A method for determining the tensile strength of mixed fibers in concrete

The minimum fiber mixing length in concrete was determined by calculation and experimentation, which solved the problem of the difficulty in determining the fiber length and quantity, improved the tensile strength of concrete and avoided waste.

CN114720276BActive Publication Date: 2024-11-26ZHONGYU HUAZHU ENGINEERING (HENAN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210314204.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-28
Publication Date
2024-11-26
Estimated Expiration
2042-03-28

AI Technical Summary

Technical Problem

In existing technologies, it is difficult to determine the length and quantity of fibers mixed in concrete, which leads to insufficient or excessive interaction between the fibers and concrete, resulting in waste and failure to meet the design tensile strength.

Method used

The number of fibers and tensile strength per unit cross section were calculated using formulas. Multiple specimens were prepared for tension tests to measure the tensile strength of the fibers and determine the minimum blending length of the fibers. A gelling agent was used as a base material to simplify the test process.

Benefits of technology

It enables precise determination of the amount of fiber to be mixed, ensuring that the tensile strength of the concrete meets the design requirements, while avoiding waste caused by excessive fiber length.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114720276B_ABST
    Figure CN114720276B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for determining the tensile strength of mixed fibers in concrete. On a unit cross section, the minimum tensile strength provided by the fibers for concrete is Ftotal, and Ftotal has the following two forms: 1): #imgabs0#2): #imgabs1#In the above formula, n represents the number of fibers on a unit cross section, n is a positive integer not less than, and F represents the tensile strength of a single fiber. In formula 1, n is an odd number, and in formula 2, n is an even number. In the present invention, the minimum tensile strength that can be provided by n fibers on a unit cross section can be calculated by the above formula, so as to solve the technical problem that the tensile strength of mixed fibers in concrete cannot be determined in the prior art.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of concrete production, and in particular to a method for determining the tensile strength of fibers mixed in concrete. Background Art

[0002] Concrete is a commonly used building material. Common concretes include asphalt concrete and cement concrete. Asphalt concrete is a mixture of crushed stone, asphalt and other materials, while cement concrete is a mixture of crushed stone, cement and other materials. The asphalt in asphalt concrete and the cement in cement concrete can become gelling agents.

[0003] In the prior art, in order to improve the tensile strength of concrete, a general practice is to mix fibers into the corresponding concrete. The fibers may be basalt fibers, and the tensile strength of the concrete is improved through the interaction between the fibers and the concrete.

[0004] The problem with the prior art is that it is difficult to determine the length of the fibers to be mixed into concrete, and they are generally added based on experience. In fact, if the fiber length is too short, the interaction force between the fiber and the concrete, i.e., the bond strength, is insufficient, and the fiber addition will not play a role. If the fiber length is too long, not only will it cause a waste of materials, but the fibers that are too long will also be difficult to disperse and evenly distribute in the concrete. Of course, there is no clear operation in the prior art on how much fiber to add to a certain amount of concrete, and whether it can meet the designed tensile strength of the concrete is an unknown. Summary of the invention

[0005] The purpose of the present invention is to provide a method for determining the tensile strength of fibers mixed in concrete, so as to solve the technical problem in the prior art that the tensile strength of fibers mixed in concrete cannot be determined.

[0006] In order to solve the above technical problems, the technical solution of a method for determining the tensile strength of mixed fibers in concrete in the present invention is as follows:

[0007] A method for determining the tensile strength of mixed fibers in concrete.

[0008] The tensile strength provided by the fiber to the concrete per unit cross section is Ftotal.

[0009] Then F has the following two forms: 1)

[0010] 2):

[0011] In the above formula, n represents the number of fibers per unit cross section, n is a positive integer not less than, F represents the tensile strength of a single fiber, n is an odd number in Formula 1, and n is an even number in Formula 2.

[0012] The beneficial effect of the present invention is that the minimum tensile force that can be provided by n fibers on a unit cross section can be calculated by the above formula, thereby providing a basis for the mixing quantity of the fibers.

[0013] Furthermore, the F is obtained in the following manner: in the first step, m specimens are made, where m is a positive integer not less than 3, and each specimen is referred to as the first specimen, the second specimen, ... the mth specimen, respectively; each specimen includes a base material and fibers, and the fibers include a base material connecting end fixed in the base material and a tensioning end exposed outside the base material; from the first specimen to the mth specimen, in each specimen, the length of the base material connecting end gradually increases; in the second step, from the first specimen to the mth specimen, the tensioning end of the fiber is tensioned by a tensioning mechanism, and the tensioning force exerted on the fiber is measured; the extension direction of the tensioning end is consistent with the extension direction of the base material connecting end; from the first specimen to the pth specimen, the fibers are pulled out of the corresponding base materials; in the p+1th specimen, the fibers are broken; the tension exerted on the fibers in the p+1th specimen is F, p+1≤m; in the n+1th specimen, the length of the base material connecting end of the fiber is a, and the basic length L of the blended fiber is L=2a.

[0014] Furthermore, there are three 1st test piece, three 2nd test piece, ..., and three test pieces with the same length of the base material connection end.

[0015] Furthermore, the base material is composed of a gelling agent.

[0016] Furthermore, the gelling agent is asphalt or cement.

[0017] Furthermore, a test specimen is made by a test device and the fibers of the test specimen are tensioned. The test device includes a device bracket and a mold box. The mold box includes a box bottom plate and a box side plate. The box bottom plate is provided with fiber perforations. A lower fiber positioning structure is provided on the device bracket at the lower side of the fiber perforations. A tensioning mechanism for connecting to the tensioning end of the fiber is provided on the device bracket at the upper side of the mold box. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] By reading the following detailed description with reference to the accompanying drawings, the above and other objects, features and advantages of the exemplary embodiments of the present disclosure will become readily understood. In the accompanying drawings, several embodiments of the present disclosure are shown in an exemplary and non-limiting manner, and the same or corresponding reference numerals represent the same or corresponding parts, wherein:

[0019] Figure 1 It is a schematic diagram of the state of the test piece during preparation in the present invention;

[0020] Figure 2 yes Figure 1 Schematic diagram of the coordination of the middle tensioning cylinder, the lower fiber positioning structure and the mold box;

[0021] Figure 3 It is a schematic diagram of the state when the fiber is stretched in the present invention;

[0022] Figure 4 yes Figure 3 A in the enlarged view;

[0023] Figure 5 It is the ideal configuration diagram of fiber distribution in concrete;

[0024] Figure 6 yes Figure 5 Schematic diagram of the state where the fiber is divided into n equal parts;

[0025] Explanation of the reference numerals in the accompanying drawings: 1. tensioning cylinder; 2. lifting beam; 3. mold box; 4. device column; 5. mold box support; 6. device base; 7. base material; 8. fiber; 9. lower fiber positioning structure; 10. top pressure bolt; 11. sealing gasket; 12. fiber perforation; 13. telescopic cylinder; 14. connecting ring; 15. box side plate; 16. box bottom plate; 17. first connecting bolt; 18. second connecting bolt; 19. base material connecting end; 20. tensioning end; 21. concrete; 22. assumed broken section; 23. point 1; 24. point 2; 25. point n. DETAILED DESCRIPTION

[0026] In order to facilitate the understanding of the present invention, the present invention is described in more detail below in conjunction with the accompanying drawings and specific embodiments. Preferred embodiments of the present invention are provided in the accompanying drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described in this specification. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present invention more thorough and comprehensive.

[0027] It should be noted that, unless otherwise defined, all technical and scientific terms used in this specification have the same meanings as those commonly understood by those skilled in the art to which the present invention belongs. The terms used in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. An embodiment of a method for determining the tensile strength of mixed fibers in concrete in the present invention: Figures 1 to 5 As shown:

[0028] The tensile strength provided by the fiber to the concrete per unit cross section is F. 合 ,

[0029] Then F 合 There are two forms: 1)

[0030] 2): In the above formula, n represents the number of fibers per unit cross section, n is a positive integer not less than, F represents the tensile strength of a single fiber, n is an odd number in Formula 1, and n is an even number in Formula 2.

[0031] The F in the above formula can be obtained by the following method:

[0032] The first step is to make m specimens, where m is a positive integer not less than 3. Each specimen is referred to as the first specimen, the second specimen, ... the mth specimen. Each specimen includes a base material and fibers. The fibers include a base material connecting end fixed in the base material and a tensioning end 19 exposed outside the base material. From the first specimen to the mth specimen, the length of the base material connecting end in each specimen gradually increases. The second step is to tension the tensioning end of the fiber from the first specimen to the mth specimen through a tensioning mechanism, and measure the tensioning force on the fiber. The extension direction of the tensioning end is consistent with the extension direction of the base material connecting end. From the first specimen to the pth specimen, the fibers are pulled out of the corresponding base materials. In the p+1th specimen, the fibers are broken, and the force for breaking the fibers of the p+1th specimen is F, p+1≤m. In the n+1th specimen, the length of the base material connecting end of the fiber is a, and the basic length of the blended fiber is L=2a.

[0033] In the above method, the extension direction of the tensioning end 20 is consistent with the extension direction of the base material connecting end 19. This is because, if the extension directions of the tensioning end and the base material connecting end are inconsistent, there will not be absolute friction between the fiber and the base material, but there will be a stopping force along the tensioning direction, or there will be component forces in other directions. In the present invention, the purpose is to determine a minimum mixing length of the fiber under the tensile effect of the fiber, so other influences that may increase the force between the fiber and the base material should be eliminated as much as possible.

[0034] In the present invention, there are three first test pieces, three second test pieces, ..., three mth test pieces, and three test pieces with the same length of the base material connection end, that is, three first test pieces form a group, three second test pieces form a group, ..., three mth test pieces form a group. In the present invention, m is preferably 10, the length of the base material connection end of the first test piece is 2 cm, and the length difference between the base material connection ends of two adjacent test pieces is 0.5 cm.

[0035] In the present invention, the base material is solely composed of concrete gelling agent or asphalt gelling agent. This is because, after the fibers are mixed in concrete, the fibers may be connected with sand, gravel and gelling agent together, or the fibers may be connected with the gelling agent alone. In fact, most of the fibers are connected with the gelling agent alone, and the tensile strength of the fibers connected with sand, gravel and gelling agent together is greater than the tensile strength of the fibers connected with the gelling agent alone. Therefore, by selecting a base material consisting only of gelling agent, the shortest length of the mixed fibers that meets the requirements can be achieved, and only using gelling agent can reduce the cost and difficulty of the experiment.

[0036] In this embodiment, a test piece is made by a test device and the fiber of the test piece is tensioned. The test device includes a device bracket and a mold box 3. The mold box 3 includes a box bottom plate 16 and a box side plate 15. The box bottom plate 16 is provided with a fiber perforation 12. A lower fiber positioning structure 9 is provided on the device bracket at the lower side of the fiber perforation. A tensioning mechanism for connecting to the tensioning end of the fiber is provided on the device bracket at the upper side of the mold box.

[0037] The tensioning mechanism is located just above the lower fiber positioning structure.

[0038] The device support includes a device base 6 and a device column 4. The device column 4 is equipped with a lifting beam 2 that can be lifted and lowered and is guided and moved in the up and down directions. The tensioning mechanism includes a tensioning cylinder 1 fixed on the lifting beam.

[0039] The box bottom plate 16 is provided with a first bolt through hole for the box bottom plate, and the bottom of the box side plate is provided with a lower side threaded hole for the box side plate corresponding to the first bolt through hole for the box bottom plate, and the first connecting bolt 17 for realizing a detachable connection between the box bottom plate and the box side plate is installed in the first bolt through hole for the box bottom plate and the lower side threaded hole for the box side plate, and a second bolt through hole for the box bottom plate is provided on the box bottom plate at the periphery of the first bolt through hole for the box bottom plate, and a mold box support 5 located on the lower side of the box bottom plate is provided on the device base, and a second connecting bolt 18 for realizing a detachable connection between the mold box and the mold box support is installed between the second bolt through hole for the box bottom plate and the mold box support.

[0040] The upper end of the box side plate is threadedly connected with a pressing bolt 10 for pressing the upper end of the base material in the mold box.

[0041] The lower fiber positioning structure in this embodiment includes a vertically arranged telescopic cylinder 13, which is coaxially arranged with the tensioning cylinder, and a connecting ring 14 is provided at the upper end of the telescopic cylinder and the lower end of the tensioning cylinder. A sealing pad 11 is provided at the upper end of the fiber perforation for the fiber to pass through in the up and down direction. The sealing pad 11 cooperates with the hole wall of the fiber perforation and the fiber seal, so that when the gelling agent is poured into the mold box, the gelling agent will not enter the fiber perforation, which is convenient for the subsequent demolding of the gelling agent. More importantly, the thickness of the gelling agent is consistent with the length of the base material connection end of the fiber, and no excess base material will enter the fiber perforation to affect the test results.

[0042] The process of making the test piece is as follows Figure 2As shown, the upper end of the fiber 8 is first connected to the tensioning cylinder, and the lower end of the fiber 8 is connected to the telescopic cylinder. The tensioning cylinder and the telescopic cylinder do not need to apply tension to the fiber, but only need to ensure that the fiber is vertical. Then, the gelling agent is injected into the mold box through the upper opening of the mold box. After reaching the specified height, the injection is stopped, and then the port fiber is connected to the tensioning cylinder and the telescopic cylinder. The mold box is removed to realize the placement and fixation of the gelling agent, and the next mold box is taken over to make the next test piece. The base material connection end refers to a section where the fiber is connected to the base material. In this embodiment, the length direction of the base material connection end is consistent with the thickness of the base material, so the thickness of the base material is the length of the base material connection end.

[0043] When the fiber is subjected to a tension test, after the gelling agent is solidified, the corresponding mold box containing the base material is fixed on the mold box support, and the top pressure bolt is screwed downward, so that the bottom of the top pressure bolt presses against the upper end of the base material to prevent the base material from falling out of the mold box when the tensioning cylinder pulls the fiber. Since there is also a certain force between the base material and the mold box, the top pressure required for the top pressure bolt is not particularly large. The telescopic cylinder does not need to be connected to the lower end of the fiber, and the tensioning end of the upper end of the fiber is tensioned by the tensioning cylinder. In the present invention, since the fiber penetrates the base material in the up and down directions, the thickness of the base material is the length of the base material connection end, and the length of the base material connection end is easy to control.

[0044] The tensioning force of the tensioning cylinder on the fiber can be measured by a tension sensor. For the pulled-off specimen, the average holding force f per millimeter can be calculated. The holding force in this embodiment refers to the force between the fiber and. When the specimen is broken for the first time, the force reading of the tension sensor is F, then the breaking tension of the blended fiber = F. At this time, the length of the connecting end of the base material, that is, the thickness of the base material, is a, then the basic length of the blended fiber in the concrete is L = 2a. This method can be used to test out a preferred blending strength. Fibers with a length of 2a are mixed into concrete, which can ensure the tensile strength of the concrete without causing waste due to excessive fiber length. After the test, remove the side panels of the box and easily take out the base material for use in the next test.

[0045] In the present invention, F 合 The calculation process is:

[0046] F 合 It represents the sum of the minimum tensile strength provided by all fibers on a unit cross section to concrete. In this embodiment, it is assumed that after the fibers and concrete are evenly mixed, there are n fibers at a certain assumed cross section, and the cross-sectional area of ​​the assumed cross section is 1 cm 2 For example, n is a positive integer not less than 10, assuming that the cross section is perpendicular to the left and right directions, F 合 The calculation of is based on the following two ideal models. The first ideal model is as follows: Figure 5As shown, the lengths of n fibers 8 are all perpendicular to the assumed cross section 22. The reason why this is an ideal treatment is that the present invention calculates the sum of the minimum tensile resistance, and when each fiber is perpendicular to the assumed cross section 22, the tensile resistance that the fiber can provide is the minimum. If the fiber intersects the assumed cross section at an angle, when the concrete is pulled in the left and right directions, there is not only adhesive friction between the fiber and the concrete, but also a stopping force, that is, when the fiber intersects the assumed cross section at an angle, the force between the fiber and the concrete 21 is greater than the force between the fiber and the concrete when the fiber is perpendicular to the assumed cross section. The present invention is to obtain the sum of the minimum tensile resistance, so an ideal model can be constructed in which each fiber is perpendicular to the assumed cross section. In this assumed ideal model, the length of the concrete is at least 1.5L.

[0047] The second ideal model is: Figure 6 As shown, it is assumed that each fiber 8 is divided into n equal parts, that is, the fiber has n-1 equal division points, plus the two endpoints of the fiber, the left end point of the fiber is the 1st point 23, and the right end point of the fiber is the nth point 25. From left to right, each fiber has the 1st point, the 2nd point 24...nth point respectively. The fiber between two adjacent points is called the minimum length unit of tension contribution. Assuming the length of the fiber is L, the two ends of the midpoint of the fiber are gripped by concrete with the same grip force, and the average grip force per unit length, that is, per millimeter, is the same.

[0048] Assume that the first point of the first fiber intersects with the assumed broken section, the second point of the second fiber intersects with the assumed broken section, the third point of the third fiber intersects with the assumed broken section... the nth point of the nth fiber intersects with the assumed broken section. The reason why the ideal model can be constructed in this way is that under this ideal model, the tensile resistance provided by each fiber to the concrete is the smallest.

[0049] Then, the tensile force contribution of the first fiber is zero, the tensile force contribution of the second fiber is F / ((n-1) / 2)=2F / (n-1); the tensile force contribution of the third fiber is 2*2F / (n-1); ... the middle one or the two middle fibers are the largest; ... the tensile force contribution of the n-2th fiber is 2*2F / (n-1); the tensile force contribution of the n-1th fiber is F / ((n-1) / 2)=2F / (n-1); the tensile force contribution of the nth fiber is zero.

[0050] When n is an odd number,

[0051] The minimum number of length units for the tensile contribution of n fibers

[0052]

[0053] The tensile strength of a single fiber is F, so the tensile contribution of the minimum length unit is

[0054] When n is an even number:

[0055] The minimum number of length units for the tensile contribution of n fibers

[0056]

[0057] The tensile strength of a single fiber is F, so the tensile contribution of the minimum length unit is

[0058] The sum of the tensile forces of each fiber per unit area is F 合 Adding the tensile force of the concrete's own gelling agent per unit area gives the tensile strength of the concrete mixed with fibers.

[0059] The tensile force of the concrete's own gelling agent per unit area, i.e., the tensile strength, can be obtained through testing, that is, by tensioning concrete without fiber admixture.

[0060] In the present invention, n can be obtained in the following two ways: 1. Experimental method, cutting a cross section of 1 cm 2 A concrete specimen strip is cut at a certain position, and the number of fibers cut off at the cut surface is found by visual inspection, which is the n value; 2. The calculation method is that when the fiber placement amount is known, the fiber placement amount in a concrete with a length of 1.5L under a certain cross-sectional area can be calculated. The number of fibers under this placement amount is the number of fibers at the assumed broken section, which is the n value.

[0061] In the above description of this specification, unless otherwise clearly specified and limited, the terms "fixed", "installed", "connected" or "connected" should be understood in a broad sense. For example, with regard to the term "connection", it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, or it can be the internal connection of two elements or the interaction relationship between two elements. Therefore, unless otherwise clearly defined in this specification, those skilled in the art can understand the specific meanings of the above terms in the present invention according to the specific circumstances.

[0062] According to the above description of this specification, those skilled in the art may also understand that the terms used below, such as "up", "down", "front", "back", "left", "right", "length", "width", "thickness", "vertical", "horizontal", "top", "bottom", "inside", "outside", "axial", "radial", "circumferential", "center", "longitudinal", "lateral", "clockwise" or "counterclockwise", etc., which indicate the orientation or position relationship, are based on the orientation or position relationship shown in the drawings of this specification, and are only for the purpose of facilitating the explanation of the scheme of the present invention and simplifying the description, rather than explicitly or implicitly indicating that the device or element involved must have the specific orientation, be constructed and operate in a specific orientation. Therefore, the above-mentioned orientation or position relationship terms cannot be understood or interpreted as limitations on the scheme of the present invention.

[0063] In addition, the terms "first" or "second" used in this specification to refer to numbers or ordinals are only used for descriptive purposes and cannot be understood as explicitly or implicitly indicating relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include at least one such feature. In the description of this specification, the meaning of "plurality" is at least two, such as two, three or more, etc., unless otherwise clearly and specifically defined.

[0064] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for determining the tensile strength of mixed fibers in concrete, characterized in that: The minimum tensile strength that the fiber provides to concrete per unit cross section is F. 合 , then F 合 There are two forms: 1) 2): In the above formula, n represents the number of fibers per unit cross section, n is a positive integer not less than 10, F represents the tensile strength of a single fiber, in formula 1), n ​​is an odd number, in formula 2), n is an even number, and F is obtained by the following method: in the first step, m test pieces are made, m is a positive integer not less than 3, and each test piece is respectively referred to as the first test piece, the second test piece, ... the mth test piece, each test piece includes a base material and fibers, the fibers include a base material connection end fixed in the base material and a tension end exposed outside the base material, and from the first test piece to the mth test piece, in each test piece, the base material connection end is fixed in the base material and the tension end is exposed outside the base material. The length of the connecting end gradually increases. In the second step, from the 1st specimen to the mth specimen, the tensioning end of the fiber is tensioned by the tensioning mechanism, and the tensioning force on the fiber is measured. The extension direction of the tensioning end is consistent with the extension direction of the base material connecting end. From the 1st specimen to the pth specimen, the fibers are pulled out of the corresponding base materials. In the p+1th specimen, the fibers are broken. The tension on the fibers in the p+1th specimen is F, p+1≤m. In the p+1th specimen, the length of the base material connecting end of the fiber is a, and the basic length of the blended fiber is L=2a.

2. The method for determining the tensile force according to claim 1, characterized in that: There are three 1st test piece, three 2nd test piece, ..., three mth test piece, and three test pieces with the same length of base material connection ends.

3. The method for determining the tensile force according to claim 1, characterized in that: The base is composed of a gelling agent.

4. The method for determining the tensile force according to claim 3, characterized in that: The gelling agent is asphalt or cement.

5. The method for determining the tensile force according to any one of claims 1 to 4, characterized in that: A test piece is made by a test device and the fiber of the test piece is tensioned. The test device includes a device bracket and a mold box. The mold box includes a box bottom plate and a box side plate. The box bottom plate is provided with fiber perforations. A lower fiber positioning structure is provided on the device bracket at the lower side of the fiber perforations. A tensioning mechanism for connecting to the tensioning end of the fiber is provided on the device bracket at the upper side of the mold box.