Method for forming trench of embedded epitaxial layer
By adding a saturated oxidation step in the trench formation process of the embedded epitaxial layer, the natural oxidation of the silicon nitride sidewalls is controlled, which solves the problem of uneven spacing caused by the waiting time between dry etching and wet etching, and improves the efficiency of the embedded epitaxial layer. Device electrical performance and production efficiency.
Patent Information
- Application Number
- CN202210862806.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-20
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-07-20
AI Technical Summary
In the prior art, during the trench formation process of the embedded epitaxial layer, due to the waiting time between dry etching and wet etching, the spacing between the embedded epitaxial layer and the gate structure is uneven, which affects the performance of the device. Electrical properties.
Add a saturated oxidation step after dry etching to control the natural oxidation of the silicon nitride sidewalls and ensure that the idle time during the waiting process does not exceed the allowable time, thereby maintaining the loss of the hard mask layer during wet etching. Stable, forming a uniform groove structure.
By stably controlling the etching amount of the trench, the uniformity of the spacing between the embedded epitaxial layer and the gate structure of the device is improved, the stability of the electrical performance is improved, the product circulation time window is expanded, and production risks are reduced. .
Smart Images

Figure CN115312461B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing a semiconductor integrated circuit, and in particular to a method for forming a groove of an embedded epitaxial layer. Background Art
[0002] The gate structure in the process nodes below 28nm and 22nm will use high dielectric constant metal gate (HKMG) and embedded epitaxial layer. The embedded epitaxial layer (EPI) is used to change the stress in the channel region, thereby improving the carrier mobility in the channel region. The embedded epitaxial layer of PMOS usually uses an embedded silicon germanium (SiGe) epitaxial layer, and the embedded SiGe EPI is composed of SiGe EPI formed in a groove (recess). The shape of the groove used by the embedded SiGe EPI is usually Σ (sigma) type, which is also called diamond (Diamond) type.
[0003] The current method widely used in the industry to form diamond-shaped grooves is to first use a dry-etching process to etch a U-shaped or ball-shaped groove, where the cross-section of a U-shaped groove is U-shaped, and the cross-section of a ball-shaped groove is a circle with an open top; then use tetramethylammonium hydroxide (TMAH) to selectively etch the crystal surface to produce a diamond-shaped groove. Figures 1A to 1D , which is a device structure diagram in each step of a method of forming a trench and filling an epitaxial layer in the trench, i.e., an embedded epitaxial process ring (EPIloop); the method of forming a trench and filling an epitaxial layer in the trench, i.e., an embedded epitaxial process ring, includes the following steps:
[0004] Step 1: Figure 1A As shown, a first etching is performed to form a groove 105 in a selected area of the silicon substrate 101. The first etching adopts dry etching to make the groove 105 U-shaped or spherical. Figure 1A It is shown in the figure that the groove 105 is spherical, that is, the cross-sectional structure is circular; it can also be that the groove 105 is U-shaped.
[0005] Typically, the top surface of the silicon substrate 101 is a (100) plane.
[0006] The selected regions of the trench 105 are source and drain formation regions on both sides of the gate structure.
[0007] The gate structure is usually a stacked layer of a gate dielectric layer and a metal gate, the gate dielectric layer includes a high dielectric constant layer, that is, the gate structure is HKMG; in step 1, a dummy gate structure is formed on the top surface of the silicon substrate 101, the dummy gate structure is formed in the formation area of the gate structure, and the dummy gate structure is formed by stacking a dummy gate dielectric layer and a dummy polysilicon gate 102; the dummy gate structure is replaced by the gate structure in the subsequent process. Figure 1A As shown, a gate hard mask layer 103 is formed on the top of the pseudo polysilicon gate 102, and a sidewall 104 is formed on the side of the pseudo gate structure. The gate hard mask layer 103 is formed by stacking a nitride layer 103b and an oxide layer 103b. The sidewall 104 is formed by stacking a silicon oxide sidewall 104a and a silicon nitride sidewall 104b.
[0008] Step 2: Figure 1B As shown, a wet etching process is used to perform a second etching on the trench 105. The wet etching liquid 106 of the second etching is usually TMAH. Before TMAH etching, dilute hydrofluoric acid (DHF) etching is usually also included.
[0009] like Figure 1C As shown, the second TMAH etching makes the groove 105 diamond-shaped.
[0010] Typically, in step 2, the second TMAH etching has different etching rates for each crystal plane, so that the groove 105 has a diamond-shaped structure. For example, the etching rates of the TMAH etching for the (110) surface, the (100) surface, and the (111) surface decrease in sequence. Figure 1B In the figure, the straight arrows are used to show the etching directions of the (110) and (100) surfaces. It can be seen that the arrow corresponding to the etching direction of the (100) surface points downward, and the arrow corresponding to the etching direction of the (110) surface points to the left and right. That is, the TMAH etching solution can selectively etch the crystal orientation surface of the silicon substrate 101, thereby forming a diamond-shaped groove 105.
[0011] The dilute hydrofluoric acid of the second etching will remove the natural oxide layer on the surface of the groove 105 before the TMAH etching.
[0012] Step 3: After that, Figure 1D As shown, an epitaxial growth process is performed to form an epitaxial layer 107 to completely fill the trench 105. The epitaxial layer 107 is an embedded epitaxial layer. Generally, the formed epitaxial layer 107 includes a germanium silicon epitaxial layer. The epitaxial growth process needs to be performed in an epitaxial process chamber.
[0013] In the existing method, since the first etching is dry etching and the second etching is wet etching, there is a waiting process between the two. The time of the waiting process is the idle time, and the idle time needs to be less than the allowable time (queque time, Q-time). Q-time is the maximum time interval set to ensure product quality.
[0014] The experiment found that in the existing methods, products with different idle time, Figure 1D The spacing between the top of the embedded epitaxial layer 107 and the gate structure, that is, the silicon to gate (S2G) spacing, will vary. Figure 1D The S2G spacing in the circuit has a great impact on product performance. Summary of the invention
[0015] The technical problem to be solved by the present invention is to provide a method for forming a groove of an embedded epitaxial layer, which can stabilize the wet etching amount of the silicon nitride side wall serving as a hard mask layer in the trench etching, thereby improving the uniformity of the spacing between the embedded epitaxial layer and the gate structure of the device, thereby stabilizing the electrical performance of the device.
[0016] In order to solve the above technical problems, the present invention provides a method for forming a trench of an embedded epitaxial layer, comprising the following steps:
[0017] Step 1: providing a semiconductor substrate having a first gate structure formed thereon, wherein a sidewall spacer is formed on a side of the first gate structure, and the sidewall spacer comprises a silicon nitride sidewall spacer.
[0018] Step 2: Performing a first dry etching on the semiconductor substrate to form a groove using the silicon nitride sidewall on the side of the first gate structure as a self-aligned condition, wherein the groove is U-shaped or spherical; the first dry etching causes the surface of the silicon nitride sidewall and the surface of the groove to have dangling bonds.
[0019] Step three: saturate oxidation is performed on the dangling bonds on the surface of the silicon nitride sidewall and the trench to form a saturated oxide layer.
[0020] Step 4: subjecting the semiconductor substrate to a waiting process.
[0021] The idle time of the waiting process is less than or equal to the allowed time; the allowed time is less than the first time required for the dangling bonds to be saturated and naturally oxidized. Under the condition that it is less than the first time, the thickness of the natural oxide layer formed by the natural oxidation of the dangling bonds increases with time.
[0022] Under the condition of being less than or equal to the allowable time, the idle time may vary according to the actual situation of the production line.
[0023] During the waiting process, the saturated oxide layer is used to prevent the dangling bonds from being naturally oxidized, and thereby prevent the thickness of the natural oxide layer formed by the dangling bonds from changing when the idle time changes, so that the thickness of the saturated oxide layer is consistent when the idle time is different.
[0024] Step 5: Perform a second wet etching.
[0025] The second wet etching adopts DHF etching plus TMAH etching.
[0026] The DHF etching is used to remove the saturated oxide layer.
[0027] The TMAH etching is used to continue etching the semiconductor substrate exposed on the surface of the groove so as to expand the volume of the groove and make the expanded groove diamond-shaped.
[0028] The second wet etching will also cause loss to the silicon nitride sidewalls. By utilizing the characteristic that the thickness of the saturated oxide layer remains unchanged with the idle time, the thickness of the silicon nitride sidewalls remains unchanged with the idle time.
[0029] A further improvement is that in step one, the semiconductor substrate includes a silicon substrate.
[0030] A further improvement is that the first gate structure is formed by stacking a first gate dielectric layer and a polysilicon gate.
[0031] A further improvement is that the sidewalls are composed of the silicon nitride sidewalls or are formed by stacking silicon oxide sidewalls and silicon nitride sidewalls.
[0032] A further improvement is that in step 2, the first dry etching is controlled by APC.
[0033] A further improvement is that in step three, the saturated oxidation is achieved by oxygen plasma (O2 plasma) treatment.
[0034] A further improvement is that in step 4, the first time is 18 hours.
[0035] A further improvement is that the allowable time is less than or equal to 8 hours.
[0036] A further improvement is that after step 5, the following is also included:
[0037] Step six: filling the trench with an epitaxial layer to form an embedded epitaxial layer.
[0038] A further improvement is that in step 2, the trench is formed in a PMOS formation region;
[0039] In step six, the embedded epitaxial layer includes a silicon germanium epitaxial layer.
[0040] A further improvement is that PMOS and NMOS are integrated on the semiconductor substrate at the same time;
[0041] In step 1, the step of forming the silicon nitride sidewall comprises:
[0042] forming a silicon nitride hard mask layer;
[0043] Photolithography opens the PMOS formation area;
[0044] The silicon nitride hard mask layer is etched, and in the formation area of the PMOS, the silicon nitride hard mask layer on the top of the first gate structure and outside the first gate structure are removed, and the silicon nitride hard mask layer retained on the side of the first gate structure forms the silicon nitride side wall; the silicon nitride hard mask layer in the formation area of the NMOS is retained.
[0045] A further improvement is that an N-well is formed on the semiconductor substrate in the PMOS formation region, and the first gate structure is formed on a surface of the N-well.
[0046] A further improvement is that a P-well is formed on the semiconductor substrate in the NMOS formation region, the P-well is formed in a deep N-well, and the first gate structure is formed on the surface of the P-well.
[0047] A further improvement is that the first gate structure is used as a dummy gate structure; in the subsequent process, the step of replacing the first gate structure with a second gate structure is also included, and the second gate structure is formed by stacking a second gate dielectric layer and a metal gate.
[0048] A further improvement is that the second gate dielectric layer includes a high dielectric constant layer;
[0049] The metal gate includes a work function metal layer and a metal conductive material layer stacked in sequence.
[0050] In the process of forming a diamond-shaped groove by a first dry etching and a second wet etching, the present invention adds a saturation oxidation step after the first dry etching is completed, thereby preventing the dangling bonds formed in the first dry etching process from being naturally oxidized during the waiting process and thereby avoiding the formation of natural oxide layers with different thicknesses depending on the idle time of the waiting process, thereby accurately controlling the loss of the silicon nitride side wall as a hard mask layer in the second wet etching. Therefore, the present invention can stabilize the wet etching amount of the silicon nitride side wall as a hard mask layer in the groove etching, thereby improving the spacing between the embedded epitaxial layer and the gate structure of the device, that is, the uniformity of the S2G spacing, that is, improving the fluctuation type of the S2G parameters, thereby stabilizing the electrical performance of the device.
[0051] Since the change of idle time in the waiting process of the present invention has a smaller impact on the electrical performance of the device, the present invention can increase the allowable time window and reduce the risk of idle time exceeding the allowable time; the present invention can also increase the circulation of products and improve production capacity by controlling the allowable time. BRIEF DESCRIPTION OF THE DRAWINGS
[0052] The present invention is further described in detail below with reference to the accompanying drawings and specific embodiments:
[0053] Figure 1A-Figure 1D It is a device structure diagram in each step of a method for forming a trench of an existing embedded epitaxial layer;
[0054] Figure 2 is a flow chart of a method for forming a trench of an embedded epitaxial layer according to an embodiment of the present invention;
[0055] Figure 3A-Figure 3F It is a device structure diagram in each step of the method for forming a trench of an embedded epitaxial layer according to an embodiment of the present invention. DETAILED DESCRIPTION
[0056] Before introducing the embodiments of the present invention in detail, the applicant has made the following detailed analysis on the technical problems of the existing methods, which are now explained as follows:
[0057] In the existing method, after the first etching, i.e., dry etching, dangling bonds will appear on the surface of the silicon nitride sidewall 104b. The silicon nitride layer of the silicon nitride sidewall 104b is usually used as a hard mask layer in the NMOS formation area, and in the PMOS formation area, it also serves as a hard mask layer that only protects the gate structure of the PMOS during the etching process. The hard mask layer is also referred to as SGHM.
[0058] The existence of the dangling bonds of the silicon nitride sidewall 104b makes it easier to absorb oxygen elements in the environment and be oxidized. Experimental data show that the oxidation of SGHM conforms to the conventional oxidation kinetic model. The oxidation rate is fast in the early stage of oxidation, gradually reaches saturation at the end of oxidation, and the oxidation rate gradually slows down until it stabilizes. In the unsaturated oxidation area, such as when the oxidation time is less than 18h, the second etching, that is, wet etching, that is, DHF etching + TMAH etching, the etching amount of SGHM varies with the idle time after dry etching, so the fluctuation (variation) of the S2G parameter in this time interval is relatively large, which will affect the morphology (shape) of the embedded epitaxial layer, and then affect the electrical properties of the product on the wafer (wafer), such as (IONDP_3_P03. When the oxidation time is greater than 18h after oxidation saturation, the etching amount of SGHM by DHF etching + TMAH etching is relatively stable.
[0059] like Figure 2 As shown, it is a flow chart of a method for forming a groove of an embedded epitaxial layer 7 according to an embodiment of the present invention; FIG. 3A to FIG. 3F , is a device structure diagram in each step of the method for forming the groove of the embedded epitaxial layer 7 according to an embodiment of the present invention; the method for forming the groove of the embedded epitaxial layer 7 according to an embodiment of the present invention comprises the following steps:
[0060] Step 1: Figure 3A As shown, a semiconductor substrate 1 having a first gate structure is provided, and a sidewall spacer 4 is formed on the side of the first gate structure. The sidewall spacer 4 includes a silicon nitride sidewall spacer 4b.
[0061] In the embodiment of the present invention, the semiconductor substrate 1 includes a silicon substrate.
[0062] The first gate structure is formed by stacking a first gate dielectric layer and a polysilicon gate 2 .
[0063] The sidewall spacer 4 is composed of the silicon nitride sidewall spacer 4 b or is formed by stacking the silicon oxide sidewall spacer 4 and the silicon nitride sidewall spacer 4 b.
[0064] A gate hard mask layer 3 is also formed on the top of the polysilicon gate 2. The gate hard mask layer 3 is formed by stacking a nitride layer 3b and an oxide layer 3b. The gate hard mask layer 3 is used to define the formation area of the polysilicon gate 2.
[0065] PMOS and NMOS are integrated on the semiconductor substrate 1 at the same time. Figure 3A The NMOS formation region 205 and the PMOS formation region 206 are included in the subsequent trench 5. FIG. 3B to FIG. 3F Only the structure in the PMOS formation region 206 is shown.
[0066] like Figure 3A As shown, the steps of forming the silicon nitride sidewall 4b include:
[0067] A silicon nitride hard mask layer 204 is formed.
[0068] Photolithography is performed to open a PMOS formation region 206 .
[0069] The silicon nitride hard mask layer 204 is etched, and in the PMOS formation area 206, the silicon nitride hard mask layer 204 on the top of the first gate structure and outside the first gate structure is removed, and the silicon nitride hard mask layer 204 retained on the side of the first gate structure forms the silicon nitride side wall 4b; the silicon nitride hard mask layer 204 in the NMOS formation area 205 is retained.
[0070] An N-well 201 is formed on the semiconductor substrate 1 in the PMOS formation region 206 , and the first gate structure is formed on the surface of the N-well 201 .
[0071] A P-well 202 is formed on the semiconductor substrate 1 in the NMOS formation region 205 . The P-well 202 is formed in a deep N-well 203 . The first gate structure is formed on the surface of the P-well 202 .
[0072] Shallow trench isolation is also formed on the semiconductor substrate.
[0073] The first gate structure is used as a dummy gate structure. In the subsequent process, the first gate structure is also replaced by a second gate structure, where the second gate structure is formed by stacking a second gate dielectric layer and a metal gate.
[0074] The second gate dielectric layer includes a high dielectric constant layer;
[0075] The metal gate includes a work function metal layer and a metal conductive material layer stacked in sequence.
[0076] Step 2: Figure 3B As shown, the semiconductor substrate 1 is first dry-etched to form a groove 5 with the silicon nitride sidewall 4b on the side of the first gate structure as a self-aligned condition. The groove 5 is U-shaped or spherical. The first dry-etching causes the surface of the silicon nitride sidewall 4b and the surface of the groove 5 to have dangling bonds.
[0077] In the embodiment of the present invention, the first dry etching adopts APC control. APC control can realize precise control of the etching amount of the first dry etching, so the etching amount of the silicon nitride sidewall 4b by the first dry etching can also be precisely controlled.
[0078] Step 3: Figure 3C As shown, the dangling bonds on the surface of the silicon nitride sidewall 4 b and the trench 5 are saturated oxidized to form a saturated oxide layer. The saturated oxidation is shown by arrow line 301 .
[0079] In the embodiment of the present invention, the saturated oxidation is achieved by oxygen plasma treatment 301 .
[0080] Step 4: subjecting the semiconductor substrate 1 to a waiting process.
[0081] The idle time of the waiting process is less than or equal to the allowed time; the allowed time is less than the first time required for the dangling bonds to be saturated and naturally oxidized. Under the condition that it is less than the first time, the thickness of the natural oxide layer formed by the natural oxidation of the dangling bonds increases with time.
[0082] Under the condition of being less than or equal to the allowable time, the idle time may vary according to the actual situation of the production line.
[0083] During the waiting process, the saturated oxide layer is used to prevent the dangling bonds from being naturally oxidized, and thereby prevent the thickness of the natural oxide layer formed by the dangling bonds from changing when the idle time changes, so that the thickness of the saturated oxide layer is consistent when the idle time is different.
[0084] In the embodiment of the present invention, the first time is 18 hours.
[0085] The permissible time is less than or equal to 8 hours.
[0086] Step 5: Figure 3D As shown, a second wet etching is performed.
[0087] The second wet etching adopts DHF etching plus TMAH etching. The TMAH etching solution is shown as mark 6.
[0088] The DHF etching is used to remove the saturated oxide layer.
[0089] like Figure 3E As shown, the TMAH etching is used to continue etching the semiconductor substrate 1 exposed on the surface of the trench 5 so as to expand the volume of the trench 5 and make the expanded trench 5 diamond-shaped. Figure 3D As shown, the TMAH etching of the second wet etching has different etching rates for each crystal plane, so that the groove 105 has a diamond-shaped structure. For example, the etching rates of the TMAH etching for the (110) surface, the etching rates for the (100) surface, and the etching rates for the (111) surface decrease in sequence. Figure 1BIn the figure, the straight arrows are used to show the etching directions of the (110) and (100) surfaces. It can be seen that the arrow corresponding to the etching direction of the (100) surface points downward, and the arrow corresponding to the etching direction of the (110) surface points to the left and right. That is, the TMAH etching solution can selectively etch the crystal orientation surface of the silicon substrate 1, thereby forming a diamond-shaped groove 5.
[0090] The second wet etching will also cause loss to the silicon nitride sidewall 4b. By taking advantage of the fact that the thickness of the saturated oxide layer remains unchanged as the idle time changes, the thickness of the silicon nitride sidewall 4b remains unchanged as the idle time changes. In this way, when the idle time is different, Figure 3E The S2G spacing in the structure remains unchanged, and the S2G spacing is the spacing between the top of the subsequently formed embedded epitaxial layer 7 and the gate.
[0091] After step 5, it also includes:
[0092] Step 6: Figure 3F As shown, an epitaxial layer is filled in the trench 5 to form an embedded epitaxial layer 7 .
[0093] The embedded epitaxial layer 7 includes a silicon germanium epitaxial layer.
[0094] In the process of forming the diamond-shaped groove 5 by the first dry etching plus the second wet etching in the embodiment of the present invention, a saturation oxidation step is added after the first dry etching is completed, so that the dangling bonds formed in the first dry etching process can be prevented from being naturally oxidized during the waiting process and thus the formation of a natural oxide layer with different thicknesses depending on the idle time of the waiting can be avoided, so that the loss amount of the silicon nitride side wall 4b serving as the hard mask layer can be accurately controlled in the second wet etching. Therefore, the embodiment of the present invention can stabilize the wet etching amount of the silicon nitride side wall 4b serving as the hard mask layer in the etching of the groove 5, thereby improving the spacing between the embedded epitaxial layer 7 of the device and the gate structure, that is, the uniformity of the S2G spacing, that is, the fluctuation type of the S2G parameter can be improved, thereby stabilizing the electrical performance of the device.
[0095] Since the change of idle time in the waiting process of the embodiment of the present invention has a smaller impact on the electrical performance of the device, the embodiment of the present invention can improve the allowable time window and reduce the risk of idle time exceeding the allowable time; the embodiment of the present invention can also increase the circulation of products and improve production capacity by controlling the allowable time.
[0096] The present invention has been described in detail above through specific embodiments, but these do not constitute limitations of the present invention. Without departing from the principle of the present invention, those skilled in the art may also make many variations and improvements, which should also be considered as the protection scope of the present invention.
Claims
1. A method for forming a trench of an embedded epitaxial layer, characterized in that: The steps include: Step 1, providing a semiconductor substrate having a first gate structure formed thereon, wherein a sidewall is formed on a side of the first gate structure, and the sidewall comprises a silicon nitride sidewall; Step 2: performing a first dry etching on the semiconductor substrate to form a groove with the silicon nitride sidewall on the side of the first gate structure as a self-aligned condition, wherein the groove is U-shaped or spherical; the first dry etching causes the surface of the silicon nitride sidewall and the surface of the groove to have dangling bonds; Step 3, saturatingly oxidizing the dangling bonds on the surface of the silicon nitride sidewall and the trench to form a saturated oxide layer; Step 4, subjecting the semiconductor substrate to a waiting process; The idle time of the waiting process is less than or equal to the allowable time; the allowable time is less than the first time required for the dangling bonds to be saturated and naturally oxidized, and under the condition that the time is less than the first time, the thickness of the natural oxide layer formed by the natural oxidation of the dangling bonds increases with time; Under the condition that it is less than or equal to the allowable time, the idle time will change according to the actual situation of the production line; During the waiting process, the saturated oxide layer is used to prevent the dangling bonds from being naturally oxidized, thereby preventing the thickness of the natural oxide layer formed by the dangling bonds from changing when the idle time changes, so that the thickness of the saturated oxide layer is consistent when the idle time is different; Step 5: performing a second wet etching; The second wet etching adopts DHF etching plus TMAH etching; The DHF etching is used to remove the saturated oxide layer; The TMAH etching is used to continue etching the semiconductor substrate exposed on the surface of the groove so as to expand the volume of the groove and make the expanded groove diamond-shaped; The second wet etching will also cause loss to the silicon nitride sidewalls. By utilizing the characteristic that the thickness of the saturated oxide layer remains unchanged with the change of the idle time, the thickness lost by the silicon nitride sidewalls remains unchanged with the change of the idle time.
2. The method for forming a trench of an embedded epitaxial layer according to claim 1, wherein: In step one, the semiconductor substrate includes a silicon substrate.
3. The method for forming a trench of an embedded epitaxial layer according to claim 1, wherein: The first gate structure is formed by stacking a first gate dielectric layer and a polysilicon gate.
4. The method for forming a trench of an embedded epitaxial layer according to claim 1, wherein: The sidewall spacer is composed of the silicon nitride sidewall spacer or is formed by stacking a silicon oxide sidewall spacer and a silicon nitride sidewall spacer.
5. The method for forming a trench of an embedded epitaxial layer according to claim 1, wherein: In step 2, the first dry etching is controlled by APC.
6. The method for forming a trench of an embedded epitaxial layer according to claim 1, wherein: In step three, the saturated oxidation is achieved by oxygen plasma treatment.
7. The method for forming a trench of an embedded epitaxial layer according to claim 1, wherein: In step 4, the first time is 18 hours.
8. The method for forming a trench of an embedded epitaxial layer according to claim 7, characterized in that: The permissible time is less than or equal to 8 hours.
9. The method for forming a trench of an embedded epitaxial layer according to claim 1, wherein: After step 5, it also includes: Step six: filling the trench with an epitaxial layer to form an embedded epitaxial layer.
10. The method for forming a trench of an embedded epitaxial layer according to claim 9, wherein: In step 2, the trench is formed in the PMOS formation area; In step six, the embedded epitaxial layer includes a silicon germanium epitaxial layer.
11. The method for forming a trench of an embedded epitaxial layer according to claim 10, characterized in that: PMOS and NMOS are integrated on the semiconductor substrate at the same time; In step 1, the step of forming the silicon nitride sidewall comprises: forming a silicon nitride hard mask layer; Photolithography opens the PMOS formation area; The silicon nitride hard mask layer is etched, and in the formation area of the PMOS, the silicon nitride hard mask layer on the top of the first gate structure and outside the first gate structure are removed, and the silicon nitride hard mask layer retained on the side of the first gate structure forms the silicon nitride side wall; the silicon nitride hard mask layer in the formation area of the NMOS is retained.
12. The method for forming a trench of an embedded epitaxial layer according to claim 11, characterized in that: An N-well is formed on the semiconductor substrate in the PMOS formation region, and the first gate structure is formed on a surface of the N-well.
13. The method for forming a trench of an embedded epitaxial layer according to claim 11, characterized in that: A P-well is formed on the semiconductor substrate in the NMOS formation region, the P-well is formed in a deep N-well, and the first gate structure is formed on the surface of the P-well.
14. The method for forming a trench of an embedded epitaxial layer according to claim 3, characterized in that: The first gate structure is used as a dummy gate structure. In the subsequent process, the first gate structure is also replaced by a second gate structure, where the second gate structure is formed by stacking a second gate dielectric layer and a metal gate.
15. The method for forming a trench of an embedded epitaxial layer according to claim 14, characterized in that: The second gate dielectric layer includes a high dielectric constant layer; The metal gate includes a work function metal layer and a metal conductive material layer stacked in sequence.
Citation Information
Patent Citations
Method for manufacturing MOS transistor with germanium silicon source and drain
CN109545658A
Method for improving stability of Sigma trench etching process and method for forming germanium-silicon epitaxial layer