarized detection light II is irradiated on the non-magnetic material sample element 5 by a curved reflector 10b to form a light spot b, and the light spots a and b do not overlap.
[0063] A transient spectrometer (11) is used to detect the change of the light spot a (overlapping detection light) compared with the light spot b (reference light) to obtain a left-handed transient absorption signal ΔA (L).
[0064] Example 2
[0065] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except that the delay time Δt is replaced from 200 fs to 1 ps, other conditions are exactly the same as those in Embodiment 1.
[0066] Example 3
[0067] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200 fs to 5 ps, other conditions are exactly the same as those in Embodiment 1.
[0068] Example 4
[0069] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except that the delay time Δt is replaced from 200 fs to 10 ps, other conditions are exactly the same as those in Embodiment 1.
[0070] Example 5
[0071] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except that the delay time Δt is replaced from 200 fs to 15 ps, other conditions are exactly the same as those in Embodiment 1.
[0072] Example 6
[0073] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except that the rotation angle of the detection light is replaced from 315° to 45°, that is, the left-handed circularly polarized detection light is replaced by right-handed circularly polarized detection light, other conditions are exactly the same as those in Embodiment 1.
[0074] Example 7
[0075] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200 fs to 1 ps, other conditions are exactly the same as those of Embodiment 6.
[0076] Example 8
[0077] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except that the delay time Δt is replaced from 200 fs to 5 ps, other conditions are exactly the same as those of Embodiment 6.
[0078] Example 9
[0079] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200 fs to 10 ps, other conditions are exactly the same as those of Embodiment 6.
[0080] Example 10
[0081] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200 fs to 15 ps, other conditions are exactly the same as those of Embodiment 6.
[0082] Fixing the circularly polarized pump light to be left-handed circularly polarized pump light
[0083] Embodiment 11
[0084] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except that the rotation angle of the pump light is replaced from 45° to 315°, that is, the right-handed circularly polarized pump light is replaced by the left-handed circularly polarized pump light, other conditions are exactly the same as those in Embodiment 1.
[0085] Example 12
[0086] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200fs to 1ps, other conditions are exactly the same as those of Embodiment 11.
[0087] Embodiment 13
[0088] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200fs to 5ps, other conditions are exactly the same as those of Embodiment 11.
[0089] Embodiment 14
[0090] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200 fs to 10 ps, other conditions are exactly the same as those of Embodiment 11.
[0091] Embodiment 15
[0092] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200 fs to 15 ps, other conditions are exactly the same as those of Embodiment 11.
[0093] Example 16
[0094] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except that the rotation angle of the detection light is replaced from 315° to 45°, that is, the left-handed circularly polarized detection light is replaced by right-handed circularly polarized detection light, other conditions are exactly the same as those in Embodiment 11.
[0095] Embodiment 17
[0096] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200fs to 1ps, other conditions are exactly the same as those of Embodiment 16.
[0097] Embodiment 18
[0098] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200fs to 5ps, other conditions are exactly the same as those of Embodiment 16.
[0099] Embodiment 19
[0100] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200fs to 10ps, other conditions are exactly the same as those of Embodiment 16.
[0101] Embodiment 20
[0102] This embodiment provides a method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials. Except for replacing the delay time Δt from 200fs to 15ps, other conditions are exactly the same as those of Embodiment 16.
[0103] The left-handed transient absorption signals ΔA(L) obtained in Examples 1-5 are summarized in Figure 2 In the figure, under the in-band excitation of right-handed circularly polarized pump light, the left-handed transient absorption signal ΔA(L) corresponding to the delay time Δt of the gold nanorods is 200fs, 1ps, 5ps, 10ps, and 15ps respectively;
[0104] The right-handed transient absorption signals ΔA(R) obtained in Examples 6-10 are summarized in Figure 3 In the figure, under the in-band excitation of right-handed circularly polarized pump light, the right-handed transient absorption signal ΔA(R) corresponding to the delay time Δt of the gold nanorods is 200fs, 1ps, 5ps, 10ps, and 15ps respectively;
[0105] The net spin state accumulation ΔA(L)-ΔA(R) (i.e., the photoinduced magnetization intensity ΔA(L)-ΔA(R) of the gold nanorods) obtained by subtracting the transient absorption signals of Example 1 from those of Example 6 is plotted on Figure 4 In the figure, we can obtain the photoinduced magnetization intensity ΔA(L)-ΔA(R) of the gold nanorods when the delay time Δt is 200fs under the intra-band excitation of right-handed circularly polarized pump light;
[0106] The net spin state accumulation ΔA(L)-ΔA(R) (i.e., the photoinduced magnetization intensity ΔA(L)-ΔA(R) of the gold nanorods) obtained by subtracting the transient absorption signals of Example 11 from those of Example 16 is plotted on Figure 4 In the figure, we can obtain the photoinduced magnetization intensity ΔA(L)-ΔA(R) of the gold nanorods when the delay time Δt is 200fs under the intra-band excitation of left-handed circularly polarized pump light;
[0107] From the above results, we can see that:
[0108] (1) Under the intra-band excitation of right-handed circularly polarized pump light, the gold nanorod has two plasmon resonance signals in different bands, one at 510nm corresponding to the transverse (long axis) resonance mode and the other at 630nm corresponding to the longitudinal (short axis) resonance mode. The difference in the resonance bands corresponds to the different number of hot electrons generated, which will affect the photoinduced magnetization and ultrafast demagnetization process of the gold nanorod. Under the intra-band excitation of right-handed circularly polarized pump light, and when the delay time Δt is 200fs, the photoinduced magnetization intensity Δ A(L)-ΔA(R) is 0.148, and the photoinduced magnetization intensity ΔA(L)-ΔA(R) at 630nm corresponding to the longitudinal (short axis) resonance mode is 0.005; under the intra-band excitation of right-handed circularly polarized pump light, the ultrafast demagnetization relaxation time of the gold nanorods corresponding to the transverse (long axis) is 4.4ps, and the ultrafast demagnetization relaxation time corresponding to the longitudinal (short axis) is 2.9ps. The corresponding results are shown in Table 1; It should be noted that although the wavelength range of the circularly polarized probe light with a spectrum is 350-1600nm, in order to highlight 510nm and 630nm, Figure 2 and Figure 3 Only the spectra corresponding to the wavelength range of 450-750nm are shown;
[0109] Table 1
[0110] Size of gold nanorods Photoinduced magnetization ΔA(L)-ΔA(R) Ultrafast demagnetization relaxation time Long axis 40.3nm 0.148 4.4ps Short axis 17.3nm 0.005 2.9ps
[0111] (2) The transient absorption signals corresponding to circularly polarized probe lights of different polarization states detected by the transient spectrometer show that the transient absorption signals of gold nanorods excited by right-handed circularly polarized pump light to circularly polarized probe lights of different polarization states are different. According to the spin selection rule, the signals detected by circularly polarized probe lights of different polarization states correspond to the number of internal excited spin states. By changing the circularly polarized probe lights of different polarization states, the difference in transient absorption signals reflected by direct comparison proves the realization of photoinduced magnetization of gold nanorods by circularly polarized pump light, that is, the realization of net spin state accumulation ΔA(L)-ΔA(R);
[0112] (3) Under the intra-band excitation of right-handed circularly polarized pump light, the transient absorption signal of the gold nanorods to different circularly polarized detection light varies. The selective detection of the accumulation of different spin states in the gold nanorods and their relaxation process over time can be monitored. The transient absorption signal rises rapidly within 200 fs, corresponding to the excitation of hot electrons, and then shows a regular signal decay process at 1 ps, 5 ps, 10 ps, and 15 ps. The decay process shows exponential decay, and the ultrafast demagnetization relaxation time of the gold nanorods can be obtained by exponential fitting.
[0113] (4) By Figure 4It can be seen that the net spin state accumulation ΔA(L)-ΔA(R) of the gold nanorods (i.e., the photoinduced magnetization intensity ΔA(L)-ΔA(R) of the gold nanorods) can be reversed by the polarization state of the circularly polarized pump light, corresponding to the realization of photoinduced magnetization direction (spin) regulation, which can be used in device design applications of ultrafast optomagnetic switches or ultrafast light-controlled storage.
[0114] The applicant declares that the present invention illustrates the detailed structural features of the present invention through the above-mentioned embodiments, but the present invention is not limited to the above-mentioned detailed structural features, that is, it does not mean that the present invention must rely on the above-mentioned detailed structural features to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of the components selected by the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.
[0115] The preferred embodiments of the present invention are described in detail above. However, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, a variety of simple modifications can be made to the technical solution of the present invention, and these simple modifications all belong to the protection scope of the present invention.
[0116] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present invention will not further describe various possible combinations.
[0117] In addition, various embodiments of the present invention may be arbitrarily combined, and as long as they do not violate the concept of the present invention, they should also be regarded as the contents disclosed by the present invention.
Claims
1. A method for detecting photoinduced magnetization and ultrafast demagnetization of non-magnetic materials, characterized in that: The detection method comprises the following contents: The linearly polarized laser pulse is divided into two paths: a pump light path and a detection light path; The linearly polarized laser pulses of the pump optical path are sequentially adjusted through optical parameter amplification and polarization rotation to obtain circularly polarized pump light of a single wavelength, and the circularly polarized pump light is irradiated on the non-magnetic material sample to form a light spot a and realize in-band excitation; The linearly polarized laser pulse of the detection light path is sequentially subjected to delay adjustment, white light generation adjustment and polarization rotation adjustment to obtain a circularly polarized detection light with a spectrum, and then the circularly polarized detection light is divided into a circularly polarized detection light I and a circularly polarized detection light II, the circularly polarized detection light I is irradiated on the light spot a to achieve light spot overlap, the circularly polarized detection light II is irradiated on the non-magnetic material sample to form a light spot b, and the light spot a does not overlap with the light spot b; The circularly polarized pump light is fixed to be right-handed circularly polarized pump light, and the circularly polarized detection light is adjusted to be left-handed circularly polarized detection light and right-handed circularly polarized detection light, respectively. The change of the light spot a compared with the light spot b is detected at the same time, and the left-handed transient absorption signal ΔA(L) and the right-handed transient absorption signal ΔA(R) are obtained respectively, and then the net spin state accumulation ΔA(L)-ΔA(R) is obtained, which is the photoinduced magnetization intensity ΔA(L)-ΔA(R) of the non-magnetic material, and the delay time Δt corresponding to the circularly polarized detection light is further adjusted, and the ultrafast demagnetization relaxation time of the non-magnetic material is obtained by fitting the change of the photoinduced magnetization intensity ΔA(L)-ΔA(R); The circularly polarized pump light is fixed to be left-handed circularly polarized pump light, and the detection method thereof is the same as the detection method corresponding to the case where the circularly polarized pump light is right-handed circularly polarized pump light; Wherein, the non-magnetic material comprises gold nanorods; the aspect ratio of the gold nanorods is 2-2.5; the long axis of the gold nanorods is 30-50 nm, and the short axis is 15-20 nm; The gold nanorods are prepared by the following preparation method: first, chloroauric acid is reduced by sodium borohydride to prepare a seed solution, then a mixed solution of chloroauric acid, hexadecyltrimethylammonium bromide, silver nitrate and ascorbic acid is used as a growth solution, and finally the seed solution is added to the growth solution for growth to obtain the gold nanorod solution; wherein, the preparation method of the seed solution comprises: mixing a chloroauric acid solution with a hexadecyltrimethylammonium bromide solution, then adding a newly prepared sodium borohydride solution, and keeping warm in a water bath at 30°C for 10-15h to obtain the seed solution; wherein, the molar ratio of the chloroauric acid, hexadecyltrimethylammonium bromide, sodium borohydride and water is controlled to be 1:
1. :(200-400):(2-3):(200-250); The preparation method of the growth solution comprises: mixing a chloroauric acid solution with a hexadecyltrimethylammonium bromide solution, first adding a silver nitrate solution, and then adding an ascorbic acid solution until the color of the system becomes colorless to obtain the growth solution; wherein the molar ratio of the chloroauric acid, hexadecyltrimethylammonium bromide, silver nitrate, ascorbic acid and water is controlled to be 1:(190-210):(0.1-0.13):(0.012-0.013):(950-1050); the volume ratio of the seed solution to the growth solution is (1-1.4) μL:1 mL.
2. The detection method according to claim 1, characterized in that: The pulse width of the linearly polarized laser pulse is 10-50 fs, and the repetition frequency is 0.5-1.5 kHz.
3. The detection method according to claim 1, characterized in that: The delay time Δt is 0.2-15 ps.
4. The detection method according to claim 1, characterized in that: The wavelength of the circularly polarized pump light is 750-800nm; the spectrum of the circularly polarized detection light is 350-1600nm.
5. A device for the detection method according to any one of claims 1 to 4, characterized in that: The device comprises: a laser (1), a beam splitter (2), an optical parametric amplifier (3), a pump light polarization rotation element (4), a non-magnetic material sample element (5), a plane reflector (6), an electric delay line (7), a white light generator (8), a detection light polarization rotation element (9), a curved reflector (10) and a transient spectrometer (11); The linearly polarized laser pulse emitted by the laser (1) is divided into two paths, a pump light path and a detection light path, by a beam splitter (2a); the linearly polarized laser pulse of the pump light path passes through an optical parameter amplifier (3) and a pump light polarization rotation element (4) in sequence to obtain a circularly polarized pump light of a single wavelength, and the circularly polarized pump light is irradiated on a non-magnetic material sample element (5) to form a light spot a and realize in-band excitation; the linearly polarized laser pulse of the detection light path is firstly delayed and adjusted by a plane reflector (6) and an electric delay line (7), and then passes through a white light generator (8) and a detection light polarization rotation element in sequence. The device (9) obtains circularly polarized detection light with a spectrum, then uses a beam splitter (2b) to split the circularly polarized detection light into circularly polarized detection light I and circularly polarized detection light II, uses a curved reflector (10a) to irradiate the circularly polarized detection light I onto the light spot a to achieve light spot overlap, and uses a curved reflector (10b) to irradiate the circularly polarized detection light II onto a non-magnetic material sample element (5) to form a light spot b, wherein the light spot a and the light spot b do not overlap; and uses a transient spectrometer (11) to detect the change of the light spot a compared to the light spot b to obtain a transient absorption signal.
6. The device according to claim 5, characterized in that The laser (1) is a femtosecond laser, and the transient spectrometer (11) is a femtosecond transient spectrometer.
7. An application of the detection method according to any one of claims 1 to 4, characterized in that: The detection method is used for ultrafast optical magnetic switching or ultrafast optical controlled storage.
Citation Information
Patent Citations
System for measuring linear and non-linear magneto-optical Kerr rotation
CN101776575A
Frequency-adjustable ultrafast time resolution transient reflection spectrometer
CN111307756A
Apparatus and method of modulating polarization of light using magnetophoton meta-surfaces
RU2703487C1