A hybrid waveguide integrated two-dimensional material mid-infrared photodetector

Through the hybrid waveguide structure of sapphire-silica-sulfur material-two-dimensional material system, the problems of high growth cost and lattice mismatch of traditional mid-infrared photodetector materials are solved, and high responsiveness and high signal-to-noise ratio are achieved Infrared photoelectric detection supports low loss transmission and efficient detection in the 3-5μm band.

CN115224134BActive Publication Date: 2024-11-19ZHEJIANG UNIV
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202210792791.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-05
Publication Date
2024-11-19
Estimated Expiration
2042-07-05

AI Technical Summary

Technical Problem

Traditional mid-infrared photodetector materials have high growth costs and lattice mismatch problems, which limits their wide application and promotion, especially when integrating with other photonic devices.

Method used

The hybrid waveguide structure adopts a sapphire-silica-sulfur material-two-dimensional material system, and realizes a high-response detector through the strong interaction between the two-dimensional material and TE0 mode light, and utilizes the advantages of waveguide integration to achieve ultra-high bandwidth detection and High signal-to-noise ratio.

Benefits of technology

It realizes low loss transmission and high responsiveness detection in the mid-infrared band at room temperature, improves the signal-to-noise ratio and bandwidth of the detector, supports low loss transmission of signal light in the 3-5μm band, and the intensity of two-dimensional materials and light field are mutually connected. The effect enhances the detection performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115224134B_ABST
    Figure CN115224134B_ABST
Patent Text Reader

Abstract

The present invention discloses a hybrid waveguide integrated two-dimensional material mid-infrared photodetector. It includes a sapphire substrate; a silicon waveguide transmission layer is formed on the sapphire substrate; a two-dimensional material layer is located on the middle of the silicon waveguide transmission layer; a chalcogenide strip waveguide is formed in the middle of the two-dimensional material layer; two electrodes are formed on both sides of the two-dimensional material layer; a chalcogenide cap layer is formed on the silicon waveguide transmission layer and covers the two-dimensional material layer, the chalcogenide strip waveguide and the electrode. The present invention is a mid-infrared low-loss sapphire-silicon-chalcogenide material hybrid waveguide structure, the two-dimensional material is easy to integrate through van der Waals force and has the advantage of working at room temperature, by greatly enhancing the interaction between light and matter.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to a photoelectric conversion device in the field of optical sensing and communication technology, and specifically relates to a hybrid waveguide integrated mid-infrared photodetector of a sapphire-silicon-chalcogenide material-two-dimensional material system. Background Art

[0002] The mid-infrared band (2-20μm) is an optical band with great engineering application value. First of all, it contains the absorption fingerprints of most chemical molecules and biological molecules (7μm-20μm), which can be used for chemical gas sensing and biological information sensing. It contains atmospheric windows (3-5μm and 8-14μm), which can be used for thermal imaging, infrared countermeasures, and free space communication. Water absorption in the 2μm band is strong, and it has low penetration into human tissue, so it can be used for wind direction tracking and precision surgery. Among them, free space communication is a technology for point-to-point bidirectional information transmission without optical fiber. It has important significance and broad application prospects in bandwidth access, wide area network and metropolitan area network expansion, local area network interconnection, deep space communication, etc. In the above applications, mid-infrared lasers, amplifiers, optical switches, optical modulators, detectors, wavelength division multiplexers, power dividers and other functional devices are indispensable. At present, mid-infrared photodetectors are mainly based on traditional narrow-bandgap semiconductor materials, such as HgCdTe alloys, group III and V, and group II and VI compounds. However, these materials are mainly grown using epitaxial growth methods such as molecular beam epitaxy and metal organic chemical vapor deposition, which have high growth costs and require a strict cooling environment.

[0003] In addition, heterogeneous integration of these materials and silicon has problems such as lattice mismatch, which seriously limits the widespread application and promotion of traditional infrared detectors. Mid-infrared photodetectors based on traditional materials currently usually adopt free-space geometric structures, which limits their integration with other photonic devices such as lasers and modulators. Summary of the invention

[0004] In order to improve the detection bandwidth, responsiveness and signal-to-noise ratio of the current 3-5μm band mid-infrared photodetector at room temperature, the purpose of the embodiment of the present invention is to provide a hybrid waveguide integrated mid-infrared photodetector based on a sapphire-silicon-chalcogenide glass-two-dimensional material system, which realizes a high-responsiveness detector through the strong interaction between the two-dimensional material and the TE0 mode light; utilizes the advantages of waveguide integration and miniaturization to achieve ultra-high bandwidth detection; and utilizes the construction of a heterojunction between two-dimensional materials and other materials to achieve high signal-to-noise ratio detection.

[0005] The technical solution adopted by the present invention includes:

[0006] including a sapphire substrate;

[0007] It includes a silicon waveguide transmission layer formed on a sapphire substrate;

[0008] including a two-dimensional material layer located on a middle portion of the silicon waveguide transmission layer;

[0009] including a chalcogenide strip waveguide formed on the middle of a two-dimensional material layer;

[0010] comprising two electrodes, respectively formed on two sides of the two-dimensional material layer;

[0011] It includes a chalcogenide cap layer formed on a silicon waveguide transmission layer and covering a two-dimensional material layer, a chalcogenide strip waveguide and an electrode.

[0012] The two electrodes are connected to an external detection control circuit for outputting an electrical signal for detection.

[0013] No sulphur-based capping layer is arranged on the electrode, and the sulphur-based capping layer is removed by etching.

[0014] The silicon waveguide transmission layer and the chalcogenide strip waveguide form a hybrid ridge waveguide, and the optical signal of the TE0 mode propagates from the hybrid ridge waveguide formed by the silicon waveguide transmission layer and the chalcogenide strip waveguide, and interacts strongly with the two-dimensional material layer.

[0015] The two-dimensional material layer is a two-dimensional material such as graphene, black phosphorus or tellurene that can realize photoelectric conversion in the mid-infrared band, or a heterojunction material formed by a two-dimensional material that can realize photoelectric conversion in the mid-infrared band and other zero-dimensional, one-dimensional, and two-dimensional materials, or a two-dimensional-three-dimensional heterojunction material composed of a two-dimensional material that can realize photoelectric conversion in the mid-infrared band and silicon. In this type of waveguide structure, the two-dimensional material layers can be respectively concentrated at the TE0 mode field intensity maximum.

[0016] The sapphire substrate is made of sapphire material.

[0017] The graphene layer is made of graphene material.

[0018] The silicon waveguide transmission layer is made of silicon material.

[0019] The chalcogenide strip waveguide and chalcogenide cap layer include but are not limited to Ge 23 S7S 70 and Ge2Sb2Se5 components.

[0020] The sapphire substrate, silicon waveguide layer and chalcogenide material of the present invention all support low-loss transmission of light waves with a wavelength of 3-5 μm. The waveguide layer used includes but is not limited to a hybrid ridge waveguide structure composed of a silicon flat layer and a chalcogenide strip waveguide, supporting TE0 mode optical signal transmission.

[0021] The material system has the characteristics of a wide infrared window and high optical nonlinearity, so the device can operate in the mid-infrared band with low loss.

[0022] For the silicon / chalcogenide hybrid waveguide structure, the two-dimensional material is transferred to the lower surface of the chalcogenide waveguide structure.

[0023] The technical solution provided by the embodiments of the present invention may have the following beneficial effects:

[0024] The substrate and waveguide structure of the present invention support low-loss transmission of signal light in the 3-5μm band, and the two-dimensional material and its heterojunction can absorb mid-infrared light and generate photocurrent. Based on this material system, a silicon slab / chalcogenide waveguide structure can be prepared to support TE0 mode transmission. The two-dimensional material is transferred at the maximum point of the mode light field, which greatly enhances the interaction between the two-dimensional material and the signal light, thereby improving the detector responsivity.

[0025] The present invention is a mid-infrared low-loss sapphire-silicon-chalcogenide material hybrid waveguide structure. The two-dimensional material is easy to integrate through van der Waals forces and works at room temperature. By greatly enhancing the interaction between light and matter, a new solution is proposed for realizing high-speed and high-response detectors in the mid-infrared band. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.

[0027] Figure 1 It is a schematic diagram of a sapphire substrate / silicon slab waveguide layer / chalcogenide strip waveguide / chalcogenide cladding structure according to an exemplary embodiment.

[0028] Figure 2 yes Figure 1 TE0 mode field distribution diagram of the sapphire substrate / silicon slab waveguide layer / chalcogenide strip waveguide / chalcogenide cap layer structure shown.

[0029] Figure 3 It is a photodetector in the form of a straight waveguide.

[0030] Figure 4 It is a photodetector in the form of a microring.

[0031] Figure 5 It is a schematic diagram of the waveguide loss situation of Example 1.

[0032] In the figure: sapphire substrate (1); silicon waveguide transmission layer (2); two-dimensional material layer (3); electrode (4); chalcogenide strip waveguide (5); chalcogenide cladding (6). DETAILED DESCRIPTION

[0033] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, the same numbers in different drawings represent the same or similar elements unless otherwise indicated. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with the present invention. Instead, they are merely examples of devices and methods consistent with some aspects of the present invention as detailed in the appended claims.

[0034] The terms used in the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The singular forms "a", "the" and "the" used in the present invention and the appended claims are also intended to include plural forms unless the context clearly indicates other meanings. It should also be understood that the term "and / or" used herein refers to and includes any or all possible combinations of one or more associated listed items.

[0035] like Figure 1 As shown, the structure of the specific implementation device includes:

[0036] comprising a sapphire substrate 1;

[0037] It includes a silicon waveguide transmission layer 2, which is formed on a sapphire substrate 1 and is integrated with the sapphire substrate 1 using a bonding process;

[0038] It includes a two-dimensional material layer 3, which is located on the middle of the silicon waveguide transmission layer 2 and is transferred and prepared on the silicon waveguide transmission layer 2;

[0039] A chalcogenide strip waveguide 5 is formed on the middle of the two-dimensional material layer 3, specifically grown on the two-dimensional material layer 3 by thermal evaporation;

[0040] It includes two electrodes 4, which are respectively formed on two sides of the two-dimensional material layer 3;

[0041] It includes a chalcogenide capping layer 6 formed on the silicon waveguide transmission layer 2, specifically grown on the silicon waveguide transmission layer 2 using thermal evaporation, and covers the two-dimensional material layer 3, the chalcogenide strip waveguide 5 and the electrode 4 to provide waveguide protection.

[0042] The two electrodes 4 are connected to an external detection control circuit for outputting electrical signals for detection.

[0043] No sulphur-based capping layer 6 is disposed on the electrode 4 , and the sulphur-based capping layer 6 is removed by etching.

[0044] Under such a structure of the present invention, the two-dimensional material layer 3 is located between the silicon waveguide transmission layer 2 and the chalcogenide strip waveguide 5, and is in the middle. The two-dimensional material layer 3 is located where the light field is strongest. The two-dimensional material layer 3 interacts with the light field, and the light field effect is enhanced, thereby enhancing the detection performance.

[0045] The present invention uses the structure of a silicon-chalcogenide glass hybrid waveguide to make the two-dimensional material coincide with the strongest point of the optical mode field (at the interface between silicon and chalcogenide), thereby enhancing the interaction between light and matter and achieving high-performance mid-infrared photoelectric detection effects.

[0046] A hybrid ridge waveguide is formed by the silicon waveguide transmission layer 2 and the chalcogenide strip waveguide 5 , and the optical signal of the TE0 mode propagates from the hybrid ridge waveguide formed by the silicon waveguide transmission layer 2 and the chalcogenide strip waveguide 5 , and interacts strongly with the two-dimensional material layer 3 .

[0047] The two-dimensional material layer 3 directly interacts with the TE0 mode optical signal, absorbs light and generates electrical signals, realizes photoelectric conversion in the mid-infrared band, and the generated electrical signals are collected by the electrode 4.

[0048] The two-dimensional material layer 3 is a two-dimensional material such as graphene, black phosphorus or tellurene that can realize photoelectric conversion in the mid-infrared band, or a heterojunction material formed by a two-dimensional material that can realize photoelectric conversion in the mid-infrared band and other zero-dimensional, one-dimensional, and two-dimensional materials, or a two-dimensional-three-dimensional heterojunction material composed of a two-dimensional material that can realize photoelectric conversion in the mid-infrared band and silicon. In this type of waveguide structure, the two-dimensional material layers can be concentrated at the TE0 mode field intensity maximum.

[0049] Figure 2 This is the simulation result of the field distribution of the TE0 mode of the waveguide structure of the present invention. The sub-figures from left to right are the total field intensity E, the x component E x , y component E y , z component E z The direction of the electric field component is shown in the figure, where the z direction is perpendicular to the cross section and is the direction of light propagation.

[0050] Specifically, the two-dimensional material layer 3 is at the maximum value of the total field strength E, and is also at the E x The maximum value E xmax The x component of the electric field E x The polarization direction is parallel to the plane of the two-dimensional material and can interact strongly with the two-dimensional material. Using the photoelectric conversion of the two-dimensional material 3, mid-infrared light detection can be achieved.

[0051] Example 1

[0052] Constructing a photodetector in the form of a straight waveguide, such as Figure 3 shown.

[0053] The chalcogenide strip waveguide 5 is a straight waveguide arranged in a straight line along the propagation direction of the optical signal. The silicon waveguide transmission layer 2, the two-dimensional material layer 3, and the electrode 4 are all arranged in a straight line along the propagation direction of the optical signal on the required waveguide section to form the structure of the present invention. By aligning the two-dimensional material layer 3 with the strongest mode field in the waveguide, the interaction between light and matter is maximized, so that high-performance detection of the signal light is performed.

[0054] Taking tellurene as an example, the two-dimensional material layer 3 is set to have a thickness of 50 nm at an operating wavelength of 3 μm. The waveguide loss calculation is performed for the case where there is no two-dimensional material layer 3 and the two-dimensional material layer 3 is located above and below the chalcogenide waveguide layer 5. The results are as follows: Figure 5 As shown. It can be seen that for the same two-dimensional material layer 3, when it is located above and below the chalcogenide waveguide layer 5, the waveguide loss is very different. The greater the waveguide loss, the stronger the interaction between light and matter, and the higher the photoelectric conversion efficiency.

[0055] Example 2

[0056] Constructing photodetectors in the form of microrings, such as Figure 4 shown.

[0057] The chalcogenide strip waveguide 5 includes a straight waveguide arranged in a straight line along the propagation direction of the optical signal and a micro-ring waveguide coupled to the side of the straight waveguide. The silicon waveguide transmission layer 2, the two-dimensional material layer 3, and the electrode 4 are all arranged in a straight line along the propagation direction of the optical signal on the side where the micro-ring waveguide is located to form the structure of the present invention. In this example, based on the overlap of the two-dimensional material layer 3 and the strongest part of the mode field in the waveguide, the micro-ring resonator is used to further enhance the interaction between light and matter at the resonant wavelength, thereby improving the photoelectric conversion efficiency.

[0058] Those skilled in the art will readily appreciate other embodiments of the present invention after considering the specification and practicing what is disclosed herein. The present invention is intended to cover any variations, uses or adaptations of the present invention that follow the general principles of the present invention and include common knowledge or customary techniques in the art that are not disclosed by the present invention. The specification and examples are to be considered as exemplary only, and the true scope and spirit of the present invention are indicated by the following claims.

[0059] It should be understood that the present invention is not limited to the exact construction that has been described above and shown in the drawings and that various modifications and changes may be made without departing from the scope thereof. The scope of the present invention is limited only by the appended claims.

Claims

1. A hybrid waveguide integrated two-dimensional material mid-infrared photodetector, Features: comprising a sapphire substrate (1); It comprises a silicon waveguide transmission layer (2) formed on a sapphire substrate (1); It comprises a two-dimensional material layer (3) located on the middle part of the silicon waveguide transmission layer (2); It includes a chalcogenide strip waveguide (5) formed in the middle of a two-dimensional material layer (3) and grown on the two-dimensional material layer (3) by thermal evaporation; It comprises two electrodes (4) formed on two sides of the two-dimensional material layer (3); It includes a chalcogenide cap layer (6) formed on a silicon waveguide transmission layer (2), grown on the silicon waveguide transmission layer (2) by thermal evaporation, and covering a two-dimensional material layer (3), a chalcogenide strip waveguide (5) and an electrode (4); The hybrid waveguide is a hybrid waveguide based on a sapphire-silicon-chalcogenide glass-two-dimensional material system.

2. A hybrid waveguide integrated two-dimensional material mid-infrared photodetector according to claim 1, Features: The two electrodes (4) are connected to an external detection control circuit for outputting an electrical signal for detection.

3. The hybrid waveguide integrated two-dimensional material mid-infrared photodetector according to claim 1, Features: No sulphur-based capping layer (6) is provided above the electrode (4), and the sulphur-based capping layer (6) is removed by etching.

4. The hybrid waveguide integrated two-dimensional material mid-infrared photodetector according to claim 1, Features: The silicon waveguide transmission layer (2) and the chalcogenide strip waveguide (5) form a hybrid ridge waveguide, and a TE0 mode optical signal propagates through the hybrid ridge waveguide formed by the silicon waveguide transmission layer (2) and the chalcogenide strip waveguide (5), and interacts strongly with the two-dimensional material layer (3).

5. The hybrid waveguide integrated two-dimensional material mid-infrared photodetector according to claim 1, Features: The two-dimensional material layer (3) is a two-dimensional material capable of realizing photoelectric conversion in the mid-infrared band, or a heterojunction material formed by a two-dimensional material capable of realizing photoelectric conversion in the mid-infrared band and other zero-dimensional, one-dimensional, or two-dimensional materials, or a two-dimensional-three-dimensional heterojunction material composed of a two-dimensional material capable of realizing photoelectric conversion in the mid-infrared band and silicon.

Citation Information

Patent Citations

  • Planar waveguide type near-and-mid infrared light modulator based on graphene-chalcogenide glass

    CN105700203A

  • Intermediate infrared modulator based on black phosphorus chalcogenide glass optical waveguides

    CN105759467A

  • Black phosphorus mid-infrared optical router based on fluoride waveguide or chalcogenide glass waveguide

    CN106199838A

  • Embedded graphene optical detector based on silicon nitride ridge waveguide and manufacturing method

    CN112635589A

  • Phase change device and preparation method thereof, optical excitation modulation method and electric excitation modulation method

    CN112820827A