A carbon fiber-based piezoresistive pressure sensor array and its preparation method and application

Through the carbon fiber-based piezoresistive pressure sensing array, the orthogonal electrode array structure of flexible substrates and conductive composite materials is used to solve the problems of complex and high cost in the preparation of traditional arrays, and achieve large-area and high-sensitivity pressure space resolution. It is suitable for use in the process of using flexible substrates and conductive composite materials. Application in multiple fields.

CN115389064BActive Publication Date: 2024-11-08TONGJI UNIV
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
CN202211181412.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-09-27
Publication Date
2024-11-08
Estimated Expiration
2042-09-27

AI Technical Summary

Technical Problem

Traditional pressure sensing arrays are costly, complex in large-scale mass production, and difficult to achieve large-area and high-sensitivity pressure spatial resolution, which limits their wide application in the fields of wearable health monitoring and intelligent robots.

Method used

Using carbon fiber-based piezoresistive pressure sensing array, a quadrature electrode array is formed through a flexible substrate and a conductive composite material. PDMS-SWCNTs or PDMS-GR/SWCNTs are used as conductive composite materials to achieve high sensitivity and longitudinal elasticity of pressure signals. deformation.

Benefits of technology

It realizes a high-sensitivity, low-cost pressure sensing array, which can prepare and accurately identify pressure spatial distribution on a large scale. It is suitable for wearable health monitoring, electronic prosthetics and intelligent robots and has great application prospects and production potential.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115389064B_ABST
    Figure CN115389064B_ABST
Patent Text Reader

Abstract

The present invention relates to a flexible pressure sensor, and in particular to a carbon fiber-based piezoresistive pressure sensor array and its preparation method and application, comprising a pair of flexible substrates and a pressure sensing layer encapsulated between the flexible substrates; the pressure sensing layer is formed by two sets of electrode groups fixedly connected by a conductive composite material; the two sets of electrode groups respectively include a number of electrodes arranged in parallel at equal intervals, and the two sets of electrode groups are orthogonally arranged to form an array. Compared with the prior art, the present invention improves the preparation efficiency of the pressure sensor and reduces the preparation cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a flexible pressure sensor, and in particular to a carbon fiber-based piezoresistive pressure sensor array and a preparation method and application thereof. Background Art

[0002] As the largest organ of the human body, the skin not only has the basic functions of protection, secretion and respiration, but also is an important human body perception system that interacts and communicates with our real world. By imitating the characteristics and functional stimulation of natural skin, many scholars have successively developed bionic electronic skin (e-skin) based on flexible sensors, and applied them in the fields of wearable health monitoring equipment, intelligent prostheses, artificial intelligence, human-computer interaction and robotics. Electronic skin based on flexible sensors can detect and quantify the diversity of environmental stimuli, including temperature, humidity, pressure and vibration, and convert them into visual electronic pulses in real time. Flexible pressure sensors are the most important type of flexible electronic devices. They have the advantages of high sensitivity, wide measurement range, and can fit any shape of curved surfaces. They can generate electrical signals under the pressure generated by typical human activities, such as body contact and regular physiological processes of the human body. They have broad application prospects in frontier fields such as human-computer interaction, health monitoring, and soft robots.

[0003] According to different physical sensing mechanisms, flexible pressure sensors can be divided into piezoresistive, piezoceramic, triboelectric and piezoelectric sensors. Among them, flexible pressure sensors based on the "piezoresistive sensing mechanism" (by converting external pressure into a resistance signal) show great potential in practical applications due to their advantages such as easy manufacturing, simple structure, simple readout circuit, high sensitivity, low cost, and the availability of metal coatings / nanoparticles / nanowires, etc. Piezoresistive sensors usually use elastomers and conductive nanomaterials. Elastomers include materials such as polydimethylsiloxane (PDMS), polyurethane (PU), polyimide (PI) and silicone rubber (SR). PDMS has been widely used in flexible electronic devices and wearable devices due to its commercial availability, good stretchability, affinity to human skin, and non-toxicity. A variety of nanomaterials such as carbon nanotubes (CNTs), graphene (GR), M-Xene, PEDOT:PSS, metal nanowires and nanoparticles are used in piezoresistive sensors due to their excellent electrical and mechanical properties to improve the stretchability and sensitivity of elastomers, or to build a conductive network for sensing response by covering it on the surface of flexible elastomers in the form of a film. Among them, the high aspect ratio, low percolation threshold, good conductivity and mechanical properties of CNTs make the CNTs network have good sensing ability, so CNTs have become an ideal material for piezoresistive flexible pressure sensors. However, traditional pressure sensing arrays usually require the integration of more pressure sensing units, which not only increases the workload, but also further increases the preparation cost, limiting its large-scale mass production.

[0004] So far, flexibility, stretchability, sensitivity, super conformality and mechanical durability have become the most concerned and popular research directions of electronic skin. In order to overcome the existing shortcomings of electronic skin, the design of materials and / or the design of the microstructure of the elastomer surface, and then the development of sensitive and stable flexible pressure sensors with a wide pressure range, fast response time, high linearity and low hysteresis pressure response has become the mainstream. Although more and more flexible pressure sensors have proven their feasibility in human health monitoring and medical testing, the mass production of large-area and highly sensitive flexible pressure sensors remains a huge challenge. In addition, constructing a pressure sensing array that can be prepared on a large area and can accurately identify the spatial resolution of pressure can further expand its application in wearable health monitoring systems, electronic prostheses and intelligent robots.

[0005] In summary, it is of great significance and practical value to find a method for preparing a pressure sensor array with simple process, low cost, and controllable size, and to prepare a large-area, high-sensitivity pressure sensor array that can accurately identify the spatial distribution of pressure. Summary of the invention

[0006] The purpose of the present invention is to solve at least one of the above problems and to provide a carbon fiber-based piezoresistive pressure sensor array and its preparation method and application, so as to improve the preparation efficiency of the pressure sensor and reduce the preparation cost.

[0007] The purpose of the present invention is achieved through the following technical solutions:

[0008] The first aspect of the present invention discloses a carbon fiber-based piezoresistive pressure sensing array, comprising a pair of flexible substrates and a pressure sensing layer encapsulated between the flexible substrates;

[0009] The pressure sensing layer is formed by two electrode groups fixedly connected by a conductive composite material; the two electrode groups respectively include a number of electrodes arranged in parallel with equal intervals, and the two electrode groups are orthogonally arranged to form an array.

[0010] The two electrode groups form the upper electrode and the lower electrode, and the conductive composite material connecting the two becomes the "node" of the pressure sensing layer.

[0011] Preferably, the flexible substrate includes but is not limited to a PDMS substrate; the electrodes include but are not limited to carbon fiber bundles or conductive yarns; the conductive composite material includes but is not limited to PDMS-SWCNTs or PDMS-GR / SWCNTs (conductive filler mixed with GR and SWCNTs).

[0012] Preferably, the CNTs are SWCNTs.

[0013] Preferably, the PDMS substrate is prepared by the following method:

[0014] The PDMS precursor and the PDMS curing agent are stirred and mixed at a mass ratio of 10:1 to form a PDMS mixed solution, and then degassed at room temperature until there are no bubbles in the PDMS mixed solution. The degassed PDMS mixed solution is placed in a mold and pre-cured at 50-80° C., but not 80° C., for 5-20 minutes to obtain the PDMS substrate.

[0015] Preferably, the PDMS-SWCNTs are prepared by the following method:

[0016] The PDMS precursor is dissolved in toluene and fully stirred to obtain a PDMS precursor mixed solution; SWCNTs are dispersed in toluene and ultrasonically treated to obtain a toluene dispersion of SWCNTs; the PDMS precursor mixed solution is added to the toluene dispersion of SWCNTs, and stirred to fully disperse the SWCNTs in the mixed solution; the mixed solution is heated to evaporate the toluene, and then a PDMS curing agent is added and stirred to obtain the PDMS-SWCNTs.

[0017] Preferably, in the PDMS precursor mixed solution, the mass ratio of the PDMS precursor to toluene is 1:0.5-2.0; in the toluene dispersion of SWCNTs, the mass ratio of SWCNTs to toluene is 1:40-200, and is not 1:40; the mass of SWCNTs in the mixed solution is 0.5wt%-2.0wt% of the PDMS precursor, and is not 0.5wt%; the mass ratio of the PDMS precursor to the PDMS curing agent is 10:1.

[0018] Further preferably, in the PDMS precursor mixed solution, the mass ratio of PDMS precursor to toluene is 1:1; in the toluene dispersion of SWCNTs, the mass ratio of SWCNTs to toluene is 1:200; and the mass of SWCNTs in the mixed solution is 1.5wt% of the PDMS precursor.

[0019] Preferably, in the array formed by two orthogonally arranged electrode groups, the interval between adjacent parallel electrodes is 1.25 cm-2.5 cm.

[0020] Further preferably, in the array formed by two orthogonally arranged electrode groups, the interval between adjacent parallel electrodes is 1.25 cm.

[0021] The second aspect of the present invention discloses a method for preparing any one of the above-mentioned carbon fiber-based piezoresistive pressure sensor arrays, comprising the following steps:

[0022] S1: Take a group of electrodes and arrange them horizontally on a flexible substrate to form a lower electrode; then, drop-coat the conductive composite material on the electrode at intervals to form a pressure sensing unit; finally, arrange another group of electrodes orthogonally to the lower electrode and fix them on the lower electrode through the pressure sensing unit to form an upper electrode;

[0023] S2: The array formed in step S1 is solidified and flexibly packaged with another flexible substrate to obtain the pressure sensing array.

[0024] Preferably, the curing temperature is 80° C. and the curing time is 90 minutes; and the number of flexible packaging is 2-3 times.

[0025] More preferably, the number of times of flexible packaging is 2 times.

[0026] The third aspect of the present invention discloses an application of a carbon fiber-based piezoresistive pressure sensor array as described above in the fields of wearable health monitoring systems, electronic prostheses and intelligent robots.

[0027] When the pressure sensor is subjected to pressure at a certain position, it will cause the resistance of the surrounding pressure sensing units to change. The resistance measuring instrument connected to the end of the carbon fiber bundle can measure the position of the pressure sensing unit where the resistance changes, thereby determining the pressure action area. Furthermore, the pressure value can be calculated based on the resistance change value.

[0028] Compared with the prior art, the present invention has the following beneficial effects:

[0029] Traditional pressure sensing arrays usually require the integration of more pressure sensing units, which not only increases the workload, but also further increases the preparation cost, limiting its large-scale mass production.

[0030] 1. The sensor obtained by the preparation method of the present invention is not only highly sensitive and low-cost, but also can be miniaturized and prepared on a large area by changing the PDMS substrate area, the number of electrodes and the spacing of the electrode group. This pressure sensing array can also accurately identify the distribution of pressure.

[0031] 2. The carbon fiber-based piezoresistive pressure sensor array prepared by the method of the present invention senses the external pressure by converting the external pressure signal into a resistance signal, and at the same time has the ability of longitudinal elastic deformation, which can meet the flexibility requirements of the pressure sensor.

[0032] 3. In the present invention, the functions of the pressure sensing array can be customized according to different usage scenarios. For example, in terms of electrodes, if the carbon fiber bundles are replaced with stretchable conductive yarns as the upper and lower electrodes, it can not only maintain its longitudinal elastic deformation ability, but also significantly improve its lateral stretchability; in terms of the pressure sensing unit "node", if the PDMS-GR / SWCNTs (conductive filler mixed with GR and SWCNTs) conductive composite material is used to replace the PDMS-SWCNTs conductive composite material, its sensitive response under a wide pressure range can be further improved. Therefore, this preparation method not only makes the carbon fiber-based piezoresistive pressure sensing array have greater advantages and application prospects in the fields of wearable health monitoring systems, electronic prostheses and intelligent robots, but also is expected to be used for large-scale production.

[0033] 4. The carbon fiber-based piezoresistive pressure sensor array prepared by the method of the present invention converts external pressure signals into resistance signals, realizes highly sensitive perception of the size and distribution of external pressure, has the ability of longitudinal elastic deformation, meets the flexibility requirements of pressure sensors, and can be miniaturized and prepared on a large area. The preparation method disclosed in the present invention is simple, efficient, and low-cost, and is expected to be used for large-scale production. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 Schematic diagram of the preparation process of the carbon fiber-based piezoresistive pressure sensor array of Example 1;

[0035] Figure 2 Schematic diagram of the structure of the carbon fiber-based piezoresistive pressure sensor array of Example 1;

[0036] Figure 3 It is a schematic diagram of the structural explosion of the carbon fiber-based piezoresistive pressure sensor array of Example 1;

[0037] Figure 4 This is a physical picture of the carbon fiber-based piezoresistive pressure sensor array of Example 1;

[0038] Figure 5 A schematic diagram of a method for testing the piezoresistive properties of each node of a carbon fiber-based piezoresistive pressure sensor array;

[0039] Figure 6 This is a piezoresistive response diagram of each node of the carbon fiber-based piezoresistive pressure sensor array of Example 1. DETAILED DESCRIPTION

[0040] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.

[0041] Unless otherwise specified, the reagents used in the following examples and comparative examples can be commercially available products that can be routinely obtained by those skilled in the art. Unless otherwise specified, the test methods used in the following examples can be conventional test methods in the art.

[0042] Example 1

[0043] (1) Preparation of PDMS-SWCNTs conductive composite material: First, weigh 2g of PDMS precursor in a beaker and dissolve it in 2g of toluene. Stir thoroughly for 30 minutes at room temperature to mix the raw materials evenly and reduce the viscosity of PDMS. Take another beaker, add 0.03g of SWCNTs and disperse it in 6g of toluene, and ultrasonically treat for 30 minutes to completely debundle the SWCNTs. Then pour the PDMS precursor mixture into the toluene dispersion of SWCNTs and stir thoroughly for 30 minutes at room temperature at 1500rpm to completely disperse the SWCNTs in the mixture of PDMS precursor and toluene. Then transfer the beaker to a fume hood and completely evaporate the toluene at 80°C. Finally, add 0.2g of PDMS curing agent and stir thoroughly until mixed to obtain the PDMS-SWCNTs conductive composite material;

[0044] (2) Preparation of flexible PDMS substrate: 5 g of PDMS precursor and 0.5 g of curing agent were accurately weighed and thoroughly stirred to mix, and then placed in a vacuum drying oven at room temperature for 30 min to degas until there were no bubbles in the PDMS mixture. The PDMS mixture was then poured into a mold (5 mm × 5 mm × 1 mm). After it was naturally leveled, it was quickly placed in an oven preset at 70 ° C for pre-curing for 10 min to obtain a flexible PDMS substrate with a certain viscosity.

[0045] (3) After the PDMS substrate obtained in step (2) is pre-cured, firstly, three pre-cut carbon fiber bundles are arranged transversely to the PDMS substrate at equal intervals to form a lower electrode (the interval between adjacent electrodes is 1.25 mm), and then the PDMS-SWCNTs conductive composite material prepared in step (1) is evenly drop-coated on the carbon fiber bundles at equal intervals to form a pressure sensing unit, and finally, three carbon fiber bundles are orthogonally arranged to the bottom carbon fiber bundles and the pressure sensing unit to form an upper electrode, as shown in FIG. Figure 1-4 As shown, at this time, the PDMS-SWCNTs conductive composite material exists in the form of a pressure sensing unit "node" between the upper and lower carbon fiber bundle electrodes, and a "3×3" pressure sensing array is obtained;

[0046] (4) The pressure sensing array obtained in step (3) was cured at 80°C for 90 min to maintain the stability of the PDMS-SWCNTs pressure sensing unit nodes. Finally, the pressure sensing array was flexibly encapsulated twice with PDMS (5g PDMS precursor + 0.5g curing agent) to obtain a carbon fiber-based piezoresistive pressure sensing array.

[0047] When the carbon fiber-based piezoresistive pressure sensor array of this embodiment is used for piezoresistive sensing and identification of pressure distribution, for example, a resistance measuring instrument is connected to one end of the carbon fiber bundles numbered A1 and a3 (e.g. Figure 5 In the example, the horizontal carbon fiber bundles are named a1-a3, and the vertical carbon fiber bundles are named A1-A3, so that each intersection point has different coordinates for easy recording). Figure 5 As shown in FIG. 1 , when the pressure sensing unit at the intersection of two carbon fiber bundles is subjected to pressure, the resistance measuring instrument will detect a significant resistance change, such as Figure 6 The resistance change rate of the node 13 in the middle can be measured in the same way as the resistance change rate of the other nodes. The piezoresistive response of each node of the carbon fiber-based piezoresistive pressure sensor array is shown in Figure 6 As shown, it shows that each node has a sensitive response to pressure.

[0048] Comparative Example 1

[0049] The difference from Example 1 is that 0.03 g of SWCNTs is added to a beaker and dispersed in 1.2 g of toluene, and ultrasonic treatment is performed for 30 min. At this time, the mass ratio of SWCNTs to toluene is 1:40, and the other experimental steps and dosages are the same as those in Example 1. However, due to the low content of the dispersant toluene, SWCNTs are not easy to debundle in toluene, resulting in the failure to form uniformly dispersed and stable PDMS-SWCNTs pressure sensing unit nodes, and thus the piezoresistive response of each node of the prepared carbon fiber-based piezoresistive pressure sensing array is not obvious, which is not conducive to pressure spatial resolution.

[0050] Comparative Example 2

[0051] The difference from Example 1 is that the mass of SWCNTs added to the system is 0.01 g, that is, the mass fraction is 0.5%, and the other experimental steps and dosages are the same as those in Example 1. However, due to the low content of SWCNTs, the viscosity of the PDMS-SWCNTs conductive composite material finally obtained is low, resulting in the inability to form a structurally stable PDMS-SWCNTs pressure sensing unit node; and the lower SWCNTs do not reach the percolation threshold of the conductive composite material, which further makes the piezoresistive response of each node of the obtained carbon fiber-based piezoresistive pressure sensing array not obvious, which is not conducive to pressure spatial resolution.

[0052] Comparative Example 3

[0053] The difference from Example 1 is that the pre-curing condition used in preparing the flexible PDMS substrate is 80°C / 10min, and the other experimental steps and dosages are the same as those in Example 1. However, due to the excessively high pre-curing temperature or the excessively long pre-curing time, the pre-curing of the flexible PDMS substrate is too thorough, and its surface is not sticky, which makes it difficult for the lower carbon fiber bundle (lower electrode) to adhere to the flexible PDMS substrate and easily slip, so it is not easy to evenly drip the PDMS-SWCNTs conductive composite material and the subsequent flexible packaging. This not only affects the piezoresistive response performance of the obtained carbon fiber-based piezoresistive pressure sensor array, but also affects the overall aesthetics.

[0054] Comparative Example 4

[0055] The difference from Example 1 is that 4 pre-cut carbon fiber bundles are arranged horizontally and vertically to the PDMS substrate in a mold (5mm×5mm×1mm) to form upper and lower electrodes, and a "4×4" pressure sensing array is obtained. At this time, the interval between adjacent carbon fiber bundles is about 1mm, and the other experimental steps and dosages are the same as those in Example 1. However, since the spacing between carbon fiber bundles is reduced under the mold of the same size, it is not conducive to the subsequent drip coating of the PDMS-SWCNTs conductive composite material, and it is easy to produce the convergence of adjacent pressure sensing unit nodes, and it is not easy to form a PDMS-SWCNTs pressure sensing unit node with a stable structure, thereby making the piezoresistive response of each node of the obtained carbon fiber-based piezoresistive pressure sensing array not obvious, which is not conducive to the pressure space resolution.

[0056] Comparative Example 5

[0057] The difference from Example 1 is that the pressure sensing array is only flexibly encapsulated once at the end, and the other experimental steps and dosages are the same as those in Example 1. However, when the flexible encapsulation is only performed once, the upper PDMS flexible matrix after curing cannot completely wrap the carbon fiber bundle, resulting in the exposure of the upper carbon fiber bundle (upper electrode). Therefore, it will not only affect the piezoresistive response of each node of the prepared carbon fiber-based piezoresistive pressure sensing array, which is not conducive to the spatial resolution of pressure, but will also further cause pollution and damage to the pressure sensing layer and affect the aesthetics of the entire carbon fiber-based piezoresistive pressure sensing array.

[0058] The above description of the embodiments is to facilitate the understanding and use of the invention by those skilled in the art. It is obvious that those skilled in the art can easily make various modifications to these embodiments and apply the general principles described herein to other embodiments without creative work. Therefore, the present invention is not limited to the above embodiments, and improvements and modifications made by those skilled in the art based on the disclosure of the present invention without departing from the scope of the present invention should be within the scope of protection of the present invention.

Claims

1. A carbon fiber-based piezoresistive pressure sensor array, characterized in that: The invention comprises a pair of flexible substrates and a pressure sensing layer encapsulated between the flexible substrates; The pressure sensing layer is formed by two electrode groups fixedly connected by a conductive composite material; the two electrode groups respectively include a number of electrodes arranged in parallel at equal intervals, and the two electrode groups are orthogonally arranged to form an array; The conductive composite material is drop-coated at the intersection of the two electrode groups to serve as the node of the pressure sensing layer; When the pressure sensing array is subjected to pressure at a certain position, the resistance of the pressure sensing layer around the pressure position will change. The resistance measuring instrument connected to the end of the carbon fiber bundle can measure the position where the resistance changes in the pressure sensing layer, thereby determining the pressure action area, and then calculating the pressure value based on the resistance change value.

2. The carbon fiber-based piezoresistive pressure sensor array according to claim 1, characterized in that: The flexible substrate comprises a PDMS substrate; the electrode comprises a carbon fiber bundle or a conductive yarn; and the conductive composite material comprises PDMS-SWCNTs or PDMS-GR / SWCNTs.

3. The carbon fiber-based piezoresistive pressure sensor array according to claim 2, characterized in that: The CNTs are SWCNTs.

4. The carbon fiber-based piezoresistive pressure sensor array according to claim 2, characterized in that: The PDMS substrate is prepared by the following method: The PDMS precursor and the PDMS curing agent are stirred and mixed at a mass ratio of 10:1 to form a PDMS mixed solution, and then degassed at room temperature until there are no bubbles in the PDMS mixed solution. The degassed PDMS mixed solution is placed in a mold and pre-cured at 50-80° C., but not 80° C., for 5-20 minutes to obtain the PDMS substrate.

5. The carbon fiber-based piezoresistive pressure sensor array according to claim 2, characterized in that: The PDMS-SWCNTs are prepared by the following method: Dissolving a PDMS precursor in toluene and stirring the mixture thoroughly to obtain a PDMS precursor mixed solution; dispersing SWCNTs in toluene and ultrasonically treating the mixture to obtain a toluene dispersion of SWCNTs; adding the PDMS precursor mixed solution to the toluene dispersion of SWCNTs and stirring the mixture to fully disperse the SWCNTs in the mixed solution; The mixed solution is heated to evaporate the toluene, and then a PDMS curing agent is added and stirred to mix well to obtain the PDMS-SWCNTs.

6. The carbon fiber-based piezoresistive pressure sensor array according to claim 5, characterized in that: In the PDMS precursor mixed solution, the mass ratio of PDMS precursor to toluene is 1:0.5-2.0; in the toluene dispersion of SWCNTs, the mass ratio of SWCNTs to toluene is 1:40-200, and is not 1:40; the mass of SWCNTs in the mixed solution is 0.5wt%-2.0wt% of the PDMS precursor, and is not 0.5wt%.

7. The carbon fiber-based piezoresistive pressure sensor array according to claim 1, characterized in that: The array is formed by two groups of electrodes arranged orthogonally, and the interval between adjacent parallel electrodes is 1.25cm-2.5cm.

8. A method for preparing a carbon fiber-based piezoresistive pressure sensor array as claimed in any one of claims 1 to 7, characterized in that: The steps include: S1: Take a group of electrodes and arrange them horizontally on a flexible substrate to form a lower electrode; then, drop-coat the conductive composite material on the electrode at intervals to form a pressure sensing unit; finally, arrange another group of electrodes orthogonally to the lower electrode and fix them on the lower electrode through the pressure sensing unit to form an upper electrode; S2: The array formed in step S1 is solidified and flexibly packaged with another flexible substrate to obtain the pressure sensing array.

9. The method for preparing a carbon fiber-based piezoresistive pressure sensor array according to claim 8, characterized in that: The curing temperature is 80° C. and the curing time is 90 minutes; the number of flexible packaging is 2-3 times.

10. An application of the carbon fiber-based piezoresistive pressure sensor array according to any one of claims 1 to 7 in the fields of wearable health monitoring systems, electronic prostheses and intelligent robots.

Citation Information

Patent Citations

  • Array type ultra-thin submissive force sensor and preparation method thereof

    CN101201277A

  • Functionalized carbon nanotube flame-retardant polylactic acid and preparation method thereof

    CN102329487A

  • Carbon nanotube / polymer composite membrane array type flexible force sensor and manufacturing method thereof

    CN102374910A

  • Resistance-type pressure distribution fabric sensor

    CN107144379A

  • Flexible electronic skin capable of sensing pressure and preparation method thereof

    CN109307565A