Early life prediction method and system for long-life lithium-ion batteries based on degradation sequence temporal correlation modeling
Through a method based on time series correlation modeling of degradation sequences, multiple sequence-to-sequence models are established and multiple time domain dependencies are integrated to solve the problems of poor accuracy and stability in traditional lithium-ion battery prediction methods and achieve capacity degradation and High accuracy and stability of life prediction.
Patent Information
- Application Number
- CN202210420404.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-04-21
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-04-21
Smart Images

Figure CN114781262B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of lithium-ion battery health management and remaining life prediction, and in particular to a method and system for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling. Background Art
[0002] Lithium-ion batteries have become one of the most commonly used energy storage devices in the industrial field, and are widely used in electric vehicles, energy storage power stations, and a series of consumer electronic products. As lithium-ion batteries continue to charge and discharge, their capacity will continue to degrade until they cannot complete the given task, and even cause certain safety hazards. Especially for space application backgrounds, the life of space lithium-ion batteries is constantly improving, and their life prediction is often used in space online scenarios, so it is difficult to obtain their full life cycle degradation data through ground experiments. Therefore, accurately predicting the capacity degradation process and remaining life of lithium-ion batteries in the early stage of battery degradation is crucial for the safe and stable operation of electrical equipment. Traditional lithium-ion battery performance degradation prediction mostly adopts a single-point iteration method, that is, the prediction model only outputs a single prediction result at a time, and predicts data for multiple time steps in the future through an iterative update strategy. For the more common lithium-ion batteries currently, their cycle life is long, but the performance degradation process is different. The single-step iteration prediction mode often leads to cyclic iteration, resulting in excessive coupling of prediction errors into the prediction model, which ultimately causes the prediction model to lose its prediction ability and cannot make accurate and stable predictions. Summary of the invention
[0003] The present invention aims to solve one of the technical problems in the related art at least to a certain extent.
[0004] To this end, an object of the present invention is to propose a method for predicting the early life of long-life lithium-ion batteries based on degradation sequence temporal correlation modeling, which solves the problems of poor long-term prediction accuracy and stability caused by the existing single-step iterative prediction mode.
[0005] Another object of the present invention is to provide a long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling.
[0006] To achieve the above-mentioned purpose, an embodiment of the present invention proposes a method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling, comprising the following steps: Step S1, obtaining battery capacity data of a preset number of lithium-ion battery cells in each cycle Wherein, t is the cycle number, i is the cell number (i=1, 2, ..., n), and a total of n battery cell capacity degradation data are obtained, which includes the cell to be predicted; step S2, reconstructing the capacity degradation data of n-1 other battery cells working under the same working conditions as the cell to be predicted into a training data set Step S3, establishing j capacity prediction models based on sequence-to-sequence models with different input and output structures, and using the training data set Train j capacity prediction models based on sequence-to-sequence models respectively; Step S4, the first k capacity prediction models of the battery cells to be tested are j The discharge capacity of the j-cycle is used as the initial input of the j-th trained capacity prediction model based on the sequence to sequence model (Sequence to Sequence model, Seq2Seq) to obtain the first step prediction output result; Step S5, input the first step prediction output result as a new input sequence into the j-th trained capacity prediction model based on the sequence to sequence model to obtain the next step prediction output result, iteratively execute until it is lower than the failure threshold, and connect the output results of each step end to end to obtain the degradation process curve and the life cut-off point; Step S6, respectively execute steps S4-S5 on the j trained capacity prediction models based on the sequence to sequence model to obtain j capacity degradation curves and j life cut-off points; Step S7, average the capacity of the j capacity degradation curves over the cycle t to obtain the final prediction result
[0007] The embodiment of the present invention provides a long-life lithium-ion battery early life prediction method based on degradation sequence time series association modeling, by establishing a lithium-ion battery capacity degradation prediction model, and realizing the prediction of the life end period through the capacity degradation curve; the capacity degradation prediction model is based on a sequence-to-sequence model, and the number of iteration steps in the long-term prediction process is greatly reduced by outputting the sequence prediction results; in addition, by constructing a sequence-to-sequence model with different structures and fusing the prediction results of each model, a fused prediction result integrating multiple time domain dependencies can be obtained, and finally the long-term stable prediction of the lithium-ion battery capacity degradation process and the life end period is realized, which solves the problem of low long-term accuracy and stability of the single-step iterative prediction method based on historical data in the field of long-life satellite lithium-ion capacity degradation estimation and remaining life prediction, and can achieve fragmented prediction results compared with traditional degradation trajectory prediction and life prediction methods.
[0008] In addition, the long-life lithium-ion battery early life prediction method based on degradation sequence temporal association modeling according to the above embodiment of the present invention may also have the following additional technical features:
[0009] Further, in one embodiment of the present invention, the step S2 is specifically as follows: the battery cell i is Where k is the input and output length of the model, and both satisfy (m+2)k≤EOL i , m is a positive integer; the capacity data of the n battery cells are reconstructed and then connected end to end to obtain a complete training data set for training the jth model
[0010] Furthermore, in one embodiment of the present invention, the capacity prediction model based on the sequence-to-sequence model includes an encoder and a decoder, wherein the encoder selects a long short-term memory network and sets it as a sequence output, and the decoder selects an LSTM network and maps the output sequence to an output format through a fully connected layer.
[0011] Furthermore, in one embodiment of the present invention, the failure threshold is when the single-cycle discharge capacity of the cell degrades to 80% of its capacity, and the life end point is the number of cycles at which the predicted capacity value reaches the failure threshold.
[0012] Furthermore, in one embodiment of the present invention, the final prediction result for:
[0013]
[0014] Where, j is the number of capacity degradation curves, is the capacity prediction value of the qth model in period t.
[0015] To achieve the above-mentioned purpose, another embodiment of the present invention proposes a long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling, including: an acquisition module for acquiring battery capacity data of a preset number of lithium-ion battery cells in each cycle Wherein, t is the cycle number, i is the cell number (i=1, 2, ..., n), and a total of n battery cell capacity degradation data are obtained, which includes the cell to be predicted; a reconstruction module is used to reconstruct the capacity degradation data of n-1 other battery cells working under the same working conditions as the cell to be predicted into a training data set A training module is used to establish j capacity prediction models based on sequence-to-sequence models with different input and output structures, and use the training data set j capacity prediction models based on sequence-to-sequence models are trained respectively; the first prediction module is used to calculate the first k capacity prediction models of the battery cells to be tested. jThe discharge capacity of the j-cycle is used as the initial input of the j-th trained capacity prediction model based on the sequence-to-sequence model to obtain the first step prediction output result; an iterative prediction module is used to input the first step prediction output result as a new input sequence into the j-th trained capacity prediction model based on the sequence-to-sequence model to obtain the next step prediction output result, iteratively execute until it is lower than the failure threshold, and connect the output results of each step end to end to obtain a degradation process curve and a life cutoff point; an overall iterative prediction module is used to execute the first prediction module and the iterative prediction module on the j trained capacity prediction models based on the sequence-to-sequence model respectively to obtain j capacity degradation curves and j life cutoff points; a solution module is used to average the capacity of the j capacity degradation curves over the cycle t to obtain a final prediction result
[0016] The long-life lithium-ion battery early life prediction system based on degradation sequence time series association modeling in the embodiment of the present invention establishes a lithium-ion battery capacity degradation prediction model and realizes the prediction of the life end period through the capacity degradation curve; the capacity degradation prediction model is based on a sequence-to-sequence model, and greatly reduces the number of iteration steps in the long-term prediction process by outputting the sequence prediction result; in addition, by constructing a sequence-to-sequence model with different structures and fusing the prediction results of each model, a fused prediction result integrating multiple time domain dependencies can be obtained, and finally the long-term stable prediction of the lithium-ion battery capacity degradation process and the life end period is realized, which solves the problem of low long-term accuracy and stability of the single-step iterative prediction method based on historical data in the field of long-life satellite lithium-ion capacity degradation estimation and remaining life prediction, and can achieve fragmented prediction results compared with traditional degradation trajectory prediction and life prediction methods.
[0017] In addition, the long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling according to the above embodiment of the present invention may also have the following additional technical features:
[0018] Furthermore, in one embodiment of the present invention, the reconstruction module is specifically: battery cell i is Where k is the input and output length of the model, and both satisfy (m+2)k≤EOL i , m is a positive integer; the capacity data of the n battery cells are reconstructed and then connected end to end to obtain a complete training data set for training the jth model
[0019] Furthermore, in one embodiment of the present invention, the capacity prediction model based on the sequence-to-sequence model includes an encoder and a decoder, wherein the encoder selects a long short-term memory network and sets it as a sequence output, and the decoder selects an LSTM network and maps the output sequence to an output format through a fully connected layer.
[0020] Furthermore, in one embodiment of the present invention, the failure threshold is when the single-cycle discharge capacity of the cell degrades to 80% of its capacity, and the life end point is the number of cycles at which the predicted capacity value reaches the failure threshold.
[0021] Furthermore, in one embodiment of the present invention, the final prediction result for:
[0022]
[0023] Where, j is the number of capacity degradation curves, is the capacity prediction value of the qth model in period t.
[0024] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the following description of the embodiments in conjunction with the accompanying drawings, in which:
[0026] Figure 1 It is a flow chart of a method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling according to an embodiment of the present invention;
[0027] Figure 2 It is a schematic diagram of the structure of a Seq2Seq prediction model according to an embodiment of the present invention;
[0028] Figure 3 It is an overall block diagram of a method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling according to an embodiment of the present invention;
[0029] Figure 4 This is a schematic diagram of monomer fusion prediction results according to an embodiment of the present invention;
[0030] Figure 5 It is a structural schematic diagram of a system for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling according to an embodiment of the present invention. DETAILED DESCRIPTION
[0031] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0032] The following describes a method and system for predicting the early life of a long-life lithium-ion battery based on degradation sequence timing association modeling proposed in an embodiment of the present invention with reference to the accompanying drawings. First, the method for predicting the early life of a long-life lithium-ion battery based on degradation sequence timing association modeling proposed in an embodiment of the present invention will be described with reference to the accompanying drawings.
[0033] Figure 1 The present invention is a flowchart of a method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling according to an embodiment of the present invention.
[0034] like Figure 1 As shown, the long-life lithium-ion battery early life prediction method based on degradation sequence temporal correlation modeling includes the following steps:
[0035] In step S1, the battery capacity data of each cycle of a preset number of lithium-ion battery cells is obtained. Wherein, t is the cycle number, i is the cell number (i=1, 2, ..., n), and the capacity degradation data of n battery cells are obtained in total, which includes the cell to be predicted.
[0036] In step S2, the capacity degradation data of n-1 other battery cells operating under the same working conditions as the cell to be predicted are reconstructed into a training data set
[0037] Specifically, for battery cell i, Where k is the input and output length of the model. For different models, k takes different values and all satisfy (m+2)k≤EOL. i , m is a positive integer; the capacity data of n battery cells are reconstructed and then connected end to end to obtain a complete training data set for training the jth model Right now
[0038] In step S3, j capacity prediction models based on sequence-to-sequence models with different input and output structures are established, and the training data set is used Train j capacity prediction models based on sequence-to-sequence models respectively.
[0039] Furthermore, in one embodiment of the present invention, a capacity prediction model based on a sequence-to-sequence model includes an encoder and a decoder, wherein the encoder selects a long short-term memory network and sets it as a sequence output, and the decoder selects an LSTM network and maps the output sequence to an output format through a fully connected layer.
[0040] Specifically, Figure 2 As shown in the figure, a capacity prediction model based on the sequence-to-sequence model Seq2Seq is established. The Seq2Seq model consists of two parts, namely the encoder and the decoder. The encoder selects the Long Short-Term Memory (LSTM) network and sets it as a sequence output; the decoder also selects the LSTM network and maps the decoder's output sequence to the output format through the fully connected layer. The input and output formats of the Seq2Seq model are both (k, 1). The j Seq2Seq models with different input and output structures are constructed, and the input and output lengths are k1, k1…, k j , and then use the training data set Train j capacity prediction models based on sequence-to-sequence models respectively.
[0041] In step S4, the first k cells of the battery to be tested are j The discharge capacity of the jth cycle is used as the initial input of the jth trained capacity prediction model based on the sequence-to-sequence model to obtain the first step prediction output result.
[0042] Specifically, Figure 3 As shown in the figure, for the monomer to be predicted, a cyclic charge and discharge experiment is first performed on it. i The prediction starts when the capacity data of each cycle is obtained. Since the length of the initial segment data is different, the prediction starting point is considered to be max(k1, k2, ..., k j )+1, the first k j The discharge capacity of the jth cycle is used as the initial input of the jth trained capacity prediction model based on the sequence-to-sequence model, that is, (where the superscript represents the number of cycles), and the first step prediction output result is obtained, which is recorded as in Indicates k j +1 is the capacity forecast value at time.
[0043] In step S5, the prediction output result of the first step is input as a new input sequence into the jth trained capacity prediction model based on the sequence-to-sequence model to obtain the prediction output result of the next step, and the iterative execution is performed until it is lower than the failure threshold. The prediction output results of each step are connected end to end and spliced to obtain the degradation process curve and the life cutoff point.
[0044] Furthermore, in one embodiment of the present invention, the failure threshold is when the single-cycle discharge capacity of the battery cell degrades to 80% of its capacity, and the end-of-life point is the number of cycles at which the capacity prediction value reaches the failure threshold. That is, the end-of-life cycle of the i-th battery cell is recorded as EOL. j , which is the number of cycles when the single-cycle discharge capacity of the monomer degrades to 80% of its maximum capacity.
[0045] Specifically, Figure 3 As shown, As a new input sequence, it is input into the Seq2Seq model to obtain the next prediction result. And so on, until the predicted capacity is lower than the failure threshold, the prediction results of each step are connected end to end to obtain a complete degradation process curve. At the same time, the number of cycles to reach the predicted value of the failure threshold capacity is the life cutoff point predicted by the model, recorded as
[0046] In step S6, steps S4-S5 are respectively executed on the j trained capacity prediction models based on the sequence-to-sequence model to obtain j capacity degradation curves and j life cut-off points.
[0047] In step S7, the capacity of j capacity degradation curves is averaged over period t to achieve the fusion of prediction results of different Seq2Seq models and obtain the final prediction result. Specifically:
[0048]
[0049] Where, j is the number of capacity degradation curves, is the capacity prediction value of the qth model in period t.
[0050] The method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling proposed in the embodiment of the present invention is further described below through a specific embodiment.
[0051] First, a certain model of 18650 commercial lithium-ion battery cycle charge and discharge data was used for testing. There were 8 cells in the data set, and one of the cells was unavailable due to equipment failure, so the remaining 7 sets of data were used for testing. The battery capacity data of each lithium-ion battery cell in each cycle was recorded, where t is the cycle number, i=1,2,…,7 is the cell number, and a total of 7 battery cell capacity degradation data were obtained;
[0052] Then, the end-of-life cycle of the i-th battery cell is recorded as EOL i , which is the number of cycles when the single-cycle discharge capacity of the monomer degrades to 80% of its maximum capacity.
[0053] The capacity degradation data of #1-#6 battery cells are constructed into a training data set for training model j For monomer i, Where k represents the input and output length of the model. For different models, k takes different values and all satisfy (m+2)k≤EOL. i , m is a positive integer. After the capacity data of the six monomers are reconstructed, they are connected end to end to obtain a complete training data set for training the jth model, that is,
[0054] 10 capacity prediction models based on Seq2Seq model are established, i.e., j=10. Seq2Seq model consists of two parts, namely encoder and decoder. The encoder selects LSTM network and sets it as sequence output; the decoder also selects LSTM network and maps the output sequence of the decoder to the output format through the fully connected layer. The input and output formats of Seq2Seq model are (k i , 1)
[0055] Ten Seq2Seq models with different input and output structures were established, i.e., j = 10, and the input and output lengths were 57, 61, 67, 74, 82, 90, 92, 93, 100, and 105 respectively;
[0056] Use the constructed training dataset Train 10 Seq2Seq models separately;
[0057] The first k of the battery cell to be predicted j The discharge capacity of the jth cycle is used as the initial input of the jth Seq2Seq model, that is, (where the superscript represents the number of cycles), and the first step prediction output result is obtained, which is recorded as in Indicates k j +1 capacity forecast value at time;
[0058] Will The new input sequence is input into the Seq2Seq model to obtain the next prediction result. This process is repeated until the predicted capacity is lower than the failure threshold. The prediction results of each step are connected end to end to obtain a complete degradation process curve; the number of cycles to reach the predicted value of the failure threshold capacity is the life cutoff point predicted by the model, recorded as
[0059] The first two steps were performed on 10 Seq2Seq models respectively to obtain 10 capacity degradation curves and 10 life end points. The capacity and EOL prediction results of 7 groups of batteries are shown in Table 1 below:
[0060]
[0061] The capacity degradation curves obtained from the 10 predictions are averaged on a cycle scale to achieve the fusion of prediction results from different Seq2Seq models and obtain the final prediction result. like Figure 4 shown.
[0062] In the figure, the red curve is the discharge capacity fusion prediction result, and the blue curve is the real capacity degradation curve of the #7 monomer. The uncertainty of EOL in the fusion prediction result is calculated by statistical analysis, and the uncertainty of EOL estimation of each monomer is shown in Table 2 below:
[0063] Table 2 Confidence results of the proposed method for each monomer EOL estimation
[0064]
[0065] From the above results, it can be seen that the capacity degradation curve and the remaining life (life end cycle) of the lithium-ion battery using the method proposed in the embodiment of the present invention are more accurate and have a higher confidence level.
[0066] In summary, the method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling proposed in the embodiment of the present invention has the following beneficial effects:
[0067] (1) Compared with the conventional iterative multi-step prediction method that only updates the capacity data of one cycle in each update step, the embodiment of the present invention uses a fragmented input and output structure, and uses the fragment data as the update content in the iterative process, that is, the capacity data of one fragment is updated in each step;
[0068] (2) Compared with the existing deep learning-based lithium battery long-term capacity prediction methods, which mostly model and predict based on only one fixed time domain dependency, the prediction results of the embodiments of the present invention integrate multiple time domain dependencies (i.e., the mapping relationship between the time series data before and after), thereby having the advantages of higher long-term accuracy and stability.
[0069] The use of sequence-to-sequence model realizes accurate and stable prediction of capacity degradation and remaining life of long-life lithium batteries, which to some extent solves the problems of poor long-term prediction accuracy and stability caused by the single-step iterative prediction mode commonly used in this field; at the same time, the output results of multiple sequence-to-sequence models are fused to obtain the final estimation result; compared with the traditional single-step iterative method, this method integrates multiple time domain dependencies in the capacity degradation process, which improves the overall prediction accuracy of the method while ensuring good model generalization ability and prediction stability; in addition, the global accuracy of capacity prediction of this method can reach about 0.3%, and the confidence of EOL estimation results is relatively high, which has better accuracy and stability than traditional methods.
[0070] Next, a long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling proposed in accordance with an embodiment of the present invention will be described with reference to the accompanying drawings.
[0071] Figure 5 It is a structural schematic diagram of a system for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling according to an embodiment of the present invention.
[0072] like Figure 5 As shown, the system 10 includes: an acquisition module 100 , a training module 200 , a first prediction module 300 , an iterative prediction module 400 , an overall iterative prediction module 500 and a solution module 600 .
[0073] The acquisition module 100 is used to acquire the battery capacity data of each cycle of a preset number of lithium-ion battery cells. Where t is the cycle number, i is the cell number (i=1, 2, ..., n), and the capacity degradation data of n battery cells are obtained, which includes the cell to be predicted. The reconstruction module 200 is used to reconstruct the capacity degradation data of n-1 other battery cells working under the same working conditions as the cell to be predicted into a training data set. The training module 300 is used to establish j capacity prediction models based on sequence-to-sequence models with different input and output structures, and use the training data set The first prediction module 400 is used to train j capacity prediction models based on the sequence-to-sequence model. j The discharge capacity of the jth cycle is used as the initial input of the jth trained capacity prediction model based on the sequence-to-sequence model to obtain the first step prediction output result. The iterative prediction module 500 is used to input the first step prediction output result as a new input sequence into the jth trained capacity prediction model based on the sequence-to-sequence model to obtain the next step prediction output result, iteratively execute until it is lower than the failure threshold, and splice the prediction output results of each step end to obtain the degradation process curve and the life cutoff point. The overall iterative prediction module 600 is used to execute the first prediction module and the iterative prediction module respectively on the j trained capacity prediction models based on the sequence-to-sequence model to obtain j capacity degradation curves and j life cutoff points. The solution module 700 is used to average the capacity of the j capacity degradation curves over period t to obtain the final prediction result.
[0074] Furthermore, in one embodiment of the present invention, the reconstruction module is specifically:
[0075] Battery cell i is Where k is the input and output length of the model, and both satisfy (m+2)k≤EOL i , m is a positive integer;
[0076] Reconstruct the capacity data of n battery cells and then connect them end to end to obtain a complete training data set for training the jth model.
[0077] Furthermore, in one embodiment of the present invention, a capacity prediction model based on a sequence-to-sequence model includes an encoder and a decoder, wherein the encoder selects a long short-term memory network and sets it as a sequence output, and the decoder selects an LSTM network and maps the output sequence to an output format through a fully connected layer.
[0078] Furthermore, in one embodiment of the present invention, the failure threshold is when the single-cycle discharge capacity of the cell degrades to 80% of its capacity, and the life end point is the number of cycles at which the predicted capacity value reaches the failure threshold.
[0079] Furthermore, in one embodiment of the present invention, the final prediction result for:
[0080]
[0081] Where, j is the number of capacity degradation curves, is the capacity prediction value of the qth model in period t.
[0082] It should be noted that the aforementioned explanation of the embodiment of the method for predicting the early life of a long-life lithium-ion battery based on time series correlation modeling of degradation sequences is also applicable to the system for predicting the early life of a long-life lithium-ion battery based on time series correlation modeling of degradation sequences of this embodiment, and will not be repeated here.
[0083] The long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling proposed in an embodiment of the present invention has the following beneficial effects:
[0084] (1) Compared with the conventional iterative multi-step prediction method that only updates the capacity data of one cycle in each update step, the embodiment of the present invention uses a fragmented input and output structure, and uses the fragment data as the update content in the iterative process, that is, the capacity data of one fragment is updated in each step;
[0085] (2) Compared with the existing deep learning-based lithium battery long-term capacity prediction methods, which mostly model and predict based on only one fixed time domain dependency, the prediction results of the embodiments of the present invention integrate multiple time domain dependencies (i.e., the mapping relationship between the time series data before and after), thereby having the advantages of higher long-term accuracy and stability.
[0086] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0087] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0088] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.
Claims
1. A method for predicting the early life of long-life lithium-ion batteries based on degradation sequence temporal correlation modeling, characterized in that: The following steps are involved: Step S1, obtaining the battery capacity data of each cycle of a preset number of lithium-ion battery cells ,in, is the number of cycles, Number the monomers ( =1, 2, …, n ), a total of Capacity degradation data of battery cells, including the battery cell to be predicted; Step S2: -1 Capacity degradation data of other battery cells working under the same working conditions as the battery cell to be predicted is reconstructed into a training data set ; Step S3, establish A capacity prediction model based on a sequence-to-sequence model with different input and output structures, and using the training dataset Separate training A capacity prediction model based on a sequence-to-sequence model; Step S4: The discharge capacity of the first cycle is taken as The initial input of a trained capacity prediction model based on a sequence-to-sequence model is used to obtain the first step prediction output result; Step S5, inputting the prediction output result of the first step as a new input sequence into the The next prediction output is obtained from a trained capacity prediction model based on a sequence-to-sequence model, and it is iterated until it is below the failure threshold. The prediction output results of each step are connected end to end to obtain the degradation process curve and the life cutoff point. Step S6: The capacity prediction models based on the sequence-to-sequence model execute steps S4-S5 respectively, and obtain Capacity degradation curves and Life end point; Step S7, The capacity degradation curve is Take the average of the capacity above to get the final prediction result ; The capacity prediction model based on the sequence-to-sequence model includes an encoder and a decoder, wherein the encoder selects a long short-term memory network and sets it as a sequence output, and the decoder selects an LSTM network and maps the output sequence to an output format through a fully connected layer.
2. The method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling according to claim 1 is characterized in that: The step S2 is specifically as follows: Battery Cell for , ,in, is the input and output length of the model, and both satisfy , is a positive integer; the end-of-life cycle of the i-th battery cell is recorded as EOL i , which is the number of cycles when the single-cycle discharge capacity of the monomer degrades to 80% of its maximum capacity; The The capacity data of each battery cell is reconstructed and then connected end to end to obtain a complete data set for training the first The training dataset for the model , .
3. The method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling according to claim 1 is characterized in that: The failure threshold is when the single-cycle discharge capacity of the cell degrades to 80% of its capacity, and the life end point is the number of cycles at which the predicted capacity value reaches the failure threshold.
4. The method for predicting the early life of a long-life lithium-ion battery based on degradation sequence temporal correlation modeling according to claim 1 is characterized in that: The final prediction result for: in, is the number of capacity degradation curves, For the Models in Capacity forecast for the period.
5. A long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling, characterized in that: include: The acquisition module is used to obtain the battery capacity data of each cycle of a preset number of lithium-ion battery cells. ,in, is the number of cycles, Number the monomers ( =1, 2, …, n ), a total of Capacity degradation data of battery cells, including the battery cell to be predicted; Refactoring module to -1 capacity degradation data of other battery cells working under the same working conditions as the battery cell to be predicted is reconstructed into a training data set ; Training module, used to build A capacity prediction model based on a sequence-to-sequence model with different input and output structures, and using the training dataset Separate training A capacity prediction model based on a sequence-to-sequence model; The first prediction module is used to predict the battery cell The discharge capacity of the first cycle is taken as The initial input of a trained capacity prediction model based on a sequence-to-sequence model is used to obtain the first step prediction output result; Iterative prediction module, used to input the first step prediction output result as a new input sequence into the first step prediction output The next prediction output is obtained from a trained capacity prediction model based on a sequence-to-sequence model, and it is iterated until it is below the failure threshold. The prediction output results of each step are connected end to end to obtain the degradation process curve and the life cutoff point. The overall iterative prediction module is used to convert the trained The capacity prediction models based on the sequence-to-sequence model respectively execute the first prediction module and the iterative prediction module to obtain Capacity degradation curves and Life end point; Solving module, used for The capacity degradation curve is Take the average of the capacity above to get the final prediction result ; The capacity prediction model based on the sequence-to-sequence model includes an encoder and a decoder, wherein the encoder selects a long short-term memory network and sets it as a sequence output, and the decoder selects an LSTM network and maps the output sequence to an output format through a fully connected layer.
6. The long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling according to claim 5 is characterized in that: The reconstruction module is specifically: Battery Cell for , ,in, is the input and output length of the model, and both satisfy , is a positive integer; the end-of-life cycle of the i-th battery cell is recorded as EOLi, which is the number of cycles when the single-cycle discharge capacity of the cell degrades to 80% of its maximum capacity; The The capacity data of each battery cell is reconstructed and then connected end to end to obtain a complete data set for training the first The training dataset for the model , .
7. The long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling according to claim 5 is characterized in that: The failure threshold is when the single-cycle discharge capacity of the cell degrades to 80% of its capacity, and the life end point is the number of cycles at which the predicted capacity value reaches the failure threshold.
8. The long-life lithium-ion battery early life prediction system based on degradation sequence temporal correlation modeling according to claim 5 is characterized in that: The final prediction result for: in, is the number of capacity degradation curves, For the Models in Capacity forecast for the period.
Citation Information
Patent Citations
Method for monitoring state and predicting cut-off voltage of spatial lithium ion battery
CN103336913A
Cycle life indirect prediction method for lithium ion battery provided with uncertain intervals on basis of GPR (general purpose register)
CN103389471A