A packaging method for a packaging structure of a planar power device

By utilizing precise plastic packaging technology of metal bumps and three-dimensional metal frame strips in the packaging structure of planar power devices, low on-resistance and efficient heat dissipation are achieved, solving the problems of high on-resistance and poor heat dissipation performance of traditional packaging structures, and improving improves current carrying capabilities and signal integrity.

CN115394657BActive Publication Date: 2024-10-01ZHE JIANG HE XIN SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210604664.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-05-31
Publication Date
2024-10-01
Estimated Expiration
2042-05-31

AI Technical Summary

Technical Problem

The traditional wire-bonded package has a large on-resistance, which affects the current carrying capacity, and the heat dissipation performance is insufficient, making it difficult to meet the needs of high-power consumption equipment such as 5G base stations.

Method used

It adopts the packaging structure of planar power devices, pre-sets metal bumps and heat dissipation layers on the wafer, and uses three-dimensional metal frame strips for precise molding and formation of flow channels to achieve direct interconnection between the chip and the PCB and efficient heat dissipation.

Benefits of technology

It reduces the on-resistance of the package, improves the current carrying capacity and heat dissipation performance, simplifies the packaging process, improves signal integrity and radio frequency performance, and reduces production costs and production time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115394657B_ABST
    Figure CN115394657B_ABST
Patent Text Reader

Abstract

The present invention discloses a packaging method for a packaging structure of a planar power device, and belongs to the field of semiconductor packaging technology. The method adopts a metal bump under the chip on the front side of the chip to be flipped onto the etched surface of a three-dimensional metal frame, and realizes direct interconnection between the chip and the PCB through the folding of the metal bump under the chip and the three-dimensional metal frame, thereby streamlining the packaging structure, avoiding the traditional wire bonding process, reducing the packaging resistance, and increasing the current carrying capacity; at the same time, shortening the interconnection distance between the chip and the outside world, and enhancing the conductive effect of the chip; the back side of the chip is exposed and directly welded to the PCB for heat dissipation, thereby improving the heat dissipation capacity of the package, improving the stability of the chip when running at high speed, and improving the quality of the product; in addition, the metal pins of the three-dimensional metal frame are in a concave arc columnar shape, which enhances the bonding force between the metal pins and the plastic packaging material, and achieves the purpose of increasing product reliability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a packaging method for a packaging structure applied to a planar power device, belonging to the technical field of semiconductor packaging. Background Art

[0002] With the development of the 5G industry, consumer electronics and new energy vehicle industries, for example, the power consumption of 5G base stations has increased. The power consumption of 5G base stations is twice that of 4G. In order to reduce power consumption requirements, it is necessary to increase the requirements for low loss and high thermal stability of chips. At the same time, this also places higher requirements on the package type's low on-resistance, low heat generation and fast heat dissipation.

[0003] Traditional wire bonding packages all use wire bonding packaging, and the wire resistance R w Large, which will increase the on-resistance of the entire package and ultimately affect the current carrying capacity of the product. Summary of the invention

[0004] In order to overcome the shortcomings of the prior art, the present invention provides a packaging method for a packaging structure applied to a planar power device, so that the chip using this packaging method can achieve low on-resistance, carry large current, have excellent heat dissipation performance, and have a simple packaging structure.

[0005] The technical solution of the present invention:

[0006] The present invention provides a packaging method for a packaging structure of a planar power device, and the process method thereof is as follows:

[0007] Step 1: prepare the incoming wafer, on which there are neatly arranged horizontal and vertical cross-cutting lanes I, which pre-divide the wafer into a plurality of chips, each of which is provided with a plurality of metal bumps under the chip on the front side and a heat dissipation layer on the back side, one end of the metal bump under the chip corresponds to the electrode of the chip, and the other end is provided with a welding layer;

[0008] Step 2: Using a cutting process to form a plurality of independent chips along the cutting path I;

[0009] Step 3, prepare a three-dimensional metal frame bar, and use the etching surface on the back side as the working surface. The three-dimensional metal frame bar etches the back side of the three-dimensional metal frame bar through a half-etching process to remove excess metal material. A plurality of hollow patterns I and hollow patterns II and alignment points are arranged in an array on the back side of the three-dimensional metal frame bar to form an etching surface, and a horizontal cutting path III and a longitudinal cutting path III are designed. The alignment points are arranged on the four sides of the three-dimensional metal frame bar, the hollow pattern I and the hollow pattern II are parallel and staggered in the center of the three-dimensional metal frame bar, and are both rectangles of equal length, and the width of the hollow pattern I is greater than the width of the hollow pattern II; the hollow pattern I divides the three-dimensional metal frame bar into a plurality of block-shaped metal frame bodies, and the hollow pattern II is parallel to the hollow pattern I to further divide the metal frame body into a plurality of strip-shaped metal frame support bars, and the hollow pattern II divides the metal frame body into a number of metal frame support bars;

[0010] Metal pins are formed on both ends of the etched surface of the metal frame support bar, and the metal pins are located inside the long sides of the hollow pattern I and the hollow pattern II;

[0011] The longitudinal cutting path III is parallel to the length direction of the hollow pattern I and cuts the hollow pattern I. The transverse cutting path III is set on the upper and lower sides of the three-dimensional metal frame bar and passes through the upper and lower ends of the hollow pattern I and the hollow pattern II to pre-cut the metal frame support bars from the three-dimensional metal frame bar one by one.

[0012] The etched surface of the metal frame support bar and the metal pins thereon together form a cavity;

[0013] Step 4: Place the front side of the chip inverted into the cavity of the three-dimensional metal frame bar in sequence, and align the points so that the metal bumps under the chip are fixedly connected to the metal frame support bar through the welding layer to achieve circuit conduction of the chip;

[0014] Step 5: After the plastic encapsulation material is melted by a film-assisted plastic encapsulation single-sided molding process, the three-dimensional metal frame strip and the chip are covered by pressure, and hollow patterns I and II are filled. The hollow patterns I and II play a role in guiding the plastic encapsulation material to form a guide channel;

[0015] Step 6: exposing the upper surface of the metal pins of the three-dimensional metal frame strip and the heat dissipation layer on the back of the chip through a grinding process;

[0016] Step 7: Laminating a protective film with adhesive backing on the flat front surface of the three-dimensional metal frame strip through a lamination process;

[0017] Step 8, forming a conductive metal layer I and a conductive metal layer III on the upper surface of the metal pin and the surface of the heat dissipation layer respectively by sputtering, chemical deposition, printing or spraying;

[0018] Step nine, along the horizontal cutting line III and the vertical cutting line III, the above-mentioned package body is divided into a package structure monomer of a plurality of chips, and the chip is folded upward through the metal bumps under the chip and the three-dimensional metal frame to directly connect and dissipate heat with the back side of the chip and the PCB.

[0019] Furthermore, in step three, the forming process of the metal pin is as follows:

[0020] Symmetrical metal columns are formed on both ends of the etched surface of the metal frame support bar by sputtering, corrosion, chemical deposition, printing or spraying as metal pins.

[0021] Furthermore, in step three, the forming process of the metal pin is as follows:

[0022] A plurality of metal pillars of the same height are formed by photoresist patterning and metal deposition method, and the bottoms of the metal pillars are connected to the etched surfaces of the above-mentioned metal frame support bars by welding process to form metal pins.

[0023] Furthermore, in step three, the forming process of the metal pin is as follows:

[0024] Prepare a metal sheet, use a high-reflection laser to form a number of metal columns with the same height through a laser cutting process, and connect the bottom of the metal column to the etched surface of the above-mentioned metal frame support bar through a welding process to form a metal pin.

[0025] Furthermore, in step three, the forming process of the metal pin is as follows:

[0026] When the three-dimensional metal frame bar is formed, the back side of the three-dimensional metal frame bar is etched through a semi-etching process to remove excess metal material, and a plurality of hollow patterns I, hollow patterns II, alignment points and metal pins are arranged in an array on the back side of the three-dimensional metal frame bar, and a horizontal cutting path III and a longitudinal cutting path III are designed. Due to the different etching speeds, the cylindrical surface of the metal pin is a concave arc column, and its curvature R is controlled by the actual process. The metal pin and the metal frame support bar are an integrated structure.

[0027] Furthermore, the surface of the metal pin or the surface of the metal pin and the etched surface of the three-dimensional metal frame strip are roughened by a plasma etching process, and the roughness Ra is controlled in the range of Ra 0.2-0.4.

[0028] Furthermore, the welding layer is a metal selected from titanium, copper, silver, nickel, gold, tin, and tin-silver, or a combination of several metals.

[0029] Furthermore, the cross-sectional dimension of the heat dissipation layer is not smaller than the cross-sectional dimension of the chip.

[0030] Furthermore, the cross section of the metal pin is circular, rectangular or hexagonal.

[0031] Beneficial Effects

[0032] The present invention discloses a packaging method for a packaging structure of a planar power device, provides a single-sided precise plastic sealing and low-temperature bonding protective film process, simplifies the packaging process, and compared with the traditional wire bonding method, the FC process transmission performance is improved, the interconnection structure size is short, the inductance, resistance and capacitance are reduced, the signal integrity, the radio frequency performance is better, the production efficiency is improved and the production cost is reduced; the traditional wire bonding method is avoided, and the resistance R between the chip and the lead frame is reduced. D , reducing the bond wire resistance R W , thereby achieving the purpose of reducing the on-resistance RDS (on) of the packaged product; the package structure formed by the present invention is applied to planar power devices, and the metal bump under the chip on the front side of the chip is flipped onto the etched surface of the three-dimensional metal frame, and the chip and the PCB are directly connected through the metal bump under the chip and the folding of the three-dimensional metal frame, which simplifies the package structure, avoids the traditional wire bonding process, reduces the package resistance, and increases the current carrying capacity; at the same time, the interconnection distance between the chip and the outside world is shortened, and the conductive effect of the chip is enhanced; the back side of the chip is exposed and directly welded to the PCB for heat dissipation, which improves the heat dissipation capacity of the package, improves the stability of the chip when it runs at high speed, and improves the quality of the product; in addition, the metal pins of the three-dimensional metal frame are in a concave arc columnar shape, which enhances the bonding force between the metal pins and the plastic packaging material, and achieves the purpose of increasing product reliability. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 A flow chart of a packaging method for a packaging structure applied to a planar power device according to the present invention;

[0034] Figure 2 A schematic diagram of a cross-sectional structure of a packaging structure applied to a planar power device of the present invention;

[0035] Figure 3 A schematic diagram of a cross-sectional structure of an embodiment of a packaging structure applied to a planar power device of the present invention;

[0036] Figure 4 for Figure 2 A schematic diagram of the relative positions of the chip and the three-dimensional metal frame;

[0037] Figure 5 A schematic diagram of an embodiment of a cross-sectional structure of a packaging structure applied to a planar power device of the present invention;

[0038] FIG. 6A to FIG. 6OA flowchart of a process of a packaging method for a packaging structure of a planar power device according to the present invention;

[0039] Among them: Chip 10

[0040] Metal bumps under the chip 11

[0041] Welding layer 12

[0042] Metal frame support strip 21

[0043] Metal pin 22

[0044] Cavity 26

[0045] Heat dissipation layer 30

[0046] Conductive metal layer Ⅰ61

[0047] Conductive metal layer III63

[0048] Plastic packaging material 90;

[0049] Wafer 100

[0050] Cutting channel Ⅰ110

[0051] Three-dimensional metal frame bar 200

[0052] Horizontal cutting channel Ⅲ210

[0053] Hollow pattern Ⅰ221

[0054] Hollow pattern Ⅱ222

[0055] Longitudinal cutting channel Ⅲ230

[0056] Counterpoint 250

[0057] Protective film 40. DETAILED DESCRIPTION

[0058] The present application will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the relevant invention, rather than to limit the invention. It should also be noted that, for ease of description, only the parts related to the relevant invention are shown in the accompanying drawings.

[0059] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0060] The present invention is a flow chart of a packaging method for a packaging structure of a planar power device, as shown in FIG. Figure 1 As shown:

[0061] Step S1: preparing incoming wafers;

[0062] Step S2: using a dicing process to cut the wafer into a plurality of independent chips;

[0063] Step S3: preparing a three-dimensional metal frame bar, forming a metal frame support bar by a half-etching process, and forming metal pins at both ends of the etched surface of the metal frame support bar to form a mold cavity;

[0064] Step S4: sequentially flip the front side of the chip into the cavity of the three-dimensional metal frame bar;

[0065] Step S5: plastic-sealing the three-dimensional metal frame strip and the new chip unit by a film-assisted plastic-sealing single-sided molding process;

[0066] Step S6: exposing the upper surface of the metal pins of the three-dimensional metal frame strip and the heat dissipation layer on the back side of the chip through a grinding process;

[0067] Step S7: laminating a protective film on the front surface of the three-dimensional metal frame strip through a lamination process;

[0068] Step S8: forming a conductive metal layer I and a conductive metal layer III on the upper surface of the metal pin and the surface of the heat dissipation layer respectively by sputtering, chemical deposition, printing or spraying;

[0069] Step S9: dividing the package body into a plurality of package structure units.

[0070] The examples are as follows:

[0071] The present invention provides a packaging structure for a planar power device, such as Figures 2 to 5 As shown, the front side of the chip 10 is provided with a plurality of metal bumps 11 under the chip, and the back side is provided with a heat dissipation layer 30. One end of the metal bump 11 under the chip is connected to the electrode of the chip 10 (the electrode is not shown in the figure), and the electrode of the chip 10 is buried in the silicon base under the passivation layer on the surface of the chip; the other end of the metal bump 11 under the chip is provided with a welding layer 12, which becomes the I / O terminal of the chip 10, and the solder used for the welding layer 12 can be one metal selected from titanium, copper, silver, nickel, gold, tin, tin-silver, or a combination of several metals.

[0072] The cross-sectional dimension of the heat dissipation layer 30 is not less than the cross-sectional dimension of the chip 10, and its material is preferably metallic copper with excellent conductive properties. The heat dissipation layer 30 is arranged on the back side of the chip 10. The chip 10 is directly soldered to the PCB through the heat dissipation layer 30 for heat dissipation, thereby improving the heat dissipation capacity of the package, improving the quality of the product, and achieving excellent heat dissipation performance of the packaged product.

[0073] The three-dimensional metal frame 20 includes a plurality of metal frame support bars 21 and metal pins 22 . The back of the metal frame support bars 21 is an etched surface. The metal pins 22 are arranged at both ends of the etched surface of each metal frame support bar 21 .

[0074] Generally, the metal frame support bars 21 are of equal length and are arranged in parallel and equidistantly on the same plane with gaps between them. The cross-section of the metal pins 22 is circular, rectangular, hexagonal, etc. Figure 4 The cross section of the metal pin 22 is shown as a rectangle. The etched surface of the metal frame support bar 21 and the inner side of the metal pin 22 form a cavity 26. The etched surface of the metal frame support bar 21 is a rough surface, which helps to strengthen the connection between the three-dimensional metal frame 20, the metal pin 22 and the vertical MOSFET chip 10.

[0075] The front side of the chip 10 is flipped inside the cavity 26 , and the metal bumps 11 under the chip are fixedly connected to the etched surface of the metal frame support bar 21 through the welding layer 12 , and are electrically connected to the three-dimensional metal frame 20 .

[0076] The chip 10 is directly electrically connected to the PCB by the metal bump 11 under the chip and the folding of the three-dimensional metal frame 20, and the chip 10 is efficiently cooled by the PCB, which shortens the distance between the chip 10 and the outside world, enhances the conductive effect of the chip, avoids the use of traditional wire bonding, and reduces the resistance R between the chip drain and the lead frame. D , reducing the bond wire resistance R W , thereby achieving the purpose of reducing the on-resistance RDS (on) of the packaged product.

[0077] The front of the three-dimensional metal frame 20 is a flat exposed surface, and a protective film 40 with adhesive backing is provided, such as Adwill LC tape. The protective film 40 has a uniform thickness and is attached to the front of the three-dimensional metal frame 20 through a lamination process. It can be carried out at a relatively low temperature, and is easy to install, thereby reducing the risk of damage to the circuit due to heat. It can protect the chip from external solvents, moisture, impact, etc., and at the same time, electrically insulate the chip from the external environment. It can also block light to minimize the impact of light on the circuit surface.

[0078] The plastic encapsulation material 90 fills and encapsulates the gaps between the three-dimensional metal frame 20 and the chip 10 and the metal frame support bars 21 as a whole. The gaps between the metal frame support bars 21 form a guide channel for the plastic encapsulation material 90, and only the outer surface of the heat dissipation layer 30 and the upper surface 223 of the metal pin are exposed. The plastic encapsulation material 90 arranged between the chip 10 and its heat dissipation layer 30 and the metal pin 22 can effectively prevent short circuits caused by voltage breakdown, thereby improving product reliability.

[0079] In an optional embodiment, the metal pin 22 is an integral structure with the three-dimensional metal frame 20, and the metal pin 22 is in a concave arc column shape, and its curvature R is generated during the half-etching process of the three-dimensional metal frame 20 due to the difference in etching rate, such as Figure 3 As shown, the actual required arc R is obtained by controlling the half-etching process. The concave arc shape of the metal pin 22 can also increase the bonding force between the metal pin 22 and the plastic packaging material 90, thereby achieving the purpose of increasing product reliability.

[0080] In an optional embodiment, the cylindrical surface of the metal pin 22 may also be a rough surface with a roughness Ra ranging from Ra 0.2 to 0.4, which may also increase the bonding force between the metal pin 22 and the plastic packaging material 90 to achieve the purpose of increasing product reliability.

[0081] In an optional embodiment, the plastic packaging material 90 may also be exposed on both sides of the metal frame body 21. Figure 5 shown.

[0082] In an optional embodiment, a packaging structure of the present invention for a planar power device also includes a conductive metal layer I61 arranged on the upper surface 223 of the metal pin and a conductive metal layer III63 arranged on the outer surface of the heat dissipation layer 30. The conductive metal layer I61 and the conductive metal layer III63 are used for subsequent mounting of the packaged chip, so as to facilitate electrical connection and heat dissipation with other external devices.

[0083] The present invention provides a packaging method for a packaging structure of a planar power device, such as Figures 6A to 6O As shown, the process is as follows:

[0084] Step 1: Fig. 6A and Figure 6B As shown, the incoming wafer 100 is prepared, and qualified wafers are selected through the incoming material inspection process, and a cleaning process is performed to remove dust, oil, etc. There are neatly arranged horizontal and vertical cutting lanes Ⅰ110 on the wafer 100. The cutting lanes Ⅰ110 pre-divide the wafer 100 into a plurality of chips 10. The front side of each chip 10 is provided with a plurality of under-chip metal bumps 11, and the back side is provided with a heat dissipation layer 30. One end of the under-chip metal bump 11 corresponds to the electrode of the chip 10 (the electrode is not shown in the figure), and the electrode of the chip 10 is buried in the silicon base under the passivation layer on the surface of the chip; the other end of the under-chip metal bump 11 is provided with a welding layer 12.

[0085] Step 2: Figure 6C and Fig.6D As shown, a plurality of independent chips 10 are formed along the cutting path I 110 by using a cutting process. Fig.6D It is a front view of the chip, showing the metal bumps 11 under the chip in a 3*5 array.

[0086] Step 3: Fig. 6E , Fig. 6F and Figure 6G As shown, a three-dimensional metal frame bar 200 is prepared. The material of the three-dimensional metal frame bar 200 is selected with reference to the lead frame of the chip carrier used for integrated circuits, and the etching surface on the back side is used as the working surface. Fig. 6E is a top view of the back side of the three-dimensional metal frame bar 200, Fig. 6F and Figure 6G for Fig. 6E In the BB cross-sectional view, the three-dimensional metal frame bar 200 is etched on the back of the three-dimensional metal frame bar 200 by a half-etching process to remove the excess metal material, and a plurality of hollow patterns I221 and hollow patterns II222 and alignment points 250 are arranged in an array on the back of the three-dimensional metal frame bar 200 to form an etching surface, and a horizontal cutting path III210 and a vertical cutting path III230 are designed. The alignment points 250 are arranged on the four sides of the three-dimensional metal frame bar 200, the hollow patterns I221 and the hollow patterns II222 are parallel and staggered in the center of the three-dimensional metal frame bar 200, and are both equal-length rectangles, and the width of the hollow pattern I221 is greater than the width of the hollow pattern II222. The hollow pattern I 221 divides the three-dimensional metal frame bar 200 into a plurality of block-shaped metal frame bodies, and the hollow pattern II 222 is parallel to the hollow pattern I 221 and further divides the metal frame body into a plurality of strip-shaped metal frame support bars 21. Fig. 6E In the figure, four hollow patterns II 222 are arranged between adjacent hollow patterns I 221, and the hollow patterns II 222 divide the metal frame body into five metal frame support bars 21. Symmetrical metal columns are formed on both ends of the etched surface of the metal frame support bar 21 by sputtering, corrosion, chemical deposition, printing or spraying in sequence as metal pins 22, and the metal pins 22 are located on the inner side of the long sides of the hollow patterns I 221 and the hollow patterns II 222, as shown in FIG. Fig. 6F As shown, the transverse cutting path III 210 is avoided so that the metal pins 22 are not damaged.

[0087] The longitudinal cutting road III230 cuts the hollow pattern I221 in parallel with the length direction of the hollow pattern I221. Generally, the longitudinal cutting road III230 coincides with the center line of the hollow pattern I221. For the outermost hollow pattern I221, the longitudinal cutting road III230 only cuts off a part of the hollow pattern I221 along the length direction of the hollow pattern I221.

[0088] The transverse cutting path III 210 is set on the upper and lower sides of the three-dimensional metal frame bar 200 and passes through the upper and lower ends of the hollow pattern I 221 and the hollow pattern II 222 to pre-cut the metal frame support bars 21 from the three-dimensional metal frame bar 200 one by one.

[0089] The etched surfaces of the five metal frame support bars 21 and the metal pins 22 thereon together form a cavity 26, such as Fig. 6F As shown; or, when the three-dimensional metal frame bar 200 is formed, the raw material of the three-dimensional metal frame bar 200 is removed by a semi-etching process to remove excess metal material, and the above-mentioned array-arranged multiple hollow patterns I221 and hollow patterns II222, alignment points 250 and metal pins 22 are formed on the etched surface, and transverse cutting paths III210 and longitudinal cutting paths III230 are designed. Due to the different etching speeds, the cylindrical surface of the metal pin 22 is a concave arc column, and its curvature R is controlled by the actual process. The metal pin 22 and the metal frame support bar 21 are an integrated structure, and the five metal frame support bars 21 and the metal pins 22 thereon together form a cavity 26, as shown Figure 6G shown.

[0090] Alternatively, a plurality of metal pillars of the same height are formed by photoresist patterning and metal deposition, and the bottoms of the metal pillars are connected to the etched surfaces of the metal frame support bars 21 by welding to form metal pins 22. The solder used for welding can be one of the metals selected from titanium, copper, silver, nickel, gold, tin, and tin-silver, or a combination of several metals.

[0091] Alternatively, prepare a metal sheet, use a high-reflection laser to form several metal columns of the same height through a laser cutting process, and connect the bottom of the metal column to the etched surface of the above-mentioned metal frame support bar 21 through a welding process to form a metal pin 22. The solder used for welding can be one of titanium, copper, silver, nickel, gold, tin, tin-silver, or a combination of several of them.

[0092] In this step, the surface of the metal pin 22 or the surface of the metal pin 22 and the etched surface of the three-dimensional metal frame bar 200 may be roughened by plasma etching process, and the roughness Ra is controlled in the range of Ra 0.2-0.4.

[0093] Step 4: Figure 6H and Fig.6I As shown, the front side of the chip 10 is flipped and placed into the cavity 26 of the three-dimensional metal frame bar 200 in sequence, and the metal bumps 11 under the chip are fixedly connected to the metal frame support bar 21 through the welding layer 12 to realize the circuit conduction of the chip 10. Figure 6H is a schematic diagram of the relative positions of the three-dimensional metal frame bar 200 and the chip 10, Fig.6I for Figure 6H CC cross-section diagram.

[0094] The welding layer 12 is a metal selected from titanium, copper, silver, nickel, gold, tin, and tin-silver, or a combination of several metals.

[0095] Step 5: Figure 6JAs shown, after the encapsulation material 90 is melted by the film-assisted encapsulation single-sided molding process (FAM), the three-dimensional metal frame bar 200 and the chip 10 are covered by pressure, and the hollow pattern I 221 and the hollow pattern II 222 are filled. The hollow pattern I 221 and the hollow pattern II 222 play a role in guiding the encapsulation material 90 to form a guiding channel.

[0096] Step 6: Figure 6K As shown, the upper surface 223 of the metal pins of the three-dimensional metal frame bar 200 and the heat dissipation layer 30 on the back side of the chip 10 are exposed through the grinding process.

[0097] Step 7: Figure 6L As shown, at a relatively low temperature, a protective film 40 with adhesive backing, such as Adwill LC tape, is attached to the flat front side of the three-dimensional metal frame strip 200 through a lamination process, which is easy to install, thereby reducing the risk of circuit damage due to heat and simplifying the traditional EMC process.

[0098] Step 8: Figure 6M As shown, a conductive metal layer I61 and a conductive metal layer III63 are respectively manufactured on the upper surface 223 of the metal pin and the surface of the heat dissipation layer 30 by sputtering corrosion, chemical deposition, printing or spraying. The conductive metal layer I61 and the conductive metal layer III63 are used for the subsequent mounting of the packaged chip.

[0099] Step 9: Figure 6N and Fig.6O As shown, the above-mentioned package body is divided into a package structure monomer of a plurality of chips along the horizontal cutting road III210 and the vertical cutting road III230, and the chip 10 is folded upward through the metal bump 11 under the chip and the three-dimensional metal frame 20 to be directly interconnected with the back side of the chip 10 and the PCB, so as to realize direct and efficient heat dissipation of the chip 10 through the PCB.

[0100] The above is only a preferred specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed in the embodiments of the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. A packaging method for a packaging structure of a planar power device, the process method of which is as follows: Step 1, preparing an incoming wafer (100), on which neatly arranged horizontal and vertical intersecting cutting paths I (110) are arranged, the cutting paths I (110) pre-dividing the wafer (100) into a plurality of chips (10), each chip (10) being provided with a plurality of under-chip metal bumps (11) on the front side and a heat dissipation layer (30) on the back side, one end of the under-chip metal bump (11) corresponding to the electrode of the chip (10), and a welding layer (12) being provided on the other end; Step 2: using a cutting process to form a plurality of independent chips (10) along the cutting path I (110); Step 3: prepare a three-dimensional metal frame bar (200), with the etching surface on the back thereof serving as a working surface. The three-dimensional metal frame bar (200) is etched on the back of the three-dimensional metal frame bar (200) by a half-etching process to remove excess metal material. A plurality of hollow patterns I (221) and hollow patterns II (222) and alignment points (250) are arrayed on the back of the three-dimensional metal frame bar (200), and an etching surface is formed. A horizontal cutting path III (210) and a vertical cutting path III (230) are designed. The alignment points (250) are arranged on four sides of the three-dimensional metal frame bar (200) at the top, bottom, left and right sides. The hollow pattern I (221) and the hollow pattern II (222) are parallel and staggeredly distributed in the center of the three-dimensional metal frame bar (200), both of which are rectangular with equal length, and the width of the hollow pattern I (221) is greater than the width of the hollow pattern II (222); the hollow pattern I (221) divides the three-dimensional metal frame bar (200) into a plurality of block-shaped metal frame bodies, and the hollow pattern II (222) is parallel to the hollow pattern I (221) and further divides the metal frame body into a plurality of strip-shaped metal frame support bars (21), and the hollow pattern II (222) divides the metal frame body into a plurality of metal frame support bars (21); Metal pins (22) are formed on both ends of the etched surface of the metal frame support bar (21), and the metal pins (22) are located inside the long sides of the hollow pattern I (221) and the hollow pattern II (222); The longitudinal cutting path III (230) cuts the hollow pattern I (221) in parallel with the length direction of the hollow pattern I (221); the transverse cutting path III (210) is arranged on the upper and lower sides of the three-dimensional metal frame strip (200) and passes through the upper and lower ends of the hollow pattern I (221) and the hollow pattern II (222), so as to pre-cut the metal frame support strips (21) from the three-dimensional metal frame strip (200) one by one; The etched surface of the metal frame support bar (21) and the metal pins (22) thereon together form a cavity (26); Step 4: sequentially flip the front side of the chip (10) into the cavity (26) of the three-dimensional metal frame bar (200), align the chip through the alignment point (250), and fix the metal bump (11) under the chip to the metal frame support bar (21) through the welding layer (12), so as to realize circuit conduction of the chip (10); Step 5: After the plastic encapsulation material (90) is melted by a film-assisted plastic encapsulation single-sided molding process, the three-dimensional metal frame strip (200) and the chip (10) are covered by pressure, and the hollow pattern I (221) and the hollow pattern II (222) are filled. The hollow pattern I (221) and the hollow pattern II (222) play a role in guiding the plastic encapsulation material (90) to form a guiding channel; Step six: exposing the upper surface (223) of the metal pins of the three-dimensional metal frame strip (200) and the heat dissipation layer (30) on the back side of the chip (10) through a grinding process; Step 7: Laminating a protective film (40) with adhesive backing onto the flat front surface of the three-dimensional metal frame strip (200) through a lamination process; Step eight, forming a conductive metal layer I (61) and a conductive metal layer III (63) on the upper surface (223) of the metal pin and the surface of the heat dissipation layer (30) respectively by sputtering, chemical deposition, printing or spraying; Step nine: along the horizontal cutting line III (210) and the vertical cutting line III (230), the package structure completed in the above step eight is divided into package structure monomers of a plurality of chips, and the chip (10) is folded upward through the metal bump (11) under the chip and the three-dimensional metal frame (20) to be directly connected to the back side of the chip (10) and the PCB for heat dissipation.

2. The packaging method according to claim 1, characterized in that: In step 3, the forming process of the metal pin (22) is as follows: Symmetrical metal columns are formed on both ends of the etched surface of the metal frame support bar (21) in sequence by sputtering, corrosion, chemical deposition, printing or spraying to serve as metal pins (22).

3. The packaging method according to claim 1, characterized in that: In step 3, the forming process of the metal pin (22) is as follows: A plurality of metal columns of the same height are formed by photoresist patterning and metal deposition, and the bottoms of the metal columns are connected to the etched surfaces of the metal frame support bars (21) by welding processes to form metal pins (22).

4. The packaging method according to claim 1, characterized in that: In step 3, the forming process of the metal pin (22) is as follows: A metal sheet is prepared, and a high-reflection laser is used to form a plurality of metal columns of the same height through a laser cutting process, and the bottom of the metal column is connected to the etched surface of the metal frame support bar (21) through a welding process to form a metal pin (22).

5. The packaging method according to claim 1, characterized in that: In step 3, the forming process of the metal pin (22) is as follows: When the three-dimensional metal frame bar (200) is formed, the three-dimensional metal frame bar (200) is etched on the back side of the three-dimensional metal frame bar (200) through a half-etching process to remove excess metal material, and a plurality of hollow patterns I (221), hollow patterns II (222), alignment points (250) and metal pins (22) are arranged in an array on the back side of the three-dimensional metal frame bar (200), and a transverse cutting path III (210) and a longitudinal cutting path III (230) are designed. Due to different etching speeds, the cylindrical surface of the metal pin (22) is in the shape of a concave arc column, and its curvature R is controlled by the actual process. The metal pin (22) and the metal frame support bar (21) are an integral structure.

6. The packaging method according to any one of claims 1 to 5, characterized in that: The surface of the metal pin (22) or the surface of the metal pin (22) and the etched surface of the three-dimensional metal frame bar (200) are roughened by a plasma etching process, and the roughness Ra is controlled in the range of Ra 0.2-0.

4.

7. The packaging method according to claim 1, characterized in that: The welding layer (12) is a metal selected from the group consisting of titanium, copper, silver, nickel, gold, tin, and tin-silver, or a combination of several metals.

8. The packaging method according to claim 1, characterized in that: The cross-sectional dimension of the heat dissipation layer (30) is not smaller than the cross-sectional dimension of the chip (10).

9. The packaging method according to claim 1, characterized in that: The cross section of the metal pin (22) is circular, rectangular or hexagonal.