A method for preparing a multi-threshold stacked nanosheet GAA-FET device array

By using different polarity stacked HK covering and annealing technologies in the GAA-FET device array to change the Si-O polarity intensity, the difficulty in threshold control caused by uneven filling of multi-layer HKMG films in the traditional method is solved, and multi-thresholds are achieved Effective control and current driving performance improvement.

CN115172168BActive Publication Date: 2024-10-01INST OF MICROELECTRONICS CHINESE ACAD OF SCI LTD +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202210810604.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-11
Publication Date
2024-10-01
Estimated Expiration
2042-07-11

AI Technical Summary

Technical Problem

Traditional multi-layer HKMG films are difficult to fill uniformly in stacked nanosheet GAA-FET devices, making it difficult to accurately control the device threshold. In particular, it is challenging to realize multi-threshold integration of CMOS devices under space constraints.

Method used

By using different polarity stacked HK covering and annealing in the GAA-FET device array, the Si-O polarity intensity in the IL is changed and the covering layer is removed to achieve different device thresholds without increasing the overall thickness of the multi-layer HKMG. Based on multi-threshold control.

Benefits of technology

It achieves effective control of multiple thresholds in the GAA-FET device array, avoids the difficulty of thickness change due to space limitations in traditional methods, and improves the current driving performance and gate control capabilities of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115172168B_ABST
    Figure CN115172168B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for preparing a multi-threshold stacked nanosheet GAA-FET device array, wherein the formation process of a high-k dielectric layer in a device wraparound gate is as follows: first, after interface oxidation, a non-polar high-k dielectric layer is deposited to cover, then a first-type polar high-k dielectric layer is deposited to cover, annealed, and then removed in part of the device array by an etching process, so as to subsequently form the first-type device threshold; then a second-type polar high-k dielectric is deposited to cover, annealed, and then removed in part of the device array by an etching process to form the second-type device threshold, and more device thresholds are obtained by combining different coverage areas. The present invention changes the Si-O polarity strength in the interface oxide layer by covering with stacked high-k dielectric layers of different polarities in the integrated manufacturing of the GAA-FET device array, so as to realize a manufacturing method for different device thresholds.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductors, and in particular to a method for preparing a multi-threshold stacked nanosheet GAA-FET device array. Background Art

[0002] As transistor feature sizes continue to shrink, traditional MOSFET devices have undergone a transition from planar structures to three-dimensional structures, improving device performance while reducing the impact of short channel effects. The current mainstream three-dimensional structure transistor is FinFET. However, FinFET faces huge challenges in the technology generation below 5nm. In the latest International Roadmap for Devices and Systems (IRDS), Nanosheet-GAAFET is a key device that can effectively replace FinFET after the 3nm node, and can significantly suppress the short channel effect and improve the current driving performance of the device.

[0003] At present, the research progress of GAA stacked nanosheet FET has attracted wide attention from academia and industry. The constantly updated preparation process and key processes, as well as the optimized device structure are the hot research directions of new CMOS devices.

[0004] GAA stacked nanosheet FET is a new device developed on the basis of FinFET and Nanowire-FET, with a ring gate structure and horizontal nanosheet (NS) as a conductive channel. In terms of gate control, the ring gate structure has better gate control capability than the FinFET device structure, which can effectively suppress the short channel effect of the device; in terms of current drive, Nanosheet-GAAFET has an effective gate adjustable and vertical and horizontal stacking design, which can also significantly enhance the current drive performance of the device.

[0005] However, in the current HKMG manufacturing process of conventional stacked nanosheet GAA-FET, due to the influence of many factors such as narrow gate length, upper and lower spacing of nanosheets, nanosheet width, pitch, etc., the traditional multi-layer HKMG film is difficult to fill or fills unevenly on the stacked nanosheet channel, resulting in difficulty in accurately controlling the device threshold. Especially in GAA-FET, using conventional methods, due to the space limitation between stacked nanosheets, it will face great challenges to realize the multi-threshold integration of CMOS (NMOS / PMOS) by changing the thickness of the work function metal layer (WFL) or other metal gate film layers in HKMG. Summary of the invention

[0006] In view of the above technical problems, the present invention proposes a method for preparing a multi-threshold stacked nanosheet GAA-FET device array, in which different polarity stacked layers HK are covered and annealed to change the Si-O polarity strength in the IL in the integrated manufacturing of the GAA-FET device array, and then the covering layer is removed to achieve different device thresholds.

[0007] The present invention adopts the following technical solutions:

[0008] A method for preparing a multi-threshold stacked nanosheet GAA-FET device array, characterized in that it comprises the following steps:

[0009] providing a substrate;

[0010] epitaxially growing a superlattice stack of alternately stacked first semiconductors and second semiconductors on the substrate;

[0011] Etching the superlattice stack to form a plurality of fins;

[0012] forming a dummy gate on the fin and etching the fin;

[0013] Selectively etching the superlattice stack of the first semiconductor and the second semiconductor on the fin to form a nanosheet stack portion, and etching away a portion of the nanosheet formed by the first semiconductor in the superlattice stack from the outside to the inside;

[0014] Selecting an epitaxial growth process to form source and drain regions;

[0015] Dielectric deposition and planarization to expose the dummy gate;

[0016] Achieving channel release of nanosheets, wherein the stack of nanosheets forms a plurality of conductive channels;

[0017] A wraparound gate is formed, wrapping around the nano stack portion; wherein the high-k dielectric layer in the wraparound gate of the device is formed by: firstly, a non-polar high-k dielectric layer is deposited to cover the interface after oxidation, and then a first type of polar high-k dielectric layer is deposited to cover, annealing is performed, and then it is removed in part of the device array through an etching process, so as to subsequently form a first type of device threshold; then a second type of polar high-k dielectric is deposited to cover, annealing is performed, and then it is removed in part of the device array through an etching process, so as to form a second type of device threshold, and thereby more device thresholds are obtained through different combinations of coverage areas.

[0018] The technical solution of the present invention ensures effective regulation of multiple thresholds in a GAA-FET device array device without increasing the overall thickness of the multi-layer HKMG. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] By reading the detailed description of the preferred embodiment below, various other advantages and benefits will become clear to those of ordinary skill in the art. The accompanying drawings are only used for the purpose of illustrating the preferred embodiment and are not considered to be limitations of the present invention. In addition, the same reference symbols are used to represent the same components throughout the accompanying drawings.

[0020] Figure 1 It is a schematic diagram of growing a superlattice stack on a substrate according to the present invention.

[0021] Figure 2 The diagram is a schematic diagram of forming a first sidewall on a superlattice stack according to the present invention.

[0022] Figure 3 Schematic diagram of etching a superlattice stack to form fins according to the present invention.

[0023] Figure 4 The schematic longitudinal cross-sectional view of the present invention is a schematic diagram of removing the first sidewall to form a shallow trench isolation region along a direction perpendicular to the fin line.

[0024] Figure 5 The figure is a schematic longitudinal cross-sectional view of forming a dummy gate on a fin according to the present invention along a direction perpendicular to the fin line.

[0025] Figure 6 These are the XX and YY directions defined in the device of the present invention.

[0026] Figure 7 It is a cross-sectional schematic diagram along line XX, where a second sidewall spacer is formed on both sides of the dummy gate and source and drain etching is performed.

[0027] Figure 8 It is a cross-sectional schematic diagram of etching away a portion of the first semiconductor layer from the outside to the inside, further depositing the second sidewall, and etching the outer second sidewall along the XX line of the present invention.

[0028] Fig. 9 It is a cross-sectional schematic diagram of depositing source and drain regions, doping source and drain regions, and depositing an isolation layer according to the present invention.

[0029] Fig.10 This is a cross-sectional schematic diagram along line XX of the present invention for removing the dummy gate, releasing the nanochannel, and depositing the interface oxide layer.

[0030] Fig.11 Schematic diagram of the formation of a multi-threshold high-K dielectric layer.

[0031] Fig.12 It is a cross-sectional schematic diagram of forming a metal gate and depositing a dielectric CMP layer in the present invention.

[0032] Fig.13 The cross-sectional schematic diagram of the multi-threshold stacked nanosheet GAA-FET device array finally formed by photolithography and etching of contact holes in the present invention. DETAILED DESCRIPTION

[0033] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. However, it should be understood that these descriptions are exemplary only and are not intended to limit the scope of the present invention. In addition, in the following description, descriptions of known structures and technologies are omitted to avoid unnecessary confusion of the concept of the present invention.

[0034] Various structural schematic diagrams according to embodiments of the present invention are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified and some details may be omitted for the purpose of clear expression. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships therebetween are only exemplary, and may deviate in practice due to manufacturing tolerances or technical limitations, and those skilled in the art may additionally design regions / layers with different shapes, sizes, and relative positions according to actual needs.

[0035] In the context of the present invention, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element or an intervening layer / element may exist between them. In addition, if a layer / element is "on" another layer / element in one orientation, the layer / element may be "under" the other layer / element when the orientation is reversed.

[0036] In this embodiment, a method for manufacturing a semiconductor device array is provided. For the convenience of illustration, the following diagram illustrates a method for manufacturing a device array using a method for manufacturing a device. Figure 1-13 FIG. 1 is a schematic diagram of a process for preparing a FET device array of the present invention. The process for preparing a FET device array includes:

[0037] like Figure 1 As described above, a substrate 101 is provided, which may be bulk silicon.

[0038] The substrate 101 is a part of a semiconductor wafer suitable for forming one or more IC devices. When a bulk silicon substrate is used, a highly doped well region is formed in the bulk silicon substrate by injecting impurities, diffusing, and annealing to achieve the desired well depth. For a P-type FET, the highly doped well region is an N-well, and the injected impurities are n-type impurity ions, such as phosphorus (P) ions; for an N-type FET, the highly doped well region is a p-well, and the injected impurities are p-type impurity ions, such as boron (B) ions. In the process of superlattice stack epitaxy, the SiGe thickness and the Si thickness are respectively regulated, and the Ge content is regulated to form a multi-component SiGe conductive channel.

[0039] Silicon dioxide (SiO2) on the surface of the bulk silicon substrate is removed, and multiple periods of a first semiconductor 201' / second semiconductor 202' superlattice structure stack are epitaxially grown on the bulk silicon substrate; the thickness of each semiconductor layer in the superlattice structure is less than 30 nanometers, and the final thickness produced will directly determine the height of the nanosheet channel and the electrostatic performance.

[0040] For P-type FET, the first semiconductor 201 ′ / second semiconductor 202 ′ superlattice is a Si / SiGe stack, and for N-type FET, the first semiconductor 201 ′ / second semiconductor 202 ′ superlattice is a SiGe / Si stack.

[0041] like Figure 2 The self-aligned spacer transfer (SIT) process is used to form a nanoscale first spacer 301 device array, and the first spacer 301 is silicon nitride (SiN X The specific formation process is as follows: a sacrificial layer 302 is covered on the superlattice stack, and the sacrificial layer can be polysilicon (PolySi, p-si) or amorphous silicon (a-si), and a part of the sacrificial layer is etched away to deposit silicon nitride (SiN x ) layer, and then anisotropic etching is used to etch away the remaining sacrificial layer, so that only multiple periodic silicon nitride (SiN x ) first spacers 301, the silicon nitride (SiN x ) The first sidewall spacer 301 acts as a hard mask in photolithography.

[0042] The epitaxially grown superlattice stack is made into multiple periodically distributed fins by etching. The first sidewall 301 is used as a mask for etching to form a fin with a superlattice stack structure. The upper part of the fin is a conductive channel area formed by the superlattice stack, and the lower part is a substrate, forming a Figure 3 The fin shown. The fin includes not only a superlattice stacked structure, but also a single crystal silicon structure that penetrates into the substrate. The etching process is dry etching or wet etching, and in one embodiment, reactive ion etching (RIE) can be used. The fin will be used to form one or more horizontal nanosheets of n-type field effect transistors and / or p-type field effect transistors. Although Figure 3 One fin is shown, and it should be understood that any suitable number and configuration of fins may be used. The height of the fin is about 10 nm-400 nm, and the width is about 1-100 nm.

[0043] like Figure 4As shown, a shallow trench isolation (STI) region 103 is formed between two adjacent fins. First, a dielectric insulating material is deposited and then planarized, for example, using a CMP process, and then the dielectric insulating material is selectively etched back to expose a three-dimensional fin structure, thereby forming a shallow trench isolation region 103 adjacent to the fin. The upper surface of the shallow trench isolation region 103 is generally flush with the interface between the superlattice stacked structure in the fin and the substrate single crystal silicon, and may be higher or lower than the interface level. The shallow trench isolation region 103 can be formed of a suitable dielectric material, such as silicon dioxide (SiO2), silicon nitride (SiN x ) etc. The shallow trench isolation region 103 is used to separate transistors on adjacent fins. The shallow trench isolation region 103 exposes the bottommost first semiconductor layer 201' of the superlattice stack.

[0044] like Figure 5 As shown, a dummy gate stack is formed on the exposed fin in a direction perpendicular to the fin line (i.e., the YY direction). The dummy gate stack is a multi-layer structure, including a gate insulating dielectric (not shown), a dummy gate layer 106 and a hard mask layer 108. The dummy gate stack structure can be formed by processes such as thermal oxidation, chemical vapor deposition, and sputtering. The dummy gate stack structure spans the superlattice stack on the top of the fin, and multiple dummy gates are periodically distributed along the fin line direction. The material used for the dummy gate layer 106 can be polysilicon (PolySi, p-si) or amorphous silicon (a-si). The material used for the hard mask layer 108 can be oxide, carbide, carbide, organic matter, etc.

[0045] like Figure 6 The direction is defined in Figure 6 Two dotted lines XX and YY are set in the figure. The XX line is the center line of the fin along the fin line direction, and the YY line is the center line of the fin perpendicular to the fin line direction. The subsequent drawings are all cross-sectional schematic diagrams based on the XX and YY lines.

[0046] Figure 7 As shown, silicon nitride (SiN) is disposed on both sides of the dummy gate stack and along the fin line direction (ie, XX direction). x ) The second spacers 107 are formed on both sides of the fin, and the second spacers 107 have the same thickness. Then, the dummy gate layer 106, the hard mask 108, and the second spacers 107 are used as masks to perform source and drain etching on the fins through an etching process.

[0047] Then, if Figure 8 As shown, pull-back etching is performed to etch away a portion of the first semiconductor layer 201' from the source and drain regions toward the center. Then, silicon nitride (SiN) is deposited on the periphery of the fin. x) The third sidewall spacer 107' is etched until it is flush with the second semiconductor layer 202' in the vertical direction. The missing portion of the first semiconductor layer 201' caused by the pull-back etching is replaced by the silicon nitride (SiN) of the third sidewall spacer 107'. x )Fill up.

[0048] like Fig. 9 As shown, for a P-type FET, the source and drain region material is boron (B) doped SiGe (SiGe:B), and for an N-type FET, the source and drain region material is phosphorus (P) doped silicon (Si) (Si:P), and finally the source and drain region 110 is formed.

[0049] Then, an isolation layer 111 is deposited on the surface of the dummy gate and the source and drain regions 110 to prevent interconnection short circuit between the dummy gate layer 106 and the source and drain regions 110 in subsequent steps, and the isolation layer 111 is chemically mechanically polished to make it flat, and the hard mask layer 108 is removed to expose the dummy gate layer 106.

[0050] Then, if Fig.10 As shown, the dummy gate layer 106 formed of the aforementioned polysilicon (PolySi, p-si) or amorphous silicon (a-si) is etched or corroded by a selective etching or corrosion process, that is, the dummy gate layer 106 is removed.

[0051] Subsequently, the sacrificial layer in the superlattice stack is selectively etched to release the nanosheet channel. The conductive channel region exposed by the fin is processed to remove each first semiconductor layer 201', which is the sacrificial layer, and release the nanosheet 202 formed by the second semiconductor. The nanosheet 202 has a width range of 1-100nm, a thickness range of 1-30nm, and a spacing range of 3-30nm between each nanosheet 202.

[0052] In one embodiment, for both P-type and N-type FETs, the sacrificial layer is a GeSi layer, the GeSi layer is selectively removed, and the Si layer is retained to form a Si horizontal stack nano stack device. In the selective removal process, an etchant that selectively etches SiGe at a faster rate than Si can be used. In one embodiment, a conventional wet process is used to isotropically etch the sacrificial layer to release the nano channel, thereby forming a nano sheet conductive channel.

[0053] In another embodiment, channel release is performed separately for P-type and N-type FETs.

[0054] For a P-type FET, the sacrificial layer is a Si layer, the Si layer is selectively removed, and the SiGe layer is retained to form a SiGe horizontal stack nano stack device. In the selective removal process, an etchant that selectively etches Si at a faster rate than SiGe can be used. In one embodiment, a conventional wet process is used to isotropically etch the sacrificial layer to release the nano channel, thereby forming a nanosheet conductive channel.

[0055] For N-type FET, the sacrificial layer is a SiGe layer, the SiGe layer is selectively removed, and the Si layer is retained to form a Si horizontal stacked nano stack device. In the selective removal process, an etchant that selectively etches SiGe at a faster rate than Si can be used. In one embodiment, a conventional wet process is used to isotropically etch the sacrificial layer to release the nano channel, thereby forming a nano sheet conductive channel. The second semiconductor nano layer sheet 202 is stacked to form a nano stack portion.

[0056] Then, if Fig.11 As shown, an interface oxide layer (IL, not shown) is deposited or grown, and then a high-k dielectric layer is deposited to cover the surface of the nano stack portion such that the high-k dielectric layer surrounds the surface of the nano stack portion. The details are as follows: first, a non-polar high-k dielectric layer 115-1 is deposited, and the non-polar high-k dielectric layer 115-1 does not form a dipole control in the IL layer, and forms a standard threshold; then, some devices are selected from them to continue to deposit a first polarity high-k dielectric layer 115-2, and then an annealing process is performed, and then the first polarity high-k dielectric layer 115-2 is removed by an etching process, so that a strong dipole control is formed in the IL layer, and a first type of low threshold is formed. In one embodiment, the first type of low threshold is the lowest threshold; then, some devices are selected from the above-mentioned devices on which the first polarity high-k dielectric layer 115-2 is deposited, and then an annealing process is performed, and then the second polarity high-k dielectric layer 115-3 is removed by an etching process, and the second polarity high-k dielectric layer 115-3 forms a sub-medium dipole control in the IL layer, and forms a first type of low threshold. In one embodiment, the second type of low threshold is a sub-low threshold.

[0057] The Si-O polarity strength in the IL is changed by covering and annealing with different polarity stacked layers HK, and then the covering layer is removed to achieve different device thresholds. The high-k dielectric layer may have a dielectric constant higher than about 6.0. In one embodiment, the first polarity high-k dielectric layer in NMOS may be one or a combination of LaOx, MgOx, ScOx, YOx, and NdOx, and the second polarity high-k dielectric layer may be one or a combination of AlOx, MnOx, ZrOx, TiOx, and MoOx; and in PMOS, the first polarity high-k dielectric layer and the second polarity high-k dielectric layer are opposite to those in NMOS. The annealing temperature range is 200°C to 1000°C.

[0058] A manufacturing method in which the first and second polar high-k dielectric materials are exchanged, the first-type regulation threshold is a maximum threshold (absolute value) compared to a standard threshold without polarity coverage, and the second-type regulation threshold is a second-largest threshold (absolute value).

[0059] Next, a metal gate is deposited outside the space formed by the dummy gate 106 and the high-k dielectric layer to form a multi-layer high-k / metal gate structure. The metal gate includes a capping layer, a barrier layer, a work function layer, and a filling layer. Film structures with different effective work functions can be formed by selective photolithography and etching to adjust the device threshold. Generally, chemical vapor deposition, physical vapor deposition and other processes are used to form a metal gate. The metal gate material is TaC, TiN, TaTbN, TaErN, TaYbN, TaSiN, HfSiN, MoSiN, RuTa x 、NiTa x ,MoN x , TiSiN, TiCN, TaAlC, TiAlN, TaN, PtSi x , Ni3Si, Pt, Ru, Ir, Mo, Ti, Al, Cr, Au, Cu, Ag, HfRu or RuO x One or a combination of Fig.11 As shown in the figure, the metal gate fills the space after the dummy gate layer 106 is removed. Then, the multi-layer high-k / metal gate structure is chemically mechanically polished to make it flat, and the excess multi-layer high-k / metal gate material exposed on the surface of the dielectric layer outside the dummy gate space is removed to form a high-k dielectric layer and a metal gate 113, wherein the two are filled in the space of the original first semiconductor layer 201' to form a ring gate structure.

[0060] Next, an ILD-1 dielectric is deposited on the top to form a dielectric CMP layer 112 , contact hole photolithography and etching are performed on the dielectric CMP layer 112 , hole silicide 114 is deposited, and contact electrodes are drawn out.

[0061] Subsequently, multi-layer back-end interconnection and passivation protection processes are completed.

[0062] The above is the process flow for preparing a complete semiconductor device, forming a Fig.11 FET device shown.

[0063] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:

[0064] The technical solution of the present invention ensures effective regulation of multiple thresholds in a GAA-FET device array device without increasing the overall thickness of the multi-layer HKMG.

[0065] In the above description, the technical details of the patterning and etching of each layer are not described in detail. However, those skilled in the art should understand that various technical means can be used to form layers, regions, etc. of desired shapes. In addition, in order to form the same structure, those skilled in the art can also design methods that are not completely the same as the methods described above. In addition, although the various embodiments are described above separately, this does not mean that the measures in the various embodiments cannot be used in combination to advantage.

[0066] The embodiments of the present invention are described above. However, these embodiments are only for illustrative purposes and are not intended to limit the scope of the present invention. The scope of the present invention is defined by the appended claims and their equivalents. Without departing from the scope of the present invention, those skilled in the art may make various substitutions and modifications, which should all fall within the scope of the present invention.

Claims

1. A method for preparing a multi-threshold stacked nanosheet GAA-FET device array, characterized in that: The steps include: providing a substrate; epitaxially growing a superlattice stack of alternately stacked first semiconductors and second semiconductors on the substrate; Etching the superlattice stack to form a plurality of fins; forming a dummy gate on the fin and etching the fin; Selectively etching the superlattice stack of the first semiconductor and the second semiconductor on the fin to form a nanosheet stack portion, and etching away a portion of the nanosheet formed by the first semiconductor in the superlattice stack from the outside to the inside; Selecting an epitaxial growth process to form source and drain regions; Dielectric deposition and planarization to expose the dummy gate; Achieving channel release of nanosheets, wherein the stack of nanosheets forms a plurality of conductive channels; A wraparound gate is formed, wrapping around the nano stack portion; wherein the high-k dielectric layer in the wraparound gate of the device is formed by: firstly, depositing a non-polar high-k dielectric layer to cover the interface after oxidation, then depositing a first-type polar high-k dielectric layer to cover, annealing, and then removing it in part of the device array through an etching process, so as to subsequently form a first-type device threshold; then depositing a second-type polar high-k dielectric to cover, annealing, and then removing it in part of the device array through an etching process, so as to form a second-type device threshold, and thereby obtaining more device thresholds through different coverage area combinations; In NMOS, the first type of polar high-k dielectric is one or a combination of LaOx, MgOx, ScOx, YOx or NdOx, and the second type of polar high-k dielectric is one or a combination of AlOx, MnOx, ZrOx, TiOx, and MoOx; for PMOS, the first type of polar high-k dielectric is one or a combination of AlOx, MnOx, ZrOx, TiOx or MoOx, and the second type of polar high-k dielectric is one or a combination of LaOx, MgOx, ScOx, YOx or NdOx.

2. The method according to claim 1, characterized in that: The step of forming the plurality of fins is specifically as follows: providing a first sidewall on the superlattice stack; and etching the superlattice stack using the first sidewall as a mask to form the plurality of fins.

3. The method according to claim 2, characterized in that: The method also includes forming a shallow trench isolation region, specifically, generating a shallow trench isolation region between adjacent fins, so that the plurality of conductive channels are located above the shallow trench isolation region.

4. The method according to claim 3, characterized in that: The method also includes forming source and drain regions, specifically, etching away the fin structure between adjacent dummy gates to form source and drain growth space; epitaxially growing the source and drain regions in the growth space, and depositing an isolation layer on the source and drain regions.

5. The method according to claim 4, characterized in that: The steps of forming the wraparound gate are as follows: after forming the source and drain regions, selectively etching to remove the dummy gate, and after releasing the nanosheet channel, depositing the gate at the original dummy gate position.

6. The method according to claim 1, characterized in that: The threshold of the first type of device is the smallest threshold compared to the threshold of the device that is not finally covered by polarity, and the threshold of the second type of device is the second smallest threshold.

7. The method according to claim 1, characterized in that: The first semiconductor is SiGe and the second semiconductor is Si, or the first semiconductor is Si and the second semiconductor is SiGe.

8. The method according to claim 1, characterized in that: The wraparound gate includes an interface oxide layer, a high-K dielectric layer and a metal gate in sequence from the outside to the inside.

9. The method according to claim 1, characterized in that: The annealing temperature ranges from 200°C to 1000°C.

Citation Information

Patent Citations

  • Preparation method of semiconductor device and semiconductor device

    CN113178488A

  • Stacked nanosheet ring gate CMOS (complementary metal oxide semiconductor) device and preparation method thereof

    CN114551357A

  • Protection of high-k dielectric during reliability anneal on nanosheet structures

    US20170323949A1

  • Gate structures for semiconductor devices

    US20210134951A1

  • Semiconductor Devices Having Gate Dielectric Layers of Varying Thicknesses and Methods of Forming the Same

    US20210225839A1