Single crystal manufacturing equipment
By using a cooling auxiliary cylinder such as graphite material embedded in the cooling cylinder in a single crystal manufacturing device, and optimizing heat conduction with the heat insulation components, the problem of insufficient cooling efficiency in the prior art is solved, and the single crystal is realized High-speed growth and efficient cooling.
Patent Information
- Application Number
- CN202080091664.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-01-10
- Filing Date
- 2020-11-20
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2040-11-20
AI Technical Summary
The existing single crystal manufacturing devices have limitations in improving the growth rate and cooling effect of single crystals, especially the inability to efficiently conduct radiant heat from the heater, resulting in insufficient temperature gradient in the crystal, limiting the growth rate and quality of single crystals.
The cooling auxiliary cylinder is built into the cooling cylinder, made of graphite material, carbon composite material, stainless steel or molybdenum, covering the bottom surface of the cooling cylinder and contacting its bottom surface, increasing the ability of the cooling auxiliary cylinder to withstand radiant heat, thereby improving the Heat conduction efficiency and further optimize the heat conduction path through thermal insulation components.
The growth rate and cooling effect of single crystals are significantly improved, the temperature gradient in the crystal is increased, and the high-speed growth and efficient cooling of single crystals are achieved.
Smart Images

Figure CN114929951B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a manufacturing apparatus for single crystal silicon and the like using the Czochralski method. Background Art
[0002] Semiconductors such as silicon and gallium arsenide are composed of single crystals and are used in memories of computers ranging from small to large computers. There is a demand for storage devices with larger capacity, lower cost, and higher quality.
[0003] Conventionally, as one of the single crystal manufacturing methods for manufacturing single crystals that meet the requirements of these semiconductors, there is a known method (generally referred to as the Czochralski method (CZ method)), in which a seed crystal is immersed in a molten semiconductor raw material contained in a crucible and then pulled up to thereby manufacture a large-diameter, high-quality semiconductor.
[0004] Hereinafter, a conventional single crystal manufacturing apparatus utilizing the CZ method will be described by taking the growth of single crystal silicon as an example. Figure 7 A schematic cross-sectional view showing an example of an existing single crystal manufacturing device. In a single crystal manufacturing device (existing example) 200 used when manufacturing single crystal silicon by the CZ method, a quartz crucible 4 and a graphite crucible 5 that can be raised and lowered and contain a raw material melt 6 are usually arranged in a main chamber 2 for growing a single crystal, and a heater 11 that is arranged in a manner to surround the quartz crucible 4 and the graphite crucible 5 is arranged, and a pulling chamber 3 for accommodating and taking out the grown single crystal is continuously arranged at the upper part of the main chamber 2. In addition, a heat insulating member 13 is provided between the main chamber 2 and the heater 11, and a heat insulating member 14 is provided between the pulling chamber 3 and the raw material melt 6. The heat insulating member 14 extends downward from the top of the main chamber 2.
[0005] When using such a single crystal manufacturing apparatus 200 to manufacture a single crystal, the seed crystal 9 is immersed in the raw material melt 6, and the seed crystal 9 and the crucible rotating shaft 12 are rotated while the seed crystal 9 is gently pulled upward to grow a rod-shaped single crystal. On the other hand, in order to obtain the desired diameter and crystal quality, the quartz crucible 4 and the graphite crucible 5 are raised in a manner that coordinates the growth of the crystal in a manner so that the height of the melt surface is always kept constant.
[0006] Moreover, when cultivating a single crystal, after the seed crystal 9 installed on the seed crystal holder 10 is immersed in the raw material melt 6, the seed crystal 9 is rotated in the desired direction by using a pulling mechanism (not shown), and the wire 8 is gently wound to grow the single crystal 7 at the front end of the seed crystal 9. However, in order to eliminate the dislocation generated when the seed crystal 9 is immersed in the raw material melt 6, the crystal is temporarily reduced in diameter to about 3 to 5 mm in the early stage of growth, and the diameter is expanded to the desired diameter at the place where the dislocation disappears, so that the target single crystal 7 is grown.
[0007] However, in the above method, with the increase in the diameter of the single crystal 7 in recent years, the strength is insufficient for supporting the increased weight of the single crystal 7. For example, for a reduced diameter (in Japanese: 絞り) of 5 mm in diameter, considering the safety factor, lifting a single crystal 7 of about 250 kg is the limit. Therefore, in recent years, by tapering the shape of the front end of the seed crystal 9, the heat capacity of the front end of the seed crystal 9 in contact with the raw material melt 6 is reduced, and very few dislocations are generated at the moment when the seed crystal 9 comes into contact with the raw material melt 6, so that the cultivation of a single crystal 7 without a necking is practically implemented.
[0008] At this time, the pulling speed of the sizing part with a constant diameter of the single crystal 7 depends on the diameter of the pulled single crystal and is a very slow speed of about 0.4 to 2.0 mm / min. If forced to pull quickly, the single crystal 7 under cultivation will deform and a cylindrical product with a constant diameter cannot be obtained. Or, problems such as slip dislocations occurring in the single crystal 7 or the single crystal 7 separating from the raw material melt and not becoming a product exist, and there is a limit to achieving high-speed crystal growth rate.
[0009] However, in the process of manufacturing the single crystal 7 using the above-mentioned existing CZ method, in order to improve productivity and reduce costs, increasing the growth speed of the single crystal 7 is an important means, and many improvements have been made so far to achieve high-speed growth of the single crystal 7.
[0010] The growth speed of the single crystal 7 is determined by the heat balance of the single crystal 7 during growth. To increase its speed, it is known that as long as the heat discharged from the surface of the single crystal 7 is effectively removed. That is to say, if the cooling effect of the single crystal 7 can be improved, single crystals can be manufactured more efficiently.
[0011] Moreover, it is known that the quality of the crystal varies according to the cooling rate of the single crystal 7. For example, in single crystal silicon, the grown-in defects formed during single crystal cultivation can be controlled by the ratio of the temperature gradient inside the crystal to the pulling speed (growth speed) of the single crystal, and defect-free single crystals can also be cultivated by controlling this ratio (Patent Document 1).
[0012] Therefore, whether it is to manufacture defect-free crystals or to increase the growth speed of single crystals to improve productivity, it is important to improve the cooling effect of the single crystal under cultivation.
[0013] To efficiently cool the single crystal 7 in the CZ method, the following method is effective, that is, the radiation from the heater 11 is not directly irradiated onto the crystal, and the object to be forcibly cooled such as the chamber absorbs the radiation heat from the single crystal 4. As the structure of the device that can achieve this method, a filter structure is cited (Patent Document 2).
[0014] However, in this structure, if a filter structure is set to avoid contact with the upper end of the crucible due to the rise of the crucible, the inner diameter of the upper part of the filter needs to be reduced, resulting in a disadvantage that it is difficult to cool the single crystal. In addition, in order to prevent contamination caused by oxidizing gas during single crystal pulling, inert gas is introduced from the gas inlet 18 and exhausted from the gas outlet 19. At this time, in such a filter structure, there is also a problem that the cooling effect of the single crystal by the inert gas cannot be expected.
[0015] Therefore, a structure has been proposed, which has a rectifying cylinder for rectifying the inert gas and a heat insulating ring for shielding the rectifying cylinder from direct radiation from the heater and the raw material melt (Patent Document 3). In this method, the cooling effect of the single crystal produced by the inert gas can be expected, but the cooling capacity is not high in terms of making the cooling chamber absorb the radiation heat from the single crystal.
[0016] As a method for solving the problems of the filter structure and the rectifying cylinder and cooling efficiently, a method of configuring a cooling cylinder for cooling with water around the crystal has been proposed (Patent Document 4). In this method, the outer side of the cooling cylinder is protected by a cooling cylinder protection material such as a protective cover made of graphite material, and the heat of the single crystal can be efficiently removed from the inner side of the cooling cylinder. However, for safety reasons, the cooling cylinder is not extended to the vicinity of the melt surface, and the cooling effect of the single crystal up to the cooling cylinder is slightly weak.
[0017] In addition, Patent Document 5 discloses a method of extending a graphite material embedded in a cooling tube. However, in this method, the cooling tube and the extended graphite receive heat from the outside and cannot exert a sufficient cooling effect, and the cooling tube and the graphite material are difficult to contact, so that heat cannot be efficiently transferred from the graphite material to the cooling tube.
[0018] In order to solve this problem, Patent Document 6 proposes a method as follows. Figure 7 The method shown uses a cooling auxiliary cylinder 217 fitted in the cooling cylinder 15. The heat generated from the crystallization is transferred to the cooling cylinder 15 via the cooling auxiliary cylinder 217, and the cooling medium is supplied to the cooling cylinder 15 from the cooling medium inlet 16, so that the heat generated from the crystallization is dissipated. According to this method, the pulling speed of the crystal can be increased.
[0019] Prior art literature
[0020] Patent Literature
[0021] Patent Document 1: Japanese Patent Application Laid-Open No. 11-157996
[0022] Patent Document 2: Japanese Patent Publication No. 57-40119
[0023] Patent Document 3: Japanese Patent Application Laid-Open No. 1-65086
[0024] Patent Document 4: International Publication No. 01 / 57293
[0025] Patent Document 5: Japanese Patent Application Laid-Open No. 6-199590
[0026] Patent Document 6: Japanese Patent Application Publication No. 2009-161416
[0027] Patent Document 7: Japanese Patent Application Publication No. 2013-193897 Summary of the invention
[0028] 1. Technical issues to be resolved
[0029] Figure 7 The cooling auxiliary cylinder 217 is a structure that contacts only the inner side surface of the cooling cylinder 15 surrounding the single crystal 7, and does not contact the bottom surface of the cooling cylinder 15 facing the raw material melt 6. As described above, in order to increase the pulling speed of the crystal, it is sufficient to make the object for forced cooling such as the chamber absorb the radiant heat from the single crystal 7, but removing the radiant heat from the high temperature part such as the heater 11 is also effective in increasing the pulling speed of the crystal.
[0030] Therefore, by using a cooling auxiliary cylinder that is also in contact with the bottom surface of the cooling cylinder facing the raw material melt, in addition to conducting the radiant heat from the single crystal to the cooling cylinder, it is also possible to efficiently conduct the radiant heat from high-temperature parts such as the heater to the cooling cylinder, thereby increasing the temperature gradient within the crystal. There is room for improvement in further increasing the pulling speed of the single crystal.
[0031] In Patent Document 7 Figure 2 The structure in which the bottom surface of the cooling cylinder facing the raw material melt is covered with an insulating material is shown, but the insulating material is a material with low thermal conductivity, and there is a problem that it is not expected that the pulling speed of the single crystal can be further increased by efficiently conducting the radiant heat of the single crystal, heater, etc. to the cooling cylinder.
[0032] The present invention has been completed in view of the above-mentioned problems, and its purpose is to provide a single crystal manufacturing device, which, by using a cooling auxiliary cylinder, in addition to conducting radiant heat from the single crystal to the cooling cylinder, also efficiently conducts radiant heat from high-temperature parts such as heaters to the cooling cylinder, thereby increasing the temperature gradient within the crystal and significantly improving the pulling speed of the single crystal, wherein the above-mentioned cooling auxiliary cylinder has a structure for contacting the bottom surface of the cooling cylinder facing the raw material melt in addition to the inner side surface of the cooling cylinder surrounding the single crystal.
[0033] (II) Technical solution
[0034] The present invention is made to achieve the above-mentioned purpose, and provides a single crystal manufacturing device, which cultivates single crystals using the Czochralski method, and comprises: a main chamber, which accommodates a crucible for storing a raw material melt and a heater for heating the raw material melt; a pulling chamber, which is connected to the upper part of the main chamber, and the growing single crystal is pulled and stored in the pulling chamber; a cooling cylinder, which extends from at least the top of the main chamber to the raw material melt in a manner to surround the single crystal being pulled and is forcibly cooled by a cooling medium; and a cooling auxiliary cylinder, which is embedded in the cooling cylinder, the material of the cooling auxiliary cylinder is composed of any one or more of graphite material, carbon composite material, stainless steel, molybdenum, and tungsten, and the cooling auxiliary cylinder has a structure covering the bottom surface of the cooling cylinder facing the raw material melt, and the gap between the cooling auxiliary cylinder and the bottom surface of the cooling cylinder is less than 1.0 mm.
[0035] If it is such a single crystal manufacturing device, not only can the amount of radiation heat from the high temperature parts such as the heater that the part of the cooling auxiliary tube covering the bottom surface of the cooling tube bears can be increased, but also the part of the cooling auxiliary tube covering the bottom surface of the cooling tube can be further heated, so that the cooling auxiliary tube thermally expands, and the gap with the bottom surface of the cooling tube can be reduced, and heat can be easily transferred to the cooling tube. In addition, the part of the cooling auxiliary tube covering the bottom surface of the cooling tube is heated because it bears more radiation heat from the raw material melt and the heater, and the radiation heat emitted by the cooling auxiliary tube itself toward the bottom surface of the cooling tube becomes larger. Therefore, even if there is a gap of less than 1.0 mm between the cooling auxiliary tube and the bottom surface of the cooling tube, heat can be transferred to the cooling tube. Therefore, in addition to transferring the radiation heat from the single crystal to the cooling tube, the radiation heat from the high temperature parts such as the heater is also efficiently transferred to the cooling tube, so that the temperature gradient in the crystal can be increased, and the pulling speed of the single crystal can be further improved.
[0036] In this case, at least 50% of the entire area of the bottom surface of the cooling cylinder can be covered by the auxiliary cooling cylinder.
[0037] In this way, not only the amount of radiant heat received from high-temperature parts such as heaters can be increased, but the part of the cooling auxiliary tube covering the bottom surface of the cooling tube can also be further heated and thermally expanded, which can reduce the gap with the bottom surface of the cooling tube and make it easier to conduct heat to the cooling tube, thereby further increasing the temperature gradient within the crystal and further improving the pulling speed of the single crystal.
[0038] Preferably, the auxiliary cooling cylinder has a flange that projects from the inside to the outside of the cooling cylinder to cover the bottom surface of the cooling tower as a structure that covers the bottom surface of the cooling cylinder facing the raw material melt.
[0039] Such a flange is subjected to more radiation heat from the raw material melt and the heater and becomes high temperature compared to the portion of the cooling auxiliary tube covering the inner side of the cooling tube. Therefore, even if the flange of the cooling auxiliary tube covering the bottom surface of the cooling tube leaves a gap at room temperature, it can expand thermally by becoming high temperature when manufacturing a single crystal, and the gap with the bottom surface of the cooling tube can be reduced, making it easy to conduct heat to the cooling tube. In addition, the flange of the cooling auxiliary tube covering the bottom surface of the cooling tube is subjected to more radiation heat from the raw material melt and the heater and becomes high temperature, and the radiation heat emitted by the cooling auxiliary tube itself toward the bottom surface of the cooling tube becomes larger, so that heat can be conducted to the cooling tube even if there is a gap of less than 1.0 mm between the flange and the bottom surface of the cooling tube. Therefore, it is easy to conduct heat using the cooling tube, which can further increase the temperature gradient in the crystal and further improve the pulling speed of the single crystal.
[0040] In this case, it is more preferable that the single crystal manufacturing apparatus further includes a heat insulating member extending from the ceiling of the main chamber and surrounding the bottom surface of the cooling cylinder and the flange of the auxiliary cooling cylinder.
[0041] The heat insulating member extends from the top of the main chamber and surrounds the bottom surface of the cooling cylinder and the flange of the auxiliary cooling cylinder. Therefore, by providing such a heat insulating member, the radiant heat generated by the flange of the auxiliary cooling cylinder can be more efficiently conducted to the bottom surface of the cooling cylinder.
[0042] The gap between the flange of the auxiliary cooling cylinder and the bottom surface of the cooling cylinder can be 0.1 mm or more and 1.0 mm or less.
[0043] In the single crystal manufacturing device of the present invention, the flange of the cooling auxiliary cylinder covering the bottom surface of the cooling cylinder is heated by being subjected to more radiation heat from the raw material melt and the heater, and the radiation heat emitted by the cooling auxiliary cylinder itself toward the bottom surface of the cooling cylinder becomes larger. Therefore, even if there is a gap of more than 0.1 mm and less than 1.0 mm between the bottom surface of the cooling cylinder, heat can be fully transferred to the cooling cylinder.
[0044] (III) Beneficial effects
[0045] As described above, the single crystal manufacturing device of the present invention has a forced cooling cylinder and a cooling auxiliary cylinder made of a specific material embedded in the cooling cylinder. The cooling auxiliary cylinder covers the bottom surface of the cooling cylinder facing the raw material melt, so that the radiation heat from the single crystal and the radiation heat from the high temperature parts such as the heater can be efficiently conducted to the cooling cylinder. As a result, the temperature gradient in the single crystal being grown can be increased, and the growth rate of the single crystal can be accelerated. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figure 1 It is a schematic cross-sectional view showing an example of a single crystal production apparatus according to the present invention.
[0047] Figure 2 Yes Figure 1 FIG. 1 is a schematic cross-sectional view showing an enlarged view of the periphery of a cooling tube of an example of a single crystal production apparatus according to the present invention.
[0048] Figure 3 This is a graph showing the rate of increase in the growth rate of a single crystal with respect to the gap between the bottom surface of the cooling cylinder and the auxiliary cooling cylinder in Example 1 and the comparative example.
[0049] Figure 4 This is a schematic cross-sectional view showing an example of another embodiment of the single crystal production apparatus of the present invention.
[0050] Figure 5 Yes Figure 4 FIG. 1 is a schematic cross-sectional view showing an enlarged view of the peripheral portion of a cooling tube in one example of another embodiment of the single crystal production apparatus of the present invention.
[0051] Figure 6 This is a graph showing the rate of increase in the growth rate of a single crystal relative to the area of the bottom surface of the cooling cylinder covered by the auxiliary cooling cylinder in Examples 2 and 3. The result of Example 2 is plotted as a colored circle, and the result of Example 3 is plotted as a hollow circle.
[0052] Figure 7 This is a schematic cross-sectional view showing an example of a conventional single crystal production apparatus using the CZ method. DETAILED DESCRIPTION
[0053] Embodiments of the present invention will be described below, but the present invention is not limited thereto.
[0054] As mentioned above, it is known that in the manufacture of single crystals using the CZ method, in order to improve productivity and reduce costs, speeding up the growth rate of the single crystal is a common method. In order to speed up the growth rate of the single crystal, it is only necessary to effectively remove the radiant heat from the single crystal and the radiant heat from high-temperature parts such as heaters, thereby increasing the temperature gradient within the crystal.
[0055] In order to overcome this technical problem, a technology has been developed, as described in Patent Document 6, in which a cooling auxiliary cylinder is embedded inside a cooling cylinder that extends from the top of the main chamber to the raw material melt in a manner to surround the single crystal being pulled and is forcibly cooled by a cooling medium. This effectively transfers heat absorbed by the single crystal being grown from the embedded portion to the cooling cylinder, thereby efficiently cooling the single crystal being grown and achieving a faster growth rate of the single crystal.
[0056] However, in the technology described in Patent Document 6, the bottom surface of the cooling cylinder facing the raw material melt is not covered by the cooling auxiliary cylinder. As described above, in order to achieve a high growth rate of the single crystal, in addition to efficiently removing the radiant heat from the single crystal, it is also important to efficiently remove the radiant heat from the high temperature parts such as the heater.
[0057] The inventors of the present invention have repeatedly conducted in-depth studies on the above-mentioned technical problems, and as a result, have come up with the idea of using the following single crystal manufacturing device to efficiently remove not only the radiant heat from the single crystal but also the radiant heat from the high-temperature parts such as the heater, thereby achieving a significantly high-speed growth rate of the single crystal, and have completed the present invention. The single crystal manufacturing device uses the Czochralski method to grow a single crystal, and comprises: a main chamber that accommodates a crucible for storing a raw material melt and a heater for heating the raw material melt; a pulling chamber that is connected to the upper part of the main chamber, and the growing single crystal is pulled and stored in the pulling chamber; a cooling cylinder that extends from at least the top of the main chamber to the raw material melt in a manner that surrounds the single crystal being pulled and is forcibly cooled by a cooling medium; and a cooling auxiliary cylinder that is embedded in the cooling cylinder, the material of the cooling auxiliary cylinder being composed of any one or more of a graphite material, a carbon composite material, stainless steel, molybdenum, and tungsten, the cooling auxiliary cylinder having a structure that covers the bottom surface of the cooling cylinder facing the raw material melt, and the gap between the cooling auxiliary cylinder and the bottom surface of the cooling cylinder is less than 1.0 mm.
[0058] Reference Figure 1 An example of a single crystal manufacturing device of the present invention is described. In addition, the description of the same structure as that of the existing device is sometimes appropriately omitted. The single crystal manufacturing device 1 of the present invention has: a main chamber 2, which accommodates a quartz crucible 4 and a graphite crucible 5 for storing a raw material melt 6 and a heater 11 for heating the raw material melt 6; a pulling chamber 3, which is connected to the upper part of the main chamber 2, and the growing single crystal is pulled and stored in the pulling chamber 3; a cooling cylinder 15, which extends from at least the top of the main chamber 2 to the raw material melt 6 in a manner to surround the single crystal being pulled and is forcibly cooled by a cooling medium; and a cooling auxiliary cylinder 17, which is embedded in the cooling cylinder 15. The cooling auxiliary cylinder 17 of the single crystal manufacturing device 1 has a structure that covers the bottom surface of the cooling cylinder 15 facing the raw material melt 6, and uses it as a flange 30. In Figure 2 1 shows an example of an enlarged view of the periphery of the cooling cylinder 15 of the single crystal production apparatus 1 of the present invention. A gap 20 between the auxiliary cooling cylinder 17 and the bottom surface of the cooling cylinder 15 is 1.0 mm or less. Preferably, the gap 20 is 0 mm (complete contact).
[0059] The flange 30 of the auxiliary cooling cylinder 17 protrudes from the inside of the cooling cylinder 15 to the outside, thereby covering the bottom surface of the cooling tower 15. That is, the auxiliary cooling cylinder 17 has the flange 30 that protrudes from the inside of the cooling cylinder 15 to the outside, thereby covering the bottom surface of the cooling cylinder 15 facing the raw material melt 6.
[0060] in addition, Figure 1 The single crystal manufacturing apparatus 1 shown in the figure further includes a heat insulating member 14 extending from the ceiling of the main chamber 2. The heat insulating member 14 surrounds the bottom surface of the cooling cylinder 15 and the flange 30 of the cooling auxiliary cylinder 17.
[0061] In order to efficiently absorb the radiant heat from the single crystal and the radiant heat from the high temperature parts such as the heater, and to conduct the heat to the cooling tube more efficiently, the material of the cooling auxiliary tube of the present invention is any one or more of graphite material, carbon composite material, stainless steel, molybdenum, and tungsten. Among the above materials, graphite material having a thermal conductivity equal to or higher than that of metal and a higher emissivity than that of metal is particularly preferred.
[0062] The auxiliary cooling cylinder has a structure that covers the bottom surface of the cooling cylinder that faces the raw material melt, and the gap between the auxiliary cooling cylinder and the bottom surface of the cooling cylinder is 1.0 mm or less. The reason for this will be described below.
[0063] The portion of the cooling auxiliary cylinder covering the bottom surface of the cooling cylinder (the portion of the flange 30) is subjected to more than 1000°C raw material melt and the radiation heat of the heater and becomes high temperature compared to the portion covering the inner side of the cooling cylinder. Therefore, even if the portion of the cooling auxiliary cylinder covering the bottom surface of the cooling cylinder is spaced out at room temperature, it can become high temperature and thermally expand when manufacturing a single crystal, and the gap with the bottom surface of the cooling cylinder can be reduced, and heat can be easily conducted to the cooling cylinder. In addition, the portion of the cooling auxiliary cylinder covering the bottom surface of the cooling cylinder is subjected to more than 1000°C raw material melt and the radiation heat of the heater and becomes high temperature, and the radiation heat emitted by the cooling auxiliary cylinder itself toward the bottom surface of the cooling cylinder becomes larger, so that heat can be conducted to the cooling cylinder even if there is a gap of less than 1.0 mm between the bottom surface of the cooling cylinder. Moreover, as described later, the inventors have found that the growth rate of the single crystal can be increased by making the gap less than 1.0 mm. Therefore, in order to achieve the high growth rate of the single crystal, the gap between the bottom surface of the cooling cylinder and the cooling auxiliary cylinder must be less than 1.0 mm. If the gap is 1.0 mm or less, the radiant heat from the single crystal and the radiant heat from the high temperature parts such as the heater can be fully conducted to the cooling tube according to the thermal expansion and radiant heat of the cooling auxiliary tube portion covering the bottom surface of the cooling tube facing the raw material melt. The gap is preferably 0 mm, but may be greater than 0.1 mm and less than 1.0 mm.
[0064] The auxiliary cooling cylinder is made of the above material and has the above structure, so it can efficiently conduct radiant heat from the single crystal and radiant heat from high temperature parts such as the heater to the cooling cylinder. This can increase the temperature gradient in the growing single crystal and increase the growth rate of the single crystal.
[0065] Furthermore, regarding the bottom surface of the cooling cylinder, at least 50% or more of the entire area of the bottom surface may be covered by the auxiliary cooling cylinder.
[0066] The larger the area of the portion of the cooling auxiliary tube that covers the bottom surface of the cooling tube, the greater the amount of radiant heat from the single crystal and the radiant heat from the high temperature parts such as the heater that is conducted to the bottom surface of the cooling tube. If the area of the portion of the cooling auxiliary tube that covers the bottom surface of the cooling tube is more than 50% of the entire area of the bottom surface of the cooling tube, not only can the amount of radiant heat from the high temperature parts such as the heater be increased, but the portion of the cooling auxiliary tube that covers the bottom surface of the cooling tube can also be further heated up and thermally expanded, which can reduce the gap with the bottom surface of the cooling tube and facilitate heat conduction to the cooling tube. In addition, the portion of the cooling auxiliary tube that covers the bottom surface of the cooling tube is heated up by being subjected to more radiant heat from the raw material melt and the heater, and the radiant heat emitted by the cooling auxiliary tube itself toward the bottom surface of the cooling tube becomes larger. Therefore, even if there is a slight gap between the bottom surface of the cooling tube, heat can be further conducted to the cooling tube. Of course, it is preferred that the cooling auxiliary tube cover 100% of the bottom surface of the cooling tube, such as Figure 1 and Figure 2 As shown, the flange 30 may also extend beyond the outer diameter of the bottom surface of the cooling cylinder to the outside.
[0067] As described above, the single crystal manufacturing device of the present invention has a forced cooling cylinder and a cooling auxiliary cylinder made of a specific material embedded in the cooling cylinder, and the cooling auxiliary cylinder has a structure that covers the bottom surface of the cooling cylinder facing the raw material melt, so that the radiation heat from the single crystal and the radiation heat from the high temperature parts such as the heater can be efficiently conducted to the cooling cylinder. As a result, the temperature gradient in the growing single crystal can be increased, and the growth rate of the single crystal can be accelerated.
[0068] Furthermore, when a single crystal is actually manufactured using the single crystal manufacturing apparatus of the present invention, the single crystal can be manufactured by, for example, applying a magnetic field to the raw material melt according to the specifications of the single crystal to be manufactured.
[0069] Example
[0070] Hereinafter, the present invention will be described in detail with reference to Examples, but the present invention is not limited thereto.
[0071] In Examples 1 to 3 and Comparative Example, a single crystal silicon having a diameter of 300 mm was produced by a magnetic field application Czochralski method (MCZ method) using a single crystal production apparatus described below. At this time, the diameter of the quartz crucible 4 was 800 mm.
[0072] (Example 1)
[0073] use Figure 1 The single crystal manufacturing apparatus 1 shown in the figure manufactures single crystals. The cooling auxiliary cylinder 17 used has a structure that covers the bottom surface of the cooling cylinder 15 facing the raw material melt 6. Figure 2As shown, the gap 20 between the bottom surface of the cooling cylinder 15 facing the raw material melt 6 and the upper surface of the flange 30 of the cooling auxiliary cylinder 17, which is a structure covering the bottom surface of the cooling cylinder 15 facing the raw material melt 6, is prepared in six levels of 0 mm (complete contact), 0.1 mm, 0.2 mm, 0.5 mm, 0.8 mm, and 1.0 mm, and the area of the bottom surface of the cooling cylinder 15 facing the raw material melt 6 covered by the flange 30 of the cooling auxiliary cylinder 17 is set to 100% of the bottom surface of the cooling cylinder 15 facing the raw material melt 6. In addition, the material of the cooling auxiliary cylinder 17 is a graphite material having a thermal conductivity equal to or higher than that of metal and a higher emissivity than that of metal.
[0074] Single crystals 7 are grown using such a single crystal manufacturing apparatus 1, and the growth rate at which all of them are defect-free is determined. The boundary of the growth rate required to obtain defect-free crystals is very narrow, so it is easy to determine the appropriate growth rate. For evaluating whether a single crystal has defects, a sample is cut out from the produced single crystal, and whether it is a defect-free crystal is evaluated by selective etching.
[0075] (Comparative Example)
[0076] A single crystal was manufactured using the same apparatus as the single crystal manufacturing apparatus 1 described in Example 1, except that the gap 20 between the bottom surface of the cooling cylinder 15 facing the raw material melt 6 and the upper surface of the flange 30 of the cooling auxiliary cylinder 17, which is a structure covering the bottom surface of the cooling cylinder 15 facing the raw material melt 6, was changed to three levels of 1.1 mm, 1.2 mm, and 1.5 mm. Regarding the conditions other than these, single crystals were manufactured in the same manner as the conditions described in Example 1.
[0077] exist Figure 3 The results of Example 1 and the comparative example are shown in FIG. 1. In Example 1 using the single crystal manufacturing apparatus of the present invention, a growth rate of about 16.7% was achieved when the gap between the bottom surface of the cooling cylinder and the cooling auxiliary cylinder was 0 mm (complete contact), compared with a case where a conventional single crystal manufacturing apparatus was used, wherein the conventional single crystal manufacturing apparatus had a cooling auxiliary cylinder, and the cooling auxiliary cylinder was Figure 7 As shown in the figure, there is no structure to cover the bottom surface of the cooling cylinder facing the raw material melt. Figure 3It can be confirmed that if the gap between the bottom surface of the cooling cylinder and the cooling auxiliary cylinder is less than 1.0 mm, the growth rate of the single crystal can be significantly increased by covering the bottom surface of the cooling cylinder with the cooling auxiliary cylinder. On the other hand, in the single crystal manufacturing device used in the comparative example, if the gap between the bottom surface of the cooling cylinder and the cooling auxiliary cylinder is more than 1.1 mm, not only the radiant heat from the single crystal cannot be efficiently removed, but also the radiant heat from the high temperature parts such as the heater cannot be efficiently removed. It can be seen that even in the case of a gap of 1.1 mm, the high-speed rate is about 1.4%, and compared with the existing single crystal manufacturing device, it is not possible to achieve a significant increase in the growth rate of the single crystal.
[0078] In this way, the single crystal manufacturing device of the present invention can not only efficiently remove the radiant heat from the single crystal, but also efficiently remove the radiant heat from the high temperature parts such as the heater, and can significantly increase the growth rate of the single crystal. In addition, if the gap between the bottom surface of the cooling cylinder and the cooling auxiliary cylinder is less than 1.0 mm, it can help to increase the growth rate of the single crystal.
[0079] (Example 2)
[0080] As another method relative to Example 1, using Figure 4 The single crystal manufacturing apparatus 100 shown in FIG. 1 performs single crystal manufacturing. Figure 5 As shown in FIG. 1 , nine levels of 100%, 90%, 80%, 70%, 60%, 50%, 40%, 30%, and 20% of the bottom surface of the cooling cylinder 15 facing the raw material melt 6, which was covered by the flange 130 of the cooling auxiliary cylinder 117, were prepared, and the single crystal 7 was manufactured under the same manufacturing conditions as in Example 1, and the same evaluation as in Example 1 was performed. In addition, at this time, the gap 120 between the bottom surface of the cooling cylinder 15 facing the raw material melt 6 and the upper surface of the flange 130 of the cooling auxiliary cylinder 117, which is the structure covering the bottom surface of the cooling cylinder 15 facing the raw material melt 6, was set to 0.1 mm.
[0081] exist Figure 6 The results of Example 2 are shown in FIG. 1 . It was found that compared with the case where the conventional single crystal manufacturing apparatus was used, Figure 6 It can be seen that if the bottom surface of the cooling cylinder covered by the cooling auxiliary cylinder accounts for more than 50% of the entire area, the growth rate of the single crystal can be significantly increased by covering the bottom surface of the cooling cylinder with the cooling auxiliary cylinder. Figure 7 As shown in the figure, the bottom surface of the cooling cylinder facing the raw material melt is not covered. In addition, when the area of the cooling cylinder bottom surface covered by the cooling auxiliary cylinder is 100%, a growth rate of about 13.4% is achieved.
[0082] In this way, it can be confirmed that, with respect to the single crystal manufacturing device of the present invention, the larger the area of the bottom surface of the cooling cylinder covered by the cooling auxiliary cylinder facing the raw material melt, the more heat can be conducted to the cooling cylinder, which can not only remove more radiant heat from the single crystal, but also remove more radiant heat from high-temperature parts such as heaters, thereby achieving a further increase in the growth rate of the single crystal.
[0083] (Example 3)
[0084] As another method relative to Example 2, the same device as the single crystal manufacturing device described in Example 2 is used, and the gap between the bottom surface of the cooling cylinder facing the raw material melt and the upper surface of the flange of the cooling auxiliary cylinder, which is a structure covering the bottom surface of the cooling cylinder facing the raw material melt, is set to 0 mm (complete contact). In addition, as in Example 2, nine levels of areas of the bottom surface of the cooling cylinder facing the raw material melt covered by the flange of the cooling auxiliary cylinder are prepared, namely, 100%, 90%, 80%, 70%, 60%, 50%, 40%, 30%, and 20% of the bottom surface of the cooling cylinder facing the raw material melt, and crystal manufacturing is carried out.
[0085] exist Figure 6 The results of Example 3 are shown in . Compared with the case where the gap between the bottom surface of the cooling cylinder facing the raw material melt and the upper surface of the flange of the cooling auxiliary cylinder, which is a structure covering the bottom surface of the cooling cylinder facing the raw material melt, is 0.1 mm in Example 2, in Example 3, since the gap is completely in contact with the upper surface of the flange of the cooling auxiliary cylinder, which is a structure covering the bottom surface of the cooling cylinder facing the raw material melt, the growth rate is high. In addition, in Example 3 where the gap between the bottom surface of the cooling cylinder facing the raw material melt and the upper surface of the flange of the cooling auxiliary cylinder, which is a structure covering the bottom surface of the cooling cylinder facing the raw material melt, is 0 mm (complete contact), even when the area of the bottom surface of the cooling cylinder facing the raw material melt covered by the flange of the cooling auxiliary cylinder is 40% of the bottom surface of the cooling cylinder facing the raw material melt, a growth rate of 5.6% can be achieved. Therefore, if the gap between the bottom surface of the cooling cylinder facing the raw material melt and the upper surface of the flange of the cooling auxiliary cylinder, which is a structure covering the bottom surface of the cooling cylinder facing the raw material melt, is 0 mm (complete contact), then even if the area of the bottom surface of the cooling cylinder facing the raw material melt covered by the flange of the cooling auxiliary cylinder is less than 50% of the bottom surface of the cooling cylinder facing the raw material melt, it can help to increase the growth rate.
[0086] As described above, as in Example 1 of the present invention, according to the single crystal manufacturing device of the present invention, it is not only possible to efficiently remove the radiant heat from the single crystal, but also possible to efficiently remove the radiant heat from the high temperature parts such as the heater, and it is possible to significantly increase the growth rate of the single crystal compared to the existing single crystal manufacturing device, wherein the material of the cooling auxiliary cylinder of the single crystal manufacturing device of the present invention is composed of a specific material, the cooling auxiliary cylinder has a structure that covers the bottom surface of the cooling cylinder facing the raw material melt, and the gap between the cooling auxiliary cylinder and the bottom surface of the cooling cylinder is 1.0 mm or less. In addition, according to Example 2 and Example 3, with respect to the cooling auxiliary cylinder, it is more preferred that at least 50% of the entire area of the bottom surface of the cooling cylinder facing the raw material melt is covered by the cooling auxiliary cylinder.
[0087] The present invention is not limited to the above-described embodiments. The above-described embodiments are illustrative, and any scheme having substantially the same structure and achieving the same function and effect as the technical concept described in the claims of the present invention is included in the technical scope of the present invention.
Claims
1. A single crystal manufacturing device, which grows a single crystal using the Czochralski method, comprising: a main chamber, which accommodates a crucible for storing a raw material melt and a heater for heating the raw material melt; a pulling chamber, which is connected to the upper part of the main chamber, and the growing single crystal is pulled and stored in the pulling chamber; a cooling cylinder, which extends from at least the top of the main chamber to the raw material melt in a manner of surrounding the single crystal being pulled and is forcibly cooled by a cooling medium; and a cooling auxiliary cylinder, which is embedded in the cooling cylinder, characterized in that The cooling auxiliary cylinder is made of any one or more of graphite material, carbon composite material, stainless steel, molybdenum, and tungsten. The auxiliary cooling cylinder has a flange that protrudes from the inside to the outside of the cooling cylinder to cover the bottom surface of the cooling cylinder facing the raw material melt, and a gap between the flange of the auxiliary cooling cylinder and the bottom surface of the cooling cylinder is 1.0 mm or less.
2. The single crystal manufacturing device according to claim 1, characterized in that: Regarding the bottom surface of the cooling cylinder, at least 50% of the entire area of the bottom surface is covered by the auxiliary cooling cylinder.
3. The single crystal manufacturing device according to claim 1, characterized in that: The single crystal manufacturing apparatus further includes a heat insulating member extending from the ceiling of the main chamber and surrounding the bottom surface of the cooling cylinder and the flange of the auxiliary cooling cylinder.
4. The single crystal manufacturing device according to any one of claims 1 to 3, characterized in that: A gap between the flange of the auxiliary cooling cylinder and the bottom surface of the cooling cylinder is not less than 0.1 mm and not more than 1.0 mm.