A method for preparing a semi-floating gate transistor, a semi-floating gate transistor and a memory device
By forming the second gate in the semi-floating gate transistor and determining the line width of the contact window using a maskless etching process, the problem of inconsistency in the contact window in the prior art is solved, and the consistency of data storage time and process stability are improved sex.
Patent Information
- Application Number
- CN202211139739.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-19
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-09-19
AI Technical Summary
The contact window line widths of existing semi-floating gate transistors are inconsistent, resulting in a large deviation in data storage time and is greatly affected by the accuracy of the two-step lithography process.
By adopting a preparation method, by providing a gate insulating layer on the first surface of the substrate, a first gate electrode is formed, and the exposed part of the insulating layer is removed to form a contact window, and then a second gate electrode is formed at the contact window position, the first The second gate forms a semi-floating gate layer, and the line width of the final contact window is determined using a maskless etching process to avoid lithography errors.
The consistency of the contact window line width of the semi-floating gate transistor is improved, the deviation of data storage time is reduced, the final line width uniformity of different contact windows is ensured, and the process error is reduced.
Smart Images

Figure CN115394653B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductors, and in particular to a method for preparing a semi-floating gate transistor, a semi-floating gate transistor and a memory device. Background Art
[0002] In traditional floating-gate transistors, electrons tunnel through the high-potential barrier silicon dioxide insulating medium with a bandgap width of 8.9 eV, while in semi-floating gates, electrons tunnel through silicon material with a bandgap width of 1.1 eV. The tunneling barrier is greatly reduced, enabling faster data writing and erasing at low voltage, meeting the chip's low power consumption requirements.
[0003] The contact window of a semi-floating gate transistor is a key factor affecting the data retention time of the device. The current preparation process of the final contact window includes: etching the gate insulating layer through the first photolithography to form a contact window with a larger line width; depositing the gate layer in the contact window; etching away part of the gate layer in the contact window through the second photolithography, and the remaining part of the gate layer overlapping the contact window is the final contact window. Affected by the overlay accuracy of these two photolithography processes, the line width deviation between different final contact windows is large, which in turn leads to a large deviation in the data retention time of the device made of the semi-floating gate transistor. Summary of the invention
[0004] The main technical problem solved by the present application is to provide a method for preparing a semi-floating gate transistor, a semi-floating gate transistor and a memory device, which can improve the consistency of the contact window line width of the semi-floating gate transistor.
[0005] In order to solve the above technical problems, a technical solution adopted in the present application is: to provide a method for preparing a semi-floating gate transistor, comprising: providing a substrate, on the first surface of which a gate insulating layer is arranged; forming a first gate on the gate insulating layer; removing a portion of the gate insulating layer exposed from the first gate to form a contact window; forming a second gate at least at the position of the contact window, the first gate and the second gate constituting a semi-floating gate layer of the semi-floating gate transistor.
[0006] In order to solve the above technical problems, another technical solution adopted in the present application is: to provide a semi-floating gate transistor, which is prepared by the above-mentioned preparation method, comprising: a substrate, including a first surface; a gate insulating layer, located on the first surface of the substrate, and provided with at least one contact window, and the substrate is exposed from the contact window; a first gate, located on the gate insulating layer; a second gate, at least partially located in the contact window, and the first gate and the second gate constitute a semi-floating gate layer of the semi-floating gate transistor.
[0007] In order to solve the above technical problem, another technical solution adopted by the present application is: to provide a memory device, including the above-mentioned half-floating gate transistor.
[0008] Different from the prior art, the beneficial effect of the present application is that the preparation method of the semi-floating gate transistor includes: providing a substrate, a gate insulating layer is arranged on the first surface of the substrate; forming a first gate on the gate insulating layer; removing a portion of the gate insulating layer exposed from the first gate to form a contact window; forming a second gate at least at the contact window position, and the first gate and the second gate constitute the semi-floating gate layer of the semi-floating gate transistor. In the above manner, the line width of the second gate in contact with the substrate in the contact window is used as the final line width of the final contact window, and the deviation of the final line width is only affected by the process of forming the second gate, avoiding the large process error caused by using two-step photolithography for the gate insulating layer and the gate layer respectively, improving the consistency of the line width of the contact window of the semi-floating gate transistor, and also improving the consistency of the data storage time of the device made of the semi-floating gate transistor. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. Among them:
[0010] Figure 1 It is a schematic flow chart of an implementation method of a semi-floating gate transistor manufacturing method of the present application;
[0011] Figure 2 yes Figure 1 A structural diagram of an implementation method of step S101;
[0012] Figure 3 for Figure 1 A schematic structural diagram of forming a first gate material layer in step S102;
[0013] Figure 4 A schematic diagram of the structure of forming a first gate in step S102;
[0014] Figure 5 for Figure 1 A schematic structural diagram of an embodiment of the process after photoresist coating, exposure and development in step S103;
[0015] Figure 6 for Figure 1 A schematic structural diagram of an implementation method of forming a contact window in step S103;
[0016] Figure 7 for Figure 1 A structural schematic diagram of an implementation method of forming a second gate material layer in step S104;
[0017] Figure 8 for Figure 1 Step S104 is a schematic structural diagram of an implementation method of forming a second gate;
[0018] Fig. 9 for Figure 1 A structural schematic diagram of another implementation method of forming a second gate material layer in step S104;
[0019] Fig.10 for Figure 1 A structural schematic diagram of another implementation method of forming a second gate in step S104;
[0020] Fig.11 for Figure 8 A schematic structural diagram of an implementation method of performing post-processing to form an inter-gate dielectric layer;
[0021] Fig.12 for Fig.11 A structural schematic diagram of an implementation method of forming a control gate material layer after the step of forming a control gate material layer;
[0022] Fig.13 for Fig.12 A structural diagram of an embodiment of forming an independently separated half-floating gate transistor after the steps. DETAILED DESCRIPTION
[0023] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0024] Please refer to Figure 1 , Figure 1 1 is a flow chart of an embodiment of a method for preparing a semi-floating gate transistor of the present application. The method for preparing a semi-floating gate transistor may include the following steps S101-S104:
[0025] S101 : providing a substrate 1 , on which a gate insulating layer 2 is disposed, on a first surface a1 of the substrate 1 .
[0026] Please refer to Figure 2 , Figure 2 for Figure 1The structural schematic diagram of an embodiment of step S101 in the figure, the substrate 1 may include but is not limited to silicon materials of single crystal, polycrystalline or amorphous structure applied to semiconductors, and may be an intermediate product of the intermediate link in the processing of wafers, crystal blocks or chips, and may be doped or undoped. The substrate 1 may be any suitable substrate known in the art, for example, it may be at least one of the following materials: silicon (Si), germanium (Ge), silicon germanium (SiGe), carbon silicon (SiC), carbon germanium silicon (SiGeC), indium arsenide (InAs), gallium arsenide (GaAs), indium phosphide (InP) or other III / V compound semiconductors, including multilayer structures composed of these semiconductors, or silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI). The cross section of the groove H may be U-shaped, trapezoidal, square, etc. The gate insulating layer 2 can play an insulating role, and the material can include at least one of silicon oxide, silicon nitride, silicon oxynitride, zirconium oxide and the like, for example, silicon oxide. Figure 2 In the embodiment shown in FIG. 1 , a groove H is provided on the first surface a1 of the substrate 1 , and a gate insulating layer 2 is formed on the first surface a1 and on the inner wall of the groove H. As shown in FIG. Figure 2 In the figure, there are two grooves H. In other embodiments, there may be one or more grooves H. "Multiple" means greater than or equal to 2. Each groove can be used to form a semi-floating gate transistor. The semi-floating gate transistor with grooves can better control the short channel effect.
[0027] In another embodiment, the groove H may not be provided, a planar channel is formed, and the gate insulating layer 2 is formed on the first surface a1 of the substrate 1 .
[0028] S102 : forming a first gate 32 on the gate insulating layer 2 .
[0029] In one embodiment, please refer to Figure 3-Figure 4 , Figure 3 for Figure 1 A schematic diagram of a structure in which a first gate material layer is formed in step S102, Figure 4The schematic diagram of the structure of forming the first gate in step S102, S102 may include: (1) forming a first gate material layer 31 on the gate insulating layer 2, the first gate material layer 31 may be polysilicon, may have a first type of doping, and its formation method may include chemical vapor deposition, plasma-assisted chemical vapor deposition, physical vapor deposition, atomic layer deposition, etc., after depositing the first gate material layer 31, a CMP (chemical mechanical polishing) process is performed to make its surface flat, and the thickness of the first gate material layer 31 can also be controlled. (2) forming a hard mask layer 4 on the first gate material layer 31, the hard mask layer 4 may be one of silicon oxide and silicon nitride, for example, silicon nitride, and the thickness may be (For example, The hard mask layer 4 is used as a mask when patterning the first gate 32, and can also protect the first gate material layer 31, and protect the first gate material layer 31 from damage when the first gate material layer 31 or the gate insulating layer 2 needs to be etched; the patterned photoresist can also be used as a mask to etch and form the first gate 32. (3) Etching the first gate material layer 31 to form the first gate 32, please refer to Figure 4 , so that the first gate 32 fills the groove H and covers the surface of the gate insulating layer 2 adjacent to the groove H. The thickness of the first gate 32 on the first surface a1 can be (For example, (4) Removing the hard mask layer 4. For example, if the material of the hard mask layer 4 is silicon nitride, phosphoric acid may be used to remove the hard mask layer 4.
[0030] S103: removing a portion of the gate insulating layer 2 exposed from the first gate 32 to form a contact window 6;
[0031] like Figure 6 As shown, the substrate 1 is exposed from the contact window 6, and the side b of the contact window 6 close to the first gate 32 is aligned with the first gate 32, so that when the second gate is subsequently formed on the contact window, the final line width of the contact window is completely determined by the maskless etching process, that is, Figure 8 The middle line widths W1 and W2 are determined by the maskless etching process. The volatility of the photolithography process has no effect on the final line width of the contact window, and the process is more stable.
[0032] The side b of the contact window 6 close to the first gate 32 may not be aligned with the first gate 32 , and a portion of the gate insulating layer 2 is retained between the contact window 6 and the first gate 32 .
[0033] In some embodiments, step S103 may include: Figure 5 , Figure 5 for Figure 1A schematic diagram of the structure of an embodiment after exposure and development after coating the photoresist in step S103. A negative photoresist 5 is coated on the second surface a2 of the first gate 32 away from the first surface a1 and the third surface a3 of the gate insulating layer 2 away from the first surface a1, and the negative photoresist 5 is photoetched from the upper side of the first gate 32 away from the first surface a1 along the direction N1. After exposure and development, the gate insulating layer 2 on the contact window area is exposed, and the gate insulating layer 2 exposed in the contact window area is etched to form a contact window. Please refer to Figure 6 , Figure 6 for Figure 1 Schematic diagram of the structure of an embodiment of forming a contact window in step S103. This ensures that the surface b of the contact window 6 formed close to the first gate 32 is aligned with the first gate 32. After the contact window 6 is formed, the remaining negative photoresist 5 can be removed.
[0034] In another embodiment, before applying the negative photoresist 5, the hard mask layer 4 is still retained on the first gate 32. The hard mask layer 4 is removed after the contact window 6 is formed.
[0035] In another embodiment, a photolithography process with positive photoresist coating and etching may be used to form the contact window 6. In another embodiment, the contact window 6 is formed by plasma etching the gate insulating layer 2.
[0036] S104: forming a second gate 72 at least at the position of the contact window 6, the first gate 32 and the second gate 72 constitute a semi-floating gate layer of the semi-floating gate transistor.
[0037] In one embodiment, step S104 may include: cleaning the etching residue of the gate insulating layer 2 in the contact window 6 with hydrofluoric acid to ensure the bonding strength between the second gate 72 and the substrate 1 in the contact window 6; forming a second gate material layer 71 on the first gate 32, the contact window 6 and the gate insulating layer 2, please refer to Figure 7 , Figure 7 for Figure 1 Schematic diagram of the structure of an embodiment of forming a second gate material layer in step S104. The second gate material layer 71 can be polysilicon, and its material and structure can be the same as or different from the first gate 32. The second gate material layer 71 can have the same first type of doping as the first gate 32. At this time, the thickness of the second gate material layer 71 on the gate insulating layer 2 or the first gate 32 can be (For example, Then, the second gate material layer 71 is etched without a mask to form a second gate 72. The second gate 72 is attached to the contact window 6 near the side b of the first gate 32. Figure 8 , Figure 8 for Figure 1Step S104 forms a schematic diagram of a structure of an embodiment of a second gate. The etching method may be a Blanket Etch process until the width of the second gate 72 in contact with the substrate 1 in the contact window 6 (ie Figure 8 The line widths W1 and W2 indicated in the figure are preset line widths.
[0038] After this step, the second gate 72 makes contact with the substrate 1 and the first gate 32 in the contact window 6, making it possible for the first gate 32 to be electrically connected to the contact window 6 through the second gate 72, and the line widths W1 and W2 of the second gate in the contact window become the final line widths of the contact window. Since the maskless etching method has good controllability, the final line width uniformity of the prepared semi-floating gate transistor is high. The number of contact windows 6 can be multiple (for example, 2, 3, 4, etc.), and the final line width deviation of different contact windows 6 can be reduced to within 5nm. The final line width difference of different contact windows made by traditional processes can reach about 20nm, and the data storage deviation is large. The above-mentioned semi-floating gate transistor preparation method can reduce this deviation to 5nm and below, which can ensure the final line width consistency between different contact windows.
[0039] like Figure 8 As shown, the second gate 72 formed by maskless etching forms the structure of the gate sidewall shown in the figure. In one embodiment, the material of the gate sidewall is polysilicon. In the direction N2 from the first gate 32 to the second gate 72, the surface of the second gate 72 away from the first gate 32 can be a convex arc, which is different from the gate structure at the contact window in the prior art that is basically perpendicular to the substrate 1. Compared with the prior art, the second gate 72 with a convex arc surface formed by maskless etching has higher dimensional stability. Its specific shape can be adjusted according to the actual maskless etching process conditions and the actual requirements of the product. The first gate 32 and the second gate 72 constitute the semi-floating gate layer of the semi-floating gate transistor.
[0040] The semi-floating gate transistor prepared by steps S101-S104 has a line width where the second gate 72 contacts the substrate 1 in the contact window 6 as the final line width of the contact window 6, and the traditional two-step photolithography method is changed to a one-step photolithography plus a one-step maskless etching method, thereby avoiding the large process error caused by using two-step photolithography for the gate insulating layer 2 and the first gate material layer 31, improving the consistency of the line width of the semi-floating gate transistor contact window 6, and also improving the consistency of the device storage data time made by the semi-floating gate transistor. The final line width can be adjusted according to the characteristics of the device, for example, 40nm-60nm.
[0041] In some application scenarios, such as Fig. 9 As stated, Fig. 9 for Figure 1The second gate material layer 71 is deposited on the substrate 1, covering the gate insulating layer 2, the contact window 6 and the first gate 32. Fig.10 As shown, Fig.10 for Figure 1 The schematic diagram of the structure of another implementation method of forming the second gate in step S104 is as follows. After the second gate material layer 71 is etched without a mask, the second gates 72 and 73 are formed on both sides of the first gate 32. The second gates 72 and 73 are located on the drain side and the source side, respectively. The second gates 72 and 73 are made of the same material, and the line widths W3 and W4 of the second gate 73 bonded to the gate insulating layer 2 and the line widths W1 and W2 of the second gate 72 in the contact window 6 are all preset line widths, and the deviations of the line widths W1, W2, W3, and W4 are 5nm or less. Fig.10 Only two semi-floating gate transistors are shown. Of course, in other embodiments, the memory device may include more than two semi-floating gate transistors, and the deviation of the line width of the contact windows 6 of different semi-floating gate transistors may be 5 nm or less. In this embodiment, not only the second gate 72 is formed at the contact window 6, but also a second gate 73 is formed on the other side of the first gate 32.
[0042] In one embodiment, please refer to Figure 2-Figure 8 The method for preparing the semi-floating gate transistor of the application may include the following steps:
[0043] S101: providing a substrate 1, and providing a gate insulating layer 2 on a first surface a1 of the substrate 1;
[0044] S102: forming a first gate 32 on the gate insulating layer 2;
[0045] S103: removing a portion of the gate insulating layer 2 exposed from the first gate 32 to form a contact window 6;
[0046] S104: forming a second gate 72 at least at the position of the contact window 6, the first gate 32 and the second gate 72 constitute a semi-floating gate layer of the semi-floating gate transistor.
[0047] After the above steps, the inter-gate dielectric layer 8, the control gate 92, the insulating sidewall SP, the source 111 and the drain 112 of the semi-floating gate transistor can be prepared:
[0048] like Fig.11 As shown, Fig.11 for Figure 8A schematic diagram of a post-processing method for forming an inter-gate dielectric layer is shown in FIG. 1. The gate insulating layer 2 on the side of the contact window 6 away from the groove H is removed, and an inter-gate dielectric layer 8 is deposited on the side of the first gate 32 and the second gate 72 away from the first surface a1 and the exposed first surface a1. The inter-gate dielectric layer 8 may include a silicon oxide layer 81 and a silicon nitride layer 82 to form an ON structure.
[0049] Please refer to Fig.12 , Fig.12 for Fig.11 A structural schematic diagram of an implementation method of forming a control gate material layer after the step of forming a control gate material layer, on the side of the silicon nitride layer 82 away from the first surface a1, a control gate material layer 91 of a certain thickness, such as polycrystalline silicon, is deposited, and planarization is performed to make the control gate material layer 91 reach the required thickness, and the control gate material layer 91 covers the silicon nitride layer 82.
[0050] Please refer to Fig.13 , Fig.13 for Fig.12 The schematic diagram of the structure of an embodiment of an independent and separated semi-floating gate transistor is formed after the steps of etching the control gate material layer 91, the inter-gate dielectric layer 8 and the first gate 32, wherein the control gate material layer 91 is etched to form a control gate 92.
[0051] After etching, the control gate 92 , the inter-gate dielectric layer 8 and the first gate 32 form a gate stack, insulating sidewalls SP are formed on both sides of the gate stack, and source and drain ions are implanted into the substrate 1 to form a source 111 and a drain 112 .
[0052] After the above steps, independent and separated semi-floating gate transistors J1 and J2 can be formed on the substrate 1 .
[0053] The present application also relates to a semi-floating gate transistor, which is prepared by the above-mentioned preparation method. Please refer to Figure 8 and Fig.10 The semi-floating gate transistor includes a substrate 1 , a gate insulating layer 2 , a first gate 32 and a second gate 72 .
[0054] The substrate 1 includes a first surface a1, and optionally, a groove H or a planar channel is provided on the first surface a1 to form a semi-floating gate structure. The substrate 1 may include but is not limited to a silicon material of a single crystal, polycrystalline or amorphous structure used for semiconductors, and may be an intermediate product of an intermediate link in the processing of a wafer, a crystal block or a chip, and may be doped or undoped. The substrate 1 may be any suitable substrate known in the art, for example, at least one of the following materials: silicon (Si), germanium (Ge), silicon germanium (SiGe), carbon silicon (SiC), carbon germanium silicon (SiGeC), indium arsenide (InAs), gallium arsenide (GaAs), indium phosphide (InP) or other III / V compound semiconductors, and also includes a multilayer structure composed of these semiconductors, or silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI). The cross section of the groove H may be U-shaped, trapezoidal, square, etc. There may be one or more grooves H, depending on the actual device structure.
[0055] The gate insulating layer 2 is located on the first surface a1 of the substrate 1 and includes a contact window 6, through which the substrate 1 is exposed. The gate insulating layer 2 can play an insulating role, and the material can include at least one of silicon oxide, silicon nitride, silicon oxynitride, zirconium oxide and the like.
[0056] The first gate 32 is located on the gate insulating layer 2 and can be made of polysilicon.
[0057] The second gate 72 is at least partially located in the contact window 6 and at least partially adhered to the first gate 32. The first gate 32 and the second gate 72 constitute a semi-floating gate layer of the semi-floating gate transistor. The second gate 72 can be polysilicon and can have the same doping as the first gate 32. In the direction N2 from the first gate 32 to the second gate 72, the surface of the second gate 72 away from the first gate 32 can be a convex arc, which is different from the gate structure at the contact window in the prior art that is basically perpendicular to the substrate 1. Compared with the prior art, the second gate 72 with a convex arc surface formed by maskless etching has higher dimensional stability, that is, the stability of the line width of different contact windows 6 is higher. The width of the second gate 72 set in each contact window 6 can be a preset line width, and the preset line width can be 40nm-60nm, which can ensure the consistency of storage time.
[0058] In one embodiment, each contact window 6 may correspond to a groove H, the inner wall of the groove H may be provided with a gate insulating layer 2, the first gate 32 at least fills the groove H, and the semi-floating gate transistor with the groove H may better control the short channel effect. Optionally, the groove H may also be replaced by a planar channel.
[0059] The line width of the contact window of the semi-floating gate transistor is obtained by only one photolithography process, which reduces the preparation deviation caused by the photolithography process, improves the uniformity between the line widths of the contact windows, and is conducive to ensuring the consistency of the storage time of the semi-floating gate transistor.
[0060] The present application also relates to a memory device, comprising the aforementioned semi-floating gate transistor.
[0061] In some embodiments, the number of the semi-floating gate transistors of the memory device may be multiple (e.g., 2, 3, 4, etc.), and the width deviation of the second gate 72 in the contact windows 6 of different semi-floating gate transistors is less than or equal to 5 nm. Figure 8 The deviation between W1 and W2 is less than or equal to 5nm, Figure 8 Only two semi-floating gate transistors are shown. Of course, in other embodiments, the memory device may include more than two semi-floating gate transistors, and the line width deviation of the contact window of each semi-floating gate transistor may be 5nm or less. The width deviation of the prior art is about 20nm, so the memory device has higher line width uniformity and better storage time consistency than the prior art.
[0062] In one embodiment, in the memory device, at least two adjacent half-floating gate transistors may share a source, for example Fig.13 The adjacent half-floating gate transistors J1 and J2 in the memory device can share the source 111. This arrangement helps to reduce the area occupied by all the half-floating gate transistors on the substrate and improve the integration density of the memory device.
[0063] In one embodiment, please refer to Fig.10 , between two adjacent grooves H, the first gate 32 can be discontinuous, that is, two adjacent semi-floating gate transistors do not share a source. The second gate material layer 71 is deposited on the substrate 1, covering the gate insulating layer 2, the contact window 6 and the first gate 32. Second gates 72 and 73 are formed on both sides of the first gate 32. The second gates 72 and 73 are located on the drain side and the source side, respectively. The second gates 72 and 73 are made of the same material, and the line widths W3 and W4 of the second gate 73 and the gate insulating layer 2 are in contact with the line widths W1 and W2 of the second gate 72 in the contact window 6. The deviation of the line widths W1, W2, W3, and W4 can be 5nm or less. In this embodiment, not only is the second gate 72 formed at the contact window 6, but a second gate 73 is also formed on the other side of the first gate 32. Fig.10Only two semi-floating gate transistors are shown. Of course, in other embodiments, the memory device may include more than two semi-floating gate transistors, and the deviations of the line widths of the second gate 72 and the second gate 73 of each semi-floating gate transistor and different semi-floating gate transistors may be 5 nm or less. When two adjacent grooves H do not share the same gate, the uniformity of the contact line widths can be improved, which is conducive to ensuring the consistency of the storage time of the semi-floating gate transistors.
[0064] As can be seen from the above, the method for preparing a semi-floating gate transistor used in the present invention includes: providing a substrate, and providing a gate insulating layer on a first surface of the substrate; forming a first gate on the gate insulating layer; removing a portion of the gate insulating layer exposed from the first gate to form a contact window; and forming a second gate at least at the position of the contact window, wherein the first gate and the second gate constitute a semi-floating gate layer of the semi-floating gate transistor. By means of the above method, the consistency of the line width of the contact window of the semi-floating gate transistor can be improved.
[0065] The above are only implementation methods of the present application, and are not intended to limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. A method for preparing a semi-floating gate transistor, characterized in that: include: Providing a substrate, wherein a gate insulating layer is disposed on a first surface of the substrate; forming a first gate on the gate insulating layer; removing a portion of the gate insulating layer exposed from the first gate to form a contact window; forming a second gate at least at the contact window position, wherein the first gate and the second gate constitute a semi-floating gate layer of the semi-floating gate transistor; The step of forming a second gate at least at the contact window position comprises: forming a second gate material layer on the gate insulating layer, the contact window and the first gate; The second gate material layer is etched without a mask until the width of the second gate in the contact window reaches a preset line width; in the direction from the first gate to the second gate, a surface of the second gate away from the first gate is a convex arc.
2. The preparation method according to claim 1, characterized in that: A groove is arranged on the first surface of the substrate, the gate insulating layer is arranged on the inner wall of the groove, and the first gate at least fills the groove.
3. The preparation method according to claim 1, characterized in that: The substrate is exposed from the contact window, and a side of the contact window close to the first gate is aligned with the first gate.
4. The preparation method according to claim 1, characterized in that: There are a plurality of semi-floating gate transistors, and a width deviation of the second gate in the contact windows of different semi-floating gate transistors is less than or equal to 5 nm.
5. The preparation method according to claim 1, characterized in that: The second gate is also formed on a side of the first gate away from the contact window.
6. The preparation method according to any one of claims 1 to 5, characterized in that: After the step of forming a second gate at least at the contact window position, the method further comprises: An inter-gate dielectric layer and a control gate are sequentially formed on the first gate, the second gate, and the exposed surface of the substrate away from the first surface, wherein the inter-gate dielectric layer, the control gate, and the first gate form a gate stack; Forming insulating sidewalls on both sides of the gate stack; Using the sidewall as a mask, ion implantation is performed on the substrate to form a source and a drain, thereby forming the semi-floating gate transistor.
7. A semi-floating gate transistor, characterized in that: include: a substrate comprising a first surface; a gate insulating layer, located on the first surface of the substrate; a contact window, wherein the substrate is exposed from the contact window; A first gate, located on the gate insulating layer; A second gate, at least partially located in the contact window, the first gate and the second gate forming a semi-floating gate layer of the semi-floating gate transistor; In the direction from the first gate to the second gate, a surface of the second gate away from the first gate is a convex arc; the convex arc is formed by maskless etching of a second gate material layer arranged on the gate insulating layer, the contact window and the first gate.
8. The semi-floating gate transistor according to claim 7, characterized in that: The width of the second gate arranged in each of the contact windows is a preset line width, and the preset line width is 40nm-60nm.
9. The semi-floating gate transistor according to claim 7, characterized in that: A groove is provided on the first surface of the substrate, the inner wall of the groove is provided with the gate insulating layer, and the first gate at least fills the groove.
10. A storage device, characterized in that: A semi-floating gate transistor comprising any one of claims 7 to 9, characterized in that there are multiple semi-floating gate transistors, and the width deviation of the second gate in the contact windows of different semi-floating gate transistors is less than or equal to 5 nm.
11. The memory device according to claim 10, wherein: At least two adjacent semi-floating gate transistors share a source.
Citation Information
Patent Citations
Manufacturing method of semi-floating gate transistor
CN113471294A
Manufacturing method of memory device
CN113823566A
Semiconductor storage device and method for manufacturing the same
JP2003289114A
Non-volatile memory device and method of manufacturing the same
US20060145237A1